Edge shrinking device for rolled glass forming passage outlet
By designing an edge reducer including an adjustment gear and an electric heating function at the outlet of the rolled glass forming passage, the problem of low adjustment accuracy in the existing technology is solved, and the effect of precise adjustment of the baffle and prevention of cold patterns is achieved.
Patent Information
- Application Number
- CN202323383868.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-12
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2033-12-12
AI Technical Summary
The adjustment accuracy of the edge reducer at the exit of the existing rolled glass forming passage is not high, resulting in inconsistent widths on both sides.
A side reducer is designed that includes a base plate, lip brick, adjustment box, support rod, adjustment gear and electric heating joint. Through the synchronous movement of the adjustment gear and tooth plate and the electric heating function, the baffle can be accurately adjusted and prevent cold pattern.
The adjustment accuracy of the baffle is improved, and cold patterns on the outlet are prevented through electric heating to ensure the quality of glass molding.
Smart Images

Figure CN221917769U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of rolled glass processing, in particular to an edge shrinking device for an outlet of a rolled glass forming passage. Background Art
[0002] Rolled glass is a type of flat glass. Its manufacturing process is divided into single-roll method and double-roll method. In the single-roll method, the molten glass is poured onto a rolling forming table. Various patterns can be pressed out of the table top using a patterned mold. In the double-roll method, the molten glass is pressed into a plate shape through two relatively rotating rollers, and then cooled and solidified. When producing and processing glass of different widths, it is often necessary to design two corresponding production lines, resulting in serious waste of resources.
[0003] In the utility model patent with patent announcement number CN21838722U, a lip brick shrinker is arranged above the lip brick at the outlet of the rolled glass forming passage, the lip brick is arranged at the outlet of the rolled glass forming passage, and is fixed on the lip brick water bag through a lip brick fixing piece, the width and height of the lip brick shrinker match the width and height of the outlet of the rolled glass forming passage, the lip brick shrinker is composed of left and right independent lip brick shrinkers, respectively, a left lip brick shrinker and a right lip brick shrinker, and are symmetrically arranged along the outlet of the rolled glass forming passage, the lip brick shrinker is respectively provided with hand bricks and shrinker baffles, the hand bricks are fixed on both sides of the lip brick by hand brick fixing pieces, the inner width of the hand brick is adjusted to the initial position, the shrinker baffle is fixed on the inner side of the hand brick by the baffle fixing piece, and can slide back and forth within a certain range, although this method can achieve the purpose of adjusting the width, but there is also a problem: since the shrinking baffles on both sides are manually adjusted twice, insufficient precision will be caused when adjusting the width, resulting in unequal width gaps on both sides.
[0004] Therefore, it is necessary to provide a shrinking device for the outlet of the rolled glass forming passage to solve the above technical problems. Utility Model Content
[0005] In view of the above situation, in order to overcome the defects of the prior art, the utility model provides a shrinking device for the outlet of the rolled glass forming passage to solve the problem that the adjustment accuracy of the existing device is low, which easily leads to inconsistent widths on both sides.
[0006] In order to achieve the above purpose, the technical solution adopted by the utility model is as follows:
[0007] A shrinking device for the outlet of a rolling glass forming passage, comprising: a bottom plate;
[0008] The bottom plate as a whole is a lip brick water bag, and a lip brick is installed on the top surface of the bottom plate. Both sides of the lip brick are fixed and limited by fixing parts, and an adjusting box is mounted above the lip brick. Both sides of the adjusting box are connected to the support rod, and the bottom surface of the support rod is installed in abutment with the top surface of the bottom plate. A sliding groove is opened on the bottom surface of the adjusting box, and an adjusting gear is rotatably installed on the inner middle part of the adjusting box. The shaft of the adjusting gear passes through the adjusting box and is connected to the adjusting handle. The top and bottom of the adjusting gear are respectively meshed with the left tooth plate and the right tooth plate, and the side edges of the left tooth plate and the right tooth plate are slidably connected to the adjusting box. The two side ends of the left tooth plate and the right tooth plate are connected to the fixing rod, and the fixing rod is L-shaped. The short side end of the fixing rod is installed and connected to the baffle, and the top surface of the short side of the fixing rod is installed with an electric heating joint.
[0009] In one embodiment, a threaded hole is provided on the outer side of the bottom of the fixing rod, and a locking hole is provided on the lower outer side of the supporting rod. The locking hole and the threaded hole are coaxial and have the same size, and a screw is installed in the locking hole.
[0010] In one embodiment, the electric heating joint is electrically connected to the heating wire inside the baffle through an electric wire.
[0011] In one embodiment, the bottom of the support rod is fixedly connected to the base plate by bolts.
[0012] In one embodiment, the width and height of the baffle are both set to match the inner diameter of the outlet of the forming passage.
[0013] The beneficial effects of the utility model are as follows:
[0014] (1) The utility model connects the support rod to the bottom plate so that the adjustment box is located above the lip brick. At this time, the baffles on both sides are located on both sides of the top surface of the lip brick. By holding the adjustment handle and rotating it, the adjustment gear is driven to rotate, so that the left tooth plate and the right tooth plate move relative to each other, and the baffles on both sides can be synchronously displaced. After the baffle is adjusted, the position of the baffle is fixed by gradually screwing the screw rod into the threaded hole until it enters the threaded hole and stops after the thread is inserted.
[0015] (2) The utility model heats the baffle in advance through the electric heating joint, so that its surface temperature is close to the temperature of the glass when it is formed, thereby preventing the occurrence of cold patterns. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a front view of the overall structure of the utility model;
[0017] Figure 2 This is a detailed diagram of the overall structure of the utility model;
[0018] Figure 3This is a detailed diagram of the installation of the baffle of the utility model;
[0019] Figure 4 This is a detailed diagram of the internal structure of the baffle of the utility model.
[0020] Among them, the names corresponding to the figure marks are: base plate 1, lip brick 2, fixing part 21, adjustment box 3, slide groove 31, adjustment gear 32, adjustment handle 33, left tooth plate 34, right tooth plate 35, fixing rod 36, baffle 37, threaded hole 38, heating wire 39, support rod 4, locking hole 41, screw 42, electric heating connector 5, wire 51. DETAILED DESCRIPTION
[0021] The present invention is further described below in conjunction with the accompanying drawings and embodiments. The present invention includes but is not limited to the following embodiments.
[0022] like Figure 1-Figure 2 As shown, the utility model provides a shrinking device for the outlet of a rolling glass forming passage, comprising: a bottom plate 1, a lip brick 2, an adjustment box 3, a support rod 4, and an electric heating joint 5;
[0023] like Figure 1-Figure 2 As shown, the bottom plate 1 is a lip brick water bag as a whole, and a lip brick 2 is installed on the top surface of the bottom plate 1. The two sides of the lip brick 2 are fixed and limited by fixing parts 21. An adjustment box 3 is set above the lip brick 2. Both sides of the adjustment box 3 are connected to the support rod 4. The bottom surface of the support rod 4 is installed in abutment with the top surface of the bottom plate 1. A slide groove 31 is opened on the bottom surface of the adjustment box 3. An adjustment gear 32 is rotatably installed in the inner middle part of the adjustment box 3. The shaft of the adjustment gear 32 passes through the adjustment box 3 and is connected to the adjustment handle 33. The upper and lower parts of the adjustment gear 32 are meshed and connected with the left tooth plate 34 and the right tooth plate 35 respectively. The left tooth plate 34 and the right tooth plate 35 are meshed and connected. 5 is slidably connected to the adjustment box 3, and the two side ends of the left tooth plate 34 and the right tooth plate 35 are connected to the fixing rod 36. The fixing rod 36 is L-shaped. The short side end of the fixing rod 36 is installed and connected with the baffle 37. The top surface of the short side of the fixing rod 36 is installed with an electric heating joint 5. When working, the adjustment box 3 is located above the lip brick 2 by installing and connecting the support rod 4 with the bottom plate 1. At this time, the baffles 37 on both sides are located on both sides of the top surface of the lip brick 2. By holding the adjustment handle 33 and rotating it, the adjustment gear 32 is driven to rotate, so that the left tooth plate 34 and the right tooth plate 35 move relative to each other, and the baffles 37 on both sides can be synchronously displaced, so that the width adjustment accuracy is higher.
[0024] Preferably, in one embodiment, Figure 2-Figure 3As shown, a threaded hole 38 is opened on the outer side of the bottom of the fixing rod 36, and a locking hole 41 is opened on the lower outer side of the supporting rod 4. The locking hole 41 is coaxial with the threaded hole 38 and has the same size. A screw 42 is installed in the locking hole 41. After the baffle 37 is adjusted, the screw 42 is gradually screwed into the threaded hole 38 until it enters the threaded hole 38 and stops after the thread is inserted, so that the position of the baffle 37 is fixed.
[0025] Preferably, in one embodiment, Figure 3-Figure 4 As shown, the electric heating joint 5 is electrically connected to the heating wire 39 inside the baffle 37 through the wire 51. Before working, the baffle 37 is heated in advance by the electric heating joint 5 to make its surface temperature close to the temperature when the glass is formed, so as to prevent the situation of cold patterns on the wire.
[0026] Preferably, in one embodiment, Figure 3 As shown, the bottom of the support rod 4 is fixedly connected to the base plate 1 by bolts, which aims to make the installation of the support rod 4 simpler and faster.
[0027] Preferably, in one embodiment, the width and height of the baffle 37 are matched with the inner diameter of the outlet of the forming passage.
[0028] Working principle of this utility model:
[0029] During operation, the support rod 4 is installed and connected to the bottom plate 1 so that the adjustment box 3 is located above the lip brick 2. At this time, the baffles 37 on both sides are located on both sides of the top surface of the lip brick 2. By holding the adjustment handle 33 and rotating it, the adjustment gear 32 is driven to rotate, so that the left tooth plate 34 and the right tooth plate 35 move relative to each other, and the synchronous displacement of the baffles 37 on both sides can be completed. After the baffle 37 is adjusted, the screw 42 is gradually screwed into the threaded hole 38 until it enters the threaded hole 38 and stops after being threaded, so that the position of the baffle 37 is fixed. The baffle 37 is heated and heated in advance by the electric heating joint 5 so that its surface temperature is close to the temperature when the glass is formed, so as to prevent the situation of cold patterns on the line.
[0030] The above embodiment is only one of the preferred implementation modes of the present utility model and should not be used to limit the protection scope of the present utility model. Any changes or modifications that are made to the main design concept and spirit of the present utility model without any substantive significance, as long as the technical problems solved are still consistent with the present utility model, should be included in the protection scope of the present utility model.
Claims
1. A shrinking device for the outlet of a rolling glass forming passage, characterized in that: include: Base plate; The bottom plate as a whole is a lip brick water bag, and a lip brick is installed on the top surface of the bottom plate. Both sides of the lip brick are fixed and limited by fixing parts, and an adjusting box is mounted above the lip brick. Both sides of the adjusting box are connected to the support rod, and the bottom surface of the support rod is installed in abutment with the top surface of the bottom plate. A sliding groove is opened on the bottom surface of the adjusting box, and an adjusting gear is rotatably installed on the inner middle part of the adjusting box. The shaft of the adjusting gear passes through the adjusting box and is connected to the adjusting handle. The top and bottom of the adjusting gear are respectively meshed with the left tooth plate and the right tooth plate, and the side edges of the left tooth plate and the right tooth plate are slidably connected to the adjusting box. The two side ends of the left tooth plate and the right tooth plate are connected to the fixing rod, and the fixing rod is L-shaped. The short side end of the fixing rod is installed and connected to the baffle, and the top surface of the short side of the fixing rod is installed with an electric heating joint.
2. The shrinking device for the outlet of the rolling glass forming passage according to claim 1, characterized in that: A threaded hole is provided on the outer side of the bottom of the fixing rod, and a locking hole is provided on the lower outer side of the supporting rod. The locking hole and the threaded hole are coaxially provided and have the same size, and a screw is installed in the locking hole.
3. The shrinking device for the outlet of the rolling glass forming passage according to claim 1, characterized in that: The electric heating joint is electrically connected to the electric heating wire inside the baffle through an electric wire.
4. The shrinking device for the outlet of the rolling glass forming passage according to claim 1, characterized in that: The bottom of the support rod is fixedly connected to the bottom plate by bolts.
5. The shrinking device for the outlet of the rolling glass forming passage according to claim 1, characterized in that: The width and height of the baffle are both set to match the inner diameter of the outlet of the forming passage.