Lithium-ion battery anode slurry preparation device
By heating deionized water to 45°C on the delivery pipe and mixing it with solid components, the problem of uneven dispersion of lithium battery negative electrode slurry was solved, improving the uniformity and fluidity of the slurry, extending the service life of lithium batteries, and saving energy.
Patent Information
- Application Number
- CN202521623722.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-31
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-07-31
AI Technical Summary
Poor dispersion of lithium battery negative electrode slurry during stirring results in poor slurry uniformity and conductivity, affecting electrode quality and lithium battery performance and lifespan.
A heating unit is installed on the conveying pipe to heat the deionized water to about 45°C before it is mixed with the solid components. This increases the frequency of water molecule movement, promotes the dispersion of solid components, and improves the uniformity of the slurry.
Heating deionized water significantly improves the uniformity and fluidity of the slurry, enhances electrode quality, extends the lifespan of lithium batteries, and facilitates energy-saving upgrades to existing equipment.
Smart Images

Figure CN224976170U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of lithium battery production equipment technology, and in particular to a lithium battery negative electrode slurry preparation device. Background Technology
[0002] The negative electrode slurry of a lithium battery consists of solid components and a dispersion medium. The solid components include graphite, while the dispersion medium includes deionized water and binders. The uniformity of the lithium battery negative electrode slurry directly affects the overall performance and lifespan of the lithium battery.
[0003] Currently, during the mixing process of lithium battery negative electrode slurry, poor mixing and dispersion often leads to poor slurry uniformity, manifesting as agglomeration and clumping within the slurry, and uneven particle size distribution of various components. Poor mixing and dispersion directly affects the uniformity and conductivity of the negative electrode slurry, resulting in abnormal viscosity and reduced flowability. This, in turn, leads to problems during the coating process such as inconsistent coating thickness, surface roughness, and increased internal electrode resistance, ultimately reducing electrode quality and affecting the overall performance and lifespan of the lithium battery. Utility Model Content
[0004] This application provides a lithium battery negative electrode slurry preparation device to solve the problem of poor stirring and dispersion effect of negative electrode slurry in the prior art.
[0005] To solve the above-mentioned technical problems, this application is implemented as follows: This application discloses a lithium battery anode slurry preparation apparatus, which includes: a water storage tank for storing deionized water; Mixing tank; A first conveying pipe is connected at one end to the water storage tank and at the other end to the stirring tank. The first conveying pipe is used to convey deionized water from the water storage tank to the stirring tank. The stirring tank is used to mix and stir the deionized water and solid components. The first conveying pipe is equipped with a heating unit, which is used to heat the deionized water in the first conveying pipe.
[0006] Optionally, the heating unit includes a heating element that is wound around the first conveying pipe and extends spirally along the axial direction of the first conveying pipe.
[0007] Optionally, the heating unit further includes a mounting cylinder; The mounting sleeve is fitted outside the first conveying pipe and is located between the heating element and the first conveying pipe; The mounting cylinder is used to connect the heating element to the first delivery pipe.
[0008] Optionally, the mounting cylinder includes a plurality of mounting plates; Multiple mounting pieces are connected sequentially around the circumference of the first conveying pipe to form the mounting cylinder.
[0009] Optionally, a first connector is provided between adjacent mounting pieces, the first connector being used to connect two adjacent mounting pieces.
[0010] Optionally, the first connector includes a protrusion and a recess that engage with each other, the protrusion being connected to one of two adjacent mounting pieces, and the recess being connected to the other of two adjacent mounting pieces.
[0011] Optionally, the mounting cylinder is provided with a second connector for detachably connecting the plurality of mounting pieces to the outside of the first delivery pipe.
[0012] Optionally, the heating unit further includes a protective cylinder; The protective sleeve is fitted over the heating element and connected to the mounting sleeve. There is a gap between the protective cylinder and the heating element to reduce heat loss.
[0013] Optionally, the protective cylinder includes multiple protective plates; Multiple protective plates are connected sequentially around the circumference of the mounting cylinder to form the protective cylinder.
[0014] Optionally, the first delivery pipe is further provided with a temperature control unit, which is used to detect and adjust the temperature of the deionized water.
[0015] In this embodiment, by setting a heating unit on the first conveying pipe, deionized water is heated before being conveyed to the mixing tank to mix with the solid components. During the mixing process, the movement of water molecules accelerates, and the collisions between water molecules and solid component molecules become more frequent. This helps to break the interaction forces between slurry particles, making it easier for the solid component molecules to disperse, improving the overall fluidity of the slurry. Consequently, the negative electrode slurry is more evenly dispersed, improving its uniformity and ultimately enhancing the quality of the electrode sheet, thus improving the overall performance and lifespan of the lithium battery. Moreover, in this embodiment, heating the deionized water in the first conveying pipe is more economical and energy-efficient than heating the mixed slurry, and it is also easier to modify existing slurry preparation equipment.
[0016] Additional aspects and advantages of this invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description
[0017] The above and / or additional aspects and advantages of this application will become apparent and readily understood from the description of the embodiments taken in conjunction with the following drawings, in which: Figure 1 This is a schematic diagram of the overall structure of a lithium battery negative electrode slurry preparation device according to an embodiment of this application; Figure 2 This is a three-dimensional structural schematic diagram of a heating unit according to an embodiment of this application; Figure 3 This is a partially exploded view of a heating unit in one embodiment of this application; Figure 4 This is a top view of a portion of the structure of a heating unit in an embodiment of this application.
[0018] Figure label: 1. Water storage tank; 2. First delivery pipe; 3. Mixing tank; 4. Heating unit; 41. Heating element; 42. Mounting cylinder; 421. Mounting plate; 43. First connector; 431. Protrusion; 432. Recess; 44. Second connector; 45. Protective cylinder; 451. Protective plate; 5. Temperature control unit; 51. Temperature sensor; 52. Controller; 6. Water purifier; 7. Second delivery pipe; 8. Pump body. Detailed Implementation
[0019] The embodiments of this application will now be described in detail. Examples of these embodiments are illustrated in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain this application, and should not be construed as limiting this application. All other embodiments obtained by those skilled in the art based on the embodiments of this application without inventive effort are within the scope of protection of this application.
[0020] The terms "first" and "second" in the specification and claims of this application may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise stated, "multiple" means two or more. Furthermore, "and / or" in the specification and claims indicates at least one of the connected objects, and the character " / " generally indicates that the preceding and following objects are in an "or" relationship.
[0021] In the description of this application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application.
[0022] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.
[0023] The inventors of this application have discovered through research that in the production of lithium-ion battery anodes in related technologies, excessively low temperatures of deionized water significantly impact the dispersion of the slurry. Low temperatures increase the viscosity of the dispersion medium and slow down molecular motion, leading to increased dispersion resistance when mixing active materials, conductive agents, and binders. This results in uneven distribution and agglomeration or clumping. Simultaneously, low temperatures may reduce the dissolution efficiency of the binder, preventing it from fully swelling and encapsulating the components, thus deteriorating the stability of the slurry system and causing uneven viscosity distribution. Under these conditions, energy transfer efficiency decreases during stirring, dispersion time is prolonged, and the particle size distribution of the dispersed slurry widens, affecting the uniformity of subsequent coating and even causing a decline in electrode performance, such as reduced conductivity and cycle stability.
[0024] The following is combined Figures 1-4 This application describes an apparatus for preparing lithium battery negative electrode slurry according to an embodiment.
[0025] refer to Figure 1 In some embodiments of this application, an apparatus for preparing lithium battery negative electrode slurry is proposed, comprising: a water storage tank 1 for storing deionized water; a stirring tank 3; and a first conveying pipe 2, one end of which is connected to the water storage tank 1 and the other end of which is connected to the stirring tank 3. The first conveying pipe 2 is used to convey deionized water from the water storage tank 1 to the stirring tank 3, and the stirring tank 3 is used to mix and stir the deionized water and solid components. The first conveying pipe 2 is provided with a heating unit 4 for heating the deionized water in the first conveying pipe 2.
[0026] In the embodiments of this application, by setting a heating unit 4 on the first conveying pipe 2, the deionized water is heated and then conveyed to the stirring tank 3 to mix with the solid components. During the mixing process of deionized water and solid components, the movement of water molecules is accelerated, and the collision between water molecules and solid component molecules is more frequent. This helps to break the interaction forces between slurry particles, making the solid component molecules easier to disperse, improving the overall fluidity of the slurry, thereby making the negative electrode slurry more uniformly stirred and dispersed, improving the uniformity of the negative electrode slurry, and ultimately improving the quality of the electrode sheet, improving the overall performance and service life of the lithium battery. Moreover, in the embodiments of this application, heating the deionized water in the first conveying pipe 2 is more economical and energy-saving than heating the mixed slurry, and it is also easier to modify existing slurry preparation equipment.
[0027] In the above embodiments, the mixing tank 3 is used to mix and stir the solid components and dispersion medium evenly. The solid components include graphite, etc., and the dispersion medium includes deionized water and binders, etc., wherein the mass of deionized water accounts for 99% of the mass of the dispersion medium. Therefore, heating the deionized water can significantly accelerate the molecular motion during the mixing process of the solid components and dispersion medium. Moreover, the fluidity of deionized water is stronger than that of the negative electrode slurry. Therefore, heating deionized water is not only economical and energy-saving, but also provides better temperature uniformity and operability during the heating process. It can be understood that the mixing tank 3 is also provided with a feed inlet for adding solid components and other dispersion media, and the mixing tank 3 is also provided with a stirring mechanism for stirring and mixing the dispersion medium and solid components evenly. The feed inlet and stirring mechanism are not shown in the figure.
[0028] In the above embodiments, the temperature of the deionized water after heating by heating unit 4 is approximately 45°C, with a temperature range of 40°C-50°C. Data obtained from the inventors' experiments shows that when the deionized water is not heated, the D90 value of the resulting negative electrode slurry is 23 μm; when the deionized water is heated to 45°C, the D90 value of the resulting negative electrode slurry is 16 μm. The lithium battery negative electrode slurry preparation device in this application typically operates in a constant temperature environment, with an ambient temperature of approximately 25°C. The D90 value reflects the uniformity of the material and refers to the particle size value corresponding to the cumulative percentage of particles from smallest to largest reaching 90% in the particle size distribution; that is, in a given material, the number of particles with a diameter smaller than D90 accounts for 90% of the total number of particles. From the above experimental data, it can be seen that by setting heating unit 4 and heating the deionized water to 45°C, the particle size of the resulting negative electrode slurry can be effectively reduced, improving the uniformity of the negative electrode slurry.
[0029] In the above embodiments, reference is made to Figure 1The lithium battery negative electrode slurry preparation device may further include a water maker 6, which is connected to the water storage tank 1 via a second conveying pipe 7. After the raw water is processed by the water maker 6, the deionized water is obtained. A pump body 8 may also be provided on the first conveying pipe 2 to ensure the conveying efficiency of the deionized water when it is conveyed from the water storage tank 1 to the mixing tank 3. The pump body 8 may be a rotary pump or other types of pump body, and this application embodiment does not make specific limitations.
[0030] refer to Figure 1 In the above embodiment, the water generator 6 produces deionized water, which is then transported to the storage tank 1 through the second conveying pipe 7, and then to the mixing tank 3 through the first conveying pipe 2. Simultaneously, the solid components and other dispersion media also enter the mixing tank 3 through the inlet. Under the action of the stirring mechanism, the solid components and dispersion media are mixed and stirred to produce a negative electrode slurry. The deionized water in the first conveying pipe 2 is heated to approximately 45°C by the heating unit 4. After entering the mixing tank 3, the deionized water mixes with the solid components and other dispersion media. Due to the more vigorous movement of the deionized water molecules after heating, the negative electrode slurry becomes more uniform.
[0031] In some optional embodiments of this application, reference is made to Figure 2 , Figure 3 The heating unit 4 includes a heating element 41, which is wound around the first conveying pipe 2 and extends spirally along the axial direction of the first conveying pipe 2.
[0032] In the above embodiment, by winding the heating element 41 around the first conveying pipe 2 and extending it spirally along the axial direction of the first conveying pipe 2, the contact area between the heating element 41 and the first conveying pipe 2 can be increased. This not only allows for uniform heating of the deionized water in the first conveying pipe 2, but also reduces heat loss and is more economical and energy-saving.
[0033] Specifically, the heating element 41 can be a heating wire or a flexible pipe containing a heat exchange medium, etc., and this application embodiment does not make specific limitations.
[0034] In some alternative embodiments, the heating unit 4 may also include multiple heating elements, each of which can contact the first conveying pipe 2, and the multiple heating elements can be evenly arranged along the circumference of the first conveying pipe 2. Those skilled in the art can set it according to actual needs, and this application does not make specific limitations.
[0035] Optionally, refer to Figures 2 to 4 The heating unit 4 also includes a mounting cylinder 42; the mounting cylinder 42 is sleeved outside the first conveying pipe 2 and is located between the heating element 41 and the first conveying pipe 2; the mounting cylinder 42 is used to connect the heating element 41 and the first conveying pipe 2.
[0036] In this embodiment, the heating unit 4 is an upgraded and newly added structure based on the existing first conveying pipe 2. An installation cylinder 42 is set between the first conveying pipe 2 and the heating element 41, which not only facilitates construction, but also avoids damage to the original first conveying pipe 2 during the upgrade process, thereby avoiding production stoppages caused by the upgrade.
[0037] In the above embodiment, the mounting cylinder 42 can be a cylindrical shape, and its inner diameter matches the outer diameter of the first conveying pipe 2. The inner wall of the mounting cylinder 42 can be fitted against the outer wall of the first conveying pipe 2 so that the mounting cylinder 42 can be stably installed on the outer wall of the first conveying pipe 2, thereby improving the heat conduction effect. The mounting cylinder 42 is preferably made of a material with good thermal conductivity, such as stainless steel.
[0038] In the above embodiments, the connection method between the heating element 41 and the mounting cylinder 42 is not specifically limited. For example, a buckle for fixing the heating element 41 can be provided on the mounting cylinder 42, or it can be fixed with aluminum foil tape, etc.
[0039] Optionally, refer to Figures 3 to 4 The mounting cylinder 42 includes multiple mounting pieces 421; the multiple mounting pieces 421 are connected in sequence around the circumference of the first conveying pipe 2 to form the mounting cylinder 42.
[0040] By setting multiple mounting pieces 421 and connecting them sequentially around the circumference of the first conveying pipe 2, multiple mounting pieces 421 can be installed around the circumference of the first conveying pipe 2 without damaging the existing first conveying pipe 2, and then formed into a mounting cylinder 42, so that the heating element 41 can be installed on the first conveying pipe 2.
[0041] In the above embodiments, the number of mounting pieces 421 can be two, three, or four, etc., and this application does not impose a specific limitation. The mounting piece 421 can be an arc-shaped piece. (See reference...) Figure 2 When multiple mounting pieces 421 are connected, the two sides of two adjacent mounting pieces 421 that are close to each other can be fitted together or have a gap. Two adjacent mounting pieces 421 can also be partially overlapped. This application embodiment does not make specific limitations.
[0042] Optionally, refer to Figure 2 A first connector 43 is provided between adjacent mounting pieces 421, and the first connector 43 is used to connect two adjacent mounting pieces 421.
[0043] In the above embodiment, by providing the first connector 43, two adjacent mounting pieces 421 can be connected. In this way, when multiple mounting pieces 421 are arranged into a mounting cylinder 42, it can play a temporary fixing role, which not only facilitates installation, but also improves the assembly speed.
[0044] Optionally, refer to Figures 3 to 4 The first connector 43 includes a protrusion 431 and a recess 432 that engage with each other. The protrusion 431 is connected to one of the two adjacent mounting pieces 421, and the recess 432 is connected to the other of the two adjacent mounting pieces 421.
[0045] In the above embodiment, the structure is simple by setting the interlocking protrusions 431 and recesses 432, and it is easy to operate when connecting two adjacent mounting pieces 421.
[0046] Specifically, the protrusion 431 can be a regular column or an irregular serrated shape, etc., and this application embodiment does not make a specific limitation. The first connector 43 between two adjacent mounting pieces 421 can be one or more. When there are multiple first connectors 43, one of the two adjacent mounting pieces 421 can be connected to only multiple protrusions 431 or multiple recesses 432, or it can be connected to both protrusions 431 and recesses 432, and this application embodiment does not make a specific limitation.
[0047] Optionally, refer to Figure 2 The mounting cylinder 42 is provided with a second connector 44, which is used to detachably connect multiple mounting pieces 421 to the outside of the first delivery pipe 2.
[0048] In the above embodiment, by providing the second connector 44, multiple mounting pieces 421 can be detachably connected to the outer wall of the first conveying pipe 2, which facilitates later maintenance and repair.
[0049] Specifically, refer to Figure 2 The second connector 44 can be a clamp well known to those skilled in the art, or it can be other types of connectors. This application embodiment does not make specific limitations.
[0050] Optionally, refer to Figures 2 to 4 The heating unit 4 also includes a protective cylinder 45; the protective cylinder 45 is sleeved outside the heating element 41 and connected to the mounting cylinder 42; there is a gap between the protective cylinder 45 and the heating element 41 to reduce heat loss.
[0051] In the above embodiments, by covering the heating element 41 with a protective sleeve 45, heat loss from the heating element 41 can be reduced, and workers can be prevented from accidentally touching the heating element 41, thus achieving a protective effect. By creating a gap between the protective sleeve 45 and the heating element 41, the heating element 41 can be prevented from directly contacting the protective sleeve 45, further reducing heat loss and preventing workers from being burned by excessively high temperatures from the protective sleeve 45.
[0052] In the above embodiments, the protective cylinder 45 can be cylindrical, elliptical, or other shapes; this application does not impose specific limitations. The connection between the protective cylinder 45 and the mounting cylinder 42 can be detachable or fixed. For example, connecting plates can be provided at corresponding positions on the inner wall of the protective cylinder 45 and the outer wall of the mounting cylinder 42, and the two corresponding connecting plates can be connected by bolts. The connecting plates and bolts are not shown in the figure.
[0053] Optionally, refer to Figures 2 to 4 The protective cylinder 45 includes multiple protective plates 451; the multiple protective plates 451 are connected in sequence around the circumference of the mounting cylinder 42 to form the protective cylinder 45.
[0054] In the above embodiment, by setting multiple protective plates 451 and connecting them sequentially around the circumference of the mounting cylinder 42, multiple protective plates 451 can be arranged into a protective cylinder 45 along the circumference of the mounting cylinder 42 without damaging the existing first conveying pipe 2.
[0055] In the above embodiments, the number of protective plates 451 can be two, three, or four, etc., and this application does not impose a specific limitation. The mounting plate 421 can be an arc-shaped plate or other shapes. When multiple protective plates 451 are connected, the two sides of two adjacent protective plates 451 that are close to each other can fit together, and two adjacent protective plates 451 can also be partially overlapped. The connection method between multiple protective plates 451 is not specifically limited; for example, they can be connected by clamps.
[0056] Optionally, refer to Figure 1 The first delivery pipe 2 is also equipped with a temperature control unit 5, which is used to detect and adjust the temperature of the deionized water.
[0057] In the above embodiment, by setting a temperature control unit 5, it is convenient to detect the temperature of the deionized water after it has been heated by the heating unit 4, and adjust it in real time after the temperature of the deionized water deviates from the appropriate range, so as to ensure that the temperature of the deionized water is always within the appropriate range, thereby ensuring the uniformity of the negative electrode slurry.
[0058] For example, refer to Figure 1 The temperature control unit 5 may include a temperature sensor 51 and a controller 52; the probe of the temperature sensor 51 is located inside the first delivery pipe 2 and between the heating unit 4 and the stirring tank 3; the controller 52 is connected to the temperature sensor 51 and the heating element 41; the controller 52 is used to adjust the heating power of the heating element 41 according to the temperature collected by the temperature sensor 51, so that the temperature of the deionized water is within a suitable range.
[0059] In this embodiment, by installing a heating unit 4 on the first conveying pipe 2, deionized water is heated and then conveyed to the mixing tank 3 to mix with the solid components. During the mixing process, the movement of water molecules accelerates, and the collisions between water molecules and solid component molecules become more frequent. This helps to break the interaction forces between slurry particles, making it easier for the solid component molecules to disperse, improving the overall fluidity of the slurry. Consequently, the negative electrode slurry is more evenly dispersed, improving its uniformity and ultimately enhancing the quality of the electrode sheet, thus improving the overall performance and lifespan of the lithium battery. Moreover, in this embodiment, heating the deionized water in the first conveying pipe 2 is more economical and energy-efficient than heating the mixed slurry, and it is also easier to modify existing slurry preparation equipment.
[0060] In the description of this specification, references to terms such as "some embodiments," "other embodiments," "exemplarily," "specifically," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of this application. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0061] Although embodiments of this application have been shown and described, those skilled in the art will understand that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of this application, the scope of which is defined by the claims and their equivalents.
Claims
1. A lithium battery negative electrode slurry preparation apparatus, characterized in that, include: Water storage tank (1), the water storage tank (1) is used to store deionized water; Mixing tank (3); The first conveying pipe (2) is connected at one end to the water storage tank (1) and at the other end to the stirring tank (3). The first conveying pipe (2) is used to convey deionized water from the water storage tank (1) to the stirring tank (3). The stirring tank (3) is used to mix and stir the deionized water and solid components. The first conveying pipe (2) is provided with a heating unit (4), which is used to heat the deionized water in the first conveying pipe (2); The heating unit (4) includes a heating element (41) which is wound around the first conveying pipe (2) and extends spirally along the axial direction of the first conveying pipe (2); The heating unit (4) also includes a mounting cylinder (42); The mounting cylinder (42) is sleeved outside the first conveying pipe (2) and is located between the heating element (41) and the first conveying pipe (2); The mounting cylinder (42) is used to connect the heating element (41) and the first delivery pipe (2); The mounting cylinder (42) includes multiple mounting pieces (421); Multiple mounting pieces (421) are connected in sequence around the circumference of the first delivery pipe (2) to form the mounting cylinder (42).
2. The lithium battery negative electrode slurry preparation apparatus according to claim 1, characterized in that, A first connector (43) is provided between adjacent mounting pieces (421), and the first connector (43) is used to connect two adjacent mounting pieces (421).
3. The lithium battery negative electrode slurry preparation apparatus according to claim 2, characterized in that, The first connector (43) includes a protrusion (431) and a recess (432) that engage with each other. The protrusion (431) is connected to one of the two adjacent mounting pieces (421), and the recess (432) is connected to the other of the two adjacent mounting pieces (421).
4. The lithium battery negative electrode slurry preparation apparatus according to claim 1, characterized in that, The mounting cylinder (42) is provided with a second connector (44), which is used to detachably connect a plurality of mounting pieces (421) to the outside of the first delivery pipe (2).
5. The lithium battery negative electrode slurry preparation apparatus according to claim 1, characterized in that, The heating unit (4) also includes a protective cylinder (45); The protective sleeve (45) is fitted over the heating element (41) and connected to the mounting sleeve (42); There is a gap between the protective cylinder (45) and the heating element (41) to reduce heat loss.
6. The lithium battery negative electrode slurry preparation apparatus according to claim 5, characterized in that, The protective cylinder (45) includes multiple protective plates (451); Multiple protective plates (451) are connected in sequence around the circumference of the mounting cylinder (42) to form the protective cylinder (45).