A vertical cavity surface-emitting laser

By utilizing the phase transition properties of vanadium dioxide in a vertical cavity surface-emitting laser, the light source and optical switch are integrated, solving the problems of low integration and high complexity caused by the independence of the optical system, and realizing the optical switch function with high integration and low power consumption.

CN224986883UActive Publication Date: 2026-11-17JLIGHT SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522729521.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-23
Publication Date
2026-11-17
Estimated Expiration
2035-12-23

AI Technical Summary

Technical Problem

The optical systems of existing vertical cavity surface-emitting lasers are usually independent of optical switches, resulting in low integration, high system complexity, and high cost.

Method used

Vanadium dioxide is used as the material for the top DBR structure. By utilizing the phase transition properties of vanadium dioxide, the temperature of the vanadium dioxide layer is controlled by the third electrode to switch between its insulating and metallic phases, thereby realizing the opening and closing of the vertical cavity surface-emitting laser and integrating the light source and optical switch.

Benefits of technology

It achieves a high degree of integration between the light source and the optical switch, reducing system complexity and cost, and has higher integration and lower power consumption, making it suitable for high-speed optical switch applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224986883U_ABST
    Figure CN224986883U_ABST
Patent Text Reader

Abstract

This invention relates to the field of laser technology, and more particularly to a vertical-cavity surface-emitting laser (VCSEL). The VCSEL comprises: a first electrode, a substrate layer, an N-type dielectric barrier layer (DBR) structure, a first spacer layer, an active layer, a second spacer layer, an oxide confinement layer, and a third spacer layer stacked sequentially; a dielectric barrier layer (DBR) structure and a second electrode, both located on the surface of the third spacer layer away from the oxide confinement layer, with the second electrode spaced apart from the DBR structure. The DBR structure is composed of alternating vanadium dioxide layers and low-refractive-index dielectric layers in multiple cycles; and a third electrode located on the top surface of the DBR structure away from the third spacer layer, surrounding the light exit aperture. The third electrode is used to apply a voltage to change the temperature of the vanadium dioxide layer, thereby controlling the VCSEL to turn on or off. This invention at least improves the integration of optical systems.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of laser technology, and particularly relates to a vertical cavity surface-emitting laser. Background Technology

[0002] Vertical-cavity surface-emitting semiconductor lasers (VCSELs) differ from traditional edge-emitting semiconductor lasers. The epitaxial structure of a VCSEL mainly includes an upper Bragg mirror, a lower Bragg mirror, a conductive confinement region, an active region, and a semiconductor substrate. Feedback from the upper and lower Bragg mirrors causes the laser beam to exit the cavity in a direction perpendicular to the substrate. VCSELs offer numerous advantages, including low threshold current, circular spot size, high modulation bandwidth, single-mode lasing, ease of fabrication into high-density two-dimensional arrays, and relatively low manufacturing cost. VCSELs have wide applications in many fields, such as optical switches, optical communications, consumer electronics, atomic sensing, and lidar.

[0003] In optical systems, the optical switch that controls the vertical-cavity surface-emitting semiconductor laser is usually independent of the vertical-cavity surface-emitting semiconductor laser. Utility Model Content

[0004] In view of this, the present invention aims to provide a vertical cavity surface-emitting laser, which at least helps to improve the integration of optical systems.

[0005] To achieve the above objectives, the technical solution of this utility model is implemented as follows: This invention provides a vertical-cavity surface-emitting laser (VCSEL), comprising: a first electrode, a substrate layer, an N-type dielectric barrier layer (DBR) structure, a first spacer layer, an active layer, a second spacer layer, an oxide confinement layer, and a third spacer layer stacked sequentially; a dielectric barrier layer (DBR) structure and a second electrode, both located on the surface of the third spacer layer away from the oxide confinement layer, with the second electrode spaced apart from the dielectric barrier layer; the dielectric barrier layer (DBR) structure being composed of alternating vanadium dioxide layers and low-refractive-index dielectric layers in multiple cycles; and a third electrode located on the top surface of the dielectric barrier layer away from the third spacer layer, surrounding the light exit aperture. The third electrode is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the VCSEL to turn on or off.

[0006] Furthermore, the second electrode surrounds the dielectric film DBR structure, and the material of the low refractive index dielectric layer is silicon dioxide.

[0007] Furthermore, the third electrode is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the switching of the vanadium dioxide layer between the insulating phase and the metallic phase, so as to realize the turning on or off of the vertical cavity surface emission laser. The refractive index of the vanadium dioxide layer when it is in the insulating phase is greater than that when it is in the metallic phase. When the vertical cavity surface emission laser is turned on, the vanadium dioxide layer is in the insulating phase, and when the vertical cavity surface emission laser is turned off, the vanadium dioxide layer is in the metallic phase.

[0008] Furthermore, the refractive index of the vanadium dioxide layer when it is in an insulating phase is in the range of 2.5 to 3.5, and the refractive index of the vanadium dioxide layer when it is in a metallic phase is in the range of 0.5 to 1.5.

[0009] Furthermore, when the vertical cavity surface-emitting laser is turned on, the reflectivity of the dielectric film DBR structure is greater than 95%.

[0010] Furthermore, when the temperature of the vanadium dioxide layer is higher than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide absorption layer is in a metallic phase; when the temperature of the vanadium dioxide layer is lower than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide layer is in an insulating phase.

[0011] Furthermore, the first electrode serves as the negative electrode of the vertical-cavity surface-emitting laser (VCSEL), and the second electrode serves as the positive electrode of the VCSEL. The first and second electrodes provide electric pumping for the VCSEL. The second electrode serves as the negative electrode of the dielectric film DBR structure, and the third electrode serves as the positive electrode of the dielectric film DBR structure. The second and third electrodes are subjected to corresponding voltages to change the temperature of the vanadium dioxide layer.

[0012] Furthermore, when the vertical-cavity surface-emitting laser is turned on, the voltage applied to the first electrode is less than the voltage applied to the second electrode, and the third electrode is applied with the same voltage as the second electrode; when the vertical-cavity surface-emitting laser is turned off, the voltage applied to the third electrode is greater than the voltage applied to the second electrode.

[0013] Compared with existing technologies, this invention achieves the following beneficial effects: The vertical-cavity surface-emitting laser (VCSEL) provided by this invention is a VCSEL laser with high-speed optical switching characteristics. Specifically, vanadium dioxide is used as one of the materials in the top DBR structure. Utilizing the phase transition characteristics of vanadium dioxide, the temperature of the vanadium dioxide layer is controlled by the third electrode to achieve the switching between the insulating and metallic phases of vanadium dioxide, thereby controlling whether the VCSEL emits laser light or not, thus realizing the function of optical switching. This invention integrates the light source and the optical switch, eliminating the need for a complex optical system and achieving higher integration. Furthermore, the vanadium dioxide phase change material switch has lower power consumption compared to electro-optic switches (lithium niobate or silicon-based) or MEMS (Micro-Electro-Mechanical System) switches. Monolithically integrating the optical switch and the light source expands the functionality of the VCSEL chip, featuring a simple and compact structure. It eliminates the need for additional light source and switch system links, reducing the complexity of system construction, decreasing system size, and also helping to reduce system setup costs. Attached Figure Description

[0014] The accompanying drawings, which form part of this utility model, are used to provide a further understanding of the utility model. The illustrative embodiments of the utility model and their descriptions are used to explain the utility model and do not constitute an undue limitation of the utility model. In the drawings: Figure 1 This is a schematic diagram of the structure of the vertical cavity surface-emitting laser described in an embodiment of the present invention. Detailed Implementation

[0015] To make the objectives, technical solutions, and advantages of this utility model clearer, the present utility model will be further described in detail below with reference to the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present utility model and do not constitute a limitation thereof.

[0016] It should be noted that, unless otherwise specified, the embodiments and features described in these embodiments of the present invention can be combined with each other.

[0017] In the description of this utility model, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," and "counterclockwise," etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings and are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model. Furthermore, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, features defined with "first," "second," etc., may explicitly or implicitly include one or more of that feature. In the description of this utility model, unless otherwise stated, "a plurality of" means two or more.

[0018] In the description of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.

[0019] The present invention will now be described in detail with reference to the accompanying drawings and embodiments.

[0020] refer to Figure 1This invention provides a vertical-cavity surface-emitting laser, comprising: a first electrode 111, a substrate layer 100, and an N-type distributed Bragg optics layer stacked sequentially. The structure comprises a distributed Bragg reflector (DBR) 101, a first spacer layer 102, an active layer 103, a second spacer layer 104, an oxide confinement layer 105, and a third spacer layer 106; a dielectric film DBR structure 107 and a second electrode 112, both located on the surface of the third spacer layer 106 away from the oxide confinement layer 105, with the second electrode 112 spaced apart from the dielectric film DBR structure 107. The dielectric film DBR structure 107 is composed of alternating vanadium dioxide layers and low-refractive-index dielectric layers in multiple cycles; and a third electrode 113 located on the top surface of the dielectric film DBR structure 107 away from the third spacer layer 106, surrounding the light exit aperture. The third electrode 113 is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the vertical-cavity surface-emitting laser to turn on or off.

[0021] The vanadium dioxide layer can consist solely of vanadium dioxide, or it can include vanadium dioxide and dopants. When vanadium dioxide undergoes a phase transition, this is manifested as a change in refractive index and absorption coefficient. Below the critical phase transition temperature, vanadium dioxide is an insulating phase; above the critical phase transition temperature, it is a metallic phase. When vanadium dioxide is in the metallic phase, it has a high absorption coefficient, resulting in strong absorption loss, and a low refractive index. When vanadium dioxide is in the insulating phase, it has a high refractive index. The refractive index difference between the metallic and insulating phases can be approximately 1 to 2, depending on the corresponding wavelength. The critical phase transition temperature of vanadium dioxide can be adjusted through doping, with an adjustment range of approximately 20℃ to 26℃. Therefore, the vanadium dioxide layer can be doped according to practical application requirements to meet specific needs. Doping elements that increase the critical phase transition temperature can be at least one of Ti, Al, and Cr, while doping elements that decrease the critical phase transition temperature can be at least one of W, Mo, F, and Ta.

[0022] It should be noted that if the vanadium dioxide layer is not doped, its phase transition critical temperature is generally 68℃.

[0023] Furthermore, the second electrode 112 surrounds the dielectric film DBR structure 107, and the material of the low refractive index dielectric layer is silicon dioxide.

[0024] This invention designs a vanadium dioxide layer as the high-refractive-index portion of the dielectric film DBR structure 107. The optical thickness of the vanadium dioxide layer is one-quarter wavelength. Vanadium dioxide has a high refractive index below its critical temperature (insulating phase). The low-refractive-index portion of the dielectric film DBR structure 107 can be made of silicon dioxide or other low-refractive-index oxide films. The optical thickness of the low-refractive-index dielectric layer is also one-quarter wavelength. The vanadium dioxide layer and the low-refractive-index dielectric layer are arranged alternately for multiple cycles. When the reflectivity of the dielectric film DBR structure 107 is >95%, it can provide sufficient reflectivity for the resonant cavity of the vertical-cavity surface-emitting laser, thereby achieving lasing.

[0025] In some embodiments, in the dielectric film DBR structure 107, the number of alternating vanadium dioxide layers and low refractive index dielectric layers is greater than 6.

[0026] Furthermore, the third electrode 113 is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the vanadium dioxide layer to switch between the insulating phase and the metallic phase, so as to realize the vertical cavity surface emission laser is turned on or off. The refractive index of the vanadium dioxide layer when it is in the insulating phase is greater than the refractive index of the vanadium dioxide layer when it is in the metallic phase. When the vertical cavity surface emission laser is turned on, the vanadium dioxide layer is in the insulating phase, and when the vertical cavity surface emission laser is turned off, the vanadium dioxide layer is in the metallic phase.

[0027] Furthermore, the refractive index of the vanadium dioxide layer when it is in an insulating phase is in the range of 2.5 to 3.5, and the refractive index of the vanadium dioxide layer when it is in a metallic phase is in the range of 0.5 to 1.5.

[0028] Furthermore, when the vertical cavity surface-emitting laser is turned on, the reflectivity of the dielectric film DBR structure 107 is greater than 95%.

[0029] Furthermore, when the temperature of the vanadium dioxide layer is higher than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide absorption layer is in a metallic phase; when the temperature of the vanadium dioxide layer is lower than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide layer is in an insulating phase.

[0030] Furthermore, the first electrode 111 serves as the negative electrode of the vertical-cavity surface-emitting laser (VCSEL), and the second electrode 112 serves as the positive electrode of the VCSEL. The first electrode 111 and the second electrode 112 provide electrical pumping for the VCSEL. The second electrode 112 serves as the negative electrode of the dielectric film DBR structure 107, and the third electrode 113 serves as the positive electrode of the dielectric film DBR structure 107. The second electrode 112 and the third electrode 113 are subjected to corresponding voltages to change the temperature of the vanadium dioxide layer.

[0031] Furthermore, when the vertical-cavity surface-emitting laser is turned on, the voltage applied to the first electrode 111 is less than the voltage applied to the second electrode 112, and the third electrode 112 can be applied with the same voltage as the second electrode 112; when the vertical-cavity surface-emitting laser is turned off, the voltage applied to the third electrode 113 is greater than the voltage applied to the second electrode 112.

[0032] Since the dielectric film DBR structure 107 is a high-resistivity region, even if the third electrode 112 is subjected to a third voltage, it will not affect the electric pumping of the vertical cavity surface-emitting laser.

[0033] The oxidation confinement layer 105 includes an oxidized portion and a non-oxidized portion, with the oxidized portion surrounding the non-oxidized portion, which serves as an oxidation pore.

[0034] In the vertical cavity surface-emitting laser provided by this utility model, the active layer 103 is an active region composed of multiple quantum well structures. The active layer 103 is used to generate the optical gain required to form laser light. The active layer 103, the first spacer layer 102, the second spacer layer 104, and the third spacer layer 106 together constitute the resonant cavity of the vertical cavity surface-emitting laser. The first spacer layer 102, the second spacer layer 104, and the third spacer layer 106 are used to adjust the cavity length. The first spacer layer 102, the second spacer layer 104, and the third spacer layer 106 are all spacer layers. The band gap of the spacer layer is larger than the band gap of the quantum well to confine the charge carriers.

[0035] In some embodiments, the oxide confinement layer 105 can be an AlGaAs material with a high aluminum content. The molar fraction of the Al content in the oxide confinement layer 105 before oxidation is greater than 0.98. The oxidized portion is formed by lateral oxidation using wet nitrogen oxidation. The oxidation rate can be controlled by adjusting parameters such as oxidation temperature, water vapor temperature, pressure, and flow rate. The lateral oxidation depth can be controlled by controlling the time. Finally, a non-oxidized portion with an unoxidized center and an oxidized portion around the perimeter are formed. The oxidized portion forms a high-resistance region, and the current injected into the laser will be restricted to only pass through the non-oxidized center.

[0036] In some embodiments, the vertical cavity surface-emitting laser further includes an insulating layer 108, which may be located on the surface of the remaining third spacer layer 106, excluding the second electrode 112 and the dielectric film DBR structure 107, away from the oxide confinement layer 105.

[0037] In some embodiments, the vertical-cavity surface-emitting laser (VCSEL) is a VCSEL with a center wavelength of 850 nm, and the substrate layer 100 is made of GaAs. The N-type DBR structure 101 is composed of alternating high-refractive-index N-type semiconductor layers and low-refractive-index N-type semiconductor layers arranged in 35-40 cycles, and the reflectivity of the N-type DBR structure 101 is >99.9%. The reflectivity of the dielectric film DBR structure 107 is lower than that of the N-type DBR structure 101, so that light is emitted from the top. The material of the first spacer layer 102 is lattice-matched with the material of the substrate layer 100, and the material of the first spacer layer 102 is AlGaAs. The active layer 103 is composed of alternating quantum well layers and barrier layers arranged in multiple cycles, the quantum well layer is made of GaAs, and the barrier layer is made of AlGaAs. x Ga 1-x As, x=0.2~0.4; the materials of the second spacer layer 104 and the third spacer layer 106 are lattice-matched with the material of the substrate layer 100. The material of the second spacer layer 104 is AlGaAs, the material of the third spacer layer 106 is AlGaAs, and the dopants of the second spacer layer 104 and the third spacer layer 106 are both C; the total optical thickness of the first spacer layer 102, the active layer 103, the second spacer layer 104, the oxide confinement layer 105, and the third spacer layer 106 is half a wavelength that is an integer multiple of 850nm, thereby satisfying the standing wave condition of the laser; the material of the insulating layer 108 can be SiO2 or Si3N4, and the thickness of the insulating layer 108 is in the range of 300nm~500nm; the materials of the first electrode 111 include Ti, Pt, and Au; the materials of the second electrode 112 include Au, Ge, and Ni, and the materials of the third electrode 113 include Au, Ge, and Ni.

[0038] In some embodiments, the vertical cavity surface-emitting laser provided by this invention can be fabricated using the following method, which includes: forming a first electrode 111, a substrate layer 100, an N-type DBR structure 101, a first spacer layer 102, an active layer 103, a second spacer layer 104, an oxide confinement layer 105, and a third spacer layer 106 stacked sequentially; forming a dielectric film DBR structure 107 and a second electrode 112, both of which are located on the surface of the third spacer layer 106 away from the oxide confinement layer 105, and the second electrode 112 is spaced apart from the dielectric film DBR structure 107, wherein the dielectric film DBR structure 107 is composed of alternating vanadium dioxide layers and low refractive index dielectric layers arranged in multiple cycles; and forming a third electrode 113, which is located on the top surface of the dielectric film DBR structure 107 away from the third spacer layer 106, and the third electrode 113 is arranged around the light exit hole.

[0039] Furthermore, vanadium dioxide layers and low-refractive-index dielectric layers are alternately grown using atomic layer deposition (ALD) or chemical vapor deposition (CVD) processes to form a dielectric film DBR structure 107. The vanadium dioxide layer formation process is highly compatible with mainstream VCSEL fabrication processes, which helps to avoid increasing the fabrication difficulty of vertical-cavity surface-emitting lasers.

[0040] In some embodiments, an N-type DBR structure 101 can be epitaxially grown on a substrate layer 100 using MOCVD (Metal-Organic Chemical Vapor Deposition). Then, a first spacer layer 102, an active layer 103, a second spacer layer 104, an initial oxide confinement layer 105, and a third spacer layer 106 are epitaxially grown sequentially on the N-type DBR structure 101. After the third spacer layer 106 is formed, the epitaxial growth portion is complete.

[0041] In some embodiments, after the epitaxial growth is completed, the initial oxidation confinement layer 105 is laterally oxidized using a wet nitrogen oxidation device to form the oxidation confinement layer 105. The oxidation rate is controlled by adjusting parameters such as oxidation temperature, water vapor temperature, pressure, and flow rate, and the lateral oxidation depth is controlled by controlling the time. Finally, a hole region with the center not oxidized is formed, and the oxidized part forms a high-resistance region. The current injected into the laser will be restricted to only passing through the hole region with the center not oxidized.

[0042] In some embodiments, after forming the oxide confinement layer 105, an initial dielectric film DBR structure can be formed on the third spacer layer 106 using a PECVD (Plasma-Enhanced Chemical Vapor Deposition) device or an ALD (Atomic Layer Deposition) device. After forming the initial dielectric film DBR structure, photoresist coating, photolithography, development, and dry etching are performed to form the dielectric film DBR structure 107. The etching gas for dry etching can be a typical Cl2-based or F-based reactive gas.

[0043] In some embodiments, after forming the dielectric film DBR structure 107, an insulating layer 108 can be deposited on the sample surface using a PECVD device. The sample is then subjected to a second photolithography process, followed by spin coating, photolithography, development, and dry etching to expose the areas forming the second electrode 112, the third electrode 113, and the light exit aperture. The etching gases used for dry etching of the insulating layer 108 can be typical CF4 and O2. Subsequently, the sample undergoes a third photolithography process, followed by spin coating, photolithography, and development to form a photoresist layer with deposition windows. The second electrode 112 and the third electrode 113 are then deposited using electron beam evaporation or magnetron sputtering. The deposited sample is then subjected to a stripping process in acetone solution to remove the electrode material at the light exit aperture. The substrate is then thinned and polished, and the first electrode 111 is deposited using electron beam evaporation or magnetron sputtering.

[0044] The vertical-cavity surface-emitting laser (VCSEL) provided by this invention uses a third electrode 113 to energize the dielectric film DBR structure 107 on the light-emitting side, increasing the operating temperature of the DBR structure 107 and causing a phase transition in vanadium dioxide. After the phase transition, the absorption coefficient of vanadium dioxide increases, and its refractive index decreases, making the DBR structure 107 unable to provide sufficient reflectivity. At this point, the VCSEL is in a non-lasing state. By controlling the second electrode 112, the rapid switching function of the VCSEL can be achieved. The optical switching speed based on vanadium dioxide is very fast, reaching the 0.5ns~10ns level, and has extremely low power consumption (less than 10fJ / bit), meeting the technical requirements of high-speed optical switching. The vanadium dioxide can be prepared using conventional thin-film deposition growth methods such as chemical vapor deposition or atomic layer deposition, which are highly compatible with the traditional VCSEL fabrication process. In summary, this invention achieves a high degree of integration between the laser source and the optical switch, reducing the complexity of system construction, shrinking the structural volume, and lowering the system setup cost.

[0045] It should be understood that the various forms of processes shown above can be used, with steps reordered, added, or deleted. For example, the steps described in this utility model disclosure can be executed in parallel, sequentially, or in different orders, as long as the desired result of the technical solution disclosed in this utility model can be achieved, and this is not limited herein.

[0046] The specific embodiments described above do not constitute a limitation on the scope of protection of this utility model. Those skilled in the art should understand that various modifications, combinations, sub-combinations, and substitutions can be made according to design requirements and other factors. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this utility model should be included within the scope of protection of this utility model.

Claims

1. A vertical-cavity surface-emitting laser, characterized in that, include: The first electrode, substrate layer, N-type DBR structure, first spacer layer, active layer, second spacer layer, oxide confinement layer and third spacer layer are stacked sequentially. The dielectric film DBR structure and the second electrode are both located on the surface of the third spacer layer away from the oxide confinement layer, and the second electrode is spaced apart from the dielectric film DBR structure. The dielectric film DBR structure is composed of multiple cycles of alternating vanadium dioxide layers and low refractive index dielectric layers. The third electrode is located on the top surface of the dielectric film DBR structure away from the third spacer layer, and is arranged around the light exit hole. The third electrode is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the vertical cavity surface emission laser to turn on or off.

2. The vertical-cavity surface-emitting laser according to claim 1, characterized in that, The second electrode surrounds the dielectric film DBR structure, and the material of the low refractive index dielectric layer is silicon dioxide.

3. The vertical-cavity surface-emitting laser according to claim 1, characterized in that, The third electrode is used to apply a corresponding voltage to change the temperature of the vanadium dioxide layer, thereby controlling the vanadium dioxide layer to switch between the insulating phase and the metallic phase, so as to realize the vertical cavity surface emission laser is turned on or off. The refractive index of the vanadium dioxide layer when it is in the insulating phase is greater than the refractive index of the vanadium dioxide layer when it is in the metallic phase. When the vertical cavity surface emission laser is turned on, the vanadium dioxide layer is in the insulating phase, and when the vertical cavity surface emission laser is turned off, the vanadium dioxide layer is in the metallic phase.

4. The vertical-cavity surface-emitting laser according to claim 3, characterized in that, The refractive index of the vanadium dioxide layer is in the range of 2.5 to 3.5 when it is in the insulating phase, and in the range of 0.5 to 1.5 when it is in the metallic phase.

5. The vertical-cavity surface-emitting laser according to claim 4, characterized in that, When the vertical cavity surface-emitting laser is turned on, the reflectivity of the dielectric film DBR structure is greater than 95%.

6. The vertical-cavity surface-emitting laser according to claim 3, characterized in that, When the temperature of the vanadium dioxide layer is higher than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide absorption layer is in a metallic phase; when the temperature of the vanadium dioxide layer is lower than the critical phase transition temperature of vanadium dioxide, the vanadium dioxide layer is in an insulating phase.

7. The vertical-cavity surface-emitting laser according to claim 1, characterized in that, The first electrode serves as the negative electrode of the vertical-cavity surface-emitting laser (VCSEL), and the second electrode serves as the positive electrode. The first and second electrodes provide electric pumping for the VCSEL. The second electrode serves as the negative electrode of the dielectric film DBR structure, and the third electrode serves as the positive electrode of the dielectric film DBR structure. The second and third electrodes are subjected to corresponding voltages to change the temperature of the vanadium dioxide layer.

8. The vertical-cavity surface-emitting laser according to claim 7, characterized in that, When the vertical-cavity surface-emitting laser is turned on, the voltage applied to the first electrode is less than the voltage applied to the second electrode, and the third electrode is applied with the same voltage as the second electrode; when the vertical-cavity surface-emitting laser is turned off, the voltage applied to the third electrode is greater than the voltage applied to the second electrode.