A quenching device for processing oxidation-resistant and high-conductivity copper alloys
The quenching device driven by a spiral heating rod and a rotary motor solves the problems of uneven heating and cooling in existing devices, achieving uniform quenching of copper alloy workpieces and improving quenching quality and performance stability.
Patent Information
- Application Number
- CN202522372186.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-08
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-08
AI Technical Summary
Existing quenching equipment cannot achieve simultaneous quenching of multiple products, resulting in uneven heating, difficulty in loading and unloading materials, and inability to adjust the quenching depth, leading to high processing costs and unstable quenching quality.
A spiral heating rod is used in conjunction with a rotary motor and a reducer. The copper alloy workpiece is clamped by a cylinder jaw to achieve uniform heating and cooling in the quenching tank. The position of the workpiece is stabilized by a limit seat and a limit rod to ensure temperature consistency and uniformity.
It achieves uniform heating and cooling of copper alloy workpieces, reduces defects such as hardness differences, dimensional deformation and cracks, improves quenching quality and performance stability, and reduces processing costs.
Smart Images

Figure CN224981646U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of quenching equipment, specifically a quenching equipment for processing oxidation-resistant high-conductivity copper alloys. Background Technology
[0002] Beryllium copper is a supersaturated solid solution copper-based alloy, a non-ferrous alloy that combines excellent mechanical, physical, chemical, and corrosion resistance properties. After solution and aging treatment, it possesses high strength limit, elastic limit, yield limit, and fatigue limit comparable to special steels, while also exhibiting high electrical and thermal conductivity, high hardness and wear resistance, high creep resistance, and corrosion resistance. During processing, beryllium copper alloys require quenching equipment to improve their quality. However, existing quenching equipment has a limited workload and cannot simultaneously quench multiple batches of products, thus extending the overall quenching cycle and increasing processing costs. Furthermore, existing technologies also suffer from difficulties in loading and unloading materials and the inability to independently adjust the quenching depth. To address the aforementioned issues, a search revealed Chinese patent CN220012715U, which discloses a quenching apparatus for preparing and processing beryllium copper alloy. The apparatus includes a quenching box with an opening at the top, a concave frame horizontally mounted across the middle of the top of the quenching box, and multiple storage units slidably mounted on the concave frame. The storage units are used to store and quench the beryllium copper alloy. Cooling units are symmetrically mounted on both sides of the quenching box to cool the coolant inside the quenching box. Although the above-mentioned device can continuously cool the quenching liquid in the quenching box and ensure its good quenching state, in actual use, the high temperature generated by the heating device cannot uniformly heat the alloy parts during the quenching operation. There are problems of local overheating or underheating of the alloy parts, and the temperature consistency of the copper alloy workpiece during the heating stage cannot be guaranteed. Utility Model Content
[0003] The purpose of this invention is to provide a quenching device for processing high-conductivity, oxidation-resistant copper alloys, in order to solve the problems mentioned in the background art.
[0004] To achieve the above objectives, a quenching device for processing oxidation-resistant and high-conductivity copper alloys is provided, including a quenching pool, a quenching mechanism installed on the quenching pool, and a copper alloy workpiece disposed inside the quenching mechanism. The quenching mechanism includes a core frame fixed on the quenching pool, and a mounting seat fixed on the core frame. A transmission seat is provided on one side of the core frame, and a cylinder clamp is provided on the transmission seat. The copper alloy workpiece is clamped and fixed on the cylinder clamp.
[0005] Furthermore, a speed reducer is also installed on the core frame, and the output shaft of the speed reducer is fixed to the transmission seat through the core frame via a bearing. At the same time, the input shaft of the speed reducer is fixed to the output shaft of the rotary motor.
[0006] Furthermore, the transmission seat is L-shaped, and a drive motor is provided at the bottom of the transmission seat. The output shaft end of the drive motor is connected to a cylinder gripper; the copper alloy workpiece is driven to rotate axially by the drive motor.
[0007] Furthermore, the bottom of the cylinder gripper is provided with multiple sets of sliders at equal intervals, and the surface of the transmission seat is provided with an annular slide rail. The slide rail is adapted to the size of the slider, and the slider is slidably disposed inside the slide rail.
[0008] Furthermore, the quenching mechanism also includes a heating rod, which is spiral in shape, with a copper alloy workpiece inserted through the middle of the heating rod, and a fixing seat provided at the end of the heating rod.
[0009] Furthermore, a limiting seat is provided on one side of the fixed seat, and two sets of limiting rods are inserted inside the limiting seat. The bottom of the limiting rod is provided with a mounting seat, and the two sets of limiting rods are provided with support plates.
[0010] Furthermore, the support plate supports the limiting seats sleeved on the two sets of limiting rods, and the two sets of limiting rods are distributed in parallel.
[0011] Compared with the prior art, the beneficial effects of this utility model are: 1. This solution utilizes a slow axial rotation in conjunction with a spiral heating rod to ensure that the high temperature generated by the heating rod can be applied evenly and comprehensively to the entire surface of the copper alloy workpiece, forming a uniform annular heating effect. This effectively avoids the problem of local overheating or underheating of the copper alloy workpiece, ensuring temperature consistency during the heating stage. This lays a good foundation for uniform cooling during subsequent quenching, further reducing defects such as hardness differences, dimensional deformation, and cracks caused by uneven temperature, and improving the quenching quality and performance stability of the copper alloy workpiece.
[0012] 2. This solution is started by a rotary motor installed on the core frame. Its output shaft drives the input shaft of the reducer to rotate, which in turn drives the transmission seat to rotate. The drive motor installed at the bottom of the transmission seat moves together with the transmission seat. When the copper alloy workpiece moves with the transmission seat into the quenching water in the quenching pool, the high-temperature copper alloy workpiece is submerged in the water, ensuring that all parts of the copper alloy workpiece can be evenly contacted with the quenching medium and achieve uniform cooling. Attached Figure Description
[0013] Figure 1 This is a three-dimensional structural diagram of the present invention; Figure 2 This is a three-dimensional structural diagram of the quenching mechanism of this utility model; Figure 3 This is a bottom view of the quenching mechanism of this utility model. Figure 4 This is a top view of the quenching mechanism of this utility model. Figure 5 This is a cross-sectional view of the heating rod and its installation structure according to the present invention.
[0014] The following numbers are labeled in the diagram: 100, quenching pool; 200, quenching mechanism; 20, heating rod; 21, fixed seat; 22, limit seat; 23, limit rod; 231, support plate; 24, mounting seat; 25, core frame; 26, rotary motor; 27, reducer; 28, transmission seat; 29, drive motor; 291, cylinder gripper; 2911, slider; 2912, slide rail; 300, copper alloy workpiece. Detailed Implementation
[0015] Please see Figure 1-5 This utility model provides a quenching device for processing high-conductivity, oxidation-resistant copper alloys, including a quenching pool 100, a quenching mechanism 200 installed on the quenching pool 100, and a copper alloy workpiece 300 disposed inside the quenching mechanism 200. The quenching mechanism 200 includes a core frame 25 fixed on the quenching pool 100, and a mounting seat 24 fixed on the core frame 25. A transmission seat 28 is provided on one side of the core frame 25, and a cylinder gripper 291 is provided on the transmission seat 28. The copper alloy workpiece 300 is clamped and fixed on the cylinder gripper 291.
[0016] In a preferred embodiment, a reducer 27 is also installed on the core frame 25, and the output shaft of the reducer 27 is fixed to the transmission seat 28 by passing through the core frame 25 through a bearing. At the same time, the input shaft of the reducer 27 is fixed to the output shaft of the rotary motor 26.
[0017] The transmission seat 28 is L-shaped, and a drive motor 29 is provided at the bottom of the transmission seat 28. The output shaft end of the drive motor 29 is connected to a cylinder gripper 291; the copper alloy workpiece 300 is driven to rotate axially by the drive motor 29.
[0018] The quenching mechanism 200 also includes a heating rod 20, which is spiral in shape. A copper alloy workpiece 300 is inserted through the middle of the heating rod 20, and a fixing seat 21 is provided at the end of the heating rod 20.
[0019] A limiting seat 22 is provided on one side of the fixed seat 21, and two sets of limiting rods 23 are inserted inside the limiting seat 22. The bottom of the limiting rods 23 is provided with a mounting seat 24, and the two sets of limiting rods 23 are provided with support plates 231.
[0020] The support plate 231 supports the limiting seat 22 sleeved on the two sets of limiting rods 23, and the two sets of limiting rods 23 are distributed in parallel.
[0021] Working principle: First, the copper alloy workpiece 300 is clamped and fixed by the cylinder jaws 291 in the quenching mechanism 200. Specifically, the core frame 25 fixed on the quenching pool 100 provides overall support. The mounting seat 24 fixed on the core frame 25 provides the mounting base for the limiting rod 23. The support plate 231 on the limiting rod 23 supports the limiting seat 22 sleeved on the limiting rod 23. The fixing seat 21 on one side of the limiting seat 22 is used to install the spiral heating rod 20, so that the middle of the heating rod 20 can accurately penetrate the copper alloy workpiece 300. Then, the heating equipment is started, and the copper alloy workpiece 300 inserted inside is heated by the spiral heating rod 20 to meet the temperature conditions required for quenching. After the copper alloy workpiece 300 is heated, it needs to be quenched. At this time, on the one hand, the rotary motor 26 installed on the core frame 25 starts, and its output shaft drives the input shaft of the reducer 27 to rotate, which in turn drives the transmission seat 28 to rotate. The transmission seat 28 is L-shaped, and the drive motor 29 installed at its bottom moves together with the transmission seat 28. At the same time, the quenching pool 100 provides quenching water. When the copper alloy workpiece 300 moves with the transmission seat 28 into the quenching water in the quenching pool 100, the high-temperature copper alloy workpiece 300 is submerged in the water, ensuring that all parts of the copper alloy workpiece 300 can be evenly contacted with the quenching medium to achieve uniform cooling. Throughout the process, the limiting seat 22 and the limiting rod 23 limit and stabilize the positions of the heating rod 20 and the copper alloy workpiece 300 during the heating and quenching stages, ensuring that all components work together. Furthermore, before immersing the high-temperature copper alloy workpiece 300 in water, the heating rod 20 must be detached from the outside of the workpiece to prevent motion interference between the workpiece 300 and the heating rod 20 during operation. The rotational design of the copper alloy workpiece 300 is achieved by rotating the transmission seat 28 through the rotary motor 26 and the reducer 27. This allows the copper alloy workpiece 300 to be in uniform contact with the quenching medium during the quenching process, effectively avoiding uneven cooling caused by the inability to rotate, and reducing defects such as uneven hardness, dimensional deformation, and cracks. The spiral heating rod 20 can uniformly heat the copper alloy workpiece 300. With the limiting support of the limiting seat 22 and the limiting rod 23, the quenching quality is further guaranteed, and the performance stability and pass rate of the copper alloy workpiece 300 are improved.
[0022] In a preferred embodiment, the cylinder gripper 291 has multiple sets of sliders 2911 equidistantly arranged at the bottom, and the surface of the transmission seat 28 is provided with an annular slide rail 2912. The slide rail 2912 is adapted to the size of the sliders 2911, and the sliders 2911 are slidably arranged inside the slide rail 2912.
[0023] When the drive motor 29 starts, the cylinder jaw 291 connected to the end of its output shaft drives the copper alloy workpiece 300 to rotate slowly in the axial direction, so that the high temperature generated by the heating rod 20 can uniformly heat the copper alloy workpiece 300 in a ring.
[0024] like Figures 1-5 As shown: Multiple sets of sliders 2911 equidistantly arranged at the bottom of the cylinder gripper 291 are size-matched and slidably engaged with the annular slide rail 2912 on the surface of the transmission seat 28. This provides stable support for the cylinder gripper 291, preventing it from shifting or wobbling when rotating the copper alloy workpiece 300, ensuring the smoothness of the rotation process. The sliding connection also reduces motion resistance, allowing the drive motor 29 to more smoothly drive the cylinder gripper 291 to slowly rotate the copper alloy workpiece 300 axially. Simultaneously, the slow axial rotation, combined with the spiral heating rod 20, ensures that the high temperature generated by the heating rod 20 can act comprehensively and evenly on the entire surface of the copper alloy workpiece 300, forming a uniform annular heating effect. This effectively avoids the problem of localized overheating or underheating of the copper alloy workpiece 300, ensuring temperature consistency during the heating stage. This lays a good foundation for uniform cooling during subsequent quenching, further reducing defects such as hardness differences, dimensional deformation, and cracks caused by uneven temperature, and improving the quenching quality and performance stability of the copper alloy workpiece 300.
Claims
1. A quenching device for processing of an oxidation-resistant high-conductivity copper alloy, comprising a quenching tank (100), characterized in that: The quenching pool (100) is equipped with a quenching mechanism (200), and the quenching mechanism (200) has a copper alloy workpiece (300) inside. The quenching mechanism (200) includes a core frame (25) fixed on the quenching pool (100), and a mounting seat (24) is fixed on the core frame (25). A transmission seat (28) is provided on one side of the core frame (25), and a cylinder clamp (291) is provided on the transmission seat (28). The copper alloy workpiece (300) is clamped and fixed on the cylinder clamp (291).
2. The quenching device for processing an oxidation-resistant high-conductive copper alloy of claim 1, characterized in that: A speed reducer (27) is also installed on the core frame (25), and the output shaft of the speed reducer (27) is fixed to the transmission seat (28) by passing through the core frame (25) with a bearing. At the same time, the input shaft of the speed reducer (27) is fixed to the output shaft of the rotary motor (26).
3. The quenching device for processing an oxidation-resistant high-conductive copper alloy of claim 2, characterized in that: The transmission seat (28) is L-shaped, and a drive motor (29) is provided at the bottom of the transmission seat (28). The output shaft end of the drive motor (29) is connected to a cylinder gripper (291). The copper alloy workpiece (300) is driven to rotate axially by the drive motor (29).
4. The quenching device for processing an oxidation-resistant high-conductive copper alloy of claim 3, characterized in that: The cylinder gripper (291) has multiple sets of sliders (2911) at equal intervals at its bottom. The surface of the transmission seat (28) is provided with an annular slide rail (2912). The slide rail (2912) is adapted to the size of the slider (2911), and the slider (2911) is slidably disposed inside the slide rail (2912).
5. The quenching device for processing an oxidation-resistant high-conductivity copper alloy according to claim 1, characterized in that: The quenching mechanism (200) also includes a heating rod (20), which is spiral in shape. A copper alloy workpiece (300) is inserted through the middle of the heating rod (20), and a fixing seat (21) is provided at the end of the heating rod (20).
6. The quenching device for processing an oxidation-resistant high-conductivity copper alloy according to claim 5, characterized in that: The fixed seat (21) is provided with a limiting seat (22) on one side, and two sets of limiting rods (23) are inserted inside the limiting seat (22). The bottom of the limiting rod (23) is provided with a mounting seat (24), and the two sets of limiting rods (23) are provided with support plates (231).
7. The quenching device for processing an oxidation-resistant high-conductive copper alloy of claim 6, wherein the quenching device is characterized by: The support plate (231) supports the limiting seat (22) sleeved on the two sets of limiting rods (23), and the two sets of limiting rods (23) are distributed in parallel.
Citation Information
Patent Citations
Quenching device for beryllium copper alloy preparation and processing
CN220012715U