Method for welding two components together

The described welding process addresses error detection and correction in complex geometries by using a quality assessment system and AI-optimized second weld seams to improve weld quality and reduce cracking and personnel costs.

DE102023001602A1Pending Publication Date: 2024-10-24MERCEDES BENZ GROUP AG

Patent Information

Application Number
DE102023001602
Authority / Receiving Office
DE · DE
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing welding processes struggle with identifying and correcting welding errors, particularly in complex geometries like lily seams, leading to potential cracking and increased personnel costs due to manual intervention.

Method used

A procedure that involves producing a first weld seam, assessing it for errors using a quality assessment system, categorizing the error type, and applying additional welding parameters to correct the errors through a second weld seam, optimized by artificial intelligence, to achieve a reliable connection.

Benefits of technology

This method reduces component rejection, lowers personnel costs, and enhances automation, ensuring high-quality welds with reduced cracking, particularly suitable for welding components like cell connectors and pole contacts in battery cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention relates to a method for welding two components (B1, B2), wherein a first weld seam (S1) connecting the two components (B1, B2) is produced and this first weld seam (S1) is subsequently evaluated by a quality assessment system (1), wherein, in the event of a detected weld seam defect (F) s ) this weld defect (F s ) is categorized into an error type (F1 to Fn). According to the invention, the defective first weld (S1) is at least partially welded over in the correct position using welding parameters specified according to the type of defect (F1 to Fn).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method for welding two components according to the features of the preamble of claim 1.

[0002] As described in EP 1 618 984 B1, a laser welding process is known from the prior art in which welds are monitored for welding defects and, if necessary, repair welds are performed. Potential welding defects and associated sets of repair welding parameters are stored in advance. A detected defective weld is compared with the stored welding defects. If the comparison is positive, a repair weld is performed in the area of ​​the defective weld using the repair welding parameters associated with the detected welding defect.

[0003] The invention is based on the object of providing a method for welding two components that is improved compared to the prior art.

[0004] The object is achieved according to the invention by a method for welding two components having the features of claim 1.

[0005] Advantageous embodiments of the invention are the subject of the subclaims.

[0006] In a method for welding two components, a first weld seam connecting the two components is produced and this first weld seam is subsequently evaluated by a quality assessment system, wherein if a weld seam defect is detected, this weld seam defect is categorized into a defect type, ie in particular is assigned to one of several predetermined defect types, ie is classified therein.

[0007] According to the invention, the defective first weld seam is at least partially, i.e. at least partially overlapping, welded over in a position that is accurate to the position, using welding parameters that are predetermined according to the type of defect and thus using a welding program that is individual according to the type of defect. By welding over, in particular, a second weld seam is produced, which can be arranged on the first weld seam and / or can partially or completely surround it. For example, by welding over and thus by producing the second weld seam, the first weld seam is partially or completely melted. By this partial or complete re-melting of the first weld seam, its geometry and characteristics are corrected, so that the overall connection is satisfactory after this repair. In other words, a final weld seam orThe entire weld seam consists of a first and second weld seam.

[0008] The inventive method enables a reduction in component scrap and thus improved cost and sustainability. The method can be carried out with a high degree of automation, thus requiring minimal personnel expenditure. The method is particularly suitable for repairing fillet welds on joining partners, i.e., components to be joined, made of similar materials. For example, both components to be joined are made of aluminum or an aluminum alloy. With such joints, repeated welding is trivial and possible without increased crack formation. With different material combinations, there is a risk of crack formation.

[0009] The method, in particular the defect detection and repair by overwelding, can be directly integrated into an existing production process, as this can be carried out using identical plant technology, in particular with identical welding equipment, for example, laser welding equipment, hold-down clamps, and all other required components. For example, an existing quality assessment system can also be used, which then only needs to be modified if necessary so that it can perform defect detection and categorize the respective defect type. The method according to the invention is thus, for example, a further development of a conventional welding process in which the two components are previously welded together, with the additional process steps mentioned above.

[0010] The method according to the invention requires only a small amount of space on the components, since the original, ie the first, weld seam is welded over in the correct position.

[0011] The method according to the invention, for example, opens up new design possibilities.

[0012] The method according to the invention is particularly suitable for the repair of cell connector connections on battery cells, for example on prismatic hardcase cells or round cells.

[0013] Particularly due to the achievable advantages described above, it is specifically intended that the first weld seam be a fillet weld, i.e., that a fillet weld is welded as the first weld seam in the process. A fillet weld is always formed when the two components overlap in some areas and the upper component is welded into the lower component at its end.

[0014] Particularly due to the achievable advantages described above, it is provided in particular that a cell connector and a pole contact of a battery cell of a battery, in particular a drive battery for a vehicle, are welded together as components. The method is thus intended in particular for welding a cell connector, in particular to a pole contact, by means of a first weld seam designed as a fillet weld and for repairing the defective first weld seam and thus for repairing a resulting defective electrically conductive contact. Such electrically conductive contacts, which are produced via fillet welds on cell connectors, can be subject to various weld seam defects as a result of a production or welding process, in particular a laser welding process. Special component geometries, for example component curvatures, also severely limit the possible welding area.

[0015] The special feature of the fillet weld is that its strength and current-carrying capacity are limited by an A dimension. According to DIN EN ISO 2553, the A dimension of the fillet weld is the height of an isosceles triangle, which can be drawn into the weld cross-section. The A dimension of the fillet weld after overwelding can be composed of parts of the first weld and the second weld. If the power used during laser welding is too low, the first weld can be completely overlaid by the second weld, for example, or the first weld can be completely melted into the second weld.

[0016] Particularly due to the achievable advantages described above, it is intended that the components be welded together by laser welding and / or that the over-welding be carried out by laser welding. Laser welding is also referred to as laser beam welding.

[0017] For example, the quality assessment system is intended to evaluate the first weld seam using a camera and / or triangulation. A camera used for this purpose can be, for example, a 2D camera, in particular a mono camera, a 3D camera, in particular a stereo camera, or a line scanner.

[0018] In particular, it is intended that, in advance, i.e., before the first welds are produced in a production process, defect types and the welding parameters associated with the respective defect type are stored in a database. From this database, the defect types for the above-described categorization of the detected weld defect of the first weld and the welding parameters associated with the relevant category, i.e., the categorized defect type, can then be retrieved.

[0019] The evaluation of the first weld, the categorization of the detected weld defect into a defect type and / or a selection of the welding parameters specified according to the defect type is carried out, for example, using artificial intelligence.

[0020] The welding parameters include, for example: - a scan width for laser welding, - a weld position of a second weld to be created by overwelding, - a power distribution over a beam path for laser welding, - power modulation via a beam path for laser welding, and / or - an angle of incidence for laser welding.

[0021] The scan width is particularly relevant for wobble welding. Wobble welding is a possible technique in laser welding. In wobble welding, the laser beam is guided across a welding path at a low amplitude, perpendicular to the feed. Using wobble welding, which operates similarly to a stirring process, a wider second weld seam can be achieved through the deflection of the welding beam.

[0022] For the evaluation of the first weld seam by the quality assessment system, the following values ​​are determined, for example: - a weld seam width, - a weld seam position, - a weld height, and / or - at least one weld defect.

[0023] The types of defects into which the detected weld defect can be categorized include, for example: - no or insufficient welding depth, - a strong weld collapse and / or an insufficient A-dimension of the first weld seam formed as a fillet weld, - a weld roughness and / or a weld reinforcement, - an incorrect weld position, and / or - Holes and / or pores in the first weld.

[0024] In particular, camera-based measurements can be used to detect the weld roughness and / or weld reinforcement, the weld position, holes and / or pores in the first weld.

[0025] The A-dimension of the fillet weld cannot be recorded directly by camera image. Therefore, it is specifically planned that camera images of the fillet weld are taken after welding and linked to a corresponding A-dimension. As already mentioned above, it is specifically planned that defect types and the welding parameters assigned to the respective defect type are stored in the database in advance, i.e. before the first welds are produced in a production process. With regard to the defect type or types relating to the A-dimension, it is specifically planned that a plurality of fillet welds are welded in advance and their A-dimension is then examined. An A-dimension is then assigned to the respective fillet weld recorded by camera image. The assignments are then stored in the database. The quality assessment system therefore has camera images of welds, each of which is linked to an A-dimension.In this way, the weld seam defect identified in the described method can then be categorized, for example, as an insufficient A-dimension defect if this is determined by comparing the recorded camera image of the first weld seam produced with the camera images stored in the database and associated with an insufficient A-dimension. The quality assessment system can thus assign the recorded camera image of the first weld seam to a corresponding camera image in the database and thus assign the A-dimension linked to this camera image in the database to the first weld seam.

[0026] When artificial intelligence is used, it can access the data in the database or be trained using this data. When artificial intelligence is used, it is particularly intended that it continuously trains and optimises itself. After welding over, i.e. after the second weld seam has been produced, a camera image is again taken using the quality assessment system's camera of a final weld seam consisting of the first and second weld seam. After the repair process, a camera image is taken using the camera and the overall result is documented. The overall results that arise with similar initial fillet welds, i.e. with similar first weld seams, can be compared with one another and an optimum overall result can be assigned to an optimum target state and saved as an optimum, for example in the database.This allows optimized welding parameters to be assigned to each first weld seam for its overwelding. The artificial intelligence learns / trains itself to determine which repair process, and thus which welding parameter set, is most promising for a particular faulty first weld seam, especially a fillet weld. The artificial intelligence can optimize the procedure or repair process by comparing repair results to determine whether a repair process result is better than a previous result in similar initial situations. The better result achieved can therefore be assigned a higher rating and saved in the database, and this better result can be used for subsequent welding processes.

[0027] This training of the artificial intelligence can, for example, be carried out in advance using welded and subsequently inspected fillet welds, as described above, and / or during the production process, i.e., even while the first welds are being welded in the production process and, if they are defective, are welded over in the manner described above. Advantageously, a combination of these two options is provided: first, the training in advance to achieve a sufficiently high level of artificial intelligence to perform the process sufficiently well, and then the ongoing training of the artificial intelligence during the production process to further optimize the results as far as possible.

[0028] An apparatus for carrying out the method described herein is also provided.

[0029] Embodiments of the invention are explained in more detail below with reference to drawings.

[0030] Showing: Fig. 1 schematically shows an example of welding components with two defective first welds and subsequent over-welding of the two first welds, Fig. 2 schematically shows an example of detecting a weld defect of the first weld and the subsequent overwelding of the first weld, Fig. 3 schematically shows another example of detecting a weld defect of the first weld and the subsequent overwelding of the first weld, Fig. 4 schematically shows a process sequence for detecting a weld defect in the first weld and subsequently overwelding the first weld, Fig. 5 schematically shows a process sequence of a method for welding two components, and Fig. 6 schematically shows a sequence of a development and learning phase, in particular a training of an artificial intelligence, for the method for welding two components before its application in a production process.

[0031] Corresponding parts are provided with the same reference numerals in all figures.

[0032] Based on the Fig. 1 to 6, a method for welding two components B1, B2 is described below. In the examples shown, the components B1, B2 to be welded together are a cell connector and a terminal contact of a respective battery cell of a battery, in particular a drive battery for a vehicle. The cell connector is the first component B1, and the terminal contact of the respective battery cell is the second component B2.

[0033] In Fig. 1, the cell connector is thus connected to the respective of the two second components B2 by a weld. This is also shown in the Fig. 2 and Fig. 3 is the case, where sectional views are shown, in which only one pole contact and only a part of the cell connector are shown. For a better understanding of the respective view, Fig. Figures 1 to 3 each depict a coordinate system with a Y-axis (Y) and a Z-axis (Z). The Y-axis (Y) forms a transverse axis and the Z-axis (Z) forms a vertical axis.

[0034] In the process described here, a first weld seam S1 connecting the two components B1, B2 is produced, here as a fillet weld, as shown in the Fig. 1 to 3 are shown on the left. In the examples shown, this is done using laser welding.

[0035] This first weld S1 is then assessed by a quality assessment system 1, as described in the Fig. 2 and Fig. 3 is shown as an example on the left side, in particular camera-based and / or using triangulation. A camera used for this purpose can be, for example, a 2D camera, in particular a mono camera, a 3D camera, in particular a stereo camera, or a line scanner. If a weld defect F is detected, s this weld defect F s categorized into error types F1 to Fn.

[0036] Subsequently, the defective first weld seam S1 is to be over-welded at least partially, i.e. at least partially overlying, in the correct position using welding parameters specified according to the defect type F1 to Fn and thus using an individual welding program according to the defect type F1 to Fn. Thus, a repair R is carried out. In the examples shown, this is also carried out using laser welding. Fig. 1 to 3 schematically show only one laser beam 2 of a laser welding device carrying out this laser welding.

[0037] By means of the overwelding U, a second weld seam S2 is produced, which can be arranged on the first weld seam S1 and / or can partially or completely surround it. For example, by means of the overwelding U and thus by means of the production of the second weld seam S2, the first weld seam S1 is partially or completely melted. By means of this partial or complete re-melting of the first weld seam S1, its geometry and shape are corrected, so that the overall connection is satisfactory after this repair R. By means of the overwelding U, an overall seam GN is thus formed, which encompasses the second weld seam S2 and can include areas of the first weld seam S1 that were not melted. If the first weld seam S1 has been completely melted, the overall seam GN consists only of the second weld seam S2 created by the overwelding U.

[0038] The defect types F1 to Fn, into which the detected weld defect F s can be categorised, for example: - no or insufficient welding depth, - a strong weld collapse and / or an insufficient A-dimension A of the first weld seam S1 formed as a fillet weld, - a weld roughness and / or a weld reinforcement, - an incorrect weld seam position Y s , and / or - Holes and / or pores in the first weld S1.

[0039] Fig. Figure 1 shows, as an example, the defect types F1 to Fn of non-existent or insufficient penetration using the left first weld seam S1, and the defect types F1 to Fn of severe weld collapse and thus an insufficient A dimension A using the right first weld seam S1. On the right side, the overwelding U of these defective first weld seams S1 is shown with the welding parameters specified for the respective defect types F1 to Fn.

[0040] The welding parameters include, for example: - a scan width S B for laser welding, - a weld seam position Y s a second weld seam S2 to be created by overwelding U, - a power distribution over a beam path for laser welding, - power modulation via a beam path for laser welding, and / or - an angle of incidence for laser welding.

[0041] The scan width S B is particularly relevant for wobble welding. Wobble welding is a possible procedure for laser welding. In wobble welding, the laser beam 2 is guided with a small amplitude a across a welding path, as shown in the Fig. 1 to 3 are shown on the right. Here, laser beam 2 is shown in one transverse deflection with solid lines and in the other transverse deflection with dashed lines. Using wobble welding, a wider second weld seam S2 can be achieved with the described welding beam deflection.

[0042] The Fig. 2 and Fig. 3 shows, on the left, an example of the assessment B of the first weld seam S1 by the quality assessment system 1, in particular camera-based and / or using triangulation. For this purpose, it is particularly intended that the components B1, B2, especially in the area of ​​the first weld seam S1, and the first weld seam S1 are measured. For example, the following values ​​are determined: - a weld seam width b s , - a weld seam position Y s in the Y-axis direction, - a weld height h s , and / or - at least one weld defect F s .

[0043] In Fig. 2 a weld collapse is classified as weld defect F s The weld defect F s is thus categorized into defect types F1 to Fn seam collapse.

[0044] This results in the corresponding welding parameters for the Fig. 2 overwelds U shown on the right. In the example shown, these are a given scan width S B , a given weld seam position Y s in the Y-axis direction, and a power P along the beam path. In the example shown, three points A L , B L , C L and the power P at the respective point A L , B L , C L specified, shown as an example in a performance chart.

[0045] Fig. 3 shows the special feature regarding the fillet weld and the A-dimension A. The Fig. 3 The first weld seam S1, schematically shown on the left, has an A dimension A that is too small. The overwelding U shown on the right increases the A dimension A to a sufficient value. It can be composed of parts of the first weld seam S1 and the second weld seam S2. The A dimension A limits the strength and current-carrying capacity.

[0046] The A-dimension A of the fillet weld cannot be directly captured using the camera image KB. Therefore, it is specifically planned that camera images KB of the fillet weld be taken after welding and linked to a corresponding A-dimension A.

[0047] In particular, it is intended that defect types F1 to Fn and the welding parameters associated with the respective defect types F1 to Fn are stored in a database in advance, i.e. before the first weld seams S1 are produced in a production process. From this database, the defect types F1 to Fn can then be used for the categorization K of the detected weld seam defect F described above. s the first weld S1 and the welding parameters assigned to the relevant category, ie the categorised defect type F1 to Fn, are retrieved.

[0048] With regard to the A-dimension A, it is particularly intended that a plurality of fillet welds are welded in advance, the A-dimension A of which is then examined. An A-dimension A is then assigned to the respective fillet weld recorded by camera image KB. The assignments are then stored in the database. Camera images KB of welds are thus available to the quality assessment system 1, each of which is linked to an A-dimension A. In this way, the weld defect F identified in the described method can then be sFor example, they can be categorized into defect types F1 to Fn of insufficient A-dimension A if this is determined by comparing the recorded camera image KB of the produced first weld seam S1 with the camera images KB stored in the database and assigned to an insufficient A-dimension A. The quality assessment system 1 can thus assign the recorded camera image KB of the first weld seam S1 to a corresponding camera image KB in the database and thus assign the A-dimension A linked to this camera image KB in the database to the first weld seam S1. The camera images KB can, for example, be analyzed using a suitable image processing program, and individual features of a camera image KB can be compared with individual features of another camera image KB.

[0049] Fig. 4 shows a procedure for detecting the weld defect F sof the first weld seam S1 and the subsequent overwelding U of the first weld seam S1. First, the weld defect F is determined s and then its categorization K into one of several defect types F1 to Fn. Depending on the defect type F1 to Fn, the repair R is then carried out by overwelding U the first weld S1 with the welding parameters assigned to the respective defect type F1 to Fn. The welding parameters assigned to the respective defect type F1 to Fn form, in particular, a respective welding parameter set SP1 to SPm. As in Fig. As shown in Figure 4 as an example, the same welding parameter set SP3 can be assigned to several fault types F3, F4.

[0050] Fig. Figure 5 shows the sequence of the method described herein. First, the first weld seam S1 is welded. A camera image KB of the first weld seam S1 is then acquired. Subsequently, the evaluation B, i.e., assessment, of the first weld seam S1 is performed based on the acquired camera image KB. This can be done, in particular, using artificial intelligence. If the first weld seam S1 is OK (i.e., OK), the process end PE is reached. If the first weld seam S1 is not OK (i.e., not OK), the welding defect F is detected, in particular, using artificial intelligence. s identified, categorized into a defect type F1 to Fn and the overwelding U of the first weld seam S1 is carried out with the welding parameters assigned to the respective defect type F1 to Fn, ie with the respective welding parameter set SP1 to SPm.

[0051] The method can advantageously be continued here, whereby the first weld seam S1 is now replaced by the entire weld seam GN created from the first weld seam S1 and the second weld seam S2. A camera image KB of the created entire weld seam GN is thus acquired. Subsequently, the evaluation B of the entire weld seam GN is performed based on the acquired camera image KB. This can be done, in particular, again using artificial intelligence. If the entire weld seam GN is now OK (iO), the process end PE is reached. If the entire weld seam GN is not OK (niO), the welding defect F is evaluated, again, in particular, using artificial intelligence. s identified, categorized into a defect type F1 to Fn and the overwelding U of the entire seam GN is carried out with the welding parameters assigned to the respective defect type F1 to Fn, ie with the respective welding parameter set SP1 to SPm.

[0052] This procedure can now be Fig. 5, as indicated schematically, the process continues with the overall seam GN produced in each case until the last overall seam GN produced is assessed as OK based on the captured camera image KB and thus the process end PE is reached.

[0053] As already mentioned above, it is particularly intended that in advance, i.e. before the first weld seams S1 are produced in the production process, defect types F1 to Fn and the welding parameters assigned to the respective defect type F1 to Fn are stored in the database, so that the defect types F1 to Fn for the above-described categorization K of the detected welding defect F s the first weld S1 and the welding parameters assigned to the relevant category, ie the categorised defect type F1 to Fn, can be retrieved.

[0054] This approach is exemplary in Fig. 6. On the one hand, several SiO welds are welded, which are OK, as shown in Fig. 6 above, and on the other hand several welds SniO welded, which are not in order, as in Fig. 6 shown schematically below.

[0055] After welding the SiO welds that are satisfactory, a camera image KB is captured of the respective SiO weld. Subsequently, an analysis of the respective SiO weld is performed, for example, by cross-section, computer tomography (CT), and / or other means. Geometric data GD of the respective SiO weld are determined, in particular the above-mentioned values ​​for weld width b. s , Weld seam position Y s , weld seam height h sand / or the A dimension A. The values ​​determined for the respective weld seam SiO are now assigned ZO to the camera image KB of the weld seam SiO and stored S in the database. As a result, as already described above, conclusions can be drawn in the method from a recorded camera image KB of a respective first weld seam S1 to the A dimension A and / or to the other stated values ​​of the first weld seam S1. As described, this is done in particular by means of artificial intelligence, ie the artificial intelligence has, for example, access to the database and / or the camera images KB are also stored in the artificial intelligence as an alternative or in addition to being stored in the database, and / or the artificial intelligence is trained using these camera images KB.

[0056] After welding the welds SniO that are not satisfactory, a camera image KB is also captured of the respective weld SniO. The categorization K of the welding defects F is then s into a respective defect type F1 to Fn and an assignment ZW of the camera image KB of the respective weld SniO to the defect type F1 to Fn, into which their welding defects F swas categorized. The respective weld seam SniO is then overwelded U, whereby welding parameters for the respective defect type F1 to Fn are specified. The overall weld GN produced in this way is then assessed B, i.e. the assessment B using the quality assessment system 1. If the overall weld GN is OK, the welding parameters are saved S in the database and / or in the artificial intelligence, or the artificial intelligence is trained using it. If the overall weld GN is not OK, the welding parameters are rejected V as unsuccessful. The process is then advantageously repeated with changed specified welding parameters. This is carried out in particular until welding parameters are found for the respective defect type F1 to Fn that lead to an assessment B of the overall weld GN produced as OK.

[0057] The advantages described herein relate to the method described herein and also relate to a device which is configured to carry out the method described herein. List of reference symbols 1 Quality assessment system 2 laser beam a amplitude A A-measure A L Point An analysis b s Weld seam width B rating B1, B2 component B L Point C L Point F Determination F1 to Fn error type F s Weld defects GD geometric data GN total seam h s Weld height OK OK K Categorization KB camera image not OK P Performance PE process end R Repair S Storage S1 first weld S2 second weld S B Scan width SiO weld seam OK SP1 to SPm welding parameter set SniO weld seam not OK U Overwelding V Discard Y Y-axis Y s Weld seam position Z Z-axis ZO assignment ZW allocation QUOTES CONTAINED IN THE DESCRIPTION

[0000] This list of documents submitted by the applicant was generated automatically and is included solely for the convenience of the reader. This list is not part of the German patent or utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature

[0000] EP 1618984 B1

[0002]

Claims

[1] Method for welding two components (B1, B2), wherein a first weld seam (S1) connecting the two components (B1, B2) is produced and this first weld seam (S1) is subsequently evaluated by a quality assessment system (1), wherein in the case of a detected weld seam defect (F s ) this weld defect (F s ) is categorised into an error type (F1 to Fn), characterized by that the defective first weld seam (S1) is at least partially welded over in the correct position using welding parameters specified according to the type of defect (F1 to Fn). [2] Method according to claim 1, characterized by that the first weld seam (S1) is a fillet weld. [3] Method according to one of the preceding claims, characterized by that a cell connector and a pole contact of a battery cell of a battery are welded together as components (B1, B2). [4] Method according to one of the preceding claims, characterized by that the components (B1, B2) are welded together by laser welding and / or the over-welding (U) is carried out by laser welding. [5] Method according to one of the preceding claims, characterized by that the quality assessment system (1) assesses the first weld seam (S1) using a camera and / or triangulation. [6] Method according to one of the preceding claims, characterized by that defect types (F1 to Fn) and welding parameters assigned to the respective defect type (F1 to Fn) are stored in a database in advance. [7] Method according to one of the preceding claims, characterized by that the welding parameters include: - a scan width (S B ) for laser welding, - a weld seam position (Y s ) a second weld seam (S2) to be produced by overwelding (U), - a power distribution over a beam path for laser welding, - power modulation via a beam path for laser welding, and / or - an angle of incidence for laser welding. [8] Method according to one of the preceding claims, characterized by that the evaluation (B) of the first weld (S1), the categorisation (K) of the detected weld defect (F s ) into a defect type (F1 to Fn) and / or a selection of the welding parameters specified according to the defect type (F1 to Fn) is carried out using artificial intelligence. [9] Method according to one of the preceding claims, characterized by that for the assessment (B) of the first weld (S1) by the quality assessment system (1) the following values ​​are determined: - a weld seam width (b s ), - a weld seam position (Y s ), - a weld seam height (h s ), and / or - at least one weld defect (F s ). [10] Method according to one of the preceding claims, characterized by that the defect types (F1 to Fn) into which the detected weld defect (F s ) can be categorised as follows: - no or insufficient welding depth, - a strong seam collapse and / or a too small A-measurement (A), - a weld roughness and / or a weld reinforcement, - an incorrect weld seam position (Y s ), and / or - Holes and / or pores in the first weld (S1).

Citation Information

Patent Citations

  • Laser welding process and device

    EP1618984B1

  • Method for joining an electronic contact

    DE102021005187A1

  • Laser welding process and device

    EP1618984A1

  • Repair welding control device and repair welding control method

    US20220097178A1

  • Repair welding inspection device and repair welding inspection method

    US20220120697A1

Cited By

  • Methods for quality assurance in laser beam welding and welding device for laser beam welding

    DE102024004189A1

  • Methods for quality assurance in laser beam welding and welding device for laser beam welding

    DE102024004189B4