Continuous reinforced concrete composite asphalt pavement
By adopting a steel frame structure and a triangular binding shape in the continuously reinforced concrete composite asphalt pavement, the problems of insufficient load strength and construction complexity in the existing technology are solved, and a pavement structure with high shear strength and high load-bearing capacity is achieved. Simplifies the construction process and improves overall rigidity and hydrophobic properties.
Patent Information
- Application Number
- CN202420446177.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-03-08
AI Technical Summary
In scenarios where the existing continuous reinforced concrete composite asphalt pavement is used under heavy loads, there is still room for improvement in the strength of the horizontal and vertical erection of steel bars. It is difficult to effectively resist deformation and torsion, and the construction complexity is high.
A steel frame structure is adopted, which includes pre-embedded vertical steel bars, longitudinal steel bars and transverse steel bars. The triangular binding shape is used to increase the tensile force distribution and the bonding area between steel bars and concrete. Combined with the laying of concrete and asphalt surface layers, it forms a high shear resistance Strength and high load-carrying capacity pavement structure.
It improves the shear strength and shear load-bearing capacity of the pavement, enhances the bonding force between steel bars and concrete, can effectively resist deformation and torsion under load, simplifies the construction process, and improves the overall rigidity and hydrophobic performance.
Smart Images

Figure CN221877592U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of composite asphalt pavement, in particular to a continuous reinforced concrete composite asphalt pavement. Background Art
[0002] Continuously reinforced concrete composite asphalt pavement is a pavement structure that combines concrete and asphalt. It consists of a concrete surface layer and an asphalt surface layer.
[0003] In the prior art, there is a Chinese utility model patent document with publication number CN215561620U, which discloses a crack-free continuously reinforced concrete composite pavement structure. The continuous reinforced concrete described therein is installed horizontally and vertically with steel bars, which is similar to the square steel bar binding shape. For the installation of the continuous reinforced concrete layer, straight steel bars can be conveniently used for binding, which reduces the complexity and construction period of the construction. However, for the use scenarios with larger loads, the continuous reinforcement strength of the horizontal and vertical installation method mentioned above still has a large room for improvement. For this reason, we propose a continuously reinforced concrete composite asphalt pavement. Utility Model Content
[0004] In view of the deficiencies in the prior art, the utility model provides a continuous reinforced concrete composite asphalt pavement having the advantages of high shear strength, high bearing capacity, high hydrophobicity, etc., which can effectively solve the problems in the background technology.
[0005] To achieve the above-mentioned purpose, the technical solution adopted by the utility model is: a continuous reinforced concrete composite asphalt pavement, comprising a gravel layer, a concrete base layer is paved on the surface of the gravel layer, and a concrete surface layer is paved on the surface of the concrete base layer, a steel frame is erected between the concrete base layer and the concrete surface layer, and an asphalt surface layer is paved on the surface of the concrete surface layer;
[0006] The steel frame includes a plurality of vertical steel bars pre-embedded in the gravel layer, and the plurality of vertical steel bars are arranged in groups along the longitudinal direction of the road surface. Longitudinal steel bars are also arranged between the plurality of groups of vertical steel bars, and transverse steel bars are arranged at the joints between the plurality of groups of vertical steel bars and the longitudinal steel bars. The transverse steel bars are based on the relative inclination of the vertical steel bars to form a stable triangle.
[0007] Preferably, the plurality of vertical steel bars, longitudinal steel bars and transverse steel bars are all tied together by wire.
[0008] Preferably, the horizontal spacing between the plurality of vertical steel bars is 350-500 mm.
[0009] Preferably, the spacing between the plurality of longitudinal steel bars is 180-250 mm.
[0010] Preferably, the concrete surface layer comprises cast concrete, and the surface layer of the cast concrete is formed with protrusion one and protrusion two.
[0011] Preferably, two protrusions 2 are provided, respectively located at the adjacent edges on both sides of the road surface.
[0012] Preferably, the thickness of the asphalt surface layer is equivalent to the height of the second protrusion.
[0013] Preferably, the steel frame is embedded in the inner layer of the gravel layer, the concrete base layer is bonded to the gravel layer, the concrete surface layer is bonded to the concrete base layer, and the asphalt surface layer is bonded to the surface layer of the concrete surface layer.
[0014] Preferably, the concrete base layer and the concrete surface layer are both bonded to the steel frame.
[0015] Preferably, the thickness of the gravel layer is 5-10 mm.
[0016] Compared with the prior art, the utility model provides a continuous reinforced concrete composite asphalt pavement, which has the following beneficial effects:
[0017] The continuous reinforced concrete composite asphalt pavement is provided with a steel bar frame. Because the binding shape of the steel bar frame is similar to a triangle, the triangular binding shape can form a continuous tension force distribution in the concrete structure, increase the shear strength and shear bearing capacity of the structure, and can effectively increase the bonding area between the steel bar and the concrete, making the steel bar more firm in the structure, and being able to effectively resist deformation and torsion when subjected to force, thereby improving the overall rigidity of the structure and enabling the composite asphalt pavement to withstand a larger load. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 The utility model is a structural schematic diagram of a continuous reinforced concrete composite asphalt pavement.
[0019] Figure 2 This is a structural analysis diagram of a continuous reinforced concrete composite asphalt pavement of the utility model.
[0020] Figure 3 This is a structural analysis diagram of a concrete surface layer for a continuously reinforced concrete composite asphalt pavement of the utility model.
[0021] Figure 4 The utility model is a structural schematic diagram of a steel bar frame for a continuously reinforced concrete composite asphalt pavement.
[0022] In the figure: 1. Gravel layer; 2. Concrete base layer; 3. Concrete surface layer; 4. Steel bar frame; 5. Asphalt surface layer; 31. Pouring concrete; 32. Bump 1; 33. Bump 2; 41. Vertical steel bars; 42. Longitudinal steel bars; 43. Horizontal steel bars. DETAILED DESCRIPTION
[0023] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the present invention will be further described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] In order to address the shortcomings of the existing technology, such as Figure 1 , 2 As shown, the utility model provides a continuous reinforced concrete composite asphalt pavement, in which a steel frame 4 is pre-buried in the inner layer of a gravel layer 1, a concrete base layer 2 is bonded to the gravel layer 1, and a concrete surface layer 3 is bonded to the concrete base layer 2, and an asphalt surface layer 5 is bonded to the surface layer of the concrete surface layer 3.
[0025] It should be noted that, in the process of paving the continuous reinforced concrete composite asphalt pavement, the ground of the road to be paved is first leveled, and then gravel is evenly spread on the road to be paved, the thickness of the gravel layer 1 is 5-10 mm, and the gravel layer 1 is rolled by a roller to make the surface of the gravel layer 1 uniform and flat;
[0026] After the gravel layer 1 is laid flat, a steel frame 4 is erected on the gravel layer 1 , and then a concrete base layer 2 and a concrete surface layer 3 are erected, and finally an asphalt surface layer 5 is spread.
[0027] Specifically, Figure 4 As shown, a steel frame 4 for a continuous reinforced concrete composite asphalt pavement, the steel frame 4 includes a plurality of vertical steel bars 41 pre-buried in the gravel layer 1, and the plurality of vertical steel bars 41 are arranged in groups along the longitudinal direction of the pavement, longitudinal steel bars 42 are arranged between the plurality of groups of vertical steel bars 41, and transverse steel bars 43 are arranged at the joints between the plurality of groups of vertical steel bars 41 and the longitudinal steel bars 42, and the transverse steel bars 43 are relatively inclined based on the vertical steel bars 41 to form a stable triangle.
[0028] It should be noted that the utility model is a continuously reinforced concrete composite asphalt pavement. Through the steel bar frame 4, in the process of continuous reinforcement, a plurality of vertical steel bars 41 are transversely and firmly fixed to the gravel layer 1 at a suitable spacing. The transverse spacing between the plurality of vertical steel bars 41 is most suitable to be 350-500 mm, and the plurality of vertical steel bars 41 are erected in groups along the longitudinal direction of the road surface to be paved.
[0029] Then, based on the multiple groups of vertical steel bars 41, multiple longitudinal steel bars 42 are erected, and wire is used for binding. The spacing between the multiple longitudinal steel bars 42 is 180-250mm, which is the most suitable. In addition, multiple transverse steel bars 43 are used for wire binding at the joints of the multiple vertical steel bars 41 and the longitudinal steel bars 42. The multiple transverse steel bars 43 are relatively inclined based on the vertical steel bars 41, such as Figure 4 Status shown.
[0030] Among them, because the binding shape of the steel frame 4 is similar to a triangle, the triangular binding shape can form a continuous tension force distribution in the concrete structure, increase the shear strength and shear bearing capacity of the structure, and can effectively increase the bonding area between the steel bars and the concrete, making the steel bars more firm in the structure, and can effectively resist deformation and torsion when subjected to force, thereby improving the overall rigidity of the structure and enabling the composite asphalt pavement to withstand larger loads.
[0031] Specific, and Figure 3 As shown, a concrete surface layer 3 for a continuous reinforced concrete composite asphalt pavement, the concrete surface layer 3 includes cast concrete 31, and the surface layer of the cast concrete 31 is formed with protrusion 1 32 and protrusion 2 33; there are two protrusions 2 33, which are respectively located at the adjacent edges on both sides of the road surface.
[0032] It should be noted that the utility model is a continuous reinforced concrete composite asphalt pavement. The concrete surface layer 3 is set up by mixing sand and cement in a ratio of 3:1 and then pouring. Before paving the concrete surface layer 3, sand and cement are mixed in a ratio of 4:1 and poured to form a concrete base layer 2. During the paving process of the concrete base layer 2, the concrete base layer 2 also needs to be leveled.
[0033] Another example Figure 3As shown, in order to form multiple protrusions 1 32 and 33 on the surface of the poured concrete 31, it is necessary to set up a template to support the poured concrete 31. After the concrete surface layer 3 is formed, the asphalt surface layer 5 is directly spread on the surface of the concrete surface layer 3. The ratio of sand and gravel to asphalt in the asphalt surface layer 5 is 4:1, and the laying thickness of the asphalt should be the protrusion height of the protrusion 2 33. In this way, the protrusion 2 33 formed on the poured concrete 31 protrudes to the road surface and is distributed on both sides of the road surface. In this way, during the use, domestic rainwater on the surface of the asphalt surface layer 5 can be timely leaked through the two protrusions 2 33 to the poured concrete 31 for effective discharge.
[0034] The surface of the poured concrete 31 is also formed with a plurality of protrusions 32. When domestic rainwater penetrates from the asphalt surface layer 5 to the ground, it can contact the poured concrete 31 as soon as possible to achieve drainage.
[0035] The above shows and describes the basic principle and main features of the utility model and the advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments, and the above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, and these changes and improvements fall within the scope of the utility model to be protected.
Claims
1. A continuously reinforced concrete composite asphalt pavement, characterized in that: It comprises a gravel layer (1), the surface of the gravel layer (1) is paved with a concrete base layer (2), the surface of the concrete base layer (2) is paved with a concrete surface layer (3), a steel frame (4) is erected between the concrete base layer (2) and the concrete surface layer (3), and the surface of the concrete surface layer (3) is paved with an asphalt surface layer (5); The steel bar frame (4) comprises a plurality of vertical steel bars (41) pre-buried in the gravel layer (1), and the plurality of vertical steel bars (41) are arranged in groups along the longitudinal direction of the road surface, longitudinal steel bars (42) are arranged between the plurality of groups of vertical steel bars (41), and transverse steel bars (43) are arranged at the joints between the plurality of groups of vertical steel bars (41) and the longitudinal steel bars (42), and the transverse steel bars (43) are relatively inclined based on the vertical steel bars (41) to form a stable triangle.
2. The continuous reinforced concrete composite asphalt pavement according to claim 1, characterized in that: The horizontal spacing between the plurality of vertical steel bars (41) is 350-500 mm.
3. The continuous reinforced concrete composite asphalt pavement according to claim 1, characterized in that: The spacing between the plurality of longitudinal steel bars (42) is 180-250 mm.
4. The continuous reinforced concrete composite asphalt pavement according to claim 1, characterized in that: The concrete surface layer (3) comprises cast concrete (31), and the surface layer of the cast concrete (31) is formed with a first protrusion (32) and a second protrusion (33).
5. The continuous reinforced concrete composite asphalt pavement according to claim 4, characterized in that: There are two protrusions (33), which are respectively located at the edges of both sides of the road surface.
6. The continuous reinforced concrete composite asphalt pavement according to claim 5, characterized in that: The thickness of the asphalt surface layer (5) is equivalent to the height of the second protrusion (33).
7. The continuous reinforced concrete composite asphalt pavement according to claim 1, characterized in that: The thickness of the gravel layer (1) is 5-10 mm.