Sharp-bottomed rhinestone with polyamide hot melt adhesive

By setting oxide film, paint and polyamide hot melt adhesive layers on the bottom of pointed rhinestones, the problem that existing rhinestones cannot be hot melt pasted is solved, and a wider use and colorful effect is achieved, especially in clothing and shoes. and bag-like fabrics.

CN222291361UActive Publication Date: 2025-01-03GUANGZHOU SALMAN ACCESSORIES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421062674.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-05-16
Publication Date
2025-01-03
Estimated Expiration
2034-05-16

AI Technical Summary

Technical Problem

The existing rhinestones fail to achieve hot melt adhesive on the pointed bottom, which limits their use, especially on the bonding and embellishment effects on fabrics such as clothing, leather and footwear, and cannot achieve hot melt adhesive through heating and blanching.

Method used

A pointed-bottomed rhinestone with polyamide hot melt adhesive was designed, with an oxide film layer, a paint layer and a polyamide hot melt adhesive layer in turn, which are attached by vacuum plating and spraying, and are uniformly coated with hot melt by electrostatic spraying. Gluten layer, suitable temperature is 100-200℃ to achieve hot melt adhesive.

Benefits of technology

The scope of use of rhinestones has been expanded, the convenience of hot melt pasting is achieved, and the effect is provided is colorful and shining, and it is used more widely in clothing, footwear, and luggage fabrics. The processing efficiency and additionalness are worth improving.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222291361U_ABST
    Figure CN222291361U_ABST
Patent Text Reader

Abstract

The utility model discloses a sharp-bottomed rhinestone with polyamide hot melt adhesive, which comprises a sharp-bottomed rhinestone body, an oxidation film layer, a paint layer and a polyamide hot melt adhesive layer are sequentially arranged at the bottom of the sharp-bottomed rhinestone body, the oxidation film layer is connected with the sharp-bottomed rhinestone body, the paint layer is arranged on the oxidation film layer, and the polyamide hot melt adhesive layer is arranged on the paint layer. The polyamide hot melting gelatinous layer is arranged on the paint layer, and the paint layer is arranged between the polyamide hot melting gelatinous layer and the oxidation film layer. The utility model belongs to the technical field of sharp-bottomed rhinestones, and particularly relates to a sharp-bottomed rhinestone with polyamide hot melt adhesive, the bottom of the sharp-bottomed rhinestone is provided with adhesive, and the sharp-bottomed rhinestone can be directly adhered to an object in a heating and ironing manner and can also be fixed in a processing manner of AB glue or acryl thermosensitive adhesive. The condition that the rhinestone is fixed only through a processing mode of AB glue and acryl thermosensitive glue is avoided, the application range of the rhinestone is expanded, and the technical effect that hot melting and pasting are convenient is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of pointed-bottom diamonds, in particular to a pointed-bottom diamond with polyamide hot-melt adhesive. Background Art

[0002] Rhinestone, also known as crystal diamond and rhinestone, is mainly composed of crystal glass. It is a kind of jewelry accessory obtained by grinding, polishing and cutting glass into diamond facets, making it have a colorful and gorgeous appearance like natural diamonds. It is an important embellishment supporting material for jewelry, shoes, handicrafts, clothing, luggage and leather goods, and has a huge market.

[0003] At present, the diamonds on the market are mainly divided into flat-bottom diamonds and pointed-bottom diamonds. Flat-bottom diamonds are further divided into those with hot-melt adhesive and those without hot-melt adhesive. The ones with hot-melt adhesive are called hot-drills in the market; flat-bottom hot-drills have a hot-melt adhesive layer on the bottom plane, which can be directly adhered to objects by hot pressing and heating; pointed-bottom diamonds are also called water diamonds in the market. They have a diamond shape composed of an inverted rhombus shape at the bottom and a horizontal surface on the face. The bottom of the water diamond is then coated with a reflective layer and a protective layer (to protect the paint) to make it have a refractive and reflective effect and brightness similar to that of a diamond.

[0004] Among the existing rhinestones on the market, the existing technology cannot realize the pointed bottom drill with hot melt glue on the bottom of the rhinestone cone, so the use of the existing rhinestones is limited to relying on AB glue, acrylic pressed heat-sensitive glue and other processing methods to bond with objects for embellishment effect, which greatly reduces the scope of use, especially for clothing fabrics, leather, shoes, bags and other fabrics. The scope of use cannot achieve the purpose of adding highlights and added value to the products by heating and pressing with hot melt glue on the bottom like hot rhinestones. Utility Model Content

[0005] The technical problem to be solved by the utility model is that the utility model provides a pointed-bottom water rhinestone with built-in polyamide hot-melt adhesive, so that the bottom of the pointed-bottom water rhinestone has its own adhesive, and can be directly adhered to an object by heating and pressing, and can also be fixed by using AB glue or acrylic thermosensitive adhesive processing methods, avoiding the situation where the water rhinestone is fixed only by relying on the processing methods of AB glue and acrylic thermosensitive adhesive, expanding the use scope of the water rhinestone, and achieving the technical effect of convenient hot-melt pasting.

[0006] In order to solve the above technical problems, the technical solution adopted by the utility model is as follows: the utility model proposes a pointed-bottom rhinestone with built-in polyamide hot-melt adhesive, comprising a pointed-bottom rhinestone body, the bottom of which is sequentially provided with an oxide film layer, a paint layer and a polyamide hot-melt adhesive layer, the oxide film layer is connected to the pointed-bottom rhinestone body, the paint layer is arranged on the oxide film layer, the polyamide hot-melt adhesive layer is arranged on the paint layer, and the paint layer is arranged between the polyamide hot-melt adhesive layer and the oxide film layer.

[0007] As an improvement, the pointed-bottom rhinestone body has a conical cut-out bottom, the pointed-bottom rhinestone body is in the shape of a cone head, and the side surface of the cone is cut into a plurality of equally divided planes.

[0008] As an improvement, the oxide film layer is attached to the bottom of the pointed-bottom rhinestone by one of vacuum electroplating and water electroplating. The thickness of the oxide film layer can be set according to actual requirements. After the light is emitted from the oxide film layer and the pointed-bottom rhinestone body, a glittering effect of light refraction is generated, making the rhinestone present a colorful and glittering effect.

[0009] As an improvement, the paint layer is a special protective gold oil for crystal glass products, which is composed of a primer, a primer curing agent, a topcoat and a topcoat curing agent in a component bottom-surface combination. The paint layer is attached to the bottom of the pointed-bottom rhinestone body of the oxide layer by spraying. After the light passes through the oxide film layer, the pointed-bottom rhinestone body reflects a bright and shiny effect through the refraction of the conical section bottom. The main function is to protect the oxide layer at the bottom of the attached rhinestone and the hot melt adhesive attachment fusion processing to prepare for the next step.

[0010] As an improvement, the polyamide hot melt adhesive layer is made of polyamide resin powder particles. The melt viscosity of the polyamide hot melt adhesive layer is 2000-3500CPS, with good adhesion effect, applicable temperature of 100-200°C, high heat resistance, good fluidity, and both adhesion and anti-sticking properties. The thickness of the polyamide hot melt adhesive layer is less than or equal to 0.3mm.

[0011] The beneficial effects achieved by the utility model with the above structure are as follows: the pointed-bottom rhinestone with polyamide hot-melt adhesive proposed in the scheme is no longer limited to the previous processing method. After the pointed-bottom rhinestone body is cut and polished, an oxide film layer, a paint layer and a polyamide hot-melt adhesive layer are sequentially arranged on the bottom. The principle of flat-bottom hot-drilling is applied to the pointed-bottom rhinestone, which not only ensures the dazzling luster of the rhinestone itself refracted by the conical cross section, but also has the advantage of being more glittering and colorful than flat-bottom hot-drilling, and is more convenient for hot-melt pasting, especially for embellishment on cloth fabrics and leather of clothing, shoes, bags, etc., and is more widely applicable;

[0012] Unlike flat-bottom rhinestones, which are coated with polyamide resin powdered hot melt adhesive on the bottom, flat-bottom rhinestones are coated with polyamide resin powdered hot melt adhesive by using a sieve to sprinkle the powdered hot melt adhesive micro-particles on the bottom of the flat-bottom rhinestone, while pointed-bottom rhinestones cannot be coated with powdered hot melt adhesive micro-particles in this way. Electrostatic spraying equipment must be used to use the electrostatic spraying process to evenly apply the powdered hot melt adhesive to the conical bottom of the rhinestone. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 This is an enlarged schematic diagram of the structural cross-section of a pointed-bottom diamond with polyamide hot-melt adhesive proposed by the utility model;

[0014] Figure 2 This is a bottom view of a pointed-bottom rhinestone with polyamide hot-melt adhesive proposed by the utility model;

[0015] Figure 3 This is a top view of a pointed-bottom rhinestone with polyamide hot-melt adhesive proposed by the utility model;

[0016] Figure 4 It is a schematic diagram of the hot melt adhesive structure of a pointed-bottom rhinestone with a polyamide hot melt adhesive proposed by the utility model;

[0017] Figure 5 The utility model provides a schematic diagram of the structure of a pointed-bottom diamond with polyamide hot-melt adhesive and a comparison diagram of a diamond without hot-melt adhesive.

[0018] Among them, 1. pointed bottom rhinestone body, 2. oxide film layer, 3. paint layer, 4. polyamide hot melt adhesive layer. DETAILED DESCRIPTION

[0019] The technical solutions in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, rather than all of the embodiments; based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0020] like Figure 1-5 As shown, the utility model proposes a pointed bottom rhinestone with built-in polyamide hot melt adhesive, comprising a pointed bottom rhinestone body 1, an oxide film layer 2, a paint layer 3 and a polyamide hot melt adhesive layer 4 are sequentially arranged on the bottom of the pointed bottom rhinestone body 1, the oxide film layer 2 is connected to the pointed bottom rhinestone body 1, the paint layer 3 is arranged on the oxide film layer 2, the polyamide hot melt adhesive layer 4 is arranged on the paint layer 3, and the paint layer 3 is arranged between the polyamide hot melt adhesive layer 4 and the oxide film layer 2.

[0021] like Figure 1-5As shown, the pointed-bottom rhinestone body 1 has a conical cut-out bottom, and the pointed-bottom rhinestone body 1 is in the shape of a cone head, and the side surface of the cone is cut into a plurality of equally divided planes.

[0022] like Figure 1-5 As shown, the oxide film layer 2 is attached to the bottom of the pointed bottom rhinestone by one of vacuum electroplating and water electroplating. The thickness of the oxide film layer 2 can be set according to actual requirements. After the light is emitted from the oxide film layer 2 and the pointed bottom rhinestone body 1, a glittering effect of light refraction is generated, making the rhinestone present a colorful and glittering effect.

[0023] like Figure 1-5 As shown, the paint layer 3 is a special protective gold oil for crystal glass products, which is composed of a primer, a primer curing agent, a topcoat and a topcoat curing agent according to the component bottom surface. The paint layer 3 is attached to the bottom of the pointed bottom rhinestone body 1 of the oxide layer by spraying. After the light passes through the oxide film layer 2, the pointed bottom rhinestone body 1 reflects a bright and shiny effect through the refraction of the conical section bottom. The main function is to protect the bottom oxide layer of the attached rhinestone and the hot melt adhesive attachment fusion processing to prepare for the next step.

[0024] like Figure 1-5 As shown, the polyamide hot melt adhesive layer 4 is made of polyamide resin powder particles. The melt viscosity of the polyamide hot melt adhesive layer 4 is 2000-3500CPS, with good adhesion effect, applicable temperature of 100-200°C, high heat resistance, good fluidity, and both adhesion and anti-sticking properties. The thickness of the polyamide hot melt adhesive layer 4 is less than or equal to 0.3mm.

[0025] When in use, align the pointed-bottom rhinestone body 1 with the installation position, use a point drilling machine or an ironing press and other equipment to melt the polyamide hot-melt adhesive layer 4 at the bottom of the pointed-bottom rhinestone body 1 and fix it to the clothing fabric or leather fabric. This not only ensures the dazzling luster of the rhinestone itself, but also has the advantage of being more shiny and colorful than flat-bottom hot-drilled rhinestones, and is more convenient for hot-melt pasting, while taking into account processing efficiency and processing cost.

[0026] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

[0027] The above description of the utility model and its implementation methods is not restrictive. The drawings show only one implementation method of the utility model, and the actual structure is not limited thereto. In short, if ordinary technicians in this field are inspired by it and design structural methods and embodiments similar to the technical solution without creativity without departing from the purpose of the invention of the utility model, they should all fall within the protection scope of the utility model.

Claims

1. A pointed-bottom diamond with polyamide hot-melt adhesive, characterized in that: The invention comprises a pointed-bottom diamond body (1), wherein an oxide film layer (2), a paint layer (3) and a polyamide hot-melt adhesive layer (4) are sequentially arranged at the bottom of the pointed-bottom diamond body (1), wherein the oxide film layer (2) is connected to the pointed-bottom diamond body (1), the paint layer (3) is arranged on the oxide film layer (2), the polyamide hot-melt adhesive layer (4) is arranged on the paint layer (3), and the paint layer (3) is arranged between the polyamide hot-melt adhesive layer (4) and the oxide film layer (2).

2. The pointed-bottom diamond with polyamide hot-melt adhesive according to claim 1, characterized in that: The pointed-bottom diamond body (1) has a conical cut-out bottom, and the pointed-bottom diamond body (1) is in the shape of a cone head, and the side surface of the cone is cut into a plurality of equally divided planes.

3. The pointed-bottom diamond with polyamide hot-melt adhesive according to claim 2, characterized in that: The oxide film layer (2) is attached to the bottom of the pointed-bottom diamond by one of vacuum electroplating and water electroplating.

4. The pointed-bottom diamond with polyamide hot-melt adhesive according to claim 3, characterized in that: The paint layer (3) is a special protective gold oil for crystal glass products, and the paint layer (3) is attached to the bottom of the pointed bottom rhinestone body (1) of the oxide layer by spraying.

5. The pointed-bottom diamond with polyamide hot-melt adhesive according to claim 4, characterized in that: The polyamide hot melt adhesive layer (4) is made of polyamide resin powder particles, the melting viscosity of the polyamide hot melt adhesive layer (4) is 2000-3500 CPS, and the thickness of the polyamide hot melt adhesive layer (4) is less than or equal to 0.3 mm.