Waterproof and moistureproof composite film

Through the multi-layer membrane structure design, combined with mesh fibers and polyethylene microspheres, the problems of fragile edges and poor moisture-proof performance of the composite membrane are solved, achieving excellent waterproof and moisture-proof performance and longer service life.

CN221892729UActive Publication Date: 2024-10-25ZHEJIANG HETONG DOMESTIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420382772.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-29
Publication Date
2024-10-25
Estimated Expiration
2034-02-28

Smart Images

  • Figure CN221892729U_ABST
    Figure CN221892729U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of composite films, and particularly relates to a waterproof and moistureproof composite film which comprises a wear-resistant layer, a waterproof layer, a fiber layer, a first elastic layer, a PET (polyethylene terephthalate) layer, a second elastic layer and a moistureproof layer from outside to inside, protective layers are adhered to two sides of the waterproof and moistureproof composite film, and the total thickness of the waterproof and moistureproof composite film is 165-315 microns. According to the waterproof and moistureproof composite film, through multiple waterproof and moistureproof arrangements of the waterproof layer, the fiber layer, the PET layer, the moistureproof layer and the protective layer, the waterproof and moistureproof performance of the composite film is relatively good, so that the service life and the performance of the composite film are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of composite films, and in particular relates to a waterproof and moisture-proof composite film. Background Art

[0002] Composite film is a composite material formed by alternating two or more different material layers. It is formed by combining different material layers by co-extrusion, veneer, etc.

[0003] The edges of existing composite membranes usually need to be cut and trimmed during use, which makes the edges vulnerable to damage and allows liquid to easily penetrate through the edges, thus affecting the waterproof performance of the composite membrane.

[0004] The existing composite membrane has poor moisture resistance, and the composite membrane is easily invaded by external water vapor, which affects the performance and service life of the composite membrane.

[0005] Therefore, a composite film with waterproof and moisture-proof properties is needed to solve the above problems. Utility Model Content

[0006] The purpose of the utility model is to solve the problem of insufficient waterproof and moisture-proof performance of the current composite membrane described in the above background technology, and propose a new waterproof and moisture-proof composite membrane, which has excellent waterproof and moisture-proof performance.

[0007] The technical solution adopted to achieve the above-mentioned purpose is a waterproof and moisture-proof composite film, which includes a wear-resistant layer, a waterproof layer, a fiber layer, a first elastic layer, a PET layer, a second elastic layer and a moisture-proof layer from the outside to the inside. Protective layers are bonded on both sides of the waterproof and moisture-proof composite film. A plurality of cavities are arranged in the first elastic layer and the second elastic layer, and a plurality of polyethylene microspheres are filled in the cavities. The total thickness of the waterproof and moisture-proof composite film is 165-315μm.

[0008] Furthermore, mesh polyamide fibers are arranged in the fiber layer, and the surface of the mesh polyamide fibers is covered with a reinforcing film layer.

[0009] In the above technical scheme, the mesh polyamide fiber can enhance the toughness of the composite membrane. At the same time, the utility model also processes the surface film of the mesh polyamide fiber, immerses the fiber in a cationic emulsion to form a reinforced membrane layer, and the reinforced membrane layer is formed by combining the cationic emulsion with the mesh polyamide fiber. The reinforced membrane layer has excellent waterproof properties, so that the fiber layer obtains waterproof properties while enhancing the toughness of the composite membrane.

[0010] Furthermore, the mesh spaces of the mesh polyamide fiber are filled with flame retardant particles.

[0011] In the above technical solution, flame retardant particles are filled in the mesh spaces of the mesh polyamide fibers to enhance the flame retardant ability of the composite film.

[0012] Furthermore, the diameter of the polyethylene microspheres is 5-10 μm.

[0013] In the above technical solution, the first elastic layer and the second elastic layer are layered structures, a number of cavities are opened in the layered structures, and polyethylene microspheres with good elasticity are filled in the cavities to provide better elastic properties for the composite film.

[0014] Furthermore, the thickness of the first elastic layer and the second elastic layer is 50-100 μm.

[0015] Furthermore, the waterproof layer has a thickness of 10-20 μm.

[0016] Furthermore, the fiber layer has a thickness of 20-30 μm.

[0017] Furthermore, the moisture-proof layer has a thickness of 10-20 μm.

[0018] In the utility model, the wear-resistant layer can be made of high-hardness ceramic materials such as alumina ceramics and silicon carbide ceramics, and the wear-resistant layer is formed on the waterproof layer by spraying; the waterproof layer can be made of a polyethylene and polypropylene combined film, and is attached to the first elastic layer by hot pressing or glue bonding; the first elastic layer and the second elastic layer can be made of thermoplastic polyurethane material, and are attached to the PET layer by hot pressing or glue bonding; the moisture-proof layer can be made of high-density polyethylene material, and is attached to the bottom of the second elastic layer by hot pressing or glue bonding.

[0019] The advantages of the utility model are:

[0020] 1. The utility model enhances the waterproof performance of the composite membrane by setting a multi-layer membrane structure, wherein the waterproof layer adopts a polyethylene and polypropylene combined film, the polyethylene film has a low water absorption capacity and good air permeability, the polypropylene can enhance and protect the polyethylene film, the surface of the mesh polyamide fiber in the fiber layer is coated with a cationic emulsion to form a reinforced waterproof film, and the PET layer also has good waterproof performance. The above multi-layer combination greatly enhances the waterproof performance of the composite membrane.

[0021] 2. The utility model sets a first elastic layer and a second elastic layer to enhance the elasticity of the composite film, and fills the cavity of the elastic layer with polyethylene microspheres, which have good elastic properties and can improve the touch feel of the composite film when used;

[0022] 3. The utility model bonds protective layers on both sides of the composite film, which can protect the edge of the composite film, prevent moisture from entering from the side of the composite film to affect the performance of the composite film, and enhance the service life of the composite film. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.

[0024] Figure 1 It is a structural schematic diagram of the utility model.

[0025] Illustration: 1. wear-resistant layer, 2. waterproof layer, 3. fiber layer, 4. first elastic layer, 5. PET layer, 6. second elastic layer, 7. moisture-proof layer, 8. protective layer, 9. cavity, 10. polyethylene microspheres. DETAILED DESCRIPTION

[0026] In order to enable those skilled in the art to better understand the present invention, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only embodiments of a part of the present invention rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work belong to the protection scope of the present invention.

[0027] Example 1

[0028] like Figure 1 As shown, a waterproof and moisture-proof composite membrane is composed of a wear-resistant layer 1, a waterproof layer 2, a fiber layer 3, a first elastic layer 4, a PET layer 5, a second elastic layer 6 and a moisture-proof layer 7 from the outside to the inside. Protective layers 8 are also bonded on both sides of the waterproof and moisture-proof composite membrane. The total thickness of the waterproof and moisture-proof composite membrane is 165-315μm. In this embodiment, the total thickness of the waterproof and moisture-proof membrane is preferably 165μm.

[0029] The wear-resistant layer is made of silicon carbide ceramic powder, which has high hardness and enhances the wear resistance of the composite film; the waterproof layer is made of polyethylene and polypropylene, and is formed by hot pressing polyethylene and polypropylene films; the first elastic layer and the second elastic layer are made of thermoplastic polyurethane, which has good elasticity and recovery properties and enhances the touch feel of the composite film; the moisture-proof layer is made of high-density polyethylene, which has better waterproof and moisture-proof properties than ordinary polyethylene; the protective layer is made of silicone film, which is attached to both sides of the composite film to prevent water vapor from invading the composite film, extend the service life of the composite film, and further enhance the waterproof and moisture-proof properties of the composite film.

[0030] A mesh polyamide fiber is arranged in the fiber layer, and a reinforcing film layer is coated on the surface of the mesh polyamide fiber. The preparation method of the reinforcing film layer is as follows: after the mesh polyamide fiber is immersed in a cationic emulsion and taken out, the cationic emulsion combines with the hydroxyl groups on the polyamide fiber to form a reinforcing film layer on the surface of the polyamide fiber. The film layer has excellent waterproof performance and can further enhance the waterproofness of the composite membrane. The above-mentioned cationic emulsion can be selected from hexadecyltrimethylammonium bromide.

[0031] The grid spaces of the reticular polyamide fiber are filled with flame retardant particles, which can be aluminum hydroxide particles, to give the composite film a certain flame retardant ability.

[0032] A plurality of cavities 9 are provided in the first elastic layer and the second elastic layer, and a plurality of polyethylene microspheres 10 are filled in the cavities. The diameter of the polyethylene microspheres is 5-10 μm, preferably 5 μm in the present embodiment. The polyethylene microspheres are prior art and have good elasticity, thereby further enhancing the elasticity of the composite film and improving the feel of the composite film.

[0033] The thickness of the first elastic layer and the second elastic layer is 50 μm, the thickness of the waterproof layer is 10 μm, the thickness of the fiber layer is 20 μm, the thickness of the moisture-proof layer is 20 μm, the thickness of the PET layer is 10 μm, and the thickness of the wear-resistant layer is 5 μm.

[0034] Example 2

[0035] A waterproof and moisture-proof composite membrane, which consists of a wear-resistant layer 1, a waterproof layer 2, a fiber layer 3, a first elastic layer 4, a PET layer 5, a second elastic layer 6 and a moisture-proof layer 7 from outside to inside, and protective layers 8 are also bonded on both sides of the waterproof and moisture-proof composite membrane. The total thickness of the waterproof and moisture-proof composite membrane is 315μm.

[0036] The wear-resistant layer is made of alumina ceramic powder; the waterproof layer is made of polyethylene and polypropylene, and is formed by hot pressing polyethylene and polypropylene films; the first elastic layer and the second elastic layer are made of thermoplastic polyurethane; the moisture-proof layer is made of high-density polyethylene; and the protective layer is made of silicone.

[0037] A mesh polyamide fiber is arranged in the fiber layer, and a reinforcing film layer is coated on the surface of the mesh polyamide fiber. The preparation method of the reinforcing film layer is as follows: the mesh polyamide fiber is immersed in a cationic emulsion and then taken out, and the cationic emulsion combines with the hydroxyl groups on the polyamide fiber to form a reinforcing film layer on the surface of the polyamide fiber. The cationic emulsion is hexadecyltrimethylammonium bromide.

[0038] The grid spaces of the mesh polyamide fiber are filled with flame retardant particles, and the flame retardant particles are magnesium hydroxide particles.

[0039] A plurality of cavities 9 are provided in the first elastic layer and the second elastic layer, and a plurality of polyethylene microspheres 10 are filled in the cavities. The diameter of the polyethylene microspheres is 10 μm.

[0040] The thickness of the first elastic layer and the second elastic layer is 100 μm, the thickness of the waterproof layer is 20 μm, the thickness of the fiber layer is 30 μm, the thickness of the moisture-proof layer is 30 μm, the thickness of the PET layer is 20 μm, and the thickness of the wear-resistant layer is 15 μm.

[0041] Finally, it should be noted that this embodiment is only used to illustrate the present invention and does not limit the scope of the present invention. In addition, it should be understood that after reading the content of the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.

Claims

1. A waterproof and moisture-proof composite film, characterized in that: The waterproof and moisture-proof composite membrane comprises, from outside to inside, a wear-resistant layer (1), a waterproof layer (2), a fiber layer (3), a first elastic layer (4), a PET layer (5), a second elastic layer (6) and a moisture-proof layer (7); protective layers (8) are bonded to both sides of the waterproof and moisture-proof composite membrane; a plurality of cavities (9) are arranged in the first elastic layer and the second elastic layer; a plurality of polyethylene microspheres (10) are filled in the cavities; and the total thickness of the waterproof and moisture-proof composite membrane is 165-315 μm.

2. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The fiber layer is provided with mesh polyamide fibers, and the surface of the mesh polyamide fibers is covered with a reinforcing film layer.

3. The waterproof and moisture-proof composite membrane according to claim 2, characterized in that: The grid spaces of the mesh polyamide fibers are filled with flame-retardant particles.

4. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The diameter of the polyethylene microspheres is 5-10 μm.

5. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The thickness of the first elastic layer and the second elastic layer is 50-100 μm.

6. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The waterproof layer has a thickness of 10-20 μm.

7. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The fiber layer has a thickness of 20-30 μm.

8. The waterproof and moisture-proof composite membrane according to claim 1, characterized in that: The moisture-proof layer has a thickness of 10-20 μm.