Novel dry type composite ceramic tile

By introducing a buffer elastic layer into the composite tiles and setting a splicing part on the composite tiles, the cracking problem caused by the expansion difference between the tiles and the composite tiles is solved, the accuracy and construction convenience of the tiles are improved, and the number of rubber components is more Functionality improves the overall performance of the tiles.

CN221941813UActive Publication Date: 2024-11-01FOSHAN YIBAIFEN WOOD IND CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420228159.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-01
Estimated Expiration
2034-08-21

AI Technical Summary

Technical Problem

The different expansion coefficients of existing composite tiles between the ceramic plate and the composite plate lead to cracking, and the tiles are spliced ​​with low accuracy, difficult construction, and affecting the quality of the ceramic tiles.

Method used

Using ceramic tile boards, buffer elastic layer and composite boards that are laminated from top to bottom, buffer expansion deformation through buffer elastic layer, and matchable splicing parts are set on the composite board to achieve rapid splicing between ceramic tiles and improve construction convenience and splicing accuracy.

Benefits of technology

It effectively avoids cracks between the tiling board and the composite board, improves the flatness and splicing accuracy of tiling laying, simplifies the construction process, and improves the use effect of tiles through the sound insulation and moisture-proof and waterproof functions of rubber components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221941813U_ABST
    Figure CN221941813U_ABST
Patent Text Reader

Abstract

The novel dry type composite ceramic tile comprises a ceramic tile plate, a buffering elastic layer and a composite plate which are sequentially attached from top to bottom, and a first splicing part and a second splicing part which can be matched and spliced with each other are arranged on the two opposite sides of the composite plate respectively. Deformation and displacement caused by different expansion coefficients between the ceramic tile plate and the composite plate are buffered through the buffer elastic layer, the cracking phenomenon is avoided, the buffer elastic layer also has a vibration reduction effect, and during paving, adjacent composite ceramic tiles are spliced through the first splicing parts and the second splicing parts, so that the adjacent composite ceramic tiles can be kept flush, and the service life of the composite ceramic tiles is prolonged. Rapid laying and mounting are achieved, construction is convenient, the problem that adjacent composite tiles are uneven during laying is solved, tile plates do not need to be machined, the plasticity of the composite plates is better than that of the tile plates, machining is more convenient, the splicing precision is higher, and the tile plates can be made of conventional tiles.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of building materials, in particular to a novel dry composite tile. Background Art

[0002] With the rapid development of the current construction industry, the building decoration industry is also rising rapidly. Composite ceramic tiles are now used more and more widely. In order to reduce weight and increase the strength of the structure, a layer of composite board is generally set at the bottom of the ceramic plate. However, in actual use, due to the different expansion coefficients between the ceramic plate and the composite board, the connection between the composite board and the ceramic plate is prone to cracking. At the same time, in order to facilitate the laying construction, two adjacent ceramic tiles are now spliced ​​by snapping. Generally, a splicing part is set on the side of the ceramic tile. At present, the splicing part is integrally formed or processed on the side of the ceramic plate. However, in actual production and manufacturing, due to certain errors in the molding of the ceramic plate, the grooving accuracy is reduced when the side of the ceramic plate is grooved, resulting in a reduction in the final splicing matching accuracy. In addition, due to the high hardness of the ceramic tile, it is difficult to grooving the ceramic tile, which can easily affect the quality of the ceramic tile. Utility Model Content

[0003] The utility model aims to provide a novel dry composite tile to solve one or more technical problems existing in the prior art and at least provide a beneficial choice or create conditions.

[0004] The technical solutions adopted to solve the above technical problems are:

[0005] The utility model provides a novel dry composite tile, comprising: a tile plate, a buffer elastic layer and a composite plate which are sequentially attached from top to bottom, wherein the opposite sides of the composite plate are respectively provided with a first splicing part and a second splicing part which can be matched and spliced ​​with each other.

[0006] The beneficial effects of the utility model are:

[0007] The utility model arranges a buffer elastic layer between the ceramic tile plate and the composite plate, and uses the buffer elastic layer to buffer the deformation and displacement caused by the different expansion coefficients between the ceramic tile plate and the composite plate, thereby avoiding cracking. The buffer elastic layer also has a vibration reduction effect. When paving, adjacent composite ceramic tiles are spliced ​​by the first splicing part and the second splicing part, so that the adjacent composite ceramic tiles can be kept flat, and rapid paving and installation are achieved, which is convenient for construction and solves the problem of unevenness when adjacent composite ceramic tiles are paved. In addition, the first splicing part and the second splicing part are both processed on the composite plate, so there is no need to process the ceramic tile plate. The plasticity of the composite plate is better than that of the ceramic tile plate, and it is more convenient to process. The splicing accuracy is higher, and the ceramic tile plate can use conventional ceramic tiles.

[0008] As a further improvement of the above technical solution, the buffer elastic layer is a rubber component. The elasticity of the rubber component can buffer the displacement caused by different expansions, and the rubber has a certain sound insulation effect and is also moisture-proof and waterproof, which can prevent water vapor in the ground from seeping out.

[0009] As a further improvement of the above technical solution, the first splicing portion is a splicing groove, and the second splicing portion is a splicing strip.

[0010] This solution realizes the splicing between two composite tiles by engaging the splicing groove with the splicing strip. The structure is simple and the splicing strip can be inserted into the splicing groove.

[0011] The splicing groove is a groove structure recessed on the side wall of the composite board, and the splicing strip is a convex strip structure convexly disposed on the side wall of the composite board.

[0012] For the forming of the groove structure and the convex strip structure, the groove structure can be grooved from the side wall of the composite board, and the convex strip structure can be grooved from both surfaces of the composite board to form a boss; or the splicing groove and splicing strip can be formed together during the composite molding of the composite board, and changes can be made on the mold.

[0013] As a further improvement of the above technical solution, the ceramic tile board, the buffer elastic layer and the composite board are bonded together by gluing.

[0014] During assembly, the ceramic tile plate, the buffer elastic layer and the composite plate are fixed by gluing, thereby improving the firmness of the connection between the ceramic tile plate, the buffer elastic layer and the composite plate.

[0015] As a further improvement of the above technical solution, adhesive grooves are distributed on the top surface and the bottom surface of the buffer elastic layer.

[0016] In this solution, a plurality of adhesive grooves are arranged on the buffer elastic layer, which can increase the contact area of ​​the bonding surface, so as to improve the bonding strength per unit area, thereby improving the firmness of the buffer elastic layer.

[0017] As a further improvement of the above technical solution, the adhesive grooves on the top surface and the bottom surface of the buffer elastic layer are staggered up and down.

[0018] When gluing and fixing, the glue will fill the glue groove and form glue strips after solidification. The glue strips on the upper and lower sides of the buffer elastic layer are staggered with each other, so that the support effect of the buffer elastic layer is better and the processing of the glue groove is convenient. At this time, the depth of the glue groove can be set larger without considering the glue groove on the opposite side, while maintaining the buffering effect of the buffer elastic layer.

[0019] As a further improvement of the above technical solution, the bottom surface of the ceramic tile board and the top surface of the composite board are both provided with rough lines, which further improves the adhesion of the glue.

[0020] As a further improvement of the above technical solution, the side wall of the splicing groove is provided with a hook, and the side wall of the splicing strip is provided with a slot engaged with the hook. The engagement of the hook and the slot realizes the locking engagement of the splicing groove and the splicing strip, improves the firmness of the splicing of the splicing groove and the splicing strip, and avoids the splicing groove and the splicing strip from separating from each other during the construction process.

[0021] As a further improvement of the above technical solution, the first splicing portion and the second splicing portion are both locking structures. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The utility model is further described below in conjunction with the accompanying drawings and embodiments;

[0023] Figure 1 This is an exploded view of an embodiment of the novel dry composite tile provided by the utility model;

[0024] Figure 2 This is a cross-sectional view of an embodiment of the novel dry composite tile provided by the utility model;

[0025] Figure 3 It is a schematic diagram of the joints between the joint grooves and the joint strips of two composite tiles in one embodiment of the new dry composite tile provided by the utility model;

[0026] Figure 4 This is a schematic diagram of a new type of dry composite tile provided by the utility model, in which two composite tiles of one embodiment are connected by a lock. DETAILED DESCRIPTION

[0027] This section will describe in detail the specific embodiments of the utility model. The preferred embodiments of the utility model are shown in the accompanying drawings. The purpose of the accompanying drawings is to supplement the description of the text part of the specification with graphics, so that people can intuitively and vividly understand each technical feature and the overall technical solution of the utility model, but it cannot be understood as a limitation on the protection scope of the utility model.

[0028] In the description of the present invention, it should be understood that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0029] In the description of the present utility model, if there are words such as "several", it means one or more, "more" means more than two, greater than, less than, exceed, etc. are understood to exclude the number, and above, below, within, etc. are understood to include the number.

[0030] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.

[0031] Reference Figure 1 to Figure 3 The new dry composite tile of the utility model is made into the following embodiments:

[0032] like Figure 1 As shown, the new dry composite tile of this embodiment includes a tile plate 100, a buffer elastic layer 200 and a composite plate 300. The tile plate 100, the buffer elastic layer 200 and the composite plate 300 are sequentially attached from top to bottom to form a composite tile.

[0033] The buffer elastic layer 200 of this embodiment is made of rubber material, and the buffer elastic layer 200 has a rubber component with certain elasticity.

[0034] A buffer elastic layer 200 is arranged between the tile plate 100 and the composite plate 300. The elasticity of the buffer elastic layer 200 is used to buffer the deformation and displacement between the tile plate 100 and the composite plate 300 due to the different expansion coefficients, thereby avoiding cracking. Rubber has certain sound insulation and vibration reduction effects, and also has moisture-proof and waterproof functions, which can prevent water vapor in the ground from seeping out.

[0035] Furthermore, the tile plate 100, the buffer elastic layer 200 and the composite plate 300 of the present embodiment are bonded together by gluing. During assembly, the tile plate 100, the buffer elastic layer 200 and the composite plate 300 are fixed by gluing, thereby improving the firmness of the connection between the tile plate 100, the buffer elastic layer 200 and the composite plate 300.

[0036] In this embodiment, adhesive grooves 210 are provided on the top and bottom surfaces of the buffer elastic layer 200. A plurality of adhesive grooves 210 are provided on the buffer elastic layer 200 to increase the contact area of ​​the bonding surface to improve the bonding strength per unit area, thereby improving the firmness of the buffer elastic layer 200.

[0037] Among them, multiple glue grooves 210 of this embodiment are arranged at intervals along the buffering elastic layer 200, and the glue grooves 210 on the top and bottom surfaces of the buffering elastic layer 200 are staggered up and down. When gluing and fixing, the glue will fill the glue grooves 210 and form glue strips after solidification. The glue strips on the upper and lower sides of the buffering elastic layer 200 are staggered with each other, so that the supporting effect of the buffering elastic layer 200 is better, and the processing of the glue grooves 210 is also convenient. At this time, the depth of the glue grooves 210 can be set larger without considering the glue grooves 210 on the opposite side, and the buffering effect of the buffering elastic layer 200 is maintained.

[0038] In other embodiments, the adhesive grooves 210 on the top and bottom surfaces of the buffer elastic layer 200 may be crisscrossed, and the adhesive strips on the upper and lower sides may support each other.

[0039] Furthermore, rough textures are provided on the bottom surface of the ceramic tile board 100 and the top surface of the composite board 300, and the provision of the rough textures further improves the adhesion of the glue.

[0040] In order to achieve rapid paving, the present embodiment provides a first splicing portion and a second splicing portion on opposite sides of the composite panel 300, respectively. The first splicing portion and the second splicing portion are matched and spliced ​​with each other. The composite panel 300 of the present embodiment is rectangular, and two first splicing portions and two second splicing portions are distributed around the composite panel 300. When paving, adjacent composite tiles are spliced ​​through the first splicing portion and the second splicing portion. In this way, adjacent composite tiles can be kept level, rapid paving and installation can be achieved, construction is convenient, and the problem of unevenness when adjacent composite tiles are laid is solved.

[0041] In addition, the first splicing part and the second splicing part are both processed on the composite board 300, so there is no need to process the ceramic tile board 100. The plasticity of the composite board 300 is better than that of the ceramic tile board 100, which is more convenient to process and makes the splicing accuracy higher. The ceramic tile board 100 can use conventional ceramic tiles.

[0042] The first splicing part of this embodiment includes a splicing groove 310, and the second splicing part includes a splicing strip 320. This embodiment realizes the splicing between two composite tiles by engaging the splicing groove 310 with the splicing strip 320. The structure is simple, and the splicing strip 320 can be inserted into the splicing groove 310.

[0043] like Figure 2 As shown, the splicing groove 310 of this embodiment is a groove structure recessed on the side wall of the composite board 300 , and the splicing strip 320 is a convex strip structure convexly disposed on the side wall of the composite board 300 .

[0044] Regarding the formation of the groove structure and the convex strip structure, in other embodiments, the groove structure may be grooved from the side wall of the composite plate 300, and the convex strip structure may be grooved from both surfaces of the composite plate 300 to form a boss;

[0045] In this embodiment, the composite board 300 is formed together with the splicing groove 310 and the splicing strip 320 during composite molding, and changes are made to the mold.

[0046] Furthermore, if Figure 3 As shown, the inner side wall of the splicing groove 310 is provided with a hook 311 , and the outer side wall of the splicing strip 320 is provided with a slot 321 corresponding to the hook 311 .

[0047] In this embodiment, the locking connection between the splicing groove 310 and the splicing strip 320 is achieved by the engagement of the hook 311 and the slot 321, thereby improving the firmness of the splicing between the splicing groove 310 and the splicing strip 320 and avoiding the splicing groove 310 and the splicing strip 320 from separating from each other during the construction process.

[0048] In order to facilitate the insertion of the splicing strip 320 into the splicing groove 310, the hook 311 is provided with an introduction slope 3111, and the introduction slope 3111 is inclined outward from the opening of the splicing groove 310 toward the bottom of the groove. The inner end of the introduction slope 3111 is provided with a clamping surface 3112, and the clamping surface 3112 and the introduction slope 3111 form a triangular clamping block structure, and the clamping surface 3112 contacts the side of the clamping groove 321 to achieve a buckle fit.

[0049] In some other embodiments, such as Figure 4 As shown, the first splicing portion and the second splicing portion are both lock structures, and the first splicing portion and the second splicing portion are fastened together by means of a lock.

[0050] The preferred implementation modes of the present invention are specifically described above, but the present invention is not limited to the described embodiments. Those skilled in the art may make various equivalent modifications or substitutions without violating the spirit of the present invention, and these equivalent modifications or substitutions are all included in the scope defined by the claims of this application.

Claims

1. A new type of dry composite tile, characterized in that: include: A ceramic tile plate (100), a buffer elastic layer (200) and a composite plate (300) are sequentially attached from top to bottom, wherein two opposite sides of the composite plate (300) are respectively provided with a first splicing portion and a second splicing portion that can be matched and spliced ​​with each other.

2. The novel dry composite tile according to claim 1 is characterized in that: The buffer elastic layer (200) is a rubber component.

3. The novel dry composite tile according to claim 1 is characterized in that: The first splicing portion is a splicing groove (310), and the second splicing portion is a splicing strip (320).

4. The novel dry composite tile according to claim 3 is characterized in that: The splicing groove (310) is a groove structure recessed on the side wall of the composite plate (300), and the splicing strip (320) is a convex strip structure convexly disposed on the side wall of the composite plate (300).

5. The novel dry composite tile according to claim 3 is characterized in that: The side wall of the splicing groove (310) is provided with a hook (311), and the side wall of the splicing strip (320) is provided with a slot (321) that is engaged with the hook (311).

6. The novel dry composite tile according to claim 3 is characterized in that: The splicing groove (310), the splicing strip (320) and the composite plate (300) are integrally formed.

7. The novel dry composite tile according to claim 1 is characterized in that: The ceramic tile plate (100), the buffer elastic layer (200) and the composite plate (300) are bonded together by gluing.

8. The novel dry composite tile according to claim 7 is characterized in that: The top surface and the bottom surface of the buffer elastic layer (200) are both provided with adhesive grooves (210).

9. The novel dry composite tile according to claim 8 is characterized in that: The adhesive grooves (210) on the top surface and the bottom surface of the buffer elastic layer (200) are arranged in an up-and-down staggered manner.

10. The novel dry composite tile according to claim 1 is characterized in that: The first splicing portion and the second splicing portion are both locking structures.