Photovoltaic welding strip and photovoltaic module
By designing a diffuse reflective structure on the upper surface of the photovoltaic welding tape, the problem of the welding tape blocking light is solved, the CTM value of the photovoltaic module is improved, and the light utilization rate is improved.
Patent Information
- Application Number
- CN202323387891.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-12
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2033-12-12
AI Technical Summary
The presence of welding tapes in existing photovoltaic modules leads to light occlusion, reducing the light utilization rate of photovoltaic modules, and thus lowering the CTM of the module.
A photovoltaic welding tape is designed with a diffuse reflection structure on the upper surface. The diffuse reflection rate of light is increased through suede or pyramid structure, so that light can form diffuse reflection on the welding tape, thereby improving the light utilization rate of photovoltaic modules.
Through the design of the diffuse reflection structure, the CTM value of the photovoltaic module is improved, the light utilization rate is increased by 1% to 2%, and the output power of the module is improved.
Smart Images

Figure CN221977951U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of photovoltaic power generation technology, and in particular to a photovoltaic welding strip and a photovoltaic module. Background Art
[0002] With the continuous development of technology, the photoelectric conversion efficiency of photovoltaic cells has been greatly improved.
[0003] However, because the cells in the photovoltaic module need to be connected by welding ribbons, the presence of welding ribbons will block part of the light, affecting the utilization rate of light by the photovoltaic module, resulting in a low CTM of existing photovoltaic modules.
[0004] Therefore, the prior art needs to be improved. Utility Model Content
[0005] The technical problem to be solved by the present application is to provide a photovoltaic welding strip and a photovoltaic module to solve the problem in the prior art that the CTM of the photovoltaic module is low due to the presence of the welding strip.
[0006] In order to solve the above problems, the present application is implemented through the following technical solutions:
[0007] The present application proposes a photovoltaic welding strip, which includes a welding strip body, the cross-section of the welding strip body is rectangular, and the upper surface of the welding strip body has a diffuse reflection structure, and the diffuse reflection structure is used to diffusely reflect light.
[0008] Optionally, in the photovoltaic welding strip, the diffuse reflection structure is velvet.
[0009] Optionally, in the photovoltaic welding ribbon, the velvet surface includes a pyramid structure with a bottom size of 2 to 8 microns and a height of 1 to 5 microns.
[0010] Optionally, in the photovoltaic welding strip, the reflectivity of the upper surface of the welding strip body is greater than or equal to 85%.
[0011] Optionally, in the photovoltaic welding strip, the welding strip body also includes a lower surface, the lower surface is used to contact the light-receiving surface of the photovoltaic cell, and the lower surface is a planar structure.
[0012] Optionally, in the photovoltaic welding strip, an anti-corrosion coating is provided on the upper surface of the welding strip.
[0013] Optionally, in the photovoltaic welding ribbon, the material of the anti-corrosion coating is parabens.
[0014] The present application proposes a photovoltaic module, which includes a cover glass, a plurality of photovoltaic cells and a back panel stacked in sequence from top to bottom, wherein adjacent photovoltaic cells are connected by the photovoltaic welding strip as described above, and the upper surface of the photovoltaic welding strip is located on the side of the welding strip away from the photovoltaic cell.
[0015] Optionally, the photovoltaic module also includes a front adhesive film and a back adhesive film; the front adhesive film is arranged between the cover glass and the photovoltaic cell, and is used to bond the cover glass and the photovoltaic cell; the back adhesive film is arranged between the photovoltaic cell and the back panel, and is used to bond the photovoltaic cell and the back panel.
[0016] Optionally, in the photovoltaic module, the front adhesive film and the back adhesive film are both POE films.
[0017] Compared with the prior art, this application has the following advantages:
[0018] The photovoltaic welding strip in the present application includes a welding strip body, the cross-section of the welding strip body is rectangular, and the upper surface of the welding strip body has a diffuse reflection structure, which is used to diffusely reflect light; wherein, by designing a diffuse reflection structure on the upper surface of the welding strip, light can be diffusely reflected on the welding strip, which can effectively improve the utilization rate of light by the photovoltaic module, so that the CTM of the photovoltaic module is increased by 1% to 2%.
[0019] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is a schematic diagram of the structure of the photovoltaic welding strip in the embodiment of the present application;
[0021] Figure 2 It is a schematic diagram of the optical path of the welding strip in the prior art;
[0022] Figure 3 This is a schematic diagram of the optical path of the photovoltaic welding strip in the embodiment of the present application;
[0023] Figure 4 A schematic diagram of the structure of a photovoltaic module provided in an embodiment of the present application;
[0024] Figure 5 This is an exploded view of the photovoltaic module provided in an embodiment of the present application. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0026] It should be understood that the references to "one embodiment" or "an embodiment" throughout the specification mean that the specific features, structures, or characteristics associated with the embodiment are included in at least one embodiment of the present application. Therefore, the references to "in one embodiment" or "in an embodiment" appearing throughout the specification do not necessarily refer to the same embodiment. In addition, these specific features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.
[0027] The welding tape is an important raw material in the photovoltaic module welding process. The quality of the welding tape will directly affect the current collection efficiency of the photovoltaic module and has a great impact on the power of the photovoltaic module. In practical applications, the thickness of the welding tape needs to be determined according to the thickness of the battery cell and the amount of short-circuit current. The width of the welding tape should be consistent with the width of the main line of the battery, and the hardness of the welding tape generally depends on the thickness of the battery cell and the welding tool. In the production process of photovoltaic modules, the electrode (current) of the battery cell is led out through the welding process, and then the led-out electrode is effectively connected to the junction box in series or parallel.
[0028] The module CTM is the percentage of the sum of the module output power and the battery cell power, which is used to indicate the degree of module power loss. The higher the CTM value, the smaller the degree of module packaging power loss.
[0029] The applicant found that the factors affecting CTM include optical loss, resistance loss, current mismatch loss caused by connecting cells of different currents in series, heat loss, output power loss caused by increased module temperature, cell efficiency attenuation and intrinsic decay loss caused by BO recombination, and hidden cracks or fragments generated during module production. In existing photovoltaic modules, each cell needs to be connected by a welding ribbon, and the presence of the welding ribbon will block part of the light, affecting the utilization rate of light by the photovoltaic module, resulting in a low CTM of the existing photovoltaic module.
[0030] In view of the above problems, the present application provides a photovoltaic welding strip 16, such as Figure 1 As shown, it includes a solder strip body 160 , the cross section of the solder strip body 160 is rectangular, and the upper surface 161 of the solder strip body 160 has a diffuse reflection structure, which is used to diffusely reflect light.
[0031] Because the surface of the soldering tape used in existing photovoltaic modules is smooth and flat, when light is incident on the surface of the soldering tape, it will be directly reflected. Figure 2 As shown, this part of the light cannot be utilized by the component, which not only reduces the input power of the component, but also reduces the CTM value of the component.
[0032] Diffuse reflection is the phenomenon that light projected on a rough surface is reflected in all directions. Because the rough surface is uneven, and the reflection of light follows the law of light reflection, when a beam of parallel incident light hits the rough surface, the surface will reflect the light in all directions. Therefore, although the incident rays are parallel to each other, the normal directions of each point are inconsistent, causing the reflected light to be reflected irregularly in different directions. This reflection is called "diffuse reflection" or "diffuse".
[0033] In the embodiment of the present application, the upper surface 161 of the welding strip body 160 is designed with a diffuse reflection structure so that light is diffusely reflected on the photovoltaic welding strip 16. Figure 3 As shown, light can enter the cell after multiple reflections, thereby improving the light utilization rate of the photovoltaic module and increasing the CTM of the photovoltaic module by 1% to 2%.
[0034] The velvet surface on the upper surface of the solder strip body 160 may be formed by embossing, specifically, mechanical or hot embossing technology may be used to process the surface of the solder strip body 160 to form a velvet texture, making the surface of the solder strip body 160 rougher.
[0035] Optionally, in a specific implementation, the roughness of the upper surface 161 of the welding strip body 160 is Ra4-3.2 microns.
[0036] Among them, the velvet surface of the upper surface 161 of the above-mentioned welding body 160 can be formed by chemical treatment, specifically, the surface of the welding strip 16 can be treated by chemical methods such as natural oxidation, pickling or anodizing, which can not only make the surface of the welding strip 16 have a velvet effect, but also increase its corrosion resistance.
[0037] Optionally, in a specific embodiment, the velvet surface of the upper surface 161 of the solder strip body 160 can be formed by coating a layer of anti-corrosion coating 17 on the surface, and the coating can be a polymer or a paint, which can not only slightly corrode the solder strip body 160, so that the surface of the solder strip body 160 has a velvet effect, but also increase the weather resistance and corrosion resistance of the solder strip body 160. Specifically, the coating can be parabens, such as methyl paraben, ethyl paraben, propyl paraben, butyl paraben, etc.
[0038] Optionally, in one embodiment, the diffuse reflection structure is a suede surface, that is, the concave-convex structure of the suede surface is used to achieve diffuse reflection of incident light, thereby improving the utilization rate of light by the photovoltaic module.
[0039] Optionally, in one embodiment, the velvet surface includes a pyramid structure with a bottom size of 2 to 8 microns and a height of 1 to 5 microns, which can effectively improve the diffuse reflection performance of the welding strip body 160 while maintaining the welding performance of the welding strip body 160. The pyramid structure is fully distributed on the upper surface 161 of the welding strip body 160.
[0040] Optionally, the bottom size of the pyramid structure may be 2 microns, 3 microns, 4 microns, 5 microns, 6 microns, 7 microns, 8 microns or any two of the above range values; the bottom size of the pyramid structure may be 1 micron, 2 microns, 3 microns, 4 microns, 5 microns or any two of the above range values.
[0041] Optionally, in one embodiment, the velvet surface comprises a pyramid structure with a bottom size of 4 to 5 microns and a height of 2 to 3 microns.
[0042] In the embodiment of the present application, by providing the velvet surface on the upper surface 161 , the reflectivity of the upper surface 161 of the solder strip body 160 reaches more than 85%, which can effectively improve the diffuse reflection performance of the solder strip body 106 and increase the utilization rate of the front incident light.
[0043] In actual welding applications, the upper surface 161 is located on the side of the welding strip body 160 away from the photovoltaic cell 13 , that is, located on the front side of the cell, so as to facilitate diffuse reflection of incident light.
[0044] Optionally, in one embodiment, the above-mentioned welding strip body 160 also includes a lower surface 162, which is used to contact the light-receiving surface of the photovoltaic cell 13. The lower surface 162 is a planar structure, that is, the lower surface 162 of the welding strip 16 is smooth and flat, which facilitates welding and increases welding tension.
[0045] In the embodiment of the present application, the welding strip body is composed of a copper substrate and a welding coating coated on the surface of the copper substrate.
[0046] Among them, the copper substrate plays a conductive role. The copper substrate is high-purity oxygen-free copper. The lower its resistivity, the greater its load-bearing capacity and the better its plasticity. Oxygen-free copper is pure copper that does not contain oxygen or any deoxidizer residues; the solder coating is a tin-lead coating, which has low cost, is easy to use and has good effect. In the embodiment of the present application, the thickness of the solder coating is 0.01 to 0.05 mm.
[0047] Optionally, in one embodiment, the surface of the solder strip body 160 is provided with an anti-corrosion coating 17, which can slightly corrode the solder strip body 160, so that the surface of the solder strip body 160 produces a suede effect, and can increase the weather resistance and corrosion resistance of the solder strip body 160.
[0048] Optionally, in a specific embodiment, the material of the above-mentioned anti-corrosion coating 17 can be parabens, such as methyl paraben, ethyl paraben, propyl paraben, butyl paraben, etc., which can not only increase the weather resistance and corrosion resistance of the solder strip body 160, but also slightly corrode the solder strip body 160, so that the surface of the solder strip body 160 further produces a suede effect.
[0049] Optionally, in a specific embodiment, the thickness of the anti-corrosion coating 17 can be 2 to 15 microns, for example, 2 microns, 3 microns, 5 microns, 8 microns, 10 microns, 12 microns, 14 microns, 15 microns or any two of the above ranges.
[0050] In practical applications, the photovoltaic welding strip 10 is a long rectangular copper wire as a whole.
[0051] The present application also provides a photovoltaic assembly 20, such as Figures 4-5 As shown, it includes a cover glass 11, a plurality of photovoltaic cells 13 and a back plate 15 stacked in sequence from top to bottom, adjacent photovoltaic cells 13 are connected by the above-mentioned photovoltaic welding strips 16, and the upper surface 161 of the welding strip body 160 in the above-mentioned photovoltaic welding strip 16 is located on the side of the welding strip away from the photovoltaic cell.
[0052] In the photovoltaic module provided in the embodiment of the present application, the upper surface 161 is located on the side of the welding strip body 160 away from the photovoltaic cell 13, that is, located on the front side of the cell, so as to facilitate diffuse reflection of incident light.
[0053] The above-mentioned photovoltaic welding ribbon is welded on the front side of the battery cell to conduct the current collected by the battery cell. The width is consistent with the width of the main grid line of the battery cell, and the thickness is 200 to 260 microns. Avoid the welding ribbon being too thick to prevent the battery cell from crushing the component during the lamination stage.
[0054] Optionally, the photovoltaic module 10 provided in the embodiment of the present application further includes a front adhesive film 12 and a back adhesive film 14; the front adhesive film 12 is disposed between the cover glass 11 and the photovoltaic cell 13, and is used to bond the cover glass 11 and the photovoltaic cell 13; the back adhesive film is disposed between the photovoltaic cell 13 and the back plate 15, and is used to bond the photovoltaic cell 13 and the back plate 15. The cover glass 11 and the photovoltaic cell 13 are bonded together by the front adhesive film 12, and the photovoltaic cell 13 and the back plate 15 are bonded together by the back adhesive film.
[0055] Optionally, in one embodiment, the front adhesive film 12 and the back adhesive film 14 are both POE films, which have poor water permeability but good light transmittance. They can achieve sealing protection for the photovoltaic cell 13 while ensuring the amount of light entering, making the photovoltaic cell 13 not easily corroded by water vapor.
[0056] In the embodiment of the present application, the photovoltaic cell 13 may be an N-type cell or a P-type cell, and may be specifically an N-type Topcon cell.
[0057] In practical applications, the preparation process of the photovoltaic module provided in the embodiment of the present application includes steps 1 to 7.
[0058] Step 1: Take an N-type Topcon cell with a storage efficiency of 24.3%.
[0059] Step 2: Use lossless laser scribing, and the utilization rate of laser power is 50.5%.
[0060] Step 3: Serial welding of battery cells.
[0061] In this step, the photovoltaic welding strip in the embodiment of the present application is used for welding, and the welding method adopts a non-contact welding method, that is, the welding work is completed by selecting infrared rays of appropriate wavelengths to radiate heating on the welding points.
[0062] Step 4: Layering:
[0063] Arrange the battery cells after string welding, then weld the bus bars, set POE film in front and behind each battery cell, and then place the glass sheet.
[0064] Step 5, front electroluminescence test:
[0065] By applying voltage to the two poles of the battery to generate an electric field, the electrons excited by the back electric field collide with the luminescence center, causing the electron dissociation level to jump, change, and recombine, resulting in luminescence.
[0066] In this step, the above test is used to detect whether there are problems such as mixed packing, bright and dark pieces, over-soldering, and cold soldering of the battery cells.
[0067] Step 6: Lamination:
[0068] The stacked components are placed in a laminator, the air in the components is extracted by vacuuming, and then the POE is heated to melt and bond the battery cells and glass together. Finally, the components are cooled and taken out.
[0069] After the laminated components are inspected, framed, cured, cleaned, etc., photovoltaic component products are obtained.
[0070] Experiments show that in the case of 72 panels - 144 half-cell cells, the power of the photovoltaic module in the embodiment of the present application is 576.8W, and its CTM value is 99%, which is 1.5% higher than the CTM value of the traditional circular welding strip.
[0071] In summary, in this embodiment, the photovoltaic module includes a cover glass, a plurality of photovoltaic cells and a back panel stacked in sequence from top to bottom, and adjacent photovoltaic cells are connected by a photovoltaic welding ribbon. The cross-section of the welding ribbon body is rectangular, and the upper surface of the welding ribbon body has a velvet structure. Among them, by performing a velvet design on the upper surface of the welding ribbon body, light can be diffusely reflected on the welding ribbon body, which can effectively improve the utilization rate of light by the photovoltaic module, so that the CTM of the photovoltaic module is increased by 1% to 2%.
[0072] It should be noted that the various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0073] Although the optional embodiments of the present application have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including optional embodiments and all changes and modifications that fall within the scope of the present application.
[0074] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity from another entity, and do not necessarily require or imply any such actual relationship or order between these entities. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that an article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such article or terminal device. In the absence of further restrictions, the elements defined by the sentence "including one..." do not exclude the existence of other identical elements in the article or terminal device including the elements.
[0075] The technical solution provided by the present application is introduced in detail above. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. At the same time, for those skilled in the art, according to the principles and implementation methods of the present application, there may be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present application.
Claims
1. A photovoltaic welding ribbon, characterized in that: It comprises a welding strip body, the cross section of the welding strip body is rectangular, the upper surface of the welding strip body has a diffuse reflection structure, and the diffuse reflection structure is used to diffusely reflect light; The diffuse reflection structure is a suede surface; The velvet surface includes a pyramid structure with a bottom size of 2 to 8 microns and a height of 1 to 5 microns; The roughness of the upper surface of the welding strip body is Ra4-3.2 microns; The velvet surface is obtained by coating a layer of anti-corrosion coating on the upper surface of the welding strip; The photovoltaic welding strip is used to be welded on the front side of the battery cell to conduct the current collected by the battery cell, and the width is consistent with the width of the main grid line of the battery cell, and the thickness is 200 to 260 microns.
2. The photovoltaic welding strip according to claim 1, characterized in that: The reflectivity of the upper surface of the welding strip body is greater than or equal to 85%.
3. The photovoltaic welding strip according to claim 2, characterized in that: The welding strip body also includes a lower surface, which is used to contact the light-receiving surface of the photovoltaic cell sheet, and the lower surface is a planar structure.
4. The photovoltaic welding ribbon according to claim 1, characterized in that: The upper surface of the welding strip is provided with an anti-corrosion coating.
5. The photovoltaic welding strip according to claim 4, characterized in that: The material of the anti-corrosion coating is parabens.
6. A photovoltaic module, characterized in that: It comprises a cover glass, a plurality of photovoltaic cells and a back plate which are stacked in sequence from top to bottom, wherein adjacent photovoltaic cells are connected by a photovoltaic welding strip as described in any one of claims 1 to 5, and the upper surface is located on a side of the photovoltaic welding strip away from the photovoltaic cells.
7. The photovoltaic module according to claim 6, characterized in that: The photovoltaic module also includes a front adhesive film and a back adhesive film; the front adhesive film is arranged between the cover glass and the photovoltaic cell, and is used to bond the cover glass and the photovoltaic cell; the back adhesive film is arranged between the photovoltaic cell and the back plate, and is used to bond the photovoltaic cell and the back plate.
8. The photovoltaic module according to claim 7, characterized in that: The front adhesive film and the back adhesive film are both POE films.