Composite electrode plate and battery cell

By designing a stacked structure of a first active material layer with high energy density and a second active material layer with high conductivity on the electrode sheet, the problem that the energy density and charge and discharge rate of the electrode sheet cannot coexist is solved, and high energy density and high conductivity are achieved. The coexistence of charge and discharge rates improves the safety performance of the electrode sheet.

CN221928131UActive Publication Date: 2024-10-29ZHEJIANG LIWINON ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420131626.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-18
Publication Date
2024-10-29
Estimated Expiration
2034-01-18

AI Technical Summary

Technical Problem

Existing electrode sheets cannot coexist when increasing energy density and charge and discharge rate. High energy density is often accompanied by a decrease in safety performance, leading to potential cycle safety performance risks.

Method used

A composite electrode sheet structure is adopted, in which a first active material layer with high energy density is arranged on the base body, with one end close to the tab having a thickness smaller than the other end, and covered with a second active material layer with high conductivity, forming a laminated structure to improve energy storage. capacity and charge and discharge rates.

Benefits of technology

While ensuring high energy density, the charge and discharge rate is increased, the cycle safety performance of the electrode sheet is improved, and the problems of heating and lithium deposition caused by high current density are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221928131U_ABST
    Figure CN221928131U_ABST
Patent Text Reader

Abstract

The utility model discloses a composite electrode plate which comprises a base body, a tab, a first active material layer and a second active material layer, the tab is arranged on one side of the base body; at least one surface of the substrate is covered with a first active material layer and a second active material layer which are laminated, one end of the first active material layer close to the tab is thinner than the other end, and the conductivity of the first active material layer is smaller than that of the second active material layer; the energy density of the first active material layer is greater than that of the second active material layer; the thickness of one end, close to the tab, of the second active material layer is greater than that of the other end. In the technical scheme of the utility model, the first active material layer with high energy density is arranged on the base body to improve the capacity, and the thickness of one end close to the tab is smaller than that of the other end; a second active material with high conductivity is arranged on the first active material layer, and the thickness close to the tab is greater than the thickness of the other end. Therefore, the quantity density and the charge-discharge rate can be improved at the same time. In addition, the utility model further discloses a battery cell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of batteries, in particular to a composite electrode sheet and a battery core. Background Art

[0002] The energy density and charge and discharge rate of a battery are closely related to the material and structure of the battery. Energy density refers to the amount of electrical energy that a battery can provide per unit mass or volume, reflecting the battery's endurance. The charge and discharge rate refers to the amount of current that a battery can charge and discharge per unit time, reflecting the battery's power output capacity. The energy density and charge and discharge rate of a battery are mainly determined by the capacity of the electrode material. The higher the capacity, the higher the energy density and charge and discharge rate.

[0003] Currently, in order to improve battery energy density, a common practice is to coat high-capacity materials on the surface of the current collector, which can store more lithium ions, thereby increasing the battery capacity and voltage.

[0004] However, materials with high capacity have poor safety performance and cannot be charged and discharged with large currents, which means that high energy density and high charge and discharge rates cannot coexist. Utility Model Content

[0005] The main purpose of the utility model is to provide a composite electrode sheet, aiming to solve the problem that the high energy density and high charge and discharge rate of the existing electrode sheets cannot coexist.

[0006] In order to achieve the above-mentioned purpose, the utility model provides a composite electrode sheet, which comprises:

[0007] matrix;

[0008] A tab, disposed on one side of the substrate;

[0009] At least one side of the substrate is covered with a first active material layer and a second active material layer stacked together, the thickness of the first active material layer near one end of the electrode ear is smaller than the thickness at the other end, and the conductivity of the first active material layer is smaller than that of the second active material layer; the energy density of the first active material layer is greater than that of the second active material layer, and the thickness of the second active material layer near one end of the electrode ear is greater than the thickness at the other end.

[0010] In some embodiments, after the second active material layer covers the first active material layer, the outer shape forms a rectangle.

[0011] In some embodiments, the first active material layer and the second active material layer are formed on both surfaces of the substrate.

[0012] In some embodiments, the second active material layer partially covers the first active material layer.

[0013] In some embodiments, a step is configured on one side of the first active material layer, and the second active material layer is formed on the step, and an outer surface of the second active material layer is flush with an outer surface of the first active material layer.

[0014] In some embodiments, the steps are stair-like steps.

[0015] In some embodiments, a slope is configured on one side of the first active material layer, and the second active material layer is formed on the slope, and an outer surface of the second active material layer is flush with an outer surface of the first active material layer.

[0016] In some embodiments, a surface of the first active material layer facing the second active material layer is a non-smooth surface.

[0017] In some embodiments, the first active material layer is graphite with a gram capacity of 350 mAh / g to 372 mAh / g; and the second active material layer is graphite with a conductivity greater than 1000 s / m.

[0018] The utility model further provides a battery core, comprising the aforementioned composite electrode sheet.

[0019] In the technical solution of the utility model, a first active material layer with high energy density is arranged on the substrate to improve the energy storage capacity; since the current density near the pole ear is large, the first active material layer is prone to heat and lithium precipitation; therefore, the thickness of the first active material layer near one end of the pole ear is set to be less than the thickness at the other end, and the second active material layer with higher conductivity is stacked on the first active material layer, and the thickness near the pole ear is greater than the thickness at the other end. In this way, while ensuring high energy density, the charge and discharge rate can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a schematic diagram of the structure of a composite electrode sheet in one embodiment of the utility model;

[0021] Figure 2 This is a schematic diagram of the structure of a composite electrode sheet in another embodiment of the utility model;

[0022] Figure 3 This is a schematic diagram of the structure of a composite electrode sheet in another embodiment of the utility model;

[0023] Figure 4 This is a schematic diagram of the structure of a composite electrode sheet in another embodiment of the present utility model;

[0024] Figure 5 This is a schematic diagram of the structure of a composite electrode sheet in another embodiment of the present utility model;

[0025] Figure 6This is a schematic diagram of the structure of a composite electrode sheet in another embodiment of the present utility model;

[0026] Figure 7 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0027] Description of Figure Numbers:

[0028] 100, substrate; 200, tab; 110, first active material layer; 110a, mounting portion; 112, second active material layer; 113, third active material layer; 114, fourth active material layer.

[0029] The realization of the purpose, functional features and advantages of the utility model will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0030] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the scheme in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0031] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back...) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0032] It should also be noted that when an element is referred to as being "fixed on" or "disposed on" another element, it may be directly on the other element or there may be an intermediate element at the same time. When an element is referred to as being "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.

[0033] In addition, the descriptions of "first", "second", etc. in the present utility model are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in this field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present utility model.

[0034] Energy density and battery cell performance can be said to be issues that any company has to encounter when designing batteries. When a company has a great advantage in energy density, the battery cell's cycle safety performance may have certain hidden dangers. When its cycle safety performance is 100% correct, the energy density is often low, making the product lack strong competitiveness.

[0035] In this regard, an embodiment of the utility model proposes a composite electrode sheet that can improve energy density and charge and discharge rate while ensuring safety performance.

[0036] See also Figure 1 , Figure 1 It is a schematic diagram of the structure of a composite electrode sheet in one embodiment of the utility model.

[0037] In this embodiment, the composite electrode sheet includes:

[0038] Base 100;

[0039] The tab 200 is disposed on one side of the substrate 100;

[0040] At least one side of the substrate 100 is covered with a first active material layer 110 and a second active material layer 112 which are stacked. The thickness of the first active material layer 110 at one end close to the tab 200 is smaller than that at the other end. The conductivity of the first active material layer 110 is smaller than that of the second active material layer 112. The energy density of the first active material layer 110 is greater than that of the second active material layer 112. The thickness of the second active material layer 112 at one end close to the tab 200 is greater than that at the other end.

[0041] In this embodiment, the substrate 100 (referred to as the current collector in this embodiment) is a component used for conducting electricity and carrying active materials in lithium-ion batteries, and generally uses high-purity metal materials such as copper, aluminum, nickel, stainless steel, etc. The selection of the material of the current collector should take into account factors such as its conductivity, electrochemical stability, mechanical strength, cost, etc. Therefore, copper foil is usually used for the negative electrode current collector and aluminum foil is used for the positive electrode current collector because they have good conductivity and corrosion resistance.

[0042] The tab 200 is a metal conductor that leads the positive and negative electrodes from the battery cell. In layman's terms, the tabs of the positive and negative electrodes of the battery are the contact points during charging and discharging. This contact point is not the copper sheet on the outside of the battery that we see, but a connection inside the battery. The tab 200 is divided into three types of materials. The positive electrode of the battery uses aluminum (Al) material, the negative electrode uses nickel (Ni) material, and the negative electrode also has copper-plated nickel (Ni-Cu) material. They are all composed of two parts: film and metal strip.

[0043] The film is the insulating part of the tab 200. Its function is to prevent short circuit between the metal strip and the aluminum-plastic film when the battery is packaged, and to heat (about 140°C) and hot-melt seal the aluminum-plastic film together to prevent leakage. A tab 200 is made of two pieces of film sandwiching the metal strip. There are three types of films on the market: black film, white film and single-layer film.

[0044] The first active material layer 110 is a material layer that improves energy density, increases battery capacity and improves endurance, and can use high-capacity materials. For example, high-capacity graphite is mainly graphite with high crystallinity, good layered structure and high gram capacity (graphite with high capacity such as AGR173, etc.). However, the part of the first active material layer 110 graphite close to the pole ear 200 is very easy to heat up when a large amount of current passes through it. Therefore, the thickness of the first active material layer 110 close to one end of the pole ear 200 is set to be less than the thickness of the other end. Instead, a second active material layer 112 with high conductivity is used.

[0045] The second active material layer 112 is a material layer for improving the charge and discharge rate, and graphite with high conductivity can be used. For example, graphite with small particle size, large specific surface area, and carbon coating (such as 7C materials with fast charge and discharge rates such as AGR126, etc.). This material adopts a special preparation process to form a turbine-shaped structure of graphene sheets, which has higher conductivity than ordinary graphite. This is conducive to reducing the internal resistance and heat loss of the pole piece, can improve the charge and discharge efficiency and life, and is conducive to the rapid transmission of internal ions, which can overcome safety issues such as lithium precipitation and heat generation caused by high current density.

[0046] In the technical solution of the utility model, a first active material layer 110 with high energy density is arranged on the substrate 100 to improve the energy storage capacity; since the current density near the pole ear is large, the first active material layer 110 is prone to heat and lithium precipitation; therefore, the thickness of the first active material layer 110 near one end of the pole ear 200 is set to be less than the thickness of the other end, and then the second active material layer 112 with higher conductivity is stacked on the first active material layer 110, and the thickness near the pole ear 200 is greater than the thickness of the other end. In this way, while ensuring high energy density, the charge and discharge rate can be improved.

[0047] Continue reading Figure 1 In order to facilitate subsequent packaging, in this embodiment, after the second active material layer 112 covers the first active material layer 110, the shape forms a rectangle.

[0048] In this embodiment, a small amount of the first active material layer 110 is sprayed on one side of the substrate 100 and close to the tab 200, and then a large amount of the second active material layer 112 is sprayed on the basis of the small amount of the first active material layer 110 to improve the charge and discharge rate. At the same time, in order to improve the high energy density, the coating amount of the first active material layer 110 is increased at a position away from the tab 200, and the corresponding coating amount of the second active material layer 112 is reduced, that is, the first active material layer 110 and the second active material layer 112 fill each other's missing parts.

[0049] The specific method of coating the first active material layer 110 and the second active material layer 112 can be a spraying process, which mainly involves mixing graphite in the form of powder with a binder and a solvent, and then depositing it on the current collector through a spraying device to form a thin film. For example, during the spraying process, a small amount of the first active material 110 is sprayed near the pole ear 200. As the distance from the pole ear 200 increases, the flow rate increases proportionally, so that the sprayed slurry increases; when spraying the second active material layer 112, a large amount of slurry is sprayed near the pole ear 200. As the distance from the pole ear 200 increases, the flow rate decreases proportionally, so that the sprayed slurry decreases, and finally ensures that after the two layers of active material are coated, the whole is in a rectangular plane, and the shape of the rectangular plane can be easily rolled into a cylindrical or square shape, which can adapt to different battery shells.

[0050] In addition to coating the active material layer on one side of the substrate 100 in the above embodiment, the active material layer may also be coated on both sides of the substrate 100 .

[0051] See also Figure 2 , Figure 2 It is a schematic structural diagram of a composite electrode sheet in another embodiment of the utility model.

[0052] In order to further improve the energy storage capacity and charge-discharge efficiency, the first active material layer 110 and the second active material layer 112 can be coated on the other side of the substrate 100 (current collector) based on the above embodiment. Therefore, in this embodiment, the first active material layer 110 and the second active material layer 112 are formed on both surfaces of the substrate 100.

[0053] In this embodiment, the end of the first active material layer 110 facing away from the substrate 100 may be configured with an inclined surface, and the second active material layer 112 is formed on the inclined surface of the first active material layer 110. In other words, the active material layers on both sides of the substrate 100 are arranged in the same manner, and the two are combined to form a rectangular shape. In the technical solution of this embodiment, since the first active material layer 110 and the second active material layer 112 are arranged on both sides of the substrate, the energy storage capacity can be further improved compared to the active material layer arranged on one side, while the charge and discharge rate can be improved.

[0054] See also Figure 3 , Figure 3 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0055] In addition to the above-mentioned embodiments, the active material layer on the other side of the substrate is stacked obliquely, and can also be stacked in parallel. For example, the first active material layer 110 is formed along the surface of the substrate 100, and the second active material layer 112 is formed on the surface of the first active material layer 110. The thickness of the two layers can be the same, or one of them can be larger than the other, which is not particularly limited here.

[0056] See also Figure 4 , Figure 4 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0057] In addition to fully covering the surface of the first active material layer 110 with the second active material layer 112, the second active material layer 112 may also be partially coated on the surface of the first active material layer 110. In this embodiment, the second active material layer 112 partially covers the first active material layer 110. It should be noted that part of the second active material layer 112 is coated on one end of the first active material layer 110 close to the pole ear 200, and the rest of the substrate 100 is coated with the first active material layer 110. That is, in this embodiment, the second active material layer 112 is only arranged at a position close to the pole ear 200 to improve the charge and discharge rate and avoid heat and lithium precipitation, and the rest is coated with the first active material layer, which can avoid the redundancy of the second active material layer 112 and cause unnecessary waste.

[0058] There are many ways to coat part of the second active material layer 112 on the first active material layer 110 , and a variety of optional implementations are provided below for illustration.

[0059] Continue reading Figure 4 In this embodiment, a step is configured on one side of the first active material layer 110 , and the second active material layer 112 is formed on the step, and its outer surface is flush with the outer surface of the first active material layer 110 .

[0060] In this embodiment, the step can be formed by reservation or processing. For example, when spraying the first active material layer 110 on the surface of the substrate 100, the slurry near the tab 200 is less than that of the second active material layer 112, and the discharge of the first active material layer 110 increases after a certain distance away from the tab 200.

[0061] The subsequent processing method for forming steps is that the amount of slurry in the first active material layer 110 close to the electrode ear 200 and away from the electrode ear 200 is consistent; the dried first active material layer 110 is subsequently processed, such as grinding, cutting, laser engraving, etc. to form steps. This method is suitable for the modification of ordinary electrode sheets.

[0062] After the step is processed, the second active material layer 112 can be sprayed on the step. The sprayed second active material layer 112 is flush with the outer surface of the first active material layer 110, which can ensure the flatness of the electrode and avoid puncturing the aluminum-plastic film.

[0063] See also Figure 5 , Figure 5 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0064] To further improve the charge and discharge rate, it can be achieved by improving the migration efficiency of ions inside the active material layer. The contact area between the first active material layer 110 and the second active material layer 112 is one of the factors affecting the ion migration efficiency. Therefore, in this embodiment, the step is a stepped step, which can increase the contact area between the first active material layer 110 and the second active material layer 112, which means that the diffusion distance of lithium ions inside the active material can be shortened, thereby reducing the resistance of solid phase diffusion and increasing the diffusion rate of lithium ions.

[0065] See also Figure 6 , Figure 6 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0066] One side of the first active material layer 110 is configured with an inclined surface, and the second active material layer 112 is formed on the inclined surface, and its outer surface is flush with the outer surface of the first active material layer.

[0067] In this embodiment, a slope is constructed on one side of the first material layer close to the pole ear 200, and the slope faces the pole ear 200; the slope can be constructed on the first active material layer 110 in the form of a cut angle. Of course, it can also be constructed in a form with a certain curvature. In either case, the contact area between the first active material layer 110 and the second active material layer 112 can be increased, which is conducive to the migration of internal ions. In addition, the outer surface of the second active material layer 112 is flush with the outer surface of the first active material layer 110, which can avoid puncturing the aluminum-plastic film.

[0068] See also Figure 7 , Figure 7 Schematic diagram of the structure of a composite electrode sheet in another embodiment of the present invention.

[0069] The surface of the first active material layer 110 facing the second active material layer 112 is a non-smooth surface.

[0070] In this embodiment, the side of the first active material layer 110 facing the second active material layer 112 is a non-smooth surface. The non-smooth surface can be formed by spraying the first active material layer 110 on the substrate 100 and then processing it, such as by laser engraving. After the processing is completed, the second active material layer 112 is directly sprayed on the non-smooth surface, and the two can form a whole. Since the side of the first active material layer 110 facing the second active material layer 112 is a non-smooth surface, the two have a high degree of bonding, which can improve the migration efficiency of internal ions.

[0071] In some embodiments, the first active material layer 110 is graphite with a gram capacity of 350 mAh / g to 372 mAh / g; and the second active material layer 112 is graphite with a conductivity greater than 1000 s / m.

[0072] In this embodiment, the gram capacity of the first active material layer 110 is taken as 350 mAh / g, 360 mAh / g, and 372 mAh / g for illustration.

[0073] Energy density refers to the energy that can be released per gram or per liter of material, usually expressed in Wh / kg or Wh / L. The energy density of AGR173 material is related to its gram capacity, operating voltage, compaction density and other factors. For example, the operating voltage of AGR173 material is 3.8V and the compaction density is 1.8g / cm3. Therefore, the energy density of AGR173 material can be calculated using the following formula:

[0074] Energy density = gram capacity × working voltage × compaction density

[0075] Substituting the gram capacity of AGR173 material into the formula, the following results can be obtained:

[0076] When the gram capacity is 350mAh / g, the energy density is 2.38Wh / g;

[0077] When the gram capacity is 360mAh / g, the energy density is 2.45Wh / g;

[0078] When the gram capacity is 372mAh / g, the energy density is 2.54Wh / g.

[0079] For lithium batteries, the energy density of 2.38Wh / g to 2.54Wh / g is relatively high, because it is close to the theoretical limit of lithium batteries and exceeds most lithium battery products on the market. For example, the energy density of the battery used in Tesla's Model 3 is about 2.5Wh / g, while the energy density of lithium iron phosphate batteries is generally around 1.5Wh / g.

[0080] The second active material layer 112 may be made of a highly conductive graphite 7C material AGR126, which uses a method of turbulent flow and isotropic capillary compression to form a turbine-shaped structure of graphene sheets, thereby improving the conductivity of the material.

[0081] The utility model further proposes a battery cell, comprising the aforementioned composite electrode sheet. The specific structure of the composite electrode sheet refers to the above embodiment. Since the battery cell adopts all the technical solutions of all the above embodiments, it at least has all the technical effects brought by the technical solutions of the above embodiments, which will not be described one by one here.

[0082] The above description is only a partial or preferred embodiment of the present invention. Neither the text nor the drawings can limit the scope of protection of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the overall concept of the present invention, or direct / indirect application in other related technical fields are included in the scope of protection of the present invention.

Claims

1. A composite electrode sheet, characterized in that: include: matrix; A tab, provided on one side of the substrate; At least one side of the substrate is covered with a first active material layer and a second active material layer arranged in a stacked manner, the thickness of the first active material layer near one end of the electrode tab is thinner than the thickness at the other end, and the conductivity of the first active material layer is thinner than the second active material layer; the energy density of the first active material layer is greater than that of the second active material layer, and the thickness of the second active material layer near one end of the electrode tab is thicker than the thickness at the other end.

2. The composite electrode sheet according to claim 1, characterized in that: After the second active material layer covers the first active material layer, the outer shape forms a rectangle.

3. The composite electrode sheet according to claim 2, characterized in that: The first active material layer and the second active material layer are formed on both surfaces of the substrate.

4. The composite electrode sheet according to claim 3, characterized in that: The second active material layer partially covers the first active material layer.

5. The composite electrode sheet according to claim 4, characterized in that: A step is formed on one side of the first active material layer, and the second active material layer is formed on the step, with an outer surface of the second active material layer being flush with an outer surface of the first active material layer.

6. The composite electrode sheet according to claim 5, characterized in that: The steps are stepped steps.

7. The composite electrode sheet according to claim 4, characterized in that: One side of the first active material layer is configured with an inclined surface, and the second active material layer is formed on the inclined surface, and the outer surface of the second active material layer is flush with the outer surface of the first active material layer.

8. The composite electrode sheet according to any one of claims 1 to 7, characterized in that: A surface of the first active material layer facing the second active material layer is a non-smooth surface.

9. The composite electrode sheet according to claim 8, characterized in that: The first active material layer is graphite with a gram capacity of 350 mAh / g to 372 mAh / g; the second active material layer is graphite with a conductivity greater than 1000 s / m.

10. A battery cell, characterized in that: The composite electrode sheet comprises the composite electrode sheet according to any one of claims 1 to 9.