A temporary spot welding fixture for pipe joints

By designing a temporary spot welding fixture for pipe joints with automatic pre-tightening force adjustment, the problem of inconvenience in manual adjustment in the existing technology is solved, and the stability and quality of electrothermal sleeve welding are improved.

CN224979212UActive Publication Date: 2026-11-17HEBEI XICHANG ENG CONSTR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522584134.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-05
Publication Date
2026-11-17
Estimated Expiration
2035-12-05

AI Technical Summary

Technical Problem

The existing temporary spot welding fixtures require manual pre-tightening force adjustment, which is inconvenient and leads to insufficient connection between the electrothermal sleeve and the outer sleeve of the insulation pipe. Changes in diameter affect the welding quality.

Method used

A clamp body comprising an arc plate, a locking plate, and a locking bar is designed, equipped with a preload adjustment mechanism. Automatic preload adjustment is achieved using a cylinder and a plug-in block, and precise measurement and cutting are performed in conjunction with a measuring rod and a scale.

Benefits of technology

It achieves automatic adjustment of the clamp preload, improves the stability and quality of electrothermal welding, avoids the inconvenience of manual adjustment, and enhances the welding effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224979212U_ABST
    Figure CN224979212U_ABST
Patent Text Reader

Abstract

This utility model discloses a temporary spot welding fixture for pipe joints, belonging to the field of pipeline construction technology. It includes a fixture body and a pre-tightening force adjustment mechanism. The fixture body consists of an arc-shaped plate, a locking plate, and locking strips. The locking plate is fixedly connected to the outer wall of one side of the arc-shaped plate. Two locking strips are provided, each fixedly connected to the outer wall of the other side of the arc-shaped plate. The pre-tightening force adjustment mechanism is located on the fixture body. The arc-shaped plate, locking plate, and two locking strips constitute the fixture body. The fixture body facilitates the fixing of the electrofusion sleeve at the joint of the insulated pipe, thus facilitating subsequent electrofusion sleeve welding. The fixing plate in the pre-tightening force adjustment mechanism provides support for the cylinder, improving its stability. The insertion block facilitates docking with the insertion slot on the joint block, and the cylinder facilitates the movement of the joint plate. This allows for automatic pre-tightening force adjustment of the fixture body during welding, improving the clamping effect of the fixture body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of pipeline construction technology, and more specifically, to a temporary spot welding fixture for pipeline docking interfaces. Background Technology

[0002] Polyurethane insulated pipes are high-strength insulated pipes that mainly use steel pipes as the main material, rigid polyurethane foam as the protective layer, and high-density polyethylene as the protective shell. They are mainly used in various hot and cold pipeline transportation industries. Direct-buried polyurethane insulated pipes are directly connected and laid underground during installation. When connecting the pipes, it is necessary to insulate and repair the metal steel pipes of the two interconnected polyurethane insulated pipes.

[0003] Temporary spot welding fixtures are positioning and pre-fixing tools in the electrofusion sleeve repair process of polyurethane insulation pipes, and are crucial for ensuring the quality of the repair.

[0004] Currently available temporary spot welding fixtures mostly require manual adjustment of the pre-tightening force during use, which is inconvenient. In addition, during the welding of the electrofusion sleeve, its diameter will change slightly. Manually adjusting the pre-tightening force of the fixture can easily lead to insufficient connection between the electrofusion sleeve and the outer sleeve of the insulation pipe. Utility Model Content

[0005] In view of the problems existing in the prior art, the purpose of this utility model is to provide a temporary spot welding fixture for pipe docking interfaces, which aims to solve the problems mentioned in the background art.

[0006] To solve the above problems, the present invention adopts the following technical solution: A temporary spot welding fixture for pipe joints, comprising: The clamp body comprises an arc-shaped plate, a locking plate, and locking strips. The locking plate is fixedly connected to the outer wall of one side of the arc-shaped plate. Two locking strips are provided, each fixedly connected to the outer wall of the other side of the arc-shaped plate. The preload adjustment mechanism is located on the fixture body and is used to adjust the preload of the fixture body.

[0007] As a preferred embodiment of this utility model, the preload adjustment mechanism includes a fixed plate and a docking plate. The fixed plate is fixedly installed on the outer wall of the locking plate. A cylinder is fixedly installed on the outer wall of the locking plate. A plug-in block is fixedly installed on the telescopic end of the cylinder. The docking plate is fixedly installed between the outer walls of the two locking strips. A docking block is fixedly installed on one side of the outer wall of the docking plate. A plug-in groove is opened on one side of the outer wall of the docking block.

[0008] As a preferred embodiment of this utility model, a support plate is fixedly installed on one side of the outer wall of the locking plate, and the support plate is fixedly sleeved on the outer surface of the cylinder. Multiple reinforcing plates are fixedly installed between the support plate and the outer wall of the locking plate.

[0009] As a preferred embodiment of this utility model, an installation tube is fixedly embedded between the outer walls of the arc-shaped plate, a measuring rod is movably embedded inside the installation tube, and the outer wall of the measuring rod is engraved with a scale.

[0010] As a preferred embodiment of this utility model, a pull plate is fixedly installed at one end of the measuring rod.

[0011] As a preferred embodiment of this utility model, the outer walls of the arc-shaped plate, the locking plate, and the two locking strips are all provided with fixing grooves. Beneficial effects

[0012] Compared with the prior art, this utility model provides a temporary spot welding fixture for pipe joints, which has the following advantages: 1. In this solution, the arc plate, the locking plate and two locking strips constitute the clamp body. The clamp body can be used to fix the electrofusion sleeve at the joint of the insulation pipe, which facilitates the subsequent electrofusion sleeve welding work. The pre-tightening force adjustment mechanism can automatically adjust the pre-tightening force of the clamp body during the welding process, thereby improving the clamping effect of the clamp body.

[0013] 2. In this solution, the fixed plate provides support for the cylinder, improving its stability. The plug-in block facilitates docking with the plug slot on the docking block, and the cylinder can easily drive the docking plate to move. This facilitates the adjustment of the preload of the fixture body, avoiding the problem of insufficient manual adjustment and improving the welding effect of the electrothermal sleeve. Attached Figure Description

[0014] Figure 1 This is a perspective view of the present utility model; Figure 2 This is a second-view perspective perspective view of the present invention; Figure 3 This is a third-person perspective view of the present invention; Figure 4 This is a schematic diagram of the measuring rod in use in this utility model; Figure 5 This utility model Figure 4 Enlarged view of point A in the middle.

[0015] Explanation of the labels in the diagram: 1. Fixture body; 101. Arc plate; 102. Locking plate; 103. Locking strip; 2. Preload adjustment mechanism; 201. Fixing plate; 202. Butt joint plate; 203. Cylinder; 204. Insertion block; 205. Butt joint block; 206. Insertion groove; 3. Support plate; 4. Reinforcing plate; 5. Mounting tube; 6. Measuring rod; 7. Scale; 8. Pull plate. Detailed Implementation

[0016] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present utility model, not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present utility model without creative effort are within the scope of protection of the present utility model. Example

[0017] Please see Figure 1-5 A temporary spot welding fixture for pipe joints, comprising: The clamp body 1 and the preload adjustment mechanism 2 are provided. The clamp body 1 is composed of an arc plate 101, a locking plate 102 and a locking bar 103. The locking plate 102 is fixedly connected to the outer wall of one side of the arc plate 101. There are two locking bars 103, and each locking bar 103 is fixedly connected to the outer wall of the other side of the arc plate 101. The preload adjustment mechanism 2 is provided on the clamp body 1 to adjust the preload of the clamp body 1.

[0018] In this embodiment, the arc plate 101, the locking plate 102, and the two locking strips 103 constitute the clamp body 1. The clamp body 1 facilitates the fixing of the electrofusion sleeve at the joint of the insulation pipe, thereby facilitating the subsequent electrofusion sleeve welding work. The pre-tightening force adjustment mechanism 2 can automatically adjust the pre-tightening force of the clamp body 1 during the welding process, thereby improving the clamping effect of the clamp body 1.

[0019] Please refer to the specific details. Figure 1-2 and Figure 4 As shown, the preload adjustment mechanism 2 includes a fixed plate 201 and a docking plate 202. The fixed plate 201 is fixedly installed on the outer wall of the locking plate 102. A cylinder 203 is fixedly installed on the outer wall of the locking plate 102. A plug-in block 204 is fixedly installed on the telescopic end of the cylinder 203. The docking plate 202 is fixedly installed between the outer walls of the two locking bars 103. A docking block 205 is fixedly installed on one side of the outer wall of the docking plate 202. A plug-in groove 206 is opened on one side of the outer wall of the docking block 205.

[0020] In this embodiment, the fixing plate 201 provides support for the cylinder 203, improving its stability. The plug block 204 can be easily connected to the plug slot 206 on the docking block 205, and the cylinder 203 can easily drive the docking plate 202 to move, thereby facilitating the adjustment of the pre-tightening force of the fixture body 1, avoiding the problem of insufficient manual adjustment, and improving the welding effect of the electrothermal sleeve.

[0021] Please refer to the specific details. Figure 4 As shown, a support plate 3 is fixedly installed on one side of the outer wall of the locking plate 102, and the support plate 3 is fixedly sleeved on the outer surface of the cylinder 203. Multiple reinforcing plates 4 are fixedly installed between the support plate 3 and the outer wall of the locking plate 102.

[0022] In this embodiment, the stability of the cylinder 203 is further improved by the support plate 3, and the strength of the support plate 3 is improved by the reinforcing plate 4, thereby improving the performance of the cylinder 203.

[0023] Please refer to the specific details. Figure 3-5 As shown, an installation tube 5 is fixedly embedded between the outer walls of the arc plate 101, and a measuring rod 6 is movably embedded inside the installation tube 5. The outer wall of the measuring rod 6 is engraved with a scale 7.

[0024] In this embodiment, the measuring rod 6 is conveniently stored and retracted through the mounting tube 5. The measuring rod 6 and the surface scale 7 are convenient for measuring the edge of the clamped electrothermal sleeve, which in turn facilitates the cutting of the excess longitudinal overlap of the electrothermal sleeve.

[0025] Please refer to the specific details. Figure 4-5 As shown, a pull plate 8 is fixedly installed at one end of the measuring rod 6.

[0026] In this embodiment, the measuring rod 6 can be easily moved by the pull plate 8, which facilitates the measurement work.

[0027] Please refer to the specific details. Figure 1-4 As shown, the outer walls of the arc plate 101, the locking plate 102, and the two locking strips 103 are all provided with fixing grooves.

[0028] In this embodiment, the arc plate 101, the locking plate 102, and the two locking strips 103 are all made of high-strength aluminum alloy or composite material. At the same time, fixing grooves are opened on the outer walls of the arc plate 101, the locking plate 102, and the two locking strips 103 to reduce the weight of the clamp body 1 and make it convenient to carry and use.

[0029] Working principle: During use, after cleaning the pipe and the electrofusion sleeve, the electrofusion sleeve is overlapped on the outer wall of the insulation pipe. The electrofusion sleeve is clamped and fixed by the clamp body 1. Specifically: the arc plate 101 is close to the electrofusion sleeve, the locking plate 102 and the locking strip 103 are both around the electrofusion sleeve, and the locking plate 102 is inserted between the two locking strips 103. The insertion block 204 on the cylinder 203 is inserted into the insertion groove 206 on the mating block 205. The cylinder 203 is started, and the cylinder 203 drives the mating block 205 to... The docking plate 202 moves, the pre-tightening force of the clamp body 1 is adjusted, and the electrofusion sleeve is stably clamped. The measuring rod 6 is pulled out by the pull plate 8, and the longitudinal length of the electrofusion sleeve is measured by the measuring rod 6 and its surface scale 7. The excess overlapping part is cut off, and the output line of the welding machine is connected to the connecting line of the electrofusion sleeve. After power is turned on, the resistance wire of the electrofusion sleeve heats up, causing the electrofusion sleeve to melt and fuse with the pipe protection layer. At this time, the cylinder 203 continuously adjusts the pre-tightening force of the clamp body 1 accordingly to improve its use effect.

[0030] The control method of this utility model is to control the device by manually starting and stopping the switch. The wiring diagram of the power element and the supply of power are common knowledge in the field. Since this utility model is mainly used to protect mechanical devices, the control method and wiring layout will not be explained in detail.

[0031] The above description is only a preferred embodiment of the present utility model, but the protection scope of the present utility model is not limited thereto. Any equivalent substitutions or changes made by those skilled in the art within the technical scope disclosed in the present utility model based on the technical solution and its improved concept should be covered within the protection scope of the present utility model.

Claims

1. A pipe butt joint interface temporary spot welding jig, characterized by, include: The clamp body (1) is composed of an arc-shaped plate (101), a locking plate (102), and locking strips (103). The locking plate (102) is fixedly connected to one outer wall of the arc-shaped plate (101). There are two locking strips (103), each of which is fixedly connected to the other outer wall of the arc-shaped plate (101). The preload adjustment mechanism (2) is installed on the clamp body (1) and is used to adjust the preload of the clamp body (1).

2. A pipe butt joint temporary spot welding jig according to claim 1, characterized in that, The preload adjustment mechanism (2) includes a fixed plate (201) and a docking plate (202). The fixed plate (201) is fixedly installed on the outer wall of the locking plate (102). A cylinder (203) is fixedly installed on the outer wall of the locking plate (102). A plug-in block (204) is fixedly installed on the telescopic end of the cylinder (203). The docking plate (202) is fixedly installed between the outer walls of the two locking bars (103). A docking block (205) is fixedly installed on one side of the outer wall of the docking plate (202). A plug-in groove (206) is opened on one side of the outer wall of the docking block (205).

3. A pipe butt joint temporary spot welding jig according to claim 2, wherein A support plate (3) is fixedly installed on one side of the outer wall of the locking plate (102), and the support plate (3) is fixedly sleeved on the outer surface of the cylinder (203). Multiple reinforcing plates (4) are fixedly installed between the support plate (3) and the outer wall of the locking plate (102).

4. A temporary spot welding fixture for pipe joints according to claim 3, characterized in that, An installation tube (5) is fixedly embedded between the outer walls of the arc plate (101), and a measuring rod (6) is movably embedded inside the installation tube (5). The outer wall of the measuring rod (6) is engraved with a scale (7).

5. A temporary spot welding fixture for pipe joints according to claim 4, characterized in that, A pull plate (8) is fixedly installed at one end of the measuring rod (6).

6. A temporary spot welding fixture for pipe joints according to claim 5, characterized in that, The outer walls of the arc plate (101), the locking plate (102), and the two locking strips (103) are all provided with fixing grooves.