Thin-shell sheet part forming die
By designing the combination of the fixed mold, moving mold, oblique top mechanism and core pulling mechanism of the thin shell sheet part mold, the problem of difficult demolding of thin shell sheet parts during injection molding is solved, and efficient demolding is achieved and high-quality molding.
Patent Information
- Application Number
- CN202323619528.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2033-12-28
AI Technical Summary
There are difficulties in demolding during injection molding of existing thin shell sheet parts, resulting in problems of low molding quality and low efficiency, especially because their irregular shape clamping features affect mold release.
A thin shell sheet part forming mold including a fixed mold, a moving mold, an inclined top mechanism and a core extraction mechanism is designed. Through the cooperation of a fixed mold core, a moving mold core, an inclined top mechanism and a core extraction mechanism, a thin shell part is formed for injection molding. The mold cavity is used to separate the moving mold and the fixed mold when the mold is opened, and the core pulling mechanism and the molding parts are synchronously demolded. The thimble mechanism drives the mold release and separation of the oblique top mechanism and the molding parts to reduce the demolding process. Collision and friction.
The molding and demolding processing efficiency and demolding quality of thin shell sheet parts are improved, collision and friction during the demolding process is reduced, and production efficiency and product quality are improved.
Smart Images

Figure CN222039465U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of injection molds, and in particular to a thin shell sheet part forming mold. Background Art
[0002] Injection mold is a tool for producing plastic products, which can give plastic products a complete structure and precise size. Injection molding is a common processing method for mass production of certain complex-shaped parts. The product is usually made by injecting heated and molten plastic into the mold cavity under high pressure by an injection molding machine, and then cooling and solidifying it.
[0003] Thin plate parts are usually made by injection molding using an injection mold. The injection mold generally includes an upper mold and a lower mold that cooperate with each other. When the upper mold and the lower mold are combined, a cavity for molding thin plate parts is formed. The molten plastic is passed into the cavity for cooling and solidification, thereby producing a thin plate part.
[0004] There is currently a thin sheet product, refer to Figure 1 , which has a large surface area, and has multiple first core pulling positions, second core pulling positions, third core pulling positions, multiple first inner buckle positions, multiple second inner buckle positions, multiple third inner buckle positions and multiple fourth inner buckle positions on its side and inner surface, making its shape irregular. During the injection molding process, the buckle position features on the part will have a certain impact on demolding. Therefore, there is still a lack of a mold structure that can achieve fast and high-quality molding, so there is still room for improvement. Utility Model Content
[0005] In order to enable the injection mold to mold thin-sheet parts quickly and with high quality, the present application provides a thin-shell sheet part molding mold.
[0006] The present application provides a thin shell sheet material part forming die adopting the following technical solution:
[0007] A thin shell sheet part forming mold comprises a fixed mold, a movable mold, an inclined ejector mechanism and a core pulling mechanism, wherein a fixed mold core is installed on the fixed mold, a movable mold core is installed on the movable mold, and the core pulling mechanism is installed between the movable mold core and the fixed mold core. The fixed mold core, the movable mold core, the inclined ejector mechanism and the core pulling mechanism form a cavity for injection molding a thin shell sheet part when the mold is closed, and the core pulling mechanism is demolded and separated from the thin shell sheet part when the mold is opened. An ejector mechanism is provided on the movable mold, and the ejector mechanism is used to eject the molded thin shell sheet part. The inclined ejector mechanism is installed on the ejector mechanism, and the ejector mechanism drives the inclined ejector mechanism to be demolded and separated from the molded thin shell sheet part during the process of ejecting the molded thin shell sheet part.
[0008] By adopting the above technical scheme, the fixed mold core, the movable mold core, the inclined ejector mechanism and the core pulling mechanism form a cavity for injection molding the thin shell sheet part when the mold is closed. After injection molding, the mold is opened to separate the movable mold core from the fixed mold core, the core pulling mechanism is demolded and separated from the thin shell sheet part when the mold is opened, and the ejector mechanism ejects the molded thin shell sheet part. In the process of ejecting the molded thin shell sheet part, the ejector mechanism drives the inclined ejector mechanism to demold and separate from the molded thin shell sheet part, thereby demolding and separating the molded thin shell sheet part from the movable mold core. This process improves the molding and demolding processing efficiency and demolding processing quality of this type of thin shell sheet part.
[0009] Preferably, the fixed mold core is provided with an exhaust groove surrounding the cavity.
[0010] By adopting the above technical solution, the thin shell sheet parts have the problem of difficulty in exhausting during the injection molding process. By providing an exhaust groove, the gas can be discharged, the bubble defects of the thin shell sheet parts can be reduced, and the production quality of the thin shell sheet parts can be improved.
[0011] Preferably, the core pulling mechanism includes a first core pulling assembly, which includes a first guide push rod, a first core pulling sliding block and a first core pulling block. The first guide push rod is fixedly connected to the fixed mold core, the first guide push rod is inclined, the first core pulling sliding block is slidingly connected to the movable mold core, the end of the first guide push rod passes through the first core pulling sliding block, and the end of the first core pulling sliding block is provided with a first avoidance opening, the first core pulling block is fixedly connected to the first core pulling sliding block, and a first injection cavity is formed between the first core pulling sliding block, the first core pulling block and the movable mold core, which is consistent with the first core pulling position shape on the side of the thin shell sheet part and is connected to the mold cavity.
[0012] By adopting the above technical scheme, a first injection cavity which is consistent with the shape of the first core-pulling position on the side of the thin-shell sheet part and is connected to the mold cavity is formed between the first core-pulling sliding block, the first core-pulling block and the movable mold core. The molten plastic is passed into the first injection cavity and cooled and solidified to form the first core-pulling position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core. Since the first core-pulling sliding block is fixedly connected to the movable mold core, the movement of the movable mold core will drive the first core-pulling sliding block to move away from the fixed mold core. In addition, since the first guide push rod passes through the first core-pulling sliding block and The first core-pulling block is arranged in an inclined manner so that the first core-pulling sliding block is subjected to a force in the inclined direction from the first guide push rod, thereby causing the first core-pulling sliding block and the movable mold core to slide horizontally. Since the first core-pulling block is fixedly connected to the first core-pulling sliding block, the first core-pulling block and the first core-pulling sliding block are moved away from the first injection cavity together, thereby realizing the demoulding of the first core-pulling position on the side of the thin-shell sheet part. The demoulding operation is carried out synchronously with the mold opening, and the collision and friction on the first core-pulling position on the side of the thin-shell sheet part during the demoulding process are reduced, thereby improving the molding and demoulding processing efficiency and demoulding processing quality of this type of thin-shell sheet part.
[0013] Preferably, the core pulling mechanism includes a second core pulling assembly, the second core pulling assembly includes a second guide push rod and a second core pulling sliding block, the second guide push rod is fixedly connected to the fixed mold core, the second guide push rod is inclined, the second core pulling sliding block is slidably connected to the movable mold core, the end of the second guide push rod passes through the second core pulling sliding block, the end of the second core pulling sliding block is provided with a second avoidance opening, and a second injection cavity is formed between the second core pulling sliding block and the movable mold core, which is consistent with the second core pulling position shape on the side of the thin shell sheet part and is connected to the mold cavity.
[0014] By adopting the above technical solution, a second injection cavity is formed between the second core-pulling sliding block and the movable mold core, which is consistent with the shape of the second core-pulling position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the second injection cavity and cooled and solidified to form the second core-pulling position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core. Since the second core-pulling sliding block is fixedly connected to the movable mold core, the movement of the movable mold core will drive the second core-pulling sliding block to move away from the fixed mold core. The rod passes through the second core-pulling sliding block and is arranged at an angle, so that the second core-pulling sliding block is subjected to a force in the inclined direction of the second guide push rod, thereby causing the second core-pulling sliding block and the movable mold core to slide horizontally, thereby causing the second core-pulling sliding block to move away from the second injection cavity, thereby realizing the demolding of the second core-pulling position on the side of the thin shell sheet part. The demolding operation is carried out simultaneously with the mold opening and reduces the collision and friction on the second core-pulling position on the side of the thin shell sheet part during the demolding process, thereby improving the molding and demolding processing efficiency and demolding processing quality of this type of thin shell sheet part.
[0015] Preferably, the core pulling mechanism includes a third core pulling assembly, and the third core pulling assembly includes a third guide push rod, a third core pulling sliding block and a third core pulling block. The third guide push rod is fixedly connected to the fixed mold core, and the third guide push rod is inclined. The third core pulling sliding block is slidingly connected to the movable mold core, and the end of the third guide push rod passes through the third core pulling sliding block. The end of the third core pulling sliding block is provided with a third avoidance opening, and the third core pulling block is fixedly connected to the third core pulling sliding block. A third injection cavity is formed between the third core pulling sliding block, the third core pulling block and the movable mold core, which is consistent with the third core pulling position shape on the side of the thin shell sheet part and is connected to the mold cavity.
[0016] By adopting the above technical scheme, a third injection cavity is formed between the third core-pulling sliding block, the third core-pulling block and the movable mold core, which is consistent with the shape of the third core-pulling position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the third injection cavity and cooled and solidified to form the third core-pulling position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core. Since the third core-pulling sliding block is fixedly connected to the movable mold core, the movement of the movable mold core will drive the third core-pulling sliding block to move away from the fixed mold core. In addition, since the third guide push rod passes through the third core-pulling sliding block and The third core-pulling sliding block is arranged in an inclined manner, so that the third core-pulling sliding block is subjected to a force in the inclined direction of the third guide push rod, thereby causing the third core-pulling sliding block and the movable mold core to slide horizontally. Since the third core-pulling block is fixedly connected to the third core-pulling sliding block, the third core-pulling block and the third core-pulling sliding block are moved away from the third injection cavity together, thereby realizing the demoulding of the third core-pulling position on the side of the thin shell sheet part. The demoulding operation is carried out simultaneously with the mold opening, and the collision and friction on the third core-pulling position on the side of the thin shell sheet part during the demoulding process are reduced, thereby improving the molding and demoulding processing efficiency and demoulding processing quality of this type of thin shell sheet part.
[0017] Preferably, the inclined ejector mechanism includes a first inclined ejector assembly, which includes a first fixed seat, a first sliding guide block and a first main inclined ejector block, the first fixed seat is fixed on the ejector mechanism, the first sliding guide block is fixed on the movable mold core, the first main inclined ejector block is slidably set on the first fixed seat, the first main inclined ejector block is inclinedly set, the end of the first main inclined ejector block passes through the first sliding guide block and then passes through the movable mold core, a fourth avoidance opening is provided at the end of the first main inclined ejector block, and a fourth injection cavity is formed between the first main inclined ejector block and the movable mold core, which is consistent with the first inner buckle shape of the side of the thin shell sheet part and is connected to the mold cavity.
[0018] By adopting the above technical scheme, a fourth injection cavity is formed between the first main inclined ejector block and the movable mold core, which has the same shape as the first inner buckle position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the fourth injection cavity and cooled and solidified to form the first inner buckle position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move in the direction away from the fixed mold, so that the movable mold core is separated from the fixed mold core, and the ejector mechanism ejects the thin-shell sheet part. Since the first fixed seat is fixed on the ejector mechanism, the ejector mechanism will drive the first fixed seat to move when ejecting the thin-shell sheet part. Since the first main inclined ejector block is slidably arranged on the first fixed seat, relative sliding can occur between the first main inclined ejector block and the first fixed seat. The block is arranged obliquely, the first sliding guide block is fixed on the movable mold core, the end of the first main inclined ejector block passes through the first sliding guide block and then passes through the movable mold core. When the first fixed seat moves, the first main inclined ejector block is subjected to the force from the first fixed seat and the force from the inclined direction of the first sliding guide block, so that the first main inclined ejector block slides relative to the movable mold core, thereby making the first main inclined ejector block move away from the fourth injection cavity, realizing the demoulding of the first inner buckle position on the side of the thin shell sheet part, and the demoulding operation and the ejector mechanism ejecting the thin shell sheet part are carried out synchronously, and the collision and friction on the first inner buckle position on the side of the thin shell sheet part during the demoulding process are reduced, thereby improving the molding demoulding processing efficiency and demoulding processing quality of this kind of thin shell sheet part.
[0019] Preferably, the inclined ejector mechanism also includes a second inclined ejector assembly, which includes a second fixed seat, a second sliding guide block and a second main inclined ejector block, the second fixed seat is fixed on the ejector mechanism, the second sliding guide block is fixed on the movable mold core, the second main inclined ejector block is slidably set on the second fixed seat, the second main inclined ejector block is inclined, the end of the second main inclined ejector block passes through the second sliding guide block and then passes through the movable mold core, a fifth avoidance opening is provided at the end of the second main inclined ejector block, and a fifth injection cavity is formed between the second main inclined ejector block and the movable mold core, which is consistent with the second inner buckle shape of the side of the thin shell sheet part and is connected to the mold cavity.
[0020] By adopting the above technical scheme, a fifth injection cavity is formed between the second main inclined ejector block and the movable mold core, which has the same shape as the second inner buckle position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the fifth injection cavity and cooled and solidified to form the second inner buckle position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core, and the ejector mechanism ejects the thin-shell sheet part. Since the second fixed seat is fixed on the ejector mechanism, the ejector mechanism will drive the second fixed seat to move when ejecting the thin-shell sheet part. Since the second main inclined ejector block is slidably arranged on the second fixed seat, relative sliding can occur between the second main inclined ejector block and the second fixed seat. The block is arranged obliquely, the second sliding guide block is fixed on the movable mold core, the end of the second main inclined ejector block passes through the second sliding guide block and then passes through the movable mold core, when the second fixed seat moves, the second main inclined ejector block is subjected to the force from the second fixed seat and the force from the inclined direction of the second sliding guide block, so that the second main inclined ejector block slides relative to the movable mold core, thereby making the second main inclined ejector block move away from the fifth injection cavity, realizing the demoulding of the second inner buckle position on the side of the thin shell sheet part, the demoulding operation is carried out synchronously with the operation of ejecting the thin shell sheet part by the ejector mechanism, and the collision and friction on the second inner buckle position on the side of the thin shell sheet part during the demoulding process are reduced, thereby improving the molding demoulding processing efficiency and demoulding processing quality of this kind of thin shell sheet part.
[0021] Preferably, the inclined ejector mechanism also includes a third inclined ejector assembly, and the third inclined ejector assembly includes a third fixed seat, a third sliding guide block and a third main inclined ejector block. The third fixed seat is fixed on the ejector mechanism, and the third sliding guide block is fixed on the movable mold core. The third main inclined ejector block is slidably set on the third fixed seat, and the third main inclined ejector block is inclined. The end of the third main inclined ejector block passes through the third sliding guide block and then passes through the movable mold core. A sixth avoidance opening is provided at the end of the third main inclined ejector block, and a sixth injection cavity is formed between the third main inclined ejector block and the movable mold core, which is consistent with the third inner buckle shape of the side of the thin shell sheet part and is connected to the mold cavity.
[0022] By adopting the above technical scheme, a sixth injection cavity is formed between the third main inclined ejector block and the movable mold core, which has the same shape as the third inner buckle position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the sixth injection cavity and cooled and solidified to form the third inner buckle position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core, and the ejector mechanism ejects the thin-shell sheet part. Since the third fixed seat is fixed on the ejector mechanism, the ejector mechanism will drive the third fixed seat to move when ejecting the thin-shell sheet part. Since the third main inclined ejector block is slidably arranged on the third fixed seat, relative sliding can occur between the third main inclined ejector block and the third fixed seat. The block is inclined, the third sliding guide block is fixed on the movable mold core, the end of the third main inclined ejector block passes through the third sliding guide block and then passes through the movable mold core. When the third fixed seat moves, the third main inclined ejector block is subjected to the force from the third fixed seat and the force from the inclined direction of the third sliding guide block, so that the third main inclined ejector block slides relative to the movable mold core, thereby making the third main inclined ejector block move away from the sixth injection cavity, thereby realizing the demoulding of the third inner buckle position on the side of the thin shell sheet part, and the demoulding operation is synchronously performed with the ejector mechanism to eject the thin shell sheet part, and the collision and friction on the third inner buckle position on the side of the thin shell sheet part during the demoulding process are reduced, thereby improving the molding demoulding processing efficiency and demoulding processing quality of this type of thin shell sheet part.
[0023] Preferably, the inclined ejector mechanism also includes a fourth inclined ejector assembly, the fourth inclined ejector assembly includes a fourth fixed seat, a fourth sliding guide block and a fourth main inclined ejector block, the fourth fixed seat is fixed on the ejector mechanism, the fourth sliding guide block is fixed on the movable mold core, the fourth main inclined ejector block is slidably set on the fourth fixed seat, the fourth main inclined ejector block is inclinedly set, the end of the fourth main inclined ejector block passes through the fourth sliding guide block and then passes through the movable mold core, the end of the fourth main inclined ejector block is provided with a seventh avoidance opening, and a seventh injection cavity is formed between the fourth main inclined ejector block and the movable mold core, which is consistent with the fourth inner buckle shape of the side of the thin shell sheet part and is connected to the mold cavity.
[0024] By adopting the above technical scheme, a seventh injection cavity is formed between the fourth main inclined ejector block and the movable mold core, which has the same shape as the fourth inner buckle position on the side of the thin-shell sheet part and is connected to the mold cavity. The molten plastic is passed into the seventh injection cavity and cooled and solidified to form the fourth inner buckle position of the thin-shell sheet part. After the molding is completed, the movable mold is started to move away from the fixed mold, so that the movable mold core is separated from the fixed mold core, and the ejector mechanism ejects the thin-shell sheet part. Since the fourth fixed seat is fixed on the ejector mechanism, the ejector mechanism will drive the fourth fixed seat to move when ejecting the thin-shell sheet part. Since the fourth main inclined ejector block is slidably arranged on the fourth fixed seat, relative sliding can occur between the fourth main inclined ejector block and the fourth fixed seat. The block is inclined, the fourth sliding guide block is fixed on the movable mold core, the end of the fourth main inclined ejector block passes through the fourth sliding guide block and then passes through the movable mold core. When the fourth fixed seat moves, the fourth main inclined ejector block is subjected to the force from the fourth fixed seat and the force from the inclined direction of the fourth sliding guide block, so that the fourth main inclined ejector block slides relative to the movable mold core, thereby making the fourth main inclined ejector block move away from the seventh injection cavity, thereby realizing the demoulding of the fourth inner buckle position on the side of the thin shell sheet part, and the demoulding operation and the ejector mechanism ejecting the thin shell sheet part are carried out simultaneously, and the collision and friction on the fourth inner buckle position on the side of the thin shell sheet part during the demoulding process are reduced, thereby improving the molding demoulding processing efficiency and demoulding processing quality of this type of thin shell sheet part.
[0025] In summary, the present application includes at least one of the following beneficial technical effects: the fixed mold core, the movable mold core, the inclined ejector mechanism and the core pulling mechanism form a cavity for injection molding a thin shell sheet part when the mold is closed; after injection molding, the mold is opened to separate the movable mold core from the fixed mold core; the core pulling mechanism is demolded and separated from the thin shell sheet part when the mold is opened; the ejector mechanism ejects the molded thin shell sheet part; and the ejector mechanism drives the inclined ejector mechanism to demold and separate from the molded thin shell sheet part during the process of ejecting the molded thin shell sheet part, thereby demolding the molded thin shell sheet part from the movable mold core; this process improves the molding and demolding processing efficiency and demolding processing quality of this type of thin shell sheet part. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the overall structure of the thin shell sheet part of the embodiment of the present application.
[0027] Figure 2 It is a schematic diagram of the overall structure of the mold of an embodiment of the present application.
[0028] Figure 3 It is a schematic diagram of the assembly relationship of the mold in the embodiment of the present application.
[0029] Figure 4 It is a schematic diagram of the assembly relationship between the fixed mold and the movable mold in the embodiment of the present application.
[0030] Figure 5It is a structural schematic diagram of the core pulling mechanism of an embodiment of the present application.
[0031] Figure 6 It is a schematic diagram of the matching relationship between the movable mold core, the inclined ejector mechanism and the movable mold bottom plate in the embodiment of the present application.
[0032] Figure 7 It is a schematic diagram of the matching relationship between the inclined ejector mechanism and the movable mold bottom plate of the embodiment of the present application.
[0033] Figure 8 yes Figure 7 A partial enlarged schematic diagram of part A in FIG.
[0034] Fig. 9 yes Figure 7 A partial enlarged schematic diagram of part B in FIG.
[0035] Fig.10 It is a schematic diagram of the coordination relationship between the movable mold core, the inclined ejector mechanism and the movable mold bottom plate in the embodiment of the present application from another perspective.
[0036] Fig.11 It is a structural schematic diagram of the fixed mold core in the embodiment of the present application.
[0037] Description of reference numerals: 1, main board; 2, first core-pulling position; 3, second core-pulling position; 4, third core-pulling position; 5, first inner buckle position; 6, second inner buckle position; 7, third inner buckle position; 8, fourth inner buckle position; 9, fixed mold; 10, movable mold; 101, movable mold bottom plate; 102, movable mold frame; 11, inclined ejector mechanism; 111, first inclined ejector assembly; 1111, first fixed seat; 1112, first sliding guide block; 1113, The first main inclined top block; 112, the second inclined top assembly; 1121, the second fixed seat; 1122, the second sliding guide block; 1123, the second main inclined top block; 113, the third inclined top assembly; 1131, the third fixed seat; 1132, the third sliding guide block; 1133, the third main inclined top block; 114, the fourth inclined top assembly; 1141, the fourth fixed seat; 1142, the fourth sliding guide block; 1143, the fourth main Lift block; 12, core pulling mechanism; 121, first core pulling assembly; 1211, first guide push rod; 1212, first core pulling sliding block; 1213, first core pulling block; 122, second core pulling assembly; 1221, second guide push rod; 1222, second core pulling sliding block; 123, third core pulling assembly; 1231, third guide push rod; 1232, third core pulling sliding block; 1233, third core pulling block; 13 , fixed mold core; 14, movable mold core; 15, accommodating groove; 16, ejector mechanism; 161, ejector plate; 162, ejector; 17, first limit block; 18, protrusion; 19, first avoidance opening; 20, second limit block; 21, second avoidance opening; 22, third limit block; 23, third avoidance opening; 24, fourth avoidance opening; 25, fifth avoidance opening; 26, sixth avoidance opening; 27, seventh avoidance opening; 28, exhaust groove. DETAILED DESCRIPTION
[0038] The following is combined with Figure 1-4 This application is described in further detail.
[0039] The embodiment of the present application discloses a thin shell sheet part forming mold, which is used for injection molding a thin shell sheet part. Figure 1 A thin shell sheet material part includes a main board 1, on which a plurality of first core pulling positions 2, a second core pulling position 3, a third core pulling position 4, a plurality of first inner buckle positions 5, a plurality of second inner buckle positions 6, a plurality of third inner buckle positions 7 and a plurality of fourth inner buckle positions 8 are arranged, and the shapes of the first core pulling position 2, the second core pulling position 3, the third core pulling position 4, the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 all have their own specific shapes. The plurality of first core pulling positions 2, the second core pulling position 3, the third core pulling position 4, the plurality of first inner buckle positions 5, the plurality of second inner buckle positions 6, the plurality of third inner buckle positions 7 and the plurality of fourth inner buckle positions 8 are all integrally formed with the bottom of the main board 1 and are irregularly distributed, so that the shape of the thin shell sheet material part is irregular. Therefore, during the injection molding process, the buckle position characteristics on the part will have a certain influence on demolding.
[0040] Reference Figure 2 and Figure 3 A thin-shell sheet part forming mold comprises a fixed mold 9, a movable mold 10, a tilting mechanism 11 and a core pulling mechanism 12. The fixed mold 9 is provided with a fixed mold core 13, and the movable mold 10 is provided with a movable mold core 14. In order to adapt to the shape processing requirements of the workpiece, combined with Figure 5 and Figure 7 The core pulling mechanism 12 includes a first core pulling assembly 121, a second core pulling assembly 122 and a third core pulling assembly 123, which are installed between the movable mold core 14 and the fixed mold core 13, and the inclined ejection mechanism 11 includes a first inclined ejection assembly 111, a second inclined ejection assembly 112, a third inclined ejection assembly 113 and a fourth inclined ejection assembly 114. The fixed mold core 13, the movable mold core 14, the first inclined ejection assembly 111, the second inclined ejection assembly 112, the third inclined ejection assembly 113, the fourth inclined ejection assembly 114, the first core pulling assembly 121, the second core pulling assembly 122 and the third core pulling assembly 123 form a cavity for injection molding thin shell sheet parts when the mold is closed.
[0041] The first core pulling assembly 121, the second core pulling assembly 122 and the third core pulling assembly 123 are demolded and separated from the thin shell sheet part when the mold is opened. The movable mold 10 includes a movable mold core bottom plate 101 and a movable mold frame 102. The movable mold frame 102 is provided with a receiving groove 15, and the movable mold core 14 is received in the receiving groove 15. The movable mold core bottom plate 101 is provided with an ejector mechanism 16. Specifically, the ejector mechanism 16 includes an ejector plate 161 and a plurality of ejector pins 162. The ejector plate 161 is slidably connected to the movable mold core bottom plate 101. The ejector pins 162 are vertically fixed on the ejector plate 161. A plurality of ejector pin holes are correspondingly provided on the movable mold core 14. The ends of the ejector pins 162 are received in the ejector pin holes. The ejector pins 162 are used to eject the formed thin shell sheet part. The first inclined ejector assembly 111, the second inclined ejector assembly 112, the third inclined ejector assembly 113 and the fourth inclined ejector assembly 114 are all installed on the ejector plate 161. The ejector plate 161 drives the ejector 162 to eject the formed thin shell sheet part, thereby driving the first inclined ejector assembly 111, the second inclined ejector assembly 112, the third inclined ejector assembly 113 and the fourth inclined ejector assembly 114 to be demolded and separated from the formed thin shell sheet part.
[0042] The fixed mold core 13, the movable mold core 14, the first inclined ejector assembly 111, the second inclined ejector assembly 112, the third inclined ejector assembly 113, the fourth inclined ejector assembly 114, the first core pulling assembly 121, the second core pulling assembly 122 and the third core pulling assembly 123 form a cavity for injection molding the thin shell sheet part when the mold is closed. After injection molding, the mold is opened to separate the movable mold core 14 from the fixed mold core 13, and the first core pulling assembly 121, the second core pulling assembly 122 and the third core pulling assembly 123 are demolded and separated from the thin shell sheet part when the mold is opened. The ejector pin 162 ejects the formed thin shell sheet part. In the process of driving the ejector pin 162 to eject the formed thin shell sheet part, the ejector plate 161 drives the inclined ejector mechanism 11 to demold and separate the formed thin shell sheet part, thereby demolding and separating the formed thin shell sheet part from the movable mold core 14. This process improves the molding and demolding processing efficiency and demolding processing quality of this type of thin shell sheet part.
[0043] In this embodiment, refer to Figure 4 and Figure 5 The first core pulling assembly 121 is provided with three groups, and the first core pulling assembly 121 includes a first guide push rod 1211, a first core pulling sliding block 1212 and a first core pulling block 1213. The first core pulling sliding block 1212 and the first core pulling block 1213 are arranged horizontally, and the first guide push rod 1211 is fixedly connected to the fixed mold core 13. The three first guide push rods 1211 are arranged in parallel and side by side, and the first guide push rod 1211 is inclined from the inner side of the fixed mold core 13 to the outer side of the fixed mold core 13. The movable mold core 14 is fixed with a first limit block 17, and there are three groups of the first limit blocks 17. Each group of the first limit blocks 17 includes two first limit blocks 17, and the two first limit blocks 17 are arranged horizontally opposite to each other. The first limit blocks 17 are arranged in an inverted L shape. The first core-pulling sliding block 1212 is provided with protrusions 18 on both sides, and the protrusions 18 extend to both sides of the first core-pulling sliding block 1212, so that the first core-pulling sliding block 1212 is arranged in a T shape. The side wall of the protrusion 18 abuts against the side wall of the first limit block 17, and the top of the protrusion 18 abuts against the bottom of the first limit block 17. The first core-pulling sliding block 1212 is slidably arranged between the two first limit blocks 17, and the three first core-pulling sliding blocks 1212 are arranged in parallel, and the upper surface of the first core-pulling sliding block 1212 is flush with the upper surface of the first limit block 17. The end of the first guide push rod 1211 passes through the first core-pulling sliding block 1212, and the end of the first core-pulling sliding block 1212 is provided with a first avoidance opening 19. The first core-pulling block 1213 is fixedly connected to the first core-pulling sliding block 1212, and the first core-pulling block 1213 is located below the first avoidance opening 19. A first injection cavity that is consistent with the shape of the first core-pulling position 2 on the side of the thin shell sheet part and is connected to the mold cavity is formed between the first core-pulling sliding block 1212, the first core-pulling block 1213 and the movable mold core 14.
[0044] Specifically, the second core pulling assembly 122 includes a second guide push rod 1221 and a second core pulling sliding block 1222. The second guide push rod 1221 is fixedly connected to the fixed mold core 13. The second guide push rod 1221 is fixed to the side of the fixed mold core 13 adjacent to the side where the first guide push rod 1211 is fixed. The second guide push rod 1221 is tilted from the inside of the fixed mold core 13 toward the outside of the fixed mold core 13. The movable mold core 14 is provided with a second limit block 20. Two second limit blocks 20 are provided. The two second limit blocks 20 are horizontally arranged opposite to each other. The second core pulling sliding block 1222 is horizontally arranged. The two sides of the second core pulling sliding block 1222 are respectively slidably connected to the two second limit blocks 20. The end of the second guide push rod 1221 passes through the second core pulling sliding block 1222. A second avoidance opening 21 is provided at the end of the second core-pulling sliding block 1222 , and a second injection cavity which is consistent in shape with the second core-pulling position 3 on the side of the thin shell sheet part and connected to the mold cavity is formed between the second core-pulling sliding block 1222 and the movable mold core 14 .
[0045] Further, the third core pulling assembly 123 includes a third guide push rod 1231, a third core pulling sliding block 1232 and a third core pulling block 1233. The third guide push rod 1231 is fixedly connected to the fixed mold core 13. The third guide push rod 1231 is arranged parallel to one side of the second guide push rod 1221. The third core pulling sliding block 1232 and the third core pulling block 1233 are arranged horizontally. The movable mold core 14 is provided with a third limit block 22. There are two third limit blocks 22. The two third limit blocks 22 are arranged horizontally facing each other. The two sides of the third core pulling sliding block 1232 are respectively slidably connected with the two third limit blocks 22. The end of the third guide push rod 1231 passes through the third core pulling sliding block 1232. The end of the third core pulling sliding block 1232 is provided with a third avoidance opening 23. The third core pulling block 1233 is fixedly connected to the third core pulling sliding block 1232, and the third core pulling block 1233 is located below the third core pulling sliding block 1232. A third injection cavity is formed between the third core pulling sliding block 1232, the third core pulling block 1233 and the movable mold core 14, which is consistent with the shape of the third core pulling position 4 on the side of the thin shell sheet part and is connected to the mold cavity.
[0046] Correspondingly, the molten plastic is passed into the first injection cavity to cool and solidify to form the first core-pulling position 2 of the thin-shell sheet part, the molten plastic is passed into the second injection cavity to cool and solidify to form the second core-pulling position 3 of the thin-shell sheet part, and the molten plastic is passed into the third injection cavity to cool and solidify to form the third core-pulling position 4 of the thin-shell sheet part. After the molding is completed, the movable mold 10 is started to move away from the fixed mold 9, so that the movable mold core 14 is separated from the fixed mold core 13. Since the first core-pulling sliding block 1212, the second core-pulling sliding block 1222 and the third core-pulling sliding block 1232 are all horizontally slidably arranged on the movable mold core 14, when the movable mold core 14 moves vertically in the direction away from the fixed mold core 13, it will drive the first core-pulling sliding block 1212, the second core-pulling sliding block 1222 and the third core-pulling sliding block 1232 to move away from the fixed mold core 13 together.
[0047] Since the first guide push rod 1211 passes through the first core-pulling sliding block 1212 and is inclined, the second guide push rod 1221 passes through the second core-pulling sliding block 1222 and is inclined, and the third guide push rod 1231 passes through the third core-pulling sliding block 1232 and is inclined, the first core-pulling sliding block 1212 is subjected to a force from the first guide push rod 1211 in the inclined direction, the second core-pulling sliding block 1222 is subjected to a force from the second guide push rod 1221 in the inclined direction, and the third core-pulling sliding block 1232 is subjected to a force from the third guide push rod 1231 in the inclined direction, thereby causing the first core-pulling sliding block 1212 and the movable mold core 14 to slide horizontally, the second core-pulling sliding block 1222 and the movable mold core 14 to slide horizontally, and the third core-pulling sliding block 1232 and the movable mold core 14 to slide horizontally. Since the first core pulling block 1213 is fixedly connected to the first core pulling sliding block 1212, and the third core pulling block 1233 is fixedly connected to the third core pulling sliding block 1232, the first core pulling block 1213 and the first core pulling sliding block 1212 are together away from the first injection cavity, the second core pulling sliding block 1222 is away from the second injection cavity, and the third core pulling block 1233 and the third core pulling sliding block 1232 are together away from the third injection cavity, thereby realizing the demolding of the first core pulling position 2, the second core pulling position 3 and the third core pulling position 4 on the side of the thin shell sheet part, and the demolding operation is carried out simultaneously with the mold opening, and the collision and friction on the first core pulling position 2, the second core pulling position 3 and the third core pulling position 4 on the side of the thin shell sheet part during the demolding process are reduced, thereby improving the molding demolding processing efficiency and demolding processing quality of this type of thin shell sheet part.
[0048] Further, see Figure 6 and Figure 7The first inclined ejector assembly 111 includes a first fixed seat 1111, a first sliding guide block 1112 and a first main inclined ejector block 1113. The second inclined ejector assembly 112 includes a second fixed seat 1121, a second sliding guide block 1122 and a second main inclined ejector block 1123. The third inclined ejector assembly 113 includes a third fixed seat 1131, a third sliding guide block 1132 and a third main inclined ejector block 1133. The fourth inclined ejector assembly 114 includes a fourth fixed seat 1141, a fourth sliding guide block 1142 and a fourth main inclined ejector block 1143. The first fixed seat 1111, the second fixed seat 1121, the third fixed seat 1131 and the fourth fixed seat 1141 are all fixed on the ejector plate 161, and the first sliding guide block 1112, the second sliding guide block 1122, the third sliding guide block 1132 and the fourth sliding guide block 1142 are all fixed on the movable mold core 14. The first main inclined lift block 1113 is slidably disposed on the first fixed seat 1111 , the second main inclined lift block 1123 is slidably disposed on the second fixed seat 1121 , the third main inclined lift block 1133 is slidably disposed on the third fixed seat 1131 , and the fourth main inclined lift block 1143 is slidably disposed on the fourth fixed seat 1141 . The first main inclined lift block 1113, the second main inclined lift block 1123, the third main inclined lift block 1133 and the fourth main inclined lift block 1143 are all arranged at an incline. The end of the first main inclined lift block 1113 passes through the first sliding guide block 1112 and then passes through the movable mold core 14, the end of the second main inclined lift block 1123 passes through the second sliding guide block 1122 and then passes through the movable mold core 14, the end of the third main inclined lift block 1133 passes through the third sliding guide block 1132 and then passes through the movable mold core 14, and the end of the fourth main inclined lift block 1143 passes through the fourth sliding guide block 1142 and then passes through the movable mold core 14.
[0049] Combination Figure 8 , Fig. 9 and Fig.10There are four first main inclined ejector blocks 1113, which are arranged in a straight line and parallel to each other. The first main inclined ejector block 1113 and the first core-pulling block 1213 are located on the same side of the movable mold core 14. The end of the first main inclined ejector block 1113 is provided with a fourth avoidance opening 24. A fourth injection cavity is formed between the first main inclined ejector block 1113 and the movable mold core 14, which is consistent with the first inner buckle position 5 on the side of the thin shell sheet part and connected to the mold cavity. There are four second main inclined ejector blocks 1123, which are arranged in a straight line. The ends of the four second main inclined ejector blocks 1123 are located near the middle of the movable mold core 14. The arrangement direction of the four second main inclined ejector blocks 1123 is perpendicular to the arrangement direction of the four first main inclined ejector blocks 1113. The first main inclined lift block 1113 is arranged in the same direction as the third main inclined lift block 1133, the second main inclined lift block 1123 is arranged in the same direction as the fourth main inclined lift block 1143, and the first main inclined lift block 1113 is arranged opposite to the second main inclined lift block 1123. A fifth avoidance opening 25 is arranged at the end of the second main inclined lift block 1123, and a fifth injection cavity is formed between the second main inclined lift block 1123 and the movable mold core 14, which is consistent with the second inner buckle position 6 on the side of the thin shell sheet part and is connected to the mold cavity.
[0050] There are three third main inclined ejector blocks 1133, which are arranged in parallel in a straight line, and the ends of the three third main inclined ejector blocks 1133 are located near the outer side of the movable mold core 14. The arrangement direction of the three third main inclined ejector blocks 1133 is perpendicular to the arrangement direction of the four first main inclined ejector blocks 1113, and the ends of the third main inclined ejector blocks 1133 are provided with a sixth avoidance opening 26. A sixth injection cavity is formed between the third main inclined ejector block 1133 and the movable mold core 14, which is consistent with the shape of the third inner buckle position 7 on the side of the thin shell sheet part and is connected to the mold cavity. There are three fourth main inclined ejector blocks 1143, which are arranged in parallel in a straight line, and the ends of the three fourth main inclined ejector blocks 1143 are located on the other side of the movable mold core 14 relative to the four first main inclined ejector blocks 1113. The arrangement direction of the three fourth main inclined ejector blocks 1143 is parallel to the arrangement direction of the four first main inclined ejector blocks 1113, and the ends of the fourth main inclined ejector blocks 1143 are provided with a seventh avoidance opening 27. A seventh injection cavity is formed between the fourth main inclined ejector block 1143 and the movable mold core 14, which is consistent with the shape of the fourth inner buckle position 8 on the side of the thin shell sheet part and is connected to the mold cavity.
[0051] The molten plastic is passed into the fourth injection cavity, the fifth injection cavity, the sixth injection cavity and the seventh injection cavity, and then cooled and solidified to form the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 of the thin shell sheet part. After the molding is completed, the movable mold 10 is started to move away from the fixed mold 9, so that the movable mold core 14 is separated from the fixed mold core 13, and the ejector plate 161 drives the ejector 162 to eject the thin shell sheet part again. Since the first fixed seat 1111, the second fixed seat 1121, the third fixed seat 1131 and the fourth fixed seat 1141 are all fixed on the ejector plate 161, the ejector 162 will drive the first fixed seat 1111, the second fixed seat 1121, the third fixed seat 1131 and the fourth fixed seat 1141 to move when ejecting the thin shell sheet part. Since the first main inclined lift block 1113 is slidably set on the first fixed seat 1111, the second main inclined lift block 1123 is slidably set on the second fixed seat 1121, the third main inclined lift block 1133 is slidably set on the third fixed seat 1131, and the fourth main inclined lift block 1143 is slidably set on the fourth fixed seat 1141, relative sliding can occur between the first main inclined lift block 1113 and the first fixed seat 1111, relative sliding can occur between the second main inclined lift block 1123 and the second fixed seat 1121, relative sliding can occur between the third main inclined lift block 1133 and the third fixed seat 1131, and relative sliding can occur between the fourth main inclined lift block 1143 and the fourth fixed seat 1141.
[0052] Since the first main inclined lift block 1113, the second main inclined lift block 1123, the third main inclined lift block 1133 and the fourth main inclined lift block 1143 are all arranged at an angle, the first sliding guide block 1112, the second sliding guide block 1122, the third sliding guide block 1132 and the fourth sliding guide block 1142 are all fixed on the movable mold core 14, the end of the first main inclined lift block 1113 penetrates the first sliding guide block 1112 and then penetrates the movable mold core 14, the end of the second main inclined lift block 1123 penetrates the second sliding guide block 1122 and then penetrates the movable mold core 14, the end of the third main inclined lift block 1133 penetrates the third sliding guide block 1132 and then penetrates the movable mold core 14, and the end of the fourth main inclined lift block 1143 penetrates the fourth sliding guide block 1142 and then penetrates the movable mold core 14. When the first fixed seat 1111 moves, the first main inclined lift block 1113 is subjected to the force from the first fixed seat 1111 and the force in the tilting direction from the first sliding guide block 1112; when the second fixed seat 1121 moves, the second main inclined lift block 1123 is subjected to the force from the second fixed seat 1121 and the force in the tilting direction from the second sliding guide block 1122; when the third fixed seat 1131 moves, the third main inclined lift block 1133 is subjected to the force from the third fixed seat 1131 and the force in the tilting direction from the third sliding guide block 1132; when the fourth fixed seat 1141 moves, the fourth main inclined lift block 1143 is subjected to the force from the fourth fixed seat 1141 and the force in the tilting direction from the fourth sliding guide block 1142. The first main inclined ejector block 1113, the second main inclined ejector block 1123, the third main inclined ejector block 1133 and the fourth main inclined ejector block 1143 are caused to slide relative to the movable mold core 14, so that the first main inclined ejector block 1113 is away from the fourth injection cavity, the second main inclined ejector block 1123 is away from the fifth injection cavity, the third main inclined ejector block 1133 is away from the sixth injection cavity, and the fourth main inclined ejector block 1143 is away from the seventh injection cavity, so as to realize the demoulding of the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 on the side of the thin shell sheet part. The demoulding operation is performed synchronously with the operation of ejecting the thin shell sheet part by the ejector pin 162, and the collision and friction of the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 on the side of the thin shell sheet part are reduced during the demoulding process, thereby improving the molding demoulding processing efficiency and demoulding processing quality of the thin shell sheet part.
[0053] On the other hand, thin-shell sheet parts have difficulty in exhausting during the injection molding process. In order to reduce the bubble defects of thin-shell sheet parts and improve the production quality of thin-shell sheet parts, refer to Fig.11 The fixed mold core 13 is provided with an exhaust groove 28 surrounding the cavity. The exhaust groove 28 can discharge gas, thereby reducing bubble defects of thin shell sheet parts and improving the production quality of thin shell sheet parts.
[0054] The implementation principle of a thin shell sheet part forming mold in the embodiment of the present application is:
[0055] When the mold is closed, the molten plastic is injected into the mold cavity, and the plastic is cooled and solidified. After injection molding, the mold is opened to separate the movable mold core 14 from the fixed mold core 13, the first core-pulling sliding block 1212 and the movable mold core 14 slide horizontally, the second core-pulling sliding block 1222 and the movable mold core 14 slide horizontally, and the third core-pulling sliding block 1232 and the movable mold core 14 slide horizontally. The first core-pulling block 1213 and the first core-pulling sliding block 1212 move away from the first injection cavity together, the second core-pulling sliding block 1222 moves away from the second injection cavity, and the third core-pulling block 1233 and the third core-pulling sliding block 1232 move away from the third injection cavity together, thereby realizing the demolding of the first core-pulling position 2, the second core-pulling position 3 and the third core-pulling position 4 on the side of the thin shell sheet part.
[0056] The ejector pin 162 ejects the formed thin shell sheet part, and at the same time, the first main inclined ejector block 1113, the second main inclined ejector block 1123, the third main inclined ejector block 1133 and the fourth main inclined ejector block 1143 slide relative to the movable mold core 14, the first main inclined ejector block 1113 is away from the fourth injection cavity, the second main inclined ejector block 1123 is away from the fifth injection cavity, the third main inclined ejector block 1133 is away from the sixth injection cavity, and the fourth main inclined ejector block 1143 is away from the seventh injection cavity, thereby realizing the demoulding of the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 on the side of the thin shell sheet part. At this point, the thin shell sheet part is completely demoulded.
[0057] The demolding operation is performed simultaneously with the mold opening, and the collision and friction on the first core pulling position 2, the second core pulling position 3 and the third core pulling position 4 on the side of the thin shell sheet part during the demolding process are reduced. The demolding operation is performed simultaneously with the operation of ejecting the thin shell sheet part by the ejector pin 162, and the collision and friction on the first inner buckle position 5, the second inner buckle position 6, the third inner buckle position 7 and the fourth inner buckle position 8 on the side of the thin shell sheet part during the demolding process are reduced, thereby improving the molding demolding processing efficiency and demolding processing quality of this type of thin shell sheet part.
[0058] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A thin shell sheet part forming mold, characterized in that: The invention comprises a fixed mold (9), a movable mold (10), a tilting mechanism (11) and a core pulling mechanism (12); the fixed mold (9) is provided with a fixed mold core (13); the movable mold (10) is provided with a movable mold core (14); the core pulling mechanism (12) is installed between the movable mold core (14) and the fixed mold core (13); the fixed mold core (13), the movable mold core (14), the tilting mechanism (11) and the core pulling mechanism (12) form a core for injection molding thin films when the molds are closed. The core pulling mechanism (12) is demoulded and separated from the thin shell sheet part when the mold is opened, and the movable mold (10) is provided with an ejector mechanism (16), which is used to eject the molded thin shell sheet part, and the inclined ejector mechanism (11) is installed on the ejector mechanism (16), and the ejector mechanism (16) drives the inclined ejector mechanism (11) to be demoulded and separated from the molded thin shell sheet part during the process of ejecting the molded thin shell sheet part.
2. A thin shell sheet part forming mold according to claim 1, characterized in that: The fixed mold core is provided with an exhaust groove (28) surrounding the mold cavity.
3. A thin shell sheet part forming mold according to claim 1, characterized in that: The core pulling mechanism (12) comprises a first core pulling assembly (121), the first core pulling assembly (121) comprises a first guide push rod (1211), a first core pulling sliding block (1212) and a first core pulling block (1213), the first guide push rod (1211) is fixedly connected to the fixed mold core (13), the first guide push rod (1211) is inclined, the first core pulling sliding block (1212) is slidably connected to the movable mold core (14), and the first guide push rod (1211) is fixedly connected to the fixed mold core (13). The end of the first core-pulling sliding block (11) passes through the first core-pulling sliding block (1212), the end of the first core-pulling sliding block (1212) is provided with a first avoidance opening (19), the first core-pulling sliding block (1213) is fixedly connected to the first core-pulling sliding block (1212), and a first injection cavity is formed between the first core-pulling sliding block (1212), the first core-pulling block (1213) and the movable mold core (14), which is consistent with the shape of the first core-pulling position (2) on the side of the thin shell sheet part and is connected to the mold cavity.
4. A thin shell sheet part forming mold according to claim 1, characterized in that: The core pulling mechanism (12) includes a second core pulling assembly (122), and the second core pulling assembly (122) includes a second guide push rod (1221) and a second core pulling sliding block (1222), the second guide push rod (1221) is fixedly connected to the fixed mold core (13), the second guide push rod (1221) is inclined, the second core pulling sliding block (1222) is slidingly connected to the movable mold core (14), the end of the second guide push rod (1221) passes through the second core pulling sliding block (1222), and the end of the second core pulling sliding block (1222) is provided with a second avoidance opening (21), and a second injection cavity is formed between the second core pulling sliding block (1222) and the movable mold core (14), which is consistent with the shape of the second core pulling position (3) on the side of the thin shell sheet part and is connected to the mold cavity.
5. The thin shell sheet parts forming mold according to claim 1, characterized in that: The core pulling mechanism (12) includes a third core pulling assembly (123), and the third core pulling assembly (123) includes a third guide push rod (1231), a third core pulling sliding block (1232) and a third core pulling block (1233). The third guide push rod (1231) is fixedly connected to the fixed mold core (13), and the third guide push rod (1231) is inclined. The third core pulling sliding block (1232) is slidably connected to the movable mold core (14). The end of the third core-pulling sliding block (1232) passes through the third core-pulling sliding block (1232), and the end of the third core-pulling sliding block (1232) is provided with a third avoidance opening (23). The third core-pulling sliding block (1233) is fixedly connected to the third core-pulling sliding block (1232), and a third injection cavity is formed between the third core-pulling sliding block (1232), the third core-pulling block (1233) and the movable mold core (14), which is consistent with the shape of the third core-pulling position (4) on the side of the thin shell sheet part and is connected to the mold cavity.
6. A thin shell sheet part forming mold according to claim 1, characterized in that: The inclined ejection mechanism (11) comprises a first inclined ejection assembly (111), the first inclined ejection assembly (111) comprising a first fixed seat (1111), a first sliding guide block (1112) and a first main inclined ejection block (1113), the first fixed seat (1111) being fixed on the ejector mechanism (16), the first sliding guide block (1112) being fixed on the movable mold core (14), and the first main inclined ejection block (1113) being slidably disposed on the first fixed seat (1111). 1), the first main inclined ejector block (1113) is arranged at an angle, the end of the first main inclined ejector block (1113) passes through the first sliding guide block (1112) and then passes through the movable mold core (14), the end of the first main inclined ejector block (1113) is provided with a fourth avoidance opening (24), and a fourth injection cavity is formed between the first main inclined ejector block (1113) and the movable mold core (14), which is consistent with the shape of the first inner buckle position (5) on the side of the thin shell sheet part and is connected to the mold cavity.
7. A thin shell sheet part forming mold according to claim 1, characterized in that: The inclined ejector mechanism (11) further comprises a second inclined ejector assembly (112), the second inclined ejector assembly (112) comprising a second fixed seat (1121), a second sliding guide block (1122) and a second main inclined ejector block (1123), the second fixed seat (1121) being fixed on the ejector mechanism (16), the second sliding guide block (1122) being fixed on the movable mold core (14), and the second main inclined ejector block (1123) being slidably disposed on the second fixed seat (1121). 1), the second main inclined ejector block (1123) is arranged at an angle, the end of the second main inclined ejector block (1123) passes through the second sliding guide block (1122) and then passes through the movable mold core (14), the end of the second main inclined ejector block (1123) is provided with a fifth avoidance opening (25), and a fifth injection cavity is formed between the second main inclined ejector block (1123) and the movable mold core (14), which is consistent with the shape of the second inner buckle position (6) on the side of the thin shell sheet part and is connected to the mold cavity.
8. The thin shell sheet parts forming mold according to claim 1, characterized in that: The inclined ejection mechanism (11) further comprises a third inclined ejection assembly (113), wherein the third inclined ejection assembly (113) comprises a third fixed seat (1131), a third sliding guide block (1132) and a third main inclined ejection block (1133), wherein the third fixed seat (1131) is fixed on the ejector mechanism (16), the third sliding guide block (1132) is fixed on the movable mold core (14), and the third main inclined ejection block (1133) is slidably disposed on the third fixed seat (1131). 1), the third main inclined ejector block (1133) is arranged at an angle, the end of the third main inclined ejector block (1133) passes through the third sliding guide block (1132) and then passes through the movable mold core (14), the end of the third main inclined ejector block (1133) is provided with a sixth avoidance opening (26), and a sixth injection cavity is formed between the third main inclined ejector block (1133) and the movable mold core (14), which is consistent with the shape of the third inner buckle position (7) on the side of the thin shell sheet part and is connected to the mold cavity.
9. A thin shell sheet part forming mold according to claim 1, characterized in that: The inclined ejector mechanism (11) further comprises a fourth inclined ejector assembly (114), wherein the fourth inclined ejector assembly (114) comprises a fourth fixed seat (1141), a fourth sliding guide block (1142) and a fourth main inclined ejector block (1143), wherein the fourth fixed seat (1141) is fixed to the ejector mechanism (16), the fourth sliding guide block (1142) is fixed to the movable mold core (14), and the fourth main inclined ejector block (1143) is slidably disposed on the fourth fixed seat (1141). 1), the fourth main inclined ejector block (1143) is arranged at an angle, the end of the fourth main inclined ejector block (1143) passes through the fourth sliding guide block (1142) and then passes through the movable mold core (14), the end of the fourth main inclined ejector block (1143) is provided with a seventh avoidance opening (27), and a seventh injection cavity is formed between the fourth main inclined ejector block (1143) and the movable mold core (14), which is consistent with the shape of the fourth inner buckle position (8) on the side of the thin shell sheet part and is connected to the mold cavity.