High-transmittance temperable low-radiation energy-saving glass
By coating multi-layer structures on the glass substrate, including indium tin oxide, titanium oxide, silicon oxide doped aluminum oxide and titanate layers, as well as magnesium fluoride and zinc sulfide films, existing glass products are solved inadequate strength and impact resistance. The problems of poor capabilities and poor thermal stability achieve higher safety performance and energy-saving effects.
Patent Information
- Application Number
- CN202420541329.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-20
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-03-20
AI Technical Summary
Existing glass products have shortcomings in strength, impact resistance and thermal stability, resulting in safety risks and heat management issues, especially in the construction and automotive industries.
A composite glass structure is adopted, in which the glass substrate is coated with indium tin oxide and titanium oxide conductive film, and a silicon oxide doped aluminum oxide particle layer and a titanate base layer are arranged inside, and a sodium cover and calcium borate coating are plated on the outside, combining fluorine Magnesium and zinc sulfide film layers form a multi-layer structure.
It significantly improves the impact strength and thermal stability of the glass, ensuring structural integrity under harsh environments, while effectively isolating external radiation and heat, achieving higher safety performance and energy-saving effects.
Smart Images

Figure CN222043025U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of glass, in particular to a high-transmittance tempered low-radiation energy-saving glass. Background Art
[0002] The glass processing process usually includes several key steps: melting, forming, annealing and surface treatment. During the surface treatment stage, various coating treatments may be performed, such as coating or chemical strengthening, to improve the performance of the glass, such as enhancing wear resistance, impact resistance or changing its optical properties.
[0003] Existing glass products on the market have some defects, mainly including insufficient strength, poor impact resistance, poor thermal stability, etc. Especially in the construction and automotive industries, these defects may lead to safety risks. Glass is easy to break when subjected to strong impact, producing sharp fragments, increasing the risk of injury. At the same time, if the thermal stability of the glass is insufficient, it is easy to break in an environment with large temperature changes.
[0004] Therefore, there is a need for a high-transmittance temperable low-radiation energy-saving glass to solve the above technical defects. Utility Model Content
[0005] The utility model aims to provide a high-transmittance tempered low-radiation energy-saving glass to solve the problems of insufficient strength, poor impact resistance and poor thermal stability proposed in the above-mentioned background technology.
[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a high-transmittance temperable low-radiation energy-saving glass, comprising a composite glass body, the internal matrix of the composite glass body is a glass substrate, the front and back sides of the glass substrate are coated with an indium tin oxide conductive film and a titanium oxide conductive film layer, a silicon oxide doped aluminum oxide particle layer is arranged inside the glass substrate, the inner layer of the silicon oxide doped aluminum oxide particle layer is arranged with a titanate base layer, the silicon oxide doped aluminum oxide particle layer and the titanate base layer are composited inside the glass substrate, and the outside of the glass substrate is coated with a sodium cap coating layer and a calcium borate coating layer from the inside to the outside.
[0007] Preferably, the outer surface of the glass substrate is alternately coated with magnesium fluoride thin film layers and zinc sulfide thin film layers.
[0008] Preferably, the magnesium fluoride film layer and the zinc sulfide film layer are alternately coated to form an interlayer located inside the indium tin oxide conductive film and the titanium oxide conductive film layer, and the coating is alternately performed four times.
[0009] Preferably, the calcium borate coating layer and the sodium cap coating layer have the same thickness.
[0010] Preferably, the alumina particles in the silicon oxide-doped alumina particle layer are uniformly distributed in the glass substrate.
[0011] Preferably, the thickness of the indium tin oxide conductive film is the same as that of the titanium oxide conductive film layer, and both the indium tin oxide conductive film and the titanium oxide conductive film layer are transparent films.
[0012] Preferably, the edge of the composite glass body is cut before tempering.
[0013] Preferably, the coating sequence of the glass substrate from inside to outside is: first coating the sodium cover coating layer and the calcium borate coating layer, then alternately coating the magnesium fluoride film layer and the zinc sulfide film layer, and finally coating the indium tin oxide conductive film layer and the titanium oxide conductive film layer.
[0014] Compared with the prior art, the utility model has the following beneficial effects: the high-transmittance tempered low-radiation energy-saving glass not only achieves higher impact strength and thermal stability, higher safety performance after tempering, and effectively isolates external heat radiation while maintaining high transparency, but also reduces heat energy loss and achieves better energy-saving effect;
[0015] (1) By providing a silicon oxide doped aluminum oxide particle layer, a titanate base layer, a calcium borate coating layer and a sodium cap coating layer, the glass substrate uses a silicon oxide doped aluminum oxide particle layer and a titanate base layer as a composite matrix, and is coated with a calcium borate coating layer and a sodium cap coating layer on the surface, so that the glass substrate is kept stable during the heat treatment process, so that the entire composite glass body has higher impact strength and thermal stability after tempering, ensuring that the glass still maintains structural integrity and durability when experiencing harsh environments and stresses, and can significantly enhance strength after heat treatment and tempering, providing higher safety performance;
[0016] (2) By providing an indium tin oxide conductive film and a titanium oxide conductive film layer, the glass substrate uses the indium tin oxide conductive film and the titanium oxide conductive film layer as the outermost coating. This structure not only provides excellent light transmittance, but also effectively reflects and absorbs infrared and ultraviolet rays through the application of the indium tin oxide conductive film and the titanium oxide conductive film layer, thereby reducing radiation. The high transparency ensures excellent light transmittance, while the low radiation performance reduces the heat gain in the room, especially in summer, and can effectively isolate the heat radiation from the outside, so that the glass can achieve low radiation function while maintaining high transparency;
[0017] (3) By providing a magnesium fluoride film layer and a zinc sulfide film layer, a glass substrate is provided with an interlayer formed by the magnesium fluoride film layer and the zinc sulfide film layer inside, and the magnesium fluoride film layer and the zinc sulfide film layer are alternately coated on the glass substrate as film layers. The magnesium fluoride film layer and the zinc sulfide film layer can effectively reduce the transfer of heat through the glass and reduce heat energy loss, while maintaining good optical transparency to achieve excellent thermal insulation performance, thereby achieving the purpose of energy saving. It can maintain transparency and effectively block heat transfer, which helps to reduce indoor and outdoor heat exchange, reduce energy consumption for cooling or heating, and achieve better energy saving effects. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 This is a front view structural schematic diagram of the utility model;
[0019] Figure 2 It is a schematic diagram of the layered structure of the utility model;
[0020] Figure 3 This is a schematic diagram of the internal structure of the glass substrate of the utility model;
[0021] Figure 4 Schematic diagram of the glass substrate coating structure of the utility model
[0022] Figure 5 This is a schematic diagram of the layering of the magnesium fluoride film layer and the zinc sulfide film layer of the utility model.
[0023] In the figure: 1. composite glass body; 2. indium tin oxide conductive film; 3. glass substrate; 4. titanium oxide conductive film layer; 5. silicon oxide doped aluminum oxide particle layer; 6. titanate base layer; 7. calcium borate coating layer; 8. sodium cap coating layer; 9. magnesium fluoride thin film layer; 10. zinc sulfide thin film layer. DETAILED DESCRIPTION
[0024] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0025] Example 1: Please refer to Figure 1-5 A high-transmittance temperable low-radiation energy-saving glass comprises a composite glass body 1, wherein the inner substrate of the composite glass body 1 is a glass substrate 3, wherein both the front and back sides of the glass substrate 3 are coated with an indium tin oxide conductive film 2 and a titanium oxide conductive film layer 4, wherein a silicon oxide doped aluminum oxide particle layer 5 is arranged inside the glass substrate 3, wherein the inner layer of the silicon oxide doped aluminum oxide particle layer 5 is provided with a titanate base layer 6, wherein the silicon oxide doped aluminum oxide particle layer 5 and the titanate base layer 6 are composited inside the glass substrate 3, wherein the outer surface of the glass substrate 3 is provided with an inner layer. The outer surface is coated with a sodium cover coating layer 8 and a calcium borate coating layer 7, the calcium borate coating layer 7 and the sodium cover coating layer 8 have the same thickness, the aluminum oxide particles in the silicon oxide doped aluminum oxide particle layer 5 are evenly distributed in the glass substrate 3, the edge of the composite glass body 1 is cut before tempering, and the coating sequence of the glass substrate 3 from the inside to the outside is: firstly, the sodium cover coating layer 8 and the calcium borate coating layer 7 are coated, and then, the magnesium fluoride film layer 9 and the zinc sulfide film layer 10 are alternately coated, and finally, the indium tin oxide conductive film 2 and the titanium oxide conductive film layer 4 are coated;
[0026] Specifically, Figure 1 , Figure 3 and Figure 4 As shown, the glass substrate 3 uses a silicon oxide-doped aluminum oxide particle layer 5 and a titanate base layer 6 as a composite matrix, and is coated with a calcium borate coating layer 7 and a sodium cover coating layer 8 on the surface. The stability of the glass substrate 3 is maintained during the heat treatment process, so that the entire composite glass body 1 has higher impact strength and thermal stability after tempering, ensuring that the glass still maintains structural integrity and durability when experiencing harsh environments and stresses, and can significantly enhance its strength after heat treatment and tempering.
[0027] Embodiment 2: The thickness of the indium tin oxide conductive film 2 is the same as that of the titanium oxide conductive film layer 4, and both the indium tin oxide conductive film 2 and the titanium oxide conductive film layer 4 are transparent films;
[0028] Specifically, Figure 1 and Figure 2 As shown, the glass substrate 3 uses an indium tin oxide conductive film 2 and a titanium oxide conductive film layer 4 as the outermost coating. This structure not only provides excellent light transmittance, but also effectively reflects and absorbs infrared and ultraviolet rays through the application of the indium tin oxide conductive film 2 and the titanium oxide conductive film layer 4, thereby reducing radiation. The high transparency ensures excellent light transmittance, while the low radiation performance reduces the heat gain in the room, especially in summer, and can effectively isolate external heat radiation, so that the glass has good low radiation performance while maintaining high transparency.
[0029] Embodiment 3: The outer surface of the glass substrate 3 is alternately coated with a magnesium fluoride film layer 9 and a zinc sulfide film layer 10, and the magnesium fluoride film layer 9 and the zinc sulfide film layer 10 are alternately coated to form an interlayer located inside the indium tin oxide conductive film 2 and the titanium oxide conductive film layer 4, and the coating is alternately performed four times;
[0030] Specifically, Figure 1 and Figure 5 As shown, the glass substrate 3 is internally provided with an interlayer formed by a magnesium fluoride film layer 9 and a zinc sulfide film layer 10, and the magnesium fluoride film layer 9 and the zinc sulfide film layer 10 are alternately coated on the glass substrate 3 as film layers. The magnesium fluoride film layer 9 and the zinc sulfide film layer 10 can effectively reduce the transfer of heat through the glass and reduce heat energy loss, while maintaining good optical transparency to achieve excellent thermal insulation performance, thereby achieving the purpose of energy saving, maintaining transparency and effectively blocking heat transfer, which helps to reduce indoor and outdoor heat exchange and reduce energy consumption for cooling or heating.
[0031] Working principle: First, during firing, a silicon oxide doped aluminum oxide particle layer 5 and a titanate base layer 6 are added to the glass substrate 3 as a composite matrix. A sodium cap coating layer 8 and a calcium borate coating layer 7 are first plated on the outside of the glass substrate 3, and then magnesium fluoride film layers 9 and zinc sulfide film layers 10 are alternately plated. Finally, an indium tin oxide conductive film 2 and a titanium oxide conductive film layer 4 are plated to form an integral composite glass body 1. The glass substrate 3 uses a silicon oxide doped aluminum oxide particle layer 5 and a titanate base layer 6 as a composite matrix. The stability of the glass substrate 3 is maintained during the heat treatment process, so that the entire composite glass body 1 has higher impact strength and thermal stability after tempering, ensuring that the glass maintains structural integrity and durability when experiencing harsh environments and stresses. The strength can be significantly enhanced after heat treatment and tempering. The glass substrate 3 uses an indium tin oxide conductive film 2 and a titanium oxide conductive film layer 4 as the outermost coating. This structure not only provides excellent light transmittance performance, but also through oxidation The application of indium tin conductive film 2 and titanium oxide conductive film layer 4 can effectively reflect and absorb infrared and ultraviolet rays, thereby reducing radiation. The high transparency ensures excellent light transmittance. At the same time, the low radiation performance reduces the heat gain in the room, especially in summer, it can effectively isolate the heat radiation from the outside, so that the glass has good low radiation performance while maintaining high transparency. The glass substrate 3 is internally provided with an interlayer formed by a magnesium fluoride film layer 9 and a zinc sulfide film layer 10. The magnesium fluoride film layer 9 and the zinc sulfide film layer 10 are alternately coated on the glass substrate 3 as film layers. The magnesium fluoride film layer 9 and the zinc sulfide film layer 10 can effectively reduce the transfer of heat through the glass and reduce heat energy loss. At the same time, they maintain good optical transparency to achieve excellent thermal insulation performance, thereby achieving the purpose of energy saving. It can not only maintain transparency, but also effectively block heat transfer, which helps to reduce indoor and outdoor heat exchange and reduce energy consumption for cooling or heating.
[0032] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
Claims
1. A high-transmittance temperable low-radiation energy-saving glass, comprising a composite glass body (1), characterized in that: The internal matrix of the composite glass body (1) is a glass substrate (3), the front and back surfaces of the glass substrate (3) are coated with an indium tin oxide conductive film (2) and a titanium oxide conductive film layer (4), a silicon oxide doped aluminum oxide particle layer (5) is provided inside the glass substrate (3), a titanate base layer (6) is provided inside the silicon oxide doped aluminum oxide particle layer (5), the silicon oxide doped aluminum oxide particle layer (5) and the titanate base layer (6) are composited inside the glass substrate (3), and the outside of the glass substrate (3) is coated with a sodium cap coating layer (8) and a calcium borate coating layer (7) from the inside to the outside.
2. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The outer surface of the glass substrate (3) is alternately coated with magnesium fluoride thin film layers (9) and zinc sulfide thin film layers (10).
3. The high-transmittance temperable low-emissivity energy-saving glass according to claim 2, characterized in that: The magnesium fluoride film layer (9) and the zinc sulfide film layer (10) are alternately coated to form an interlayer located inside the indium tin oxide conductive film (2) and the titanium oxide conductive film layer (4), and the coating is alternately performed four times.
4. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The calcium borate coating layer (7) and the sodium cap coating layer (8) have the same thickness.
5. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The alumina particles in the silicon oxide-doped alumina particle layer (5) are evenly distributed in the glass substrate (3).
6. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The thickness of the indium tin oxide conductive film (2) is the same as that of the titanium oxide conductive film layer (4); both the indium tin oxide conductive film (2) and the titanium oxide conductive film layer (4) are transparent films.
7. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The edge of the composite glass body (1) is cut before tempering.
8. The high-transmittance temperable low-emissivity energy-saving glass according to claim 1, characterized in that: The coating sequence of the glass substrate (3) from inside to outside is: firstly coating a sodium cover coating layer (8) and a calcium borate coating layer (7), then alternately coating a magnesium fluoride film layer (9) and a zinc sulfide film layer (10), and finally coating an indium tin oxide conductive film (2) and a titanium oxide conductive film layer (4).