Continuous glue temporary pressing plate
By designing a temporary glue pressure plate with an avoidance groove and a card slot structure, the problem of insufficient sealant application in one go is solved, thus improving construction efficiency and gluing quality.
Patent Information
- Application Number
- CN202422460320.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-12
- Publication Date
- 2025-09-16
- Estimated Expiration
- 2034-10-12
AI Technical Summary
The existing temporary pressure plate prevents the sealant from being applied in one go, resulting in sealing defects and low construction efficiency.
A temporary pressing plate for continuous gluing is designed. By setting an avoidance groove and a card slot structure on the fixed plate, the glue gun can be easily inserted into the temporary pressing plate for continuous gluing, avoiding the process of disassembly and re-application of sealant.
The sealant can be successfully applied in one go, which simplifies the construction process, improves the construction efficiency, and ensures the quality of the sealant and the fixing effect.
Smart Images

Figure CN223337719U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of temporary fixing of curtain wall glass, in particular to a temporary pressing plate with continuous glue. Background Art
[0002] In the construction of exposed frame curtain wall, the application of sealant between glass and aluminum frame is an important process for waterproof sealing. Before the sealant is applied, it is generally necessary to use a temporary pressure plate to fix the glass. Figure 1 After using temporary pressure plates to fix the glass in sections, refer to the attached Figure 5 The temporary pressure plate prevents the sealant from being applied in one go. The sealant will break at the temporary pressure plate and needs to be repaired after the temporary pressure plate is removed. However, sealing defects or omissions are likely to occur during repair. Secondly, multiple application of sealant also affects construction efficiency. Utility Model Content
[0003] The utility model provides a temporary glue-free pressing plate, which is used to solve the problem that the existing temporary pressing plate hinders the sealing glue from being injected in one go.
[0004] The utility model provides a temporary glue-free pressing plate, comprising a fixed plate, with inclined plates fixed on both sides respectively, the inclined plates being fixed to a connecting plate through a bottom plate, the inclined plates, the bottom plate and the connecting plate forming an avoidance groove, the groove width of the avoidance groove gradually decreasing from the groove mouth to the groove bottom, and a first card groove adapted to the buffer strip being fixed on the connecting plate.
[0005] Preferably, a claw plate extends forward from one end of the inclined plate close to the fixed plate, and the two claw plates and the fixed plate are enclosed to form a second slot.
[0006] Preferably, the thickness of the claw plate is smaller than the thickness of the inclined plate, and the side of the claw plate away from the fixed plate is flush with the side of the inclined plate away from the fixed plate.
[0007] Preferably, the fixing plate is provided with a mounting hole.
[0008] Preferably, the connecting plate and the bottom plate are arranged vertically.
[0009] Preferably, both groove walls of the first groove are L-shaped plates, and the width of the first groove at the groove opening is smaller than the width at the groove bottom.
[0010] Preferably, the first slot is located between the bottom plate and the fixing plate.
[0011] Preferably, the fixing plate, the avoidance groove and the first clamping groove are all made of aluminum.
[0012] Compared with the existing technology, in the present invention, the first slot is inserted into the rubber strip to press on the glass, and then the fixing plate and the aluminum frame are fixed together by self-tapping screws, thereby completing the temporary fixation of the glass and the aluminum frame. When applying sealant, continuous sealant application is achieved by extending the glue gun into the avoidance groove when passing through the temporary pressure plate, avoiding the process of disassembling the temporary pressure plate and applying sealant again. The sealant is successfully applied in one application, which simplifies the construction process, improves construction efficiency, and ensures the quality of the sealant application. Secondly, the structural design of the avoidance groove with a large groove mouth and a small groove bottom facilitates the application of sealant while also ensuring the fixing effect of the temporary pressure plate. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to more clearly illustrate the technical solutions of the present invention or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0014] Figure 1 This is a structural diagram of an existing temporary pressure plate application scenario of the present utility model;
[0015] Figure 2 This is a structural diagram of the application scenario of the temporary pressing plate of the utility model;
[0016] Figure 3 It is a structural diagram of the utility model;
[0017] Figure 4 It is a top view of the utility model;
[0018] Figure 5 This is a diagram of the construction steps of applying sealant to the existing temporary pressure plate of the utility model;
[0019] Figure 6 This is a diagram of the construction steps for applying sealant to the temporary pressure plate of the utility model.
[0020] Reference numerals:
[0021] 1. Fixed plate, 2. Inclined plate, 3. Bottom plate, 4. Connecting plate, 5. Claw plate, 6. L-shaped plate, 7. Buffer strip, 11. Mounting hole, 100. Avoidance groove, 200. First card slot, 300. Second card slot. DETAILED DESCRIPTION
[0022] To make the purpose, technical solutions, and advantages of the present invention more clear, the following will be combined with the accompanying drawings to clearly and completely describe the technical solutions of the present invention. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.
[0023] Refer to the attached Figure 2 and attached Figure 3 The present embodiment provides a temporary pressure plate with continuous glue, comprising a fixed plate 1, with inclined plates 2 fixed on both sides of the fixed plate 1, the inclined plates 2 being fixed to the connecting plates 4 via the bottom plate 3, the inclined plates 2, the bottom plate 3 and the connecting plates 4 enclosing a avoidance groove 100, which is arranged correspondingly to the places where the aluminum frame and the glass need to be sealed. When the sealant reaches the temporary pressure plate, the sealant can be applied to the places blocked by the temporary pressure plate by extending into the avoidance groove 100. Specifically, the avoidance groove 100 at one end of the temporary pressure plate is first entered to apply the sealant to the half area blocked by the temporary pressure plate, and then the avoidance groove 100 at the other end of the temporary pressure plate is entered to apply the sealant to the other half area blocked by the temporary pressure plate. The width of the avoidance groove 100 gradually decreases from the groove opening to the groove bottom. The larger the aperture of the avoidance groove 100, the more convenient it is for workers to apply the sealant, but the fixing effect of the temporary pressure plate will be correspondingly weakened. The wider slot is convenient for applying sealant, and the narrower slot bottom is conducive to ensuring the fixing effect of the temporary pressure plate. The first card slot 200 adapted to the buffer strip 7 is fixed on the connecting plate 4. Figure 6 After the first card slot 200 is inserted into the buffer strip 7, it is pressed on the glass, and then the fixing plate 1 is fixed to the aluminum frame by self-tapping screws, and sealant is applied between the glass and the aluminum frame. When passing through the temporary pressure plate, continuous sealing is achieved by extending the glue gun into the avoidance groove 100, avoiding defects or omissions in the secondary sealing application.
[0024] In another embodiment of the present invention, a claw plate 5 extends forward from one end of the inclined plate 2, near the fixed plate 1. The two claw plates 5 and the fixed plate 1 together form a second retaining groove 300. The two inclined plates 2 form two gripping points, through which the fixed plate 1 is pressed against the aluminum frame, firmly securing it to the frame. This arrangement enhances the pressing force of the temporary pressure plate and relatively shortens its width, making it easier for the glue gun to reach into the avoidance groove 100 for glue application.
[0025] As another embodiment of the present invention, the thickness of the claw plate 5 is smaller than the thickness of the inclined plate 2 , and the side of the claw plate 5 away from the fixed plate 1 is flush with the side of the inclined plate 2 away from the fixed plate 1 .
[0026] As another embodiment of the present invention: Figure 4The fixing plate 1 is provided with a mounting hole 11 for the self-tapping screw to pass through.
[0027] As another embodiment of the present invention: the connecting plate 4 and the bottom plate 3 are arranged vertically.
[0028] As another embodiment of the present invention, both walls of the first slot 200 are L-shaped plates 6, and the width of the first slot 200 at the slot opening is smaller than the width at the slot bottom to prevent the buffer strip 7 from falling off. This arrangement simplifies the structure of the first slot 200 and facilitates manufacturing.
[0029] As another embodiment of the present invention: the first slot 200 is located between the bottom plate 3 and the fixing plate 1. This arrangement enables the fixing plate 1 to be closer to the aluminum frame than the first slot 200, making it easier to fix the fixing plate 1 on the aluminum frame.
[0030] As another embodiment of the present invention, the fixing plate 1, the avoidance groove 100 and the first clamping groove 200 are all made of aluminum. Since it is a temporary pressing plate that only temporarily fixes the glass, using aluminum can reduce processing difficulty and save costs.
[0031] Specifically, the buffer strip 7 is a rubber strip.
[0032] In the present invention, the first slot 200 is inserted into the rubber strip and pressed against the glass, and then the fixing plate 1 is fixed to the aluminum frame by self-tapping screws, thereby completing the temporary fixation of the glass and the aluminum frame. When applying sealant, continuous sealant application is achieved by extending the glue gun into the avoidance slot 100 when passing through the temporary pressure plate, avoiding the process of disassembling the temporary pressure plate and applying the sealant again. The sealant is successfully applied in one application, which simplifies the construction process, improves construction efficiency, and ensures the quality of the sealant application. Secondly, the structural design of the avoidance slot 100 with a large notch and a small bottom facilitates the application of sealant while also ensuring the fixing effect of the temporary pressure plate.
[0033] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the present invention.
Claims
1. A temporary pressure plate without glue, characterized in that: It includes a fixed plate, with inclined plates fixed on both sides of the fixed plate respectively. The inclined plate is fixed to the connecting plate through the bottom plate. The inclined plate, the bottom plate and the connecting plate are surrounded to form an avoidance groove. The groove width of the avoidance groove gradually decreases from the groove mouth to the groove bottom. A first card groove adapted to the buffer strip is fixed on the connecting plate.
2. The temporary pressure plate without glue according to claim 1, characterized in that: A claw plate is extended forward from one end of the inclined plate close to the fixed plate, and the two claw plates and the fixed plate are surrounded to form a second clamping groove.
3. The temporary pressure plate without glue according to claim 2, characterized in that: The thickness of the claw plate is smaller than that of the inclined plate, and a side of the claw plate away from the fixed plate is flush with a side of the inclined plate away from the fixed plate.
4. The temporary pressure plate without glue according to claim 3, characterized in that: The fixing plate is provided with a mounting hole.
5. The temporary pressure plate without glue according to claim 4, characterized in that: The connecting plate and the bottom plate are arranged vertically.
6. The temporary pressure plate without glue according to claim 5, characterized in that: Both groove walls of the first groove are L-shaped plates, and the width of the first groove at the groove opening is smaller than the width at the groove bottom.
7. The temporary pressure plate without glue according to claim 6, characterized in that: The first slot is located between the bottom plate and the fixing plate.
8. The temporary pressure plate without glue according to claim 7, characterized in that: The fixing plate, the avoidance groove and the first clamping groove are all made of aluminum.