Combined gate trench and contact etching process
A single masking layer process for forming gate and contact trenches in semiconductor components addresses alignment issues, enhancing electrical performance and reducing defects, resulting in improved trench precision and cell density.
Patent Information
- Application Number
- DE102017111925
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-06-02
- Filing Date
- 2017-05-31
- Publication Date
- 2024-10-24
- Estimated Expiration
- 2037-05-31
AI Technical Summary
Conventional manufacturing processes for semiconductor components with gate and contact trenches require multiple masks, leading to defects and fluctuations in electrical performance due to mask alignment errors.
A single patterned masking layer is used to simultaneously form gate and contact trenches, eliminating the need for multiple masks and ensuring precise alignment, thereby improving electrical performance.
This approach reduces defects and enhances electrical performance by achieving precise trench dimensions and higher cell density, resulting in lower resistance and improved voltage characteristics.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
BACKGROUND
[0001] Power semiconductor devices, such as metal-oxide-semiconductor field-effect power transistors (MOSFETs), have been widely used in power switching devices, such as power supply units, rectifiers, low-voltage motor controllers, and so on. Power semiconductor devices can be fabricated with a trench topology to improve power density.
[0002] Conventional trench-type power semiconductor manufacturing processes often involve multiple masks to accommodate the formation of complex structures, such as gate or contact trenches. Using multiple masks to etch adjacent gate and contact trenches of varying dimensions in different steps can be challenging and may introduce defects due to errors introduced by the mask dimensions and adjustments made during each masking step. Furthermore, variations in the manufacturing process of semiconductor devices can frequently lead to variations in the electrical performance of the devices, such as on-resistance (RDS(on)). DSon ) and breakdown voltage, lead to.
[0003] Accordingly, there is a need to overcome the disadvantages and shortcomings in the field by essentially eliminating component defects in trench-type power semiconductor devices while simultaneously improving their electrical performance characteristics.
[0004] US 2010 / 0291744A1 describes how trench-gate MOSFET devices can be formed using a single mask to define gate trenches and body contact trenches. A hard mask is formed on the surface of a semiconductor substrate. A trench mask is applied to the hard mask to define a body contact trench and a gate trench. These predefined trenches are etched simultaneously into the substrate to a first predetermined depth. Next, a gate trench mask is applied to the hard mask. The gate trench mask covers the body contact trenches and has openings at the gate trenches. The gate trench, but not the body contact trench, is etched to a second predetermined depth. Conductive material of a first type can fill the gate trench to form a gate. Conductive material of a second type can fill the body contact trench to form a body contact.
[0005] US 2015 / 0 349 057 A1 describes a semiconductor device comprising: a semiconductor layer made of a wide bandgap semiconductor and having a source trench and a gate trench, each provided with a sidewall and a bottom; a gate insulating film formed on the sidewall and the bottom of the gate trench; and a gate electrode embedded in the gate trench so as to face the semiconductor layer through the gate insulating film, the semiconductor layer including: a source region of a first conductivity type formed to be exposed on the side of a front surface of the semiconductor layer to partially form the sidewall of the gate trench;a body region of a second conductivity type formed on one side of the source region, closer to a back face of the semiconductor layer, such that it is in contact with the source region to partially form the side wall of the gate trench; a drift region of the first conductivity type formed on one side of the body region, closer to the back face of the semiconductor layer, such that it is in contact with the body region to form the bottom of the gate trench; and a first failure voltage hold region of the second conductivity type selectively formed at a boundary section of the gate trench, in a subregion of the gate trench where the side wall and bottom intersect. SUMMARY
[0006] The invention is defined by independent method claim 1. Features of exemplary embodiments are specified in the subclaims. BRIEF DESCRIPTION OF THE DRAWINGS Fig. Figure 1 is a flowchart illustrating a method for forming a semiconductor structure according to an implementation of the present application. Fig. Figure 2A illustrates a cross-sectional view of a portion of a semiconductor structure, which, according to an initial process in the flowchart of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2B illustrates a cross-sectional view of a portion of a semiconductor structure, which is being built according to an intermediate step in the flowchart of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2C illustrates a cross-sectional view of a portion of a semiconductor structure, which is being built according to an intermediate step in the flowchart of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2D illustrates a cross-sectional view of a portion of a semiconductor structure formed according to an intermediate process in the flow diagram of Fig. 1 is processed according to an implementation of the present application. Fig. 2E illustrates a cross-sectional view of a portion of a semiconductor structure formed according to an intermediate process in the flow diagram of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2F illustrates a cross-sectional view of a portion of a semiconductor structure formed according to an intermediate process in the flow diagram of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2G illustrates a cross-sectional view of a portion of a semiconductor structure formed according to an intermediate process in the flow diagram of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2H illustrates a cross-sectional view of a portion of a semiconductor structure, which is being built according to an intermediate step in the flowchart of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2I illustrates a cross-sectional view of a portion of a semiconductor structure, which is being built according to an intermediate step in the flowchart of Fig. 1 is processed according to an implementation of the present application. Fig. Figure 2J illustrates a cross-sectional view of a portion of a semiconductor structure, which, according to a final operation in the flowchart of Fig. 1 is processed according to an implementation of the present application. DETAILED DESCRIPTION
[0007] The following description contains specific information regarding implementations in the present disclosure. The drawings in this application and their accompanying detailed description relate merely to exemplary implementations. Unless otherwise noted, like or corresponding elements among the figures are indicated by like or corresponding reference numerals. Furthermore, the drawings and illustrations in this application are generally not to scale and are not intended to represent actual relative dimensions.
[0008] Fig. Figure 1 presents a flowchart illustrating a process for forming an exemplary semiconductor device according to an implementation of the present application. Certain details and features that are obvious to a person skilled in the art have been omitted from the flowchart. For example, a process may consist of one or more sub-processes, or it may involve specialized equipment and materials, as is known in the field. Processes 170, 172, 174, 176, 178, 180, 182, 184, 186, and 188, which are shown in flowchart 100, are sufficient to describe one implementation of the present inventive concepts; other implementations of the present inventive concepts may use processes that differ from those shown in flowchart 100. In addition, the semiconductor structures 270, 272, 274, 276, 278, 280, 282, 284, 286 and 288 can be Fig. 2A, Fig. 2B, Fig. 2C, Fig. 2D, Fig. 2E, Fig. 2F, Fig. 2G, Fig. 2H, Fig. 2I and Fig. 2J illustrates the results of carrying out operations 170, 172, 174, 176, 178, 180, 182, 184, 186, and 188 of flowchart 100. For example, semiconductor structure 270 is an example structure of part of a semiconductor device after processing operation 170, semiconductor structure 272 is an example structure of part of a semiconductor device after processing operation 172, semiconductor structure 284 is an example structure of part of a semiconductor device after processing operation 174, and so on.
[0009] With reference to process 170 in Fig. 1 and the semiconductor structure 270 in Fig. 2A, process 170 comprises the formation of a hard mask and a patterned masking layer over a semiconductor substrate. With reference to Fig. 2A, the semiconductor structure 270 illustrates a cross-sectional view of a portion of a semiconductor structure after completion of the operation 170 in the flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. 2A, the semiconductor structure 270 includes a hard mask 250 and a patterned masking layer 252 over the semiconductor substrate 201.
[0010] As in Fig. As illustrated in Figure 2A, the semiconductor structure 201 comprises a drift region 202 and a drain region 222. The semiconductor substrate 201 can comprise any suitable semiconductor material, such as silicon. The drift region 202 is located above the drain region 222, which is located above a drain contact layer 242. In the present implementation, the drain region 222 comprises a highly doped semiconductor material as a drain of a semiconductor device, such as a power MOSFET or an insulated-gate bipolar transistor (IGBT). As shown in Fig. As illustrated in Figure 2A, the drain region 222 is of a first conductivity type and is depicted as having, for example, n+ conductivity. In the present implementation, the drain region 222 may include an n-type dopant, such as phosphorus or arsenic. In another implementation, the drain region 222 may include a p-type dopant, such as boron. The drain contact layer 242 is formed at the bottom of the drain region 222.
[0011] The drift region 202 can comprise any suitable semiconductor material that can be epitaxially grown on the drift region 202 (e.g., an epitaxial layer). For example, the drift region 202 can comprise epitaxial silicon grown on the drain region 222. As in Fig. 2A, the drift region 202 is of the first conductivity type and is depicted as having, for example, n-type conductivity. In one implementation, the drift region 202 may be intrinsic or pre-doped to be an n-type material, or it may be subsequently doped to become an n-type material, for example. In the present implementation, the drift region 202 may comprise an n-type dopant, such as phosphorus or arsenic. In another implementation, the drift region 202 may comprise a p-type dopant, such as boron.
[0012] As in Fig. As illustrated in Figure 2A, the hard mask 250 is formed over the semiconductor substrate 201. In one implementation, the hard mask 250 can comprise silicon nitride. In another implementation, the hard mask 250 can be formed, for example, by deposition or nitriding on the semiconductor substrate 201. In another implementation, the hard mask 250 can comprise silicon carbide. The patterned masking layer 252 can be formed, for example, by deposition or thermal oxidation on the hard mask 250 and, using a trench mask (in Figure 2A), Fig. (2A not explicitly shown) be patterned to form the patterned openings in it. The thickness of the hard mask 250, as well as the thickness and widths of the patterned openings of the patterned masking layer 252, can be adapted to meet the specific needs of a particular application.
[0013] With reference to process 172 in Fig. 1 and the semiconductor structure 272 in Fig. 2B, process 172 comprises the simultaneous formation of a gate trench and a contact trench in the semiconductor substrate using the patterned masking layer. With reference to Fig. Figure 2B illustrates the semiconductor structure 272, a cross-sectional view of part of a semiconductor structure after completion of process 172 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in Figure 2B, the semiconductor structure comprises 272 gate grooves 206a and 206b and a contact groove 204, which extend through the hard mask 250 into the drift region 202 of the semiconductor substrate 201.
[0014] In the present implementation, the gate trenches 206a and 206b and the contact trench 204 can be formed by etching the unmasked regions (e.g., regions not covered by the patterned masking layer 252) of the drift region 202, for example, using anisotropic etching. As shown in Fig. As illustrated in Figure 2B, gate trenches 206a and 206b and contact trench 204 extend into drift region 202. Each of gate trenches 206a and 206b and contact trench 204 essentially comprises parallel sidewalls extending into a bottom. In the present implementation, gate trenches 206a and 206b and contact trench 204 each have a U-shaped bottom. In another implementation, gate trenches 206a and 206b and contact trench 204 could each have sloping sidewalls and / or a flat bottom.
[0015] As in Fig. As illustrated in Figure 2B, in the present implementation, the gate trenches 206a and 206b and the contact trench 204 can have essentially the same dimensions (e.g., width and depth). In another implementation, the gate trenches 206a and 206b and the contact trench 204 can have different dimensions. It should be noted that the width of each of the gate trenches 206a and 206b and the contact trench 204 can be defined by the respective openings in the patterned masking layer 252 formed in step 170. It should also be noted that in the semiconductor structure 272, the cell spacing 205, measured from the center of the gate trench 206a and the center of the gate trench 206b, is in the micrometer range. In the present implementation, the cell spacing 205 is less than or equal to 0.6 micrometers.In the present implementation, the gate grooves 206a and 206b and the contact groove 204 can have a strip-shaped layout, wherein the gate grooves 206a and 206b and the contact groove 204 are substantially parallel to each other in the semiconductor substrate 201. In another implementation, the gate and contact grooves can have a cell-shaped layout.
[0016] It should be noted that, unlike a conventional trench-type semiconductor device manufacturing process, in which contact trenches are formed multiple processing steps after the formation of conductive gate fillers in gate trenches, implementations of the present application use a single patterned masking layer (e.g., patterned masking layer 252) to etch both gate trenches 206a and 206b and contact trench 204 in a single-step trenching process. Because the gate and contact trenches are formed in a single processing step, misalignments between the gate and contact trenches can be effectively eliminated, such that a conductive contact trench filler subsequently formed in contact trench 204 is self-aligned between conductive gate trench fillers subsequently formed in gate trenches 206a and 206b.It is worth noting that the widths of the patterned openings and the spacing between adjacent patterned openings in the patterned masking layer 252 can help define the dimensions of the gate and contact trenches. By controlling the appropriate dimensions (e.g., widths of the openings and the spacing between adjacent patterned openings) in the patterned masking layer 252 and etching both the gate and contact trenches in a single-step trenching process using the patterned masking layer 252, implementations of the present application can achieve well-controlled gate and contact trench alignment, a smaller cell spacing, and a higher cell density on the semiconductor substrate 201.
[0017] With reference to process 174 in Fig. 1 and the semiconductor structure 274 in Fig. 2C, process 174 includes the formation of a dielectric gate-trough cover layer in the gate-trough and the contact-trough. With reference to Fig. Figure 2C illustrates the semiconductor structure 274, a cross-sectional view of part of a semiconductor structure after completion of process 174 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in Figure 2C, the semiconductor structure 274 comprises a dielectric gate-trough cover layer 208 over the semiconductor substrate 201, in the gate-troughs 206a and 206b, and in the contact-trough 204. The dielectric gate-trough cover layer 208 covers the respective side walls and bottom of the gate-troughs 206a and 206b. The dielectric gate-trough cover layer 208 also covers the side walls and bottom of the contact-trough 204. In the present implementation, the dielectric gate-trough cover layer 208 comprises silicon dioxide (e.g., SiO2). In other implementations, the dielectric gate-trough cover layer 208 can comprise any other suitable dielectric material. It should be noted that the hard mask 250 and the patterned masking layer 252 are removed from the semiconductor substrate 201 before the formation of the dielectric gate trench cover layer 208 in the semiconductor structure 274.
[0018] With reference to process 176 in Fig. 1 and the semiconductor structure 276 in Fig. In 2D, process 176 includes the formation of conductive gate trench fillers in the gate trench and the contact trench. With reference to Fig. 2D illustrates the semiconductor structure 276, a cross-sectional view of part of a semiconductor structure after completion of process 176 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in 2D, the semiconductor structure 276 comprises conductive gate-trough fillers 210a and 210b in gate-troughs 206a and 206b, respectively, and one conductive gate-trough filler 210c in contact-trough 204. The gate-trough fillers 210a, 210b, and 210c fill the entire space in each of the gate-troughs 206a and 206b, respectively, and in contact-trough 204. In the present implementation, the conductive gate-trough fillers 210a, 210b, and 210c comprise doped polycrystalline silicon. In another implementation, the conductive gate-trough fillers 210a, 210b, and 210c can comprise any other suitable conductive material, such as a metallic material.The excess parts of the conductive gate-trough fillers 210a, 210b and 210c over the gate-troughs 206a and 206b and the contact-trough 204 as well as over the dielectric gate-trough top layer 208 are removed by chemical-mechanical polishing (CMP) such that the conductive gate-trough fillers 210a, 210b and 210c have a coplanar top surface with the dielectric gate-trough top layer 208.
[0019] With reference to process 178 in Fig. 1 and the semiconductor structure 278 in Fig. 2E, process 178 comprises the implantation of a source dopant and a body dopant to form a source region and a body region, respectively, in the semiconductor substrate. With reference to Fig. 2E illustrates the semiconductor structure 278 a cross-sectional view of a portion of a semiconductor structure after completion of the operation 178 in the flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in Figure 2E, the semiconductor structure 278 comprises a body region 218, a source region 220 in the semiconductor substrate 201 above the drift region 202.
[0020] In the present implementation, body region 218 can be formed by implanting a body or channel dopant into the semiconductor substrate 201. As in Fig. 2E, the body region 218 is located between the gate trench 206a and the contact trench 204, and between the contact trench 204 and the gate trench 206b. In the present implementation, the body region 218 is of the second conductivity type and is illustrated, for example, as having p-type conductivity. In the present implementation, the body region 218 may include a p-type dopant. For example, a p-type dopant, such as boron ions, may be implanted through the gate trench cap dielectric layer 208 and into the semiconductor substrate 201. In another implementation, an n-type dopant, such as phosphorus or arsenic, and other suitable implantation techniques may be used to form the body region 218. The implantation energy and doping concentration may vary based on the specific needs of a particular application.
[0021] In the present implementation, a source dopant is implanted through the gate trench capping dielectric layer 208 and into the semiconductor substrate 201 to form the source region 220 above the body region 218. For example, the source region 220 is located above the body region 218, between the gate trench 206a and the contact trench 204, and between the contact trench 204 and the gate trench 206b. In the present implementation, the source region 220 is of the first conductivity type and is illustrated, for example, as having n+ conductivity. In the present implementation, the source region 220 may include an n-type dopant. For example, an n-type dopant, such as phosphorus or arsenic, may be implanted through the gate trench capping dielectric layer 208 and into the semiconductor substrate 201.In another implementation, a p-type dopant, such as boron, and other suitable implantation methods can be used to form the source region 220. The implantation energy and doping concentration can vary based on the specific needs of a given application.
[0022] With reference to process 180 in Fig. 1 and the semiconductor structure 280 in Fig. 2F, the process 180 includes forming a contact mask and removing the conductive gate trench filler from the contact trench. Referring to Fig. 2F illustrates the semiconductor structure 280 a cross-sectional view of a portion of a semiconductor structure after completion of the operation 180 in the flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in Figure 2F, the semiconductor structure 280 comprises a contact mask 254 with a portion 254a over the gate groove 206a and a portion 254b over the gate groove 206b. The contact mask 254 is a photoresist mask that covers the conductive gate groove fillers 210a and 210b in the gate grooves 206a and 206b, respectively. Subsequently, the conductive gate groove filler 210c in the contact groove 204 is removed by a back-etching process, such as gate poly etching. After the removal of the conductive gate groove filler 210c from the contact groove 204, the dielectric gate groove cover layer 208 in the contact groove 204 is exposed.
[0023] With reference to process 182 in Fig. 1 and the semiconductor structure 282 in Fig. 2G, procedure 182 involves forming a deep body region under the contact trench using the contact mask. Referring to Fig. 2G illustrates the semiconductor structure 282 a cross-sectional view of part of a semiconductor structure after completion of process 182 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. 2G, the semiconductor structure 282 includes a deep body region 232 beneath the contact trench 204. In the present implementation, the deep body region 232 may be formed by implanting a deep body dopant into the semiconductor substrate 201 in areas not covered by the contact mask 254.
[0024] As in Fig. 2G, the deep body region 232 is located under the contact trench 204 between the gate trenches 206a and 206b and extends into the drift region 202. The deep body region 232, together with the drift region 202 below, forms a pn junction under the contact trench 204 to prevent a conductive contact trench filler from directly contacting the drift region 202, which would cause an electrical short between the drain and source of the semiconductor device. The deep body region 232 is also configured to move the breakdown points away from the gate trenches 206a and 206b. In the present implementation, the deep body region 232 is of the second conductivity type and is illustrated, for example, as having p+ conductivity. In the present implementation, the deep body region 232 may include a p-type dopant.For example, a p-type dopant, such as boron ions, can be implanted through the dielectric gate-groove cover layer 208 and into the semiconductor substrate 201. In another implementation, an n-type dopant, such as phosphorus or arsenic, and other suitable implantation methods can be used to form the deep body region 232. The implantation energy and doping concentration can vary based on the specific needs of a particular application.
[0025] With reference to process 184 in Fig. 1 and the semiconductor structure 284 in Fig. 2G includes process 184, which involves removing the contact mask, removing the dielectric gate-trough cover layer in the contact trench, and forming a dielectric intermediate layer (IDL) over the gate-trough. With reference to Fig. 2H illustrates the semiconductor structure 284, a cross-sectional view of part of a semiconductor structure after completion of process 184 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. As illustrated in Figure 2H, the semiconductor structure 284 comprises a dielectric intermediate layer (IDL) 212 over the semiconductor substrate 201, which covers the conductive gate-trough fillers 210a and 210b over the gate-troughs 206a and 206b, respectively, and within the contact-trough 204. In one implementation, the IDL 212 comprises any suitable dielectric material, such as silicon dioxide or boron phosphate silicate glass (BPSG). In another implementation, the IDL 212 may comprise silicon nitride or another suitable dielectric material. It should be noted that the contact mask 254 and portions of the dielectric gate-trough cover layer 208 over the top of the semiconductor substrate 201 and within the contact-trough 204 are removed from the semiconductor structure 284 prior to the formation of the IDL 212.Furthermore, in the present implementation, after deposition of the IDL 212 into the semiconductor structure 284, the body dopant in body region 218, the source dopant in source region 220, and the deep body dopant in deep body region 232 can be activated by a single implantation procedure, thus saving manufacturing costs and time. In another implementation, the body dopant in body region 218, the source dopant in source region 220, and the deep body dopant in deep body region 232 can be activated separately after each individual implantation procedure.
[0026] With reference to process 186 in Fig. 1 and the semiconductor structure 286 in Fig. 2I, process 186 comprises removing the dielectric intermediate layer (IDL) in the contact groove and depositing a contact implant into the contact groove. With reference to Fig. 2I illustrates the semiconductor structure 286 a cross-sectional view of a portion of a semiconductor structure after completion of the operation 186 in the flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. 2H, the semiconductor structure 286 includes portions 212a and 212b of the interlayer dielectric (IDL) layer 212 over the gate trenches 206a and 206b, respectively.
[0027] It should be mentioned that parts of the IDL 212 within and adjacent to contact trench 204, for example, were treated by contact oxide etching using a non-critical contact mask (in Fig. (2I not explicitly shown) are removed. Therefore, parts 212a and 212b of the dielectric intermediate layer (IDL) 212 remain as dielectric gate-trough caps over the gate-troughs 206a and 206b, respectively. Subsequently, the contact implant 234 is formed at the bottom of the contact-trough 204. For example, a p-doper, such as boron, is implanted at the bottom of the contact-trough 204 (e.g., a shallow 5-keV implant) to improve the ohmic contact resistance between the deep body region 232 and a conductive contact filler that is subsequently to be formed in the contact-trough 204.
[0028] With reference to process 188 in Fig. 1 and the semiconductor structure 288 in Fig. 2J, process 188 comprises forming a barrier layer in the contact trench, forming a conductive contact trench filler in the contact trench, and forming a metallization layer above the contact trench. With reference to Fig. Figure 2J illustrates the semiconductor structure 288, a cross-sectional view of part of a semiconductor structure after completion of process 188 in flowchart 100 of Fig. 1 according to an implementation of the present disclosure. As in Fig. 2J, the semiconductor structure 288 includes a barrier layer 214, a conductive contact trench filler 230a in the contact trench 204, and a metallization layer 236 over the conductive contact trench filler 230a and the barrier layer 214.
[0029] As in Fig. As illustrated in Figure 2J, the barrier layer 214 is a conformal layer over exposed portions of the semiconductor substrate 201, sidewalls and tops of portions 212a and 212b of the IDL 212, and lines the sidewalls and bottom of the contact trench 204. In the present implementation, the barrier layer 214 comprises a conductive material, such as titanium or titanium nitride. A conductive contact trench fill layer 230 may then be deposited into the contact trench 204, the space between portions 212a and 212b of the IDL 212 above the semiconductor substrate 201, and onto the barrier layer 214. Parts of the conductive contact trench filler layer 230 are polished away from the semiconductor structure 288 by CMP, such that the conductive contact trench filler 230a and the barrier layer 214 over parts 212a and 212b of the IDL 212 have a substantially coplanar top surface.In the present implementation, the conductive contact-groove filler 230a comprises a conductive material, such as tungsten. Subsequently, the metallization layer 236 (e.g., source metal) is formed over the conductive contact-groove filler 230a and the barrier layer 214. In the present implementation, the metallization layer 236 comprises a conductive material, such as aluminum or an aluminum alloy. It should be noted that, unlike gap-gate structures with gate, source, and contact grooves in a single substrate, the semiconductor structure 288 does not include a source groove.
[0030] As in Fig. 2J, the metallization layer 236 (e.g., source metal) is located on top of the barrier layer 214 and the conductive contact trench filler 230a in the contact trench 204 and is electrically connected thereto. The drain contact layer 242 is located below the drain region 222 and is electrically connected thereto. The metallization layer 236 and the drain contact layer 242 are used to form a current path between the drain region 222 and the source region 220 during conduction of the semiconductor structure 288 when a potential is applied to the conductive gate trench filler 210a and / or the conductive gate trench filler 210b.
[0031] As in Fig.As illustrated in Figure 2J, the conductive contact trench filler 230a in the contact trench 204 between the gate trenches 206a and 206b is self-adjusting as a result of the use of the single patterned masking layer during operations 170 and 172 of the manufacturing process according to implementations of the present application, wherein the contact trench 204 is spaced such that it is substantially centered between the adjacent gate trenches 206a and 206b.
[0032] It should be noted that, unlike a conventional trench-type semiconductor device manufacturing process, in which contact trenches are formed multiple processing steps after the formation of conductive gate fillers in gate trenches, implementations of the present application use a single patterned masking layer to etch both the gate and contact trenches in a single-step trench process. Because the gate trenches 206a and 206b and the contact trench 204 are formed in a single processing step, misalignments between the gate and contact trenches can be effectively eliminated, such that the conductive contact trench filler 230a in the contact trench 204 is self-aligned between the gate trench filler 210a in the gate trench 206a and the conductive gate trench filler 210b in the gate trench 206b.Since the widths of the patterned openings and the distances between the adjacent patterned openings in the patterned masking layer 252 can help define the dimensions of the gate trenches 206a and 206b and the contact trench 204, by controlling the appropriate dimensions (e.g., the widths of the openings and the distances between two adjacent openings) in the patterned masking layer 252 and etching both the gate and contact trenches in the single-step trenching process using the patterned masking layer 252, the semiconductor structure 288 can achieve well-controlled gate and contact trench alignment, a smaller cell pitch, and a higher cell density on the semiconductor substrate 201. For example, the cell spacing 205, measured from the center of the conductive gate trench filler 210a in gate trench 206a and the center of the conductive gate trench filler 210b in gate trench 206b, is less than or equal to 0.6 micrometers.Furthermore, implementations of the present application enable improved electrical performance characteristics, such as lower R. DSon , lower voltage nodes, for semiconductor devices such as MOSFETs, IGBTs and the like.
Claims
[1] A method of forming a semiconductor device, the method comprising: simultaneously forming a gate trench (206a, 206b) and a contact trench (204) in a semiconductor substrate (201) using a patterned masking layer such that a depth of the gate trench (206a, 206b) is substantially identical to a depth of the contact trench (204); Forming a conductive gate filler (210a, 210b) in the gate trench (206a, 206b); Forming a deep body region (232) under the contact trench (204); Forming a conductive contact filler (230a) in the contact trench (204); Forming, by implanting and after forming the conductive gate filler (210a, 210b) in the gate trench (206a, 206b), a body region (218) adjacent to the gate trench (206a, 206b), wherein - the body region (218) and the deep body region (232) have the same conductivity type and both form a pn junction with a drift region (202) of the semiconductor substrate (201) lying below them; - the pn junction between the deep body region (232) and the drift region (202) is located below the bottoms of the gate trench (206a, 206b) and the contact trench (204); - the pn junction between the body region (218) and the drift region (202) is located above the bottoms of the gate trench (206a, 206b) and the contact trench (204). [2] The method of claim 1, further comprising forming a gate trench capping dielectric layer (212a, 212b) in the gate trench (206a, 206b). [3] The method of claim 1, further comprising forming an interlayer dielectric layer, IDL (212), over the conductive gate filler (210a, 210b). [4] The method of claim 1, further comprising forming a contact implant (234) at a bottom of the contact trench (204). [5] The method of claim 1, further comprising forming a barrier layer (214) in the contact trench (204). [6] The method of claim 1, further comprising forming a source region (220) in the semiconductor substrate (201). [7] The method of claim 1, wherein the conductive gate filler (210a, 210b) comprises doped polycrystalline silicon. [8] The method of claim 1, wherein the conductive contact filler (230a) comprises tungsten. [9] The method of claim 1, further comprising forming a metallization layer (236) over the contact trench (204). [10] The method of claim 1, wherein the gate trench (206a, 206b) extends through a source region (220) and the body region (218) into the drift region (202) of the semiconductor substrate (201). [11] The method of claim 1, wherein the semiconductor device comprises a MOSFET. [12] The method of claim 1, wherein the semiconductor device comprises an IGBT. [13] The method of claim 1, wherein the semiconductor device has a cell pitch less than or equal to 0.6 micrometers.
Citation Information
Patent Citations
High density trench mosfet with single mask pre-defined gate and contact trenches
US20100291744A1