Polyimide film with low thermal expansion coefficient

By introducing interlayer components and protective film layers into the polyimide film, the problem of polyimide film being easily broken on soft circuit boards is solved, reducing the thermal expansion coefficient and improving puncture resistance, enhancing the insulation performance and stability.

CN222080298UActive Publication Date: 2024-11-29JIANGYIN JUNYOU ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420598597.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-27
Publication Date
2024-11-29
Estimated Expiration
2034-03-27

AI Technical Summary

Technical Problem

The polyimide film with low thermal expansion coefficient is easily punctured by spikes on soft circuit boards, affecting the insulation performance.

Method used

Polyimide films with a double-layer structure, interlayer components such as ceramic particle layer or glass fiber layer reduce the coefficient of thermal expansion, and protective components such as HDPE or PFA film layers on the outer surface improve puncture resistance.

Benefits of technology

Effectively reduce the thermal expansion coefficient of the polyimide film and improve its puncture resistance and acid-base protection functions, and improve its use stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222080298U_ABST
    Figure CN222080298U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of films, in particular to a low-thermal-expansion-coefficient polyimide film which comprises polyimide film bodies, the polyimide film bodies are of a double-layer structure, and an interlayer assembly for reducing the thermal expansion coefficient of the polyimide film bodies is arranged between the two layers of polyimide film bodies. The puncture-resistant polyimide film has the beneficial effects that the thermal expansion coefficient of the polyimide film body can be reduced, and the puncture-resistant and acid and alkali-resistant protection functions can be performed on the polyimide film body; the stability in the use period is facilitated, and the practicability is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of films, in particular to a polyimide film with a low thermal expansion coefficient. Background Art

[0002] Polyimide refers to a class of polymer materials whose molecular chains contain imide rings. It has excellent properties such as high and low temperature resistance, flame retardancy, and radiation resistance. Its products include films, fibers, resins, foams, composite materials, etc., and are widely used in national defense, military industry, microelectronics, vehicles, chemical industry and other fields. Among them, film materials, as one of the earliest commodities of polyimide, are used in the insulation field.

[0003] During the actual production process, our company discovered that low thermal expansion coefficient polyimide film is not resistant to puncture when used on flexible circuit boards. After installation, it is easily punctured by nearby solder joints or copper wire ends and other sharp objects, which affects its insulation performance and needs further improvement.

[0004] Therefore, it is necessary to invent a polyimide film with a low thermal expansion coefficient. Utility Model Content

[0005] To this end, the utility model provides a low thermal expansion coefficient polyimide film to solve the problem that the low thermal expansion coefficient polyimide film is not resistant to puncture when used on a flexible circuit board. After installation, it is easily punctured by sharp objects such as nearby solder joints or copper wire ends, affecting its insulation performance.

[0006] In order to achieve the above-mentioned purpose, the utility model provides the following technical solutions: a low thermal expansion coefficient polyimide film, comprising a polyimide film body, the polyimide film body is a double-layer structure, an interlayer component for reducing the thermal expansion coefficient of the polyimide film body is arranged between the two layers of the polyimide film body, and a protective component for improving the puncture resistance of the polyimide film body is arranged on the outer surface of the polyimide film body.

[0007] Preferably, the sandwich component is a ceramic particle layer, the ceramic particle layer is coated between two layers of polyimide film bodies, and the thickness of the ceramic particle layer is 5-8 μm.

[0008] Preferably, the sandwich component is a glass fiber layer, the glass fiber layer is coated between two layers of polyimide film bodies, and the thickness of the glass fiber layer is 2-5 μm.

[0009] Preferably, the protective component is a HDPE film layer, the number of the HDPE film layers is two, the inner surfaces of the two HDPE film layers are respectively bonded to the outer surfaces of the two layers of polyimide film bodies, and the thickness of the HDPE film layer is 20-50 μm.

[0010] Preferably, the protective component is a PFA film layer, the number of the PFA film layers is two, the inner surfaces of the two PFA film layers are respectively bonded to the outer surfaces of the two polyimide film bodies, and the thickness of the PFA film layer is 20-50 μm.

[0011] The beneficial effects of the utility model are as follows: through the coordinated use of the double-layer structure of the polyimide film body, the interlayer component and the protective component, the thermal expansion coefficient of the polyimide film body can be reduced, and the polyimide film body can be provided with anti-puncture and acid-alkali protection functions, which is beneficial to its stability during use and greatly improves its practicality. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 A structural stereogram of the first embodiment provided by the utility model;

[0013] Figure 2 A structural cross-sectional view of the first embodiment provided by the utility model;

[0014] Figure 3 A structural stereogram of the second embodiment provided by the utility model;

[0015] Figure 4 A structural cross-sectional view of the second embodiment provided by the utility model;

[0016] Figure 5 A structural stereogram of the third embodiment provided by the utility model;

[0017] Figure 6 A structural cross-sectional view of the third embodiment provided by the utility model;

[0018] Figure 7 A structural stereogram of the fourth embodiment provided by the utility model;

[0019] Figure 8 This is a structural sectional view of the fourth embodiment provided by the utility model.

[0020] In the figure: 1. Polyimide film body; 2. Ceramic particle layer; 3. Glass fiber layer; 4. HDPE film layer; 5. PFA film layer. DETAILED DESCRIPTION

[0021] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.

[0022] Embodiment 1:

[0023] Please refer to the attached Figure 1-2The low thermal expansion coefficient polyimide film provided by the utility model comprises a polyimide film body 1, the polyimide film body 1 is a double-layer structure, the double-layer structure polyimide film body 1 has better insulation performance, radiation resistance and other properties, an interlayer component for reducing the thermal expansion coefficient of the polyimide film body 1 is arranged between the two layers of the polyimide film body 1, and a protective component for improving the puncture resistance of the polyimide film body 1 is arranged on the outer surface of the polyimide film body 1;

[0024] The sandwich component is a ceramic particle layer 2, which is coated between two layers of the polyimide film body 1. The thickness of the ceramic particle layer 2 is 5-8 μm. It should be noted that in the present invention, the thickness of the ceramic particle layer 2 is preferably set to 6 μm. Specifically, the ceramic particle layer 2 will not expand when heated, so under the restriction of the ceramic particle layer 2, the polyimide film body 1 will not expand too much when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1.

[0025] The protective component is a HDPE film layer 4, and there are two HDPE film layers 4. The inner surfaces of the two HDPE film layers 4 are respectively bonded to the outer surfaces of the two-layer polyimide film body 1. The thickness of the HDPE film layer 4 is 20-50μm. It should be noted that in the present invention, the thickness of the HDPE film layer 4 is preferably set to 40μm. Specifically, the HDPE film has better puncture resistance and acid and alkali corrosion resistance. Under the protective effect of the HDPE film layer 4, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0026] The use process of the utility model is as follows: first, the double-layer structure of the polyimide film body 1 has better insulation performance, radiation resistance and other properties; secondly, under the limiting effect of the ceramic particle layer 2, the polyimide film body 1 will not expand excessively when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1; finally, under the protective effect of the HDPE film layer 4, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0027] Embodiment 2:

[0028] Please refer to the attached Figure 3-4The low thermal expansion coefficient polyimide film provided by the utility model has a sandwich component of a ceramic particle layer 2, which is coated between two layers of the polyimide film body 1, and the thickness of the ceramic particle layer 2 is 5-8 μm. It should be noted that in the utility model, the thickness of the ceramic particle layer 2 is preferably set to 6 μm. Specifically, the ceramic particle layer 2 will not expand when heated, so under the limiting effect of the ceramic particle layer 2, the polyimide film body 1 will not expand too much when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1;

[0029] The protective component is a PFA film layer 5, and there are two PFA film layers 5. The inner surfaces of the two PFA film layers 5 are respectively bonded to the outer surfaces of the two polyimide film bodies 1. The thickness of the PFA film layer 5 is 20-50μm. It should be noted that in the present invention, the thickness of the PFA film layer 5 is preferably set to 40μm. Specifically, the PFA film has better puncture resistance and acid and alkali corrosion resistance. Under the protective effect of the PFA film layer 5, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0030] The use process of the utility model is as follows: first, the double-layer structure of the polyimide film body 1 has better insulation performance, radiation resistance and other properties; secondly, under the limiting effect of the ceramic particle layer 2, the polyimide film body 1 will not expand excessively when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1; finally, under the protective effect of the PFA film layer 5, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0031] Embodiment three:

[0032] Please refer to the attached Figure 5-6 The low thermal expansion coefficient polyimide film provided by the utility model has a sandwich component of a glass fiber layer 3, the glass fiber layer 3 is coated between two layers of the polyimide film body 1, and the thickness of the glass fiber layer 3 is 2-5 μm. It should be noted that in the utility model, the thickness of the glass fiber layer 3 is preferably set to 4 μm. Specifically, the glass fiber layer 3 will not expand when heated, so under the restriction of the glass fiber layer 3, the polyimide film body 1 will not expand too much when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1;

[0033] The protective component is a HDPE film layer 4, and there are two HDPE film layers 4. The inner surfaces of the two HDPE film layers 4 are respectively bonded to the outer surfaces of the two-layer polyimide film body 1. The thickness of the HDPE film layer 4 is 20-50μm. It should be noted that in the present invention, the thickness of the HDPE film layer 4 is preferably set to 40μm. Specifically, the HDPE film has better puncture resistance and acid and alkali corrosion resistance. Under the protective effect of the HDPE film layer 4, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0034] The use process of the utility model is as follows: first, the double-layer structure of the polyimide film body 1 has better insulation performance, radiation resistance and other properties; secondly, under the limiting effect of the glass fiber layer 3, the polyimide film body 1 will not expand too much when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1; finally, under the protective effect of the HDPE film layer 4, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0035] Embodiment 4:

[0036] Please refer to the attached Figure 7-8 The low thermal expansion coefficient polyimide film provided by the utility model has a sandwich component of a glass fiber layer 3, the glass fiber layer 3 is coated between two layers of the polyimide film body 1, and the thickness of the glass fiber layer 3 is 2-5 μm. It should be noted that in the utility model, the thickness of the glass fiber layer 3 is preferably set to 4 μm. Specifically, the glass fiber layer 3 will not expand when heated, so under the restriction of the glass fiber layer 3, the polyimide film body 1 will not expand too much when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1;

[0037] The protective component is a PFA film layer 5, and there are two PFA film layers 5. The inner surfaces of the two PFA film layers 5 are respectively bonded to the outer surfaces of the two polyimide film bodies 1. The thickness of the PFA film layer 5 is 20-50μm. It should be noted that in the present invention, the thickness of the PFA film layer 5 is preferably set to 40μm. Specifically, the PFA film has better puncture resistance and acid and alkali corrosion resistance. Under the protective effect of the PFA film layer 5, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0038] The use process of the utility model is as follows: first, the double-layer structure of the polyimide film body 1 has better insulation performance, radiation resistance and other properties; secondly, under the limiting effect of the glass fiber layer 3, the polyimide film body 1 will not expand excessively when heated, effectively reducing the thermal expansion coefficient of the polyimide film body 1; finally, under the protective effect of the PFA film layer 5, the polyimide film body 1 can be well protected from puncture and acid and alkali, which is beneficial to its stability during use and greatly improves its practicality.

[0039] The above is only a preferred embodiment of the utility model. Any person skilled in the art can modify the utility model by using the above technical solution or modify it into an equivalent technical solution. Therefore, any simple modification or equivalent replacement based on the technical solution of the utility model shall fall within the scope of protection claimed by the utility model.

Claims

1. A low thermal expansion coefficient polyimide film, comprising a polyimide film body (1), characterized in that: The polyimide film body (1) is a double-layer structure, and an interlayer component for reducing the thermal expansion coefficient of the polyimide film body (1) is arranged between the two layers of the polyimide film body (1), and a protective component for improving the puncture resistance of the polyimide film body (1) is arranged on the outer surface of the polyimide film body (1).

2. The low thermal expansion coefficient polyimide film according to claim 1, characterized in that: The sandwich component is a ceramic particle layer (2), which is coated between two layers of polyimide film bodies (1), and has a thickness of 5-8 μm.

3. The low thermal expansion coefficient polyimide film according to claim 1, characterized in that: The sandwich component is a glass fiber layer (3), the glass fiber layer (3) is coated between two layers of polyimide film bodies (1), and the thickness of the glass fiber layer (3) is 2-5 μm.

4. The low thermal expansion coefficient polyimide film according to claim 1, characterized in that: The protective component is a HDPE film layer (4), the number of the HDPE film layers (4) is two, the inner surfaces of the two HDPE film layers (4) are respectively bonded to the outer surfaces of the two layers of polyimide film body (1), and the thickness of the HDPE film layer (4) is 20-50 μm.

5. The low thermal expansion coefficient polyimide film according to claim 1, characterized in that: The protective component is a PFA film layer (5), the number of the PFA film layers (5) is two, the inner surfaces of the two PFA film layers (5) are respectively bonded to the outer surfaces of the two layers of polyimide film bodies (1), and the thickness of the PFA film layer (5) is 20-50 μm.