Gasket and coating die head

By using the gasket design of the tapered discharge channel in the coating die head, the problem of slurry in the coating of lithium battery electrode sheets is solved, and the uniformity of the electrode sheet thickness and battery performance are improved.

CN222057872UActive Publication Date: 2024-11-26AESC DYNAMICS TECHNOLOGY (ORDOS) LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420428538.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-05
Publication Date
2024-11-26
Estimated Expiration
2034-03-05

AI Technical Summary

Technical Problem

During the lithium battery electrode sheet coating process, it is difficult for the prior art to achieve uniform coating of the slurry, resulting in uneven thickness of the electrode sheet and affecting battery performance.

Method used

A gasket is designed, and its discharge passage consists of two flow baffles, and the spacing between the flow baffles is tapered, so that a gradually increased extrusion pressure is applied in the coating die, so that the slurry is sprayed evenly. Avoid "bang edge" phenomenon.

Benefits of technology

Through the design of the tapered discharge channel, the uniformity of the slurry coating is improved, the overall thickness uniformity of the electrode sheet is ensured, and the thickness difference between the thinned zone and the non-thinned zone is avoided, which improves battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222057872U_ABST
    Figure CN222057872U_ABST
Patent Text Reader

Abstract

The utility model provides a gasket and a coating die head, the gasket comprises a gasket body and two flow baffles arranged at the two ends of the gasket body respectively, a discharging channel is arranged between the two flow baffles, each flow baffle comprises a first flow baffle part and a second flow baffle part, the first flow baffle part is arranged close to the gasket body, and the second flow baffle part is arranged close to the gasket body. The distance between the two first flow blocking parts is larger than the distance between the two second flow blocking parts. In other words, in the direction from the first flow blocking part to the second flow blocking part, the whole discharging channel is gradually shrunk, and the gradually-shrunk discharging channel can apply gradually-increased extrusion force to slurry located in the discharging channel, so that the slurry subjected to the extrusion force can be evenly sprayed out from a discharging opening of the discharging channel, and then the coating uniformity of the slurry is improved; and the problem that the coating thickness of the middle area and the two side areas is not uniform is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of pole piece coating, and in particular to a gasket and a coating die head. Background Art

[0002] Secondary batteries are widely used in electric vehicles, distributed power supply systems for solar and wind energy, power reserve, grid peak regulation, robots, portable medical electronic equipment, aerospace and other fields. With the development of technology, the performance requirements for secondary batteries are getting higher and higher, especially the power density, service life and safety performance of secondary batteries. To achieve these goals, in addition to continuous breakthroughs and innovations in materials, continuous improvement of manufacturing processes is also required.

[0003] In the manufacturing process of secondary batteries, the quality of the electrode coating process directly determines the difficulty, quality, and production efficiency of the subsequent production process of the secondary batteries. Utility Model Content

[0004] In view of this, the purpose of the present application is to propose a gasket and a coating die to solve or partially solve the problems raised by the background technology.

[0005] Based on the above-mentioned purpose, the first aspect of the present application provides a gasket, comprising: a gasket body and two baffles respectively arranged at both ends of the gasket body, a discharge channel is provided between the two baffles, each of the baffles comprises a first baffle portion and a second baffle portion, the first baffle portion is arranged close to the gasket body, and the distance between the two first baffle portions is greater than the distance between the two second baffle portions.

[0006] Optionally, each of the second baffles includes a first end and a second end, the first end is arranged close to the gasket body, and the distance between the two first ends is greater than the distance between the two second ends.

[0007] Optionally, one side of each of the second flow-blocking portions close to the discharge channel is a first flow-blocking side wall, and the first flow-blocking side wall is an inclined surface or a curved surface protruding toward the discharge channel.

[0008] Optionally, when the first flow-blocking side wall is an inclined surface, an angle between the first flow-blocking side wall and a first direction is 5-30°, and the first direction is a width direction of the gasket body.

[0009] Optionally, the second end is an arc-shaped structure protruding toward the discharge channel, the size of the arc-shaped structure in the first direction is larger than the size of the arc-shaped structure in the second direction, the first direction is the width direction of the gasket body, and the second direction is the length direction of the gasket body.

[0010] Optionally, the arc structure is an elliptical chamfered structure, the major axis of the ellipse is parallel to the first direction, the minor axis of the ellipse is parallel to the second direction, the ratio of the major axis to the minor axis is 1.5 to 2.5, the size of the major semi-axis of the ellipse is 2 to 5 mm, and the size of the minor semi-axis of the ellipse is 1 to 3 mm.

[0011] Optionally, the side of each first baffle portion close to the discharge channel is a second baffle side wall, and the side of each second baffle portion close to the gasket body is a third baffle side wall, one end of the third baffle side wall is connected to the second baffle side wall, and the other end is connected to the first baffle side wall, and the third baffle side wall is arranged parallel to the length direction of the gasket body.

[0012] Optionally, each of the second baffles includes a baffle body and a docking portion arranged along the second direction, the docking portion is arranged close to the discharge channel, the docking portion is detachably connected to the baffle body, and the second direction is the length direction of the gasket body.

[0013] Optionally, one of the baffle body and the docking portion is provided with a splicing protrusion, and the other is provided with a positioning groove for the splicing protrusion to be detachably embedded and for enabling the docking portion and the baffle body to stop fitting in a first direction and a second direction, wherein the first direction is the width direction of the gasket body.

[0014] Based on the same inventive concept, the second aspect of the present application provides a coating die, comprising an upper die, a lower die and a gasket as described in any one of the first aspects above, wherein the gasket is sandwiched between the upper die and the lower die.

[0015] From the above description, it can be seen that the gasket and coating die head provided in the present application have a discharge channel between two baffles, each baffle includes a first baffle portion and a second baffle portion, the first baffle portion is arranged close to the gasket body, and the spacing between the two first baffle portions is greater than the spacing between the two second baffle portions, that is, along the direction from the first baffle portion to the second baffle portion, the entire discharge channel is gradually contracted, and the gradually contracting discharge channel can apply a gradually increasing extrusion pressure to the slurry located in the discharge channel, so that the slurry subjected to the extrusion pressure can be evenly sprayed out from the discharge port of the discharge channel, thereby improving the uniformity of the slurry coating and avoiding the problem of uneven coating thickness in the middle area and the two side areas. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0017] Figure 1 This is a schematic diagram of the first structure of the gasket of an embodiment of the present application;

[0018] Figure 2 This is a schematic diagram of the second structure of the gasket of the embodiment of the present application;

[0019] Figure 3 It is a partial enlarged schematic diagram of the second baffle portion of the gasket of the embodiment of the present application;

[0020] Figure 4 This is a third structural schematic diagram of the gasket of the embodiment of the present application;

[0021] Figure 5 It is a partially enlarged schematic diagram of the second end of the first flow guide side wall of the embodiment of the present application;

[0022] Figure 6 This is a fourth structural schematic diagram of the gasket of the embodiment of the present application;

[0023] Figure 7 This is a fifth structural schematic diagram of the gasket of the embodiment of the present application;

[0024] Figure 8 This is a sixth structural schematic diagram of the gasket of the embodiment of the present application;

[0025] Fig. 9 This is a schematic diagram of the structure of the coating die head of an embodiment of the present application;

[0026] Fig.10 This is a schematic diagram of the structure of the gasket of Comparative Example 7.

[0027] In the figure: 1, gasket; 11, gasket body; 111, positioning hole; 12, baffle plate; 121, first baffle portion; 1211, second baffle side wall; 122, second baffle portion; 1221, first baffle side wall; 1222, first end; 1223, second end; 1224, third baffle side wall; 1225, baffle body; 1226, docking portion; 1227, splicing protrusion; 1228, positioning groove; 13, discharge channel; 131, discharge port; 132, feed port; 133, first discharge sub-channel; 134, second discharge sub-channel;

[0028] 2. Upper die head; 3. Lower die head;

[0029] D1, the distance between the two first baffles; D2, the distance between the two second baffles; D3, the distance between the two first ends; D4, the distance between the two second ends; a, the size of the major semi-axis of the ellipse; b, the size of the minor semi-axis of the ellipse; Y, the first direction; X, the second direction. DETAILED DESCRIPTION

[0030] In order to make the objectives, technical solutions and advantages of the present application more clearly understood, the present application is further described in detail below in combination with specific embodiments and with reference to the accompanying drawings.

[0031] It should be noted that, unless otherwise defined, the technical terms or scientific terms used in the embodiments of the present application should be the usual meanings understood by people with ordinary skills in the field to which the present application belongs. The "first", "second" and similar words used in the present application do not represent any order, quantity or importance, but are only used to distinguish different components. "Including" or "comprising" and similar words mean that the elements or objects appearing in front of the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connecting" or "connected" and similar words are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to represent relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0032] The performance of lithium-ion battery cells accounts for a large proportion of the overall performance of the battery pack, because in the overall system of multiple groups of battery cells connected in series and parallel, the inconsistency of the performance of a single battery cell will lead to the worst performance of the entire battery pack, and even cause the failure of the entire battery pack; among the many factors that affect battery consistency, the consistency of the electrode coating quality is the top priority, which not only directly affects the overall capacity of the battery pack, but also affects the voltage, power and life of the entire group of batteries, and the coating process is what determines the quality of the electrode coating.

[0033] At present, lithium battery manufacturing companies mainly use slit extrusion coating technology, which is characterized by high efficiency, good coating uniformity and stable coating process. The working principle of extrusion coating is to first feed the electrode slurry into the cavity in the coating die, and then under a certain pressure, the slurry is squeezed out through the slit in the die to form a uniform coating on the moving electrode. The coating die is generally composed of an upper die, a lower die and a gasket. The gasket is an open metal sheet sandwiched between the upper and lower dies. The size of the slit in the coating die is mainly determined by the opening size of the gasket and the thickness of the gasket.

[0034] The uniformity of coating thickness of lithium battery pole pieces directly affects the performance of the battery. However, currently, during the coating process, due to the surface tension of the slurry liquid, a "bulging edge" phenomenon may occur at the coating edge, resulting in uneven coating thickness of the entire pole piece, thus affecting battery performance.

[0035] The industry also makes some special designs on the gasket structure to thin the coating edge. However, most thinning designs will cause the thinning area to be too wide or the thinning depth to be too deep, which will lead to a large difference in thickness between the thinned area and the non-thinned area, resulting in uneven coating thickness of the entire electrode, affecting battery performance.

[0036] Based on this, the present application provides a gasket and a coating die head, which improve the uniformity of slurry coating by controlling the width of the discharge channel.

[0037] In some embodiments, see Figure 1 As shown, Figure 1 The first structural schematic diagram of the gasket 1 provided in the present application is shown. The gasket 1 comprises: a gasket body 11 and two baffles 12 respectively arranged at both ends of the gasket body 11, a discharge channel 13 is arranged between the two baffles 12, each baffle 12 comprises a first baffle portion 121 and a second baffle portion 122, the first baffle portion 121 is arranged close to the gasket body 11, and the spacing between the two first baffle portions 121 is greater than the spacing between the two second baffle portions 122.

[0038] Specifically, the gasket body 11 may be a thin sheet structure, and the thickness of the gasket body 11 may be 0.8 mm-1.2 mm. Exemplarily, the thickness of the gasket body 11 may be 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, etc.

[0039] Two baffles 12 are respectively disposed at both ends of the gasket body 11. For example, in order to facilitate installation and use, the gasket body 11 and the two baffles 12 can be formed into an integrated structure.

[0040] A plurality of positioning holes 111 may be provided on the gasket body 11 for positioning and installing the gasket body 11 and the die head.

[0041] A discharge channel 13 is provided between the two baffles 12, and one end of the discharge channel 13 close to the gasket body 11 is a feed port 132, and one end of the discharge channel 13 away from the gasket body 11 is a discharge port 131. In specific implementation, the electrode slurry is fed into the cavity in the coating die head, and under a certain pressure, the slurry moves from the feed port 132 to the discharge port 131 and is sprayed out from the discharge port 131, coating the moving electrode to form a coating layer.

[0042] Each baffle plate 12 includes a first baffle portion 121 and a second baffle portion 122 . For example, in order to facilitate installation and use, the first baffle portion 121 and the second baffle portion 122 may be formed as an integrated structure.

[0043] The spacing between the two first baffles 121 is greater than the spacing between the two second baffles 122, that is, along the direction from the first baffle 121 to the second baffle 122, the entire discharge channel 13 is tapered, and the tapered discharge channel 13 can apply a gradually increasing extrusion pressure to the slurry in the discharge channel 13, so that the slurry subjected to the extrusion pressure can be evenly sprayed out from the discharge port 131 of the discharge channel 13, so that the coating thickness of the entire electrode is relatively uniform. At the same time, due to the influence of the surface tension and fluidity of the slurry, the amount of slurry sprayed to the edge of the electrode is slightly less than the amount of slurry sprayed to the center area of ​​the electrode (because the slurry is subjected to the extrusion pressure, the extrusion pressure can offset part of the influence of the surface tension and fluidity of the slurry), so that a thinning area with a shallower thinning thickness and a narrower thinning width can be formed to avoid the "bulging edge" phenomenon at the coating edge. In this way, the "bulging edge" phenomenon can be avoided while ensuring that the overall coating thickness of the electrode is relatively uniform.

[0044] It is worth noting that the spacing between the various positions of the two first flow blocking portions 121 can be the same or different. For example, the two first flow blocking portions 121 can be arranged perpendicular to the gasket body 11, so that the spacing between the various positions of the two first flow blocking portions 121 is the same; or, one of the two first flow blocking portions 121 is arranged perpendicular to the gasket body 11, and the other is arranged obliquely to the gasket body 11 (at a certain angle to the vertical direction of the gasket body 11), so that the spacing between the various positions of the two first flow blocking portions 121 is different; or, both of the two first flow blocking portions 121 are arranged obliquely to the gasket body 11 or are arranged as an arc structure, so that the spacing between the various positions of the two first flow blocking portions 121 is different.

[0045] The spacing between the positions of the two second flow blocking portions 122 may be the same or different. For example, the two second flow blocking portions 122 may be arranged perpendicular to the gasket body 11, so that the spacing between the positions of the two second flow blocking portions 122 is the same; or, one of the two second flow blocking portions 122 is arranged perpendicular to the gasket body 11, and the other is arranged obliquely to the gasket body 11 (at a certain angle to the vertical direction of the gasket body 11), so that the spacing between the positions of the two second flow blocking portions 122 is different; or, both of the second flow blocking portions 122 are arranged obliquely to the gasket body 11 or are arranged as an arc structure, so that the spacing between the positions of the two second flow blocking portions 122 is different.

[0046] Although the spacing between each position of the two first baffles 121 can be the same or different, and the spacing between each position of the two second baffles 122 can be the same or different, the spacing between the two first baffles 121 must be greater than the spacing between the two second baffles 122, so that the entire discharge channel 13 is tapered to improve the uniformity of slurry coating.

[0047] Exemplarily, the spacing between each position of the two first baffles 121 can be 360mm, 355mm, 350mm, etc., and the spacing between each position of the two second baffles 122 can be 345mm, 340mm, 330mm, 320mm, etc., to ensure that the spacing between the two first baffles 121 must be greater than the spacing between the two second baffles 122.

[0048] In some embodiments, see Figure 2 As shown, Figure 2 A second structural schematic diagram of the gasket 1 provided in the present application is shown, where each second baffle portion 122 includes a first end 1222 and a second end 1223 , the first end 1222 is arranged close to the gasket body 11 , and the distance between the two first ends 1222 is greater than the distance between the two second ends 1223 .

[0049] Specifically, the first end 1222 is the end close to the feed port 132, and the second end 1223 is the end close to the discharge port 131. The distance between the two first ends 1222 is greater than the distance between the two second ends 1223, so that the portion of the discharge channel 13 located between the two second baffles 122 continues to be tapered.

[0050] Since the second baffle portion 122 is arranged close to the discharge port 131, when the portion of the discharge channel 13 located between the two second baffle portions 122 continues to be tapered, the continuously tapering discharge channel 13 can continue to apply a gradually increasing extrusion pressure to the slurry located in the discharge channel 13, so that the slurry subjected to the extrusion pressure can be evenly sprayed out from the discharge port 131 of the discharge channel 13, thereby further improving the uniformity of the slurry coating.

[0051] In some embodiments, see Figure 2 The ratio of the spacing between the two first baffles 121 to the spacing between the two second ends 1223 is 1.2 to 1.5. The test results show that when the spacing ratio is within this range, the tapering degree of the discharge channel 13 is optimal, and the extrusion pressure provided to the slurry is moderate, so that the depth of the obtained thinning area is smaller and the width is narrower, which can avoid the "bulging edge" phenomenon and will not produce a significant difference in thickness with the non-thinning area, thereby improving the uniformity of the coating thickness.

[0052] For example, the ratio of the distance between the two first flow blocking portions 121 to the distance between the two second ends 1223 may be 1.2, 1.3, 1.4, 1.5, etc.

[0053] In some embodiments, see Figure 2 As shown, one side of each second flow blocking portion 122 close to the discharge channel 13 is a first flow blocking side wall 1221 , and the first flow blocking side wall 1221 is an inclined surface.

[0054] Specifically, the first baffle sidewall 1221 is an inclined surface. Under the premise that the spacing between the two first ends 1222 is greater than the spacing between the two second ends 1223, the first baffle sidewall 1221 can only be an inclined surface inclined from the discharge port 131 to the first baffle portion 121. The first baffle sidewall 1221 is inclined in this way, so that the portion of the discharge channel 13 between the two second baffle sidewalls 1211 presents a gradually regular tapered structure, so that a gradually increasing extrusion force can be applied to the slurry to ensure that the extrusion force on the slurry near the discharge port 131 is the maximum, so that the slurry is ejected outward under the action of the maximum extrusion force, increasing the force and ejection area of ​​the slurry ejected outward, thereby improving the uniformity of the slurry coating. At the same time, under the triple influence of the extrusion force, its own surface tension and fluidity, the slurry can form a thinning area with a slightly smaller coating thickness to avoid the "bulging edge" phenomenon at the coating edge.

[0055] In some embodiments, see Figure 3 As shown, Figure 3 The schematic diagram of the second baffle portion 122 of the gasket 1 provided in the present application is shown in a partially enlarged manner. When the first baffle side wall 1221 is an inclined surface, the angle ɑ between the first baffle side wall 1221 and the first direction Y is 5 to 30°, and the first direction Y is the width direction of the gasket body 11 (i.e. Figure 3 Y direction in ).

[0056] Specifically, when the angle ɑ between the first baffle side wall 1221 and the first direction Y is 5 to 30°, the slurry can form a thinning area with appropriate coating thickness under the triple influence of extrusion pressure, its own surface tension and fluidity, which can not only avoid the "bulging edge" phenomenon, but also ensure that the thickness difference between the thinning area and the non-thinning area will not be too large, so that the coating thickness of the entire pole piece is relatively uniform as a whole.

[0057] When the angle ɑ between the first baffle side wall 1221 and the first direction Y is less than 5°, the inclination angle of the first baffle side wall 1221 is small, so that the discharge channel 13 between the two first baffle side walls 1221 tapers to a smaller extent, thereby making the extrusion pressure applied to the slurry by the discharge channel 13 very small. The small extrusion pressure cannot effectively offset the effects of the surface tension and fluidity of the slurry, resulting in the final formation of a thinning area with a very deep thinning depth. Although the "bulging edge" phenomenon at the coating edge can be avoided, the overall coating thickness of the electrode is more obviously different, and the coating thickness uniformity of the electrode is poor, which affects the battery performance.

[0058] When the angle ɑ between the first baffle side wall 1221 and the first direction Y is greater than 30°, the inclination angle of the first baffle side wall 1221 is relatively large, which is not conducive to the spraying of the slurry, resulting in the possibility of material hanging, which is not conducive to practical use.

[0059] Exemplarily, the angle ɑ between the first baffle side wall 1221 and the first direction Y can be 5°, 8°, 10°, 12°, 14°, 16°, 18°, 20°, 22°, 24°, 26°, 28°, 30°, etc.

[0060] In some embodiments, see Figure 4 As shown, Figure 4 A third structural schematic diagram of the gasket 1 provided in the present application is shown, in which the first flow-blocking side wall 1221 is a curved surface protruding toward the discharge channel 13 .

[0061] Specifically, the first baffle side wall 1221 is an arc surface protruding toward the discharge channel 13. Under the premise that the distance between the two first ends 1222 is greater than the distance between the two second ends 1223, the arc-surface second baffle side wall 1211 makes the flow of the slurry smoother and the resistance to outward spraying is smaller, thereby further increasing the spraying area of ​​the slurry and improving the uniformity of the coating.

[0062] In some embodiments, Figure 5 As shown, Figure 5 The second end 1223 of the first flow-guiding side wall is partially enlarged in schematic diagram. The second end 1223 is an arc-shaped structure protruding toward the discharge channel 13 .

[0063] Specifically, the second end 1223 is set as an arc-shaped structure, which can improve the flow path of the slurry inside the extrusion die head, so that the edge of the slurry can be dispersed before contacting the electrode, which can eliminate the slurry dead zone to a certain extent, improve the coating effect of the edge of the discharge port 131, and further avoid the "bulging edge" phenomenon at the coating edge.

[0064] The size of the arc structure in the first direction Y is greater than the size of the arc structure in the second direction X. The first direction Y is the width direction of the gasket body 11, that is, Figure 5 The second direction X is the length direction of the gasket body 11, that is, Figure 5 The X direction in .

[0065] The size of the arc structure in the first direction Y is greater than or equal to the size of the arc structure in the second direction X, that is, the size of the arc structure in the direction of slurry discharge is larger, and the range of the arc structure is larger, which can better eliminate the slurry dead zone and improve the coating effect at the edge of the discharge port 131.

[0066] If the size of the arc structure in the first direction Y is smaller than the size of the arc structure in the second direction X, the size of the arc structure in the direction of slurry discharge is too small, resulting in the inability to effectively disperse the slurry edge before contacting the electrode, and failing to effectively eliminate the slurry dead zone.

[0067] In some embodiments, see Figure 5 As shown, the arc structure is an elliptical chamfered structure, the major axis of the ellipse is parallel to the first direction Y, and the minor axis of the ellipse is parallel to the second direction X. Specifically, the elliptical chamfered structure can not only better eliminate the slurry dead zone and improve the coating effect of the edge of the discharge port 131, but also facilitate the actual manufacturing process and reduce the manufacturing cost.

[0068] Optionally, the ratio of the major axis (i.e. 2a) to the minor axis (i.e. 2b) of the ellipse is 1.5 to 2.5. The test results show that when the ratio of the major axis to the minor axis is 1.5 to 2.5, the elliptical chamfer structure can effectively eliminate the dead zone of the slurry and improve the coating effect at the edge of the discharge port 131. The width and thickness of the obtained thinning zone are moderate, which improves the uniformity of the coating.

[0069] When the ratio of the major axis to the minor axis is less than 1.5, the size of the arc structure in the direction of slurry discharge is too small, resulting in the inability to effectively disperse the slurry edge before contacting the electrode. The resulting thinning width of the thinned area is wide, which cannot effectively eliminate the slurry dead zone; when the ratio of the major axis to the minor axis is greater than 2.5, the thinning depth of the thinned area is too deep, resulting in poor coating thickness uniformity.

[0070] Illustratively, the ratio of the major axis to the minor axis may be 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, etc.

[0071] Optionally, the size a of the major semi-axis of the ellipse is 2 to 5 mm, and the size b of the minor semi-axis of the ellipse is 1 to 3 mm. Exemplarily, the size of the major semi-axis may be 2 mm, 3 mm, 4 mm, 5 mm, etc., and the size b of the minor semi-axis of the ellipse may be 1 mm, 1.5 mm, 2 mm, 2.5 mm, 3 mm, etc.

[0072] It is worth noting that the size selection of the major axis and the minor axis needs to be based on the ratio of the major axis to the minor axis. That is to say, when selecting the size of the major axis and the minor axis, it must be done under the premise of ensuring that the ratio of the major axis to the minor axis is between 1.5 and 2.5.

[0073] In some embodiments, see Figure 6 As shown, Figure 6 The fourth structural schematic diagram of the gasket 1 of the present application is shown. The side of each first flow blocking portion 121 close to the discharge channel 13 is a second flow blocking side wall 1211, and the side of each second flow blocking portion 122 close to the gasket body 11 is a third flow blocking side wall 1224, one end of the third flow blocking side wall 1224 is connected to the second flow blocking side wall 1211, and is connected to the first flow blocking side wall 1221, and the third flow blocking side wall 1224 is arranged parallel to the length direction of the gasket body 11.

[0074] Specifically, the third baffle side wall 1224 is arranged parallel to the length direction of the gasket body 11, so that the two third baffle side walls 1224, the two second baffle side walls 1211 and the gasket body 11 together form a larger first discharge sub-channel 133, and a tapered second discharge sub-channel 134 is formed between the two first baffle side walls 1221. In this way, the larger first discharge sub-channel 133 can accommodate more slurry. When more slurry flows from the first discharge sub-channel 133 to the second discharge sub-channel 134, the second discharge sub-channel 134 is narrower and tapered due to the large amount of slurry. At this time, the second discharge sub-channel 134 can apply a larger extrusion pressure to the slurry, thereby promoting the slurry to be sprayed out quickly and evenly, thereby improving the uniformity of the coating.

[0075] In some embodiments, see Figure 7 As shown, Figure 7 The fifth structural schematic diagram of the gasket 1 of the present application is shown. The second flow-blocking side wall 1211 is an arc-shaped structure that bulges away from the discharge channel 13, so that the area of ​​the first discharge sub-channel 133 can be further increased, and the amount of slurry contained in the first discharge sub-channel 133 can be further increased, so as to further improve the coating efficiency while ensuring the coating uniformity.

[0076] In some embodiments, see Figure 8 As shown, Figure 8The sixth structural schematic diagram of the gasket 1 of the present application is shown. Each second baffle 122 includes a baffle body 1225 and a docking portion 1226 arranged along the second direction X, the docking portion 1226 is arranged close to the discharge channel 13, and the docking portion 1226 is detachably connected to the baffle body 1225. The second direction X is the length direction of the gasket body 11.

[0077] Specifically, the docking portion 1226 is detachably connected to the flow blocking body 1225, which facilitates the assembly of the docking portion 1226 and the flow blocking body 1225 on the one hand, and facilitates the replacement of the docking portion 1226 on the other hand. In actual use, since the docking portion 1226 is arranged close to the discharge channel 13, that is, the first flow blocking side wall 1221 and the first end 1222 are both arranged on the docking portion 1226, the docking portion 1226 is highly worn after long-term use. By providing the detachably connected docking portion 1226 and the flow blocking body 1225, the disassembly, replacement and installation of the docking portion 1226 are relatively convenient. Only the docking portion 1226 can be replaced without replacing other parts, which is convenient for actual use.

[0078] In some embodiments, see Figure 8 One of the baffle body 1225 and the docking part 1226 is provided with a splicing protrusion 1227, and the other is provided with a positioning groove 1228 for the splicing protrusion 1227 to be detachably inserted and to enable the docking part 1226 and the baffle body 1225 to stop and cooperate in the first direction Y and the second direction X, wherein the first direction Y is the width direction of the gasket body 11.

[0079] Specifically, the structures of the two docking parts 1226 used in pairs can be the same, which is convenient for the actual manufacturing process. Figure 8 As shown, a splicing protrusion 1227 is provided on one side of the docking portion 1226 close to the flow baffle body 1225, and the cross-section of the splicing protrusion 1227 can be T-shaped to form a T-shaped splicing protrusion 1227, and a corresponding positioning groove 1228 is provided on one side of the corresponding flow baffle body 1225 close to the docking portion 1226, and the positioning groove 1228 is a T-shaped groove adapted to the shape of the T-shaped splicing protrusion 1227, and the T-shaped splicing protrusion 1227 on the docking portion 1226 cooperates with the T-shaped groove on the flow baffle body 1225 to realize a detachable connection between the docking portion 1226 and the flow baffle body 1225.

[0080] The inner wall surface of the T-slot and the side wall surface of the T-shaped splicing protrusion 1227 in the first direction Y constitute a stop surface that limits the movement of the T-shaped splicing protrusion 1227 in the horizontal plane of the gasket 1 to achieve the stop fit between the docking portion 1226 and the flow blocking body 1225 in the horizontal plane.

[0081] In other embodiments, the T-shaped splicing protrusion 1227 may be located on the side of the flow blocking body 1225 that cooperates with the docking surface, and the corresponding T-shaped groove is located on the side of the docking portion 1226 .

[0082] In the present application, the detachable cooperation between the splicing protrusion 1227 and the positioning groove 1228 can facilitate the disassembly, replacement and installation of the docking part 1226, and can also limit the relative movement between the docking part 1226 and the flow baffle body 1225, thereby ensuring the stability of the slurry coating process.

[0083] The present application also provides a coating die head, see Fig. 9 , Fig. 9 A schematic structural diagram of a coating die is shown, which includes an upper die 2, a lower die 3 and a gasket 1 described in any of the above embodiments, wherein the gasket 1 is clamped between the upper die 2 and the lower die 3, and the size of the slit in the coating die is mainly determined by the size of the discharge channel 13 of the gasket 1 and the thickness of the gasket 1.

[0084] In specific implementation, the electrode slurry is first fed into the cavity in the coating die head, and then under a certain pressure, the slurry passes through the discharge channel 13 in the gasket 1 and is squeezed and sprayed out from the discharge port 131 to be coated on the moving electrode to form a uniform coating.

[0085] In order to further verify the coating effect of the gasket 1 and the coating die provided in the present application, according to the parameters shown in Table 1 below, gaskets 1 with different parameters are assembled into a coating die, and their coating effects are tested. The test results are shown in Table 1 below.

[0086] Table 1 Coating effect test of each coating die head

[0087]

[0088] It can be seen from Table 1 above that, compared with each comparative example, in each embodiment, the thinning width of the thinning zone is narrower, the thinning depth is shallower, and there is no material hanging, which means that after coating using the coating die head of each embodiment, a thinning zone with appropriate thinning depth and thinning width is obtained, which can avoid the "drum edge" phenomenon and the problem of poor uniformity caused by the large difference in coating thickness between the thinning zone and the non-thinning zone, thereby effectively improving the uniformity of the coating thickness.

[0089] In Comparative Examples 1 and 2, since the angle ɑ between the first baffle side wall 1221 and the first direction Y is too small, the inclination angle of the first baffle side wall 1221 is small, so that the discharge channel 13 between the two first baffle side walls 1221 is less tapered, and the extrusion pressure applied to the slurry by the discharge channel 13 is very small. The small pressure cannot effectively offset the effects of the surface tension and fluidity of the slurry, resulting in the final formation of a thinning area with a very thin coating thickness and a deep thinning depth. Although the "bulging edge" phenomenon at the coating edge can be avoided, the overall coating thickness difference of the electrode piece is more obvious, and the coating thickness uniformity of the electrode piece is poor, which affects the battery performance.

[0090] In comparative example 3, since the included angle ɑ between the first baffle side wall 1221 and the first direction Y is too large, the inclination angle of the first baffle side wall 1221 is relatively large, which is not conducive to the spraying of the slurry, resulting in the situation of hanging material, which is not conducive to practical use.

[0091] In Comparative Example 4, since the ratio of the major axis to the minor axis is too small, the size of the arc structure in the direction of slurry discharge is too small, resulting in the inability of the slurry edge to be effectively dispersed before contacting the electrode. The resulting thinning width of the thinned area is wide, which cannot effectively eliminate the slurry dead zone.

[0092] In Comparative Example 5, since the ratio of the major axis to the minor axis is too large, the thinning depth of the thinned area is too deep, resulting in poor uniformity of coating thickness.

[0093] In comparative example 6, since the ratio of the spacing between the two first baffles 121 to the spacing between the two second ends 1223 is less than 1.2, the taper degree of the discharge channel 13 is poor, and the extrusion pressure provided to the slurry is small, so that the obtained thinning zone is deeper and wider.

[0094] In comparative example 7, since the distance between the two first baffles 121 is smaller than the distance between the two second ends 1223 (such as Fig.10 As shown), the discharge channel 13 cannot provide extrusion force to the slurry, and the arc-shaped structure setting of the first end 1222 alone cannot well improve the edge coating effect, and ultimately the thinning area is deeper and wider.

[0095] In comparative example 8, since the ratio of the distance between the two first baffles 121 to the distance between the two second ends 1223 is too large, it is not conducive to the spraying of the slurry, resulting in the situation of material hanging, which is not conducive to practical use.

[0096] In comparative example 9, since the first end 1222 is not configured as an arc-shaped structure, the slurry dead zone cannot be eliminated and the coating effect at the edge of the discharge port 131 cannot be improved, resulting in a wider width and thicker thickness of the obtained thinned area.

[0097] In summary, the gasket 1 and coating die head provided in the present application, the tapered discharge channel 13 can apply a gradually increasing extrusion pressure to the slurry located in the discharge channel, so that the slurry subjected to the extrusion pressure can be evenly sprayed out from the discharge port 131 of the discharge channel 13, thereby improving the uniformity of the slurry coating and avoiding the problem of uneven coating thickness in the middle area and the two side areas. At the same time, the first end 1222 is set to an arc structure, which can also avoid the "bulging edge" phenomenon.

[0098] Those skilled in the art should understand that the discussion of any of the above embodiments is merely illustrative and is not intended to imply that the scope of the present application (including the claims) is limited to these examples. In line with the concept of the present application, the technical features in the above embodiments or different embodiments may be combined, the steps may be implemented in any order, and there are many other variations of the different aspects of the present application as described above, which are not provided in detail for the sake of simplicity.

[0099] The embodiments of the present application are intended to cover all such substitutions, modifications and variations that fall within the broad scope of the appended claims. Therefore, any omissions, modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A gasket, characterized in that: include: A gasket body and two baffles respectively arranged at both ends of the gasket body, a discharge channel is arranged between the two baffles, each of the baffles includes a first baffle portion and a second baffle portion, the first baffle portion is arranged close to the gasket body, the spacing between the two first baffle portions is greater than the spacing between the two second baffle portions, each of the second baffle portions includes a first end and a second end, the first end is arranged close to the gasket body, the spacing between the two first ends is greater than the spacing between the two second ends, the second end is an arc structure protruding toward the discharge channel, the size of the arc structure in the first direction is greater than the size of the arc structure in the second direction, the first direction is the width direction of the gasket body, and the second direction is the length direction of the gasket body.

2. The gasket according to claim 1, characterized in that One side of each of the second flow-blocking portions close to the discharge channel is a first flow-blocking side wall, and the first flow-blocking side wall is an inclined surface or a curved surface protruding toward the discharge channel.

3. The gasket according to claim 2, characterized in that When the first flow-blocking side wall is an inclined surface, an angle between the first flow-blocking side wall and a first direction is 5-30°, and the first direction is a width direction of the gasket body.

4. The gasket according to claim 1, characterized in that The arc structure is an elliptical chamfered structure, the major axis of the ellipse is parallel to the first direction, the minor axis of the ellipse is parallel to the second direction, the ratio of the major axis to the minor axis is 1.5 to 2.5, the size of the major semi-axis of the ellipse is 2 to 5 mm, and the size of the minor semi-axis of the ellipse is 1 to 3 mm.

5. The gasket according to claim 1, characterized in that The side of each first baffle portion close to the discharge channel is a second baffle side wall, and the side of each second baffle portion close to the gasket body is a third baffle side wall, one end of the third baffle side wall is connected to the second baffle side wall, and the other end is connected to the first baffle side wall, and the third baffle side wall is arranged parallel to the length direction of the gasket body.

6. The gasket according to claim 1, characterized in that Each of the second baffles includes a baffle body and a docking portion arranged along a second direction, wherein the docking portion is arranged close to the discharge channel and is detachably connected to the baffle body, and the second direction is the length direction of the gasket body.

7. The gasket according to claim 6, characterized in that One of the baffle body and the docking portion is provided with a splicing protrusion, and the other is provided with a positioning groove for the splicing protrusion to be detachably embedded and for enabling the docking portion and the baffle body to stop and cooperate in the first direction and the second direction, wherein the first direction is the width direction of the gasket body.

8. A coating die head, characterized in that: The invention comprises an upper die head, a lower die head and a gasket as claimed in any one of claims 1 to 7, wherein the gasket is clamped between the upper die head and the lower die head.