Device for rivetless joining of metal and composite combination plate
By utilizing the heating and cooling technology of the nailless riveting device, the brittleness of composite materials and the problem of pre-drilled holes in traditional riveting are solved, achieving efficient and reliable connection of metal and composite material composite panels.
Patent Information
- Application Number
- CN202522675562.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-17
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-12-17
Smart Images

Figure CN224952543U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of metal and composite material connection technology, and in particular to a nail-free riveting device for metal and composite material composite plates. Background Technology
[0002] Carbon fiber reinforced composites have advantages such as high specific strength, high specific modulus, fatigue resistance, low coefficient of thermal expansion and good corrosion resistance. They are often combined with metal materials such as aluminum alloys and applied in the automotive and aerospace fields by riveting.
[0003] However, traditional riveting has two major problems: First, carbon fiber composite materials have poor plasticity, and fiber breakage, matrix cracking, interface degumming and delamination are prone to occur during riveting, leading to a decline in joint performance or even failure; Second, pre-drilled holes in the composite material are required before riveting with the metal plate, which not only increases the riveting process, but also increases the difficulty of aligning the tooling and the holes. We urgently need a nailless riveting device for metal and composite material composite plates to solve the above problems. Utility Model Content
[0004] To address the shortcomings of existing technologies, this utility model provides a nail-free riveting device for metal and composite material composite plates. By using a heating element built into the upper die punching die, a lower die annular nitrogen storage area combined with a gas pipe for liquid nitrogen delivery, and a floating structure of the cutting die and the support die, online self-piercing riveting without pre-drilled holes in the composite material is achieved, reducing cracking and delamination of the composite material and improving the performance of the riveted joint.
[0005] The purpose of this utility model is achieved as follows: it includes an upper mold and a lower mold, and further includes: a pressing ring fixedly installed on the upper mold for pressing the sheet metal, a punching die for punching material is coaxially slidable inside the pressing ring, and a heating element for heating is provided inside the punching die; a cutting die floatingly disposed inside the lower mold, a support die for supporting the material is floatingly disposed inside the cutting die, and a cooling element for cooling is provided on the support die.
[0006] Optionally, the heating element includes a placement groove formed on the stamping die, wherein a heater electrically connected to an external power supply unit is fixedly installed in the placement groove, and when the heater is working, a heating zone for the sheet metal is formed on the stamping die.
[0007] Optionally, a first floating groove is provided in the lower mold, and the cutting mold is slidably connected in the first floating groove. A first spring is provided in the first floating groove, and the two ends of the first spring are respectively connected to the bottom wall of the first floating groove and the cutting mold.
[0008] Optionally, the cutting die is provided with a second floating groove, the support die is slidably connected in the second floating groove, a second spring is provided in the second floating groove, and the two ends of the second spring are respectively connected to the support die and the inner wall of the second floating groove.
[0009] Optionally, the cooling component includes an annular step disposed on the top of the support mold. When the end face of the annular step abuts against the plate, the gap between the annular step, the second floating groove and the plate forms an annular nitrogen storage area.
[0010] Optionally, an axial air passage is provided at the inner axis of the support mold, and at least two sets of horizontal air passages are provided at equal intervals in the ring corresponding to the annular nitrogen storage area of the support mold, and the axial air passages are connected to the horizontal air passages.
[0011] Optionally, the lower mold is provided with a gas pipe for conveying nitrogen. The output end of the gas pipe is connected to the axial gas channel, and its input end passes through the cutting mold and the lower mold in sequence and is connected to an external liquid nitrogen system.
[0012] Compared with the prior art, the beneficial effects of this utility model are as follows: 1. This utility model utilizes the cooperation of the lower die support mold, the cutting mold, and the annular nitrogen storage area, combined with the delivery of liquid nitrogen to the annular nitrogen storage area via a gas pipe, to achieve targeted cooling of the composite material punching area. This rapidly increases the brittleness of the composite material to achieve online brittle fracture punching, eliminating the need for pre-drilling holes in the composite material. This not only eliminates the hole-making process in traditional riveting but also solves the problem of aligning tooling with holes, significantly simplifying the riveting process of metal and composite material composite plates and improving production efficiency.
[0013] 2. This utility model ensures the plastic deformation capability of the metal sheet during punching and forming by using the heating element built into the upper die punching die. Combined with the liquid nitrogen cooling system of the lower die, it achieves tear-free and delamination-free brittle fracture punching of the composite material. At the same time, the metal sheet forms a flange structure during the forming process, which wraps around the punching hole area of the composite material in the opposite direction. This can cover the micro-defects at the edge of the punching hole, which not only reduces the damage during composite material riveting, but also significantly improves the static tensile performance and fatigue performance of the metal-composite material riveting joint, ensuring the reliability of the connection. Attached Figure Description
[0014] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort.
[0015] Figure 1 This is a schematic diagram of the orthographic structure of the upper and lower molds provided by this utility model.
[0016] Figure 2 This is a cross-sectional structural diagram of the upper and lower molds provided by this utility model.
[0017] Figure 3This is a schematic diagram of the support mold structure provided by this utility model.
[0018] Figure 4 This is a schematic diagram of the axial and horizontal air passage structures provided by this utility model.
[0019] Figure 5 This is a schematic diagram of the riveting connection provided by this utility model.
[0020] Figure 6 This is a schematic diagram of the punching and riveting process provided by this utility model.
[0021] In the diagram: 1. Upper mold; 2. Lower mold; 3. Pressure ring; 4. Punching mold; 5. Cutting mold; 6. Support mold; 7. Placement groove; 8. Heater; 9. First floating groove; 10. First spring; 11. Second floating groove; 12. Second spring; 13. Annular step; 14. Axial air passage; 15. Horizontal air passage; 16. Air pipe. Detailed Implementation
[0022] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0023] like Figure 1-6 As shown in the figure, the present invention provides a nail-free riveting device for a metal and composite material composite plate, including an upper mold 1 and a lower mold 2. It also includes a pressure ring 3 fixedly installed on the upper mold 1 for pressing the sheet metal, and a punching die 4 for punching is coaxially slidable inside the pressure ring 3.
[0024] Here, the pressure ring 3 is fixedly installed on the lower end face of the upper mold 1, and its inner wall is clearance-fitted with the outer wall of the stamping die 4 to ensure that the stamping die 4 can slide smoothly along the axial direction of the pressure ring 3; the lower end face of the pressure ring 3 is a flat structure and its area is slightly larger than the overlapping area of the plates to be riveted. In the initial stage of riveting, the pressure ring 3 can contact the surface of the upper metal plate before the stamping die 4 and apply a uniform clamping force.
[0025] Furthermore, the overlapping structure of the metal sheet and the composite material sheet can be positioned and pressed before punching and forming to prevent the sheet from sliding or misaligning laterally during the subsequent pressing of the punching die 4 and the forming of the composite material and the metal sheet. This helps to ensure the accuracy of the riveting position and reduce the riveting deviation caused by the displacement of the sheet. At the same time, the uniform pressing force can also reduce the premature deformation of the composite material sheet due to uneven local stress, providing a stable support foundation for the subsequent punching process.
[0026] Furthermore, the stamping die 4 has a columnar structure with a punch at its lower end that matches the hole to be punched. The edge of the punch has a smooth transition structure to avoid scratching the metal sheet during punching. The heating element placement groove 7 is opened inside the stamping die 4 and extends along the axial direction of the stamping die 4. The position of the placement groove 7 corresponds to the punch area to ensure that the heat generated by the heater 8 can be efficiently transferred to the punch. The punch design of the stamping die 4 can adapt to the punching requirements of composite materials and the forming requirements of metal sheets, and the smooth edge reduces damage to the metal sheet.
[0027] The stamping die 4 is equipped with a heating element for heating. The heating element includes a placement groove 7 opened on the stamping die 4. A heater 8 electrically connected to an external power supply unit is fixedly installed in the placement groove 7. When the heater 8 is working, a heating zone for the sheet material is formed on the stamping die 4.
[0028] Here, heater 8 uses a pulse heating component, which is connected to an external power supply unit through a high-temperature resistant wire. The heating temperature and heating time can be adjusted according to the material of the metal plate (such as aluminum alloy or magnesium alloy). When heater 8 is working, a stable heating zone is formed in the punch area, covering the contact area between the punch and the metal plate. Pulse heater 8 can specifically increase the temperature of the metal plate in the punch contact area, which helps to ensure the plastic deformation ability of the metal plate during the punching process and avoid defects such as cracking or breakage of the metal plate due to low temperature or insufficient plasticity. At the same time, the adjustability of heating temperature and time allows the device to be adapted to metal plates of different materials and thicknesses, improving the versatility of the device.
[0029] The cutting mold 5 is floating inside the lower mold 2. The lower mold 2 has a first floating groove 9. The cutting mold 5 is slidably connected to the first floating groove 9. A first spring 10 is provided in the first floating groove 9. The two ends of the first spring 10 are respectively connected to the bottom wall of the first floating groove 9 and the cutting mold 5.
[0030] Here, the first floating groove 9 inside the lower mold 2 is a cylindrical hollow cavity, and the cutting mold 5 is slidably connected inside the first floating groove 9; the first spring 10 is disposed between the bottom wall of the first floating groove 9 and the lower end face of the cutting mold 5, with its two ends abutting against the bottom wall of the first floating groove 9 and the lower end face of the cutting mold 5 respectively. In the initial state, the first spring 10 is in a naturally extended state, and the top height of the cutting mold 5 is higher than the top height of the lower mold 2.
[0031] Furthermore, the first spring 10 can provide stable support for the cutting die 5. During the pressing process of the punching die 4, the cutting die 5 can gradually compress the first spring 10 and float downwards with the pressure, providing space for the subsequent metal plate to expand and form along the gap between the cutting die 5 and the composite material plate. After the riveting is completed, the restoring force of the first spring 10 can drive the cutting die 5 to move upwards, creating conditions for the ejection of composite material waste and adapting to the automation requirements of the riveting process.
[0032] A support mold 6 for supporting the material is floating inside the cutting mold 5. A second floating groove 11 is provided on the cutting mold 5. The support mold 6 is slidably connected in the second floating groove 11. A second spring 12 is provided in the second floating groove 11. The two ends of the second spring 12 are respectively connected to the support mold 6 and the inner wall of the second floating groove 11.
[0033] Here, the second floating groove 11 inside the cutting mold 5 is a cylindrical cavity adapted to the support mold 6, and the support mold 6 is slidably connected inside the second floating groove 11; the top surface of the support mold 6 is a flat structure used to support the lower composite material plate, and the annular step 13 in the middle of its outer side wall forms an adaptation gap with the inner wall of the second floating groove 11; the second spring 12 is disposed between the lower end surface of the support mold 6 and the inner bottom wall of the second floating groove 11, and its two ends abut against the support mold 6 and the inner bottom wall of the second floating groove 11 respectively. In the initial state, the elongation of the second spring 12 is greater than that of the first spring 10, and the top height of the support mold 6 is higher than the top height of the cutting mold 5.
[0034] Furthermore, the top surface of the support mold 6 can provide stable support for the composite material plate, preventing the composite material plate from bending and deforming before the pressure ring 3 is pressed. The second spring 12 can provide balanced support and reset force for the support mold 6. During punching, the support mold 6 can move downward with the pressure of the punching die 4 to compress the second spring 12, ensuring a smooth punching process and preventing the composite material from cracking due to a sudden increase in force. At the same time, the downward movement of the support mold 6 can cooperate with the punch to complete the punching of the composite material, so that the punched composite material waste falls into the second floating groove 11. After riveting is completed, the reset of the second spring 12 can drive the support mold 6 to move upward, pushing out the waste material and realizing automatic discharge of waste material, reducing manual cleaning steps.
[0035] The support mold 6 is provided with a cooling component for cooling down. The cooling component includes an annular step 13 set on the top of the support mold 6. When the end face of the annular step 13 abuts against the plate, the gap between the annular step 13, the second floating groove 11 and the plate forms an annular nitrogen storage area.
[0036] Here, the annular step 13 of the support mold 6 is a raised structure extending circumferentially along the outer side wall of the support mold 6. Its height is adapted to the thickness of the composite material plate to be riveted. The upper surface of the annular step 13 is a flat structure to ensure good fit when in contact with the composite material plate. When the pressure ring 3 presses the plate, the upper surface of the annular step 13 abuts tightly against the lower surface of the composite material plate. At this time, the outer side wall of the annular step 13, the inner side wall of the second floating groove 11, and the lower surface of the composite material plate together enclose a closed annular nitrogen storage area. The volume of the annular nitrogen storage area can be adjusted according to the punching area of the composite material to ensure that it can accommodate enough liquid nitrogen to cover the punching area.
[0037] Furthermore, the annular nitrogen storage zone can concentrate liquid nitrogen in the specific area of the composite material that needs to be punched, achieving targeted cooling and preventing liquid nitrogen diffusion that could lead to performance degradation in other areas of the composite material due to overcooling. The tight fit between the annular step 13 and the composite material plate can reduce liquid nitrogen leakage, improve cooling efficiency, and enable the punching area of the composite material to reach the required low temperature in a short time. This significantly improves the brittleness of the composite material, making it easier for the composite material to fracture along the inner wall of the cutting die 5 during subsequent punching by the punching die 4. This reduces defects such as fiber tearing and delamination, and ensures the edge quality of the composite material after punching.
[0038] An axial air passage 14 is provided at the inner axis of the support mold 6. At least two sets of horizontal air passages 15 are provided at equal intervals in the ring corresponding to the annular nitrogen storage area of the support mold 6. The axial air passage 14 and the horizontal air passages 15 are connected. A gas pipe 16 for conveying nitrogen is provided in the lower mold 2. The output end of the gas pipe 16 is connected to the axial air passage 14. Its input end passes through the cutting mold 5 and the lower mold 2 in sequence and is connected to the external liquid nitrogen system.
[0039] Here, the axial air passage 14 in the support mold 6 is a through hole opened along the axis of the support mold 6, and its inner wall is smoothed to reduce the resistance when liquid nitrogen flows; the horizontal air passage 15 is opened radially along the support mold 6 and is evenly distributed along the circumference of the annular nitrogen storage area. One end of each set of horizontal air passages 15 is connected to the axial air passage 14, and the other end extends to the inner wall of the annular nitrogen storage area; the inner walls of the axial air passage 14 and the horizontal air passage 15 are both rust-proofed to adapt to the low temperature environment of liquid nitrogen.
[0040] Furthermore, the axial air passage 14 can efficiently guide the liquid nitrogen delivered by the air pipe 16 into the interior of the support mold 6, and the smooth inner wall reduces the flow resistance of the liquid nitrogen, ensuring the liquid nitrogen delivery speed; the uniformly distributed horizontal air passage 15 can uniformly deliver liquid nitrogen to various positions in the annular nitrogen storage area, so that the liquid nitrogen temperature distribution in the annular nitrogen storage area is consistent, thereby ensuring that the cooling temperature of the composite material punching area is uniform, avoiding the situation that some areas are difficult to break or some areas are excessively brittle due to insufficient local cooling, thus improving the stability of the punching quality.
[0041] Furthermore, the air pipe 16 is made of a low-temperature resistant material to adapt to the low-temperature environment of liquid nitrogen and avoid material brittleness due to low temperature during long-term use; the outer diameter of the air pipe 16 is matched with the inner diameter of the axial air passage 14, and the connection between the two is a sealed fit to ensure sealing performance and prevent liquid nitrogen leakage; the input end of the air pipe 16 is connected to the external liquid nitrogen system, and the arrangement of the air pipe 16 inside the lower mold 2 is along the inner wall of the lower mold 2 and avoids the floating path of the cutting mold 5 and the support mold 6 to avoid interference with moving parts.
[0042] It is important to note that the low-temperature resistant material ensures the structural stability and service life of the gas pipe 16 during the liquid nitrogen transport process, reducing safety hazards caused by material failure; the sealed fit can effectively prevent liquid nitrogen leakage, improving cooling efficiency while avoiding damage to other parts of the lower mold 2 caused by low temperature; the reasonable arrangement of the gas pipe 16 avoids interference with moving parts, ensuring smooth floating flow of the cutting mold 5 and the support mold 6, and not affecting the normal progress of the riveting process.
[0043] Working principle and usage process of this utility model: Equipment assembly process: Assembly of upper mold 1: Fix the pressure ring 3 to the lower end face of the upper mold 1 with bolts, ensuring that the axis of the pressure ring 3 coincides with the axis of the upper mold 1; pass the punching die 4 through the inner wall of the pressure ring 3, and adjust the gap between the two to 0.1~0.2mm to ensure that the punching die 4 can slide smoothly; install the heater 8 into the placement slot 7 of the punching die 4, connect it to the external power supply unit through a high-temperature resistant wire, test the heating function of the heater 8, and ensure that the punch area can be stably heated.
[0044] Assembly of lower mold 2: Place the first spring 10 into the bottom wall of the first floating groove 9 of the lower mold 2, and then place the cutting mold 5 into the first floating groove 9, so that the upper end of the first spring 10 abuts against the lower end face of the cutting mold 5; place the second spring 12 into the bottom wall of the second floating groove 11 of the cutting mold 5, and then place the support mold 6 into the second floating groove 11, so that the upper end of the second spring 12 abuts against the lower end face of the support mold 6; pass the air pipe 16 through the side walls of the lower mold 2 and the cutting mold 5, and insert it into the axial air passage 14 of the support mold 6, ensuring that the air pipe 16 and the axial air passage 14 are sealed together, and finally connect the input end of the air pipe 16 to the external liquid nitrogen system; check the floating condition of the cutting mold 5 and the support mold 6 to ensure that they can slide smoothly along the axial direction without any jamming. Riveting operation procedure: A: Plate placement: Stack the upper metal plate (such as aluminum alloy plate, 1-3mm thick) with the lower composite material plate (such as carbon fiber reinforced composite material plate, 2-4mm thick), so that the center of the stacked plate is aligned with the axis of the support mold 6, and place it on the top surface of the support mold 6. At this initial state, the top of the support mold 6 is higher than the top of the cutting mold 5, and the top of the cutting mold 5 is higher than the top of the lower mold 2.
[0045] B: Plate clamping and positioning: Start the drive mechanism of the upper mold 1, which drives the upper mold 1 to move downward. The pressure ring 3 first contacts the upper end face of the metal plate. The upper mold 1 continues to move downward, and the pressure ring 3 applies a clamping force of 10-15kN. At this time, the support mold 6 and the cutting mold 5 compress the second spring 12 and the first spring 10 respectively under pressure, and gradually move downward until the top of the support mold 6 and the cutting mold 5 are flush with the top of the lower mold 2. The plate is completely positioned and clamped.
[0046] C, D: Composite material cooling: Start the external liquid nitrogen system and deliver liquid nitrogen to the axial air passage 14 of the support mold 6 through the air pipe 16. The liquid nitrogen enters the annular nitrogen storage area through the horizontal air passage 15. The pulse nitrogen passage method is adopted (nitrogen passage for 3-5 seconds, stop for 1-2 seconds, repeat 2-3 times) to reduce the temperature of the composite material punching area to -80~-100℃, and the brittleness of the composite material is significantly improved.
[0047] E: Composite material punching: The heating element is activated to raise the temperature of the punch area of the punching die 4 to 150-200℃ (suitable for aluminum alloy plates). At the same time, the upper die 1 is driven to continue to move downward. The punch of the punching die 4 contacts the metal plate and heats the metal plate. As the punching die 4 continues to press down, the support die 6 compresses the second spring 12 and moves further downward. Under the action of punch pressure and low temperature brittleness, the composite material breaks brittlely along the inner wall of the cutting die 5. The blanked composite material waste falls into the second floating groove 11 until the support die 6 is pressed to the bottom of the second floating groove 11.
[0048] F: Metal sheet forming and interlocking: The punching die 4 continues to press down, and the cutting die 5 compresses the first spring 10 and moves downward under pressure. A gap of 1-2 mm is formed between the top of the cutting die 5 and the lower end face of the composite material plate. Under the pressure of the punch and the action of heating, the metal sheet expands and deforms in all directions along the gap to form a flange structure until the cutting die 5 is pressed to the bottom of the first floating groove 9. The punch of the punching die 4 is completely pressed into the plate. The flange of the metal sheet wraps around the punching hole area of the composite material in the opposite direction, realizing the reverse wrapping interlocking of the metal and the composite material.
[0049] G: Reset and waste discharge: Stop the heating element and liquid nitrogen system, drive the upper mold 1 to reset upward; the first spring 10 and the second spring 12 gradually return to their original state under the action of elasticity, drive the cutting mold 5 and the support mold 6 to move upward, and the support mold 6 pushes out the composite material waste in the second floating groove 11 during the movement. Finally, the riveted metal-composite material combination plate is removed, and one riveting process is completed.
[0050] The above description of the embodiments is only for the purpose of helping to understand the method and core idea of this utility model. It should be noted that for those skilled in the art, several improvements and modifications can be made to this utility model without departing from the principle of this utility model, and these improvements and modifications also fall within the protection scope of the claims of this utility model.
Claims
1. A metal and composite combination plate nail-less riveting device comprising an upper die (1) and a lower die (2), characterized in that: Also include: Fixedly installed on the upper die (1) for pressing the edge of the plate (3), the edge of the plate (3) coaxially sliding for punching material punching die (4), the punching die (4) is provided with heating for heating; Floating in the lower die (2) cutting material die (5), the cutting material die (5) is provided with a support die (6) for supporting material, the support die (6) is provided with cooling for cooling.
2. The metal-to-composite panel blind rivet apparatus of Claim 1, wherein The heating element includes the placement slot (7) opened on the punching die (4), the placement slot (7) is fixedly installed with the heater (8) electrically connected with the external power supply unit, when the heater (8) works, the punching die (4) forms the heating area of the plate.
3. The metal-to-composite panel, fastenerless riveting apparatus of Claim 1, wherein: The first floating groove (9) is opened in the lower die (2), the cutting material die (5) is slidingly connected in the first floating groove (9), the first spring (10) is arranged in the first floating groove (9), and the two ends of the first spring (10) are respectively connected with the bottom wall in the first floating groove (9) and the cutting material die (5).
4. The metal-to-composite panel, fastenerless riveting apparatus of Claim 3, wherein: The second floating groove (11) is opened on the cutting material die (5), the support die (6) is slidingly connected in the second floating groove (11), the second spring (12) is arranged in the second floating groove (11), and the two ends of the second spring (12) are respectively connected with the support die (6) and the inner wall of the second floating groove (11).
5. The metal-to-composite panel, fastenerless riveting apparatus of Claim 1, wherein: The cooling element includes the annular step (13) arranged on the top of the support die (6), when the end surface of the annular step (13) abuts against the plate, the gap between the annular step (13), the second floating groove (11) and the plate forms an annular nitrogen storage area.
6. The metal-to-composite panel, fastenerless riveting apparatus of Claim 5, wherein: The axial air duct (14) is opened in the support die (6) at the axis, at least two groups of horizontal air ducts (15) are annularly and equidistantly opened in the support die (6) corresponding to the position of the annular nitrogen storage area, and the axial air duct (14) and the horizontal air duct (15) are communicated.
7. The metal-to-composite panel rivetless joining apparatus of Claim 1, wherein: The gas pipe (16) for conveying nitrogen is arranged in the lower die (2), the output end of the gas pipe (16) is communicated with the axial air duct (14), the input end of the gas pipe (16) penetrates the cutting material die (5) and the lower die (2) in sequence and is connected with the external liquid nitrogen system.