AI Technical Summary
In the existing hot stamping and printing process, the hot stamping material is prone to peeling off, which leads to a decrease in printing quality and affects the appearance and service life.
A coating layer and a base coat are applied to the surface of the hot stamping layer. The coating layer consists of an adhesive layer and a thin film, while the base coat layer enhances adhesion. The printing layer includes a white ink layer and a pattern layer to ensure that the ink adheres firmly.
It effectively prevents hot stamping material from peeling off, ensures firm adhesion of ink, and produces clear and accurate patterns and colors, thereby enhancing the aesthetics and lifespan of printed materials.
Smart Images

Figure CN224013266U_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The utility model relates to paper surface decoration technical field, especially a printed matter of first pressing and then printing. BACKGROUND
[0002] First pressing and then printing is a surface decoration process widely used in packaging, labels and high-end printed matter. This process mainly includes two steps: first, using a gold pressing device, under the dual action of high temperature and pressure, the gold foil is accurately transferred to the surface of the paper, forming a pattern or text with metal luster, adding unique texture and visual appeal to the product; then, printing on the surface of the paper after gold pressing, further adding other colors or text information, making the product present a more rich and three-dimensional visual effect, thereby improving its overall quality and market competitiveness.
[0003] In practical application, this surface decoration process often encounters the problem of gold loss. This not only seriously affects the printing quality, but also may cause damage to the gold pressing pattern, thereby reducing the aesthetic and service life of the product. The reason is that the surface of the gold foil is usually smooth and has strong chemical inertness. After gold pressing, the Darcy value of the paper surface is significantly reduced, making it difficult for printing ink to adhere firmly to the paper surface. In the subsequent printing and use process, gold loss (ink and gold pressing material falling off the paper surface) is prone to occur.
[0004] Currently, the industry usually uses methods such as increasing ink viscosity, adjusting printing pressure, and using special ink to improve adhesion, but the effect of these methods is often limited and it is difficult to fundamentally solve the problem of gold loss.
[0005] The content of the background section merely represents the knowledge of the inventors at the time of invention and does not necessarily represent the state of the art in the field. UTILITY MODEL CONTENT
[0006] In view of one or more defects in the prior art, the utility model provides a printed matter of first pressing and then printing, comprising:
[0007] Paper, including a first side and a second side;
[0008] Gold pressing layer, provided on the first side and / or the second side of the paper;
[0009] Film coating layer, provided on the surface of the gold pressing layer;
[0010] Primer layer, provided on the surface of the film coating layer; and
[0011] Printing layer, provided on the surface of the primer layer, the printing layer presents a predetermined pattern.
[0012] According to one aspect of this utility model, the paper is coated paper, offset paper, card stock, newsprint, or writing paper.
[0013] According to one aspect of the present invention, the coating layer includes an adhesive layer and a film, wherein the adhesive layer is disposed between the film and the hot stamping layer.
[0014] According to one aspect of this utility model, the amount of adhesive applied to the adhesive layer is 3-8 g / m². 2 The coating thickness is 5-8μm.
[0015] According to one aspect of this utility model, the film is a matte film, a glossy film, a frosted film, a pearl film, or an anti-counterfeiting film.
[0016] According to one aspect of this invention, the coating amount of the base oil in the base oil layer is 1.8g-2.5g / m². 2 The light transmittance of the base oil is greater than or equal to 92%.
[0017] According to one aspect of the present invention, the printed layer comprises:
[0018] A white ink layer is disposed on the surface of the base oil layer; and
[0019] A pattern layer is disposed on the surface of the white ink layer and presents the preset pattern.
[0020] According to one aspect of the present invention, the white ink layer has a coverage rate greater than or equal to 90%.
[0021] Compared with existing technologies, the embodiments of this utility model provide a pre-hot stamping and post-printing printed product, solving the common problem of gold foil flaking in traditional pre-hot stamping and post-printing processes. Specifically, this invention, by setting a laminating layer on the surface of the hot stamping layer, can firmly fix the hot stamping layer to the surface of the paper, thereby preventing the hot stamping material (hot stamping layer) from peeling off. By setting a base oil layer on the surface of the laminating layer, the surface adhesion of the laminating layer can be enhanced, thereby providing better surface conditions for subsequent printing, ensuring the firm adhesion of ink, and effectively avoiding problems such as ink peeling, fading, or blurry printing. By setting a white ink layer on the surface of the base oil layer, and then setting a pattern layer on the white ink layer, the interference of the hot stamping layer on the color of the preset pattern can be avoided, ensuring that the color of the preset pattern is clear and accurate, achieving the ideal printing effect. Attached Figure Description
[0022] The accompanying drawings are provided to further illustrate the present invention and form part of the specification. They are used together with the embodiments of the present invention to explain the present invention, but do not constitute a limitation thereof. In the drawings:
[0023] Figure 1A schematic view of a pre-ironing post-printing printed matter is shown according to one embodiment of the present application.
[0024] Figure 2 An exploded view of a pre-ironing post-printing printed matter is shown according to one embodiment of the present application.
[0025] In the figure: 100, printed matter; 110, paper; 120, gold stamping layer; 130, film coating layer; 131, glue layer; 132, film; 140, base oil layer; 150, printing layer; 151, white ink layer; 152, pattern layer. DETAILED DESCRIPTION
[0026] Hereinafter, only certain exemplary embodiments are simply described. As those skilled in the art can recognize, the described embodiments can be modified in various different ways without departing from the spirit or scope of the present application. Therefore, the drawings and the description are considered to be exemplary in nature rather than limiting.
[0027] In the description of the present application, it is to be understood that the terms "center", "longitudinal", "transverse", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and therefore cannot be understood as indicating or implying that the indicated device or element must have a particular orientation, be constructed and operated in a particular orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second" are only for the purpose of description, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined with "first", "second" can explicitly or implicitly include one or more of the features. In the description of the present application, the meaning of "multiple" is two or more, unless otherwise specifically limited.
[0028] In the description of the present application, it should be noted that, unless otherwise specifically defined and limited, the terms "mounting", "connecting", "connection" should be broadly understood, for example, it can be fixedly connected, or it can be detachably connected, or integrally connected; it can be mechanically connected, or it can be electrically connected or can communicate with each other; it can be directly connected, or indirectly connected through an intermediate medium; it can be the internal communication of two elements or the interaction relationship between two elements. For those skilled in the art, the specific meaning of the above terms in the present application can be understood according to the specific circumstances.
[0029] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0030] The following disclosure provides many different embodiments or examples for implementing various structures of this invention. To simplify the disclosure, specific examples of components and arrangements are described below. These are merely examples and are not intended to limit the scope of the invention. Furthermore, reference numerals and / or letters may be repeated in different examples; such repetition is for simplification and clarity and does not in itself indicate a relationship between the various embodiments and / or arrangements discussed. In addition, examples of various specific processes and materials are provided in this invention, but those skilled in the art will recognize the application of other processes and / or the use of other materials.
[0031] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are for illustration and explanation only and are not intended to limit the present invention.
[0032] Figure 1 A schematic diagram of a pre-stamped and post-printed article 100 according to an embodiment of the present invention is shown. Figure 2 An exploded view of a pre-stamped and post-printed printed matter 100 according to an embodiment of the present invention is shown below, in conjunction with... Figure 1 and Figure 2 Provide a detailed description.
[0033] like Figure 1 and Figure 2 As shown, the printed matter 100 includes paper 110, a hot stamping layer 120, a laminating layer 130, a base coat 140, and a printing layer 150. The paper 110 can be coated paper, for example, 128g / m². 2 The paper 110 is coated paper. In other embodiments, the paper 110 may also be offset paper, card stock, newsprint, writing paper, etc., but this utility model is not limited to the above-mentioned paper 110 type. The paper 110 has a first side ( Figure 2 (upper side) and second side ( Figure 2 (The lower side of the middle).
[0034] The gold stamping layer 120 is arranged on the first side of the paper 110, and specifically, the gold stamping layer 120 can cover the entire area of the first side of the paper 110, or can only cover part of the area of the first side of the paper 110, and the specific scheme can be determined according to actual needs. The gold stamping layer 120 can be formed by using a gold stamping device (for example, a gold stamping machine) to perform gold stamping processing on the first side of the paper 110. In the process of gold stamping processing, the gold stamping material on the gold stamping belt is completely and uniformly transferred to the surface of the paper 110, so that a high-quality gold stamping effect is achieved, and the paper 110 is endowed with unique texture and visual appeal.
[0035] The film coating layer 130 is arranged on the surface of the gold stamping layer 120, and specifically, the film coating layer 130 can cover the entire area of the gold stamping layer 120, or can only cover part of the area (the area that needs to be printed) on the gold stamping layer 120. By arranging the film coating layer 130 on the surface of the gold stamping layer 120, the gold stamping layer 120 can be firmly fixed on the surface of the paper 110, so as to avoid the gold stamping material (the gold stamping layer 120) from falling off.
[0036] The base oil layer 140 is arranged on the surface of the film coating layer 130, and specifically, the base oil layer 140 can cover the entire area of the film coating layer 130, or can only cover part of the area (the area that needs to be printed) on the film coating layer 130. The printing layer 150 is printed on the surface of the base oil layer 140 and presents a predetermined pattern. By arranging the base oil layer 140 on the surface of the film coating layer 130, the surface adhesion of the film coating layer 130 can be enhanced, so as to provide high-quality surface conditions for printing of the printing layer 150, to ensure firm adhesion of the ink, and effectively avoid problems such as ink falling off, discoloration, or blurred printing.
[0037] The above describes an embodiment in which the gold stamping layer 120, the film coating layer 130, the base oil layer 140, and the printing layer 150 are sequentially arranged on the first side of the paper 110. Those skilled in the art should understand that in other embodiments, these layers can also be sequentially arranged on the second side of the paper 110. In addition, the gold stamping layer 120, the film coating layer 130, the base oil layer 140, and the printing layer 150 can also be sequentially arranged on both the first side and the second side of the paper 110.
[0038] According to an embodiment of the present application, as shown in Figure 1 and Figure 2 The gold stamping layer 120 is formed of a gold stamping material, and can present a pattern with metallic luster on the surface of the paper, so as to endow the paper with unique texture and visual appeal.
[0039] According to an embodiment of the present application, as shown in Figure 1 and Figure 2As shown, the film coating layer 130 can include a glue layer 131 and a film 132, wherein the glue layer 131 is arranged between the film 132 and the gold stamping layer 120. The glue layer 131 can be formed by glue coating of the paper 110 by a glue coating unit (glue coating roller, etc.) of a film coating device, wherein the glue coating amount is 3-8 g / m 2 , and the glue coating thickness is 5-8 μm, which can ensure that the glue layer 131 has sufficient bonding strength, maintain the overall flexibility of the paper 110, and avoid potential problems such as prolonged drying time, increased cost, and potential problems in subsequent processing caused by excessive glue. The film 132 can be attached to the surface of the glue layer 131 by a film coating unit of the film coating device and be firmly bonded by the glue layer 131. The film 132 can be a matte film, such as a BOPP (Biaxially Oriented Polypropylene) matte film. Such a film 132 has good flexibility, wear resistance, and excellent optical properties, and can give the product a low-gloss, soft, and delicate surface texture, and can cooperate with the gold stamping layer 120 to achieve unique visual appeal. Those skilled in the art will readily understand that the selection of the film 132 is not limited to this. Other types of ready-to-coat films (such as glossy films, frosted films, pearl films, or anti-counterfeiting films, etc.) are also applicable, and these ready-to-coat films generally have specific chemical and physical properties that can significantly enhance the water resistance, oil resistance, or further optimize the printability of the surface of the paper 110, thereby meeting diverse application requirements.
[0040] According to an embodiment of the present application, as shown in Figure 1 and Figure 2 , the base oil layer 140 can be formed by base oil coating of the paper 110 by a coating device, wherein the base oil coating amount is 1.8 g-2.5 g / m 2 , which makes the base oil layer 140 not only provide sufficient dyne value (greater than or equal to 38), but also avoid problems such as prolonged drying time or increased cost caused by excessive coating amount. Preferably, the base oil has a light transmittance greater than or equal to 92%, thereby reducing the influence of the base oil layer 140 on the visual effect of the gold stamping layer 120. In a specific embodiment, the base oil can be a high-adhesion water-based base oil. Such a base oil can be stably combined with the film coating layer 130, significantly improve the dyne value (i.e., adhesion) of the paper 110, thereby providing better surface conditions for subsequent printing, ensuring firm adhesion of the ink, and effectively avoiding problems such as ink peeling, fading, or blurred printing.
[0041] According to an embodiment of the present application, as shown in Figure 1 and Figure 2As shown, the printing layer 150 can include a white ink layer 151 and a pattern layer 152, wherein the white ink layer 151 is printed on the surface of the primer layer 140, and the pattern layer 152 is printed on the surface of the white ink layer 151 and presents a preset pattern. Specifically, the white ink layer 151 is formed by printing white ink on the surface of the primer layer 140, and its shape and size are basically consistent with or slightly larger than the preset pattern, thereby providing a uniform white background for the preset pattern, blocking the color penetration of the gold stamping layer 120, avoiding the interference of the gold stamping layer 120 on the color of the preset pattern, ensuring the clear and accurate color presentation of the preset pattern, and achieving the ideal printing effect. In addition, the presence of the white ink layer 151 can also enhance the overall visual effect of the pattern, make the pattern more prominent, and improve the aesthetic appearance of the printed matter 100. The pattern layer 152 is formed by printing preset ink on the surface of the white ink layer 151, and the color of the preset ink is determined according to the design of the preset pattern. Preferably, the white ink and the preset ink are LED-UV inks, which have good adhesion and rapid curing ability, can be rapidly cured under ultraviolet irradiation, are conducive to improving printing efficiency, and ensure the stability and reliability of printing quality. Preferably, the coverage of the white ink layer 151 should be greater than or equal to 90%, which means that the white ink layer 151 can cover more than 90% of the color of the underlying gold stamping layer 120, thereby preventing the color of the gold stamping layer 120 from interfering with the preset pattern through the white ink layer 151.
[0042] Compared with the prior art, the embodiment of the utility model provides a printing matter 100 which is printed after gold stamping, solves the common gold falling problem in the traditional printing after gold stamping process. Specifically, the present application can firmly fix the gold stamping layer 120 on the surface of the paper 110 by setting the film layer 130 on the surface of the gold stamping layer 120, thereby avoiding the falling of the gold stamping material (gold stamping layer 120). By setting the primer layer 140 on the surface of the film layer 130, the surface adhesion of the film layer 130 can be enhanced, thereby providing more excellent surface conditions for subsequent printing, ensuring the firm adhesion of the ink, and effectively avoiding problems such as ink falling, fading or blurred printing. By setting the white ink layer 151 on the surface of the primer layer 140, and then setting the pattern layer 152 on the white ink layer 151, the interference of the gold stamping layer 120 on the color of the preset pattern can be avoided, the clear and accurate color presentation of the preset pattern can be ensured, and the ideal printing effect can be achieved.
[0043] Finally, it should be noted that: the above only for the preferred embodiments of the present application, and is not intended to limit the present application, although the foregoing embodiments of the present application have been described in detail, for the skilled in the art, it still can be modified, or for the equivalent replacement of part of the technical features of the technical solutions recorded in the foregoing embodiments. Any modification, equivalent replacement, improvement, etc. made within the spirit and principles of the present application, shall be included within the scope of the present application.
Claims
1. A type of printed material that is hot-stamped before printing, characterized in that, include: Paper, including the first side and the second side; A hot stamping layer is disposed on the first and / or second side of the paper; A coating layer is disposed on the surface of the hot stamping layer; A base oil layer is disposed on the surface of the coating layer; as well as A printed layer is disposed on the surface of the base coat, and the printed layer presents a preset pattern.
2. The printed matter according to claim 1, characterized in that, The paper may be coated paper, offset paper, cardstock, newsprint, or writing paper.
3. The printed matter according to claim 1, characterized in that, The coating layer includes an adhesive layer and a film, wherein the adhesive layer is disposed between the film and the hot stamping layer.
4. The printed matter according to claim 3, characterized in that, The amount of adhesive applied to the adhesive layer is 3-8 g / m². 2 The coating thickness is 5-8μm.
5. The printed matter according to claim 3, characterized in that, The film can be a matte film, a glossy film, a frosted film, a pearl film, or an anti-counterfeiting film.
6. The printed matter according to claim 1, characterized in that, The base oil coating amount of the base oil layer is 1.8g-2.5g / m. 2 The light transmittance of the base oil is greater than or equal to 92%.
7. The printed matter according to claim 1, characterized in that, The printed layer includes: A white ink layer is disposed on the surface of the base oil layer; and A pattern layer is disposed on the surface of the white ink layer and presents the preset pattern.
8. The printed matter according to claim 7, characterized in that, The white ink layer has a coverage rate of 90% or greater.