A semiconductor alignment mark structure

By employing multi-layer structure design and signal analysis techniques, the problem of coordinating rapid coarse alignment and high-precision alignment in semiconductor manufacturing was solved, enabling signal anti-crosstalk and mark integrity verification, thereby improving the yield and structural stability of semiconductor products.

CN224960034UActive Publication Date: 2026-11-10SUZHOU ASEN SEMICON CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522445914.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-18
Publication Date
2026-11-10
Estimated Expiration
2035-11-18

AI Technical Summary

Technical Problem

In existing semiconductor manufacturing technologies, it is difficult to achieve rapid coarse alignment and high-precision alignment in a coordinated manner. There is insufficient signal anti-crosstalk design, lack of mark integrity verification and real-time stress monitoring functions, and insufficient structural stability, which affects product yield.

Method used

The system employs a multi-layered structure design, including a substrate, cutting channels, positioning mark structure, adhesive layer, crystal layer, buffer layer, surface layer, barrier layer, quantum dot layer, reinforcement layer, and stress-sensing layer. Through strong reflection peak, interference fringe phase analysis, fluorescence signal, and Raman spectroscopy monitoring, it achieves rapid coarse alignment, precise vertical alignment, and real-time stress monitoring, avoiding signal crosstalk and ensuring mark integrity and structural stability.

Benefits of technology

It achieves the synergy of rapid coarse alignment and high-precision alignment, avoids signal crosstalk, ensures mark integrity verification, reduces the risk of process failure, and improves semiconductor product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224960034U_ABST
    Figure CN224960034U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of semiconductor manufacturing technology and discloses an alignment mark structure for semiconductors. It includes a substrate with dicing channels in the inter-chip gap area on the substrate, and positioning mark structures disposed within these channels. The positioning mark structure, from bottom to top, comprises an adhesive layer, a crystal layer, a buffer layer, a surface layer, a barrier layer, a quantum dot layer, a reinforcement layer, and a stress-sensing layer, with a silicon dioxide sealing wall on its outer periphery. The adhesive layer is a silicon dioxide thin film, chemically bonded to the substrate and chemically adsorbed to the single-crystal silicon crystal layer. The buffer layer is an amorphous silicon thin film, and the surface layer is titanium dioxide, connected by gradient bonding. The barrier layer is an aluminum oxide thin film, the quantum dot layer is cadmium selenide quantum dots, the reinforcement layer is a hafnium oxide thin film, and the stress-sensing layer is a silicon dioxide thin film. This structure, through multi-layer composite design and precise connection methods, improves the positioning accuracy and structural stability of the alignment marks, making it suitable for high-precision alignment processes in semiconductor manufacturing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of semiconductor manufacturing technology, specifically to an alignment mark structure for semiconductors. Background Technology

[0002] In the semiconductor manufacturing process, alignment marks are the core structure that ensures the precise execution of processes such as photolithography and bonding. Their alignment efficiency, accuracy, and structural reliability directly affect the yield and performance of semiconductor products.

[0003] A search revealed existing technology (application number: CN202421561593.4), which describes "an alignment mark and semiconductor structure." This utility model, through the projection and overlapping design of multiple pattern layers, effectively reduces the substrate area occupied by the alignment mark while ensuring basic alignment accuracy, thereby improving the effective wiring area of ​​the substrate and the manufacturing efficiency of the semiconductor structure. However, this existing technology only focuses on optimizing the space occupied by the mark and fails to achieve the synergy between rapid coarse alignment and high-precision vertical alignment. Furthermore, it lacks a signal anti-crosstalk design, making it prone to increased alignment errors due to reflected signal interference. The structure does not have a post-processing mark integrity verification mechanism, making it impossible to accurately determine the mark's validity when the mark surface is contaminated or covered. It also lacks real-time monitoring of stress changes in the mark structure during the process, making it prone to structural damage due to stress accumulation, which can lead to process failures and affect product yield. In addition, its interlayer connection design is relatively simple, and the long-term stability of the structure needs to be improved.

[0004] Therefore, there is an urgent need for a semiconductor alignment mark structure that can balance fast coarse alignment with high-precision alignment, effectively avoid signal crosstalk, and has mark integrity verification, real-time stress monitoring, and high structural stability. Utility Model Content

[0005] The purpose of this invention is to address the shortcomings of existing technologies by proposing a semiconductor alignment mark structure.

[0006] To achieve the above objectives, the present invention adopts the following technical solution: a semiconductor alignment mark structure, comprising a substrate, a dicing channel provided in the separation blank area between chips on the upper surface of the substrate, positioning mark structures provided on both sides of the dicing channel, the positioning mark structures being distributed in a ring at the four corners of the substrate, the positioning mark structure comprising an adhesive layer, the lower surface of the adhesive layer being connected to the bottom surface of the dicing channel, and the upper surface of the adhesive layer being connected to the lower surface of the crystal layer, the interior of the adhesive layer being provided with a plurality of cylindrical through holes, and the upper surface of the adhesive layer being provided with a deep groove in the middle, the bottom surface of the deep groove being connected to the lower surface of a buffer layer, and the upper surface of the buffer layer being connected to the lower surface of the surface layer.

[0007] As a further description of the above technical solution:

[0008] The upper surface of the surface layer is connected to the lower surface of the barrier layer, the upper surface of the barrier layer is connected to the lower surface of the quantum dot layer, the upper surface of the quantum dot layer is connected to the lower surface of the reinforcement layer, and the upper surface of the reinforcement layer is connected to the lower surface of the stress-sensing layer.

[0009] As a further description of the above technical solution:

[0010] The adhesive layer is made of silicon dioxide film, the crystal layer is made of monocrystalline silicon, and the adhesive layer is chemically bonded to the substrate, while the adhesive layer and the crystal layer are chemically adsorbed together.

[0011] As a further description of the above technical solution:

[0012] The buffer layer is made of amorphous silicon thin film, the surface layer is made of titanium dioxide, and the buffer layer and the crystal layer are connected by molecular deposition bonding, while the buffer layer and the surface layer are connected by gradient bonding.

[0013] As a further description of the above technical solution:

[0014] The barrier layer is made of aluminum oxide film, the quantum dot layer uses cadmium selenide quantum dots, and the barrier layer and the surface layer are connected by chemical bonding. The barrier layer and the quantum dot layer are selectively deposited by micro-contact printing.

[0015] As a further description of the above technical solution:

[0016] The reinforcing layer is made of hafnium oxide thin film, the stress sensing layer is made of silicon dioxide thin film, and the reinforcing layer and quantum dot layer are encapsulated by deposition. The reinforcing layer and stress sensing layer are connected by molecular deposition.

[0017] As a further description of the above technical solution:

[0018] The sealing wall is made of the same type of silicon dioxide as the stress-sensitive layer, and the sealing wall is formed by laser melting.

[0019] This utility model has the following beneficial effects:

[0020] First, the crystal layer achieves rapid coarse alignment through strong reflection peaks, while the surface layer completes planar accuracy and interlayer distance measurement through interference fringe phase analysis. Combined with the reflection signal enhancement and independent angle acquisition design of the crystal layer and stress sensing layer, signal crosstalk is effectively avoided, achieving high-precision control of interlayer vertical alignment and meeting the high-precision alignment process requirements of semiconductor manufacturing.

[0021] Second, the fluorescence signal of the quantum dot layer can penetrate the contamination or capping layer, ensuring the effectiveness of post-process marking integrity verification. The stress-sensing layer monitors stress changes in real time through Raman spectroscopy, providing early warning of structural damage. Combined with the high stability brought by the multi-layer composite structure and precise connection method, it significantly reduces the risk of process failure and improves the yield of semiconductor products. Attached Figure Description

[0022] Figure 1 This is a schematic diagram of the installation structure of this utility model;

[0023] Figure 2 This is a schematic diagram of the overall structure of this utility model;

[0024] Figure 3 This is an exploded view of the overall structure of this utility model;

[0025] Figure 4 This is a cross-sectional view of the internal structure of this utility model;

[0026] Figure 5 This is a schematic diagram of the material structure of this utility model.

[0027] Legend:

[0028] 1. Substrate; 2. Cutting track; 3. Positioning mark structure; 301. Adhesive layer; 302. Crystal layer; 303. Buffer layer; 304. Surface layer; 305. Barrier layer; 306. Quantum dot layer; 307. Reinforcing layer; 308. Stress-sensitive layer; 309. Sealing wall. Detailed Implementation

[0029] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.

[0030] In the description of this utility model, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings and are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance. The utility model will be further described in detail below with reference to the accompanying drawings.

[0031] In this utility model, unless otherwise explicitly specified and limited, the terms "installation," "connection," "joining," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model according to the specific circumstances.

[0032] Example 1:

[0033] like Figures 1 to 5 As shown, this embodiment provides a semiconductor alignment mark structure, including a substrate 1. A dicing channel 2 is provided in the separation blank area between chips on the upper surface of the substrate 1. Positioning mark structures 3 are provided on both sides of the dicing channel 2. The positioning mark structures 3 are distributed in a ring at the four corners of the substrate 1. The positioning mark structure 3 includes an adhesive layer 301. The lower surface of the adhesive layer 301 is connected to the bottom surface of the dicing channel 2, and the upper surface of the adhesive layer 301 is connected to the lower surface of the crystal layer 302. Multiple cylindrical through holes are provided inside the adhesive layer 301, and a deep groove is provided in the middle of the upper surface of the adhesive layer 301. The bottom surface of the deep groove is connected to the lower surface of the buffer layer 303, and the upper surface of the buffer layer 303 is connected to the lower surface of the surface layer 304.

[0034] In this embodiment, the crystal layer 302, the surface layer 304, the quantum dot layer 306, and the stress-sensing layer 308 constitute an alignment mark structure for a semiconductor according to this application.

[0035] It should also be noted that the semiconductor in this application can be a silicon-based semiconductor, a gallium arsenide semiconductor, a silicon carbide semiconductor, etc. Figure 1 In this embodiment, silicon-based semiconductors are used as an example for description. Of course, other types of semiconductors can also adopt similar structures, which will not be elaborated on later.

[0036] Understandable Figure 1 The alignment mark structure is shown only schematically, and the actual shape, size, position, and construction of these components are not subject to change. Figure 1 Due to limitations, the alignment mark structure can also include, compared to Figure 1 More or fewer parts.

[0037] Furthermore, in this embodiment, the crystal layer 302 achieves rapid coarse alignment through strong reflection peaks, and the surface layer 304 completes planar accuracy and interlayer ranging by means of interference fringe phase analysis, thereby achieving basic alignment and positioning and providing interlayer ranging data.

[0038] Specifically, the upper surface of the surface layer 304 is connected to the lower surface of the barrier layer 305, the upper surface of the barrier layer 305 is connected to the lower surface of the quantum dot layer 306, the upper surface of the quantum dot layer 306 is connected to the lower surface of the reinforcement layer 307, and the upper surface of the reinforcement layer 307 is connected to the lower surface of the stress-sensing layer 308.

[0039] In this embodiment, the enhancement layer 307 and the crystal layer 302 work together to enhance the reflection signal, and the signals of each layer are collected independently at different angles to avoid signal crosstalk and improve the vertical alignment accuracy between layers.

[0040] Specifically, the adhesive layer 301 is made of silicon dioxide film, the crystal layer 302 is made of single crystal silicon, and the adhesive layer 301 is chemically bonded to the substrate 1, while the adhesive layer 301 and the crystal layer 302 are chemically adsorbed together.

[0041] In a preferred embodiment, the silica film of the adhesive layer 301 enhances the chemical bonding strength between the substrate 1 and the crystal layer 302, preventing delamination caused by interface defects. The crystal layer 302 and the substrate 1 are precisely controlled. The single-crystal silicon of the crystal layer 302 is etched into a two-dimensional air-hole photonic crystal structure. The high refractive index of silicon and the air holes form a strong refractive index contrast, generating a photonic bandgap effect. Chemical bonding and chemical adsorption respectively achieve stable fixation, ensuring the reliability of interlayer connection and preventing delamination.

[0042] Example 2:

[0043] A buffer layer 303 is provided based on Example 1.

[0044] Specifically, the buffer layer 303 is made of amorphous silicon thin film, the surface layer 304 is made of titanium dioxide, and the buffer layer 303 and the crystal layer 302 are connected by molecular deposition bonding, while the buffer layer 303 and the surface layer 304 are connected by gradient bonding.

[0045] In this embodiment, the amorphous silicon thin film of the buffer layer 303 alleviates the lattice mismatch and thermal expansion coefficient difference between the crystal layer 302 and the surface layer 304, forming a refractive index gradient interface to reduce interlayer reflection loss. The titanium dioxide of the surface layer 304 achieves efficient phase control, maintains alignment accuracy, molecular deposition interlocking enhances the fit, and gradient bonding alleviates interlayer stress, improves the overall structural stability, and reduces deformation.

[0046] Specifically, the barrier layer 305 is made of aluminum oxide film, the quantum dot layer 306 uses cadmium selenide quantum dots, and the barrier layer 305 and the surface layer 304 are connected by chemical bonding. The barrier layer 305 and the quantum dot layer 306 are selectively deposited by micro-contact printing.

[0047] With this configuration, the alumina film of the barrier layer 305 prevents ions from diffusing into the quantum dot layer 306 during the high-temperature process, preventing fluorescence quenching in the quantum dot layer and ensuring the reliability of fluorescence verification. The cadmium selenide quantum dots in the quantum dot layer 306 produce bright fluorescence under ultraviolet excitation, and the marking position can still be identified even if the surface is contaminated or covered by CMP. The quantum dot layer 306 emits fluorescence under ultraviolet excitation, and the barrier layer 305 blocks impurities from penetrating, realizing post-processing marking integrity verification, penetrating contaminated or covered layers.

[0048] Specifically, the reinforcing layer 307 is made of hafnium oxide thin film, the stress sensing layer 308 is made of silicon dioxide thin film, and the reinforcing layer 307 and the quantum dot layer 306 are encapsulated by deposition, and the reinforcing layer 307 and the stress sensing layer 308 are connected by molecular deposition.

[0049] Among them, the hafnium oxide thin film of the reinforcing layer 307 utilizes the high dielectric constant to improve the exciton recombination efficiency of quantum dots and acts as an oxygen diffusion barrier layer to prevent the oxidation failure of quantum dots. The silicon dioxide thin film of the stress sensing layer 308 is resistant to CMP chemical corrosion and mechanical wear. The fluorescence peak position is sensitive to local stress. Raman spectroscopy is used to monitor the stress change of the marked structure in the process in real time, thereby enhancing the intensity of the reflected signal. The Raman peak position of the stress sensing layer 308 responds to local stress changes. Through Raman spectroscopy monitoring, it can provide real-time early warning of structural damage and reduce the risk of process failure.

[0050] Specifically, the sealing wall 309 is made of silicon dioxide, which is the same material as the stress-sensing layer 308, and the sealing wall 309 is formed by laser melting.

[0051] In this embodiment, the silica of the sealing wall 309 forms a micro-ring seal at the edge of the mark and is filled with nitrogen gas to achieve a gas-tight packaging, preventing the quantum dots from oxidizing and failing due to long-term exposure to air.

[0052] In actual use, when the incident light irradiates the periodic air hole structure of the crystal layer 302 for coarse alignment, strong reflection is generated only in the normal direction. When it deviates, the reflectivity decreases. At this time, the intensity peak is captured by scanning to achieve rapid positioning. Then, the surface layer 304 achieves planar accuracy and interlayer distance measurement through interference fringe phase analysis.

[0053] Subsequently, under ultraviolet excitation, the quantum dot layer 306 emits fluorescence. Even if the surface is contaminated or covered, the fluorescence signal can still penetrate and be used for post-processing label integrity verification. Then, the Raman peak position of the stress-sensing layer 308 is sensitive to local stress. The stress change of the label in the process can be monitored in real time by Raman spectroscopy to provide early warning of structural damage.

[0054] At this time, the crystal layer 302 and the stress sensing layer 308 enhance the reflected signal. The signals of each layer are acquired independently by angle to avoid crosstalk and achieve vertical alignment with high precision between layers.

[0055] Finally, it should be noted that the above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Although the present utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.

Claims

1. A structure of alignment marks of a semiconductor, characterized by: The substrate (1) includes a dicing channel (2) in the blank area separating the chips on the upper surface of the substrate (1). Positioning mark structures (3) are provided on both sides of the dicing channel (2). The positioning mark structures (3) are distributed in a ring at the four corners of the substrate (1). The positioning mark structures (3) include an adhesive layer (301). The lower surface of the adhesive layer (301) is connected to the bottom surface of the dicing channel (2), and the upper surface of the adhesive layer (301) is connected to the lower surface of the crystal layer (302). Multiple cylindrical through holes are provided inside the adhesive layer (301), and a deep groove is provided in the middle of the upper surface of the adhesive layer (301). The bottom surface of the deep groove is connected to the lower surface of the buffer layer (303), and the upper surface of the buffer layer (303) is connected to the lower surface of the surface layer (304).

2. A semiconductor alignment mark structure according to claim 1, wherein: The upper surface of the surface layer (304) is connected to the lower surface of the barrier layer (305), the upper surface of the barrier layer (305) is connected to the lower surface of the quantum dot layer (306), the upper surface of the quantum dot layer (306) is connected to the lower surface of the reinforcement layer (307), and the upper surface of the reinforcement layer (307) is connected to the lower surface of the stress-sensing layer (308).

3. A semiconductor alignment mark structure according to claim 2, wherein: The adhesive layer (301) is made of silicon dioxide film, the crystal layer (302) is made of single crystal silicon, and the adhesive layer (301) is connected to the substrate (1) by chemical bonding, and the adhesive layer (301) is connected to the crystal layer (302) by chemical adsorption.

4. A semiconductor alignment mark structure according to claim 3, wherein: The buffer layer (303) is made of amorphous silicon thin film, the surface layer (304) is made of titanium dioxide, and the buffer layer (303) and the crystal layer (302) are connected by molecular deposition interlocking, and the buffer layer (303) and the surface layer (304) are connected by gradient bonding.

5. A semiconductor alignment mark structure according to claim 4, wherein: The barrier layer (305) is made of aluminum oxide film, the quantum dot layer (306) uses cadmium selenide quantum dots, and the barrier layer (305) and the surface layer (304) are connected by chemical bonding. The barrier layer (305) and the quantum dot layer (306) are selectively deposited by micro-contact printing.

6. A semiconductor alignment mark structure according to claim 5, wherein: The reinforcing layer (307) is made of hafnium oxide thin film, the stress sensing layer (308) is made of silicon dioxide thin film, and the reinforcing layer (307) and the quantum dot layer (306) are encapsulated by deposition, and the reinforcing layer (307) and the stress sensing layer (308) are connected by molecular deposition.

7. The alignment mark structure for a semiconductor according to claim 6, characterized in that: The sealing wall (309) is made of the same type of silicon dioxide as the stress-sensitive layer (308), and the sealing wall (309) is formed by laser melting.

Citation Information

Patent Citations

  • Alignment mark and semiconductor structure

    CN222995403U