Testing device for detecting the bond strength of composite insulators

By designing a clamping test section and a tension device to measure the peeling tension value when the shed is peeled off, the problem of non-quantitative and poor stability in the existing technology for detecting the bonding strength between the shed and the core rod of composite insulators is solved, and quantitative measurement and stable detection of bonding strength are realized.

CN224985294UActive Publication Date: 2026-11-17SIMENS LIGHTNING ARRESTER WUXI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522437986.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-17
Publication Date
2026-11-17
Estimated Expiration
2035-11-17

AI Technical Summary

Technical Problem

Existing technologies for testing the bonding strength between the sheath and the core rod of composite insulators suffer from problems such as significant human influence in the testing methods, non-quantitative results, and poor stability.

Method used

Design a testing device including a fixing part, a clamping test part and a tensile device. The clamping test part clamps the umbrella leaf through a rectangular assembly groove and a movable block, and the tensile device measures the peeling tensile force value when the umbrella leaf is peeled off in order to quantify the bonding strength.

Benefits of technology

It enables quantitative measurement of bond strength, improves the stability and accuracy of testing, can flexibly adapt to umbrellas of different sizes and shapes, reduces interference from materials near the root of the umbrella, and ensures the reliability of test results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224985294U_ABST
    Figure CN224985294U_ABST
Patent Text Reader

Abstract

This disclosure discloses a testing device for detecting the bonding strength of composite insulators, comprising: a fixing part for fixing a sample block body cut from a composite insulator; a clamping testing part, comprising: a main block having a rectangular assembly groove, the side of the rectangular assembly groove opposite to the fixing part being open to allow the umbrella sheet to be inserted into the rectangular assembly groove; a movable block being assembled within the rectangular assembly groove and movable within the rectangular assembly groove to cooperate with the main block to clamp the umbrella sheet; a handle connected to the movable block for moving the movable block; a connecting part connected to the main block; and a tension device connected to the clamping testing part via the connecting part to pull the clamping testing part, thereby moving the umbrella sheet to peel it off. The tension device measures the peeling tensile force during umbrella sheet peeling and provides a peeling tensile force value to detect the bonding strength. The testing device can quantify the bonding strength between the umbrella sleeve and the core rod and has a simple structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of power equipment testing technology, and more specifically to a testing device for testing the bonding strength of composite insulators. Background Technology

[0002] Currently, the bond strength inspection between the sheath and the core rod of composite insulators mainly relies on manual judgment, especially when inspecting the bond between the silicone rubber sheath and the glass fiber core rod, where a systematic and precise evaluation method is lacking. Existing inspection methods typically involve manually peeling off the silicone rubber sheath with a knife and visually judging the bond strength. This method is not only time-consuming and labor-intensive, but also highly susceptible to the influence of the operator's subjective judgment, leading to uncertainty and non-repeatability of the test results. More importantly, such methods cannot provide quantitative data support, making it difficult to meet the requirements of modern manufacturing processes for precise control of bond quality.

[0003] In some cases, manufacturers attempt to improve the process, such as by enhancing visual inspection or using simple tools to assist peeling; however, this does not fundamentally improve the stability and reliability of the inspection. In other cases, electronic devices may be used for some preliminary performance tests, but these tests often focus on overall electrical characteristics rather than specific bonding performance, and therefore cannot effectively assess the bond strength between the umbrella sleeve and the mandrel.

[0004] Furthermore, traditional methods often overlook the potential impact of differences in material properties near the root of the umbrella fins on the bond strength test results. Since the umbrella cover is made of silicone rubber, its elastic properties make it prone to deformation during peeling, further increasing the difficulty of accurately testing bond strength.

[0005] In summary, existing technologies for detecting the bonding strength between the sheath and the core rod of composite insulators suffer from problems such as significant human influence on the detection methods, non-quantitative results, and poor stability. Utility Model Content

[0006] (a) Technical issues In view of the above-mentioned shortcomings of the prior art, this disclosure provides a testing device for detecting the bonding strength of composite insulators, which at least solves the problems of the prior art in detecting the bonding strength between the sheath and the core rod of composite insulators, such as the large influence of human factors in the testing method, non-quantitative results, and poor stability.

[0007] (II) Technical Solution According to one aspect of the present disclosure, a testing device for detecting the bonding strength of a composite insulator is provided. The composite insulator includes a core rod and a sheath disposed outside the core rod. The sheath includes a sheath body disposed outside the core rod and sheath sheets extending outward from the sheath body. The sheath body and sheath sheets are integrally formed. The testing device includes: a fixing part for fixing a sample block body cut from the composite insulator; and a clamping testing part, which includes: a main block having a rectangular assembly groove on one side opposite to the fixing part. The device includes: an open section to allow the umbrella slats to be inserted into a rectangular assembly slot; a movable block that is fitted into the rectangular assembly slot and can move within the slot to engage with a main block to clamp the umbrella slats; a handle connected to the movable block for moving the movable block; a connecting portion connected to the main block; and a tensioning device connected to a clamping test portion via the connecting portion to pull the clamping test portion, thereby moving the umbrella slats to peel them off. The tensioning device measures the peeling tension during peeling and provides a peeling tension value indicating the peeling tension to detect the bonding strength.

[0008] In this way, by designing a clamping test unit with a simple structure to peel the umbrella sheet, and by connecting the clamping test unit to a tension device, the tension device measures the peeling tension during the peeling of the umbrella sheet and provides a peeling tension value indicating the peeling tension, thereby quantifying the bonding strength. Specifically, the rectangular mounting groove and its one-sided open design of the main body block of the clamping test unit of this disclosure provide precise positioning and clamping space for the umbrella sheet. Combined with the dynamic adjustment of the movable block, it can firmly clamp umbrella sheets of different sizes and shapes, greatly increasing the applicability of the device. The handle further improves the convenience of operation. The operator can fine-tune the position of the movable block through the handle to adapt to changes in the thickness of the umbrella sheet and ensure appropriate clamping force. In addition, the connection between the tension device and the main body block ensures uniform application of tension during the peeling process, accurately capturing the maximum force value at the moment of peeling, thereby obtaining reliable bonding strength data, and thus quantifying the bonding strength between the silicone umbrella cover and the fiberglass rod.

[0009] According to an exemplary embodiment of the present disclosure, the movable block is movably connected to the main body block by a threaded pin to move within a rectangular assembly slot, and the handle is connected to the movable block through a mounting hole provided on the main body block.

[0010] This design allows the movable block to move smoothly within the rectangular mounting slot, and the connection method allows the movable block to be adjusted in position as needed to accommodate umbrella sections of different sizes and shapes. Furthermore, the handle is also connected to the movable block via mounting holes on the main body block, enabling convenient adjustment of the movable block's position and ensuring the umbrella section is securely and precisely fixed during testing.

[0011] According to an exemplary embodiment of the present disclosure, a rectangular assembly groove includes a first wall for assembling a movable block, a second wall opposite to the first wall, and a third wall connecting the first wall and the second wall and perpendicular to the first wall and the second wall. The open side of the rectangular assembly groove is opposite to the third wall. The movable block moves between the first wall and the second wall. The movable block includes a clamping surface opposite to the second wall. The surface of the clamping surface and the surface of the second wall are uneven. The umbrella-shaped flap is clamped between the clamping surface of the movable block and the second wall.

[0012] In this way, the uneven surface design of the clamping surfaces of the moving block and the main block increases the friction between the two and the umbrella slats, so that the umbrella slats can remain stable even when tension is applied, avoiding measurement errors caused by slippage.

[0013] According to an exemplary embodiment of the present disclosure, there is a gap space between the third wall of the rectangular assembly groove and the movable block, and a positioning part is assembled on the movable block. The positioning part is used to restrict the movement of the movable block in a direction perpendicular to the horizontal plane, so that the central axis of the clamped umbrella blade remains perpendicular to the horizontal plane.

[0014] In this way, by setting up a positioning part to cooperate with the movable block and the rectangular assembly slot, the umbrella slats will not tilt or rotate during the test. This ensures that the central axis of the umbrella slats remains perpendicular to the horizontal plane when clamped, resulting in a uniform force distribution when the umbrella slats are peeled from the core rod surface. This improves the accuracy of the tensile force value during the test, and thus accurately determines the bond strength between the umbrella cover and the core rod. In addition, the design of the gap space facilitates the smooth movement of the movable block.

[0015] According to an exemplary embodiment of this disclosure, the handle can adjust the gap distance between the movable block and the second wall to accommodate umbrella slats of different thicknesses.

[0016] This design allows the testing device to flexibly handle the clamping requirements of umbrella blades of varying thicknesses. By adjusting the handle, the operator can easily and accurately control the position of the movable block, avoiding testing errors caused by excessively tight or loose clamping.

[0017] According to an exemplary embodiment of this disclosure, the tensioning device is an electronic tensioning machine.

[0018] According to an exemplary embodiment of the present disclosure, the sample is pre-treated before testing. The pre-treatment includes cutting a slit along the outer periphery of the root where the umbrella blade joins the umbrella cover body to form a test area. A tensile device is used to determine the bond strength by calculating the ratio of the peel tensile force value to the area of ​​the test area.

[0019] This method reduces interference from the main body near the base of the umbrella slats, ensuring test accuracy. By creating a test area through a slit cut at the base of the slats, the slats and main body are effectively separated, allowing subsequent tensile tests to accurately reflect the bond strength between the umbrella cover and the core rod. Furthermore, by defining the test area and calculating the ratio of the peel strength to the area of ​​the test area, the bond strength can be quantified.

[0020] (III) Technical Effects In the embodiments of this disclosure, the testing device for detecting the bonding strength of composite insulators can obtain quantifiable bonding strength between the silicone umbrella and the glass fiber rod. Moreover, the entire testing device, especially the clamping test part, has a simple structure, is easy to manufacture, the testing process is easy to operate, and the test results are stable and reliable. Attached Figure Description

[0021] The accompanying drawings, which are included to provide a further understanding of this disclosure and form part of this disclosure, illustrate exemplary embodiments of the present disclosure and are used to explain the disclosure, but do not constitute an undue limitation of the disclosure. In the drawings: Figure 1 This is a schematic diagram of the configuration of a detection apparatus according to an embodiment of the present disclosure.

[0022] Figure 2 This is a schematic diagram of the configuration of the clamping and testing section of the detection apparatus according to an embodiment of the present disclosure.

[0023] Figure 3 A perspective view of the configuration of the clamping test section of a testing apparatus for detecting the bonding strength of composite insulators according to the present disclosure is shown.

[0024] Explanation of icon numbers: 100 Fixed part 200 Clamping Test Section 300 tension device 10 Main Blocks 11 Rectangular assembly slot 11A First Wall 11B Second Wall 11C Third Wall 12 active blocks 12S clamping surface 13 Handles 14 Connecting parts 15 Threaded pins 16 Positioning Section Detailed Implementation

[0025] To enable those skilled in the art to better understand the present disclosure, the technical solutions of the present disclosure will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present disclosure, and not all embodiments. Based on the embodiments of the present disclosure, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of the present disclosure.

[0026] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this disclosure are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this disclosure described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover a non-exclusive inclusion; for example, a process, control method, system, product, or device that includes a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, control methods, products, or devices.

[0027] Typically, a composite insulator may include a core rod and a sheath disposed outside the core rod. The sheath includes a sheath body fitted over the core rod and sheath plates extending outward from the sheath body; the sheath body and sheath plates are integrally formed. In the prior art, the existing methods for testing the bonding strength between the sheath and the core rod of composite insulators suffer from problems such as significant influence from human factors, non-quantifiable results, and poor stability.

[0028] Therefore, the present invention is to design a clamping test unit with a simple structure to peel the umbrella sheet and to measure the peeling tensile force during peeling by connecting the clamping test unit to a tensile device and providing a peeling tensile force value indicating the peeling tensile force, thereby enabling the quantification of the bonding strength.

[0029] Figure 1 A schematic diagram of the configuration of a testing apparatus for detecting the bond strength of composite insulators according to this disclosure is shown. Figure 1 As shown, the testing device may include: a fixing part 100 for fixing the sample block body A of the sample block cut from the composite insulator; a clamping test part 200 for clamping the umbrella leaf B of the sample block; and a tension device 300 for pulling the clamping test part 200 to move the umbrella leaf B to peel it off. The tension device 300 can measure the peeling tensile force when the umbrella leaf B is peeled off and provide a peeling tensile force value indicating the peeling tensile force to detect the bonding strength.

[0030] In this disclosure, the fixing part 100 can clamp and fix the sample body by two or more plates with spring or thread adjustment, for example, manually or pneumatically, providing sufficient clamping force to ensure that the sample body does not move during the test. Since the fixing part is not an improvement of this disclosure, and any fixing component that can provide sufficient fixing force to ensure that the sample body does not move during the test and that the umbrella blade extends outward from the fixing part to be clamped by the test part can be used to implement the fixing part, it will not be described in detail here.

[0031] In this document, the tensile testing device 300 may include an electronic tensile testing machine. During the tensile testing process, the electronic tensile tester pulls the clamping test section at a stable speed, thereby causing the umbrella leaf fixed on the clamping test to move until the umbrella leaf is completely peeled off from the surface of the mandrel. During this process, the electronic tensile tester can continuously record the tensile force value and provide a peak reading when the maximum tensile force is reached, thereby providing a peel tensile force value indicating the peel tensile force at which the umbrella leaf is peeled off.

[0032] Figure 2 A schematic diagram of the interface configuration of the clamping test section of the testing apparatus for detecting the bond strength of composite insulators according to the present disclosure is shown. Figure 3 A perspective view shows the configuration of the clamping test section of a testing apparatus for detecting the bonding strength of composite insulators according to the present disclosure.

[0033] like Figures 1 to 3 As shown, the clamping test unit 200 may include: a main body block 10, which may have a rectangular assembly groove 11, with one side of the rectangular assembly groove 11 opposite to the fixing part 100 open to allow the umbrella slab B to be inserted into the rectangular assembly groove 11; a movable block 12, which is fitted into the rectangular assembly groove 11 and can move within the rectangular assembly groove 11 to cooperate with the main body block 10 to clamp the umbrella slab B; a handle 13, which is connected to the movable block 12 and used to move the movable block 12; and a connecting part 14, which is connected to the main body block 10 and connects the main body block 10 to the tension device 300.

[0034] like Figure 1 As shown, the tension device 300 can be connected to the clamping test part 200 via the connecting part 14 to pull the clamping test part 200, thereby moving the umbrella leaf B to peel it off. The tension device 300 can measure the peeling tension when the umbrella leaf B is peeled off and provide a peeling tension value indicating the peeling tension to detect the bonding strength.

[0035] As an example, such as Figures 1 to 3As shown, the movable block 12 can be movably connected to the main body block 10 via at least two threaded pins 15 to move within the rectangular mounting slot 11, and the handle 13 can be connected to the movable block 12 via a mounting hole provided on the main body block 10. In this way, the movable block 12 can move smoothly within the rectangular mounting slot 11, and this connection method allows the movable block 12 to adjust its position as needed to accommodate umbrella fins B of different sizes and shapes.

[0036] In addition, since the handle 13 can be connected to the movable block 12 through the mounting hole provided on the main body block 10, the position of the movable block 12 can be easily adjusted to ensure that the umbrella slab B is firmly fixed during the test.

[0037] Further as Figures 1 to 3 As shown, the rectangular assembly slot 11 may include a first wall 11A for assembling the movable block 12, a second wall 11B opposite to the first wall 11A, and a third wall 11C connecting the first wall 11A and the second wall 11B and perpendicular to the first wall 11A and the second wall 11B. The open side of the rectangular assembly slot 11 faces the third wall 11C, wherein the movable block 12 moves between the first wall 11A and the second wall 11B. The movable block 12 may include a clamping surface 12S opposite to the second wall 11B. The surfaces of the clamping surface 12S and the second wall 11B may be uneven. The umbrella slat B is clamped between the clamping surface 12S of the movable block 12 and the second wall 11B. In this way, the uneven surface design of the clamping surface 12S of the movable block 12 and the second wall 11B increases the friction between the two and the umbrella slat B, so that the umbrella slat B remains stable even when tension is applied, avoiding measurement errors caused by slippage.

[0038] Further as Figure 1 As shown, optionally or additionally, a gap space exists between the third wall 11C of the rectangular assembly groove 11 and the movable block 12, which facilitates smooth movement of the movable block. Furthermore, a positioning part 16 is mounted on the movable block 12 to restrict its vertical movement or deflection, thereby ensuring that the central axis of the clamped umbrella slat B is perpendicular to the horizontal plane. In this way, by providing the positioning part 16 to cooperate with the movable block 12 and the rectangular assembly groove 11, the umbrella slat B will not tilt or rotate during the test, thus ensuring that its central axis remains perpendicular to the horizontal plane when clamped. This results in a uniform distribution of tensile force when the umbrella slat B is peeled from the core rod surface, thereby improving the accuracy of the tensile force value during the test and accurately determining the bonding strength between the umbrella cover and the core rod.

[0039] Further as Figures 1 to 3As shown, the handle 13 can adjust the gap between the movable block 12 and the second wall 11B to accommodate umbrella slats B of different thicknesses. In this way, the clamping test unit can flexibly meet the clamping requirements of umbrella slats B of different thicknesses. By operating the handle 13, the operator can easily and accurately control the position of the movable block 12, avoiding test errors caused by clamping too tightly or too loosely.

[0040] As an example, in this disclosure, the composite insulator can be divided into three sections along its length, and then each section can be cut to obtain a sample block. The bonding strength between the sheath and the core rod of each sample block can be tested using the testing device of this disclosure to determine whether the bonding performance of the entire composite insulator meets the requirements.

[0041] As an example, the sample can be pre-treated before testing. Pre-treatment includes cutting a slit along the outer periphery of the root where the umbrella blade B joins the umbrella body A to form a test area. The bond strength is determined by calculating the ratio of the peel strength to the area of ​​the test area. This reduces interference from the body portion near the root of the umbrella blade B on the test results, ensuring test accuracy. The test area formed by cutting a slit at the root of the umbrella blade B effectively separates the umbrella blade B from the body, ensuring that the measurement results accurately reflect the bond strength between the umbrella body and the core rod during subsequent tensile testing. Furthermore, by defining the test area, the bond strength can be determined by calculating the ratio of the peel strength to the area of ​​the test area, quantifying the bond strength and thus accurately determining whether the overall bonding performance of the composite insulator meets the requirements.

[0042] Furthermore, in this disclosure, the bonding performance of the entire composite insulator can be determined by judging whether the calculated bond strength exceeds a threshold. For example, when the calculated bond strength exceeds 1.5 Newtons per square meter (N / m²), the bond strength between the sheath and the core rod can be considered to have reached the qualified standard. This threshold is determined through experimental analysis of a large number of samples, combined with the maximum stress conditions that the composite insulator may encounter under actual working conditions, to ensure that the bond between the sheath and the core rod can still maintain its structural integrity and electrical insulation performance under various harsh environmental conditions (including temperature changes, humidity fluctuations, ultraviolet radiation, etc.).

[0043] Alternatively, the bonding performance of the composite insulator can be determined by observing and analyzing the stripped area.

[0044] Once the test is complete and the umbrella cover has been peeled off the sample, if the entire peeled area only shows traces of the silicone rubber material of the umbrella cover without any exposed core material, this means that the umbrella cover fractured preferentially during the peeling process, rather than being peeled off from the core. This reflects that the bond strength between the umbrella cover and the core actually exceeds the tear strength of the umbrella cover itself, confirming the strength of the adhesive layer.

[0045] Conversely, if the peeled area only exposes the material of the core rod, such as fiberglass, while the umbrella cover material is completely missing, this usually indicates that the adhesive layer has failed to maintain effective bonding between the umbrella cover and the core rod under tensile force, and the bonding strength does not meet the requirements.

[0046] Ideally, the peeling area exhibits a hybrid form of the shed material (e.g., silicone rubber) and the core material (e.g., fiberglass). This indicates that under tensile stress, the adhesive layer neither causes independent fracture of the shed material nor merely separation at the adhesive interface, but rather promotes the joint failure of the shed and core materials in the peeling area. This directly proves that the adhesive strength matches the inherent strength of the shed and core materials, meeting the standards for composite insulator design and manufacturing. The emergence of this hybrid form means that the adhesive layer not only possesses sufficient strength but also appropriate toughness, enabling it to work synergistically with the shed and core materials under external mechanical stress, preventing structural damage caused by the failure of a single material.

[0047] Therefore, this disclosure provides a comprehensive and more accurate evaluation method for assessing whether the bonding performance meets requirements by combining quantitative evaluation with observation of the microstructure of the peeled area, overcoming the limitations of traditional testing methods. This comprehensive evaluation system can ensure quality control of composite insulators during mass production, help improve the overall performance of the product, extend its service life, and reduce potential risks caused by bonding problems of composite insulators in power transmission systems.

[0048] This disclosure has at least the following advantages: 1. It can quantify the bonding strength between the sheath and the core rod, thus enabling a more accurate judgment on whether the bonding of the sheath of the composite insulator meets the requirements; 2. The entire clamping and testing unit has a simple structure, is easy to manufacture, and the testing process is easy to operate, with stable and reliable test results.

[0049] 3. After the tensile test, by observing the peeling area, the failure mode of the adhesive layer can be intuitively determined, confirming whether the adhesive strength exceeds the tear strength of the sheath or meets the expected mixed failure. This provides additional qualitative verification of whether the adhesive strength is qualified. Furthermore, through the mutual verification of qualitative and quantitative assessments, the adhesive strength of the sheath of the composite insulator can be more accurately evaluated to determine whether it meets the requirements.

[0050] In the several embodiments provided in this disclosure, it should be understood that the disclosed technical content can be implemented in other ways. The device embodiments described above are merely illustrative and represent only preferred embodiments of this disclosure. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principles of this disclosure, and such improvements and modifications should also be considered within the scope of protection of this disclosure.

Claims

1. A testing device for detecting the bonding strength of a composite insulator, the composite insulator comprising a core rod and a sheath disposed outside the core rod, the sheath comprising a sheath body sleeved outside the core rod and sheath blades extending outwardly from the sheath body, the sheath body and the sheath blades being integrally formed, characterized in that, The detection device includes: The fixing part (100) is used to fix the sample block body of the sample block cut from the composite insulator; A clamping test unit (200) includes: The main body block (10) has a rectangular assembly slot (11) with one side of the rectangular assembly slot (11) opposite to the fixing part (100) open to allow the umbrella blade to be inserted into the rectangular assembly slot (11). Movable block (12), which is assembled in the rectangular assembly slot (11) and can move in the rectangular assembly slot (11) to cooperate with the main block (10) to clamp the umbrella sheet; A handle (13), connected to the movable block (12), for moving the movable block (12); and Connecting part (14), the connecting part (14) is connected to the main body block (10); and A tensioning device (300) is connected to the clamping test part (200) via the connecting part (14) to pull the clamping test part (200) to move the umbrella leaf to peel it off. The tensioning device (300) measures the peeling tension when the umbrella leaf is peeled off and provides a peeling tension value indicating the peeling tension to detect the bonding strength.

2. The testing device for detecting the bonding strength of composite insulators according to claim 1, characterized in that, The movable block (12) is movably connected to the main body block (10) by a threaded pin to move within the rectangular assembly slot (11), and the handle (13) is connected to the movable block (12) through a mounting hole opened on the main body block (10).

3. The testing device for detecting the bonding strength of composite insulators according to claim 1, characterized in that, The rectangular assembly slot (11) includes a first wall for assembling the movable block (12), a second wall opposite to the first wall, and a third wall connecting the first wall and the second wall and perpendicular to the first wall and the second wall. The open side of the rectangular assembly slot (11) is opposite to the third wall. The movable block (12) moves between the first wall and the second wall. The movable block (12) includes a clamping surface opposite to the second wall. The clamping surface and the surface of the second wall are uneven. The umbrella leaf is clamped between the clamping surface of the movable block (12) and the second wall.

4. The testing device for detecting the bonding strength of composite insulators according to claim 3, characterized in that, There is a gap between the third wall of the rectangular assembly groove (11) and the movable block (12). The movable block (12) is equipped with a positioning part (16), which is used to restrict the movable block from moving in a direction perpendicular to the horizontal plane, so that the central axis of the clamped umbrella blade remains perpendicular to the horizontal plane.

5. The testing device for detecting the bonding strength of composite insulators according to claim 3, characterized in that, The handle (13) can adjust the gap distance between the movable block (12) and the second wall to accommodate umbrella slats of different thicknesses.

6. The testing device for detecting the bonding strength of composite insulators according to any one of claims 1-5, characterized in that, The tensioning device (300) is an electronic tensioning machine.

7. The testing device for detecting the bonding strength of composite insulators according to any one of claims 1-5, characterized in that, The sample is pretreated before testing. The pretreatment includes cutting a slit along the outer periphery of the root where the umbrella blade joins the umbrella cover body to form a test area. The tensile device (300) is used to determine the bonding strength by calculating the ratio of the peeling tensile force value to the area of ​​the test area.