Double-silver coated glass

By designing a multi-layer film structure in double-silver coated glass, using the low radiation performance and high refractive index of the silver layer and titanium nitride layer, the problem of color discoloration at different perspectives is solved, and the color stability is achieved The improvement of performance and energy-saving effects reduces the color difference of small angles, making the glass appear neutral blue-gray, suitable for energy-saving curtain walls.

CN222064386UActive Publication Date: 2024-11-26CHANGXING QIBIN ENERGY SAVING GLASS CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323351543.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-08
Publication Date
2024-11-26
Estimated Expiration
2033-12-08

AI Technical Summary

Technical Problem

Double silver Low-E glass and triple silver Low-E glass will experience obvious discoloration problems at different perspectives, resulting in visual discomfort and color difference, affecting the effect of energy-saving curtain walls.

Method used

Design a double silver coated glass, which includes a glass base surface, multi-layer dielectric and functional layer through the film layer structure, and controls the film layer thickness and composition using the low radiation properties of the silver layer and the high refractive index and stability of the titanium nitride layer. , improve color stability and transmission performance, reduce small angle color difference, and improve the structural stability and mechanical properties of the film layer through the silicon nitride layer and zinc-aluminum oxide layer.

Benefits of technology

The color stability and energy-saving effect of coated glass are improved, the color difference is reduced, the transmission performance is improved, and the glass is neutral blue-gray, which enhances the applicability and versatility, and the user looks at it from the indoor view. The scenery you visit is closer to nature.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222064386U_ABST
    Figure CN222064386U_ABST
Patent Text Reader

Abstract

The utility model discloses double-silver coated glass which comprises a glass base surface, a first dielectric layer, a first functional layer, a first protective layer, a second dielectric layer, a second functional layer, a second protective layer and a third dielectric layer from bottom to top, the first functional layer is a silver layer; the second functional layer is a silver layer; the first protection layer is a titanium nitride layer. According to the double-silver coated glass, the film layer structure of the double-silver coated glass is designed, so that the color stability of the coated glass is improved, and the small-angle chromatic aberration is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of coated glass, in particular to double-silver coated glass. Background Art

[0002] With the development of energy-saving curtain wall glass in related technologies, Low-E glass (Low-Emissivity glass, low-radiation glass) has been widely used; Low-E glass mainly includes single-silver Low-E glass, double-silver Low-E glass, triple-silver Low-E glass and silver-free Low-E glass; among them, double-silver Low-E glass and triple-silver Low-E glass have more pure silver layers and have better sun-shading performance; therefore, they have better energy-saving effects and can meet the energy-saving needs of curtain walls.

[0003] However, in the related art, double-silver Low-E glass and triple-silver Low-E glass will have obvious discoloration problems at different viewing angles (the discoloration is mainly caused by light polarization), especially at small angles; the discoloration, that is, the glass appears "colorful", will affect people's visual experience and also cause visual fatigue; due to the discoloration problem of the glass itself, the color displayed by the glass will also be slightly different due to different installation heights, that is, the "color difference" caused by the installation positions of the same film system at different heights. Utility Model Content

[0004] The main purpose of the utility model is to provide a double-silver coated glass; the coated glass adopts a double-silver structure, and through the film layer structure design, the color of the coated glass is stable and consistent, and it presents a neutral blue-gray outdoors, and has excellent applicability and versatility.

[0005] To achieve the above-mentioned purpose, the double silver-coated glass proposed by the utility model comprises, from bottom to top: a glass base surface, a first dielectric layer, a first functional layer, a first protective layer, a second dielectric layer, a second functional layer, a second protective layer and a third dielectric layer;

[0006] The first functional layer is a silver layer;

[0007] The second functional layer is a silver layer;

[0008] The first protective layer is a titanium nitride layer.

[0009] According to one technical solution of the utility model, there are at least the following beneficial effects:

[0010] The utility model designs the film structure of the double-silver coated glass, thereby improving the color stability of the coated glass and reducing the color difference at small angles (30° to 60°);

[0011] The first functional layer is a silver layer, which uses the low-radiation properties of silver to reduce the emissivity of the coated glass and filter sunlight into a cold light source, thereby improving energy-saving effects and further improving transmittance performance.

[0012] The first protective layer is a titanium nitride layer. Titanium nitride has a high refractive index and stable chemical properties. It has a strong bonding force with the adjacent film layer and can effectively improve the transmittance color of the coated glass, making the coated glass more "neutral" and the scenery that users see from indoors through the coated glass can be closer to nature. In addition, the titanium nitride layer also plays a good protective role for the first functional layer.

[0013] The second functional layer is a silver layer, which uses the low-radiation properties of silver to reduce the emissivity of the coated glass and filter sunlight into a cold light source, thereby improving energy-saving effects and further improving transmittance performance.

[0014] Optionally, the thickness of the first dielectric layer is 25 nm to 43 nm.

[0015] By controlling the thickness of the first dielectric layer within the above range, the structural stability of the film layer is further improved.

[0016] Optionally, the first dielectric layer includes a silicon oxide layer, a silicon nitride layer and a zinc aluminum oxide layer.

[0017] The silicon oxide layer has a high refractive index, which can improve the light transmittance of the film layer; and the material is similar to the glass base surface, so it can be better combined with the glass base surface.

[0018] The silicon nitride layer can block the sodium ions and potassium ions in the glass base plane from migrating into the first functional layer, thereby affecting the performance of the first functional layer.

[0019] The surface structure of the zinc aluminum oxide layer is smooth and does not form a columnar structure; therefore, it can be used as a seed layer for the first functional layer to make the first functional layer grow uniformly and achieve uniform adhesion of the first functional layer, thereby further improving the conductivity of the first functional layer.

[0020] Optionally, the thickness of the first protective layer is 6.5 nm to 8 nm.

[0021] Controlling the thickness of the first protective layer within the above range is beneficial to further improving the protective effect.

[0022] Optionally, the second dielectric layer includes an aluminum-doped zinc oxide layer, a silicon nitride layer, a zinc-tin oxide layer and a zinc-aluminum oxide layer.

[0023] The film structure of the aluminum-doped zinc oxide layer is uniform and dense, which can further improve the stability of the film structure.

[0024] The silicon nitride layer has high hardness and excellent wear resistance, which is beneficial to improving the mechanical properties of the film layer.

[0025] The zinc-tin oxide layer and the zinc-aluminum oxide layer have a dense film structure and can also adjust the reflectivity of the film to further reduce small-angle discoloration.

[0026] Optionally, the second dielectric layer has a thickness of 60 nm to 75 nm.

[0027] By controlling the thickness of the second dielectric layer within the above range, the structural stability of the film layer is further improved; the polarization of the film layer can also be further controlled, thereby reducing small-angle discoloration.

[0028] Optionally, the thickness of the first functional layer is 5 nm to 8 nm.

[0029] Optionally, the thickness of the second functional layer is 9 nm to 11 nm.

[0030] By controlling the thickness of the first functional layer and the second functional layer, the energy-saving effect of the coated glass can be further improved.

[0031] Optionally, the third dielectric layer includes an aluminum-doped zinc oxide layer, a silicon nitride layer and a silicon-zirconium alloy layer.

[0032] The aluminum-doped zinc oxide layer has a strong bonding ability with the adjacent film layer, thereby further improving the stability of the film layer.

[0033] The silicon nitride layer has high hardness and excellent wear resistance, which is beneficial to further improve the mechanical properties and scratch resistance of the film layer.

[0034] The silicon-zirconium alloy layer has high hardness, strong corrosion resistance and strong oxidation resistance, which is beneficial to further improve the mechanical properties and stability of the film layer.

[0035] Optionally, the thickness of the third dielectric layer is 30 nm to 50 nm.

[0036] By controlling the thickness of the third dielectric layer within the above range, the structural stability of the film layer is further improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0038] Figure 1 It is a schematic diagram of the cross-sectional structure of double silver-coated glass in an embodiment of the present utility model.

[0039] Description of Figure Numbers:

[0040]

[0041]

[0042] The realization of the purpose, functional features and advantages of the utility model will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0043] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0044] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back...) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0045] In addition, the descriptions of "first", "second", etc. in the present utility model are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, "and / or" in the full text includes three solutions. Taking A and / or B as an example, it includes technical solution A, technical solution B, and technical solution that satisfies both A and B; in addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in this field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present utility model.

[0046] The "range" disclosed in the utility model is defined in the form of a lower limit and an upper limit, and a given range is defined by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundaries of a particular range. The range defined in this way can be inclusive or exclusive of end values, and can be arbitrarily combined, that is, any lower limit can be combined with any upper limit to form a range. For example, if a range of 60-120 and 80-110 is listed for a particular parameter, it is understood that the range of 60-110 and 80-120 is also expected. In addition, if the minimum range values ​​1 and 2 are listed, and if the maximum range values ​​3, 4 and 5 are listed, the following ranges can all be expected: 1-3, 1-4, 1-5, 2-3, 2-4 and 2-5. In the utility model, unless otherwise specified, the numerical range "ab" represents an abbreviation of any real number combination between a and b, wherein a and b are both real numbers. For example, the numerical range "0-5" means that all real numbers between "0-5" are listed in this document, and "0-5" is just an abbreviation of these numerical combinations. In addition, when a parameter is expressed as an integer ≥ 2, it is equivalent to disclosing that the parameter is, for example, an integer of 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc.

[0047] If not otherwise specified, all embodiments and optional embodiments of the present invention can be combined with each other to form a new technical solution.

[0048] Unless otherwise specified, all technical features and optional technical features of the utility model can be combined with each other to form a new technical solution.

[0049] The double silver coated glass proposed in the utility model is as follows Figure 1 As shown, from bottom to top, it includes: a glass base 100, a first dielectric layer 101, a first functional layer 102, a first protective layer 103, a second dielectric layer 104, a second functional layer 105, a second protective layer 106 and a third dielectric layer 107;

[0050] The first functional layer 102 is a silver layer;

[0051] The second functional layer 105 is a silver layer;

[0052] The first protection layer 103 is a titanium nitride layer.

[0053] In the utility model, the film structure of the double silver coated glass is designed, thereby improving the color stability of the coated glass and reducing the small angle chromatic aberration (30°~60°); the first functional layer 102 is a silver layer, which uses the low radiation performance of silver to reduce the emissivity of the coated glass, and filters the sunlight into a cold light source, thereby improving the energy saving effect; and further improving the transmission performance. The first protective layer 103 is a titanium nitride layer, which has a high refractive index and stable chemical properties. It has a strong bonding force with the adjacent film layer, and can effectively improve the transmission color of the coated glass, making the coated glass more "neutral", and the scenery that the user sees from the indoor through the coated glass can be closer to nature. In addition, the titanium nitride layer also plays a good protective role for the first functional layer 102. The second functional layer 105 is a silver layer, which uses the low radiation performance of silver to reduce the emissivity of the coated glass, and filters the sunlight into a cold light source, thereby improving the energy saving effect; and further improving the transmission performance.

[0054] In some embodiments, the thickness of the first dielectric layer 101 is 25 nm to 43 nm.

[0055] By controlling the thickness of the first dielectric layer 101 within the above range, the structural stability of the film layer is further improved.

[0056] In some embodiments, the first dielectric layer 101 includes a silicon oxide layer, a silicon nitride layer, and a zinc aluminum oxide layer.

[0057] The silicon oxide layer has a high refractive index, thereby improving the light transmittance of the film layer; and the material is similar to the glass substrate 100 , so it can be better combined with the glass substrate 100 .

[0058] The silicon nitride layer can block sodium ions and potassium ions in the glass substrate 100 from migrating into the first functional layer 102 , thereby affecting the performance of the first functional layer 102 .

[0059] The surface structure of the zinc aluminum oxide layer is smooth and does not form a columnar structure; therefore, it can be used as a seed layer for the first functional layer 102 to make the first functional layer 102 grow uniformly and achieve uniform adhesion of the first functional layer 102, thereby further improving the conductivity of the first functional layer 102.

[0060] In some embodiments, the silicon oxide layer in the first dielectric layer 101 is a SiOx layer.

[0061] In some embodiments, the silicon nitride layer in the first dielectric layer 101 is a SiNx layer.

[0062] In some embodiments, the zinc aluminum oxide layer in the first dielectric layer 101 is a ZnAlOx layer.

[0063] In some embodiments, the first dielectric layer 101 is composed of a silicon oxide layer, a silicon nitride layer, and a zinc aluminum oxide layer in sequence.

[0064] In some embodiments, the silicon oxide layer in the first dielectric layer 101 is in contact with the glass substrate 100 .

[0065] The refractive index of the silicon oxide layer is high and close to that of glass. Using the silicon oxide layer as the bottom layer can not only improve the light transmittance, but also better combine with the glass base surface 100; the silicon nitride layer is used as the bottom layer to prevent Na in the glass base surface 100 from + , K + Plasma diffusion migrates into the film layer to destroy the first functional layer 102; the zinc-aluminum oxide layer can serve as an adhesion layer for the first functional layer 102 (Ag layer), and its role is to serve as a seed layer to make the Ag layer grow evenly on its surface. Moreover, the surface structure of the zinc-aluminum oxide layer is smooth and does not form a columnar structure, so that the Ag layer can be evenly attached to its surface, thereby improving the conductivity of the first functional layer 102 and the stability of the film structure. Through the combination of the above film layers, the performance of the film layer is further improved.

[0066] In some embodiments, the thickness of the silicon oxide layer in the first dielectric layer 101 is 5 nm to 10 nm.

[0067] In some embodiments, the thickness of the silicon nitride layer in the first dielectric layer 101 is 10 nm to 18 nm.

[0068] In some embodiments, the thickness of the zinc aluminum oxide layer in the first dielectric layer 101 is 10 nm to 15 nm.

[0069] In some embodiments, the titanium nitride layer is a TiNx layer.

[0070] In some embodiments, the thickness of the first protection layer 103 is 6.5 nm to 8 nm.

[0071] Controlling the thickness of the first protective layer 103 within the above range is beneficial to further improve the protective effect.

[0072] In some embodiments, the second dielectric layer 104 includes an aluminum-doped zinc oxide layer, a silicon nitride layer, a zinc-tin oxide layer, and a zinc-aluminum oxide layer.

[0073] The film structure of the aluminum-doped zinc oxide layer is uniform and dense, which can further improve the stability of the film structure.

[0074] The silicon nitride layer has high hardness and excellent wear resistance, which is beneficial to improving the mechanical properties of the film layer.

[0075] The zinc-tin oxide layer and the zinc-aluminum oxide layer have a dense film structure and can also adjust the reflectivity of the film to further reduce small-angle discoloration.

[0076] In some embodiments, the aluminum-doped zinc oxide layer in the second dielectric layer 104 is an AZO layer.

[0077] In some embodiments, the silicon nitride layer in the second dielectric layer 104 is a SiNx layer.

[0078] In some embodiments, the zinc tin oxide layer in the second dielectric layer 104 is a ZnSnOx layer.

[0079] In some embodiments, the zinc aluminum oxide layer in the second dielectric layer 104 is a ZnAlOx layer.

[0080] In some embodiments, the second dielectric layer 104 is composed of an aluminum-doped zinc oxide layer, a silicon nitride layer, a zinc-tin oxide layer, and a zinc-aluminum oxide layer in sequence.

[0081] In some embodiments, the aluminum-doped zinc oxide layer in the second dielectric layer 104 is in contact with the first protective layer 103 .

[0082] The zinc aluminum oxide layer is plated by ceramic targets fired with ZnOx and AlOx. The film is uniform and dense, which can improve the stability of the film structure. The ZnSnOx layer and the ZnAlOx layer are used as dielectric layers to adjust the color value of the double silver coated glass. The film can also adjust the reflectivity of the film, better adjust the polarization of light, and reduce small angle discoloration. The combination of the above film layers further improves the performance of the film.

[0083] In some embodiments, the thickness of the aluminum-doped zinc oxide layer in the second dielectric layer 104 is 5 nm to 10 nm.

[0084] In some embodiments, the thickness of the silicon nitride layer in the second dielectric layer 104 is 20 nm to 30 nm.

[0085] In some embodiments, the thickness of the zinc tin oxide layer in the second dielectric layer 104 is 15 nm to 25 nm.

[0086] In some embodiments, the thickness of the zinc aluminum oxide layer in the second dielectric layer 104 is 15 nm to 25 nm.

[0087] In some embodiments, the thickness of the second dielectric layer 104 is 55 nm to 80 nm.

[0088] In some embodiments, the thickness of the second dielectric layer 104 is 60 nm to 75 nm.

[0089] By controlling the thickness of the second dielectric layer 104 within the above range, the structural stability of the film layer is further improved; the polarization of the film layer can also be further controlled, thereby reducing small-angle discoloration.

[0090] In some embodiments, the thickness of the first functional layer 102 is 5 nm to 8 nm.

[0091] In some embodiments, the thickness of the first functional layer 102 is 6 nm to 8 nm.

[0092] In some embodiments, the thickness of the second functional layer 105 is 9 nm to 11 nm.

[0093] By controlling the thickness of the first functional layer 102 and the second functional layer 105 , the energy-saving effect of the coated glass can be further improved.

[0094] In some embodiments, the second protection layer 106 is a nickel-chromium layer.

[0095] The nickel-chromium layer can protect the second protective layer 106 (Ag layer) from being oxidized and improve the product's transmittance color, so that the user will not see "distortion" when viewing the scenery through the double-silver-coated glass.

[0096] In some embodiments, the nickel-chromium layer is a NiCr layer.

[0097] In some embodiments, the nickel-chromium layer has a thickness of 2 nm to 3 nm.

[0098] In some embodiments, the nickel-chromium layer has a thickness of 2.1 nm to 2.8 nm.

[0099] In some embodiments, the third dielectric layer 107 includes at least one of an aluminum-doped zinc oxide layer, a silicon nitride layer, and a silicon-zirconium alloy layer.

[0100] The aluminum-doped zinc oxide layer has a strong bonding ability with the adjacent film layer, thereby further improving the stability of the film layer.

[0101] The silicon nitride layer has high hardness and excellent wear resistance, which is beneficial to further improve the mechanical properties and scratch resistance of the film layer.

[0102] The silicon-zirconium alloy layer has high hardness, strong corrosion resistance and strong oxidation resistance, which is beneficial to further improve the mechanical properties and stability of the film layer.

[0103] In some embodiments, the aluminum-doped zinc oxide layer in the third dielectric layer 107 is an AZO layer.

[0104] In some embodiments, the silicon nitride layer in the third dielectric layer 107 is a SiNx layer.

[0105] In some embodiments, the silicon-zirconium alloy layer in the third dielectric layer 107 is a SiZr layer.

[0106] In some embodiments, the third dielectric layer 107 is composed of an aluminum-doped zinc oxide layer, a silicon nitride layer, and a silicon-zirconium alloy layer in sequence.

[0107] In some embodiments, the aluminum-doped zinc oxide layer in the third dielectric layer 107 is in contact with the second protective layer 106 .

[0108] The aluminum-doped zinc oxide layer improves the bonding force between the film layers and the stability of the overall film structure; silicon nitride has high hardness and strong wear resistance, thereby improving the mechanical properties and scratch resistance of the film layer, making the coated product less susceptible to scratches; the silicon-zirconium alloy layer has higher hardness and stronger corrosion and oxidation resistance; through the combination of the above film layers, the performance of the film layer is further improved.

[0109] In some embodiments, the thickness of the aluminum-doped zinc oxide layer in the third dielectric layer 107 is 5 nm to 10 nm.

[0110] In some embodiments, the thickness of the silicon nitride layer in the third dielectric layer 107 is 20 nm to 30 nm.

[0111] In some embodiments, the thickness of the silicon-zirconium alloy layer in the third dielectric layer 107 is 5 nm to 10 nm.

[0112] In some embodiments, the thickness of the third dielectric layer 107 is 30 nm to 50 nm.

[0113] By controlling the thickness of the third dielectric layer 107 within the above range, the structural stability of the film layer is further improved.

[0114] In some embodiments, the visible light reflectivity of the double-silver coated glass is 5% to 9%.

[0115] In some embodiments, the visible light transmittance of the double-silver coated glass is 65% to 70%.

[0116] In some embodiments, the glass surface color a* value of the double-silver coated glass is -1.0 to 0.5.

[0117] In some embodiments, the b* value of the glass surface color of the double-silver coated glass is -2.8 to -1.0.

[0118] In some embodiments, at a small angle, the a* value of the double-silver coated glass is -1.5 to 0.0.

[0119] In some embodiments, at a small angle, the b* value of the double-silver coated glass is -2.5 to -0.5.

[0120] In some embodiments, the transmittance color a* value of the double-silver coated glass is -2.5 to -0.5.

[0121] In some embodiments, the transmittance color b* value of the double-silver coated glass is -1.0 to 1.0.

[0122] In some embodiments, the method for preparing the double silver coated glass comprises the following steps:

[0123] A first dielectric layer 101 , a first functional layer, a first protective layer, a second dielectric layer, a second functional layer, a second protective layer and a third dielectric protective layer are sequentially sputtered on the glass substrate 100 .

[0124] In some embodiments, the glass substrate 100 is cleaned, polished and dried.

[0125] In some embodiments, the sputtering is magnetron sputtering.

[0126] In some embodiments, the target materials used for the magnetron sputtering cathode are:

[0127] Silicon aluminum target (used to form silicon oxide and silicon nitride), zinc aluminum target, silver target, titanium target, AZO metal oxide target, silicon aluminum target, zinc tin target, zinc aluminum target, silver target, nickel chromium target, AZO metal oxide target, silicon aluminum target (used to form silicon nitride), silicon zirconium target.

[0128] In some embodiments, the AZO metal oxide target is formed by sintering ZnOx and AlOx.

[0129] AZO metal oxide target is a metal oxide target with ceramic function. The purity of the target material is ≥99.95%. The plated AZO film is uniform and dense. The denser the film, the better the performance.

[0130] In some embodiments, the silicon-aluminum target is a silicon-aluminum alloy target with a silicon-aluminum weight ratio of 9:1.

[0131] In some embodiments, the zinc-aluminum target is a zinc-aluminum alloy target with a zinc-aluminum weight ratio of 98:2.

[0132] In some embodiments, the zinc-tin target is a zinc-tin alloy target with a zinc-tin weight ratio of 50:50.

[0133] In some embodiments, the silver target has a silver purity of 99.99%.

[0134] In some embodiments, the nickel-chromium target is a nickel-chromium alloy target with a nickel-chromium weight ratio of 8:2.

[0135] In some embodiments, the titanium target is a rotating titanium target.

[0136] In some embodiments, the silver target is a planar target.

[0137] In some embodiments, the nickel-chromium target is a planar target.

[0138] In some embodiments, power control is used during the magnetron sputtering.

[0139] In some embodiments, the sputtering power of the silicon aluminum target is 0 kW to 60 kW.

[0140] In some embodiments, the volume ratio of argon gas to nitrogen gas during the sputtering process of the silicon aluminum target is 1:0.9-1.1 (when silicon nitride is deposited).

[0141] In some embodiments, the volume ratio of argon gas to nitrogen gas during the sputtering process of the silicon aluminum target is 1:1.

[0142] In some embodiments, the sputtering pressure of the silicon aluminum target is 1*10 -3 mbar~4*10 -3 mbar.

[0143] In some embodiments, the sputtering power of the zinc-aluminum target is 0 kW to 50 kW.

[0144] In some embodiments, the volume ratio of argon to oxygen during the sputtering process of the zinc-aluminum target is 1:1.5-1.7.

[0145] In some embodiments, the volume ratio of argon to oxygen during the sputtering process of the zinc-aluminum target is 1:1.6.

[0146] In some embodiments, the sputtering gas pressure of the zinc-aluminum target is 1*10 -3 mbar~4*10 -3 mbar.

[0147] In some embodiments, the sputtering power of the zinc-tin target is 0 kW to 50 kW.

[0148] In some embodiments, the volume ratio of argon gas to nitrogen gas during the sputtering process of the zinc-tin target is 1:1.5-1.7.

[0149] In some embodiments, the volume ratio of argon to oxygen during the sputtering process of the zinc-tin target is 1:1.6.

[0150] In some embodiments, the sputtering pressure of the zinc-tin target is 1*10 -3 mbar~4*10 -3 mbar.

[0151] In some embodiments, the sputtering power of the silver target is 0 kW to 20 kW.

[0152] In some embodiments, the sputtering power of the NiCr target is 0 kW to 20 kW.

[0153] In some embodiments, the sputtering power of the AZO ceramic target is 0 kW to 20 kW.

[0154] In some embodiments, argon gas is used during the sputtering process of the AZO ceramic target.

[0155] In some embodiments, the sputtering gas pressure of the AZO ceramic target is 1*10 -3 mbar~4*10 -3 mbar.

[0156] In some embodiments, the sputtering power of the titanium target is 0 kW to 35 kW.

[0157] In some embodiments, the volume ratio of argon gas to nitrogen gas during the sputtering process of the titanium target is 50:0.9-1.71.

[0158] In some embodiments, the volume ratio of argon gas to nitrogen gas during the sputtering process of the titanium target is 50:1.

[0159] In some embodiments, the sputtering gas pressure of the titanium target is 1*10 -3 mbar~4*10 -3 mbar.

[0160] During magnetron sputtering, power control is used to ensure that the sputtering is stable and the target material is not damaged; by controlling the sputtering pressure, the mean free path of the molecules is relatively stable, the target sputtering is more stable, and the film layer is denser.

[0161] Example 1

[0162] This embodiment is a double silver coated glass. Figure 1 As shown, it consists of the following layers in sequence:

[0163] Glass substrate 100, first dielectric layer 101 (35 nm thick), first functional layer 102 (Ag layer, 6.05 nm thick), first protective layer 103 (TiNx layer, 6.5 nm thick), second dielectric layer 104 (74 nm thick), second functional layer 105 (Ag layer, 9.6 nm thick), second protective layer 106 (NiCr layer, 2.7 nm thick) and third dielectric layer 107 (45 nm thick);

[0164] The first dielectric layer 101 is composed of a SiOx layer (5 nm thick, the layer is in contact with the glass base surface 100), a SiNx layer (18 nm thick), and a ZnAlOx layer (12 nm thick);

[0165] The second dielectric layer 104 is composed of an AZO layer (with a thickness of 8 nm, which is in contact with the first protective layer 103), a SiNx layer (with a thickness of 28 nm), a ZnSnOx layer (with a thickness of 15 nm), and a ZnAlOx layer (with a thickness of 23 nm) in sequence;

[0166] The third dielectric layer 107 is composed of an AZO layer (with a thickness of 8 nm, which is in contact with the second protective layer 106), a SiNx layer (with a thickness of 30 nm), and a SiZr layer (with a thickness of 7 nm) in sequence.

[0167] In this embodiment, the surface emissivity of the glass base surface 100 is 0.06, and the heat transfer coefficient K value (1.70 W / m 2 ~1.80W / m 2 ), shading coefficient Sc (0.46~0.50).

[0168] Example 2

[0169] This embodiment is a double silver-coated glass. The film material in this embodiment is the same as that in Embodiment 1. The film thickness is shown in Table 1.

[0170] Example 3

[0171] This embodiment is a double silver-coated glass. The film material in this embodiment is the same as that in Embodiment 1. The film thickness is shown in Table 1.

[0172] Table 1: Film structure and thickness of double silver coated glass in Examples 1 to 3 of the present invention

[0173]

[0174]

[0175] The preparation method of the double silver coated glass in Examples 1 to 3 of this experimental novelty is composed of the following steps:

[0176] A first dielectric layer, a first functional layer, a first protective layer, a second dielectric layer, a second functional layer, a second protective layer and a third dielectric protective layer are sequentially sputtered on a glass substrate (6 mm float glass substrate) using vacuum magnetron sputtering technology.

[0177] The double-silver coated glass in Examples 1 to 3 was tested and analyzed by a professional desktop spectrophotometer Datacolor DC850 optical instrument. The single-piece color parameters (Table 2) showed that the outdoor observation was low-reflection blue-gray. The color value test results were expressed in the Lab color space (English: Lab color space), which is a color-opposition space, where:

[0178] a*(Green-Red Axis): Indicates the red-green color of the color, ranging from -128 to +127, where -128 represents green and +127 represents red.

[0179] b* (Blue-Yellow Axis): Indicates the yellow-blue degree of the color, with a value range from -128 to +127, where -128 represents blue and +127 represents yellow.

[0180] Table 2: Color values ​​of single piece of double silver coated glass in Examples 1 to 3

[0181]

[0182] The double silver coated glass in Examples 1 to 3 was processed into insulating glass (6 mm (double silver coated glass) + 12 mm A (thickness of the spacer layer) + 6 mm (double silver coated glass)), and the thermal properties were tested by a PerkinElmer Lambda950 UV-visible spectrophotometer. The test results are shown in Table 3.

[0183] Table 3: Thermal properties of insulating glass made from double silver coated glass corresponding to Examples 1 to 3

[0184]

[0185] It can be seen from Table 3 that the insulating glass prepared in Examples 1 to 3 has the characteristics of low shading coefficient, low heat transfer coefficient U value and low solar thermal radiation transmittance.

[0186] The advantages of this embodiment are as follows:

[0187] 1. In this embodiment, the raw materials for preparing the double silver-coated glass only need to use conventional target materials, and the preparation method is to use a magnetron sputtering process. The production process has low cost, controllable process and high stability.

[0188] 2. The double silver-coated glass film system in the embodiment has a reasonable structure, excellent bonding strength and good heat insulation performance. The film layer structure is stable, not easy to oxidize, has strong processability and excellent energy-saving performance.

[0189] 3. In this embodiment, the surface emissivity of the glass base is as low as 0.06, and the heat transfer coefficient K value (1.70W / m 2 ~1.80W / m 2 ), shading coefficient Sc (0.46 ~ 0.50), by adding TiNx layer, increasing the thickness of the first dielectric layer, and reducing the overall thickness of the second dielectric layer, the problem of obvious "discoloration" at small angles caused by polarized light can be further reduced.

[0190] 4. In this embodiment, the visible light reflectivity of the double silver coated glass is 5% to 9%, the visible light transmittance is 65% to 70%, the color value of the glass surface is controlled within -1.0≤a*≤0.5, -2.8≤b*≤-1.0, the color of the small-angle glass surface is controlled within -1.5≤a*≤0.0, -2.5≤b*≤-0.5, and the color value of the transmitted color is controlled within -2.5≤a*≤-0.5, -1.0≤b*≤1.0.

[0191] 5. The color of the glass surface and small-angle glass of the utility model is between -3 and 0.5 according to the color value a* and b* of the glass surface and small-angle color value at the fourth point. There is no color change from the front to the small angle when observed outdoors. The overall color tends to be gray or blue-gray when observed at different angles.

[0192] The above description is only a preferred embodiment of the utility model, and does not limit the patent scope of the utility model. All equivalent structural changes made by using the contents of the utility model specification and drawings under the utility model concept, or directly / indirectly used in other related technical fields are included in the patent protection scope of the utility model.

Claims

1. A double silver coated glass, characterized in that: The a* value of the glass surface color of the double silver coated glass is -1.0 to 0.5, and the b* value of the glass surface color is -2.8 to -1.

0. At a small angle, the a* value of the double silver coated glass is -1.5 to 0.0, and the b* value is -2.5 to -0.5; The double silver coated glass comprises from bottom to top: a glass base surface, a first dielectric layer, a first functional layer, a first protective layer, a second dielectric layer, a second functional layer, a second protective layer and a third dielectric layer; The first functional layer is a silver layer; The second functional layer is a silver layer; The first dielectric layer includes: a silicon oxide layer, a silicon nitride layer and a zinc aluminum oxide layer arranged in sequence; The second dielectric layer includes: an aluminum-doped zinc oxide layer, a silicon nitride layer, a zinc-tin oxide layer and a zinc-aluminum oxide layer arranged in sequence; The third dielectric layer includes: an aluminum-doped zinc oxide layer, a silicon nitride layer and a silicon-zirconium alloy layer arranged in sequence; The first protective layer is a titanium nitride layer.

2. The double silver coated glass according to claim 1, characterized in that: The thickness of the first dielectric layer is 25 nm to 43 nm.

3. The double silver coated glass according to claim 1, characterized in that: The thickness of the first protective layer is 6.5 nm to 8 nm.

4. The double silver coated glass according to claim 1, characterized in that: The thickness of the second dielectric layer is 55 nm to 80 nm.

5. The double silver coated glass according to claim 1, characterized in that: The thickness of the first functional layer is 5nm-8nm.

6. The double silver coated glass according to claim 1, characterized in that: The thickness of the second functional layer is 9 nm to 11 nm.

7. The double silver coated glass according to claim 1, characterized in that: The thickness of the third dielectric layer is 30nm-50nm.

Citation Information

Cited By