A nested resistance indirect heating evaporation structure
By using a nested resistance indirect heating structure and a U-shaped evaporation boat design, the problem of metal film splashing caused by direct heating evaporation is solved, improving the uniformity and smoothness of the coated workpiece and extending the service life of the equipment.
Patent Information
- Application Number
- CN202522277403.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-28
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-10-28
AI Technical Summary
In existing technologies, direct heating evaporation causes the temperature of the metal film material to rapidly exceed the boiling point under vacuum, forming metal vapor bubbles and causing splashing, which affects the uniformity and smoothness of the coated workpiece, especially in high-precision optical coating and electronic device coating.
The system employs a nested resistance indirect heating structure, which indirectly heats the ceramic evaporation boat via a heater. The ceramic evaporation boat then heats the metal film material, preventing the current from directly affecting the metal film material. Combined with the U-shaped evaporation boat and shield design, it prevents metal vapor from entering the gaps and forms a sealed shield to prevent short circuits.
It effectively avoids the splashing of metal film, improves the film quality of coated workpieces, and enhances the service life and safety of the equipment.
Smart Images

Figure CN224981693U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of vacuum coating equipment technology, and in particular to a nested resistance indirect heating evaporation structure. Background Technology
[0002] In the field of vacuum coating, resistance evaporation is a commonly used coating technology. Its core principle is to heat the metal film material with a heater, causing the metal film material to melt and evaporate in a vacuum environment, and the vapor is deposited on the surface of the workpiece to form a film layer. At present, the mainstream resistance evaporation method is "direct heating evaporation", which uses a cBN (conductive boron nitride) evaporation boat as a carrier. The current is directly applied to the evaporation boat, and the metal film material is placed directly on the surface of the evaporation boat. Melting and evaporation are achieved through the heat conduction of the evaporation boat and the self-heating of the conductive metal film material.
[0003] While the aforementioned direct heating method boasts high evaporation efficiency, it suffers from significant drawbacks: Because the current directly acts on the metal film, the film itself generates a self-heating effect, causing the local or overall temperature of the molten metal film to rapidly exceed its boiling point under the current vacuum level. At this point, a large number of metal vapor bubbles spontaneously form inside the molten metal. The intense electromagnetic stirring generated by the eddies during evaporation further promotes the rapid expansion, bursting, and upward ejection of these bubbles, forming particulate "splatter." This splattering phenomenon leads to defects such as impurities and pinholes on the surface of the coated workpiece, severely damaging the uniformity and smoothness of the film surface and reducing product yield. This impact is particularly pronounced in high-precision optical coatings and electronic device coatings. Utility Model Content
[0004] To address the aforementioned problems, this invention provides a nested resistance indirect heating evaporation structure, which solves the problem of metal film evaporation splashing and improves film surface quality.
[0005] To solve the above-mentioned technical problems, the technical solution adopted by this utility model is: a nested resistance indirect heating evaporation structure, including a negative electrode post, a negative electrode side shield, a U-shaped evaporation boat, a heater, a positive electrode shield, a positive electrode post, and a wire feeding tube. The negative electrode post and the positive electrode post are disposed on both sides of the U-shaped evaporation boat. The U-shaped evaporation boat has a through heater mounting hole in the middle, an evaporation groove at the top, and anti-plating steps extending outward on both sides. The heater is nested in the heater mounting hole, and both ends of the heater are electrically connected to the negative electrode post and the positive electrode post, respectively. The negative electrode side shield is connected to the anti-plating step on one side of the U-shaped evaporation boat, and the positive electrode shield is connected to the anti-plating step on the other side of the U-shaped evaporation boat. The output end of the wire feeding tube is disposed corresponding to the evaporation groove.
[0006] Furthermore, both the negative electrode shield and the positive electrode shield are sheet-like structures. The edges of the sheet-like structures are embedded in the anti-plating step (8), completely covering the side gaps of the U-shaped evaporation boat and the heater, preventing metal vapor from entering the gaps and condensing, which would cause a short circuit.
[0007] Furthermore, the evaporation boat is integrally sintered from insulating high-temperature resistant ceramics (such as alumina ceramics, boron nitride ceramics, etc.), and has an overall "U-shaped" structure.
[0008] Furthermore, the heater is made of high-temperature heating materials such as tungsten and graphite.
[0009] Furthermore, the heater mounting hole is a rectangular hole with a size that matches the heater. The back of the evaporation tank (7) is in contact with the heater (4), and the other three sides have a 1mm gap as a gap for thermal expansion and contraction of the material. After the heater is nested and installed, it is in close contact with the back of the evaporation tank (7) to achieve efficient heat conduction. At the same time, the reserved gap can prevent cracking caused by the heater and the evaporation tank being squeezed against each other during heating or cooling due to the different expansion coefficients of the heater and the evaporation tank.
[0010] Furthermore, the evaporation tank is a rectangular tank with a depth of 1-5 mm and a width of 25-30 mm.
[0011] Furthermore, the wire feeding tube is a stainless steel tube, with one end connected to an external wire feeding device and the other end extending 20-60mm above the evaporation tank, used to feed the filamentous metal film into the evaporation tank, ensuring that the filamentous metal film is accurately and smoothly fed into the evaporation tank.
[0012] As can be seen from the above description of the structure of this utility model, compared with the prior art, this utility model has the following advantages:
[0013] 1. This utility model adopts an indirect heating path of "heater → evaporation boat → metal film material". The ceramic insulating material is used as the evaporation boat. The current only acts on the heater itself. The heated heater indirectly heats the ceramic evaporation boat, and the ceramic evaporation boat then heats the metal film material. This avoids the current directly acting on the metal film material and avoids the generation of bubbles and splashing.
[0014] 2. The U-shaped structure of the U-shaped evaporation boat can maintain structural stability during high-temperature heating, and can withstand high temperatures for a long time without deformation. The heating surface is in close contact with the heater, achieving good heat transfer effect.
[0015] 3. The two sides of the U-shaped evaporator are equipped with shields and anti-plating steps to form a sealed barrier, which can prevent metal vapor from drifting into the gap between the evaporator and the heater, avoid short circuit failure caused by condensed metal, improve service life, and ensure high safety. Attached Figure Description
[0016] The accompanying drawings, which form part of this application, are used to provide a further understanding of the present invention. The illustrative embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an undue limitation of the present invention. In the drawings:
[0017] Figure 1 This is a schematic diagram of the overall structure of this utility model;
[0018] Figure 2 This is a schematic diagram of the U-shaped evaporation boat structure of this utility model. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this utility model clearer, the present utility model will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present utility model and are not intended to limit the present utility model.
[0020] Example
[0021] refer to Figure 1 , Figure 2 A nested resistance indirect heating evaporation structure includes a negative electrode post 1, a negative electrode side shield 2, a U-shaped evaporation boat 3, a heater 4, a positive electrode shield 5, a positive electrode post 6, and a wire feeding tube 10. The negative electrode post 1 and the positive electrode post 6 are disposed on both sides of the U-shaped evaporation boat 3. The U-shaped evaporation boat 3 is integrally sintered from insulating high-temperature resistant ceramic (such as alumina ceramic, boron nitride ceramic, etc.) and has an overall U-shaped structure. The U-shaped evaporation boat 3 has a through heater mounting hole 9 in the middle and an evaporation groove 7 at the top. The two sides extend outward to form anti-plating steps 8. The material of the heater 4 is a high-temperature heating material such as tungsten or graphite. The heater 4 is nested in the heater mounting hole 9, and the two ends of the heater 4 are electrically connected to the negative electrode post 1 and the positive electrode post 6, respectively. The negative electrode side shield 2 is connected to the anti-plating step 8 on one side of the U-shaped evaporation boat 3, and the positive electrode shield 5 is connected to the anti-plating step 8 on the other side of the U-shaped evaporation boat 3. The output end of the wire feeding tube 10 is set corresponding to the evaporation tank 7.
[0022] Both the negative electrode shield 2 and the positive electrode shield 5 are sheet-like structures. The edges of the sheet-like structures are embedded in the anti-plating step (8) to completely cover the side gaps of the U-shaped evaporation boat 3 and the heater 4, preventing metal vapor from entering the gaps and condensing to cause a short circuit.
[0023] The heater mounting hole 9 is a rectangular hole with a size that matches the heater 4. The back of the evaporation tank (7) is in contact with the heater (4), and the other three sides have a 1mm gap as a gap for thermal expansion and contraction of the material. After the heater is nested and installed, it is in close contact with the back of the evaporation tank (7) to achieve efficient heat conduction. At the same time, the reserved gap can prevent the heater and the evaporation tank from being squeezed together during heating or cooling due to the different expansion coefficients of the heater and the evaporation tank.
[0024] The evaporation tank 7 is a rectangular tank with a depth of 3 mm and a width of 25 mm.
[0025] The wire feeding tube 10 is a stainless steel tube. One end of the wire feeding tube 10 is connected to an external wire feeding device, and the other end extends to 50mm above the evaporation tank 7. It is used to feed the filamentous metal film 11 into the evaporation tank 7, ensuring that the filamentous metal film 11 is accurately and smoothly fed into the evaporation tank 7.
[0026] This invention employs an indirect heating path: heater → evaporator boat → metal film material. The ceramic insulating material serves as the evaporator boat, and the current acts only on the heater itself. The heated heater indirectly heats the ceramic evaporator boat, which in turn heats the metal film material. This avoids direct current action on the metal film material, preventing bubble formation and splashing. The evaporator boat's eccentric structure maintains structural stability during high-temperature heating, allowing it to withstand prolonged high temperatures without deformation. The heating surface is in close contact with the heater, achieving excellent heat transfer. The evaporator boat is equipped with shields and anti-plating steps on both sides, forming a sealed barrier that prevents metal vapor from entering the gap between the evaporator boat and the heater, avoiding short circuits caused by condensed metal, improving service life, and ensuring high safety.
[0027] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A nested resistance indirectly heated evaporation structure characterized by: The device includes a negative electrode post (1), a negative electrode side shield (2), a loop-shaped evaporator (3), a heater (4), a positive electrode shield (5), a positive electrode post (6), and a wire feed tube (10). The negative electrode post (1) and the positive electrode post (6) are located on both sides of the loop-shaped evaporator (3). The loop-shaped evaporator (3) has a through heater mounting hole (9) in the middle and an evaporation tank (7) at the top. The two sides extend outward to form anti-plating steps (8). The heater (4) is nested in the heater mounting hole (9), and the two ends of the heater (4) are electrically connected to the negative electrode post (1) and the positive electrode post (6), respectively. The negative electrode side shield (2) is connected to the anti-plating step (8) on one side of the loop-shaped evaporator (3), and the positive electrode shield (5) is connected to the anti-plating step (8) on the other side of the loop-shaped evaporator (3). The output end of the wire feed tube (10) is set corresponding to the evaporation tank (7).
2. The nested resistance indirect heated evaporation structure of claim 1, wherein: Both the negative electrode shield (2) and the positive electrode shield (5) are sheet-like structures, and the edges of the sheet-like structures are embedded in the anti-plating step (8).
3. The nested resistance indirect heated evaporation structure of claim 1, wherein: The circular evaporation boat (3) is integrally sintered from insulating high-temperature resistant ceramic and has an overall "circular" structure.
4. The nested resistance indirect heated evaporation structure of claim 1, wherein: The heater (4) is made of high-temperature heating materials such as tungsten and graphite.
5. The nested resistive indirect heating evaporation structure of claim 1, wherein: The heater mounting hole (9) is a rectangular hole with a size that matches the heater (4). The back of the evaporation tank (7) is in contact with the heater (4), and there is a 1mm gap on the other three sides.
6. The nested resistive indirect heating evaporation structure of claim 1, wherein: The evaporation tank (7) is a rectangular tank with a depth of 1-5 mm and a width of 25-30 mm.
7. The nested resistance indirect heating evaporation structure according to claim 1, characterized in that: The wire feeding tube (10) is a stainless steel tube. One end of the wire feeding tube (10) is connected to an external wire feeding device, and the other end extends to 20-60mm above the evaporation tank (7).