Circuit board electroplating device
By setting up buffer containers and inclined air holes in the circuit board plating device, combined with nylon shielding plates, the pinhole problem caused by bubble adhesion is solved and the plating quality and reliability are improved.
Patent Information
- Application Number
- CN202420413077.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-04
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-03-04
AI Technical Summary
During the production process of printed circuit boards, bubbles adhere to the board surface, causing pinholes and depressions, which affects the quality and reliability of electroplating. Especially when the circuit board becomes thicker and the aperture becomes smaller, the traditional electroplating process is difficult to be effective. Defects that prevent bubble formation.
A circuit board electroplating device is designed, including a main tank, a auxiliary tank, a circulating water pipe, an air pump and a buffer container. The air hole faces the circuit board and is inclined at 45°. The liquid outlet of the auxiliary tank is equipped with a nylon shielding plate. The side wall of the buffer container is There are drainage holes to reduce the impact of liquid medicine and bubble adhesion, and improve the way of gas discharge.
It effectively reduces the probability of bubbles adhering to the board surface, reduces the occurrence of pinholes, and improves the plating quality and reliability of the circuit board, especially in the case of thin lines and small line spacing.
Smart Images

Figure CN221877221U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of printed circuit board manufacturing, in particular to a circuit board electroplating device. Background Art
[0002] Pinholes are caused by the adsorption of many small bubbles on the circuit board. The location where the bubbles are attached is surrounded by air, forming a small "vacuum chamber" that the electroplating solution cannot enter, resulting in the inability to electroplate the location where the bubbles are located, thus causing pinholes. There are two ways in which bubbles are generated: one is due to the presence of supersaturated gas in the electroplating solution, and the other is that small bubbles of hydrogen are released during the electroplating process and float in the plating solution.
[0003] As the circuit board becomes thicker and the aperture becomes smaller, the line width / line spacing also develops in the direction of fine lines and small line spacing. As a result, bubbles generated during the production process of the circuit board are attached to the circuit board surface, which will cause defects such as depressions and pinholes during pattern electroplating, resulting in open circuits and short circuits. Especially after the circuit board reaches the post-process, slight depressions and pinholes on the board surface will cause abnormal reliability such as abnormal circuit board assembly and poor welding. Therefore, how to improve the pinholes on the board surface after pattern electroplating is a long-term problem faced by the circuit board industry.
[0004] In the traditional gantry pattern electroplating process, the electroplating tank uses a main tank and a sub-tank in combination. The main tank and the sub-tank are connected by a circulating water pipe at the bottom. The liquid medicine enters the bottom of the main tank through the circulating water pipe, and the water inlet in the main tank is designed to be blocked by a PP board with an inclined angle of 45°. Because the liquid medicine circulates between the main tank and the sub-tank for a long time, during pattern electroplating, the liquid medicine enters the main tank from the bottom circulating pipe and directly gushes onto the board, which easily forms pinholes.
[0005] In view of this, it is necessary to provide a new device to solve the above technical problems. Utility Model Content
[0006] The technical problem to be solved by the utility model is to provide a circuit board electroplating device, which can effectively prevent pinhole defects of the circuit board.
[0007] The technical solution of the utility model is as follows:
[0008] A circuit board electroplating device comprises a main tank, a sub-tank, a circulating water pipe connecting the main tank and the sub-tank, an air pumping pipe arranged in the main tank and connected to an air supply device, and a plurality of air pumping holes arranged on the air pumping pipe, a buffer container connected to the circulating water pipe is arranged at the bottom of the main tank, a plurality of drainage holes are arranged on the side wall of the buffer container, and the drainage holes are arranged opposite to the side wall of the main tank.
[0009] Furthermore, the drainage hole is directly opposite to the side wall of the main tank connected to the circulating water pipe.
[0010] Furthermore, the buffer container is a square container.
[0011] Furthermore, the air holes are arranged toward the circuit board.
[0012] Furthermore, the air holes are oriented at an angle of 45° downward.
[0013] Furthermore, a nylon shielding plate is provided at the liquid outlet of the auxiliary tank.
[0014] Compared with the prior art, the circuit board electroplating device provided by the utility model has the following beneficial effects:
[0015] 1. The circuit board electroplating device provided by the utility model has a buffer container connected to a circulating water pipe at the bottom of the main tank, and a plurality of drainage holes are provided on the side wall of the buffer container. The drainage holes are arranged opposite to the side wall of the main tank. The circulating water discharged from the auxiliary tank first enters the buffer container and is then discharged from the drainage holes on the side wall of the buffer container. The liquid medicine sprayed from the drainage holes directly gushes to the side wall of the main tank, thereby changing the gushing direction of the liquid medicine in the main tank in the prior art, buffering the impact force of the liquid medicine, and reducing the probability of pinholes caused by the saturated gas (bubbles) brought by the gushing of the liquid medicine attached to the board surface.
[0016] Second, in the prior art, the aeration opening of the electroplating tank near the filter water inlet is opened at a 45° angle downward, and the opening direction is toward the titanium basket (such as Figure 2 The air holes of the filter water inlet for air circulation face the titanium basket. The gas generated by the supersaturated gas in the electroplating solution after the air pumping floats in the tank liquid in the form of small bubbles, and adheres to the board surface during pattern electroplating, thereby causing pinholes. The circuit board electroplating device provided by the utility model sets the air holes on the air pumping pipe toward the circuit board, and the air holes are oriented downward at an angle of 45°. Compared with the prior art, the air stirring method is changed. During the pattern electroplating process, the impact force of the air is used to flush out the bubbles attached to the circuit board, thereby reducing the probability of pinholes caused by bubbles attached to the board.
[0017] 3. In the prior art, the electroplating solution in the auxiliary tank is not filtered by a shielding plate, and the supersaturated gas in the electroplating solution is directly circulated and pumped into the main tank, which is easy to form pinholes. The circuit board electroplating device provided by the utility model is provided with a nylon shielding plate at the liquid outlet of the auxiliary tank, and the supersaturated gas in the tank liquid of the auxiliary tank is filtered and then transported to the main tank, further reducing the probability of bubbles adhering to the board surface to cause pinholes. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0019] Figure 1 It is a structural schematic diagram of a circuit board electroplating device of the utility model;
[0020] Figure 2 yes Figure 1 A schematic diagram of the main slot from another angle;
[0021] Figure 3 yes Figure 1 Enlarged view of part A in . DETAILED DESCRIPTION
[0022] In order to enable those skilled in the art to better understand the technical solutions in the embodiments of the present invention and to make the above-mentioned purposes, features and advantages of the present invention more obvious and understandable, the specific implementation methods of the present invention are further described below.
[0023] It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in each embodiment of the present invention described below can be combined with each other as long as there is no conflict between them.
[0024] Please refer to Figure 1-Figure 3 ,in Figure 1 It is a structural schematic diagram of a circuit board electroplating device of the utility model; Figure 2 yes Figure 1 A schematic diagram of the main slot from another angle; Figure 3 yes Figure 1 The wire plate electroplating device provided by the utility model comprises a main tank 1, a sub-tank 2, a circulating water pipe 3 connecting the main tank and the sub-tank, an air pumping pipe 4 arranged in the main tank, a plurality of air pumping holes 5 arranged in the air pumping pipe 4, and a buffer container 6 arranged at the bottom of the main tank 1, and the circulating water pipe 3 is connected to the buffer container 6.
[0025] The main tank 1 and the sub-tank 2 contain electroplating liquid, wherein the electroplating liquid in the main tank 1 overflows from the top into the sub-tank 2, and the electroplating liquid in the sub-tank 2 is filtered and then pumped into the main tank by the circulation pump 8 to replenish the electroplating liquid in the main tank, and the main tank 1 and the sub-tank 2 are connected at the bottom by the circulation water pipe 3.
[0026] In the present invention, the electroplating liquid replenished from the auxiliary tank 2 to the main tank 1 enters the main tank through the circulating water pipe 3, first enters the buffer container 6, and then is discharged through the drainage hole 61 on the side wall of the buffer tank 6 to buffer the impact of the electroplating liquid. In this embodiment, the drainage hole 61 is arranged directly opposite to the side wall of the main tank, and the electroplating liquid gushing out of the drainage hole 61 collides with the side wall of the main tank, further reducing the probability of pinholes caused by the saturated gas (bubbles) brought by the gushing of the liquid attached to the board surface of the circuit board 200. Preferably, the drainage hole 61 is directly opposite to the side wall of the main tank connected to the circulating water pipe, which increases the flow path of the electroplating liquid and reduces the generation of bubbles.
[0027] In the utility model, the buffer container 6 is a square container, which is convenient for installation.
[0028] The pumping pipe 4 is connected to an external air supply device (as shown in the figure), and a pumping hole 5 is provided on the pumping pipe 4. After the air supply device provides compressed air, it is discharged from the pumping hole 5 on the pumping pipe to stir the electroplating solution so that the electroplating solution is mixed evenly. In this embodiment, the pumping pipe 4 is arranged at the bottom of the main tank 1, and the pumping hole 5 thereof is tilted downward at 45° and is arranged toward the circuit board. During the pattern electroplating process, the impact force of the air is used to flush away the bubbles attached to the circuit board 200, thereby reducing the probability of pinholes caused by bubbles attached to the board.
[0029] Preferably, a nylon baffle 7 is provided at the liquid outlet of the auxiliary tank 2 to filter the supersaturated gas in the plating liquid of the auxiliary tank, and remove the plating liquid with saturated gas from entering the main tank, thereby further reducing the probability of bubbles in the plating liquid adhering to the surface of the circuit board.
[0030] The circuit board electroplating device of the utility model is adopted, and the process parameters are set as follows: copper plating current parameter 18ASF*4200s, tin plating current parameter 7ASF*540s, pulse parameter 1# waveform (pulse width 400 / 20, reverse ratio 1 / -200).
[0031] After testing, the inspection results of the test board 10pnl and small batch 120pnl showed that the copper thickness was qualified, and the AOI first-time yield was 95% and 98.33% respectively, without pinholes, and the inspection results were qualified.
[0032] The circuit board electroplating device of the utility model improves the structure from multiple aspects, and effectively prevents pinhole defects of the circuit board.
[0033] The above is a detailed description of the embodiments of the present invention, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations made to these embodiments without departing from the principle and spirit of the present invention still fall within the scope of protection of the present invention.
Claims
1. A circuit board electroplating device, characterized in that: It includes a main tank, a sub-tank, a circulating water pipe connecting the main tank and the sub-tank, an air pumping pipe arranged in the main tank and connected to the air supply device, and a plurality of air pumping holes arranged on the air pumping pipe. A buffer container connected to the circulating water pipe is arranged at the bottom of the main tank, and a plurality of drainage holes are arranged on the side wall of the buffer container. The drainage holes are arranged opposite to the side wall of the main tank.
2. The circuit board electroplating device according to claim 1, characterized in that: The drainage hole is directly opposite to the side wall of the main tank connected to the circulating water pipe.
3. The circuit board electroplating device according to claim 1, characterized in that: The buffer container is a square container.
4. The circuit board electroplating device according to claim 1, characterized in that: The air-injection holes are arranged toward the circuit board.
5. The circuit board electroplating device according to claim 4, characterized in that: The air-injection hole is oriented at an angle of 45° downward.
6. The circuit board electroplating device according to claim 1, characterized in that: A nylon shielding plate is arranged at the liquid outlet of the auxiliary tank.