A low-pressure casting mold
By introducing heating devices, mold fixing structures, and cooling devices into low-pressure casting molds, problems such as inaccurate positioning, uneven baking, slow cooling, and gate adhesion have been solved, thereby improving mold stability and production efficiency.
Patent Information
- Application Number
- CN202522133063.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-09
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-10-09
AI Technical Summary
Existing low-pressure casting molds have problems such as inaccurate positioning leading to deformation, large mold closing gaps, uneven baking leading to cold shuts, slow cooling efficiency, and easy sticking at the gate, making demolding difficult.
The system employs a heating device for assisted baking, an overall mold base for fixation, precise positioning blocks for accurate positioning, and a cooling device for rapid cooling. It also uses a gate ceramic sleeve and a gate bushing at the gate to prevent sticking, combined with optimized positioning stops and gate structure.
It achieves uniform heating of the mold, improved stability, reduced deformation, extended service life, improved cooling efficiency, and convenient demolding, thereby improving production efficiency and product qualification rate.
Smart Images

Figure CN224977475U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of molds, and in particular to a low-pressure casting mold. Background Technology
[0002] Low-pressure casting molds are special molds used in low-pressure casting processes. They are formed by using air pressure to drive molten metal to fill the cavity from bottom to top. Existing low-pressure casting molds are prone to the following problems: 1. Most traditional low-pressure molds do not have a precise positioning structure, which makes the mold easy to be squeezed and deformed, and the large gap between the molds results in flash; 2. Traditional molds use a single gas heating method, which can easily lead to uneven heating and casting cold shuts; 3. The casting blank is self-cooled, which has a slow cooling efficiency and affects production efficiency; 4. Molten aluminum at the bottom gate is prone to sticking to the mold and is difficult to demold. Utility Model Content
[0003] To address the problems existing in the prior art, this utility model provides a low-pressure casting mold, including a mold body. The interior of the mold body is provided with a lower cavity and an upper cavity. A gate is provided at the bottom of the mold body. A mold core and a cooling device are also provided at the top of the mold body. A heating device is also provided on the outside of the mold body.
[0004] Furthermore, the mold body is also provided with a gate ceramic sleeve and a gate bushing at the gate.
[0005] Furthermore, a mold foot is provided above the mold body, and a base plate is provided below the mold body.
[0006] Furthermore, the mold foot is an integral structure fixedly connected to the low-pressure machine, and the base plate is precisely positioned with the low-pressure machine through positioning blocks.
[0007] Furthermore, both the lower and upper cavities of the mold body are provided with positioning stops.
[0008] Furthermore, the lower cavity and upper cavity of the mold body are also provided with casting blanks.
[0009] Compared with the prior art, the beneficial effects of this utility model are: This invention utilizes an oven baking system combined with a heating device for auxiliary baking, ensuring uniform heating of the mold body, reducing casting defects such as cold shuts, and improving product qualification rate. The mold body is fixed by mold feet in the overall structure, ensuring overall stress distribution and improving stability. Precise positioning is achieved through a base plate, positioning blocks, and a low-pressure press. The lower and upper cavities are positioned using positioning stops, minimizing mold deformation and extending mold life. Finally, rapid cooling is achieved through a cooling device. Furthermore, the mold body's gate uses a dedicated gate sleeve and gate bushing to prevent molten aluminum from sticking to the mold, thus facilitating rapid demolding and further improving production efficiency. Attached Figure Description
[0010] Figure 1 This is a schematic diagram of the internal structure of the present invention; Figure 2 This is a schematic diagram of the overall structure of this utility model; Figure 3 This is a bottom view of the present invention; Figure 4 This is a schematic diagram of the lower cavity and a partial structure of the upper cavity of this utility model.
[0011] Reference numerals: 1. Sprue sleeve; 2. Sprue bushing; 3. Base plate; 4. Lower cavity; 5. Heating device; 6. Casting blank; 7. Upper cavity; 8. Mold core; 9. Cooling device; 10. Mold foot; 11. Mold body. Detailed Implementation
[0012] To make the technical means, creative features, and achieved objectives and effects of this utility model easier to understand, the present utility model is further described below with reference to specific embodiments and accompanying drawings. However, the following embodiments are merely preferred embodiments of this utility model and not all of them. Other embodiments obtained by those skilled in the art based on the embodiments described in the implementation details without creative effort are all within the protection scope of this invention.
[0013] The specific embodiments of this utility model are described below with reference to the accompanying drawings.
[0014] Example 1 like Figure 1-4 As shown, a low-pressure casting mold includes a mold body 11. The interior of the mold body 11 is provided with a lower cavity 4 and an upper cavity 7. A gate is provided at the bottom of the mold body 11. A mold core 8 and a cooling device 9 are provided at the top of the mold body 11. A heating device 5 is also provided on the outside of the mold body 11. In this embodiment, the mold body 11 is also provided with a gate sleeve 1 and a gate bushing 2 at the gate. The mold body 11 is also provided with a mold foot 10 on the top and a base plate 3 on the bottom. The mold foot 10 is an integral structure and is fixedly connected to the low-pressure machine. The base plate 3 is precisely positioned with the low-pressure machine through a positioning block. The lower cavity 4 and the upper cavity 7 of the mold body 11 are both provided with positioning stops. The lower cavity 4 and the upper cavity 7 of the mold body 11 are also provided with casting blanks 6.
[0015] Working principle description: The mold body 11 is baked in an oven and then assisted by a heating device 5 to ensure uniform heating of the mold body 11, reduce casting defects such as cold shuts, and improve product qualification rate. Once the casting temperature is reached, it can be used with a low-pressure press to start casting through the gate. Before casting, the mold body 11 is first fixed to the low-pressure press by the mold feet 10, so that the mold body 11 is subjected to overall force and improves stability. The base plate 3, together with the positioning block, achieves precise positioning with the low-pressure press. The lower cavity 4 and the upper cavity 7 are positioned by positioning stops, which reduces the amount of mold deformation and extends the mold service life. Finally, the cooling device 9 achieves rapid cooling. The gate of the mold body 11 uses a special gate sleeve 1 and gate bushing 2 to prevent the bottom aluminum from sticking to the mold and making it difficult to demold, which would facilitate the subsequent rapid demolding work and further improve production efficiency.
[0016] The foregoing has shown and described the basic principles, main features, and advantages of this utility model. Those skilled in the art should understand that this utility model is not limited to the above embodiments. The embodiments and descriptions in the specification are merely preferred examples and are not intended to limit the utility model. Various changes and modifications can be made to this utility model without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed utility model. The scope of protection of this utility model is defined by the appended claims and their equivalents.
Claims
1. A low pressure casting mold comprising a mold body (11), characterized by: The mold body (11) is provided with a lower cavity (4) and an upper cavity (7) inside. The mold body (11) is provided with a gate at the bottom. The mold body (11) is also provided with a mold core (8) and a cooling device (9) at the top. The mold body (11) is also provided with a heating device (5) on the outside.
2. The low-pressure casting mold according to claim 1, characterized in that: The mold body (11) is also provided with a gate ceramic sleeve (1) and a gate bushing (2) at the gate.
3. The low-pressure casting mold according to claim 1, characterized in that: The mold body (11) is provided with mold feet (10) above it and a base plate (3) is provided below it.
4. A low-pressure casting mold according to claim 3, characterized in that: The mold foot (10) is an integral structure that is fixedly connected to the low-pressure machine, and the base plate (3) is precisely positioned with the low-pressure machine through the positioning block.
5. A low-pressure casting mold according to claim 1, characterized in that: The mold body (11) is provided with positioning stops in both the lower cavity (4) and the upper cavity (7).
6. A low-pressure casting mold according to claim 1, characterized in that: The mold body (11) is further provided with casting blanks (6) in the lower cavity (4) and upper cavity (7).