A physical vapor deposition chamber
By placing the RF coil between the lower liner and the sidewall in the physical vapor deposition chamber and using the lower liner to shield sputtered particles, the problem of easy damage to the RF coil was solved, the uniformity of the thin film and the processing stability were improved, and the production cost was reduced.
Patent Information
- Application Number
- CN202522392802.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-11
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-11
AI Technical Summary
In semiconductor manufacturing, the magnetron sputtering process in physical vapor deposition leads to unstable conductive structure performance, and the radio frequency coil is easily damaged and needs to be replaced frequently, increasing production costs.
A physical vapor deposition chamber is designed, in which an RF coil is placed between a lower liner and a sidewall. The lower liner is used to shield sputtered particles, and the target structure extends into the upper liner to improve film uniformity. The target is fixed by the sidewall, reducing the frequency of maintenance and replacement of the RF coil.
It improves the uniformity of thin film deposition and the stability of anti-sputtering effect, reduces the maintenance and replacement costs of RF coils, and improves production efficiency and processing stability.
Smart Images

Figure CN224981697U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor manufacturing equipment technology, and more particularly to a physical vapor deposition chamber. Background Technology
[0002] In semiconductor manufacturing, magnetron sputtering in physical vapor deposition (PVD) is a commonly used thin film formation process.
[0003] When forming a conductive structure in a semiconductor structure, a via structure can be formed at the corresponding location in the semiconductor structure, and then copper can be filled into the via structure to form a conductive structure. In order to improve the adhesion between copper and the via structure medium, a barrier layer can be deposited in the via structure using PVD, and then the barrier layer formed on the bottom surface of the via structure can be back-sputtered onto the sidewall of the via structure to reduce the contact resistance of the conductive structure.
[0004] During the formation of the conductive structure, the anti-sputtering effect is affected by the radio frequency coil, resulting in unstable performance of the final conductive structure. Utility Model Content
[0005] To address the aforementioned issues, this application provides a physical vapor deposition chamber that can improve the uniformity of thin film formation during the deposition process, reduce RF output power, and prevent sputtering particles from depositing on the RF coil, thereby reducing the number of RF coil replacements and lowering production costs.
[0006] To achieve the above objectives, embodiments of this application provide a physical vapor deposition chamber, comprising: a sidewall enclosing a process cavity; a first liner including an upper liner and a lower liner, the lower liner being connected to the sidewall and disposed within the process cavity, the lower liner having a first opening extending through its own thickness direction, the upper liner being fixed within the process cavity via the lower liner, the opening of the upper liner extending into the lower liner; a radio frequency coil disposed between the lower liner and the sidewall; and a target material located at the top of the process cavity, connected to the sidewall, with at least a portion of the target material extending into the upper liner.
[0007] In one alternative implementation, the device further includes: a coil support, a conductive element, and a power supply element; the power supply element passes through the sidewall and extends into the process cavity; one end of the conductive element is connected to the power supply element, and the other end is connected to the RF coil; the coil support is located between the lower inner liner and the sidewall, the coil support is connected to the sidewall, the RF coil is connected to the coil support, and the other end of the RF coil is grounded through the coil support and the sidewall.
[0008] In one alternative implementation, a first receiving groove is formed on the sidewall surface facing the lower liner; the coil support includes an insulating support, an upper metal ring, and a lower metal ring; the lower metal ring is disposed on the bottom surface of the first receiving groove and grounded through the bottom surface of the first receiving groove; the insulating support is connected between the upper metal ring and the lower metal ring, and a first snap-fit portion is provided on the surface of the insulating support facing the lower liner, the number of first snap-fit portions being the same as the number of turns of the RF coil; each turn of the RF coil is snapped into one first snap-fit portion, one end of the RF coil is electrically connected to the lower metal ring, and the other end extends through the upper metal ring toward the feeder.
[0009] In one alternative implementation, there are multiple insulating posts, each of which is detachably connected to an upper metal ring and a lower metal ring by bolts.
[0010] In one alternative implementation, the upper metal ring includes a first end and a second end disposed along the circumferential direction, with a gap between the first end and the second end along the circumferential direction of the upper metal ring; the coil support also includes an insulating fastener, the two ends of which are respectively connected to the first end and the second end, and the insulating fastener is provided with a through hole; the radio frequency coil passes through the through hole and is connected to the conductive element.
[0011] In one alternative implementation, the upper metal ring and / or the lower metal ring are provided with a second snap-fit portion; the first receiving groove is provided with a third snap-fit portion corresponding to the second snap-fit portion; the second snap-fit portion and the third snap-fit portion snap-fit together; the lower metal ring is detachably connected to the bottom surface of the first receiving groove by bolts.
[0012] In one alternative implementation, a second inner liner is further included, which surrounds the lower inner liner and is located between the radio frequency coil and the lower inner liner.
[0013] In one alternative implementation, the material of the second liner includes an insulating material.
[0014] In one alternative implementation, the second liner is made of a conductive material; the second liner has a second opening extending through its own thickness.
[0015] In one alternative implementation, the second opening is offset from the first opening.
[0016] In one alternative implementation, the device further includes a third liner, which surrounds the RF coil and is located between the RF coil and the sidewall; the third liner is made of an insulating material.
[0017] In one alternative implementation, a second receiving groove is formed on the sidewall surface facing the lower liner; the opening of the lower liner facing the upper liner has a bent portion formed by bending towards the sidewall, the bent portion being connected to the bottom surface of the second receiving groove; the physical vapor deposition chamber further includes a support member disposed on the side of the bent portion away from the bottom surface of the second receiving groove; the upper liner is connected to the support member.
[0018] In one alternative implementation, the support is made of an insulating material.
[0019] In the physical vapor deposition chamber provided in this application embodiment, dividing the first liner into an upper liner and a lower liner facilitates fabrication and connection to the sidewalls. The target material can be fixed via the sidewalls. Extending a portion of the target material into the upper liner allows it to attract ions from the plasma to bombard it, thereby sputtering additional target particles. Furthermore, the target material extending into the upper liner is closer to the workpiece, allowing the sputtered particles to more efficiently cover the edge areas of the workpiece, thus achieving uniform film deposition. Simultaneously, in the physical vapor deposition chamber provided in this application embodiment, the radio frequency (RF) coil is positioned between the lower liner and the sidewall. During sputtering deposition, the lower liner can shield the sputtered particles within the process chamber, preventing them from falling onto the RF coil and protecting it. This effectively reduces the frequency of RF coil maintenance and replacement, lowers production costs, and avoids downtime in the physical vapor deposition chamber due to RF coil replacement, thereby improving production efficiency. Compared to placing the RF coil on the outside of the sidewall, placing it between the lower liner and the sidewall reduces the RF output power during operation, facilitating process debugging. Furthermore, placing the RF coil between the lower liner and the sidewall allows for shielding against external electromagnetic fields, improving the coil's operational stability. This, in turn, enables better sputtering of the thin film at the bottom of the conductive holes in the workpiece onto the sidewall, enhancing the stability of the anti-sputtering effect. Attached Figure Description
[0020] To more clearly illustrate the technical solution of this application, the drawings used in the embodiments will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0021] Figure 1 This is a schematic diagram of a semiconductor structure; Figure 2 yes Figure 1 A schematic diagram of the formation process of the conductive structure of the semiconductor structure shown in the figure; Figure 3 yes Figure 1A schematic diagram of another formation process of the conductive structure of the semiconductor structure shown in the figure; Figure 4 This is a schematic diagram of an in-situ etching process; Figure 5 This is a schematic diagram of the structure after in-situ etching; Figure 6 This is a schematic diagram of a PVD device. Figure 7 This is a schematic diagram of another type of PVD equipment; Figure 8 This is a schematic diagram of the structure of a physical vapor deposition chamber provided in an embodiment of this application; Figure 9 yes Figure 8 A magnified structural diagram of part A in the diagram; Figure 10 This is a schematic diagram of another physical vapor deposition chamber provided in an embodiment of this application; Figure 11 yes Figure 10 A magnified structural diagram of part B in the diagram; Figure 12 yes Figure 10 A schematic diagram of the enlarged structure of part C in the diagram; Figure 13 This is a schematic diagram of the structure of a coil support provided in an embodiment of this application; Figure 14 This is an exploded view of a portion of the structure of a coil support provided in an embodiment of this application.
[0022] Illustration markings: 1-Semiconductor structure; 10-Semiconductor device; 20-Conductive structure; 20a-Conductive hole; 20b-Copper seed layer; 30-Barrier layer; 100 - PVD equipment; 110 - Outer wall of the cavity; 120 - Base; 130 - Deposition target; 140 - Metal liner; 150 - Shielding component; 160 - Support ring; 171 - Upper outer cover; 1711 - Magnetron cavity; 172 - Magnetron tube; 173 - Motor; 181 - RF coil; 182 - Second power supply; 190 - First power supply; 200 - Physical vapor deposition chamber; 210 - Side wall; 211 - Process chamber; 212 - First receiving tank; 213 - Second receiving tank; 214 - Annular stage; 220 - First liner; 221 - Upper liner; 222 - Lower liner; 2221 - Bending section; 230 - RF coil; 240 - Target material; 250 - Support; 261 - Second liner; 262 - Third liner; 271 - Conductive component; 272 - Feed component; 273 - RF matching Components: 280-Coil bracket; 281-Insulating support; 2811-First snap-fit part; 282-Upper metal ring; 2821-First end; 2822-Second end; 283-Lower metal ring; 284-Insulating fastener; 2841-Through hole; 285-Second snap-fit part; 291-Magnetic control base; 292-RF power supply; 293-Shielding ring; 294-Insulating cover; 2941-Magnetic control cavity; 295-Magnetic control device; 296-Rotating motor. Detailed Implementation
[0023] The technical solutions of the embodiments of this application will be clearly described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this application. Other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are all within the protection scope of this application.
[0024] In the following description, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first," "second," etc., may explicitly or implicitly include one or more of that feature. In the description of this application, unless otherwise stated, "a plurality of" means two or more.
[0025] Furthermore, in this application, directional terms such as "upper," "lower," "inner," and "outer" are defined relative to the indicated placement of the components in the accompanying drawings. It should be understood that these directional terms are relative concepts, used for relative description and clarification, and can change accordingly depending on the placement of the components in the accompanying drawings.
[0026] In the field of semiconductor manufacturing, in order to achieve electrical connections within a semiconductor structure, conductive structures are typically placed within the semiconductor structure. These conductive structures enable conductive connections between different semiconductor devices (such as transistors), thereby facilitating the transmission and power supply of electrical signals between the various semiconductor devices and realizing the logic functions of the semiconductor structure.
[0027] Figure 1 This is a schematic diagram of a semiconductor structure.
[0028] like Figure 1 As shown, for example, when two semiconductor devices 10 that need to be electrically connected in semiconductor structure 1 are located in different layers, a conductive structure 20 can be provided between the two semiconductor devices 10, thereby enabling the electrical connection between the two semiconductor devices 10.
[0029] Figure 2 yes Figure 1 A schematic diagram of the formation process of the conductive structure of the semiconductor structure shown.
[0030] like Figure 2 As shown in (a), before forming the conductive structure 20, a conductive hole 20a can be provided at the position of the semiconductor device 10 on the wafer.
[0031] like Figure 2 As shown in (b), after forming the conductive hole 20a, conductive material can be filled into the conductive hole 20a to fill the conductive hole 20a, thereby forming a conductive structure 20.
[0032] For example, the conductive material can be a conductive single metal material or alloy material such as aluminum or copper.
[0033] like Figure 2 As shown in (c), after forming the conductive structure 20, another semiconductor device 10 can be disposed on the surface of the conductive structure 20, and a protective layer can be formed on the outer periphery of the semiconductor device 10 to form as shown in (c). Figure 1 Semiconductor structure 1 is shown.
[0034] For example, semiconductor device 10 may be a transistor, but this is not limited in this embodiment.
[0035] As the size of semiconductor structures 1 (such as chips) becomes smaller and smaller, the reliability issues caused by RC delay and electromigration of the conductive structures 20 in semiconductor structures 1 have become major problems affecting circuit speed. To solve this problem, copper conductive structures 20 have gradually become the mainstream in semiconductor structures 1.
[0036] When forming the copper conductive structure 20, the adhesion between copper and the dielectric is poor, and copper particles easily diffuse into the surrounding silicon or silicon dioxide dielectric, contaminating the semiconductor material and affecting the stability of the semiconductor structure 1. For these two reasons, when forming the copper conductive structure 20, a barrier layer 30 can first be formed on the surface of the conductive hole 20a by magnetron sputtering in physical vapor deposition (PVD), and then the copper conductive structure 20 can be formed.
[0037] Figure 3 yes Figure 1A schematic diagram of another formation process of the conductive structure of the semiconductor structure shown.
[0038] like Figure 3 As shown in (a), for example, a barrier layer 30 can be deposited on the surface of the conductive via 20a by magnetron sputtering before the formation of the conductive structure 20. The barrier layer 30 is relatively dense and can prevent copper particles from diffusing into the dielectric layer. At the same time, the barrier layer 30 has good adhesion, which can provide a good foundation for subsequent copper deposition.
[0039] For example, the barrier layer 30 can be made of tantalum nitride (TaN) or tantalum (Ta).
[0040] like Figure 3 As shown in (b), for example, after forming the barrier layer 30, a copper seed layer 20b can be first formed on the surface of the barrier layer 30 by magnetron sputtering deposition, thereby forming a continuous and dense copper film as an electroplating substrate for subsequently filling the conductive hole 20a.
[0041] like Figure 3 As shown in (c), for example, after forming the copper seed layer 20b, copper can be electroplated into the conductive hole 20a to form a copper conductive structure 20.
[0042] As the aspect ratio of the conductive hole 20a in the semiconductor structure 1 increases, the thin film formed at the bottom of the conductive hole 20a using the PVD process becomes thicker, while the thin film formed on the sidewalls becomes thinner, resulting in an excessively thick barrier layer 30 at the bottom of the conductive hole 20a. Simultaneously, since the resistivity of the barrier layer 30 is higher than that of copper, an excessively thick barrier layer 30 increases the contact resistance between the conductive structure 20 and the semiconductor device 10.
[0043] To reduce the contact resistance between the conductive structure 20 and the semiconductor device 10, in-situ etching can be performed in the sputtering chamber after the barrier layer 30 is deposited to backsputter the barrier layer 30 deposited at the bottom of the conductive hole 20a onto the sidewall, thereby reducing the contact resistance between the conductive structure 20 and the semiconductor device 10 and also improving the step coverage of the thin film on the sidewall of the conductive hole 20a.
[0044] Figure 4 This is a schematic diagram of an in-situ etching process.
[0045] Figure 5 This is a schematic diagram of the structure after in-situ etching.
[0046] Combination Figure 4 and Figure 5As shown, during in-situ etching, etching can be performed in the same PVD chamber after depositing the barrier layer 30, without having to move the semiconductor structure 1 to another location, thus ensuring the cleanliness and high efficiency of the semiconductor structure 1.
[0047] For example, a bias voltage can be applied to the substrate 120 supporting the semiconductor structure 1, making the semiconductor structure 1 with the barrier layer 30 formed a "target" to be bombarded. An inert gas (such as argon) is introduced into the chamber to generate plasma. Positively charged argon ions are accelerated by the electric field and bombard the surface of the semiconductor structure 1 vertically, thereby ejecting particles from the bottom of the conductive hole 20a and sputtering them onto the sidewall of the conductive hole 20a.
[0048] Because the barrier layer 30 at the bottom of the conductive hole 20a faces the plasma directly, it receives the most direct vertical bombardment and is therefore etched most severely. In contrast, the barrier layer 30 on the sidewall of the conductive hole 20a receives very weak bombardment and is hardly etched, thus achieving selective etching. In this way, in-situ etching can precisely remove the excessively thick barrier layer 30 at the bottom of the conductive hole 20a, reducing the thickness of the high-resistivity material along the main current path. Simultaneously, the Ta / TaN particles sputtered from the bottom of the conductive hole 20a will redeposit onto the sidewall of the conductive hole 20a, thereby thickening the barrier layer 30 on the upper part of the sidewall, improving the uniformity of sidewall coverage, and better fulfilling its barrier function.
[0049] Figure 6 This is a schematic diagram of a PVD device.
[0050] like Figure 6 As shown, the PVD equipment 100 may include an outer wall 110 of the cavity, a base 120, a deposition target 130, a metal liner 140, a shielding component 150, and a support ring 160.
[0051] For example, the outer wall 110 of the chamber encloses a sputtering chamber. A metal liner 140 is located between a base 120 and a deposition target 130, the base 120 being used to support the workpiece to be processed (such as a wafer). A shielding member 150 is disposed between the metal liner 140 and the base 120 to prevent particles generated during sputtering from sputtering to the bottom of the chamber. A support ring 160 is disposed between the outer wall 110 of the chamber and the deposition target 130 to fix the deposition target 130.
[0052] For example, the PVD device 100 may also include an upper cover 171, a magnetron 172, a motor 173, an RF coil 181, a first power supply 190, and a second power supply 182.
[0053] An outer cover 171 is placed around the deposition target 130 to form a magnetron cavity 1711. A magnetron 172 is disposed inside the magnetron cavity 1711 and connected to a motor 173 above the deposition target 130. The magnetron 172 generates a closed annular magnetic field on the surface of the deposition target 130, increasing the probability of collisions between electrons and argon molecules in the cavity. The cooperation between the magnetron 172 and the motor 173 enables the argon molecules to bombard the deposition target 130, thereby depositing a barrier layer on the surface of the workpiece.
[0054] The first power supply 190 is connected to the base 120, and the second power supply 182 is connected to the radio frequency (RF) coil 181, which is located inside the metal liner 140. Both the first power supply 190 and the second power supply 182 are RF power supplies. Thus, after the barrier layer is deposited, the first power supply 190 can be used to turn the workpiece on the base 120 into a target material. The second power supply 182 and the RF coil 181 can provide an RF magnetic field to the argon molecules to bombard the barrier layer formed at the bottom of the conductive hole of the workpiece, thereby back-sputtering the barrier layer at the bottom of the conductive hole onto the sidewall of the conductive hole.
[0055] like Figure 6 As shown, the RF Coil coil 181 is located inside the metal liner 140. With the consumption of the deposition target 130, a large amount of Ta metal will deposit on the surface of the RF Coil coil 181. Therefore, the RF Coil coil 181 needs to be cleaned periodically to backsputter the Ta film deposited on it onto the metal liner 140 of the chamber. This prevents the Ta film deposited on the RF Coil coil 181 from falling into the chamber, which would increase the number of particles inside the chamber and cause the workpiece to be scrapped. However, cleaning the RF Coil coil 181 will prevent the chamber from performing film deposition, affecting the overall production capacity of the machine. Moreover, the built-in RF Coil coil 181 is a consumable and needs to be replaced when the metal liner 140 in the chamber is replaced. The cost of replacing the RF Coil coil 181 is tens of thousands of RMB, resulting in high operating costs.
[0056] Figure 7 This is a schematic diagram of another type of PVD equipment.
[0057] like Figure 7 As shown, in another PVD apparatus 100, the RF Coil coil 181 can be disposed on the outer periphery of the outer wall 110 of the cavity, in an atmospheric environment. This prevents the deposition of a Ta film on the surface of the RF Coil coil 181 during sputtering, thus eliminating the need for cleaning and replacement of the RF Coil coil 181.
[0058] but, Figure 7 In the PVD device 100 shown, the radio frequency coil 181 is disposed outside the cavity in order to achieve the following Figure 6 To achieve the same anti-sputtering effect as the PVD device 100 shown, it is necessary to increase the RF power of the RF coil 181. For example, Figure 6 When the PVD device 100 shown requires a 1000W RF output, Figure 7 The PVD equipment 100 shown requires 1800W or 2000W, increasing the difficulty of process debugging. Furthermore, the RF coil 181 is located outside the cavity, making it more susceptible to interference from external electromagnetic fields, leading to unstable processing results. In addition, to allow the RF generated by the RF coil 181 to enter the cavity, the outer wall of the cavity encased by the RF coil 181 needs to be made of ceramic. Ceramic components are fragile under load and have high manufacturing costs.
[0059] To address the aforementioned issues, this application provides a physical vapor deposition chamber that protects the RF coil and reduces its maintenance and replacement costs. Furthermore, the physical vapor deposition chamber provided by this application does not require increasing the RF power of the RF coil, is unaffected by external magnetic fields, and exhibits good processing stability. Moreover, the physical vapor deposition chamber provided by this application can improve the uniformity of the film formed during deposition, providing a good foundation for subsequent reverse sputtering and improving processing efficiency.
[0060] Figure 8 This is a schematic diagram of the structure of a physical vapor deposition chamber provided in an embodiment of this application.
[0061] like Figure 8As shown in the figure, a physical vapor deposition chamber 200 provided in this application embodiment includes a sidewall 210, a first liner 220, an RF coil 230, and a target 240. The sidewall 210 encloses a process cavity 211. The first liner 220 includes an upper liner 221 and a lower liner 222. The lower liner 222 is connected to the sidewall 210 and disposed within the process cavity 211. The lower liner 222 has a first opening extending through its thickness direction to form a Faraday cage structure, thereby facilitating the transmission of RF energy. The upper liner 221 is fixed within the process cavity 211 via the lower liner 222. The opening of the upper liner 221 extends into the lower liner 222, thereby preventing plasma from moving to the outside of the first liner 220 within the gap between the upper and lower liners 221 during the deposition sputtering process. The target 240 is located at the top of the process chamber 211 and is connected to the sidewall 210. At least a portion of the target 240 extends into the upper liner 221, thereby improving the uniformity of the deposited film. The RF coil 230 is disposed between the lower liner 222 and the sidewall 210. The lower liner 222 can shield the sputtering particles generated within the process chamber, thus protecting the RF coil 230. Simultaneously, the RF coil 230 is located inside the sidewall 210. During anti-sputtering, the RF coil 230 can output RF energy to generate plasma within the process chamber without requiring excessive RF output power, facilitating process debugging. Furthermore, the sidewall 210 can shield against external electromagnetic fields to prevent interference with the normal operation of the RF coil 230, improving processing stability.
[0062] In the physical vapor deposition chamber 200 provided in this embodiment, dividing the first liner 220 into two structures, an upper liner 221 and a lower liner 222, facilitates processing and shaping, and also facilitates connection with the sidewall 210. The target material 240 can be fixed through the sidewall 210. Extending a portion of the target material 240 into the upper liner 221 can attract ions in the plasma to bombard it, thereby sputtering additional target material 240 particles. Moreover, the target material 240 extending into the upper liner 221 is closer to the workpiece to be processed, and the particles sputtered from the target material 240 can more efficiently cover the edge area of the workpiece to be processed, thereby achieving uniformity of thin film deposition. At the same time, in the physical vapor deposition chamber 200 provided in this embodiment, the radio frequency coil 230 is disposed between the lower liner 222 and the sidewall 210. During sputtering deposition, the lower liner 222 can shield the particles sputtered down in the process chamber, thereby preventing particles from falling onto the radio frequency coil 230 and protecting the radio frequency coil 230. This effectively reduces the frequency of maintenance and replacement of the RF coil 230, lowers production costs, and avoids downtime in the physical vapor deposition chamber 200 due to RF coil 230 replacement, thereby improving production efficiency. Compared to placing the RF coil 230 outside the sidewall 210, placing it between the lower liner 222 and the sidewall 210 also reduces the RF output power of the RF coil 230 during operation, facilitating process debugging. Placing the RF coil 230 between the lower liner 222 and the sidewall 210 also allows the sidewall 210 to shield against external electromagnetic fields, improving the operational stability of the RF coil 230. This allows for better sputtering of the thin film at the bottom of the conductive holes in the workpiece onto the sidewall 210, improving the stability of the anti-sputtering effect.
[0063] As can be seen, in the physical vapor deposition chamber 200 provided in this application embodiment, by extending a portion of the target material 240 into the upper liner 221, the uniformity of the film formed during the deposition process can be improved. Simultaneously, by placing the RF coil 230 between the lower liner 222 and the sidewall 210, the uniformity of the backsputtering can be improved, thus considering uniformity issues from two angles. In this way, before filling the conductive holes with conductive material, a uniformly covered barrier layer on the sidewall 210 with low bottom contact resistance can be achieved, which helps to improve the generation efficiency of the conductive structure and enhance its conductivity.
[0064] In some examples, the workpiece to be processed can be a semiconductor structure such as a wafer, a chip on a wafer, or a chip, but this is not limited in the embodiments of this application.
[0065] In some examples, the sidewall 210 can be made of a conductive material (such as metal) to facilitate grounding of various structures. Furthermore, conductive materials are lighter and stronger overall than insulating materials such as ceramics and quartz.
[0066] It is understood that the physical vapor deposition chamber 200 provided in this application embodiment can not only be used to form conductive structures, but also in the semiconductor fabrication process for forming any thin film and selective etching. In other words, the physical vapor deposition chamber 200 provided in this application embodiment can be used in various sputtering and anti-sputtering process scenarios.
[0067] For example, the physical vapor deposition chamber 200 provided in this application embodiment can be used for sputtering and thin film preparation of various metal materials such as copper Cu, tantalum Ta, tantalum nitride TaN, titanium Ti, titanium nitride TiN, aluminum Al, tungsten W, nickel Ni, cobalt Co.
[0068] In some examples, the radio frequency coil 230 in the physical vapor deposition chamber 200 provided in this application embodiment can be electroplated, sputtered, or vapor-deposited with metal materials (such as Cu, Ag, Au, Ni, Ti, Al, etc.).
[0069] In some examples, the radio frequency coil 230 is placed between the lower inner liner 222 and the side wall 210. The radio frequency applied to the radio frequency coil 230 can be different frequencies such as 400kHz, 2MHz, 13.56MHz, 20MHz, 40MHz, and 60MHz, which can be adjusted according to actual needs.
[0070] like Figure 8 As shown, in some embodiments, to facilitate the placement of the radio frequency coil 230, a first receiving groove 212 is formed on the surface of the side wall 210 facing the lower inner liner 222. In this way, the first receiving groove 212 can be used to accommodate and fix the radio frequency coil 230.
[0071] For example, the first receiving groove 212 may include a groove side wall, a groove bottom surface and a groove top surface, and the radio frequency coil 230 may be located between the groove top surface and the groove bottom surface of the first receiving groove 212.
[0072] For example, the first receiving groove 212 can be formed by a material removal process, such as grinding or milling, on the side surface of the side wall 210 facing the process cavity 211, which is not limited in this embodiment.
[0073] In some embodiments, a second receiving groove 213 is further formed on the surface of the sidewall 210 facing the lower inner liner 222, and the second receiving groove 213 may be located above the first receiving groove 212. In this way, an annular platform 214 can be formed between the first receiving groove 212 and the second receiving groove 213, the upper surface of the annular platform 214 being the bottom surface of the second receiving groove 213, and the lower surface of the annular platform 214 being the top surface of the first receiving groove 212.
[0074] In some embodiments, the opening of the lower inner liner 222 toward the upper inner liner 221 has a bent portion 2221 formed by bending toward the sidewall 210, and the bent portion 2221 is connected to the bottom surface of the second receiving groove 213. In other words, the lower inner liner 222 can be connected to the annular platform 214 through the bent portion 2221, thereby enabling the lower inner liner 222 to be fixed by the annular platform 214.
[0075] In this embodiment, the annular platform 214 formed by the second receiving groove 213 can realize the connection and fixation of the lower inner liner 222, and can also avoid occupying too much space of the process cavity 211, so as to ensure the inner diameter of the upper inner liner 221, thereby increasing the bombardment surface area of the target material 240 and improving the uniformity of film deposition on the workpiece to be processed.
[0076] In some embodiments, the physical vapor deposition chamber 200 further includes a support member 250. The support member 250 may be disposed on the side of the bend 2221 opposite to the bottom surface of the second receiving groove 213, and the upper liner 221 may be connected to the support member 250. In this way, the upper liner 221 can be connected and fixed using the support member 250.
[0077] In some examples, the support member 250 can be made of a conductive material (such as metal). In this way, the upper liner 221 can be grounded through the support member 250 and the side wall 210, thereby improving the thermal conductivity of the upper liner 221 and improving the heat dissipation effect.
[0078] In other examples, the support 250 can be made of an insulating material (such as quartz, ceramic, etc.). In this way, the upper liner 221 can achieve an insulating connection with the sidewall 210, thereby increasing the plasma density inside the upper liner 221 and improving the sputtering effect.
[0079] In this embodiment, the first inner liner 220 is divided into two parts, an upper inner liner 221 and a lower inner liner 222, which not only facilitates processing and molding, but also improves the flexibility of the insulation or conductivity settings of the upper inner liner 221. The material of the support member 250 can be adjusted according to the actual processing needs to determine whether the upper inner liner 221 should be grounded, thereby meeting the process requirements.
[0080] Figure 9 yes Figure 8 A magnified structural diagram of part A in the diagram.
[0081] Combination Figure 8 and Figure 9 As shown, in some embodiments, the physical vapor deposition chamber 200 further includes a second liner 261. The second liner 261 may be disposed around the lower liner 222 and located between the RF coil 230 and the lower liner 222. In this way, the second liner 261 can provide further protection for the RF coil 230.
[0082] In some examples, the second liner 261 can be made of an insulating material, such as ceramic or quartz. In this way, the second liner 261 can not only prevent particles from moving from the first opening of the first liner 220 to the surface of the RF coil 230, but also achieve insulation between the RF coil 230 and the lower liner 222, thereby reducing the probability of arcing between the RF coil 230 and the lower liner 222.
[0083] In other examples, the second liner 261 is made of a conductive material, such as metal. Furthermore, the second liner 261 may have a second opening extending through its thickness. In this way, the second liner 261 can both protect the RF coil 230 and enable the transmission of RF energy.
[0084] For example, the second opening of the second liner 261 can be offset from the first opening of the lower liner 222. In this way, while transmitting radio frequency energy, particles during the sputtering process can be prevented from passing through the first and second openings, thus improving the protection of the radio frequency coil 230.
[0085] In some examples, the first opening on the lower liner 222 can be a circular opening or an elongated opening. The second opening on the second liner 261 can be a circular opening or an elongated opening. The shape and size of the first opening and the second opening can be the same or different, and this application embodiment does not limit this.
[0086] Figure 10 This is a schematic diagram of another physical vapor deposition chamber provided in an embodiment of this application.
[0087] Figure 11 yes Figure 10 A magnified structural diagram of part B in the diagram.
[0088] like Figure 10 and Figure 11 As shown, in some embodiments, the physical vapor deposition chamber 200 further includes a third liner 262. The third liner 262 surrounds the radio frequency coil 230 and is located between the radio frequency coil 230 and the sidewall 210. The third liner 262 is made of an insulating material, such as quartz or ceramic. This allows for insulation between the radio frequency coil 230 and the sidewall 210, thereby reducing the probability of arcing between them. Simultaneously, by using the third liner 262 to insulate between the radio frequency coil 230 and the sidewall 210, the distance between them can be reduced, eliminating the need to increase the distance to reduce the arcing probability. This improves the overall structural compactness of the physical vapor deposition chamber 200, thereby increasing the space utilization of the semiconductor processing.
[0089] Figure 12 yes Figure 10 A magnified structural diagram of part C in the diagram.
[0090] Combination Figure 10 and Figure 12 As shown, in some embodiments, the physical vapor deposition chamber 200 further includes a conductive element 271 and a power supply element 272. The power supply element 272 passes through the sidewall 210 and extends into the process chamber 211. One end of the conductive element 271 is connected to the power supply element 272, and the other end is connected to the radio frequency coil 230. In this way, the radio frequency coil 230 can achieve a power supply connection with the external structure of the process chamber 211 through the conductive element 271 and the power supply element 272.
[0091] For example, the radio frequency coil 230 and the conductive element 271 can be connected by soldering to reduce contact resistance.
[0092] For example, the conductive component 271 and the power supply component 272 can be detachably connected by means of snap-fit, threaded connection, etc., so as to facilitate the installation and disassembly of related components, and facilitate installation and maintenance.
[0093] For example, the power supply element 272 passes through the side wall of the first receiving groove 212. The physical vapor deposition chamber 200 also includes an RF matching unit 273, which is disposed on the outside of the side wall 210 and electrically connected to the power supply element 272, so as to achieve an electrical connection with the RF coil 230 through the power supply element 272, thereby delivering RF energy from the power supply element 272 and the conductive element 271 to the RF coil 230 located in the process chamber 211.
[0094] Figure 13 This is a schematic diagram of the structure of a coil support provided in an embodiment of this application.
[0095] Figure 14 This is an exploded view of a portion of the structure of a coil support provided in an embodiment of this application.
[0096] Combination Figure 10 , Figure 13 and Figure 14 As shown, in some embodiments, the physical vapor deposition chamber 200 further includes a coil support 280. The coil support 280 is located between the lower liner 222 and the sidewall 210, and is connected to the sidewall 210. The RF coil 230 is connected to the coil support 280, thereby fixing the RF coil 230. Simultaneously, the end of the RF coil 230 facing away from the conductive element 271 is grounded through the coil support 280 and the sidewall 210, thus enabling the grounding of the RF coil 230.
[0097] In some examples, the coil support 280 may include an insulating support 281, an upper metal ring 282, and a lower metal ring 283. The lower metal ring 283 is disposed on the bottom surface of the first receiving groove 212 and grounded through the bottom surface of the first receiving groove 212. One end of the RF coil 230 is electrically connected to the lower metal ring 283, thereby achieving grounding. The other end of the RF coil 230 extends through the upper metal ring 282 toward the feed element 272 to achieve a feed connection. Thus, the RF matching unit 273, the feed element 272, the conductive element 271, the RF coil 230, the lower metal ring 283, and the sidewall 210 can form a complete RF circuit.
[0098] For example, the insulating post 281 can be made of ceramic or quartz, etc.
[0099] For example, the insulating support 281 is connected between the upper metal ring 282 and the lower metal ring 283. The surface of the insulating support 281 facing the lower inner liner 222 is provided with first engaging portions 2811, the number of which is the same as the number of turns of the RF coil 230. Thus, each turn of the RF coil 230 is engaged with one first engaging portion 2811, thereby securing each turn of the RF coil 230.
[0100] In some examples, the number of turns of the RF coil 230 can be 1-50 turns, such as 2 turns, 3 turns, 4 turns, 8 turns, 10 turns, 15 turns, 20 turns, 25 turns, 28 turns, 30 turns, 32 turns, 35 turns, 40 turns, 42 turns, 45 turns, 50 turns, etc., which is not limited in this embodiment.
[0101] For example, the number of turns of the radio frequency coil 230 can be 1-6 turns, such as 2 turns, 3 turns, 4 turns, 5 turns, or 6 turns.
[0102] When the number of turns of the radio frequency coil 230 is 4, each insulating post 281 may include four first snap-fit portions 2811.
[0103] In some examples, the spacing between two adjacent turns of the RF coil 230 can be 1 to 100 mm, such as 1 mm, 10 mm, 20 mm, 30 mm, 40 mm, 50 mm, 60 mm, 70 mm, 80 mm, 90 mm, 100 mm, etc.
[0104] For example, the spacing between two adjacent turns of the RF coil 230 can be 10~40mm, such as 12mm, 15mm, 20mm, 25mm, 28mm, 30mm, 35mm, etc. Correspondingly, the spacing between two adjacent first snap-fit portions 2811 on each insulating post 281 is equal to the spacing between two adjacent turns of the RF coil 230, thereby maintaining the shape and spacing of the RF coil 230.
[0105] In some examples, the first latching portion 2811 may be a recessed structure such as a slot or hole, so that the radio frequency coil 230 can be embedded therein.
[0106] For example, the radio frequency coil 230 can be cylindrical, elongated, or other shapes, and is not limited in this embodiment. The shape of the first latching portion 2811 can be adjusted to adapt to the shape of the radio frequency coil 230, and is not limited in this embodiment.
[0107] It should be noted that the number of turns, shape, and spacing between adjacent turns of the RF coil 230 can be adjusted according to actual conditions. This application only provides relevant examples and is not intended as a specific limitation.
[0108] In some embodiments, in order to better maintain the shape of the RF coil 230, the number of insulating supports 281 can be multiple, and the multiple insulating supports 281 can be arranged at equal intervals. In this way, the RF coil 230 can be supported and fixed at multiple positions, resulting in better stability.
[0109] For example, the radio frequency coil 230 can be made of different metals or alloys such as Cu, Al, Ti, and Ni.
[0110] For example, each insulating bracket can be detachably connected to the upper metal ring 282 and the lower metal ring 283 by bolts. This facilitates the installation and replacement of the RF coil 230 and the coil bracket 280, improving installation and maintenance efficiency.
[0111] In some embodiments, the upper metal ring 282 includes a first end 2821 and a second end 2822 disposed along the circumferential direction, and a gap exists between the first end 2821 and the second end 2822 along the circumferential direction of the upper metal ring 282. The coil support 280 further includes an insulating fastener 284, the two ends of which are respectively connected to the first end 2821 and the second end 2822, and the insulating fastener 284 is provided with a through hole 2841. One end of the RF coil 230 connected to the conductive member 271 can pass through the through hole 2841 and be connected to the conductive member 271, thereby enabling the lead-out and fixation of the feed end of the RF coil 230 using the insulating fastener 284.
[0112] In some embodiments, the upper metal ring 282 and / or the lower metal ring 283 are provided with a second snap-fit portion 285.
[0113] In some examples, the upper metal ring 282 is provided with a second locking portion 285, and the groove sidewall of the first receiving groove 212 is provided with a third locking portion corresponding to the second locking portion 285. The second locking portion 285 of the upper metal ring 282 engages with the third locking portion of the first receiving groove 212. In this way, through the cooperation of the second locking portion 285 and the third locking portion, the coil support 280 can be limited in the circumferential direction, thereby preventing the coil support 280 from rotating relative to the first receiving groove 212 and affecting the electrical connection of the RF coil 230.
[0114] In other examples, the lower metal ring 283 is provided with a second locking portion 285, and the bottom surface of the first receiving groove 212 is provided with a third locking portion corresponding to the second locking portion 285. The second locking portion 285 of the lower metal ring 283 engages with the third locking portion of the first receiving groove 212. In this way, through the cooperation of the second locking portion 285 and the third locking portion, the coil support 280 can be limited in the circumferential direction, thereby preventing the coil support 280 from rotating relative to the first receiving groove 212 and affecting the electrical connection of the RF coil 230.
[0115] In some other examples, both the upper metal ring 282 and the lower metal ring 283 are provided with a second locking portion 285, and the groove sidewall of the first receiving groove 212 is provided with a third locking portion corresponding to the upper metal ring 282, and the groove bottom surface of the first receiving groove 212 is provided with a third locking portion corresponding to the second locking portion 285. In this way, through the cooperation of the second locking portion 285 and the third locking portion, the coil support 280 can be limited in the circumferential direction, thereby preventing the coil support 280 from rotating relative to the first receiving groove 212 and affecting the electrical connection of the RF coil 230.
[0116] For example, the second snap-fit portion 285 can be a groove, and the third snap-fit portion can be a protrusion provided with a corresponding groove.
[0117] Alternatively, the second latching part 285 can be a protrusion, and the third latching part can be a groove provided for the corresponding protrusion.
[0118] In this embodiment, the specific shapes of the second snap-fit portion 285 and the third snap-fit portion are not limited.
[0119] In some embodiments, the engagement of the second snap-fit portion 285 and the third snap-fit portion enables pre-positioning between the coil bracket 280 and the first receiving groove 212. To secure the coil bracket 280, the lower metal ring 283 can be detachably connected to the bottom surface of the first receiving groove 212 via bolts. This allows for the fixation of the RF coil 230 during manufacturing and facilitates installation and disassembly, thereby improving installation and maintenance efficiency.
[0120] Please refer to it again. Figure 10In some embodiments, the physical vapor deposition chamber 200 further includes a magnetron base 291, an RF power supply 292, and a shielding ring 293. The magnetron base 291 is disposed opposite to the target 240 and located within the process chamber to support the workpiece to be processed. The shielding ring 293 is disposed between the magnetron base 291 and the lower liner 222 to prevent particles generated during sputtering from falling to the bottom of the process chamber and becoming difficult to clean. The RF power supply 292 is electrically connected to the magnetron base 291, thereby enabling it to cooperate with the RF coil 230 during reverse sputtering to transform the workpiece on the magnetron base 291 into the target 240 for etching the barrier layer or other thin films at the bottom of the conductive holes.
[0121] For example, the radio frequency power supply 292 can apply radio frequency to the magnetron base 291 before, after or during the generation of plasma in the process chamber. In this embodiment of the application, the order of radio frequency generation of the radio frequency coil 230 and the magnetron base 291 is not limited.
[0122] In some examples, the radio frequency applied by the radio frequency power supply 292 to the magnetically controlled base 291 can be different frequencies such as 400kHz, 2MHz, 13.56MHz, 20MHz, 40MHz, and 60MHz.
[0123] In some examples, the radio frequency power applied to the magnetron 291 can be 10-5000W.
[0124] Please refer to it again. Figure 10 In some embodiments, the physical vapor deposition chamber 200 further includes an insulating cover 294, a magnetron sputtering device 295, and a rotary motor 296. The insulating cover 294 is disposed on the outside of the target 240 away from the process chamber, forming a magnetron sputtering cavity 2941. The magnetron sputtering device 295 is connected to the insulating cover 294 and disposed within the magnetron sputtering cavity 2941. The rotary motor 296 is connected to the magnetron sputtering device 295 and is located outside the magnetron sputtering cavity 2941. Thus, the rotary motor 296 can drive the magnetron sputtering device 295 to rotate within the magnetron sputtering cavity 2941, thereby applying an electromagnetic field to the target 240.
[0125] In some embodiments, the magnetron cavity 2941 may also be filled with deionized water to cool the target material 240 and achieve heat dissipation.
[0126] In some embodiments, when the physical vapor deposition chamber 200 is sputtering or anti-sputtering, radio frequency devices are applied in the process chamber, and the pressure of argon gas in the process chamber can be from 0.01 mT to 100 mT, which can be adjusted according to actual needs, and this application does not limit it.
[0127] It should be noted that, upon considering the specification and practicing the application disclosed herein, those skilled in the art will readily conceive of other embodiments of this application. This application is intended to cover any variations, uses, or adaptations of this application that follow the general principles of this application and include common knowledge or customary techniques in the art not disclosed herein.
[0128] It should be understood that this application is not limited to the precise structure described above and shown in the accompanying drawings, and various modifications and changes can be made without departing from its scope. The true scope is indicated by this application.
Claims
1. A physical vapor deposition chamber, comprising: include: The side walls enclose and form the process cavity; The first inner liner includes an upper inner liner and a lower inner liner. The lower inner liner is connected to the side wall and disposed in the process cavity. The lower inner liner has a first opening that extends through its own thickness direction. The upper inner liner is fixed in the process cavity through the lower inner liner. The opening of the upper inner liner towards the lower inner liner extends into the lower inner liner. A radio frequency coil is disposed between the lower inner liner and the side wall; A target material is located at the top of the process cavity, connected to the sidewall, and at least a portion of the target material extends into the upper liner.
2. The physical vapor deposition chamber of claim 1, wherein, Also includes: Coil support, conductive components, and power supply components; The power supply component passes through the side wall and extends into the process cavity; One end of the conductive element is connected to the power supply element, and the other end is connected to the radio frequency coil; The coil support is located between the lower inner liner and the side wall, the coil support is connected to the side wall, the radio frequency coil is connected to the coil support, and the other end of the radio frequency coil is grounded through the coil support and the side wall.
3. The physical vapor deposition chamber of claim 2, wherein, A first receiving groove is formed on the surface of the sidewall facing the lower liner; The coil support includes an insulating support, an upper metal ring, and a lower metal ring; The lower metal ring is disposed on the bottom surface of the first receiving groove and is grounded through the bottom surface of the first receiving groove; The insulating support is connected between the upper metal ring and the lower metal ring. The surface of the insulating support facing the lower inner liner is provided with a first snap-fit portion. The number of the first snap-fit portions is the same as the number of turns of the radio frequency coil. Each turn of the RF coil is respectively snapped into one of the first snap-fit portions. One end of the RF coil is electrically connected to the lower metal ring, and the other end extends through the upper metal ring toward the power supply component.
4. The physical vapor deposition chamber according to claim 3, characterized in that, There are multiple insulating supports, and each insulating support is detachably connected to the upper metal ring and the lower metal ring by bolts.
5. The physical vapor deposition chamber according to claim 3, characterized in that, The upper metal ring includes a first end and a second end arranged along the circumferential direction, and there is a gap between the first end and the second end along the circumferential direction of the upper metal ring; The coil support also includes an insulating fastener, the two ends of which are respectively connected to the first end and the second end, and the insulating fastener is provided with a through hole; The radio frequency coil passes through the through hole and is connected to the conductive element.
6. The physical vapor deposition chamber according to claim 3, characterized in that, The upper metal ring and / or the lower metal ring are provided with a second snap-fit portion; The first receiving groove is provided with a third locking part corresponding to the second locking part; The second snap-fit portion snaps into the third snap-fit portion; The lower metal ring is detachably connected to the bottom surface of the first receiving groove by bolts.
7. The physical vapor deposition chamber of any of claims 1-6, wherein, Also includes: A second inner liner is disposed around the lower inner liner and located between the radio frequency coil and the lower inner liner.
8. The physical vapor deposition chamber according to claim 7, characterized in that, The material of the second liner includes insulating material.
9. The physical vapor deposition chamber according to claim 7, characterized in that, The material of the second liner includes conductive materials; The second liner has a second opening extending through its own thickness direction.
10. The physical vapor deposition chamber according to claim 9, characterized in that, The second opening is offset from the first opening.
11. The physical vapor deposition chamber according to claim 7, characterized in that, Also includes: A third inner liner is disposed around the radio frequency coil and located between the radio frequency coil and the side wall; The third lining is made of insulating material.
12. The physical vapor deposition chamber according to any one of claims 1-6, characterized in that, A second receiving groove is formed on the surface of the sidewall facing the lower liner; The opening of the lower inner liner toward the upper inner liner has a bent portion formed by bending toward the side wall, and the bent portion is connected to the bottom surface of the second receiving groove. The physical vapor deposition chamber also includes a support member disposed on the side of the bent portion away from the bottom surface of the second receiving groove; The upper inner liner is connected to the support member.
13. The physical vapor deposition chamber according to claim 12, characterized in that, The support component is made of an insulating material.