Packaging structure

By directly pressing together porous gaskets, the corrosion problem of metal gaskets caused by etching in existing technologies is solved, achieving stability and simplified processing, reducing the height of the packaging structure and improving product yield.

CN224988030UActive Publication Date: 2026-11-17ADVANCED SEMICON ENG INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522329390.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-03
Publication Date
2026-11-17
Estimated Expiration
2035-11-03

AI Technical Summary

Technical Problem

In the prior art, when the seed layer on the upper surface of the silicon layer is etched and removed from the packaging structure, the metal pads are corroded, affecting the surface flatness, resulting in unstable connections and increasing the number of process steps.

Method used

The connection is made by directly pressing together porous gaskets. The first porous gasket and the second porous gasket are set opposite each other. The porosity is between 40% and 60%. The compression ratio after pressing is between 10% and 50%. The gasket is made of nickel material to protect the underlying metal layer, simplifying the process and improving stability.

Benefits of technology

By using porous gaskets for lamination, the processing difficulty is reduced, the connection stability is improved, the package structure height is reduced, and the underlying metal layer is protected during the etching process, thereby improving product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224988030U_ABST
    Figure CN224988030U_ABST
Patent Text Reader

Abstract

This application provides a packaging structure including a first metal layer; a second metal layer located above the first metal layer; a first porous gasket disposed on the upper surface of the first metal layer, the first porous gasket having holes; and a second porous gasket disposed on the lower surface of the second metal layer, the second porous gasket having holes. The first and second porous gaskets are disposed opposite to each other, and each first porous gasket is press-fitted to one second porous gasket. The advantages of this application are: direct press-fitting of the porous gaskets eliminates the need for additional solder or adhesive between the gaskets, reducing the processing difficulty of the gasket connection, improving the stability of the gasket connection, and simplifying the packaging structure; the height of the porous gaskets is compressed after press-fitting, reducing the distance between the upper and lower metal layers, thereby reducing the height of the packaging structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor packaging, and more specifically, to a packaging structure. Background Technology

[0002] Hybrid bonding, also known as direct copper-copper bonding or low-temperature bonding, is an advanced wafer-to-wafer or chip-to-wafer bonding technology. It enables simultaneous electrical interconnection between metals (usually copper) and mechanical bonding between dielectric layers in the same process step.

[0003] Figure 1 A schematic diagram of a prior art packaging structure is shown. For example... Figure 1 As shown, the prior art packaging structure includes a first component 900a and a second component 900b disposed opposite to each other. The second component 900b is located above the first component 900a and the first component 900a and the second component 900b are connected by solder 906. The first component 900a and the second component 900b respectively include a silicon layer 901, a metal layer 902, a metal pad 903 and a seed layer 904. The metal layer 902 is disposed on the silicon layer 901 and is connected to the silicon layer 901 through the seed layer 904. The metal pad 903 is disposed on the metal layer 902. The metal pad 903 of the first component 900a and the metal pad 903 of the second component 900b are connected to each other by solder 906. The first component 900a and the second component 900b can be covered by a molding layer (not shown in the figure).

[0004] Figure 2 As shown Figure 1 The diagram shows a manufacturing process diagram of the first / second component in a prior art packaging structure. (See attached diagram.) Figure 2 As shown, the manufacturing process of the existing packaging structure includes multiple steps: Step 9001: A metal layer 902 is disposed on a silicon layer 901. The metal layer 902 is connected to the silicon layer 901 through a seed layer 904. A molding compound 905 is disposed on the seed layer 904 and the metal layer 902. A portion of the upper surface of the metal layer 902 is exposed from the molding compound 905. The seed layer 904 is made of titanium / copper material, and the metal layer 902 is made of copper. Step 9002: A metal gasket 903 is disposed on the exposed upper surface of the metal layer 902; wherein the metal gasket 903 is made of copper or a copper-zinc alloy; and Step 9003: Remove the molding material 905 and remove the seed layer 904 exposed on the upper surface of the silicon layer 901 by etching.

[0005] The disadvantages of existing packaging structures are: Figure 3As shown, when the seed layer 904 exposed on the upper surface of the silicon layer 901 is removed by etching, the metal pad 903 will be corroded, affecting the flatness of the surface of the metal pad 903. Therefore, solder 906 is needed to connect the metal pad 903 of the first component 900a and the metal pad 903 of the second component 900b. This increases the number of process steps and is not conducive to the stability of the pad connection.

[0006] In summary, there is a need in the art to provide a packaging structure that can overcome the shortcomings of the prior art. Utility Model Content

[0007] This application provides a packaging structure that can solve the problems of the prior art. The objective of this application is achieved through the following technical solution.

[0008] One embodiment of this application provides a packaging structure including a first metal layer; a second metal layer located above the first metal layer; a first porous gasket disposed on the upper surface of the first metal layer, the first porous gasket having holes; and a second porous gasket disposed on the lower surface of the second metal layer, the second porous gasket having holes; wherein the first porous gasket and the second porous gasket are disposed opposite to each other, and each first porous gasket is press-fitted to one second porous gasket.

[0009] In some alternative embodiments, the encapsulation structure provided according to one of the above embodiments of this application, wherein the porosity of the first porous gasket is greater than or equal to 40% and less than or equal to 60%.

[0010] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the porosity of the second porous gasket is greater than or equal to 40% and less than or equal to 60%.

[0011] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application, wherein the compression ratio of the first porous gasket and the second porous gasket after being pressed together is between 10% and 50% relative to before being pressed together.

[0012] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application above, wherein the first metal layer and the second metal layer are electrically connected through a first porous pad and a second porous pad.

[0013] In some optional embodiments, the packaging structure provided according to one embodiment of the present application further includes a first silicon layer and a second silicon layer, wherein the first silicon layer is disposed below the first metal layer and the second silicon layer is disposed above the second metal layer.

[0014] In some optional embodiments, the packaging structure provided according to one embodiment of the present application further includes a first seed layer and a second seed layer. The first seed layer is located between the first silicon layer and the first metal layer, and the first silicon layer is fixedly connected to the first metal layer through the first seed layer. The second seed layer is located between the second silicon layer and the second metal layer, and the second silicon layer is fixedly connected to the second metal layer through the second seed layer.

[0015] In some alternative embodiments, according to the packaging structure provided by one embodiment of the present application, the edge of the first seed layer is recessed relative to the edge of the first metal layer, and the edge of the second seed layer is recessed relative to the edge of the second metal layer.

[0016] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the hardness of the first porous gasket is less than the hardness of the first metal layer.

[0017] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the hardness of the second porous gasket is less than the hardness of the second metal layer.

[0018] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application above, wherein the upper surface of the first metal layer is a smooth plane and the lower surface of the second metal layer is a smooth plane.

[0019] The advantages of the packaging structure according to the embodiments of this application are as follows: the porous gaskets are directly pressed together, eliminating the need for additional solder or adhesive between the gaskets, reducing the processing difficulty of the gasket connection, improving the stability of the gasket connection, and simplifying the packaging structure; the height of the porous gaskets is compressed after pressing together, reducing the distance between the upper and lower metal layers, thereby reducing the height of the packaging structure; the gaskets made of nickel material can protect the underlying metal layer during etching, improving product yield. Attached Figure Description

[0020] Other features, objects, and advantages of this application will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings.

[0021] Figure 1 A schematic diagram of a prior art packaging structure is shown; Figure 2 As shown Figure 1 The diagram shows a manufacturing process diagram of the first / second component in a prior art packaging structure; Figure 3 As shown Figure 1 The diagram shows a comparison of the gasket of a prior art packaging structure before and after etching. Figure 4 A schematic diagram of a packaging structure according to an embodiment of this application is shown; Figure 5 As shown Figure 4 An enlarged schematic diagram of the portion marked A in the packaging structure according to an embodiment of this application is shown; Figure 6 As shown Figure 4 The diagram shown is a manufacturing process diagram of a packaging structure according to an embodiment of this application; Figure 7 A schematic diagram of an etching process test for a gasket made of existing materials is shown; Figure 8 A schematic diagram of an etching process test of a gasket of an encapsulation structure according to an embodiment of this application is shown; Figure 9 An enlarged schematic diagram of porous gaskets with different porosities is shown.

[0022] Labels and component names: 101 - First metal layer, 102 - First porous gasket, 102a - Hole, 103 - First silicon layer, 104 - First seed layer, 201 - Second metal layer, 202 - Second porous gasket, 202a - Hole, 203 - Second silicon layer, 204 - Second seed layer, 300a - First component, 300b - Second component, 301 - Silicon wafer, 302 - Copper layer, 303 - Gasket, 303a - Hole, 304 - Seed layer, 305 - Molding material, 401 - Silicon layer, 404 - Metal layer, 404a - Titanium-copper metal layer, 404b - Copper layer, 501 - Silicon layer, 504 - Metal layer, 504a - Titanium-copper metal layer, 504b - Nickel layer, 900a - First component, 900b - Second component, 901 - Silicon layer, 902 - Metal layer, 903 - Metal pad, 904 - Seed layer, 905 - Molding material, 906 - Solder. Detailed Implementation

[0023] The specific embodiments of this application are described below with reference to the accompanying drawings and examples. Through the content described in this specification, those skilled in the art can clearly and completely understand the technical solution, the technical problem solved, and the resulting technical effects of this application. It is understood that the specific embodiments described herein are only for explaining this application and not for limiting it. Furthermore, for ease of description, only the parts related to this application are shown in the accompanying drawings.

[0024] It should be readily understood that the meanings of “on,” “above,” and “on top of” in this application should be interpreted in the broadest sense, such that “on” means not only “directly on something,” but also “on something” including intermediate components or layers existing between the two.

[0025] Furthermore, for ease of description, spatial relative terms such as “below,” “under,” “lower,” “above,” and “upper” may be used herein to describe the relationship of one element or component to another element or component shown in the accompanying drawings. In addition to the orientations described in the figures, spatial relative terms are also intended to cover different orientations of the device during use or operation. The device may be oriented in other ways (rotated 90° or otherwise), and the spatial relative descriptive terms used herein may be interpreted accordingly.

[0026] It should be noted that the structures, proportions, sizes, etc., depicted in the accompanying drawings are only for illustrative purposes to aid those skilled in the art in understanding and reading the content described in the specification, and are not intended to limit the scope of this application. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in proportions, or adjustments to size, without affecting the effects and objectives of this application, should still fall within the scope of the technical content disclosed in this application. Furthermore, the terms such as "above," "first," "second," and "a" used in this specification are merely for clarity of description and are not intended to limit the scope of this application. Changes or adjustments to their relative relationships, without substantially altering the technical content, should also be considered within the scope of this application's implementation.

[0027] As used herein, the term "layer" refers to a portion of material comprising a region of a certain thickness. A layer may extend over the entirety of an underlying or upper layer structure, or may have a extent smaller than that of the underlying or upper layer structure. Furthermore, a layer may be a region of a homogeneous or heterogeneous continuous structure with a thickness less than that of the continuous structure. For example, a layer may be located between the top and bottom surfaces of a continuous structure, or between any pair of horizontal planes therebetween. A layer may extend horizontally, vertically, and / or along a tapered surface. A layer may be a single layer, which may include one or more layers, and / or may have one or more layers on, above, and / or below it. A single layer may include multiple layers. For example, a semiconductor layer may include one or more doped or undoped semiconductor layers, and may have the same or different materials.

[0028] The term "molding sealant" or "molding seal layer" in this article may include epoxy resin, filler, catalyst, pigment, release agent, flame retardant, coupling agent, hardener, low stress absorber, adhesion promoter, ion trapping agent, etc.

[0029] Furthermore, where there is no conflict, the embodiments and features described in this application can be combined with each other. This application will now be described in detail with reference to the accompanying drawings and embodiments.

[0030] Figure 4 A schematic diagram of a packaging structure according to an embodiment of this application is shown. Figure 5 As shown Figure 4 The diagram shows an enlarged view of portion A, representing a packaging structure according to an embodiment of this application. Figure 4 and Figure 5 As shown, the encapsulation structure includes a first metal layer 101; a second metal layer 201 located above the first metal layer 101; a first porous gasket 102 disposed on the upper surface of the first metal layer 101, the first porous gasket 102 having holes 102a; and a second porous gasket 202 disposed on the lower surface of the second metal layer 201, the second porous gasket 202 having holes 202a; wherein the first porous gasket 102 and the second porous gasket 202 are disposed opposite to each other, and each first porous gasket 102 is press-fitted to one second porous gasket 202.

[0031] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the porous structure enables the first porous gasket 102 and the second porous gasket 202 to have a certain degree of compressibility and good bonding ability, thereby enabling the first porous gasket 102 and the second porous gasket 202 to be pressed together and reducing the height of the first porous gasket 102 and the second porous gasket 202 after being pressed together.

[0032] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above has a pore size range of 1-100 nanometers for the holes 102a on the first porous pad 102 and the holes 202a on the second porous pad 202.

[0033] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the porosity of the first porous gasket 102 is greater than or equal to 40% and less than or equal to 60%.

[0034] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the porosity of the second porous gasket 202 is greater than or equal to 40% and less than or equal to 60%.

[0035] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application, wherein the compression ratio of the first porous gasket 102 and the second porous gasket 202 after being pressed together is between 10% and 50% relative to before being pressed together.

[0036] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application above, wherein the first metal layer 101 and the second metal layer 201 are electrically connected through a first porous pad 102 and a second porous pad 202.

[0037] In some optional embodiments, the packaging structure provided according to one embodiment of the present application further includes a first silicon layer 103 and a second silicon layer 203, wherein the first silicon layer 103 is disposed below the first metal layer 101 and the second silicon layer 203 is disposed above the second metal layer 201.

[0038] In some optional embodiments, the packaging structure provided according to one embodiment of the present application further includes a first seed layer 104 and a second seed layer 204. The first seed layer 104 is located between the first silicon layer 103 and the first metal layer 101, and the first silicon layer 103 is fixedly connected to the first metal layer 101 through the first seed layer 104. The second seed layer 204 is located between the second silicon layer 203 and the second metal layer 201, and the second silicon layer 203 is fixedly connected to the second metal layer 201 through the second seed layer 204.

[0039] In some alternative embodiments, according to the packaging structure provided by one embodiment of the present application, the edge of the first seed layer 104 is recessed relative to the edge of the first metal layer 101, and the edge of the second seed layer 204 is recessed relative to the edge of the second metal layer 201.

[0040] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the hardness of the first porous gasket 102 is less than the hardness of the first metal layer 101.

[0041] In some alternative embodiments, the encapsulation structure provided according to one embodiment of the present application above, wherein the hardness of the second porous gasket 202 is less than the hardness of the second metal layer 201.

[0042] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application above, wherein the upper surface of the first metal layer 101 is a smooth plane and the lower surface of the second metal layer 201 is a smooth plane.

[0043] In some alternative embodiments, the packaging structure provided according to one embodiment of the present application above, wherein the first porous gasket 102 and the second porous gasket 202 are made of nickel.

[0044] In some alternative embodiments, the packaging structure provided according to one embodiment of this application above, wherein the materials of the first metal layer 101 and the second metal layer 201 are copper.

[0045] In some alternative embodiments, the packaging structure provided according to one embodiment of this application above, wherein the first seed layer 104 and the second seed layer 204 are made of copper and / or titanium.

[0046] In some optional embodiments, the packaging structure provided according to one embodiment of the present application further includes a molding layer (not shown in the figure), which fills between the first silicon layer 103 and the second silicon layer 203 and covers the first metal layer 101, the second metal layer 201, the first porous gasket 102 and the second porous gasket 202.

[0047] Figure 6 As shown Figure 4 The diagram shown illustrates the manufacturing process of a packaging structure according to an embodiment of this application. Figure 6 As shown, the manufacturing process of the packaged components includes multiple steps: Step 1001: A metal layer 302 is disposed on a silicon layer 301. The metal layer 302 is connected to the silicon layer 301 through a seed layer 304. A molding compound 305 is disposed on the seed layer 304 and the metal layer 302. A portion of the upper surface of the metal layer 302 is exposed from the molding compound 305. The seed layer 304 is made of titanium / copper material, and the metal layer 302 is made of copper. Step 1002: A metal gasket 303 is provided on the exposed upper surface of the metal layer 302; wherein the metal gasket 303 is made of copper-nickel alloy material; Step 1003: Remove the molding material 305 and remove the seed layer 304 exposed on the upper surface of the silicon layer 301 by etching, thereby obtaining the first component 300a; wherein, the metal pad 303 made of copper-nickel alloy material will form a nanoporous nickel (NP-Ni, Nanoporous-Ni) structure after etching, that is, the metal pad 303 will form a hole 303a after etching. Step 1004: A second component 300b is disposed above the first component 300a; wherein the second component 300b is manufactured using the same and similar steps as those described in steps 1001 to 1003, and the metal gasket 303 of the first component 300a is aligned with the metal gasket 303 of the second component 300b; and Step 1005: Connect the metal gasket 303 of the first component 300a to the metal gasket 303 of the second component 300b by pressing.

[0048] Figure 7 A schematic diagram of an etching process test for a gasket made of existing materials is shown. (Example) Figure 7 As shown, the first test layer 404 includes a copper layer 404a and a titanium / copper material layer 404b. After etching, the copper layer 404a will be completely removed, and the copper material in the titanium / copper material layer 404b will also be removed.

[0049] Figure 8 A schematic diagram of an etching process test of a gasket in a packaging structure according to an embodiment of this application is shown. Figure 8 As shown, the second test layer 504 includes a nickel layer 504a and a titanium / copper material layer 504b. After etching, the nickel layer 504a remains intact, while the titanium / copper material layer 504b located beneath the nickel layer 504a is also protected from corrosion by the nickel layer 504a. It can be seen that, compared to copper, nickel can avoid corrosion from the etching process and protect the metal beneath it.

[0050] Figure 9 An enlarged schematic diagram of porous gaskets with different porosities is shown. For example... Figure 9 As shown, metal gaskets made of copper-nickel alloy are etched to form porous gaskets with pores. The porosity of the porous gaskets varies depending on the copper-nickel ratio. The porous gasket labeled B1 has a porosity of approximately 14%; the porous gasket labeled B2 has a porosity of approximately 30%; the porous gasket labeled B3 has a porosity of approximately 38%; and the porous gasket labeled B4 has a porosity of approximately 50%.

[0051] The advantages of the packaging structure according to the embodiments of this application are as follows: the porous gaskets are directly pressed together, eliminating the need for additional solder or adhesive between the gaskets, reducing the processing difficulty of the gasket connection, improving the stability of the gasket connection, and simplifying the packaging structure; the height of the porous gaskets is compressed after pressing together, reducing the distance between the upper and lower metal layers, thereby reducing the height of the packaging structure; the gaskets made of nickel material can protect the underlying metal layer during etching, improving product yield.

[0052] Although this application has been described and illustrated with reference to specific embodiments thereof, such descriptions and illustrations are not intended to limit the application. It will be readily understood by those skilled in the art that various changes can be made and equivalent elements can be substituted within embodiments without departing from the scope of protection of this application as defined by the claims. Differences may exist between the technical representation in this application and actual equipment due to variables in the manufacturing process, etc. Other embodiments of this application may exist that are not specifically described. The specification and illustrations should be considered illustrative rather than restrictive, and modifications can be made to suit the purpose and spirit of this application, all of which are within the scope of the claims. While the methods disclosed herein have been described with reference to specific operations performed in a particular order, it should be understood that these operations can be rearranged, subdivided, or arranged to form equivalent methods without departing from the teachings of this application. Therefore, unless specifically indicated herein, the order and grouping of operations do not limit the application.

Claims

1. A package structure, characterized by, include: First metal layer; A second metal layer is located above the first metal layer; A first porous gasket is disposed on the upper surface of the first metal layer, and the first porous gasket has holes. A second porous gasket is disposed on the lower surface of the second metal layer, and the second porous gasket has holes. The first porous gasket and the second porous gasket are arranged opposite to each other, and each of the first porous gaskets is pressed and connected to one of the second porous gaskets.

2. The package structure of claim 1, wherein, The porosity of the first porous gasket is greater than or equal to 40% and less than or equal to 60%.

3. The package structure of claim 1, wherein, The porosity of the second porous gasket is greater than or equal to 40% and less than or equal to 60%.

4. The package structure of claim 1, wherein, The compression ratio of the first porous gasket and the second porous gasket after being pressed together is between 10% and 50% compared to before the pressing.

5. The packaging structure according to claim 1, characterized in that, The first metal layer and the second metal layer are electrically connected through the first porous gasket and the second porous gasket.

6. The packaging structure according to claim 1, characterized in that, The packaging structure further includes a first silicon layer and a second silicon layer, wherein the first silicon layer is disposed below the first metal layer and the second silicon layer is disposed above the second metal layer.

7. The packaging structure according to claim 6, characterized in that, The packaging structure further includes a first seed layer and a second seed layer. The first seed layer is located between the first silicon layer and the first metal layer, and the first silicon layer is fixedly connected to the first metal layer through the first seed layer. The second seed layer is located between the second silicon layer and the second metal layer, and the second silicon layer is fixedly connected to the second metal layer through the second seed layer.

8. The packaging structure according to claim 7, characterized in that, The edge of the first seed layer is recessed relative to the edge of the first metal layer, and the edge of the second seed layer is recessed relative to the edge of the second metal layer.

9. The packaging structure according to claim 1, characterized in that, The hardness of the first porous gasket is less than the hardness of the first metal layer, and the hardness of the second porous gasket is less than the hardness of the second metal layer.