A high-strength, sharp-angled steel cold and hot composite forming mold

By introducing an external heat dissipation and chip removal mechanism into the high-strength sharp-angle steel cold and hot composite forming mold, the problem of complex maintenance of mold cooling components is solved, realizing convenient maintenance and efficient production, and improving production quality and efficiency.

CN224977289UActive Publication Date: 2026-11-17WUXI GUANGXING DONGMAO TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522681138.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-18
Publication Date
2026-11-17
Estimated Expiration
2035-12-18

AI Technical Summary

Technical Problem

Existing high-strength, sharp-angled steel cold and hot composite forming molds are complex to maintain and repair in terms of cooling components, which affects work efficiency and makes it difficult to meet actual use needs.

Method used

A high-strength, sharp-angled steel cold-hot composite forming mold was designed. It adopts an external heat dissipation and cooling mechanism, combined with demolding and chip removal, adjustable conveying, chip collection and cold pressing refining mechanism, to realize convenient maintenance of cooling components and rapid demolding, reduce operation difficulty and improve production efficiency.

Benefits of technology

The design of external cooling components simplifies the maintenance process, reduces labor and time costs, improves work efficiency, and ensures the forming quality and production efficiency of sharp-angle steel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224977289U_ABST
    Figure CN224977289U_ABST
Patent Text Reader

Abstract

This utility model provides a high-strength, sharp-angled steel hot-cold composite forming mold, relating to the field of metal precision forming mold technology. It includes a processing table, a fixed frame mounted on top of the processing table; a heat dissipation and cooling mechanism located at one end of the fixed frame; an adjusting conveying mechanism located at the bottom of the processing table; a demolding and chip removal mechanism located on top of the adjusting conveying mechanism; a chip collection mechanism located at the bottom of the adjusting conveying mechanism; a hot pressing forming mechanism located at one top end of the processing table; and a cold pressing refining mechanism located at the other top end of the processing table. In this utility model, by setting up a heat dissipation and cooling mechanism, the cooling components can be externally mounted, ensuring heat dissipation and cooling effects while facilitating subsequent maintenance or repair, effectively reducing operational difficulty, saving labor and time costs, improving overall work efficiency, and meeting practical application needs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of metal precision forming mold technology, and in particular to a high-strength cold and hot composite forming mold for sharp-angled steel. Background Technology

[0002] As industries such as automotive, construction, and aerospace move towards lightweighting, high strength, and low carbon emissions, the application of high-strength, sharp-angled steel sections is becoming increasingly widespread. This type of steel not only requires high yield strength but also stringent requirements for angular accuracy and dimensional stability at the sharp corners. However, conventional steel sections struggle to balance high strength with the forming effect of complex sharp corners. This necessitates suitable forming dies to overcome processing limitations and meet the mass production demands of various industries for high-quality steel sections.

[0003] When using existing high-strength sharp-angle steel cold and hot composite forming molds, the heated steel is usually put into the hot pressing mold for preliminary hot pressing, and then the preliminary formed sharp-angle steel is refined by cold pressing, thereby improving the quality and strength of the sharp-angle steel.

[0004] However, most existing high-strength sharp-angle steel cold and hot composite forming molds involve cold pressing while cooling the steel inside the mold. This makes the maintenance and repair of the cooling components more complicated, which can easily affect work efficiency and make it difficult to meet actual use needs. Utility Model Content

[0005] This utility model mainly provides a high-strength, sharp-angled steel cold and hot composite forming mold with easy-to-maintain cooling components and quick demolding and chip removal capabilities.

[0006] To achieve the above objectives, this utility model adopts the following technical solution: a high-strength, sharp-angled steel cold and hot composite forming mold, comprising: a processing table, A fixed frame is installed on top of the processing table; A heat dissipation and cooling mechanism is disposed at one end of the fixed frame; An adjustable conveying mechanism is located at the bottom of the processing table; A demolding and chip removal mechanism is located on top of the adjusting conveying mechanism; A debris collection mechanism is located at the bottom of the regulating conveying mechanism; A hot pressing forming mechanism is located at one end of the top of the processing table; A cold pressing refining mechanism is located at the other end of the top of the processing table; The heat dissipation and cooling mechanism includes a tubular cooler, which is installed at one end of a fixed frame. Heat-conducting fins are installed on both sides of one end of the fixed frame. Both ends of the tubular cooler are connected to a distribution pipe. A cooling coil is connected to the outside of each distribution pipe. Each cooling coil is attached to the outside of a corresponding heat-conducting fin. A coolant inlet is installed on the outside of the tubular cooler. A coolant outlet is installed on the outside of the tubular cooler. One end of the coolant outlet is connected to a drain pipe.

[0007] Preferably, the demolding and chip removal mechanism includes a forming mold base, which is disposed on top of the adjusting conveying mechanism. A chip removal port is provided through the bottom of the forming mold base. Four dampers are installed on the inner bottom of the forming mold base. A spring is sleeved on the outer side of each damper. An ejector block is installed on the top of every two dampers. By setting up the demolding and chip removal mechanism, the demolding component can be built into the mold base, thereby greatly reducing the demolding difficulty after the sharp-angle steel is formed. At the same time, it can quickly remove the metal chips generated during the hot pressing process, prevent the surface of the sharp-angle steel from being damaged by friction, and thus improve the production quality.

[0008] Preferably, the adjusting conveying mechanism includes a mounting frame, which is installed at the bottom of the processing table. Two guide rods are installed inside the mounting frame, and a sliding frame is slidably mounted on the outer sides of the two guide rods. A connecting frame is connected to the top of the sliding frame, and a support is installed on the top of the connecting frame. A servo cylinder is installed at one end of the mounting frame, and the output end of the servo cylinder moves through the mounting frame and connects to the sliding frame. By adjusting the settings of the conveying mechanism, the processed steel can be quickly moved and transported from the hot pressing section to the cold pressing section, reducing heat loss, improving overall work efficiency, and reducing operational difficulty.

[0009] Preferably, the debris collection mechanism includes a mounting frame installed at the bottom of the sliding frame, and a collection box inserted inside the mounting frame. One end of the collection box is equipped with a pull ring. By setting up the debris collection mechanism, the discharged metal debris can be collected for convenient subsequent centralized processing.

[0010] Preferably, the hot pressing forming mechanism includes four first fixed rods, all of which are installed on the top of the processing table. A first top plate is installed on the top of the four first fixed rods, and a first servo hydraulic cylinder is installed on the top of the first top plate. The output end of the first servo hydraulic cylinder moves through the first top plate and is connected to a first mounting plate. The first mounting plate is slidably installed on the outside of the four first fixed rods, and a hot pressing upper mold is installed at the bottom of the first mounting plate. By setting up the hot pressing forming mechanism, preliminary hot pressing forming of steel can be achieved, improving the overall work efficiency.

[0011] Preferably, the cold pressing refining mechanism includes four second fixed rods, all of which are mounted on the top of the processing table. A second top plate is mounted on the top of the four second fixed rods, and a second servo hydraulic cylinder is mounted on the top of the second top plate. The output end of the second servo hydraulic cylinder passes through the second top plate and is connected to a second mounting plate. The second mounting plate is slidably mounted on the outside of the four second fixed rods, and a cold pressing upper die is mounted on the bottom of the second mounting plate. By setting up the cold pressing refining mechanism, the steel can be further cold-pressed and refined, thereby improving the quality of the sharp-angled steel.

[0012] Preferably, the processing table is equipped with support legs at all four corners of its bottom, and each support leg is equipped with an anti-slip pad at its bottom. The support legs and anti-slip pads provide stable support for the mold as a whole, while increasing the friction with the ground to prevent it from shaking or shifting.

[0013] Compared with the prior art, the advantages and positive effects of this utility model are as follows: 1. In this utility model, by setting a heat dissipation and cooling mechanism, the cooling components can be externally placed, ensuring heat dissipation and cooling effect while facilitating subsequent maintenance or repair, effectively reducing the difficulty of operation, saving labor and time costs, improving overall work efficiency, and meeting actual use needs.

[0014] 2. In this utility model, by setting a demolding and chip removal mechanism, the demolding component can be built into the mold base, thereby greatly reducing the demolding difficulty after the sharp-angled steel is formed. At the same time, it can quickly remove the metal chips generated during the hot pressing process, prevent the surface of the sharp-angled steel from being damaged by friction, and thus improve the production quality. Attached Figure Description

[0015] Figure 1 A perspective view of a high-strength, sharp-angled steel cold-hot composite forming mold is provided for this utility model; Figure 2 A side view of a high-strength, sharp-angled steel cold-hot composite forming mold is provided for this utility model; Figure 3 An enlarged perspective view of the heat dissipation and cooling mechanism of a high-strength, sharp-angled steel cold-heat composite forming mold is provided for this utility model; Figure 4 An enlarged perspective view of the adjustment and conveying mechanism of a high-strength, sharp-angled steel cold and hot composite forming mold is provided for this utility model. Figure 5 This utility model presents a partial structural cross-sectional view of a high-strength, sharp-angled steel cold-hot composite forming mold.

[0016] Legend: 1. Processing table; 2. Fixed frame; 3. Heat dissipation and cooling mechanism; 301. Tubular cooler; 302. Heat-conducting fins; 303. Diverter pipe; 304. Cooling coil; 305. Coolant inlet; 306. Coolant outlet; 307. Drain pipe; 4. Demolding and chip removal mechanism; 401. Forming mold base; 402. Chip removal port; 403. Damper; 404. Spring; 405. Ejector block; 5. Adjustable conveying mechanism; 501. Mounting bracket; 502. Guide rod; 503. Sliding bracket; 504. Connection Frame; 505, Support; 506, Servo Cylinder; 6, Debris Collection Mechanism; 601, Mounting Frame; 602, Collection Box; 603, Pull Ring; 7, Hot Press Forming Mechanism; 701, First Fixing Rod; 702, First Top Plate; 703, First Servo Hydraulic Cylinder; 704, First Mounting Plate; 705, Hot Press Upper Mold; 8, Cold Press Refining Mechanism; 801, Second Fixing Rod; 802, Second Top Plate; 803, Second Servo Hydraulic Cylinder; 804, Second Mounting Plate; 805, Cold Press Upper Mold; 9, Support Leg; 10, Anti-slip Pad. Detailed Implementation

[0017] To better understand the above-mentioned objectives, features, and advantages of this utility model, the present utility model will be further described below with reference to the accompanying drawings and embodiments. It should be noted that, unless otherwise specified, the embodiments and features described in these embodiments can be combined with each other.

[0018] Many specific details are set forth in the following description in order to provide a full understanding of the present invention. However, the present invention may also be implemented in other ways different from those described herein. Therefore, the present invention is not limited to the specific embodiments disclosed in the following specification.

[0019] Please see Figures 1-5 This utility model provides a technical solution: a high-strength, sharp-angled steel cold and hot composite forming mold, including a processing table 1. Fixed frame 2 is installed on top of processing table 1; The heat dissipation and cooling mechanism 3 is located at one end of the fixed frame 2; Adjustable conveyor mechanism 5 is located at the bottom of processing table 1; The demolding and chip removal mechanism 4 is located on top of the adjusting conveying mechanism 5; The debris collection mechanism 6 is located at the bottom of the regulating conveying mechanism 5; The hot pressing forming mechanism 7 is located at one end of the top of the processing table 1; The cold pressing refining mechanism 8 is located at the other end of the top of the processing table 1; The heat dissipation and cooling mechanism 3 includes a tubular cooler 301, which is installed at one end of the fixed frame 2. Heat-conducting fins 302 are installed on both sides of one end of the fixed frame 2. Both ends of the tubular cooler 301 are connected to branch pipes 303. A cooling coil 304 is connected to the outside of each branch pipe 303. Each cooling coil 304 is attached to the outside of a corresponding heat-conducting fin 302. A coolant inlet 305 and a coolant outlet 306 are installed on the outside of the tubular cooler 301. One end of the coolant outlet 306 is connected to a drain pipe 307. By setting up the heat dissipation and cooling mechanism 3, the cooling components can be externally mounted, ensuring heat dissipation and cooling effects while facilitating subsequent maintenance or repair. This effectively reduces operational difficulty, saves labor and time costs, improves overall work efficiency, and meets actual usage requirements.

[0020] like Figure 2 and Figure 5 As shown, the demolding and chip removal mechanism 4 includes a forming mold base 401, which is located on top of the adjusting conveying mechanism 5. A chip removal port 402 is provided through the bottom of the forming mold base 401. Four dampers 403 are installed on the inner bottom of the forming mold base 401. A spring 404 is sleeved on the outer side of each damper 403. An ejector block 405 is installed on the top of every two dampers 403. By setting up the demolding and chip removal mechanism 4, the demolding component can be built into the mold base, which greatly reduces the demolding difficulty after the sharp angle steel is formed. At the same time, it can quickly remove the metal chips generated during the hot pressing process, prevent the surface of the sharp angle steel from being damaged by friction, and thus improve the production quality.

[0021] like Figure 1 , Figure 2 and Figure 4 As shown, the adjusting conveying mechanism 5 includes a mounting frame 501, which is installed at the bottom of the processing table 1. Two guide rods 502 are installed inside the mounting frame 501, and a sliding frame 503 is slidably installed on the outer side of the two guide rods 502. A connecting frame 504 is connected to the top of the sliding frame 503, and a support 505 is installed on the top of the connecting frame 504. A servo cylinder 506 is installed at one end of the mounting frame 501. The output end of the servo cylinder 506 moves through the mounting frame 501 and is connected to the sliding frame 503. By adjusting the setting of the conveying mechanism 5, the processed steel can be quickly moved and transported from the hot pressing section to the cold pressing section, reducing heat loss, improving overall work efficiency, and reducing operation difficulty.

[0022] like Figure 1 and Figure 4As shown, the debris collection mechanism 6 includes a mounting frame 601, which is installed at the bottom of the sliding frame 503. A collection box 602 is inserted inside the mounting frame 601, and a pull ring 603 is installed at one end of the collection box 602. Through the setting of the debris collection mechanism 6, the discharged metal debris can be collected for convenient subsequent centralized processing.

[0023] like Figure 1 and Figure 2 As shown, the hot pressing forming mechanism 7 includes four first fixing rods 701, all of which are mounted on the top of the processing table 1. A first top plate 702 is mounted on the top of the four first fixing rods 701, and a first servo hydraulic cylinder 703 is mounted on the top of the first top plate 702. The output end of the first servo hydraulic cylinder 703 passes through the first top plate 702 and is connected to a first mounting plate 704. The first mounting plate 704 is slidably mounted on the outside of the four first fixing rods 701, and a hot pressing upper mold 705 is mounted on the bottom of the first mounting plate 704. By setting up the hot pressing forming mechanism 7, preliminary hot pressing forming of steel can be achieved, improving the overall work efficiency.

[0024] like Figure 1 and Figure 2 As shown, the cold pressing refining mechanism 8 includes four second fixing rods 801, all of which are mounted on the top of the processing table 1. A second top plate 802 is mounted on the top of the four second fixing rods 801, and a second servo hydraulic cylinder 803 is mounted on the top of the second top plate 802. The output end of the second servo hydraulic cylinder 803 movably passes through the second top plate 802 and is connected to a second mounting plate 804. The second mounting plate 804 is slidably mounted on the outside of the four second fixing rods 801, and a cold pressing upper mold 805 is mounted on the bottom of the second mounting plate 804. Through the setting of the cold pressing refining mechanism 8, the steel can be further cold-pressed and refined, thereby improving the quality of the sharp-angled steel.

[0025] like Figure 1 and Figure 2 As shown, each of the four corners of the bottom of the processing table 1 is equipped with a support leg 9, and each support leg 9 is equipped with an anti-slip pad 10. By setting the support leg 9 and the anti-slip pad 10, the mold can be provided with stable support, while increasing the friction with the ground to prevent it from shaking or shifting.

[0026] The operating method and working principle of this device are as follows: First, the preheated steel is placed on top of the forming mold base 401. The first servo hydraulic cylinder 703 is activated, pushing the first mounting plate 704 to slide on the first fixed rod 701, which drives the hot pressing upper mold 705 to hot press it, thus initially forming it. The metal chips generated during the hot pressing process will fall from the chip discharge port 402 into the collection box 602 and be collected. Then, after the hot pressing is completed, the damper 403 and the spring 404 push the ejector block 405 to lift the initially formed sharp-angled steel. Then, the servo cylinder 506 is activated, pushing the sliding frame 503 to slide on the guide rod 502. The forming die base 401 reaches below the cold pressing upper die 805. The second servo hydraulic cylinder 803 pushes the second mounting plate 804 to drive the cold pressing upper die 805 to press down, further refining the steel by cold pressing. Finally, during the cold pressing process, external coolant is connected to the coolant input end 305. The tubular cooler 301 drives the coolant to flow in the distribution pipe 303 and cooling coil 304. The heat-conducting fins 302 dissipate heat and cool the formed sharp-angled steel to improve its strength. After cooling, the damper 403 and spring 404 push the ejector block 405 to lift the formed sharp-angled steel for rapid demolding.

[0027] By following the steps outlined above, you can complete the use of the high-strength, sharp-angled steel cold and hot composite forming mold.

[0028] The above description is merely a preferred embodiment of the present utility model and is not intended to limit the present utility model in any other way. Any person skilled in the art may make changes or modifications to the above-disclosed technical content to create equivalent embodiments for application in other fields. However, any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of the present utility model without departing from the technical solution of the present utility model shall still fall within the protection scope of the technical solution of the present utility model.

Claims

1. A high-strength, sharp-angled steel cold and hot composite forming mold, characterized in that, include: Processing table (1) A fixed frame (2) is installed on top of the processing table (1); A heat dissipation and cooling mechanism (3) is provided at one end of the fixed frame (2); Adjust the conveying mechanism (5), which is located at the bottom of the processing table (1); The demolding and chip removal mechanism (4) is located on top of the adjusting conveying mechanism (5); A debris collection mechanism (6) is provided at the bottom of the regulating conveying mechanism (5); A hot pressing forming mechanism (7) is disposed at one end of the top of the processing table (1); The cold pressing refining mechanism (8) is located at the other end of the top of the processing table (1); The heat dissipation and cooling mechanism (3) includes a tubular cooler (301), which is installed at one end of a fixed frame (2). Heat-conducting fins (302) are installed on both sides of one end of the fixed frame (2). Both ends of the tubular cooler (301) are connected to a branch pipe (303). A cooling coil (304) is connected to the outside of each branch pipe (303). Each cooling coil (304) is attached to the outside of a corresponding heat-conducting fin (302). A coolant inlet (305) is installed on the outside of the tubular cooler (301). A coolant outlet (306) is installed on the outside of the tubular cooler (301). One end of the coolant outlet (306) is connected to a drain pipe (307).

2. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 1, characterized in that: The demolding and chip removal mechanism (4) includes a forming mold base (401), which is located on top of the adjusting conveying mechanism (5). A chip removal port (402) is opened through the bottom of the forming mold base (401). Four dampers (403) are installed on the inner bottom of the forming mold base (401). A spring (404) is sleeved on the outer side of each damper (403). An ejector block (405) is installed on the top of every two dampers (403).

3. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 1, characterized in that: The adjusting conveying mechanism (5) includes a mounting frame (501), which is installed at the bottom of the processing table (1). Two guide rods (502) are installed inside the mounting frame (501). A sliding frame (503) is slidably installed on the outside of the two guide rods (502). A connecting frame (504) is connected to the top of the sliding frame (503). A support (505) is installed on the top of the connecting frame (504). A servo cylinder (506) is installed at one end of the mounting frame (501). The output end of the servo cylinder (506) moves through the mounting frame (501) and is connected to the sliding frame (503).

4. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 3, characterized in that: The debris collection mechanism (6) includes a mounting frame (601) which is installed at the bottom of the sliding frame (503). A collection box (602) is inserted inside the mounting frame (601), and a pull ring (603) is installed at one end of the collection box (602).

5. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 1, characterized in that: The hot pressing forming mechanism (7) includes four first fixing rods (701), all four first fixing rods (701) are installed on the top of the processing table (1), a first top plate (702) is installed on the top of the four first fixing rods (701), a first servo hydraulic cylinder (703) is installed on the top of the first top plate (702), the output end of the first servo hydraulic cylinder (703) moves through the first top plate (702) and is connected to the first mounting plate (704), the first mounting plate (704) is slidably installed on the outside of the four first fixing rods (701), and a hot pressing upper mold (705) is installed at the bottom of the first mounting plate (704).

6. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 1, characterized in that: The cold pressing refining mechanism (8) includes four second fixing rods (801), all four second fixing rods (801) are installed on the top of the processing table (1), a second top plate (802) is installed on the top of the four second fixing rods (801), a second servo hydraulic cylinder (803) is installed on the top of the second top plate (802), the output end of the second servo hydraulic cylinder (803) moves through the second top plate (802) and is connected to the second mounting plate (804), the second mounting plate (804) is slidably installed on the outside of the four second fixing rods (801), and a cold pressing upper mold (805) is installed at the bottom of the second mounting plate (804).

7. The high-strength sharp-angle steel cold and hot composite forming mold according to claim 1, characterized in that: The processing table (1) has four support legs (9) installed at the bottom corners, and each support leg (9) has an anti-slip pad (10) installed at the bottom.