Bismuth-manganese-iron alloy cored wire
The bismuth-manganese-iron alloy cored wire with protective layers addresses gasification and oxidation issues, ensuring precise cutting and reducing waste in bismuth-containing free-cutting steel production.
Patent Information
- Application Number
- CN202420341628.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-23
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-02-23
AI Technical Summary
Bismuth-containing free-cutting steel production faces issues such as gasification, splashing, smoke pollution, and oxidation of the bismuth-manganese-iron alloy cored wire during cutting and transportation, leading to waste and increased costs.
A bismuth-manganese-iron alloy cored wire is designed with multiple protective layers, including a cold-rolled steel strip, steel wire armor layer, and flexible plastic material, along with a polybutyl acrylate outer skin, to protect the core during cutting and transportation, facilitating accurate sectioning and preventing oxidation.
The protective layers ensure precise cutting and minimize oxidation, reducing waste and costs by maintaining the integrity of the alloy during processing, thus enhancing production efficiency.
Smart Images

Figure CN222100029U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of alloy cored wires, in particular to a bismuth-manganese-iron alloy cored wire. Background Art
[0002] In recent years, free-cutting steel has developed rapidly, with a wide variety of types and widely used in industries such as automobiles, machinery, and precision instruments. Excellent cutting performance saves the production costs of enterprises and brings rich benefits to enterprises. With the development of free-cutting steel, problems have gradually emerged. Sulfur-containing free-cutting steel is prone to splitting during the rolling production process due to its high sulfur content; although lead-containing free-cutting steel has excellent performance, its development is restricted by the pollution of lead to the environment and harm to the human body. Bismuth metal is an environmentally friendly element with similar properties to lead. Bismuth metal (Bi) has a silvery white appearance, a strong metallic luster, is brittle, and has an orthorhombic crystal structure. Since bismuth metal is non-toxic and has a low melting point and high flexibility similar to lead metal, it is used to replace lead in the steelmaking field to improve the cutting performance of steel. The melting point of Bi element is 271.3℃ and the boiling point is 1560±5℃. It can be added to free-cutting steel as a substitute for lead element, exerting the same excellent cutting effect as lead, and significantly improving the cutting performance of steel. Current research on bismuth-containing free-cutting steel has shown that replacing lead with bismuth is the future development trend for environmentally friendly free-cutting steel.
[0003] However, the addition of bismuth to molten steel is easy to gasify, which makes it easy to cause splashing and a large amount of smoke pollution when bismuth is added to the molten steel, and bismuth is difficult to enter the molten steel to play a role, resulting in a lot of waste and greatly increased costs. Therefore, in the prior art, when adding bismuth to molten steel, the method of adding bismuth metal directly is not adopted, but the method of adding bismuth manganese iron alloy cored wire is adopted. In the process of producing bismuth-containing free-cutting steel, the bismuth manganese iron alloy is put into the molten steel for production. Therefore, the production and transportation of bismuth manganese iron alloy cored wire becomes an indispensable part of the steps of preparing bismuth-containing free-cutting steel.
[0004] In the prior art, the bismuth-manganese-iron alloy cored wire needs to be cut into sections before being put into the molten steel. If a cutting error occurs, for example, when the outer sheath of the bismuth-manganese-iron alloy cored wire has been cut off and it is found that the cut section length is too long, a cut will be left on the plastic outer sheath of the bismuth-manganese-iron alloy cored wire. The iron portion of the bismuth-manganese-iron alloy is easily oxidized by environmental elements, resulting in oxidation and rust of the cored wire portion, while the alloy portion of the bismuth-manganese-iron alloy cored wire without an outer sheath is directly exposed to the outside. During long-distance transportation or long-term storage, the iron outer sheath of the alloy cored wire is easily oxidized due to external reasons, affecting subsequent production processing. Utility Model Content
[0005] To this end, the utility model provides a bismuth-manganese-iron alloy cored wire to solve the above-mentioned problems in the prior art.
[0006] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0007] According to a first aspect of the utility model, a bismuth-manganese-iron alloy cored wire comprises a cored wire portion, wherein the outer surface of the cored wire portion is sequentially sleeved with a first protective layer, a second protective layer, a third protective layer and an outer sheath from the inside to the outside.
[0008] Furthermore, the core of the cored wire is a bismuth-manganese-iron alloy.
[0009] Furthermore, the first protective layer is made of cold-rolled steel strip, and the outer surface of the core of the cored wire is fixedly connected to the first protective layer by cold rolling and forging.
[0010] Furthermore, the second protective layer is a steel wire armor layer, that is, a structure formed by a plurality of uniform thin steel wires uniformly wound around the outer surface of the first protective layer.
[0011] Furthermore, the third protective layer is a flexible plastic material made of polypropylene.
[0012] Furthermore, the third protective layer is fixedly connected to the outer surface of the second protective layer by means of a film rolling machine sleeve connection.
[0013] Furthermore, the outer skin is a polybutyl acrylate structure containing reflective material inside.
[0014] Furthermore, the outer skin is fixedly connected to the third protective layer by gluing.
[0015] The utility model has the following advantages: when the cored wire is cut into sections and fed with molten steel to produce bismuth-containing easy-to-cut steel, when the outer skin is cut to the second protective layer formed by the steel wire armor layer, due to the different structures, it can assist the staff to judge that the non-metallic outer skin protective layer has been cut off, and the outer skin can be removed for feeding; even if the cutting is wrong, the cold-rolled steel strip on the outer layer of the core of the cored wire can still protect the internal bismuth-manganese-iron alloy structure, thereby avoiding damage and oxidation of the cored wire due to cutting errors. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a stereoscopic view of the end of a bismuth-manganese-iron alloy cored wire provided by the utility model.
[0017] Figure 2 This is a schematic diagram of a bismuth-manganese-iron alloy cored wire provided by the utility model.
[0018] Figure 3 The utility model provides a schematic diagram of the cross-sectional structure of a bismuth-manganese-iron alloy cored wire.
[0019] Figure 4A schematic diagram of a cable cutaway of a bismuth-manganese-iron alloy cored wire provided by the utility model.
[0020] In the figure: 1, core of the cored wire, 2, first protective layer, 3, second protective layer, 4, third protective layer, 5, outer sheath. DETAILED DESCRIPTION
[0021] The following is a specific embodiment of the present invention. People familiar with the technology can easily understand the other advantages and functions of the present invention from the contents disclosed in this specification. Obviously, the described embodiment is a part of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0022] Example 1
[0023] like Figures 1 to 4 As shown, a bismuth-manganese-iron alloy cored wire in an embodiment of the first aspect of the utility model comprises a cored wire core 1, and the outer surface of the cored wire core 1 is sequentially sleeved with a first protective layer 2, a second protective layer 3, a third protective layer 4 and an outer sheath 5 from the inside to the outside;
[0024] In the above embodiment, it should be noted that the bismuth-manganese-iron alloy cored wire is produced by adding the bismuth-manganese-iron alloy into the molten steel in the process of producing bismuth-containing free-cutting steel. Before adding, the length of the bismuth-manganese-iron alloy cored wire to be added is determined according to the bismuth-manganese-iron ratio calculated according to production needs, and then the bismuth-manganese-iron alloy cored wire is cut into sections for feeding;
[0025] Example 2
[0026] like Figures 1 to 4 As shown, a bismuth-manganese-iron alloy cored wire includes all the contents of Example 1, and in addition, the core 1 of the cored wire is a bismuth-manganese-iron alloy, and the bismuth-manganese-iron alloy contains, by mass fraction, a ratio of bismuth: manganese: iron of 9:1:9, and some unavoidable impurity elements;
[0027] In the above embodiment, it should be noted that the bismuth-manganese-iron alloy cored wire is cut into segments for feeding during the production of bismuth-containing free-cutting steel, and the outer skin 5 and the third protective layer 4 and the second protective layer 3 of the non-metallic material need to be removed, and the remaining parts are pure metal components, which can form bismuth-containing free-cutting steel liquid after being put into molten steel to prepare for subsequent production needs;
[0028] Example 3
[0029] like Figures 1 to 4As shown, a bismuth-manganese-iron alloy cored wire includes all the contents of Example 2, and in addition, the first protective layer 2 is made of cold-rolled steel strip, and the outer surface of the core 1 of the cored wire is fixedly connected to the first protective layer 2 by cold rolling and forging;
[0030] In the above embodiment, it should be noted that the bismuth-manganese-iron alloy cored wire is fed into the molten steel before being fed into the molten steel during the production of bismuth-containing free-cutting steel. Since the cold-rolled steel strip is mainly composed of iron, it meets the metal element ratio for producing bismuth-containing free-cutting steel.
[0031] Example 4
[0032] like Figures 1 to 4 As shown, a bismuth-manganese-iron alloy cored wire includes all the contents of Example 3, and in addition, the second protective layer 3 is a steel wire armor layer, that is, a structure formed by a plurality of uniform thin steel wires uniformly wound around the outer surface of the first protective layer 2;
[0033] In the above embodiment, it should be noted that when the second protective layer 3, i.e., the steel wire armor layer, is cut by a worker using a cutting tool, due to its different structure, the worker can feel the change in the cutting feel when cutting to the second protective layer 3, thereby assisting the worker in determining that the non-metallic protective layer has been cut, and thus performing a peeling process;
[0034] Example 5
[0035] like Figures 1 to 4 As shown, a bismuth-manganese-iron alloy cored wire includes all the contents of Example 4, and in addition, the third protective layer 4 is a flexible plastic material made of polypropylene, and the third protective layer 4 is fixedly connected to the outer surface of the second protective layer 3 by means of a film rolling machine sleeve;
[0036] In the above embodiment, it should be noted that the third protective layer 4 is a flexible plastic material made of polypropylene, which can make the core 1 of the cored wire have better heat resistance and stability, and effectively avoid the problems of mechanical stress and compression deformation during the transportation and use of the cored wire;
[0037] Example 6
[0038] like Figures 1 to 4 As shown, a bismuth-manganese-iron alloy cored wire includes all the contents of Example 6, and in addition, the outer skin 5 is a polybutyl acrylate structure containing a reflective material inside, and the outer skin 5 is fixedly connected to the third protective layer 4 by gluing;
[0039] In the above embodiment, it should be noted that the outer skin 5 is a polybutyl acrylate structure containing a reflective material inside, and the material is relatively transparent, wherein the reflective material is fine glass beads, which can protect the internal bismuth manganese iron alloy while playing a marking role, and the outer surface of the outer skin 5 can also be marked with ink such as the core wire radius, the core wire metal composition, etc.
[0040] Working principle: Bismuth-manganese-iron alloy cored wire is produced by putting bismuth-manganese-iron alloy into molten steel during the process of producing bismuth-containing free-cutting steel. Before putting in, the length of the bismuth-manganese-iron alloy cored wire to be put in is determined according to the bismuth-manganese-iron ratio calculated according to production needs, and then it is cut into sections for feeding. When the cored wire is cut into sections and fed with molten steel to produce bismuth-containing free-cutting steel, it is necessary to remove the outer skin 5 and the third protective layer 4 and the second protective layer 3 of the non-metallic material, and the rest is pure metal components. After being put into molten steel, bismuth-containing free-cutting steel molten steel can be formed to prepare for subsequent production needs. The first protective layer 2 of the cold-rolled steel strip material is also put into the molten steel. Since the cold-rolled steel strip is mainly composed of iron elements, it meets the metal element ratio for producing bismuth-containing free-cutting steel. When the staff cuts the outer skin 5 to the second protective layer 3 composed of the steel wire armor layer, the second protective layer 3, that is, the steel wire armor layer, when the staff uses a cutting tool to cut it, due to its different structure, the staff can feel the change in the cutting feel when cutting to the second protective layer 3, which can assist the staff to judge that the non-metallic outer skin 5 protective layer has been cut off, and the outer skin 5 can be removed for feeding. Even if the cutting is wrong, the first protective layer 1 of the outer layer of the cored wire core 1, that is, the cold-rolled steel strip, can still protect the internal bismuth-manganese-iron alloy structure, thereby avoiding damage and oxidation of the cored wire due to cutting errors.
Claims
1. A bismuth-manganese-iron alloy cored wire, comprising a cored wire core (1), characterized in that: The outer surface of the cored wire core (1) is covered with a first protective layer (2), a second protective layer (3), a third protective layer (4) and an outer sheath (5) in sequence from the inside to the outside.
2. The bismuth-manganese-iron alloy cored wire according to claim 1, characterized in that: The core part (1) of the cored wire is a bismuth-manganese-iron alloy.
3. The bismuth-manganese-iron alloy cored wire according to claim 2, characterized in that: The first protective layer (2) is made of cold-rolled steel strip, and the outer surface of the cored wire core (1) is fixedly connected to the first protective layer (2) by cold rolling and forging.
4. The bismuth-manganese-iron alloy cored wire according to claim 1, characterized in that: The second protective layer (3) is a steel wire armor layer, that is, a structure formed by a plurality of uniform thin steel wires uniformly wound around the outer surface of the first protective layer (2).
5. The bismuth-manganese-iron alloy cored wire according to claim 1, characterized in that: The third protective layer (4) is made of a flexible plastic material made of polypropylene.
6. The bismuth-manganese-iron alloy cored wire according to claim 5, characterized in that: The third protective layer (4) is fixedly connected to the outer surface of the second protective layer (3) by means of a film rolling machine sleeve connection.
7. The bismuth-manganese-iron alloy cored wire according to claim 1, characterized in that: The outer skin (5) is a polybutyl acrylate structure containing reflective material inside.