Winded cells, batteries and electrical equipment
By setting specially designed grooves on the negative electrode sheet of the wound cell, the lithium plating problem is solved, lithium ion transport and current distribution are improved, the cycle life of the battery is extended and the safety is improved, making it suitable for industrial production.
Patent Information
- Application Number
- CN202522484189.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-24
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-11-24
AI Technical Summary
The large gap between the separator and the electrode at the corner of the wound cell leads to lithium plating, affecting the cell's cycle life and safety.
Multiple first and second grooves are provided on the negative electrode sheet. The first and second grooves are equally spaced along the unfolding direction of the negative electrode sheet. The distance between two adjacent first grooves is greater than the distance between two adjacent second grooves. The product of the width and depth of the first groove is greater than or equal to 1.5 times the width and depth of the second groove. The groove shape is preferably wavy. The grooves are staggered to adapt to the needs of different areas.
By optimizing the groove design, a high-efficiency lithium-ion transport channel is created, resulting in uniform current distribution, reduced lithium plating risk, extended battery cycle life, and improved safety, making it suitable for large-scale industrial production.
Smart Images

Figure CN224958729U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of battery technology, and in particular to a wound battery cell, a battery and an electrical device. Background Technology
[0002] As consumer electronics products become thinner, lighter, and more high-performance, users' demand for fast-charging batteries is increasing. When batteries are charged at a high rate, insufficient negative electrode dynamics can cause lithium plating on the surface of the negative electrode, leading to electrolyte consumption and affecting the cycle life of the battery cell.
[0003] Currently, wound cells are more prone to lithium plating problems because the gap between the separator and the electrode is relatively large at the corners.
[0004] Therefore, there is an urgent need to develop a wound cell, battery, and electrical equipment to solve the above-mentioned technical problems. Utility Model Content
[0005] According to one aspect of the present invention, a wound battery cell with a low risk of lithium plating is provided, thereby extending the cycle life of the battery and improving the safety of battery use.
[0006] To achieve this objective, the present invention adopts the following technical solution:
[0007] A wound battery cell is formed by winding a negative electrode sheet, a separator, and a positive electrode sheet that are stacked in sequence. Each turn of the negative electrode sheet includes a flat area and a bent area connected to the flat area. On the active material layer of the negative electrode sheet, a plurality of first grooves and a plurality of second grooves are respectively provided in the flat area and the bent area. The first grooves and the second grooves extend along the width direction of the unfolded negative electrode sheet, and the plurality of first grooves and the plurality of second grooves are equally spaced along the length direction of the unfolded negative electrode sheet.
[0008] The distance between two adjacent first grooves is greater than the distance between two adjacent second grooves; the width of the first groove is A, the depth of the first groove is B, the width of the second groove is a, the depth of the second groove is b, and a×b≥1.5A×B.
[0009] Optionally, the distance between two adjacent first grooves is H, and the value of H is in the range of 2mm≤H≤3mm;
[0010] The distance between two adjacent second grooves is h, and the value of h is in the range of 0mm < h ≤ 1mm.
[0011] Optionally, the value range of A is: 10μm≤A≤50μm, and the value range of B is: 5μm≤B≤20μm;
[0012] The value range of a is: 15μm≤a≤75μm, and the value range of b is: 7.5μm≤b≤30μm.
[0013] Optionally, the plurality of first grooves in two adjacent rings are staggered, and the plurality of second grooves in two adjacent rings are staggered.
[0014] Optionally, the negative electrode includes a current collector, and the active material layer is provided on both sides of the current collector. The negative electrode has a plurality of first grooves and a plurality of second grooves on the active material layer of the inner winding.
[0015] Optionally, the negative electrode includes a current collector, and the active material layer is provided on both sides of the current collector. The two active material layers of the negative electrode are provided with a plurality of first grooves and a plurality of second grooves.
[0016] Optionally, the first groove is straight or wavy.
[0017] Optionally, the second groove is straight or wavy.
[0018] According to another aspect of the present invention, the present invention also provides a battery, including a casing and a wound cell as described in any of the above technical solutions, wherein the casing is filled with an electrolyte and the wound cell is immersed in the electrolyte.
[0019] According to another aspect of the present invention, the present invention also provides an electrical device comprising at least one of the aforementioned batteries.
[0020] The beneficial effects of this utility model are:
[0021] This invention provides a wound battery cell. By etching multiple first grooves and multiple second grooves on the negative electrode sheet, it creates an efficient and low-resistance transport channel for lithium ions, greatly shortening the diffusion distance of lithium ions from the electrolyte to the active material. This effectively alleviates the concentration polarization phenomenon caused by the local accumulation of lithium ions, fundamentally improving the kinetic characteristics of the negative electrode. This allows it to adapt to larger charging currents and significantly widens the charging rate window of the wound battery cell. It ensures that during high-rate charging, lithium ions can be more uniformly and quickly embedded into the active material layer, rather than being forced to precipitate as metallic lithium on the negative electrode surface, effectively reducing the risk of lithium plating. On the other hand, dividing the originally continuous negative electrode surface into multiple relatively independent micro-regions helps guide and redistribute the charging current, making the current density more uniform across the entire negative electrode surface. The uniform current distribution ensures that lithium ions undergo simultaneous embedding reactions over a larger area, further reducing the risk of local overpotential and lithium plating, allowing the overall performance of the wound battery cell to be fully utilized. Furthermore, it eliminates the need for complex and expensive additional production equipment, making it suitable for large-scale industrial production.
[0022] By setting the distance between two adjacent first grooves to be greater than the distance between two adjacent second grooves, and by setting the product of the width and depth of the second groove to be greater than or equal to 1.5 times the product of the width and depth of the first groove, the differentiation of multiple first grooves in the flat area and multiple second grooves in the bending area is achieved. This makes it more adaptable to different conditions in the flat and bending areas, further improving the uniformity of current density in various parts of the wound cell, thereby further reducing the risk of lithium plating in the wound cell, extending the cycle life of the wound cell, and improving the safety of the wound cell in use.
[0023] This utility model also provides a battery, including a casing and the aforementioned wound battery cell. Because it uses the aforementioned wound battery cell, this battery has a high energy density, a long cycle life, and high safety in use.
[0024] This utility model also provides an electrical device including at least one of the aforementioned batteries. Because this electrical device uses the aforementioned battery, it has a longer service life and higher safety during use. Attached Figure Description
[0025] To more clearly illustrate the technical solutions in the embodiments of this utility model, the drawings used in the description of the embodiments of this utility model will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on the content of the embodiments of this utility model and these drawings without creative effort.
[0026] Figure 1This is a partial cross-sectional view of the wound battery cell provided in this embodiment of the utility model;
[0027] Figure 2 This is a schematic diagram of the unfolded negative electrode sheet provided in this embodiment of the utility model.
[0028] In the picture:
[0029] 100. Negative electrode sheet; 101. Flat area; 102. Bending area; 110. First groove; 120. Second groove;
[0030] 200. Diaphragm;
[0031] 300, Positive electrode plate. Detailed Implementation
[0032] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the present invention, not the entire structure.
[0033] In the description of this utility model, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.
[0034] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0035] In the description of this embodiment, the terms "upper," "lower," "left," and "right," etc., refer to the orientation or positional relationship shown in the accompanying drawings. They are used only for ease of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model. In addition, the terms "first" and "second" are only used for distinction in description and have no special meaning.
[0036] Example 1
[0037] This embodiment provides a wound battery cell with a low risk of lithium plating, thereby extending the battery's cycle life and improving its safety.
[0038] Specifically, such as Figure 1 and Figure 2 As shown, the wound battery cell is formed by winding a negative electrode 100, a separator 200, and a positive electrode 300 arranged in sequence. Each turn of the negative electrode 100 includes a flat region 101 and a bent region 102 connected to the flat region 101. On the active material layer of the negative electrode 100, a plurality of first grooves 110 and a plurality of second grooves 120 are respectively provided in the flat region 101 and the bent region 102. The first grooves 110 and the second grooves 120 extend along the width direction of the unfolded negative electrode 100, and the plurality of first grooves 110 and the plurality of second grooves 120 are equally spaced along the length direction of the unfolded negative electrode 100.
[0039] By etching multiple first grooves 110 and multiple second grooves 120 on the negative electrode 100, a highly efficient and low-resistance transport channel for lithium ions is created, greatly shortening the diffusion distance of lithium ions from the electrolyte to the interior of the active material. This effectively alleviates the concentration polarization phenomenon caused by the local accumulation of lithium ions, fundamentally improving the kinetic characteristics of the negative electrode. This allows it to adapt to larger charging currents, significantly widening the charging rate window of the wound cell. It ensures that during high-rate charging, lithium ions can be more uniformly and quickly embedded into the active material layer, without... The lithium is forced to precipitate as metallic lithium on the negative electrode surface, effectively reducing the risk of lithium plating. On the other hand, dividing the originally continuous negative electrode 100 surface into multiple relatively independent micro-regions helps to guide and redistribute the charging current, making the current density more uniform across the entire negative electrode 100 surface. The uniform current distribution ensures that lithium ions can undergo the insertion reaction simultaneously over a larger area, further reducing the risk of local overpotential and lithium plating, allowing the overall performance of the wound cell to be fully utilized. Furthermore, there is no need to introduce complex and expensive additional production equipment, making it suitable for large-scale industrial production.
[0040] Because the distance between the negative electrode 100 and the separator 200 in the bending region 102 of the wound cell is greater than the distance between the negative electrode 100 and the separator 200 in the straight region 101 of the wound cell, electrolyte loss is more likely to occur in the bending region 102 during the later stages of the wound cell cycle, resulting in a lower risk of lithium plating.
[0041] Based on this technical problem, the wound battery cell provided in this embodiment sets the distance between two adjacent first grooves 110 to be greater than the distance between two adjacent second grooves 120, and sets the width of the first groove 110 to be A, the depth of the first groove 110 to be B, the width of the second groove 120 to be a, and the depth of the second groove 120 to be b, where a×b≥1.5A×B.
[0042] By controlling the dimensions of the first groove 110 and the second groove 120 within the aforementioned range, the differentiation of the multiple first grooves 110 in the flat region 101 and the multiple second grooves 120 in the bending region 102 is achieved, which is more adaptable to the different conditions of the flat region 101 and the bending region 102, further improving the uniformity of current density in various parts of the wound cell, thereby further reducing the risk of lithium plating in the wound cell, extending the cycle life of the wound cell, and improving the safety of the wound cell in use.
[0043] To compare the impact of the width A of the first groove 110, the depth B of the first groove 110, the width a of the second groove 120, and the depth b of the second groove 120 on battery performance, a special test was conducted, and the results are shown in Table 1 below.
[0044] Table 1
[0045]
[0046] The results above show that controlling a×b≥1.5A×B is beneficial to improving battery performance.
[0047] Optionally, see [link to relevant documentation] Figure 2 The distance between two adjacent first grooves 110 is H, and the value of H ranges from 2mm to 3mm. For example, the value of H can be 2mm, 2.2mm, 2.4mm, 2.6mm, 2.8mm, or 3mm, etc. The distance between two adjacent second grooves 120 is h, and the value of h ranges from 0mm to 1mm. For example, the value of h can be 0.2mm, 0.4mm, 0.6mm, 0.8mm, or 1mm, etc. By controlling the distances between two adjacent first grooves 110 and two adjacent second grooves 120 within the above ranges, the kinetic performance of the negative electrode 100 is effectively improved, and the risk of lithium plating is low.
[0048] To compare the impact of the distance H between two adjacent first grooves 110 and the distance h between two adjacent second grooves 120 on battery performance, a special test was conducted, and the results are shown in Table 2 below.
[0049] Table 2
[0050]
[0051] The results above show that controlling 2mm≤H≤3mm and 0mm<h≤1mm is beneficial to improving battery performance.
[0052] Optionally, in one possible embodiment, the value range of A is: 10μm ≤ A ≤ 50μm. The value range of B is: 5μm ≤ B ≤ 20μm. The value range of a is: 15μm ≤ a ≤ 75μm. The value range of b is: 7.5μm ≤ b ≤ 30μm. By controlling the values of A, B, a, and b within the above ranges, both good electrolyte storage performance and ease of processing can be ensured.
[0053] Furthermore, the multiple first grooves 110 of adjacent two turns are staggered, and the multiple second grooves 120 of adjacent two turns are staggered. This arrangement can effectively avoid the problem of large thickness differences in local areas of the wound cell, thereby improving the safety performance, electrochemical performance and reliability of the wound cell.
[0054] Optionally, in one possible embodiment, the negative electrode 100 includes a current collector, with active material layers on both sides of the current collector. The negative electrode 100 has a plurality of first grooves 110 and a plurality of second grooves 120 on the active material layer of the inner winding. Since the inner winding is the area most concentrated with mechanical stress and electrochemical strain, etching the first grooves 110 and second grooves 120 on the inner winding can maximize the overall performance, safety, and lifespan of the battery. Alternatively, in another possible embodiment, a plurality of first grooves 110 and a plurality of second grooves 120 may be provided on both active material layers of the negative electrode 100.
[0055] Optionally, the shape of the first groove 110 can be straight, wavy, etc., depending on actual needs. The first groove 110 is preferably wavy, as this shape has a better capacity to store electrolyte and is beneficial to the uniformity of current density throughout the negative electrode 100.
[0056] Optionally, the shape of the second groove 120 can be straight, wavy, etc., depending on actual needs. The second groove 120 is preferably wavy, as this shape has a better capacity to store electrolyte and is beneficial to the uniformity of current density throughout the negative electrode 100.
[0057] In this embodiment, both the first groove 110 and the second groove 120 are wavy.
[0058] Example 2
[0059] This embodiment provides a battery, including a casing and a wound cell as provided in Embodiment 1. The casing is filled with electrolyte, and the wound cell is immersed in the electrolyte.
[0060] Because it uses the aforementioned wound cells, this battery has a high energy density, a long cycle life, and high safety.
[0061] Example 3
[0062] This embodiment provides an electrical device, including at least one battery provided in Embodiment 2.
[0063] Because this electrical equipment uses the aforementioned battery, it has a long service life and high safety.
[0064] Obviously, the above embodiments of this utility model are merely examples for clearly illustrating the present utility model, and are not intended to limit the implementation of the present utility model. Those skilled in the art can make various obvious changes, readjustments, and substitutions without departing from the protection scope of this utility model. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this utility model should be included within the protection scope of the claims of this utility model.
Claims
1. A wound battery cell, comprising a negative electrode sheet (100), a separator (200), and a positive electrode sheet (300) arranged in sequence and wound together, characterized in that, Each ring of the negative electrode sheet (100) includes a flat region (101) and a bent region (102) connected to the flat region (101). On the active material layer of the negative electrode sheet (100), a plurality of first grooves (110) and a plurality of second grooves (120) are respectively provided in the flat region (101) and the bent region (102). The first grooves (110) and the second grooves (120) extend along the width direction of the unfolded negative electrode sheet (100), and the plurality of first grooves (110) and the plurality of second grooves (120) are equally spaced along the length direction of the unfolded negative electrode sheet (100). The distance between two adjacent first grooves (110) is greater than the distance between two adjacent second grooves (120); the width of the first groove (110) is A, the depth of the first groove (110) is B, the width of the second groove (120) is a, the depth of the second groove (120) is b, and a×b≥1.5A×B.
2. The wound battery cell according to claim 1, characterized in that, The distance between two adjacent first grooves (110) is H, and the value of H is in the range of 2mm≤H≤3mm; The distance between two adjacent second grooves (120) is h, and the value of h is in the range of 0mm < h ≤ 1mm.
3. The wound battery cell according to claim 1, characterized in that, The range of values for A is: 10μm≤A≤50μm, and the range of values for B is: 5μm≤B≤20μm; The value range of a is: 15μm≤a≤75μm, and the value range of b is: 7.5μm≤b≤30μm.
4. The wound battery cell according to claim 1, characterized in that, The first grooves (110) of two adjacent rings are staggered, and the second grooves (120) of two adjacent rings are staggered.
5. The wound battery cell according to claim 1, characterized in that, The negative electrode (100) includes a current collector, and the active material layer is provided on both sides of the current collector. The negative electrode (100) has a plurality of first grooves (110) and a plurality of second grooves (120) on the active material layer of the inner winding.
6. The wound battery cell according to claim 1, characterized in that, The negative electrode (100) includes a current collector, and the active material layer is provided on both sides of the current collector. The two active material layers of the negative electrode (100) are provided with a plurality of first grooves (110) and a plurality of second grooves (120).
7. The wound battery cell according to any one of claims 1-6, characterized in that, The first groove (110) is straight or wavy.
8. The wound battery cell according to any one of claims 1-6, characterized in that, The second groove (120) is straight or wavy.
9. A battery, characterized in that, The device includes a housing and a wound battery cell as described in any one of claims 1-8, wherein the housing is filled with an electrolyte and the wound battery cell is immersed in the electrolyte.
10. Electrical equipment, characterized in that, It includes at least one battery as described in claim 9.