Mold structure for overcoming flash defect of injection molded part

By designing the glue-reducing grooves and boss structures between the fixed template and the moving template in the injection mold, a tiny thin-wall cavity is formed and the melt is freezed first, which solves the problem of flashing the injection molded parts and realizes automated production and cost savings .

CN222004246UActive Publication Date: 2024-11-15JIAXING XINYUAN PRECISION MOLD TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323530162.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-22
Publication Date
2024-11-15
Estimated Expiration
2033-12-22

AI Technical Summary

Technical Problem

In injection molds, excessive plastic fluidity leads to difficulties in sealing glue around the parting surface, causing flash problems, which require manual removal, affecting work efficiency and increasing costs.

Method used

Design a mold structure, including a fixed template and a moving template. There is a parting surface and a rubber-reducing groove between the fixed template and the moving template. There is a boss on the moving template that cooperates with the rubber-reducing groove to form a tiny thin-walled shape. The distance between the cavity, the boss and the end surface of the parting surface is 0.3-0.5mm, and the width is 1/3-1/2 of the main wall thickness of the plastic product. The thin-wall cavity is preferred to freeze to prevent melt overflow.

Benefits of technology

It effectively solves the flash problem, avoids mold welding and surface reduction processing, saves maintenance costs, realizes automated production, and improves product qualification rate and work efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222004246U_ABST
    Figure CN222004246U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of injection molding production, and provides a mold structure for solving the flash defect of an injection molded part, which comprises a fixed mold plate and a movable mold plate, a plastic product is arranged between the fixed mold plate and the movable mold plate, a parting surface is arranged between the fixed mold plate and the movable mold plate, and the plastic product is provided with a glue reducing groove. The movable mold plate is provided with a boss matched with the glue reducing groove, and a tiny thin-wall cavity is formed between the boss and the fixed mold plate. The mold has the advantages that the appearance, the use function, the structural strength and the assembly relation of a plastic part product are not influenced, the characteristics are designed during mold design, the machining procedures of mold welding, mold surface lowering and the like can be avoided, the mold maintenance cost is effectively saved, the problem of burrs on the parting surface of an injection molding part is solved, production is stable, the product percent of pass is improved, and the production cost is reduced. The process of manually removing the flash is not needed, automatic production can be achieved, and the working efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of injection molding production, and in particular relates to a mold structure for solving the flash defects of injection molded parts. Background Art

[0002] In injection molds, some plastics have too good fluidity, making it difficult to seal the parting surface during mold closing and injection molding. The molten material overflows the cavity, and excess glue is generated on the parting surface, leading to flash problems. The flash needs to be removed manually with a scraper, affecting work efficiency and increasing labor costs. When existing molds encounter such problems, they usually weld and add iron to the parting surface or lower the surface to reprocess the parting surface so that the fixed mold plate and the movable mold plate fit more tightly on the parting surface sealing surface. However, although the mold closing mark can reach a better state during the mold closing process, flash will still occur during the actual injection molding machine injection molding process. Utility Model Content

[0003] The technical problem to be solved by the utility model is to provide a mold structure for solving the flash defects of injection molded parts in view of the current status of the prior art, change the flow behavior of the melt in the parting line area, so that the melt around the parting line preferentially forms a freezing layer to close the overflow channel, thereby solving the flash problem of the parting surface of the product.

[0004] The technical solution adopted by the utility model to solve the above technical problems is: a mold structure for solving the flash defects of injection molded parts, including a fixed mold plate and a movable mold plate, a plastic product is provided between the fixed mold plate and the movable mold plate, and is characterized in that a parting surface is provided between the fixed mold plate and the movable mold plate, the plastic product has a glue reduction groove, the movable mold plate has a boss matched with the glue reduction groove, and a tiny thin-wall cavity is formed between the boss and the fixed mold plate.

[0005] In the above-mentioned mold structure for solving the flash defect of injection molded parts, the end surface distance between the boss and the end surface of the parting surface is 0.3-0.5 mm.

[0006] In the above-mentioned mold structure for solving the flash defect of injection molded parts, the height distance of the boss is 0.5 mm.

[0007] In the above-mentioned mold structure for solving the flash defect of injection molded parts, the width distance of the boss is 1 / 3-1 / 2 of the main wall thickness of the plastic product.

[0008] Compared with the prior art, the advantage of the utility model is that it does not affect the appearance, use function, structural strength, and assembly relationship of the plastic product. By designing this feature during mold design, processing procedures such as mold welding and mold surface reduction can be avoided, and mold maintenance costs can be effectively saved. The problem of flash on the parting surface of injection molded parts can be solved, production can be stabilized, and the product qualification rate can be improved. There is no need for manual flash removal, and automated production can be achieved to improve work efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is an overall schematic diagram of the mold structure for solving the flash defect of injection molded parts. DETAILED DESCRIPTION

[0010] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.

[0011] In the figure, the fixed mold plate 100; the movable mold plate 200; the plastic product 300; the glue reduction groove 301; the boss 400; the height distance 401; the width distance 402; the end face distance 403; and the parting surface 500.

[0012] like Figure 1 As shown, the mold structure for solving the flash defect of injection molded parts includes a fixed mold plate 100 and a movable mold plate 200, a plastic product 300 is provided between the fixed mold plate 100 and the movable mold plate 200, and a parting surface 500 is provided between the fixed mold plate 100 and the movable mold plate 200. Before the injection mold structure is designed, the inner wall of the plastic product of the parting surface 500 is adjusted in advance, and the modification premise is based on customer needs such as not affecting the product appearance, use function, structural strength, and assembly relationship. The plastic product has a glue reduction groove 301, and the movable mold plate 200 has a boss 400 matched with the glue reduction groove 301, and a tiny thin-walled cavity is formed between the boss 400 and the fixed mold plate 100, and the end face distance 403 between the boss 400 and the end face of the parting surface 500 is 0.3-0.5mm, and the height distance 401 of the boss 400 is 0.5m m, the height distance 401 should not be too large, otherwise it will lead to appearance surface marks defects, the width distance 402 of the boss 400 is 1 / 3-1 / 2 of the main wall thickness of the plastic product 300, usually about 1mm, the boss 400 feature surrounds the entire parting surface 500 area, when the mold is closed for injection, the fixed template 100 and the movable template 200 collide and close at the parting surface 500, because the end face distance 403 of the boss 400 is a thin-wall feature, that is, there is a 0.3-0.5mm thin-wall cavity on the edge of the product, when the plastic melt is injected into the feature area, the heat of the thin-wall area dissipates faster, and it freezes first than other wall thickness areas, forming a frozen layer in the parting surface 500 area, which can prevent the plastic melt from overflowing and avoid the generation of flash in the parting surface 500 area. The technology achieves the purpose of preventing flash problems through the principle of preferential freezing of thin-wall cavities.

[0013] The specific embodiments described in this article are merely examples of the spirit of the present invention. Technicians in the technical field to which the present invention belongs can make various modifications or additions to the described specific embodiments or replace them in a similar manner, but they will not deviate from the scope defined by the spirit of the present invention.

Claims

1. A mold structure for solving the flash defect of injection molded parts, comprising a fixed mold plate and a movable mold plate, wherein a plastic product is provided between the fixed mold plate and the movable mold plate, characterized in that: A parting surface is provided between the fixed template and the movable template, the plastic product has a glue reduction groove, the movable template has a boss matched with the glue reduction groove, and a tiny thin-wall cavity is formed between the boss and the fixed template.

2. A mold structure for solving the flash defect of injection molded parts according to claim 1, characterized in that: The end surface distance between the boss and the end surface of the parting surface is 0.3-0.5mm.

3. A mold structure for solving the flash defect of injection molded parts according to claim 2, characterized in that: The height distance of the bosses is 0.5 mm.

4. A mold structure for solving the flash defect of injection molded parts according to claim 3, characterized in that: The width of the boss is 1 / 3-1 / 2 of the main wall thickness of the plastic product.