Sintered ferrite magnet

DE102017200497B4Active Publication Date: 2024-10-17TDK CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
DE102017200497
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2016-01-15
Filing Date
2017-01-13
Publication Date
2024-10-17
Estimated Expiration
2037-01-13

Smart Images

  • Figure 00000019_0000
    Figure 00000019_0000
  • Figure 00000020_0000
    Figure 00000020_0000
  • Figure 00000020_0001
    Figure 00000020_0001
Patent Text Reader

Abstract

A sintered ferrite magnet comprising a composition expressed by a following formula (1),Ca1-w-xLawAxFezComMnaO19(1)wherein 'w', 'x', 'z', 'm' and 'a' in the formula (1) satisfy the following formulas (2), (3), (4), (5), and (6), and0.21≦w≦0.620.02≦x≦0.467.43≦z≦11.030.18≦m≦0.410.049≦a≦0.114'A' in the formula (1) is at least one kind of element selected from a group consisting of Sr and Ba.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION1. Field of the InventionThe present invention relates to a sintered ferrite magnet.2. Description of the Prior ArtSr-ferrite based on hexagonal crystal or M-type Ba-ferrite (magnetoplumbite type) is known as a material of a permanent magnet made of an oxide. Magnetic materials containing these ferrites serve as a permanent magnet in the form of a sintered ferrite magnet, a bonded magnet or the like.In recent years, miniaturization and increasingly high performance of electronic components have required permanent magnets also to have high magnetic properties.The residual magnetic flux density (Br) and coercive force (HcJ) are generally used as indicators of magnetic properties of a permanent magnet. A permanent magnet is evaluated as having higher magnetic properties when these indicators are higher.For example, Patent Document 1 discloses a magnetic ferrite material having high Br and HcJ but also high Hk / HcJ by containing a certain amount of an Si component.Patent Document 2 discloses a ferrite magnetic material having high Br and HcJ by containing a certain amount of an Si component and further containing a certain amount of an Al component and a Cr component. Patent Document 3 discloses a ferrite magnetic material having a ferrite phase with a hexagonal structure and having a main composition represented by Ca 1-w-x-y R w Sr x Ba y Fe z M m O 19 wherein R is at least one element of rare earth elements (including Y) substantially comprising La and Bi, and M is at least one element of Co, Mn, Mg, Ni, Cu, and Zn. Patent Document 4 discloses a ferrite sintered magnet. The composition of the main phase constituting a ferrite sintered magnet is represented by Ca 1-w-x-y R w A x Fe z M m O 19. R is at least one element selected from a group consisting of rare earth elements and Bi, and contains at least La, A is at least one element selected from Sr and Ba, and M is at least one element selected from a group consisting of Co, Mn, Mg, Ni, Cu, and Zn, and contains at least Co.As mentioned above, the combinations of the elements added to the main components have been changed variously to obtain both good Br and HcJ, but it is still unclear what kind of combination of the added elements provides higher magnetic properties.In order to obtain higher Br and HcJ, it is also preferable for a permanent magnet to have a higher ratio of a value (Hk) of a magnetic field when the magnetization is 90% of Br to HcJ, which is referred to as squareness ratio (Hk / HcJ).Excellent moldability is required to industrially produce a large amount of products having a stable quality.However, it was not easy to obtain a permanent magnet having good magnetic properties and good moldability, because if one of the magnetic properties or moldability improves, for example, the other magnetic property or moldability decreases.Patent Document 1: WO 2011 / 004 791 A1Patent Document 2: WO 2014 / 021 426 A1Patent Document 3: US 2012 / 0 161 910 A1Patent Document 4: JP 2015-130 493 ASUMMARY OF THE INVENTIONThe present invention was carried out in view of these conditions. It is an object of the invention to provide a ferrite sintered magnet which maintains high Br and HcJ and further has good formability.In order to achieve the above-described object, a ferrite sintered magnet of the present invention is formed as follows.[1] A ferrite sintered magnet comprising a composition expressed by a following formula (1), Ca 1-w-x La w A x Fe z Co m Mn a O 19(1) wherein "w", "x", "z", "m" and "a" in the formula (1) satisfy the following formulae (2), (3), (4), (5), and (6), and"A" in the formula (1) is at least one kind of element selected from a group consisting of Sr and Ba.The present invention makes it possible to provide a ferrite sintered magnet having high formability while favorably maintaining Br and HcJ.The following modes are recited as specific modes of the above [1].[2] The ferrite sintered magnet described in the above [1], wherein w / m is 0.84-2.48.[3] The ferrite sintered magnet described in the above [1] or [2], wherein Si is further contained at 0.52% by mass to 1.18% by mass with respect to SiO 2.[4] The ferrite sintered magnet described in any one of the above [1] to [3], wherein Cr is further contained at 0.98 mass % or less with respect to Cr 2 O 3.Brief Description of the DrawingsFIG. 1 is a perspective view schematically illustrating a ferrite sintered magnet according to an embodiment of the present invention. FIG. 2A is a graph showing a relationship between an atomic ratio of Mn (a) and Br. FIG. 2B is a graph showing a relationship between an atomic ratio of Mn (a) and HcJ. FIG. 2C is a graph showing a relationship between an atomic ratio of Mn (a) and Hk / HcJ. FIG. 3A is a graph showing a relationship between an atomic ratio of Co (m) and Br. FIG. 3B is a graph showing a relationship between an atomic ratio of Co (m) and HcJ. FIG. 3C is a graph showing a relationship between an atomic ratio of Co (m) and Hk / HcJ. FIG. 4A is a graph showing a relationship between an atomic ratio of La (w) and Br. FIG. 4B is a graph showing a relationship between an atomic ratio of La (w) and HcJ. FIG. 4C is a graph showing a relationship between an atomic ratio of La (w) and Hk / HcJ. FIG. 5A is a graph showing a relationship between an atomic ratio of "A"(x) and Br. FIG. 5B is a graph showing a relationship between an atomic ratio of "A"(x) and HcJ. FIG. 5C is a graph showing a relationship between an atomic ratio of "A" (x) and Hk / HcJ. FIG. 6A is a graph showing a relationship between an atomic ratio of Fe (z) and Br. FIG. 6B is a graph showing a relationship between an atomic ratio of Fe (z) and HcJ. FIG. 6C is a graph showing a relationship between an atomic ratio of Fe (z) and Hk / HcJ. FIG. 7A is a graph showing a relationship between an SiO 2- amount and Br. FIG. 7B is a graph showing a relationship between an SiO 2- amount and HcJ. FIG. 7C is a graph showing a relationship between SiO 2- amount and Hk / HcJ.DESCRIPTION OF THE PREFERRED EMBODIMENTSThe present invention will be described in detail based on the present embodiment with reference to the drawings, but is not limited to only the embodiment described below.The following components include those which are easily devised by those skilled in the art and those which are substantially identical thereto. Furthermore, the following components may be combined as appropriate.Sintered ferrite magnetAn overall configuration of a ferrite sintered magnet according to the present invention will be described.FIG. 1 is a schematic perspective view illustrating the ferrite sintered magnet of the present embodiment. A ferrite sintered magnet 10 has a shape in which the end surfaces are curved in a circular arc shape, which is generally referred to as a circular segment shape, a C shape, a tile shape, or an arc shape. The sintered ferrite magnet 10 is preferably used as a magnet for motors, for example.The ferrite sintered magnet 10 according to an embodiment of the present invention is made of a ferrite having a main phase of a ferrite phase having a hexagonal crystal structure.A magnetoplumbite (M-type) ferrite (hereinafter referred to as an "M-type ferrite") is preferable as the above-mentioned ferrite phase. Incidentally, a main phase composed of a magnetoplumbite (M-type) ferrite is mainly referred to as an "M-phase". The sintered ferrite magnet is normally composed of a "main phase (crystal grain)" and a "grain boundary", and the "main phase composed of a ferrite phase" means that this "main phase" is a ferrite phase. A proportion of the main phase occupying the sintered body is preferably 95 percent by volume or more.The ferrite sintered magnet is in the form of a sintered body and has a structure including a crystal grain (main phase) and a grain boundary. An average crystal grain diameter of the crystal grain in this sintered body is preferably 2 μm or less, and more preferably 0.5 μm to 1.6 μm. A high HcJ can be easily obtained with such an average crystal grain diameter. Incidentally, the average crystal grain diameter referred to herein is an arithmetic mean value of a grain diameter in a magnetization heavy direction axis (a axis) of a crystal grain in an M-type ferrite sintered body. A crystal grain diameter of a sintered body of a magnetic ferrite material can be measured by scanning electron microscopy.The sintered ferrite magnet of the present embodiment has, for example, a composition expressed by a following formula (1). Ca 1-w-x La w A x Fe z Co m Mn a O 19(1)In the formula (1), "A" is at least one kind of element selected from a group consisting of Sr and Ba.In the formula (1), "w", "x", "z", "m" and "a" respectively indicate atomic ratios of La, "A", Fe, Co and Mn, and satisfy all of the following formulae (2), (3), (4), (5) and (6).Incidentally, a composition ratio of oxygen is influenced by the composition ratios of each metal element and valences of each element (ion), and increases / decreases so as to maintain electrical neutrality within a crystal. In a firing step or sintering step mentioned below, oxygen deficiency may occur if a reducing atmosphere is used as the firing atmosphere.The composition of the above-mentioned ferrite sintered magnet will be described in detail below.The sintered ferrite magnet of the present embodiment may contain SiO 2 or Cr 2 O 3 as an additional component as described below, or may contain other additional components such as a Ca component.However, the sintered ferrite magnet of the present invention contains Ca as a component constituting the ferrite phase of the main phase as mentioned above. Therefore, when Ca is contained as an additional component, an amount of Ca analyzed in the sintered body represents a total amount of the main phase and the additional component. That is, when a Ca component is used as an additional component, the atomic ratio (1-w-x) of Ca in the general formula (1) represents a value also including the additional component. A range of the atomic ratio (1-w-x) is specified based on a composition analyzed after sintering, thus, can be applied to a case where the Ca component is contained as an additional component and a case where the Ca component is not contained as an additional component.The atomic ratio of La (w) is in the range of 0.21 ≦ w ≦ 0.62, and this range achieves good moldability, while high Br and HcJ can be obtained. This region can also improve an anisotropic magnetic field. In view of the above, the atomic ratio of La is preferably 0.24 to 0.56, and more preferably 0.31 to 0.51.An element denoted by "A" is at least one element selected from a group consisting of Sr and Ba, but more preferably, "A" is only Sr or only Ba. This can reduce the number of elements and the work required in the production. Incidentally, both Sr and Ba may be contained.The atomic ratio of "A" (x) in the composition of the metal elements constituting the above-mentioned ferrite sintered magnet is in a range of 0.02 ≦ x ≦ 0.46, and this range achieves good formability while high Br and HcJ can be obtained. In view of the above, the atomic ratio of "A" (x) is preferably from 0.04 to 0.32, and more preferably from 0.07 to 0.23.Incidentally, when both Sr and Ba are contained, their total amount is preferably in the above-mentioned range of atomic ratio of "A" (x).The atomic ratio of Fe (z) is in the range of 7.43 ≦ z ≦ 11.03, and this range achieves good moldability, while high Br and HcJ can be obtained. In view of the above, the atomic ratio of Fe (z) is preferably from 8.02 to 10.65, and more preferably from 8.72 to 9.52.The atomic ratio of Co (m) is in the range of 0.18 ≦ m ≦ 0.41, and this range achieves good moldability, while high Br and HcJ can be obtained. This region also improves an anisotropic magnetic field. In view of the above, the atomic ratio of Co is preferably from 0.18 to 0.36, and more preferably from 0.21 to 0.28.The atomic ratio of Mn (a) is in the range of 0.049 ≦ a ≦ 0.114 and this range achieves good moldability, while high Br and HcJ can be obtained. In view of the above, the atomic ratio of Mn is preferably from 0.054 to 0.079.Incidentally, additional constituents of the sintered ferrite magnet such as Cr and Si may be contained in each of the main phase and the grain boundary of the sintered ferrite magnet. In the ferrite sintered magnet, the main phase is a region other than the additional constituent of the whole.With respect to the atomic ratio of La (w) and the atomic ratio of Co (m), w / m is preferably 0.84 to 2.48, which achieves good moldability while high Br and HcJ can be obtained. In view of the above, w / m is preferably 1.24 to 2.04.The sintered ferrite magnet of the present embodiment may contain Si as an additional component. An amount of Si with respect to SiO 2 is preferably 0.52% by mass to 1.18% by mass of the entire ferrite sintered magnet. This results in a ferrite sintered magnet having a good sinterability, a suitably adjusted crystal grain diameter and advantageously controlled magnetic properties. As a result, it becomes possible to obtain high Hk / HcJ and good moldability while obtaining high Br and HcJ. In view of the above, the amount of SiO 2 is more preferably 0.59 mass % to 1.01 mass % of the entire ferrite sintered magnet, and even more preferably 0.64 mass % to 0.92 mass % of the entire ferrite sintered magnet.The sintered ferrite magnet of the present embodiment may contain Cr as an additional component. An amount of Cr with respect to Cr 2 O 3 is preferably 0.98 mass % or less of the entire ferrite sintered magnet, preferably 0.30 mass % or less of the entire ferrite sintered magnet, and more preferably 0.08 mass % of the entire ferrite sintered magnet of the entire ferrite sintered magnet. This achieves good moldability.The sintered ferrite magnet contains the above-mentioned composition of metal elements and the additional component such as SiO 2, but the composition of the sintered ferrite magnet can be measured by X-ray fluorescence quantitative analysis. Further, the presence of the main phase can be confirmed by X-ray diffraction, electron beam diffraction or the like.Boron B may be contained as an additional ingredient, for example, as B 2 O 3. An amount of B as B 2 O 3 is preferably 0.5 mass % or less with respect to the whole ferrite sintered magnet. This makes it possible to reduce the calcining temperature or firing temperature at the time of obtaining the ferrite sintered magnet, to obtain the ferrite sintered magnet with good productivity, and to reduce the reduction in saturation magnetization of the ferrite sintered magnet.Further, the sintered ferrite magnet of the present embodiment may contain Ga, Mg, Cu, Ni, Zn, In, Li, Ti, Zr, Ge, Sn, V, Nb, Ta, Sb, As, W, Mo, or the like in the form of an oxide as an additional ingredient. The amounts of these in the whole ferrite sintered magnet are preferably not more than 5 mass % of gallium oxide, not more than mass % of magnesium oxide, not more than 5 mass % of copper oxide, not more than 5 mass % of nickel oxide, not more than 5 mass % of zinc oxide, not more than 3 mass % of indium oxide, not more than 1 mass % of lithium oxide, not more than 3 mass % of titanium oxide, not more than 3 mass % of zirconium oxide, not more than 3 mass % of germanium oxide, not more than 3 mass % of tin oxide, not more than 3 mass % of vanadium oxide, not more than 3 mass % of niobium oxide, not more than 3 mass % of tantalum oxide, with respect to an oxide having a stoichiometric composition of each atom, not more than 3 mass % antimony oxide, not more than 3 mass % arsenic oxide, not more than 3 mass % tungsten oxide and not more than 3 mass % molybdenum oxide. However, when many kinds of these are combined and included, their entirety is preferably set to include not more than 5 mass % in order to avoid a decrease in magnetic properties.An alkali metal element (Na, K, Rb or the like) may be contained in the starting materials of the ferrite sintered magnet and may be contained in the ferrite sintered magnet, provided it is inevitably contained. An amount of the alkali metal element that does not particularly influence the magnetic properties is not more than 3 mass %.Method for Producing Ferrite Sintered MagnetNext, a method for producing a ferrite sintered magnet, which is an embodiment of the present invention, will be specifically described.The following embodiment shows an example of the method for manufacturing the ferrite sintered magnet. In the present embodiment, the sintered ferrite magnet can be manufactured by a mixing step, a calcining step, a pulverization step, a pressing step, and a firing step. A drying step and a kneading step of a finely pulverized slurry may be performed between the pulverizing step and the pressing step, and a degreasing step may be performed between the pressing step and the firing step. Each step will be described below.< Step>In the mixing step, the raw materials of the ferrite sintered magnet are mixed to obtain a raw material mixture. First, examples of the raw material of the ferrite sintered magnet include a compound (raw material compound) including one kind or two or more kinds of elements constituting this ferrite sintered magnet. The starting material compound is preferably present, for example, as a powder.Examples of the raw material compound include an oxide of each of the elements or a compound that becomes an oxide by firing (carbonate, hydroxides, nitrates, etc.). For example, the raw material compound includes CaCO 3, La 2 O 3, SrCO 3, Fe 2 O 3, Co 3 O 4, MnO, Cr 2 O 3, SiO2, or the like. An average particle diameter of a powder of the raw material compound is, for example, preferably about 0.1 μm to 2.0 μm to allow homogeneous mixing.For example, the mixing may be performed by weighing and mixing each of the raw materials so as to obtain a desired composition of a magnetic ferrite material, and then by mixing and pulverizing treatments for about 0.1 hour to 20 hours using a wet attritor, a ball mill, and the like.Incidentally, in this mixing step, not all the raw materials need to be mixed, and some of the raw materials may be configured to be added after the above-mentioned calcination. For example, a Si starting material (for example, SiO 2) and a Cr starting material (for example, Cr 2 O 3), which are additional components, or a Mn starting material (for example, MnO) and a Ca starting material (for example, CaCO 3), which are a component of the composition of the metal elements, may be added during the pulverization step (particularly, the fine pulverization) described below after the calcination described later, or may be added during the mixing step and the pulverization step. The time of addition should be determined so that a desired composition or magnetic properties are easily obtained.<Calcination Step>During the calcining step, a raw material powder obtained in the mixing step is calcined. The calcination is preferably carried out, for example, in an oxidizing atmosphere such as air or the like. A temperature in calcination is preferably in a temperature range of 1100° C. to 1400° C., preferably 1100° C. to 1300° C., and more preferably 1150° C. to 1300° C. A duration of calcination may be 1 second to 10 hours, and preferably 1 second to 5 hours.A calcined body obtained by calcination contains 70% or more of the above-mentioned main phase (M phase). A primary particle diameter of the calcined body is preferably 10 μm or less, more preferably 5 μm or less, and even more preferably 2 μm or less.< Step>During the pulverization step, the calcined body obtained in a granular form or a lump form in the calcination step is pulverized and restored into a powder form. This facilitates pressing in the pressing step mentioned below. As mentioned above, during this pulverization step, the raw materials that were not mixed during the mixing step may be added (later addition of the raw materials). The pulverization step may be carried out in a two-step step step, in which the calcined body is pulverized to be converted into a coarse powder (coarse pulverization), and then further finely pulverized (fine pulverization).The coarse pulverization is performed using a vibration mill, etc. until the average particle diameter is 0.5 μm to 5.0 μm. During the fine pulverization, a roughly pulverized material obtained by the rough pulverization is further pulverized by a wet attritor, a ball mill, a jet mill, or the like.In the fine pulverization, the fine pulverization is performed such that the average particle diameter of a obtained fine pulverized material is preferably about 0.08 μm to 0.02 μm, more preferably about 0.1 μm to 1.0 μm, and even more preferably about 0.1 μm to 0.5 μm. A specific surface area (obtained by, for example, a BET method) of the finely pulverized material is preferably about 4 m 2 / g to 12 m 2 / g. A preferable pulverization time differs depending on the type of pulverization. For example, the pulverization time is about 30 minutes to 20 hours in the case of a wet attritor, and the pulverization time is preferably about 1 hour to 50 hours in wet pulverization in a ball mill.When some of the raw materials are added to the pulverization step, this addition may be performed during the fine pulverization, for example. In the present embodiment, SiO 2 as an Si component, CaCO 3 as a Ca component, or the like may be added during the fine pulverization, but they may also be added during the mixing step or the coarse pulverization step.In the fine pulverization step, in the case of a wet method, a nonaqueous solvent such as toluene and xylene or an aqueous solvent such as water may be used as a dispersion medium. The use of a non-aqueous solvent results in achieving a higher orientation during the wet pressing described later. On the other hand, the use of a wet solvent such as water is advantageous from the viewpoint of productivity.In the fine pulverization step, for example, a well-known polyhydric alcohol or dispersant may be added to increase a degree of orientation of a sintered body after firing.<Press and Firing Steps>In the pressing and firing steps, a pulverized material (preferably, a finely pulverized material) obtained after the pulverization step is pressed to obtain a green body, and then this green body is fired to obtain the sintered body. The pressing may be performed by any method such as wet pressing, dry pressing, or ceramic injection molding (CIM), but as the pressing, CIM or wet pressing, and particularly preferably CIM, is preferably used.In the dry pressing method, for example, a magnetic field is applied to a dried magnetic powder while being pressed, thereby forming a green body, and then the green body is fired. Since a dried magnetic powder is generally pressed inside a metal mold during the dry pressing process, the dry pressing process is advantageous because only a short time is required for the pressing step.In the wet pressing method, for example, a slurry containing a magnetic powder removes the liquid component while being pressed in a magnetic field, thereby forming a green body and then firing it. The wet pressing method is advantageous in that the magnetic powder can be easily oriented by the magnetic field during pressing, and the magnetic properties of the sintered magnet are good.The CIM method is a method in which a pellet formed by heating and kneading a dried magnetic powder together with a binder resin is injection-molded in a metal mold while applying a magnetic field to obtain a preliminary green body, and this preliminary green body is fired after being subjected to debindering.Hereinafter, CIM and wet pressing will be described in detail.(CIM and firing)In the case that the sintered ferrite magnet is obtained by the CIM method, a finely pulverized slurry containing the magnetic powder is dried after wet pulverization. A drying temperature is preferably 80° C. to 500° C., and more preferably 100° C. to 400° C. A drying time is preferably 1 second to 100 hours, and more preferably 1 second to 50 hours. A moisture content of the magnetic powder after drying is preferably not more than 1.0 mass %, and more preferably not more than 0.5 mass %. An average particle diameter of the primary particles of the magnetic powder after drying is preferably in a range of 0.08 μm to 2.0 μm, and more preferably in a range of 0.1 μm to 1.0 μm.The dried magnetic powder is kneaded together with the binder resin, a lubricant, a plasticizer, a sub-limited (sublimable) compound or the like (hereinafter referred to as "organic components") and formed into a pellet by means of a granulator or the like. The green body preferably comprises 35 vol% to 60 vol% of the organic components, and more preferably 40 vol% to 55 vol% of the organic components. Kneading may be carried out by, for example, a kneader. A twin-screw extruder is used as the granulator, for example. Kneading and pelleting may be carried out during heating depending on the melting temperature of the organic components used.A polymer compound such as a thermoplastic resin is used as the binder resin, and polyethylene, polypropylene, ethylene-vinyl acetate copolymer, atactic polypropylene, acrylic polymer, polystyrene, polyacetal, etc. are used as the thermoplastic resin, for example.Synthetic waxes such as paraffin wax, urethaneized wax and polyethylene glycol are used as the wax in addition to natural waxes such as carnauba wax, montan wax and beeswax.For example, a fatty acid is used as the lubricant. For example, a phthalic acid ester is used as the plasticizer.With respect to 100% by mass of the magnetic powder, an addition amount of the binder resin is preferably 3% by mass to 20% by mass, an addition amount of the wax is preferably 3% by mass to 20% by mass, and an addition amount of the lubricant is preferably 0.1% by mass to 5% by mass. An addition amount of the plasticizer is preferably 0.1 mass % to 5 mass % with respect to 100 mass % of the binder resin.In the present embodiment, the above-mentioned pellet is injection molded, for example, in a metal mold using a magnetic field molding apparatus. Before injection molding into the metal mold, the metal mold is closed, forming a cavity inside, and a magnetic field is applied.Incidentally, the pellet is heated and melted at 160° C. to 230° C., for example, inside the extruder, and injected into the cavity of the metal mold by a screw. A temperature of the metal mold is 20° C. to 80° C. The magnetic field applied to the magnet mold should be about 80 kA / m to 2000 kA / m.Subsequently, the preliminary green body obtained by CIM is subjected to a heat treatment at 100° C. to 600° C. in the atmosphere or in nitrogen, and is subjected to a debond treatment, thereby obtaining the green body.The debindering treatment is preferably performed by appropriately adjusting a temperature increase rate in a temperature range in which volatilization or decomposition occurs, with a low temperature increase rate of about 0.01 ° C. / min to 1 ° C. / min depending on the organic components subjected to the debindering treatment. This prevents cracks or fractures of the green body and improves the dimensional stability of the green body or sintered body. When a plurality of organic components are used, the debindering treatment may be performed a number of timesSubsequently, during the firing step, the sintered ferrite magnet according to the present invention is obtained by firing the green body subjected to a debindering treatment at a temperature of preferably 1100° C. to 1250° C., and more preferably 1180° C. to 1230° C. in the atmosphere, for example, for about 0.2 hours to 3 hours. By keeping the above-described firing temperature and holding time of the firing temperature, a sufficient sintered body density can be obtained, a reaction of the added elements is sufficient, and desired magnetic properties are obtained.Incidentally, the firing step may be implemented continuously after the aforementioned debindering step, or the firing may be implemented after the debindering treatment and subsequent cooling to room temperature are performed.(Wet Pressing and Firing)In the case where the sintered ferrite magnet is obtained by the wet pressing method, pressing is preferably performed by performing the above fine pulverization step with moisture to obtain a slurry, concentrating this slurry to a certain concentration to obtain a slurry suitable for wet pressing, and using this slurry.The slurry may be concentrated by a centrifugal separator, a filter press, or the like. The finely pulverized material constitutes about 30 mass % to 80 mass % of the total amount of the slurry suitable for wet pressing.In the slurry, water is preferably used as the dispersing agent for dispersing the finely pulverized material. In this case, a surfactant such as gluconic acid, gluconate and sorbitol may be added to the slurry. A non-aqueous solvent can be used as the dispersant. An organic solvent such as toluene and xylene can be used as the nonaqueous solvent. In this case, a surfactant such as oleic acid is preferably added.Incidentally, the slurry suitable for wet pressing may be prepared by adding the dispersion medium or so after fine pulverization to the finely pulverized material in a dried state.In the wet pressing, this slurry suitable for the wet pressing is subsequently subjected to pressing in a magnetic field. In this case, a pressing pressure is preferably about 9.8 MPa to 98 MPa (0.1 t / cm 2 to 1.0 t / cm 2) and an applied magnetic field should be about 400 kA / m to 1600 kA / m. A pressing direction and the direction of the applied magnetic field during pressing may be identical directions or orthogonal directions.The green body obtained by the wet pressing may be fired in an oxidizing atmosphere of the atmosphere or the like. A firing temperature is preferably 1050° C. to 1270 ° C., and more preferably 1080° C. to 1240 ° C. A firing time (a time for which the firing temperature is maintained) is preferably 0.5 hours to 3 hours.When the green body is obtained by the above-mentioned wet pressing, the occurrence of cracks is preferably prevented by heating at a slow temperature increase rate of about 0.5° C. / min from room temperature to about 100° C., and by sufficiently drying the green body before the green body is brought to the above-mentioned firing temperature.Further, when the surfactant (dispersant) or the like is added, it is preferable to sufficiently remove it (degreasing treatment), for example, by heating at a temperature increase rate of about 2.5° C. / min in a temperature range of about 100° C. to 500° C.). Incidentally, these treatments may be performed at the beginning of the firing step, or may be performed in advance separately before the firing step.This concludes the description of the preferred manufacturing method of the ferrite sintered magnet, but the manufacturing method is not limited to that described above, and the manufacturing conditions may be changed as appropriate.The sintered ferrite magnet obtained by the present invention has any shape provided it has the ferrite composition of the present invention. For example, the sintered ferrite magnet may have a variety of shapes, such as an arc shape having anisotropy, the shape of a flat plate, the shape of a circular tube, and a cylindrical shape. In the ferrite sintered magnet of the present invention, a high Hk / HcJ can be obtained while maintaining high Br and HcJ regardless of the shape of the magnet, particularly regardless of whether it has an arc shape.The sintered ferrite magnet of the present embodiment can be used for a general motor, a rotating device, a sensor, or the like.For example, the sintered ferrite magnet of the present embodiment can be used as an element of an engine for an automobile, such as a fuel pump, a power window, an ABS system, a fan, a wiper, a power steering, an active suspension, an igniter, a door lock, and an electric mirror.In addition, the sintered ferrite magnet of the present embodiment can be used as a member of a motor for OA / AV equipment such as an FDD spindle, VTR capstan, VTR rotary head, VTR reel, VTR loader, VTR camera capstan, VTR camera rotary head, VTR cameraazoom, VTR cameraocus, capstan of a radio cassette recorder, CD / DVD / MD spindle, CD / DVD / MD recording and CD / DVD optical recording.Further, the sintered ferrite magnet of the present embodiment can be used as a member of a motor for a household appliance, a compressor of an air conditioner, a compressor of a freezer, a drive of an electric tool, a fan of a dryer, a drive for a shaving apparatus, and an electric toothbrush. Further, the sintered ferrite magnet of the present embodiment can be used as an element of a motor for FA equipment such as a robot axis, joint drive, robot main drive, table drive for a machine tool, and machine tool rack drive.Examples of other applications include elements of a dynamo for motorcycle, magnet for speaker / earphone, magnetron tube, MRI specific magnetic field generating devices, terminals for CD-ROM, sensor for manifold, sensor for ABS, fuel / oil level sensor, magneto lock, insulator, generator and the like. Alternatively, the sintered ferrite magnet of the present invention can also be used as a target (pellet) when a magnetic layer of a magnetic recording medium is formed by a vapor deposition method, a sputtering method or the like.ExamplesHereinafter, the present invention will be explained based on more detailed examples, but is not limited to these examples.Example 1< Steps>CaCO 3, La 2 O 3, SrCO 3, Fe 2 O 3, Co 3 O 4 and MnO were prepared and weighed as starting materials, so that the compositions of each sample described in Table 1 to Table 4 were obtained. Further, 0.35 mass % of SiO 2 as an Si component was weighed with respect to 100 mass % of the starting materials.Incidentally, in Table 1, samples were prepared in which the atomic ratio Mn (a) was changed. In Table 2, samples were prepared in which the atomic ratio of Co (m) was changed. In Table 3, samples were prepared in which the atomic ratio of La (w) was changed. In Table 4, samples were prepared in which the kind of "A" element and the atomic ratio of "A" (x) were changed.The respective powders of the above-described starting materials and SiO 2 were mixed and pulverized by a wet attritor, and a slurry of the starting material mixture was obtained.<Calcination Step>After drying this raw material mixture, calcination treatment was performed by holding it for 2 hours at 1200° C. in an atmosphere to obtain a calcined body.< Step>The obtained calcined body was roughly pulverized with a rod tube mill, and a roughly pulverized material was obtained. CaCO 3, La 2 O 3, SrCO 3, Fe 2 O 3, Co 3 O 4, MnO, and SiO 2 were each appropriately added to the obtained roughly pulverized material so that the metal elements constituting the (fired) ferrite sintered magnet had the ratios indicated for each sample described in Table 1 to Table 4.Then, fine pulverization was carried out for 28 hours by means of a wet ball mill, and a slurry was obtained. The obtained slurry was converted into a slurry suitable for wet pressing by adjusting the solid concentration to 70-75 mass %.<Press and Firing Steps>Subsequently, a preliminary green body was obtained using a magnetic field wet pressing apparatus. The pressing pressure was 50 MPa and the applied magnetic field was 800 kA / m. In addition, the pressing direction and the application direction of the magnetic field during pressing were identical directions. The preliminary green body obtained by wet pressing was disc-shaped and had a diameter of 30 mm and a height of 15 mm.The green temporary body was fired while being maintained at 1190° C. to 1230° C. in the atmosphere for 1 hour, and a ferrite sintered magnet, which was a sintered body, was obtained.Example 2In Example 2, a ferrite sintered magnet was obtained similarly to Example 1 except that Sr and Ba were used as the "A" element, the atomic ratio of Sr was 0.08, the atomic ratio of Ba was 0.07, and the atomic ratio x of "A" was 0.15 (= 0.08 + 0.07), as shown in Table 5.Example 3In Example 3, a ferrite sintered magnet was obtained similarly to Example 1 except that samples in which the atomic ratio of Fe (z) was changed were prepared as shown in Table 6.Example 4In Example 4, a calcined body was prepared similarly to Example 1 by providing SiO 2 in addition to the starting materials and weighing SiO 2 to obtain the compositions of each sample described in Table 7 in the mixing step and by mixing an SiO2powder in addition to the starting materials with a wet attritor, etc. during the calcining step. In Example 4, a ferrite material powder was obtained similarly to Example 1 by appropriately adding CaCO 3, La 2 O 3, SrCO 3, Fe 2 O 3, Co 3 O 4, MnO, and SiO 2 to the obtained roughly pulverized material, so as to obtain the values indicated for each sample described in Table 7 in the pulverization step. In Example 4, a ferrite sintered magnet was obtained similarly to Example 1 except for the above steps.Example 5In Example 5, a calcined body similar to Example 1 was obtained in which Cr 2 O 3 was provided in addition to the starting materials and Cr 2 O 3 was weighed to obtain the compositions described for each sample in Table 8 in the mixing step, and by mixing a powder of Cr 2 O 3 in addition to the starting materials with the wet attritor, etc. in the calcining step. In Example 5, a ferrite material powder was obtained similarly to Example 1, in which CaCO 3, La 2 O 3, SrCO 3, Fe 2 O 3, Co 3 O 4, MnO, and Cr 2 O 3 were appropriately added to the obtained coarsely pulverized material, so as to obtain the values indicated for each sample described in Table 8 in the pulverization step. In Example 5, a ferrite sintered magnet was obtained similarly to Example 1 except for the above steps.Each of the ferrite sintered magnets of Examples 1 to 5 was subjected to X-ray fluorescence quantitative analysis, and it was confirmed that they had the compositions shown in Tables 1 to 8, respectively.Initially, each of the ferrite sintered magnets of Table 1 to Table 8 had the composition of Ca 1-w-x La w A x Fe z Co m Mn a O 19.Each of the ferrite sintered magnets of Table 1 was set to "A"=Sr, w=0.39, x=0.14, z=9.05, m=0.25, w / m=1.6 and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 2 was set to "A"=Sr, w=0.39, x=0.14, z=9.05, "a"=0.061, and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 3 was set to "A"=Sr, x=0.14, z=9.05, m=0.25, "a"=0.061, and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 4 was set to w=0.39, z=8.95, m=0.25, w / m=1.6, "a"=0.061, and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 5 was set to w=0.39, x=0.15, z=8.95, m=0.25, w / m=1.6, "a"=0.061, and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 6 was set to "A"=Sr, w=0.39, x=0.14, m=0.25, w / m=1.6, "a"=0.061, and SiO 2= 0,81 mass %.Each of the ferrite sintered magnets of Table 7 was set to "A" = Sr, w = 0.39, x = 0.14, z = 8.95, m = 0.25, w / m = 1.6, and "a" = 0.061.Each of the ferrite sintered magnets of Table 8 was set to "A"=Sr, w=0.39, x=0.14, z=8.95, m=0.25, w / m=1.6, "a"=0.061, and SiO 2= 0,81 mass %.It was confirmed by X-ray diffraction that the main phase of each of the ferrite sintered magnets of Table 1 to Table 8 was a ferrite phase having a hexagonal crystal structure.<Messung of Magnetic Properties (Br, HcJ, Hk)>After working the upper and lower surfaces of each of the ferrite sintered magnets of Examples 1 to 5, magnetic properties (residual magnetic flux density Br, coercive force HcJ, and squareness ratio Hk / HcJ) were measured using a B-H maximum applied magnetic field tracer of 1989 kA / m in an air atmosphere at 25° C. Table 1 to Table 7 show the results of Examples 1 to 4. Hk is a magnetic field intensity at a time when the magnetic flux density is 90% of the residual magnetic flux density in a second square of a magnetic hysteresis loop.<>The moldability was evaluated by the following method.Each of the 100 ferrite sintered magnets of Examples 1 to 5 was observed. The case where a magnet had 0 to 5 fractures, fractures or cracks was considered to be the best and was denoted by A, the case where a magnet had 5 to 10 fractures, fractures or cracks was considered to be extremely good and was denoted by B, the case where a magnet had 11 to 15 fractures, fractures or cracks was considered to be good and was denoted by C, and the case where a magnet had 16 or more fractures, fractures or cracks was considered to be poor and was denoted by D. The results are shown in Table 1 and Table 8, and the other results except for Table 1 or Table 8 will be described laterTable 1 to Table 7 show the evaluation results of the compositions and magnetic properties of each sample of Examples 1 to 4.Table 8 shows the evaluation results of the compositions and the moldability of each of the samples of Examples 1 to 4.Figs. 2 (2A, 2B and 2C) to 7 (7A, 7B and 7C) show the compositions and magnetic properties of each sample of Examples 1 to 4. Table 110,044449,0413,273,2D. D20,046451,0418,283,0C. C30,049453,0424,387,1C. C40,054457,0432,590,5A. A50,061458,0440,490,8A. A60,072457,5440,388,7A. A70,079456,6439,587,6A. A80,097455,2437,385,8B. B90,114455,0435,184,2B. B100,137453,7432,683,2C. C110,160448,9430,079,1C. C120,188445,3428,077,4C. C130,246438,9387,069,8D. DComposition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed to"A"=Sr, w=0.39, x=0.14, z=9.05, m=0.25, w / m=1.6, SiO 2=0,81 mass %A... best, B... extremely good, C... gut, D... poor Table 2Table 2210,142,79435,2330,190,1220,182,17451,2416,285,1230,211,86455,3426,189,8240,231,70457,1431,490,0250,251,56458,0440,490,8260,281,39459,2445,288,2270,311,26459,6455,783,2280,361,08458,7447,881,2290,410,95457,6427,076,8300,520,75445,3350,668,9Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed to"A"=Sr, w=0.39, x=0.14, z=9.05, a=0.061, SiO 2=0,81 mass % Table 3Table 3310,080,780,32418,7328,789,7320,210,650,84442,1414,288,6330,240,620,96454,0416,588,9340,310,551,24457,0423,189,1350,340,521,36457,5437,289,6360,390,471,56458,0440,490,8370,440,421,76456,8442,590,1380,510,352,04455,3443,687,8390,560,302,24452,3415,184,8400,620,242,48451,1390,180,2410,690,172,76435,2294,071,0Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed to"A"=Sr, x=0.14, z=9.05, m=0.25, a=0.061, SiO 2=0,81 mass % Table 4Table 451SrR0,010,60450,2347,351,652SrR0,020,59451,4382,576,353SrR0,040,57454,0417,281,254SrR0,070,54456,2432,085,055SrR0,110,50457,3437,185,356SrR0,130,48458,2439,888,057SrR0,150,46458,0440,490,858SrR0,170,44457,9438,587,159SrR0,200,41457,8432,586,160SrR0,230,38457,0427,686,461SrR0,260,35456,2419,486,362SrR0,320,29455,1409,085,563SrR0,460,15454,5356,786,164SrR0,560,05454,1270,786,065BaBa0,050,56453,2413,881,366BaBa0,070,54454,6432,387,967BaBa0,100,51455,8434,888,568BaBa0,150,46457,3437,689,269BaBa0,210,40456,0433,386,270BaBa0,250,36455,5415,885,7Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed tow=0.39, z=8.95, m=0.25, w / m=1.6, a=0.061, SiO 2=0,81 mass % Table 5Table 571Sr+Ba0,080,07458,2438,788,2Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed tow=0.39, x=0.15, z=8.95, m=0.25, w / m=1.6, a=0.061, SiO 2=0,81 mass % Table 6Table 6816,20429,7347,874,8827,43439,7376,578,1838,02445,5401,185,2848,24448,1415,286,0858,51452,2425,386,8868,72455,8432,290,0879,05458,0440,490,8889,21457,9439,291,1899,52457,9437,690,2909,81457,0435,189,09110,05456,7433,388,69210,23455,2427,189,19310,51453,6416,889,59410,65452,8410,188,59511,03452,2392,387,29611,45451,0317,188,5Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19, fixed to"A"=Sr, w=0.39, x=0.14, m=0.25, w / m=1.6, a=0.061, SiO 2=0,81 mass % Table 7Table 71010,38464,6397,164,31020,52463,3409,078,91030,59462,1420,085,11040,64459,7432,188,81050,81458,0440,490,81060,86457,6449,590,11070,92456,0450,189,01081,01454,5445,484,51091,18453,2426,081,31101,22451,0387,372,7Composition: Ca 1-w-x La w A x Fe z Co m Mn a O 19A value is defined as "A"=Sr, w=0.39, x=0.14, z=8.95, m=0.25, a=0.061 Table 8Table 81110,00A. A1120,01A. A1130,03A. A1140,04A. A1150,05A. A1160,08A. A1170,10B. B1180,15B. B1190,30B. B1200,50C. C1210,98C. CComposition: Ca 1-w-x La w A x Fe z Co m Mn a O 19 fixed to"A"=Sr, w=0.39, x=0.14, z=9.05, m=0.25, a=0.061, SiO 2=0,81 mass %A... best, B... extremely good, C... gut, D... poorIt was confirmed by Table 1 and FIG. 2 (2A, 2B and 2C) that the range of the atomic ratio of Mn (a) is preferably 0.049 ≦ a ≦ 0.114.It was confirmed by Table 2 and Fig. 3 (3A, 3B and 3C) that the range of the atomic ratio of Co (m) is preferably 0.18 ≦ m ≦ 0.41. Incidentally, each sample in Table 2 had a moldability of A to C.It was confirmed by Table 3 and FIG. 4 (4A, 4B and 4C) that the range of the atomic ratio of La (w) is preferably 0.21 ≦ w ≦ 0.62. Incidentally, each sample in Table 3 had a moldability of A to C.From Table 2 and Table 3, it was confirmed that the range of La / Co (w / m) is preferably 0.84 to 2.48.It was confirmed by Table 4, Table 5 and Fig. 5 (5A, 5B and 5C) that when the "A" element is at least one element selected from a group consisting of Sr and Ba, the range of the atomic ratio "A" (x) is preferably 0.02 ≦ x ≦ 0.46. Incidentally, each sample in Table 5 had a moldability of A to C.It was confirmed from Table 6 and Fig. 6 (6A, 6B and 6C that the atomic ratio of Fe (z) is preferably in a range of 7.43 ≦ z ≦ 11.03. Incidentally, each sample in Table 6 had a moldability of A to C.It was confirmed by Table 7 and FIG. 7 (7A, 7B, and 7C) that the amount range of SiO 2 is preferably 0.52% by mass to 1.18% by mass. Incidentally, each sample in Table 7 had a moldability of A to C.From Table 8, it was confirmed that the amount range of Cr 2 O 3 is preferably 0.98% by mass or less. Incidentally, as for the magnetic properties of each of the ferrite sintered magnets of Table 8, Br was 439 mT or more and HcJ was 352 kA / m or more.[Description of Reference Numerals]10 sintered ferrite magnet

Claims

A ferrite sintered magnet comprising a composition expressed by a following formula (1), Ca 1-w-x La w A x Fe z Co m Mn a O 19(1) wherein "w", "x", "z", "m" and "a" in the formula (1) are the following formulae (2), (3), (4), (5), and (6), and 0.21 ≦ w ≦ 0.62 0,02 ≦ x ≦ 0.46 7,43 ≦ z ≦ 11.03 0,18 ≦ m ≦ 0.41 0,049 ≦ a ≦ 0.114 " A" in the formula (1) is at least one kind of element selected from a group consisting of Sr and Ba.The sintered ferrite magnet according to claim 1, wherein w / m is 0.84-2.48.The ferrite sintered magnet according to claim 1 or 2, wherein Si is further contained at 0.52 mass% - 1.18 mass% with respect to SiO 2.The ferrite sintered magnet according to any one of claims 1-3, wherein Cr is further contained at 0.98 mass% or less with respect to Cr 2 O 3.

Citation Information

Patent Citations

  • Ferrite magnetic material

    WO2011004791A1

  • Ferrite magnetic material, ferrite sintered magnet, and motor

    WO2014021426A1

  • Ferrite sintered magnet

    JP2015130493A

  • Ferrite magnetic material

    US20120161910A1

  • JP002015130493A