Semiconductor device and method

The gate structure with varying widths and materials in semiconductor devices addresses the challenge of reduced critical dimensions, achieving improved process control and resistance adjustment for enhanced manufacturing efficiency.

DE102017102012B4Active Publication Date: 2024-10-24TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102017102012
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2017-01-19
Filing Date
2017-02-02
Publication Date
2024-10-24
Estimated Expiration
2037-02-02

AI Technical Summary

Technical Problem

The challenge in semiconductor manufacturing is to achieve reduced critical dimensions in semiconductor devices while maintaining an enlarged process window and better resistance adjustment.

Method used

The solution involves a gate structure with specific layer configurations and manufacturing processes, including a gate stack with varying widths and materials, such as high-k dielectric materials and metal layers, to enhance process control and resistance.

Benefits of technology

This approach allows for reduced critical dimensions with improved process control and adjusted resistance, enhancing manufacturing yield and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Semiconductor device (100), comprising: a gate structure (205) over a substrate (107) having a first width (W1), wherein the gate structure (205) has a layer of a first metal material (215) and a layer of a second metal material (217) extending over the layer of the first metal material (215); a conductive contact (501) arranged above the gate structure (205) and having a lower section which physically contacts a top surface extending parallel to a top surface of the substrate (107) and a side wall of the second metal material (217) extending perpendicular to the top surface, as well as a top surface of the first metal material (215), wherein the lower section has a second width (W2) wherein the second width (W2) is less than or equal to the first width (W1).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a semiconductor device, comprising: a gate structure having a first width, wherein the gate structure comprises a layer of a first metal material and a layer of a second metal material extending over the layer of the first metal material; a cap layer over the gate structure contacting the layer of the first metal material and the layer of the second metal material; and a conductive contact arranged over the gate structure, wherein the conductive contact has a lower portion on an upper surface of the gate structure, the lower portion having a second width, wherein the second width is smaller than or approximately equal to the first width. The invention further relates to methods for manufacturing a semiconductor device. A semiconductor device is known from US 2016 / 0190120 A1.Similar devices are also known from the documents US 2016 / 0 190 287 A1, DE 11 2013 005 871 T5 or US 2015 / 0 076 624 A1. STATE OF THE ART

[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor material layers over a semiconductor substrate, and then patterning the various material layers using lithography to form circuit components and elements thereon.

[0003] The semiconductor industry is constantly improving the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by continuously reducing the minimum feature size, allowing more components to be integrated into a given area. However, with the reduction of the smallest feature sizes, additional problems emerge that must be addressed. BRIEF DESCRIPTION OF THE DRAWINGS

[0004] Aspects of the present disclosure are best understood from the following detailed description when read in conjunction with the accompanying figures. It should be noted that, in accordance with standard industry practice, various features are not drawn to scale. Rather, the dimensions of the various features may be arbitrarily exaggerated or reduced for clarity of discussion. Fig. 1 shows steps in a process for forming a FinFET device according to some embodiments. Fig. 2 shows a formation of source / drain regions according to some embodiments. Fig. 3 shows a cross section of Fig. 2 according to some embodiments. Fig. 4 shows forming an opening according to some embodiments. Fig. 5 shows forming a first contact with the gate electrode according to some embodiments. Fig. 6A to 6D show different shapes of the gate electrode according to some embodiments. Fig. 7A to 7D illustrate forming a seam according to some embodiments. Fig. 8A to 8D illustrate additional embodiments of the shape of the gate electrode according to some embodiments. Fig. 9A to 9D illustrate forming a seam according to some embodiments. DETAILED DESCRIPTION

[0005] The following disclosure provides many different embodiments, or examples, for implementing various features of the invention. Specific examples of components and arrangements are described below to simplify the present disclosure. These are, of course, merely examples and are not intended to be limiting. For example, in the following description, forming a first feature over or on top of a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features may be formed between the first and second features such that the first and second features may not be in direct contact. Additionally, the present disclosure may repeat reference numbers and / or letters in the various examples.This repetition is for the purpose of simplicity and clarity and does not, in itself, prescribe any relationship between the various embodiments and / or configurations discussed.

[0006] In addition, terms relating to spatial relativity, such as "beneath," "under," "lower," "above," "upper," and the like, may be used herein for ease of discussion to describe the relationship of one element or feature to another element or feature(s) as illustrated in the figures. The terms relating to spatial relativity are intended to encompass various orientations of the device being used or operated in addition to the orientation illustrated in the figures. The device may be oriented in a different manner (rotated 90 degrees or oriented differently), and the terms relating to spatial relativity used herein may be equally construed accordingly.

[0007] With reference to Fig. Figure 1 illustrates a perspective view of a semiconductor device 100, such as a FinFET device. In one embodiment, the semiconductor device 100 includes a substrate 101 with first trenches 103 formed therein. The substrate 101 may be a silicon substrate, although other substrates, such as semiconductor on an insulator (SOI), stress SOI, and silicon germanium on an insulator, could be used. The substrate 101 may be a p-type semiconductor, although in other embodiments, it could be an n-type semiconductor.

[0008] The first trenches 103 may be formed as an initial step in the later formation of first isolation regions 105. The first trenches 103 may be formed using a masking layer (not shown separately in Fig. 1) using a suitable etching process. For example, the masking layer may be a hard mask comprising silicon nitride formed using a process such as chemical vapor deposition (CVD), although other materials such as oxides, oxynitrides, silicon carbide, combinations of these, or the like, and other processes such as plasma-enhanced chemical vapor deposition (PECVD), low-pressure chemical vapor deposition (LPCVD), or even silicon oxide formation followed by nitriding may be used. After it has been formed, the masking layer may be patterned using a suitable photolithographic process to expose those portions of the substrate 101 that are removed to form the first trenches 103.

[0009] However, as one skilled in the art will appreciate, the processes and materials described above for forming the masking layer are not the only method that may be used to protect portions of the substrate 101 while exposing other portions of the substrate 101 for the formation of the first trenches 103. Any suitable process, such as a patterned and developed photoresist, may be used to expose portions of the substrate 101 that are to be removed in order to form the first trenches 103. All such methods are intended to be fully encompassed within the scope of the present embodiments.

[0010] After a masking layer is formed and patterned, the first trenches 103 are formed in the substrate 101. The exposed substrate 101 may be removed using a suitable process, such as reactive ion etching (RIE), to form the first trenches 103 in the substrate 101, although any suitable process may be used. In one embodiment, the first trenches 103 may be formed to have a first depth of less than approximately 500 nm from the surface of the substrate 101, such as approximately 250 nm.

[0011] However, as one skilled in the art will appreciate, the above-described process for forming the first trenches 103 represents only one possible process and is not intended to be the only embodiment. Rather, any suitable process capable of forming the first trenches 103 may be used, and any suitable process including any number of masking and removal steps may be used.

[0012] In addition to forming the first trenches 103, the masking and etching process also forms fins 107 from those portions of the substrate 101 that were not removed. For simplicity, the fins 107 have been illustrated in the figures as being separated from the substrate 101 with a dashed line, although a physical marking of the separation may or may not be present. These fins 107 can be used, as discussed below, to form the channel region of multi-gate FinFET transistors. Although Fig. 1 illustrates only three fins 107 formed by the substrate 101, any number of fins 107 may be used.

[0013] The fins 107 may be formed to have a width of between approximately 5 nm and approximately 80 nm, such as approximately 30 nm, at the surface of the substrate 101. Furthermore, the fins 107 may be spaced apart from each other by a distance of between approximately 10 nm and approximately 100 nm, such as 50 nm. By spacing the fins 107 in this way, the fins 107 may each form a separate channel region while still being close enough to share a common gate (discussed further below).

[0014] After the first trenches 103 and the fins 107 have been formed, the first trenches 103 may be filled with a dielectric material, and the dielectric material may be recessed within the first trenches 103 to form the first isolation regions 105. The dielectric material may be an oxide material, a high-density plasma (HDP) oxide, or the like. The dielectric material may be formed after an optional cleaning and lining of the first trenches 103 using either a chemical vapor deposition (CVD) process (e.g., the HARP process), a high-density plasma (CVD) process, or another suitable formation method as known in the art.

[0015] The first trenches 103 may be filled by overfilling the first trenches 103 and the substrate 101 with the dielectric material and then removing the excess material outside the trenches 103 and the fins 107 using a suitable process, such as chemical mechanical polishing (CMP), etching, a combination of these, or the like. In one embodiment, the removal process also removes any dielectric material disposed over the fins 107, such that the removal of the dielectric material exposes the surface of the fins 107 for further processing steps.

[0016] After the first trenches 103 have been filled with the dielectric material, the dielectric material may then be recessed away from the surface of the fins 107. The recessing may be performed to expose at least a portion of the sidewalls of the fins 107 adjacent to the top surface of the fins 107. The dielectric material may be recessed using a wet etch by immersing the top surface of the fins 107 in an etchant such as HF, although other etchants such as H2 and other methods such as reactive ion etching, dry etching with etchants such as NH3 / NF3, chemical oxide removal, or chemical dry cleaning may be used. The dielectric material may be recessed from the surface of the fins 107 to a distance of between approximately 5 nm and approximately 50 nm, such as approximately 40 nm.In addition, the knockout may also remove any remaining dielectric material disposed over the fins 107 to ensure that the fins 107 are exposed for further processing.

[0017] However, as one skilled in the art will appreciate, the steps described above may be merely a part of the overall process flow used to fill and recess the dielectric material. For example, lining steps, cleaning steps, annealing steps, gap-filling steps, combinations of these, and the like may also be used to form the first trenches 103 and fill them with the dielectric material. All of the possible process steps are intended to be fully within the scope of the present embodiment.

[0018] After the first isolation regions 105 have been formed, a dummy gate dielectric 109, a dummy gate electrode 111 over the dummy gate dielectric 109, and first spacers 113 over each of the fins 107 may be formed. In one embodiment, the dummy gate dielectric 109 may be formed by thermal oxidation, chemical vapor deposition, sputtering, or any other methods known in the art and used to form a gate dielectric. Depending on the technique for forming the gate dielectric, a thickness of the dummy gate dielectric 109 on the top surface of the fins 107 may be different from a thickness of the gate dielectric on the sidewall of the fins 107.

[0019] The dummy gate dielectric 109 may comprise a material such as silicon dioxide or silicon oxynitride having a thickness ranging from approximately 0.3 nm to approximately 10 nm, such as approximately 1 nm. The dummy gate dielectric 109 may be formed from a high-permittivity (high-k) material (e.g., having a relative dielectric constant greater than approximately 5), such as lanthanum oxide (La2O3), aluminum oxide (Al2O3), hafnium oxide (HfO2), hafnium oxynitride (HfON), or zirconium oxide (ZrO2), or combinations thereof, with an equivalent oxide thickness of approximately 0.05 nm to approximately 10 nm, such as approximately 1 nm or less. In addition, a combination of silicon dioxide, silicon oxynitride, and / or high-k materials may also be used for the dummy gate dielectric 109.

[0020] The dummy gate electrode 111 may comprise a conductive material and may be selected from a group including W, Al, Cu, AlCu, W, Ti, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, Ta, TaN, Co, Ni, combinations thereof, or the like. The dummy gate electrode 111 may be deposited using chemical vapor deposition (CVD), sputter deposition, or other techniques known in the art and used to deposit conductive materials. The thickness of the dummy gate electrode 111 may range from approximately 0.5 nm to approximately 20 nm. The top surface of the dummy gate electrode 111 may have a non-planar top surface and may be planarized prior to patterning the dummy gate electrode 111 or a gate etch. At this time, ions may or may not be introduced into the dummy gate electrode 111. Ions can be introduced, for example, using ion implantation techniques.

[0021] After the dummy gate dielectric 109 and the dummy gate electrode 111 have been formed, they may be patterned to form a series of stacks 115 above the fins 107. The stacks 115 define a plurality of channel regions arranged on each side of the fins 107 beneath the dummy gate dielectric 109. The stacks 115 may be formed by depositing and patterning a gate mask (not separately described in Fig. 1) may be formed on the dummy gate electrode 111, for example, using deposition and photolithography techniques known in the art. The gate mask may include conventionally used masking and sacrificial materials, such as, but not limited to, silicon oxide, silicon oxynitride, SiCON, SiC, SiOC, and / or silicon nitride, and may be deposited to a thickness of between approximately 0.5 nm and approximately 20 nm. The dummy gate electrode 111 and the dummy gate dielectric 109 may be etched using a dry etch process to form the patterned stacks 115.

[0022] After the stacks 115 have been structured, the first spacers 113 can be formed. The first spacers 113 can be formed on opposite sides of the stacks 115. The first spacers 113 are typically formed by depositing a spacer layer (not separately in Fig. 1) on the previously formed structure. The spacer layer may comprise SiN, oxynitride, SiC, SiON, SiOCN, SiOC, oxide, and the like, and may be formed using methods used to form such a layer, such as chemical vapor deposition (CVD), plasma-enhanced CVD, sputtering, and other methods known in the art. The spacer layer may comprise a different material with different etch characteristics or the same material as the dielectric material within the first isolation regions 105. The first spacers 113 may then be patterned, such as by one or more etches, to remove the spacer layer from the horizontal surfaces of the structure to form the first spacers 113.

[0023] In one embodiment, the first spacers 113 may be formed to have a first thickness T1 of between about 0.5 nm and about 50 nm. Furthermore, after the first spacers 113 are formed, a first spacer 113 adjacent to one stack 115 may be separated from a first spacer 113 adjacent to another stack 115 by a first distance D1 of between about 10 nm and about 1000 nm, such as about 20 nm. However, any suitable thicknesses and distances may be used.

[0024] Fig. 2 to 3 show a removal of the fins 107 from those areas which are not protected by the stacks 115 and the first spacers 113, and a re-growth of source / drain regions 201 (where Fig. 3 a cross-sectional view of Fig. 2 along line BB'). The removal of the fins 107 from those areas not protected by the stacks 115 and the first spacers 113 may be performed by reactive ion etching (RIE) using the stacks 115 and the first spacers 113 as hard masks, or by any other suitable removal processes. The removal may continue until the fins 107 are either flush with the surface of the first isolation regions 105 (as shown) or lie below it.

[0025] After these portions of the fins 107 have been removed, a hard mask (not separately shown) is arranged and patterned to cover the dummy gate electrode 111 to prevent growth, and the source / drain regions 201 may be regrown in contact with each of the fins 107. In one embodiment, the source / drain regions 201 may be regrown, and in some embodiments, the source / drain regions 201 may be regrown to form a stressor that will impart strain to the channel regions of the fins 107 disposed beneath the stacks 115. In an embodiment where the fins 107 comprise silicon and the FinFET is a p-channel device, the source / drain regions 201 may be formed using a selective epitaxial process with a material such as silicon, or otherwise a material such asSilicon germanium, which has a different lattice constant than the channel regions, can be regrown. The epitaxial growth process may use precursors such as silane, dichlorosilane, germanium, and the like, and may continue for between approximately 5 minutes and approximately 120 minutes, such as approximately 30 minutes.

[0026] In one embodiment, the source / drain regions 201 may be formed to have a first height H1 above the first isolation regions 105 of between about 20 nm and about 100 nm, such as about 50 nm. In this embodiment, the source / drain regions 201 may be formed to have a height above the top surface of the first isolation regions 105 of between about 5 nm and about 250 nm, such as about 100 nm. However, any suitable height may be used.

[0027] After the source / drain regions 201 have been formed, dopants may be implanted into the source / drain regions 201 by implanting suitable dopants that complement the dopants in the fins 107. For example, p-type dopants, such as boron, gallium, indium, or the like, may be implanted to form a PMOS device. Alternatively, n-type dopants, such as phosphorus, arsenic, antimony, or the like, may be implanted to form an NMOS device. These dopants may be implanted using the stacks 115 and the first spacers 113 as masks. It should be noted that one skilled in the art will recognize that many other processes, steps, or the like may be used to implant the dopants.For example, one skilled in the art will recognize that multiple implantations can be performed using different combinations of spacers and liners to form source / drain regions having a particular shape or characteristic suitable for a specific purpose. Any of these processes can be used to implant the dopants, and the above description is not intended to limit the present invention to the steps presented above.

[0028] At this point, the hard mask covering the dummy gate electrode 111 during the formation of the source / drain regions 201 is also removed. In one embodiment, the hard mask may be removed, for example, using a wet or dry etching process that is selective with respect to the hard mask material. However, any suitable removal process may be used.

[0029] Fig. 2 also shows a formation of an interlayer dielectric layer (ILD) 203 (shown in dashed lines in Fig. 2 to more clearly show the underlying structures) over the stacks 115 and the source / drain regions 201. The ILD layer 203 may comprise a material such as borophosphosilicate glass (BPSG), although any suitable dielectrics may be used. The ILD layer 203 may be formed using a process such as PECVD, although other processes such as LPCVD may alternatively be used. The ILD layer 203 may be formed to a thickness of between approximately 10 nm and approximately 300 nm. After being formed, the ILD layer 203 may be planarized with the spacers 113, for example, using a planarization process such as a chemical mechanical polishing process, although any suitable process may be used.

[0030] After forming the ILD layer 203, the material of the dummy gate electrode 111 and the dummy gate dielectric 109 may be removed and replaced to form the gate stack 205. In one embodiment, the dummy gate electrode 111 may be removed, for example, using a wet or dry etching process that uses etchants selective to the material of the dummy gate electrode 111. However, any suitable removal process may be used.

[0031] After the dummy gate electrode 111 is removed, the remaining openings may be refilled to form the gate stack 205. In one embodiment, the gate stack 205 includes a first dielectric material 211, a first metal material 213, a second metal material 215, and a third metal material 217. In one embodiment, the first dielectric material 211 is a high-k material, such as HfO2, HfSiO, HfSiON, HfTaO, HfTiO, HfZrO, LaO, ZrO, Ta2O5, combinations of these, or the like, deposited using a process such as atomic layer deposition, chemical vapor deposition, or the like. The first dielectric material 211 may be deposited to a thickness of between about 0.5 nm and about 10 nm, although any suitable material and thickness may be used.

[0032] The first metal material 213 may be formed adjacent to the first dielectric material 211 and may be formed from a metallic material such as Ti, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, WN, other metal oxides, metal nitrides, metal silicates, transition metal oxides, transition metal nitrides, transition metal silicates, oxynitrides of metals, metal aluminates, zirconium silicate, zirconium aluminate, combinations of these, or the like. The first metal material 213 may be deposited using a deposition process such as atomic layer deposition, chemical vapor deposition, sputtering, or the like to a thickness of between about 0.5 nm and about 20 nm, although any suitable deposition process or thickness may be used.

[0033] The second metal material 215 may be formed adjacent to the first metal material 213 and, in a particular embodiment, may be similar to the first metal material 213. For example, the second metal material 215 may be formed from a metallic material such as Ti, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, WN, other metal oxides, metal nitrides, metal silicates, transition metal oxides, transition metal nitrides, transition metal silicates, oxynitrides of metals, metal aluminates, zirconium silicate, zirconium aluminate, combinations of these, or the like. Furthermore, the second metal material 215 may be formed using a deposition process such asatomic layer deposition, chemical vapor deposition, sputtering, or the like, to a thickness of between about 0.5 nm and about 20 nm, although any suitable deposition process or thickness may be used.

[0034] The third metal material 217 fills a remnant of the opening left by the removal of the dummy gate electrode 111. In one embodiment, the third metal material 217 is a metallic material, such as W, Al, Cu, AlCu, W, Ti, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, Ta, TaN, Co, Ni, combinations of these, or the like, and may be deposited using a deposition process, such as atomic layer deposition, chemical vapor deposition, sputtering, or the like, to fill and / or overfill the opening left by the removal of the dummy gate electrode 111. In a particular embodiment, the third metal material 217 may be deposited to a thickness of between approximately 0.5 nm and approximately 50 nm, although any suitable material, deposition process, and thickness may be used.

[0035] After the opening left by the removal of the dummy gate electrode 111 has been filled, the materials may be planarized to remove any material located outside the opening left by the removal of the dummy gate electrode 111. In a particular embodiment, the removal may be performed using a planarization process, such as chemical mechanical polishing. However, any suitable planarization and removal process may be used.

[0036] Furthermore, after the gate stack 205 (and therefore the gate width of the semiconductor device) has been formed, the gate stack 205 may have a first width W1 of between approximately 10 nm and approximately 200 nm. However, any suitable width may be used.

[0037] After the materials of gate stack 205 have been formed and planarized, the materials of gate stack 205 may be recessed and covered with a capping layer 221. In one embodiment, the materials of gate stack 205 may be recessed, for example, using a wet or dry etching process that uses etchants selective to the materials of gate stack 205. However, any suitable process may be used.

[0038] After the materials of the gate stack 205 have been removed, the cap layer 221 may be deposited and planarized with the spacers 113. In one embodiment, the cap layer 221 is a material such as SiN, SiON, SiCON, SiC, SiOC, combinations of these, or the like, deposited using a deposition process such as atomic layer deposition, chemical vapor deposition, sputtering, or the like. The cap layer 221 may be deposited to a thickness of between approximately 0.5 nm and approximately 20 nm and then planarized using a planarization process such as chemical mechanical polishing, such that the cap layer 221 is planar with the spacers 113.

[0039] Fig. 2 to 3 also show forming a first etch stop layer Z over the gate stack 205. In one embodiment, the first etch stop layer 223 may be formed from silicon nitride using plasma enhanced chemical vapor deposition (PECVD), although other materials, such as SiON, SiCON, SiC, SiOC, SiC x N y , SiO x , other dielectrics, combinations thereof, or the like, and alternative techniques for forming the first etch stop layer 223, such as low-pressure CVD (LPCVD), PVD, or the like, could alternatively be used. The first etch stop layer 223 may have a thickness of between.

[0040] Fig. 4 shows forming a first dielectric layer 401 over the gate stacks 205 and a first opening 403 through the first dielectric layer 401 to expose the gate stack 205. In one embodiment, the first opening 403 may be formed through the first dielectric layer 401 and the first etch stop layer 223 to expose the underlying gate stack 205. In one embodiment, the first opening 403 may be formed by first disposing and patterning a first photoresist (not separately shown) over the first etch stop layer 223. In one embodiment, the first photoresist is a three-layer photoresist comprising a bottom approximately 0.5 nm and approximately 50 nm anti-reflective coating (BARC) layer, a mask interlayer, and a top photoresist layer. However, any suitable type of photosensitive material or combination of materials may be used.

[0041] After the first photoresist has been applied, the first photoresist is patterned. In one embodiment, the first photoresist can be patterned by exposing a photosensitive material within the first photoresist (e.g., the upper photoresist layer in the three-layer photoresist) to a patterned energy source (e.g., light), e.g., through a reticle. The effect of the energy causes a chemical reaction in those parts of the photosensitive material exposed to the patterned energy source, thereby modifying the physical properties of the exposed portions of the photoresist, such that the physical properties of the exposed portions of the first photoresist are different from the physical properties of the unexposed portions of the first photoresist. The first photoresist can then, e.g.,developed with a developer (not shown separately) to separate the exposed portion of the first photoresist from the unexposed portion of the first photoresist.

[0042] After the first photoresist has been patterned, the first opening 403 may be formed using the first photoresist as a mask. In one embodiment, the first opening 403 may be formed using a first etching process (described in Fig. 4 is represented by the wavy line labeled 405), which may include one or more anisotropic etching processes, such as reactive ion etching processes. However, any suitable process, such as a wet etching process, and any suitable reactants may be used.

[0043] The first etch process 405 may be used to form the first opening 403 in preparation for forming the first contact 501. In a particular embodiment, the first etch process 405, using one or more etches, may be used to remove the material of the first dielectric layer 401, the first etch stop layer 223, and the cap layer 221 to expose the gate stack 205.

[0044] After the first opening 403 has been formed, the first photoresist may be removed. In one embodiment, the first photoresist may be removed, for example, using an ashing process in which a temperature of the first photoresist is increased until the first photoresist is thermally decomposed, at which time the first photoresist may be easily removed. However, any suitable removal process, such as wet etching, may also be used.

[0045] Fig. 5 shows forming the first contact 501 within the first opening 403 and in physical and electrical connection with the gate stack 205. In one embodiment, the first contact 501 may be a conductive material such as Ti, W, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, or WN, although any suitable material such as aluminum, copper, alloys thereof, combinations of these, or the like may be used, and it may be deposited in the first opening 403 using a deposition process such as sputtering, chemical vapor deposition, electroplating, electroless plating, or the like to fill and / or overfill the first opening 403 formed by the first etch process 405.After the opening has been filled or overfilled, any deposited material outside the first opening 403 formed by the first etching process 405 may be removed using a planarization process, such as chemical mechanical polishing (CMP). However, any suitable material and formation method may be used.

[0046] By using a series of one or more anisotropic etches, the first opening 403 may be formed to have tapered sidewalls that cause the first opening 403 to have a varying width as it extends through the first dielectric layer 401, and that also cause the first contact 501 to have a varying width as it extends through the first etch stop layer 223 and the cap layer 221. In a particular embodiment, the first contact 501 has a second width W2 of between about 3 nm and about 20 nm at a point adjacent to the gate stack 205.Furthermore, the first contact 501 has a third width W3 of between approximately 5 nm and approximately 20 nm at a point adjacent to a bottom surface of the first etch stop layer 223. At a point adjacent to a top surface of the first etch stop layer 223, the first contact 501 has a fourth width W4 of between approximately 10 nm and approximately 30 nm. Finally, the first contact 501 may have a fifth width W5 of between approximately 15 nm and approximately 50 nm at a top surface of the first contact 501.

[0047] Furthermore, the second width W2 is greater than the first width W1, and there is a ratio between the second width W2 and the first width W1 of less than at least 1.1, such as less than approximately 1.0. The fifth width W5 is also greater than the fourth width W4, and there is a ratio between the fifth width W5 and the fourth width W4 of more than at least 1, while the fourth width W4 is greater than the third width W3, and there is a ratio between the fourth width W4 and the third width W3 that is greater than 1. Finally, the third width W3 is greater than the second width W2, such as there is a ratio between the third width W3 and the second width W2 of greater than 1.

[0048] In one particular embodiment, the first width W1 is greater than the fifth width W5, which is greater than the fourth width W4, which is greater than the third width W3, which is greater than the second width W2. In another embodiment, the fifth width W5 is greater than the first width W1, which is greater than the fourth width W4, which is greater than the third width W3, which is greater than the second width W2. However, the second width W2 is less than the first width W1.

[0049] By using the embodiments described herein, the critical dimensions of the first contact 501 can be reduced, allowing for an increased process window and better tuning the resistance to lower values. Such improvements enable an overall improvement in the manufacturing process as well as a yield advantage.

[0050] Fig. 6A to 6D illustrate additional embodiments in which the heights of the first dielectric material 211, the first metal material 213, the second metal material 215, and the third metal material 217 are adjusted. In each of these embodiments, the first spacers 113 have a second height H2 of between approximately 10 nm and approximately 150 nm.

[0051] If first the Fig. 6A, the third metal material 217 may be formed to have a third height H3 that is smaller than the second height H2 and may be between about 5 nm to about 100 nm. Furthermore, the second metal material 215 has a fourth height H4 of between about 5 and about 80 nm, and the first metal material 213 has a fifth height H5 of between about 5 nm and about 80 nm. Finally, the first dielectric material 211 has a sixth height H6 of between about 5 nm and about 90 nm. However, any suitable thicknesses may be used.

[0052] In this embodiment, the third height H3 is greater than the fourth height H4, and the ratio of the third height H3 to the fourth height H4 is greater than 1. Furthermore, the second height H2 is greater than the third height H3, and the ratio of the second height H2 to the third height H3 is greater than 1. Finally, depending on the desired shape, the ratio of the sixth height H6 to the first height H1 can be greater or less than 1.

[0053] In the Fig. 6A, the gate stack 205 has only a partially planar top surface, rather than the gate stack 205 having a completely planar top surface (as described above with reference to Fig. 1 to 5). Although the second metal material 215, the first metal material 213, and the first dielectric material 211 may be planar with each other, particularly in this embodiment, the third metal material 217 may extend upwardly from the planar surface by a second distance D2 of between about 1 nm and about 20 nm, such as about 5 nm. However, any suitable distance may be used.

[0054] To achieve the partially planar top surface of the gate stack 205 (without including the third metal material 217 in the planar top surface), the top surfaces of the second metal material 215, the first metal material 213, and the first dielectric material 211 may be removed using a wet etch process with one or more etchants selective to the materials of the second metal material 215, the first metal material 213, and the first dielectric material 211. In a particular embodiment, the wet etch may be continued for a time of approximately 10 seconds to achieve the partially planar top surface of the gate stack 205. However, any suitable removal process and time may be used.

[0055] Fig. Figure 6B shows another embodiment similar to that shown in Fig. 6A, but in which the fifth height H5 of the first metal material 213 is recessed from each of the fourth height H4 and the sixth height H6 of the second metal material 215 and the first dielectric material 211 to form a "W" shape, rather than the second metal material 215, the first metal material 213, and the first dielectric material 211 being planar with each other.

[0056] In this embodiment, a wet etching similar to that described above with reference to Fig. 6A. However, in this embodiment, to achieve the recessed layers, the wet etching may be continued to deposit the materials of the second metal material 215, the first metal material 213, and the first dielectric material 211 over the steps described in Fig. 6A. For example, in one particular embodiment, a similar wet etch is used, but the etch time is increased by 10% to overetch the materials. In an embodiment where a 10-second etch achieves the planar shape, the translation to achieve the "W" shape may be performed for 11 seconds. However, any suitable removal process and time may be used.

[0057] Fig. Figure 6C shows yet another embodiment similar to that described above with reference to Fig. 6A, but in which the fourth height H4 of the second metal material 211 is less than the fifth height H5 of the first metal material 213, and the fifth height H5 of the first metal material 213 is less than the sixth height H6 of the first dielectric material 211, instead of the second metal material 215, the first metal material 213, and the first dielectric material 211 being planar with each other.

[0058] In this embodiment, a wet etching similar to that described above with reference to Fig. 6A. However, in this embodiment, to achieve the recessed layers in a concave shape, the wet etching may be continued to deposit the materials of the second metal material 215, the first metal material 213, and the first dielectric material 211 over the Fig. 6A and over the plane surface shown in Fig. 6B. For example, in one particular embodiment, a similar wet etch is used, but the etch time is increased by 20% to overetch the materials. In an embodiment where a 10-second etch achieves the planar shape, the translation to achieve the "W" shape may be performed for 12 seconds. However, any suitable removal process and time may be used.

[0059] Fig. Figure 6D shows yet another embodiment similar to that described above with reference to Fig. 6A, but in which the fourth height H4 of the second metal material 215 is greater than the fifth height H5 of the first metal material 213, and the fifth height H5 of the first metal material 213 is greater than the sixth height H6 of the first dielectric material 211, rather than the second metal material 215, the first metal material 213, and the first dielectric material 211 being flush with each other. However, any suitable heights may be used.

[0060] In this embodiment, a series of etches may be used to achieve the convex shape. In a particular embodiment, a first etching process similar to that described above with reference to Fig. 6A may be performed to achieve the planar top surface of the gate stack 205. After the wet etch is performed, a second wet etch may be performed with etchants selective to the material of the first dielectric material 211, thereby removing the material of the first dielectric material 211 at a faster rate than the material of the second metal material 215 and the first metal material 213. However, any suitable removal process or series of removal processes may be used.

[0061] Fig. 7A to 7D show embodiments which are respectively similar to those shown in Fig. 6A to 6D. However, in these embodiments, there is not a seamless third metal material 217, but rather, the third metal material 217 includes a seam 701 or a void within the material of the third metal material 217. The seam 701 is formed during the deposition process for the third metal material 217 when the gate width W1 is small for a short channel device and a non-conformal deposition process is used. To achieve the formation of the seam, in a particular embodiment, a non-conformal deposition process, such as chemical vapor deposition or physical vapor deposition, is used on a device wherein the first width W1 is less than or equal to 15 nm.

[0062] Fig. 8A to 8D show further embodiments in which the third metal material 217 does not extend outwardly, but rather is either flush with or recessed from the second metal material 215, the first metal material 213, and the first dielectric material 211. In the Fig. 8A, the top surface of the third metal material 217 may be closer to the fin 107 than a top surface of the second metal material 215. Furthermore, the top surface of the second metal material 215 may be closer to the fin 107 than a top surface of the first metal material 213, and the top surface of the first metal material 213 may be closer to the fin 107 than a top surface of the first dielectric material 211.

[0063] Instead of continuing the recessing of the gate stack 205 such that the third metal material 217 extends away from the second metal material 215, the first metal material 213, and the first dielectric material 211, in this embodiment it is instead stopped before the extension of the third metal material 217. Furthermore, in embodiments where the semiconductor device has a channel length of between approximately 30 nm and approximately 50 nm, the second metal material 215, the first metal material 213, and the first dielectric material 211 form a tapered top surface.

[0064] Fig. Figure 8B shows an embodiment similar to that described above with reference to Fig. 8B. However, in this embodiment, the third metal material 217 is further recessed from the top surface of the second metal material 215. In this embodiment, the third metal material 217 may be recessed from the top surface of the second metal material 215 by a third distance D3 of between approximately 2 nm and approximately 10 nm. However, any suitable distances may be used.

[0065] To achieve the recessing of the third metal material 217, an additional etching process may be performed. However, this etching process uses an etchant that is selective to the material of the third metal material 217, such that the material of the third metal material 217 is removed at a faster rate than the material of the second metal material 215, the first metal material 213, or the first dielectric material 211. However, any suitable process may be used.

[0066] Fig. Figure 8C shows another embodiment similar to that described above with reference to Fig. 6C, and in which the second metal material 215, the first metal material 213, and the first dielectric material 211 are tapered inward. However, in this embodiment, the third metal material 217 is flush with a top surface of the second metal material 215, rather than the third metal material 217 extending outward from the second metal material 215. However, any suitable height may be used.

[0067] Instead of continuing the recessing of the gate stack 205 such that the third metal material 217 extends away from the second metal material 215, the first metal material 213, and the first dielectric material 211, in this embodiment it is instead stopped before the extension of the third metal material 217. In embodiments where the semiconductor device has a channel length of less than approximately 30 nm, the second metal material 215, the first metal material 213, and the first dielectric material 211 also form the rounded top surface.

[0068] Fig. Figure 8D shows another embodiment similar to that described above with reference to Fig. 8C, and in which the second metal material 215, the first metal material 213, and the first dielectric material 211 are inwardly tapered. However, in this embodiment, the third metal material 217 is recessed from the top surface of the second metal material 215, rather than the third metal material 217 extending outward from the second metal material 215. In this embodiment, the third metal material 217 may be recessed from the top surface of the second metal material 215 by the third distance D3 of between approximately 2 nm and approximately 10 nm. However, any suitable distances may be used.

[0069] To achieve the recessing of the third metal material 217, an additional etching process may be performed. However, this etching process uses an etchant that is selective to the material of the third metal material 217, such that the material of the third metal material 217 is removed at a faster rate than the material of the second metal material 215, the first metal material 213, or the first dielectric material 211. However, any suitable process may be used.

[0070] Fig. 9A to 9D show further embodiments which support the device described above with reference to Fig. 8A to 8D. However, in these embodiments, the third metal material 217 includes the seam 701, as described above with reference to Fig.7A to 7D. However, any suitable method for forming the seam 701 within the third metal material 217 may be used.

[0071] The object of the invention is to improve semiconductor devices and a method for their production in such a way that an enlarged process window is enabled and the resistance can be better adjusted. The invention is defined by the main claim and the subordinate claims. Further embodiments of the invention are recited in the dependent claims.

Claims

[1] A semiconductor device (100) comprising: a gate structure (205) over a substrate (107) having a first width (W1), the gate structure (205) comprising a layer of a first metal material (215) and a layer of a second metal material (217) extending over the layer of the first metal material (215); a conductive contact (501) disposed over the gate structure (205) and having a lower portion physically contacting an upper surface extending parallel to a top surface of the substrate (107) and a sidewall of the second metal material (217) extending perpendicular to the upper surface, as well as an upper surface of the first metal material (215), the lower portion having a second width (W2), the second width (W2) being less than or equal to the first width (W1). [2] The semiconductor device (100) of claim 1, wherein the second width (W2) is at least partially disposed within lateral extensions of the first width (W1). [3] The semiconductor device (100) of claim 2, further comprising a cavity (701) disposed within the gate structure (205). [4] Semiconductor device (100) according to one of the preceding claims, wherein the gate structure (205) comprises a gate of a fin field effect transistor (FinFET). [5] A semiconductor device (100) comprising: a gate (205) over a substrate (107) having a first lateral width (W1), the gate (205) further comprising a layer of a first metal material (215) and a layer of a second metal material (217) extending over the layer of the first metal material (215); a source / drain region (201) arranged laterally adjacent to the gate (205), a dielectric layer (401) disposed over the gate (205), and a conductive contact (501) extending through the dielectric layer (401) to a top surface of the gate (205) and physically contacting a top surface extending parallel to a top surface of the substrate (107) and a sidewall of the second metal material (217) extending perpendicular to the top surface, and a top surface of the first metal material (215), wherein a lower portion of the conductive contact (501) has a second lateral width (W2), the ratio of the second lateral width (W2) to the first lateral width (W1) being less than 1. [6] The semiconductor device (100) of claim 5, wherein the second lateral width (W2) is at least partially disposed within lateral extensions of the first lateral width (W1). [7] The semiconductor device (100) of claim 6, wherein the gate further comprises: a layer of a third metal material (213), wherein the layer of the first metal material (215) extends over the layer of the third metal material (213), wherein the layer of the third metal material (213) is different from the layer of the first metal material (215). [8] The semiconductor device (100) of claim 6 or 7, wherein the second lateral width (W2) is arranged entirely within lateral extensions of the first lateral width (W1). [9] Semiconductor device (100) according to one of the preceding claims 5 to 8, wherein the gate (205) comprises a fin field effect transistor (FinFET) gate. [10] Method comprising: Forming a gate structure (205) over a substrate (107) having a first lateral width (W1), the gate structure (205) comprising a layer of a first metal material (215) and a layer of a second metal material (217) extending over the layer of the first metal material (215); Depositing a first dielectric material (401) over the gate structure (205), and Forming a first via opening (403) disposed above the gate structure (205) and through the first dielectric material (401), the first via opening (403) having a lowermost portion exposing a top surface of the gate structure (205), a ratio of the second lateral width (W2) to the first lateral width (W1) being less than 1; and Forming a first conductive contact (501) in the first via opening, wherein the conductive contact (501) is physically connected to a top surface extending parallel to a top surface of the substrate (107) and a sidewall of the layer of second metal material (217) extending perpendicular to the top surface and a top surface of the layer of first metal material (215). [11] The method of claim 10, wherein forming the first via opening (403) comprises arranging the second lateral width (W2) in a position that is at least partially within lateral extents of the first lateral width (W1). [12] The method of claim 11, wherein forming the first via opening (403) comprises substantially aligning a first vertical centerline of the first via opening (403) with a second vertical centerline of the gate structure (205). [13] The method of any one of the preceding claims 10 to 12, wherein forming the gate structure (205) comprises forming a fin field effect transistor gate. [14] The method of claim 13, wherein forming the FinFET gate is performed using a gate-last process. [15] The method of claim 14, wherein forming the gate structure (205) further comprises: Depositing a first dielectric material (211), depositing a layer of a third metal material (213) over the first dielectric material (211), Depositing the layer of the first metal material (215) over the layer of the third metal material (213), wherein the third metal material (213) is different from the first metal material (215), and Depositing the layer of second metal material (217) over the layer of first metal material (215), wherein the first metal material (215) is different from the second metal material (217).

Citation Information

Patent Citations

  • Methods for forming a FinFET structure and FinFET structure

    DE112013005871T5

  • Integrated circuits having smooth metal gates and methods for fabricating same

    US20150076624A1

  • Fin resistor with overlying gate structure

    US20160190120A1

  • Method for forming semiconductor device

    US20160190287A1