Product flash-free die
By setting up the supporting projection and concave portion of the film margin on the mold, the problem of flying during injection molding is solved, and the mold design without flying is realized, which is suitable for a variety of materials and improves product quality.
Patent Information
- Application Number
- CN202323393164.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-12
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-12
AI Technical Summary
During the injection molding process, the mold parting surface and other positions of the mold are slightly stretched due to the internal sol pressure, forming a flash, affecting the product quality.
Design a fly-free mold. The moving and fixed molds are provided with the remaining convex portions and concave portions extending along the product parting surface toward the opening direction. In the mold-closing state, the convex portions are located in the concave portion and match the arc surface to smoothly Connect to avoid plastic spills.
It effectively avoids the formation of flashes and is suitable for a variety of commonly used materials to ensure product quality during injection molding.
Smart Images

Figure CN221937388U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of molds, in particular to a product mold without flash. Background Art
[0002] Flash is also called overflow, burr, burr, etc. It occurs during the injection molding process at the parting surface of the mold, such as the parting surface of the movable mold and the static mold, the sliding part of the slider, the gap of the insert, the hole of the ejector pin, etc. Due to the high sol pressure inside the mold, the movable mold and the fixed mold are slightly stretched apart. When the stretching distance is greater than the overflow value of the material, the molten plastic runs to the parting surface and forms a flash after cooling. Therefore, it is urgent to design a product without flash mold to solve the technical problem that flash is easily generated during current mold injection molding. Utility Model Content
[0003] The purpose of the utility model is to provide a product without flash mold, which solves the technical problem that flash is easily generated during injection molding of existing molds. The preferred technical solution among the many technical solutions provided by the utility model can produce many technical effects as described below.
[0004] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0005] The utility model provides a product flash-free mold, comprising a movable mold and a fixed mold, one of the movable mold and the fixed mold is provided with a film expansion margin convex portion extending along the parting surface of the product toward the mold opening direction, and the other is provided with a film expansion margin concave portion extending along the parting surface of the product toward the mold opening direction, when the movable mold and the fixed mold are in a mold-clamping state, the film expansion margin convex portion is located in the film expansion margin concave portion.
[0006] Preferably, the extension length of the film expansion margin protrusion and the film expansion margin concave portion along the mold opening direction is in the range of 0.2 mm to 0.5 mm.
[0007] Preferably, it also includes an arc surface portion arranged on the film expansion margin convex portion and the film expansion margin concave portion away from the product direction, and the arc direction of the outer side wall of the cross section of the arc surface portion along the mold opening direction is facing away from the product.
[0008] Preferably, the arcuate outer wall of the arcuate portion is smoothly connected to the outer walls of the film expansion margin convex portion and the film expansion margin concave portion.
[0009] Preferably, the tangent direction of one end of the arc surface portion away from the film expansion margin convex portion and the film expansion margin concave portion is in the same direction as the normal direction of the mold opening direction.
[0010] This application adopts the above technical solution, which has at least the following beneficial effects:
[0011] In the present application, a film expansion margin convex portion extending along the parting surface of the product toward the mold opening direction is provided on one of the fixed mold and the movable mold, and a film expansion margin concave portion extending along the parting surface of the product toward the mold opening direction is provided on the other mold. When the movable mold and the fixed mold are in the mold-clamping state, the film expansion margin convex portion is located in the film expansion margin concave portion, so as to ensure that in the case of film expansion during injection molding, the flash problem can still be avoided by the cooperation of the film expansion margin convex portion and the film expansion margin concave portion.
[0012] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0014] Figure 1 It is a structural schematic diagram of the mold opening state of the product without flash provided by the embodiment of the utility model;
[0015] Figure 2 It is a structural schematic diagram of a mold-closing state of a product without flash provided by an embodiment of the utility model;
[0016] Figure 3 It is a schematic diagram of the partial structure of the cross-section of a flash-free mold for a product provided by an embodiment of the utility model.
[0017] In the figure, 1, movable mold; 2, fixed mold; 3, convex part of film expansion margin; 4, concave part of film expansion margin; 5, arc surface part; 6, film expansion amount. DETAILED DESCRIPTION
[0018] In order to make the purpose, technical solution and advantages of the utility model clearer, the technical solution of the utility model will be described in detail below. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other implementation methods obtained by ordinary technicians in this field without creative work belong to the scope of protection of the utility model.
[0019] The specific embodiment of the utility model provides a product without flash mold, combined with the attached Figure 1 ~Attached Figure 3, mainly comprising a movable mold 1 and a fixed mold 2, one of which is provided with a film expansion allowance convex portion 3 extending along the parting surface of the product toward the mold opening direction, and the other of which is provided with a film expansion allowance concave portion 4 extending along the parting surface of the product toward the mold opening direction, when the movable mold 1 and the fixed mold 2 are in the mold closing state, the film expansion allowance convex portion 3 is located in the film expansion allowance concave portion 4.
[0020] The specific details can be found in the attached Figure 1 As shown in the figure, a film expansion allowance convex portion 3 extending along the parting surface of the product on the movable mold 1 toward the mold opening direction is provided on the movable mold 1, and a film expansion allowance concave portion 4 extending along the parting surface of the product on the fixed mold 2 toward the mold opening direction is provided on the fixed mold 2. It is worth noting that the parting surface of the product referred to in this application is the position of the parting surface on the product; the film expansion allowance convex portion 3 and the film expansion allowance concave portion 4 on the movable mold 1 and the fixed mold 2 can be arranged vice versa.
[0021] In this way, the movable mold 1 and the fixed mold 2 can be molded together, and after reserving product space inside, the film expansion allowance convex part 3 and the film expansion allowance concave part 4 are matched at the matching position along the mold opening direction to ensure that the movable mold 1 and the fixed mold 2 will not produce flash within the range of the film expansion allowance through the matching of the film expansion allowance convex part 3 and the film expansion allowance concave part 4.
[0022] In the specific embodiment of the present application, the extension length of the expansion margin protrusion 3 and the expansion margin concave portion 4 along the mold opening direction ranges from 0.2 mm to 0.5 mm. This size range is suitable for the overflow value of most commonly used injection molding materials on the market, such as ABS, PMMA, hard PVC, soft PVC, PP, PA / PA6 / PA66, (PA / PA6 / PA66)+GF and other materials.
[0023] It is worth noting that the film expansion margin protrusion 3 and the film expansion margin concave portion 4 in the present application need to be arranged circumferentially along the parting line to ensure that the movable mold 1 and the fixed mold 2 have film expansion margin in the circumferential direction of the parting line after the mold is closed.
[0024] The specific embodiment of the present application also includes an arc portion 5 arranged on the film expansion margin convex portion 3 and the film expansion margin concave portion 4 away from the product direction, and the arc direction of the outer wall of the arc portion 5 along the cross-section of the mold opening direction is toward the direction away from the product, that is, to ensure that the arc portion 5 forms a trumpet-shaped structure at the film expansion margin concave portion 4, and correspondingly, an arc portion 5 is formed at the film expansion margin convex portion 3 to match the arc portion 5 at the film expansion margin concave portion 4.
[0025] For this purpose, the outer wall of the arc surface portion 5 is smoothly connected with the outer wall of the film expansion margin convex portion 3 and the film expansion margin concave portion 4, so as to ensure that the movable mold 1 and the fixed mold 2 can be smoothly closed and opened.
[0026] The tangent direction of one end of the arc surface portion 5 away from the film expansion allowance convex portion 3 and the film expansion allowance concave portion 4 is in the same direction as the normal direction of the mold opening direction, that is, it is ensured that the extension surface of one end of the arc surface portion 5 away from the film expansion allowance convex portion 3 and the film expansion allowance concave portion 4 is perpendicular to the wall surface of the film expansion allowance convex portion 3 and the film expansion allowance concave portion 4.
[0027] Combined with Figure 3 As shown, the product of the present application has a flash-free mold. During injection molding, the movable mold and the fixed mold will be slightly stretched apart under the action of the internal sol pressure. However, the present application adopts the design method of the film expansion margin convex part 3 and the film expansion margin concave part 4. The stretching distance is within the range of the film expansion margin. The molten plastic will not enter the parting surface and no flash will be formed after cooling.
[0028] In the present utility model, the terms "one embodiment", "some embodiments", "examples", "specific examples", "some examples", etc. mean that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present utility model. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the described specific features, structures, materials or characteristics can be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art can combine and combine different embodiments or examples described in this specification and the features of different embodiments or examples without contradiction.
[0029] The above is only a specific implementation of the utility model, but the protection scope of the utility model is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the utility model, which should be included in the protection scope of the utility model. Therefore, the protection scope of the utility model should be based on the protection scope of the claims.
Claims
1. A product without flash mold, characterized in that: It includes a movable mold and a fixed mold, one of which is provided with a film expansion margin convex portion extending along the parting surface of the product toward the mold opening direction, and the other is provided with a film expansion margin concave portion extending along the parting surface of the product toward the mold opening direction, and when the movable mold and the fixed mold are in a mold-clamping state, the film expansion margin convex portion is located in the film expansion margin concave portion.
2. The product flash-free mold according to claim 1, characterized in that: The extension length of the film expansion margin protrusion and the film expansion margin concave portion along the mold opening direction is in the range of 0.2 mm to 0.5 mm.
3. The product flash-free mold according to claim 1, characterized in that: It also includes an arc surface portion arranged on the film expansion margin convex portion and the film expansion margin concave portion away from the product direction, and the arc direction of the outer side wall of the cross section of the arc surface portion along the mold opening direction is facing away from the product.
4. The product flash-free mold according to claim 3, characterized in that: The arcuate outer wall of the arcuate portion is smoothly connected to the outer walls of the film expansion margin convex portion and the film expansion margin concave portion.
5. The product flash-free mold according to claim 4, characterized in that: The tangent direction of one end of the arc surface portion away from the film expansion margin convex portion and the film expansion margin concave portion is in the same direction as the normal direction of the mold opening direction.