Photonic crystal fiber
By designing the photonic crystal fiber formed by prefabricated rods, using the core and cladding structure distributed with regular hexagonal lattice, the nonlinear effect and structural instability of traditional optical fibers during laser output is solved, and the large-mode field area is achieved and laser output with high beam quality.
Patent Information
- Application Number
- CN202420745488.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-11
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-04-11
AI Technical Summary
When the laser output power is increased, traditional single-mode fibers are prone to produce nonlinear effects such as four-wave mixing and Brillouin scattering, and their structure is unstable, and they are prone to deformation and structural instability during the extrusion process due to the existence of holes.
设计了一种由预制棒拉丝形成的光子晶体光纤,包括外套管、第一细棒和两层第二细棒,第二细棒沿着外套管的径向方向布置,形成正六边形点阵分布的纤芯,包层的折射率高于纤芯,第一细棒和包层的折射率相等,形成全固态结构,确保结构稳定性和大模场面积。
The optical fiber with structural stability and large-mode field area is achieved, the nonlinear effect is reduced, the beam quality and the single-mode transmission capability of laser output are improved, and the needs of higher power and higher beam quality are met.
Smart Images

Figure CN222087877U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of infrared photonic crystal optical fibers, and in particular relates to a photonic crystal optical fiber. Background Art
[0002] Mid-infrared lasers in the spectral range of 3 to 20 μm have broad application prospects in the fields of spectroscopy, remote sensing, medicine, environmental protection, laser cutting, laser radar and laser weapons. Chalcogenide glass has a large infrared transmission window. Depending on the glass components, its transmission window extends across the visible light spectrum to the mid-infrared spectrum range (0.6-25 μm). It has the characteristics of very low linear absorption and two-photon absorption, high mechanical strength, good chemical stability and low production cost, making it an ideal infrared material. Due to its simple structure, high conversion efficiency, good heat dissipation and high beam quality, fiber lasers have become one of the most concerned research topics in the laser field at home and abroad. The increase in output power and improvement in beam quality of fiber lasers have made fiber lasers widely used in fiber-optic communications, fiber-optic sensing, spectral analysis, etc., and have gradually been applied to industrial processing, space communications, medical and other application fields.
[0003] However, due to the small mode field area of traditional single-mode optical fiber, as the laser output power increases, the optical power density of the fiber core increases. When the material nonlinear threshold is exceeded, the optical fiber will produce nonlinear effects such as four-wave mixing and Brillouin scattering. In addition, it may also cause photothermal damage to the material and destroy the structure of the optical fiber. In addition, due to the presence of holes in the existing optical fiber structure, deformation and structural instability are prone to occur during the extrusion process.
[0004] Therefore, it is necessary to further improve the existing optical fiber structure. Utility Model Content
[0005] The first technical problem to be solved by the utility model is to provide a photonic crystal optical fiber with a stable structure and not easy to deform in view of the current status of the above-mentioned prior art.
[0006] The second technical problem to be solved by the utility model is to provide a photonic crystal optical fiber which increases the effective mode field area of the fundamental mode.
[0007] The technical solution adopted by the utility model to solve the first technical problem is: a photonic crystal optical fiber, which is an optical fiber formed by drawing a preform rod, wherein the preform rod includes an outer sleeve; characterized in that the preform rod also includes:
[0008] A first thin rod, which is arranged in the inner hole of the outer sleeve;
[0009] Two layers of second thin rods are arranged in the inner hole of the outer sleeve, and the two layers of second thin rods are arranged on the periphery of the first thin rod. The two layers of second thin rods are arranged in sequence from the inside to the outside along the radial direction of the outer sleeve, and each layer of second thin rods has a plurality of second thin rods arranged at intervals along the circumference of the first thin rod, and the second thin rod includes a core located inside and a cladding wrapped outside the core;
[0010] The outer sleeve, the first thin rod and all the claddings in the optical fiber are an integrated structure formed by hot melting; wherein, in each cross section along the radial section of the optical fiber, all the fiber cores are distributed in a regular hexagonal lattice.
[0011] The technical solution adopted by the utility model to solve the second technical problem is: in the photonic crystal fiber, the refractive index of the cladding is higher than the refractive index of the core, and the refractive index of the cladding is equal to the refractive index of the first thin rod, and in each radial section of the optical fiber: the distance between the centers of two adjacent cores is L, and the diameter of the core is D, and the distance L and the diameter D satisfy: the value range of the duty ratio D / L is 40% to 60%. With the above-mentioned duty ratio and optical fiber structural design, it can be seen from the distribution of the basement membrane electric field that the basement membrane electric field mode is more concentrated in the core area, thereby ensuring a large mode field area.
[0012] Preferably, in the photonic crystal optical fiber, the refractive index of all the cores is the same.
[0013] Specifically, in the photonic crystal optical fiber, in the outer layer, there are 12 fiber cores, 6 fiber cores are respectively located at corresponding corners of the regular hexagonal lattice, and the other 6 fiber cores are respectively located at the central positions of corresponding sides adjacent to the regular hexagonal lattice; in the inner layer, there are 6 fiber cores, and they are respectively located at corresponding corners of the regular hexagonal lattice.
[0014] Preferably, in the photonic crystal optical fiber, the duty cycle D / L is 50%.
[0015] Specifically, in the photonic crystal optical fiber, the diameter of the fiber core is 30-40 um, and the spacing L is 60-80 um.
[0016] Preferably, in the photonic crystal fiber, the spacing L is 70 um and the diameter D is 35 um.
[0017] Preferably, in the photonic crystal optical fiber, in the inner layer of the optical fiber, the spacing Φ between the inner edges of two cores located on the diagonal lines of the regular hexagonal lattice is 105 um.
[0018] Specifically, in the photonic crystal optical fiber, the diameters of the first thin rod and the second thin rod of the preform are equal, and are both 2 to 4 mm.
[0019] Preferably, in the photonic crystal fiber, the diameters of the first thin rod and the second thin rod are both 3 mm.
[0020] Compared with the prior art, the advantages of the present invention are: in the structure of the photonic crystal fiber, the second thin rod is located between the first thin rod and the inner circumferential wall of the outer sleeve, the second thin rod is in the form of an internal core and an external cladding, the refractive index of the internal core is lower than that of the cladding and the first thin rod, and the cladding of the first thin rod, the second thin rod and the outer sleeve are hot-melted into an integrated structure, so that the photonic crystal fiber is finally made into an all-solid structure with a stable structure and not easy to collapse and deform. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a schematic diagram of the structure of the preform in this embodiment;
[0022] Figure 2 It is a structural schematic diagram of the cross section of the PCF after the preform is drawn and formed;
[0023] Figure 3 The PCF base mode (LP 01 ) and higher order modes (LP 11 )'s limiting loss versus wavelength and the fundamental mode transverse electric field distribution;
[0024] Figure 4 Schematic diagram of the relationship between the effective mode field area and nonlinear coefficient of the PCF of this embodiment and the wavelength;
[0025] Figure 5 (a) is the light spot corresponding to PCF, and (b) is the intensity corresponding to different positions on the light spot. DETAILED DESCRIPTION
[0026] The present invention will be described in further detail below in conjunction with the accompanying drawings.
[0027] like Figure 1 and Figure 2 As shown, the photonic crystal fiber of this embodiment is an optical fiber formed by drawing a preform rod 5. The aforementioned preform rod 5 includes an outer sleeve 1, a first thin rod 2 and two layers of second thin rods 3. Among them, the first thin rod 2 is arranged in the inner hole of the outer sleeve 1, and the two layers of second thin rods 3 are both arranged in the inner hole of the outer sleeve 1, and are both arranged on the periphery of the first thin rod 2, that is, the first thin rod 2 and the two layers of second thin rods 3 are all piled up in the inner hole of the outer sleeve 1. The diameters of the first thin rod 2 and the second thin rod 3 are equal, and are both 2 to 4 mm. In this embodiment, the diameters of the first thin rod 2 and the second thin rod 3 are both 3 mm. As shown Figure 1 As shown, the first thin rod and the second thin rod are both formed by extrusion, and the extrusion method is the same as that in the prior art, and will not be described in detail in this embodiment.
[0028] The two layers of second thin rods 3 are arranged in sequence from inside to outside along the radial direction of the outer sleeve 1 (i.e., an inner layer of second thin rods and an outer layer of second thin rods are arranged), and each layer of second thin rods 3 has a plurality of second thin rods 3 arranged at intervals along the circumference of the first thin rods 2. Figure 1 As shown, the second thin rod 3 includes a core 31 located inside and a cladding 32 wrapped outside the core 31. The refractive index of the cladding 32 is higher than the refractive index of the core 31, and the refractive index of the cladding 32 is equal to the refractive index of the first thin rod 2. The refractive index of all the cores 31 is the same. In this embodiment, the cladding and the first thin rod are made of Ge. 10 As 22 Se 68 , with a refractive index of 2.63. The material of the fiber core 31 is As 2 S 3 , with a refractive index of 2.42. After the preform rod 5 is drawn, all the claddings 32, the first thin rod 2 and the outer sleeve 1 are heat-fused into an integrated structure 4. On each cross section along the radial section of the optical fiber, all the fiber cores 31 are distributed in a regular hexagonal lattice. Among them, the hot melting here is a mature existing technology in this field and will not be repeated here. In this embodiment, there are 18 fiber cores 31. Among them, in the outer layer, there are 12 fiber cores 31, 6 fiber cores 31 are respectively located at the corresponding corners of the regular hexagonal lattice, and the other 6 fiber cores 31 are respectively located at the central position of the corresponding sides adjacent to the regular hexagonal lattice, that is, there is a fiber core 31 in the middle of two adjacent corners. In the inner layer, there are 6 fiber cores 31, and they are respectively located at the corresponding corners of the regular hexagonal lattice.
[0029] In each layer of the optical fiber of this embodiment, the distance between the centers of two adjacent cores 31 is L, the diameter of the core 31 is D, and the distance L and the diameter D satisfy: the value range of D / L is 40% to 60%. Specifically, the diameter of the core 31 is 30 to 40um, and the distance L is 60 to 80um. In this embodiment, the diameter of the core 31 is 35um, the distance L between the centers of any two adjacent cores is 70um, and D / L is 50%. In the inner layer, the distance Φ between the inner edges of two cores 31 located on the diagonal of the regular hexagonal lattice is 105um.
[0030] like Figure 3 As shown, the fundamental mode (LP 01 ) and higher order modes (LP 11 ) with wavelength and the corresponding transverse electric field distribution of the fundamental mode at 1.5μm and 10μm, it can be seen that the ratio of the high-order mode to the fundamental mode limiting loss is always greater than 10 in the entire wavelength range from 1.5μm to 10μm. 2 , which meets the conditions of single-mode optical fiber transmission. At a wavelength of 2μm, its limiting loss can be as low as 1.77×10 -4 dB·m-1 , and the change of the limiting loss remains relatively flat throughout the wavelength scan. From the fundamental mode electric field distribution diagram, it can be seen that the fundamental mode electric field mode of the large mode field PCF of the present application is more concentrated in the core area, which is conducive to achieving a large mode field area.
[0031] like Figure 4 It can be seen that the mode field area and the nonlinear coefficient show an obvious inverse relationship. At a wavelength of 2 μm, the effective mode field area of the photonic crystal fiber (PCF) of this embodiment can be as high as 5362 μm. 2 , and its corresponding nonlinear coefficient can be as low as 1.56×10 -3 m -1 ·W -1 , showing the excellent characteristics of large mode field area and low nonlinear effect. The figure shows the nonlinear coefficient γ; the effective mode field area A eff .
[0032] This example tests the mode distribution of PCF at 1.5 μm. Figure 5 The measured light spot (a) and the corresponding intensity (b) are given. Based on the measured collimated beam diameter, the focal spot size on the PCF is calculated to be about 95μm, which matches the core diameter of the optical fiber, and the transmission intensity distribution is Gaussian, that is, PCF is single-mode transmission. PCF has very good beam quality.
[0033] Comparative analysis: This embodiment studies the transmission characteristics of photonic crystal fiber by the equivalent refractive index method, and uses the finite difference time domain method (FDTD) combined with the PML boundary condition to calculate the effective mode field area, which is the same as the prior art and will not be described in detail in this embodiment.
[0034] The mode field area of traditional step-index optical fibers is only tens of μm 2 , and only achieves single-mode transmission within a certain wavelength range, while the large-mode-field all-solid-state chalcogenide photonic crystal fiber of this embodiment has a wavelength of about 5400μm. 2 The mode field area is increased, and single-mode transmission is achieved in the range of 1.5-2 μm. Therefore, the photonic crystal fiber of this embodiment meets the requirements of laser output with higher power and higher beam quality.
Claims
1. A photonic crystal optical fiber, which is an optical fiber formed by drawing a preform rod (5), wherein the preform rod (5) includes an outer sleeve (1); characterized in that: The preform (5) also includes: a first thin rod (2) disposed in the inner hole of the outer sleeve (1); and Two layers of second thin rods (3), which are arranged in the inner hole of the outer sleeve (1), and the two layers of second thin rods (3) are arranged on the periphery of the first thin rod (2), and the two layers of second thin rods (3) are arranged in sequence from the inside to the outside along the radial direction of the outer sleeve (1), and each layer of second thin rods (3) has a plurality of second thin rods (3) arranged at intervals along the circumference of the first thin rod (2), and the second thin rod (3) includes a core (31) located inside and a cladding (32) wrapped outside the core (31); The outer sleeve (1), the first thin rod (2) and all the claddings (32) in the optical fiber are an integrated structure (4) formed by hot melting; wherein, in each cross section along the radial section of the optical fiber, all the fiber cores (31) are distributed in a regular hexagonal lattice.
2. The photonic crystal fiber according to claim 1, characterized in that: The refractive index of the cladding (32) is higher than the refractive index of the core (31), and the refractive index of the cladding (32) is equal to the refractive index of the first thin rod (2). In each radial section of the optical fiber, the distance between the centers of two adjacent cores (31) is L, and the diameter of the core (31) is D. The distance L and the diameter D satisfy that the duty cycle D / L ranges from 40% to 60%.
3. The photonic crystal fiber according to claim 1, characterized in that: The refractive index of all the fiber cores (31) is the same.
4. The photonic crystal fiber according to claim 1, characterized in that: In the outer layer, there are 12 fiber cores (31), 6 of which are located at corresponding corners of the regular hexagonal lattice, and the other 6 fiber cores (31) are located at the central position of corresponding sides adjacent to the regular hexagonal lattice; in the inner layer, there are 6 fiber cores (31), which are located at corresponding corners of the regular hexagonal lattice.
5. The photonic crystal fiber according to claim 2, characterized in that: The duty ratio D / L is 50%.
6. The photonic crystal fiber according to claim 2, characterized in that: The diameter D of the fiber core (31) in the optical fiber is 30-40 um, and the spacing L is 60-80 um.
7. The photonic crystal fiber according to claim 6, characterized in that: The spacing L is 70 um, and the diameter D is 35 um.
8. The photonic crystal fiber according to claim 1, characterized in that: In the inner layer of the optical fiber, the spacing Φ between the inner edges of two fiber cores (31) located on the diagonal lines of the regular hexagonal lattice is 105um.
9. The photonic crystal fiber according to claim 1, characterized in that: The diameters of the first thin rod (2) and the second thin rod (3) of the preform rod (5) are equal and are both 2 to 4 mm.
10. The photonic crystal fiber according to claim 9, characterized in that: The diameters of the first thin rod (2) and the second thin rod (3) are both 3 mm.