An ultra-thin 0.3mm protective film structure made of HIPS ABS material

By combining a substrate layer, a reinforcing structural layer, and a surface treatment layer made of HIPS/ABS material, the problems of insufficient strength and easy deformation of the protective film during the ultra-thinning process are solved, and a protective film structure with high strength, flexibility and deformation resistance is achieved, which is suitable for electronic devices and precision instruments.

CN224952683UActive Publication Date: 2026-11-10YANGZHOU DEWEI NEW MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521468870.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-07-14
Publication Date
2026-11-10
Estimated Expiration
2035-07-14

AI Technical Summary

Technical Problem

Existing protective films suffer from insufficient strength and easy deformation during the ultra-thinning process, affecting assembly accuracy and aesthetics. At the same time, traditional designs are prone to bending and deformation during use, leading to a decrease in protective effect.

Method used

The design incorporates a combination of a substrate layer, a reinforcing structural layer, and a surface treatment layer made of HIPS/ABS material. The substrate layer features a honeycomb microporous structure, the reinforcing structural layer is woven with mesh-like fibers, and the surface treatment layer is made of fluorinated polymer. Stable bonding of each layer is achieved through plasma treatment, hot pressing, and ultraviolet curing processes.

Benefits of technology

It achieves high strength, flexibility and deformation resistance in a 0.3mm ultra-thin protective film, improving the overall performance of the protective film and making it suitable for electronic equipment and precision instruments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224952683U_ABST
    Figure CN224952683U_ABST
Patent Text Reader

Abstract

This application relates to the field of protective film technology, and in particular to an ultra-thin 0.3mm protective film structure made of HIPS / ABS material, comprising a substrate layer, a reinforcing structural layer, and a surface treatment layer. The substrate layer is made of a HIPS / ABS blend, with a thickness of 0.25mm and an internal honeycomb microporous structure. The reinforcing structural layer is made of high-strength polyester fibers woven into a mesh and bonded to the substrate layer by hot pressing, with a thickness of 0.05mm. The surface treatment layer is a fluorinated polymer, sprayed and then cured under ultraviolet light, with a thickness of 0.01mm. This application reduces weight and enhances flexibility through the microporous structure, improves tensile strength and deformation resistance through the mesh design, and reduces light reflection through surface texture, thus enhancing visual appeal. This application achieves an ultra-thin design while possessing high strength, high flexibility, and excellent stain and abrasion resistance, making it suitable for electronic devices and precision instruments.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model belongs to the field of polymer materials and surface protection technology, specifically a 0.3mm ultrathin protective film structure made of HIPSABS material. Background Technology

[0002] HIPS and ABS materials are widely used in the manufacture of protective films due to their excellent impact resistance, toughness, and ease of processing. In modern industrial production, the demand for ultra-thin protective films is increasing, especially in fields such as electronic equipment and precision instruments, where higher requirements are placed on the thickness and performance of protective films.

[0003] Existing protective membrane structures typically employ a relatively thick design to ensure strength and durability. However, in certain applications, excessively thick protective membranes can negatively impact assembly precision and aesthetics. Furthermore, traditional protective membranes may experience bending and deformation during production and use, affecting their protective effectiveness. While some products have attempted to improve performance by optimizing material ratios, achieving ultra-thinness while maintaining both strength and flexibility remains a technical challenge.

[0004] Therefore, to address the above issues, an ultra-thin 0.3mm protective film structure made of HIPS / ABS material is proposed to meet the higher requirements for protective film thickness and performance. Utility Model Content

[0005] This utility model relates to the field of protective film technology, specifically to an ultra-thin 0.3mm protective film structure made of HIPS / ABS material. Existing protective films present a trade-off between thickness and performance; excessively thick designs affect assembly precision and aesthetics, while ultra-thin designs often struggle to balance strength and flexibility. Furthermore, traditional protective films are prone to bending and deformation during use, leading to a decrease in their protective effect. To address these issues, this utility model provides a novel protective film structure that aims to achieve ultra-thinness while significantly improving strength and resistance to deformation.

[0006] This utility model provides an ultra-thin 0.3mm protective film structure made of HIPS / ABS material, comprising a substrate layer, a reinforcing structure layer, and a surface treatment layer. The substrate layer is made of a mixture of HIPS and ABS in a certain proportion, exhibiting excellent impact resistance and toughness. The reinforcing structure layer is located inside the substrate layer and is bonded to the substrate layer through an embedded connection. The surface treatment layer covers the outer surface of the substrate layer and forms a stable bond with the substrate layer through chemical bonding.

[0007] The substrate layer has a thickness of 0.25 mm and contains multiple microporous structures arranged in a honeycomb pattern, with each micropore having a diameter of 10-20 μm. This microporous structure effectively reduces the weight of the substrate layer while enhancing its flexibility. Both surfaces of the substrate layer undergo plasma treatment to improve its bonding strength with the reinforcing structure layer and the surface treatment layer.

[0008] The reinforcing structural layer is composed of multiple fiber filaments made of high-strength polyester material, which are woven together to form a mesh structure. The nodes of the mesh structure are fixedly connected to the substrate layer via a hot-pressing process, ensuring the stability between the reinforcing structural layer and the substrate layer. The reinforcing structural layer is 0.05 mm thick, with a mesh density of 100-150 nodes per square centimeter, which significantly improves the overall tensile strength and deformation resistance of the protective film.

[0009] The surface treatment layer has a thickness of 0.01 mm and its main component is a fluoropolymer, exhibiting excellent wear resistance and stain resistance. The surface treatment layer is uniformly applied to the outer surface of the substrate layer using a spraying process, followed by UV curing to ensure a strong chemical bond between the surface treatment layer and the substrate layer. The outer surface of the surface treatment layer also features a micron-level textured structure with a depth of 1-2 μm, effectively reducing the reflection of external light and thus enhancing the visual appeal of the protective film.

[0010] In this invention, the bonding principle between the substrate layer, the reinforcing structure layer, and the surface treatment layer is as follows: First, the substrate layer generates active groups on its surface through plasma treatment. These active groups can physically adsorb onto the surface of the fibers in the reinforcing structure layer, initially fixing their positions. Second, the mesh structure of the reinforcing structure layer interlocks with the microporous structure of the substrate layer through a hot-pressing process, further enhancing the bonding strength between the two. Finally, the surface treatment layer forms a chemical bond with the substrate layer through spraying and ultraviolet curing processes, ensuring the overall stability of the three-layer structure.

[0011] This invention, through the aforementioned structural design, solves the problems of insufficient strength and easy deformation in existing protective films during the ultra-thinning process. The microporous structure of the substrate layer reduces weight while enhancing flexibility, the grid design of the reinforcing structural layer significantly improves tensile strength and resistance to deformation, and the fluoropolymer component of the surface treatment layer endows the protective film with excellent abrasion resistance and stain resistance. In addition, the micron-level textured structure of the surface treatment layer reduces light reflection, improves the visual effect of the protective film, and makes it more suitable for electronic devices and precision instruments.

[0012] The various layers of this invention are tightly integrated through specific processes and connection methods, forming a protective membrane structure with excellent overall performance. This structure not only achieves an ultra-thin design of 0.3mm, but also possesses high strength, high flexibility, and good resistance to deformation, meeting the high-performance requirements of modern industry for protective membranes. Attached Figure Description

[0013] Figure 1 This is a schematic diagram of the overall structure of the present invention, showing the three-layer structure of the protective film and their relative positions.

[0014] Figure 2 This is a partial enlarged view of the substrate layer of this utility model, which focuses on showing the honeycomb microporous structure and its distribution morphology inside the substrate layer.

[0015] Figure 3 This is a schematic diagram of the mesh structure of the reinforcing structural layer of this utility model, which shows in detail the weaving method of the fiber filaments and the distribution of nodes.

[0016] Figure 4 This is a schematic diagram of the outer surface texture structure of the surface treatment layer of this utility model, highlighting the arrangement and depth characteristics of the micron-level texture.

[0017] The attached figures are labeled as follows:

[0018] 1. Substrate layer; 2. Reinforcing structure layer; 3. Surface treatment layer; 4. Microporous structure; 5. Fiber filament; 6. Mesh structure; 7. Micron-level texture structure. Detailed Implementation

[0019] This invention provides an ultra-thin 0.3mm protective film structure made of HIPS / ABS material, the overall structure of which is as follows: Figure 1 As shown, the structure includes a substrate layer 1, a reinforcing structural layer 2, and a surface treatment layer 3. The substrate layer 1, as the core load-bearing component, is located in the middle of the entire protective film structure, with its upper and lower sides tightly bonded to the reinforcing structural layer 2 and the surface treatment layer 3, respectively. The reinforcing structural layer 2 is embedded inside the substrate layer 1 and fixed by a hot-pressing process, while the surface treatment layer 3 covers the outer surface of the substrate layer 1 and forms a strong connection with it through chemical bonding.

[0020] The substrate layer 1 has a thickness of 0.25 mm, and its main materials are HIPS and ABS mixed in a certain proportion, specifically HIPS accounting for 60%-70% and ABS accounting for 30%-40%. The substrate layer 1 contains multiple microporous structures 4, which are distributed in a honeycomb pattern. Figure 2As shown, each micropore has a diameter of 10-20 μm, and the center-to-center distance between adjacent micropores is 30-50 μm. The design of the microporous structure 4 not only reduces the overall weight of the substrate layer 1, but also enhances its flexibility through the honeycomb arrangement. The two sides of the substrate layer 1 are plasma treated to generate active groups on their surfaces. These active groups can physically adsorb onto the fibers 5 in the reinforcing structure layer 2, thereby initially fixing their positions.

[0021] The reinforcing structural layer 2 is located inside the substrate layer 1, with a thickness of 0.05 mm. It consists of multiple fiber filaments 5, which are made of high-strength polyester material. The fiber filaments 5 are woven together to form a mesh structure 6, such as... Figure 3 As shown, the node density of the mesh structure 6 is 100-150 nodes per square centimeter. The diameter of the fiber filament 5 is 20-30 μm, and the weaving angle is 45°-60°. This weaving method ensures that the mesh structure 6 has uniform tensile strength in all directions. The reinforcing layer 2 is bonded to the substrate layer 1 through a hot-pressing process. The hot-pressing temperature is 180℃-200℃, the pressure is 10-15 MPa, and the time is 20-30 seconds. During this process, the nodes of the fiber filament 5 interlock with the microporous structure 4 inside the substrate layer 1, further enhancing the bonding strength between the two.

[0022] Surface treatment layer 3 covers the outer surface of substrate layer 1, with a thickness of 0.01 mm, and its main component is fluoropolymer. Surface treatment layer 3 is uniformly applied to the outer surface of substrate layer 1 using a spraying process, with a spraying pressure of 0.2-0.3 MPa and a spraying distance of 10-15 cm. After spraying, surface treatment layer 3 is cured in an ultraviolet curing device with an ultraviolet wavelength of 365 nm, an irradiation time of 5-10 seconds, and a power density of 800-1000 mW / cm². 2 During this process, the fluorinated polymer molecules react chemically with the active groups on the surface of the substrate layer 1, forming strong chemical bonds. The outer surface of the surface treatment layer 3 is provided with a micron-level textured structure 7, such as... Figure 4 As shown, the texture structure 7 has a depth of 1-2 μm, a width of 5-10 μm, and a spacing of 20-30 μm between textures. The texture structure 7 is formed by a mold pressing process, with a mold temperature of 120℃-150℃, a pressure of 5-8 MPa, and a pressing time of 10-15 seconds.

[0023] In practical applications, the protective film structure of this invention can be used for screen protection of electronic devices or housing protection of precision instruments. Taking screen protection of electronic devices as an example, the installation process of the protective film is as follows: First, place the protective film on the screen surface, ensuring that its edges are aligned with the screen bezel; then, use a roller tool to roll it from the center to the edge to remove air between the protective film and the screen; finally, gently wipe the outer surface of the surface treatment layer 3 with a soft cloth to remove residual dust or fingerprints. Because the micron-level textured structure 7 of the surface treatment layer 3 reduces light reflection, the installed protective film significantly improves the visual effect of the screen. At the same time, the fluoropolymer component gives it excellent wear resistance and stain resistance, effectively extending the screen's lifespan.

[0024] The three-layer structure of the protective film is tightly bonded together through specific processes and connection methods, forming a high-performance overall protective film structure. The microporous structure 4 of the substrate layer 1 reduces weight and enhances flexibility through a honeycomb arrangement. The mesh structure 6 of the reinforcing layer 2 significantly improves tensile strength and deformation resistance through the weaving method of the fiber filaments 5 and hot-pressing process. The fluoropolymer component of the surface treatment layer 3 forms a strong chemical bond with the substrate layer 1 through spraying and UV curing processes, ensuring the overall stability of the three-layer structure. The parameters for the complete hot-pressing and UV curing processes have been verified through multiple experiments to ensure that the bonding strength between each layer meets the requirements of actual use.

[0025] To enable those skilled in the art to fully understand and implement this utility model, the following supplementary explanation of the specific implementation principle of this utility model is provided in conjunction with a specific application scenario.

[0026] Firstly, in the practical application of screen protectors for electronic devices, the installation of the protective film must strictly follow the operating procedures to ensure its optimal performance. When placing the protective film on the screen surface, it is necessary to ensure that its edges are aligned with the screen bezel. The key to this step lies in the flexible design of the substrate layer 1. Its internal honeycomb microporous structure 4 effectively reduces the overall weight through a specific arrangement, while enhancing the material's bending adaptability, allowing the protective film to fit tightly against the screen surface without wrinkles or bubbles.

[0027] Subsequently, a roller tool is used to roll from the center to the edge to remove air between the protective film and the screen. During this process, the mesh structure 6 of the reinforcing structural layer 2 plays a crucial role. The fiber filaments 5 are woven to form a node density of 100-150 nodes per square centimeter, with the weaving angle controlled between 45° and 60°. This design ensures a uniform distribution of tensile strength in all directions for the protective film. When pressure is applied by the roller, the nodes of the fiber filaments 5 interlock with the microporous structure 4 inside the substrate layer 1, further enhancing the overall stability of the protective film and preventing deformation or tearing caused by external forces.

[0028] Finally, gently wipe the outer surface of the surface treatment layer 3 with a soft cloth to remove any residual dust or fingerprints. The micron-level textured structure 7 of the surface treatment layer 3 is formed through a die-pressing process, with a depth of 1-2 μm, a width of 5-10 μm, and a spacing of 20-30 μm between textures. This design not only reduces the reflection of external light but also enhances the visual effect of the screen. Furthermore, the main component of the surface treatment layer 3 is a fluorinated polymer, which is uniformly coated onto the outer surface of the substrate layer 1 through a spraying process and chemically bonded in an ultraviolet curing device. The ultraviolet light wavelength is 365 nm, the irradiation time is 5-10 seconds, and the power density is 800-1000 mW / cm². 2 The selection of these parameters has been verified through multiple experiments to ensure a strong bond between the fluorinated polymer molecules and the surface active groups of the substrate layer 1, thereby giving the protective film excellent wear resistance and anti-fouling properties.

[0029] Throughout the installation process, the synergistic effect of the three-layer structure of the protective film is fully demonstrated. The honeycomb microporous structure 4 of the substrate layer 1, through plasma treatment, generates active groups that physically adsorb onto the fibers 5 in the reinforcing structure layer 2, initially fixing their positions. Subsequently, a hot-pressing process further strengthens the bond between the reinforcing structure layer 2 and the substrate layer 1, ensuring that the protective film is not easily delaminated or peeled off during use. The surface treatment layer 3, through spraying and UV curing processes, forms a chemical bond with the substrate layer 1, ensuring the overall stability of the three-layer structure.

[0030] By combining the above steps and principles, the protective film structure of this invention achieves an ultra-thin design in practical applications while significantly improving strength, flexibility, and resistance to deformation. Its superior performance not only meets the high-performance requirements of modern industry for protective films but also provides a reliable solution for screen protection of electronic devices.

[0031] The above description is merely a preferred embodiment of this utility model and is not intended to limit this utility model. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.

Claims

1. A 0.3mm ultra-thin protective film structure made of HIPS ABS material, characterized in that, It includes a substrate layer (1), a reinforcing structure layer (2) and a surface treatment layer (3). The substrate layer (1) is located in the middle of the protective film structure, the reinforcing structure layer (2) is embedded inside the substrate layer (1), and the surface treatment layer (3) covers the outer surface of the substrate layer (1).

2. The ultra-thin 0.3mm protective film structure of HIPS ABS material according to claim 1, characterized in that, The reinforcing structure layer (2) is composed of multiple fiber filaments (5), which are made of high-strength polyester material. The fiber filaments (5) form a mesh structure (6) by weaving. The node density of the mesh structure (6) is 100-150 nodes per square centimeter. The diameter of the fiber filaments (5) is 20-30 μm, and the weaving angle is 45°-60°.

3. The ultra-thin 0.3mm protective film structure of HIPS ABS material according to claim 1, characterized in that, The surface treatment layer (3) has a thickness of 0.01 mm and its main component is a fluorinated polymer. The outer surface of the surface treatment layer (3) is provided with a micron-level texture structure (7). The texture structure (7) has a depth of 1-2 μm, a width of 5-10 μm, and a spacing of 20-30 μm between textures.

4. The ultra-thin 0.3mm protective film structure of HIPS ABS material according to claim 1, characterized in that, The two sides of the substrate layer (1) are plasma treated to generate active groups on its surface. The active groups physically adsorb onto the fibers (5) in the reinforcing structure layer (2).

5. The ultra-thin 0.3mm protective film structure of HIPS ABS material according to claim 1, characterized in that, The reinforcing structure layer (2) is bonded to the substrate layer (1) by a hot pressing process. The hot pressing temperature is 180℃-200℃, the pressure is 10-15MPa, and the time is 20-30 seconds. The nodes of the fiber filaments (5) are inter-embedded with the microporous structure (4) inside the substrate layer (1).

6. The ultra-thin 0.3mm protective film structure of HIPS ABS material according to claim 1, characterized in that, The micron-scale texture structure (7) of the surface treatment layer (3) is formed by a mold pressing process, with a mold temperature of 120℃-150℃, a pressure of 5-8MPa, and a pressing time of 10-15 seconds.