Connecting structure capable of visually detecting welding quality and connecting piece
By designing a connection structure with tin holes and solder resist layer on the battery module acquisition integration and FFC, the problem of difficulty in visually detecting the solder quality at the welding position is solved, and convenient visual inspection is achieved and detection cost is reduced.
Patent Information
- Application Number
- CN202420776912.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-15
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-15
AI Technical Summary
In the prior art, it is difficult to judge the welding position of the metal connecting sheet on the battery module acquisition integrated part and the FFC through visual inspection, and it is necessary to rely on auxiliary equipment such as ultrasonic equipment for inspection, resulting in a high detection cost.
A connecting structure including a conductor layer and an insulating layer is designed, with a front welding area, a back welding area and a tin hole. There are solder resist layers on both sides of the front welding area. Tin can only flow into the back welding area through the tin hole. Form tin crawling for visual inspection.
The solder quality is visually detected, which reduces dependence on special equipment and reduces equipment procurement costs.
Smart Images

Figure CN222072200U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of metal connecting pieces, in particular to a connecting piece used on a battery module collection integrated component (CCS) or FFC and a connecting structure used by the connecting piece, the welding quality of which can be visually detected. Background Art
[0002] Battery module collection assembly (CCS); FFC refers to flexible flat cable, which was previously widely used in various electronic products as connecting cables; it is currently also widely used in power batteries and new energy vehicles. At present, in order to achieve the connection of a large number of electrical components, battery module collection assembly and FFC need to be welded or set with a number of metal connecting pieces by other means. When the metal connecting pieces are fixed on the two by welding, the inspection of soldering quality is a necessary process. Because the welding position is not visible to the naked eye, it is difficult to judge the soldering quality by visual inspection, and can only be inspected by auxiliary equipment such as ultrasonic equipment, thereby increasing the inspection cost. Utility Model Content
[0003] In order to overcome the deficiencies of the prior art, one of the purposes of the utility model is to provide a connection structure that can visually detect welding quality.
[0004] The second purpose is to provide a connecting piece using the above-mentioned connecting structure.
[0005] The technical solution for the first purpose is: a connection structure that can visually detect the welding quality, including a main body, which includes a conductor layer, and an insulating layer arranged on its two surfaces, one end of the conductor layer is exposed, a front welding area is provided on the front side of one end of the main body, and a back welding area is provided on the back side of the end of the main body, and also includes a plurality of tin-penetrating holes that penetrate the front welding area and the back welding area, and solder resist layers are provided on both sides of the front welding area.
[0006] Preferably, the front welding area includes a plurality of mutually parallel front welding pads, and the back welding area includes a plurality of back welding pads and the number of the back welding pads is the same as that of the front welding pads; a back welding pad is provided on the back side of each front welding pad.
[0007] At least one tin-penetrating hole is provided in the integral structure formed by each front soldering pad and the back soldering pad on the back side.
[0008] The length of the front pad is smaller than the length of the back pad disposed on the back side thereof.
[0009] There are three tin-through holes arranged in the overall structure.
[0010] The technical solution for the second purpose is: a connecting piece, which includes the connecting structure that can visually detect welding quality.
[0011] Technical effect: With the connection structure of the utility model, when welding, the back welding area contacts the welding surface on the FFC or CCS. Since there are solder resist layers on both sides of the front welding area, the molten tin is restricted from flowing to the sides of the front welding area. The tin can only flow in through the tin holes to fill the space between the back welding area and the welding surface. After filling, since there are no solder resist layers on both sides of the back welding area, the molten tin overflows to the outside of both sides of the back welding area, forming tin creeping, which is convenient for observation. When welding, the connecting piece with this structure is convenient for visually detecting the soldering quality. Compared with the prior art, the utility model is conducive to visually detecting the soldering quality, without the need for special equipment for detection, thereby reducing the equipment procurement cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 This is a front view of a connecting piece according to an embodiment of the utility model;
[0013] Figure 2 This is a schematic diagram of the back side of the connecting piece of an embodiment of the utility model;
[0014] Figure 3 A schematic diagram of the welding process of the connecting piece of an embodiment of the utility model;
[0015] Figure 4 for Figure 3 A partial enlarged view of
[0016] Figure 5 It is a schematic diagram of the welding effect of the connecting piece of the embodiment of the utility model.
[0017] Figure numerals: conductor layer-1, insulating layer-2, front welding area-3, front welding pad-301, back welding area-4, back welding pad-401, tin-through hole-5, solder resist layer-6, welding surface-7, fuse part-8, tin creeping-9, tin-10. DETAILED DESCRIPTION
[0018] In order to enable those skilled in the art to better understand the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and implementation methods.
[0019] like Figure 1-2As shown, an embodiment of the utility model provides a connection structure that can visually detect welding quality, which is used in the field of CCS or FFC, especially on the metal connecting plates arranged on the two; it includes a main body, the main body includes a conductor layer 1, and an insulating layer 2 arranged on its two surfaces, that is, an insulating layer is provided on each of the two surfaces of the conductor layer 1; one end of the conductor layer 1 is exposed, a front welding area 3 is provided on the front side of one end of the main body, and a back welding area 4 is provided on the back side of the end of the main body, and also includes a plurality of tin-penetrating holes 5 that pass through the front welding area and the back welding area, and solder resist layers 6 are provided on both sides of the front welding area. Here, a fuse 8 is provided in the conductor layer 1. As shown Figure 1-2 As shown, specifically, the front welding area 3 includes a plurality of mutually parallel front welding pads 301, and the back welding area 4 includes a plurality of back welding pads 401 and the number thereof is consistent with the front welding pads; a back welding pad 401 is provided on the back side of each front welding pad 301, that is, the front welding pad 301 is actually integrally formed with the back welding pad on its back side.
[0020] The front welding area 3 and the back welding area 4 described here actually correspond to the two surfaces of the conductor layer 1. Holes are opened on the insulating layer 2 arranged on the two surfaces of the conductor layer 1 according to the circuit design, so that the conductor at the opening position is exposed, and a front welding area including a plurality of front welding pads 301 is formed on the front side of the conductor, and a back welding area including a plurality of back welding pads 401 is formed on the back side of the conductor. Therefore, the corresponding front welding pads 301 and back welding pads 401 are actually also part of the conductor, but they are located on different surfaces of the conductor respectively, so the two must be formed as one piece.
[0021] Each front solder pad 301 and the back solder pad 401 on the back thereof form an integral structure with at least one tin-penetrating hole 5. Obviously, the purpose of the tin-penetrating hole here is to allow solder to enter the space between the back soldering area 4 and the soldering surface (such as the conductor surface on the CCS or FFC) through the hole. Therefore, there is no special restriction on the number of tin-penetrating holes 5 in each integral structure, as long as it is convenient for the molten solder to fully flow during soldering so as to improve the soldering efficiency; for example, in this embodiment, three tin-penetrating holes are provided in the integral structure.
[0022] like Figure 1-2 As shown, because solder resist layers 6 are provided on both sides of the front soldering area 3, the length of the front soldering pad 301 is smaller than the length of the back soldering pad 401 provided on the back thereof; and overall, the width of the front soldering area 3 is smaller than the width of the back soldering area 4. The solder resist layers 6 here are actually insulating layers located on both sides of the front soldering area 3.
[0023] The utility model also provides a connecting piece, which adopts the above-mentioned connecting structure so as to detect the soldering quality when the connecting piece is welded to the CCS or FFC.
[0024] In summary, if Figure 3-5 As shown, with the connection structure of the present invention, during welding, the back welding area 4 is in contact with the welding surface 7. Since there are solder resist layers 6 on both sides of the front welding area 3, the molten tin is restricted from flowing to the sides of the front pad. The tin 10 can only flow in through the tin holes 5 to fill the space between the back welding area 4 and the welding surface 7. After the space is filled, since there are no solder resist layers 6 on both sides of the back welding area 4, the molten tin overflows to the outside of both sides of the back pad, forming tin creeping 9, which is convenient for observation. When welding, the connecting piece with the present structure is convenient for visually detecting the soldering quality.
[0025] In the above description, it should be noted that the terms "installed", "connected", "connected" and other corresponding terms should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal connection of two components; "provided in" should be understood as "installed in, set in", including fixed installation, movable installation and other installation methods.
[0026] Obviously, the embodiments described above are only some embodiments of the utility model, not all embodiments. The preferred embodiments of the utility model are given in the drawings, but they do not limit the patent scope of the utility model. The utility model can be implemented in many different forms. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the utility model more thorough and comprehensive. Any equivalent structure made by using the contents of the utility model specification and drawings, directly or indirectly used in other related technical fields, is also within the scope of protection of the utility model patent.
Claims
1. A connection structure capable of visually inspecting welding quality, comprising a body, which comprises a conductor layer (1), and insulating layers (2) arranged on two surfaces thereof, wherein one end of the conductor layer is exposed, characterized in that: A front welding area (3) is provided on the front side of one end of the main body, a back welding area (4) is provided on the back side of the end of the main body, and a plurality of tin-penetrating holes (5) penetrating the front welding area and the back welding area are also provided, and solder resist layers (6) are provided on both sides of the front welding area.
2. A connection structure capable of visually inspecting welding quality as claimed in claim 1, characterized in that: The front welding area (3) comprises a plurality of mutually parallel front welding pads (301), and the back welding area (4) comprises a plurality of back welding pads (401) whose number is the same as that of the front welding pads; a back welding pad (401) is provided on the back of each front welding pad (301).
3. A connection structure capable of visually inspecting welding quality as claimed in claim 2, characterized in that: At least one tin-penetrating hole (5) is provided in the overall structure formed by each front soldering pad (301) and the back soldering pad (401) on the back side thereof.
4. A connection structure capable of visually inspecting welding quality as claimed in claim 2, characterized in that: The length of the front soldering pad (301) is smaller than the length of the back soldering pad (401) disposed on the back side thereof.
5. A connection structure capable of visually inspecting welding quality as claimed in claim 3, characterized in that: There are three tin-penetrating holes (5) arranged in the overall structure.