Method for joining at least two components using a laser welding process and component arrangement
The laser welding method addresses the challenge of connecting temperature-sensitive components by using a high-speed, low-heat input path movement to create strong, defect-free welds, suitable for diverse materials and pre-assembled parts.
Patent Information
- Application Number
- DE102023002989
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-07-21
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2043-07-21
AI Technical Summary
Existing laser welding methods struggle to connect temperature-sensitive components without causing damage due to high heat input, especially when connecting components with adjacent temperature-sensitive materials or attachments.
A laser welding method that uses a specific path movement with a high speed and small beam diameter to create a weld seam with low temperature input, ensuring minimal thermal influence on surrounding areas, allowing connection of temperature-sensitive components and adjacent materials without damage.
The method enables reliable, high-strength welds with low electrical resistance, suitable for connecting components with different materials, and reduces assembly effort by allowing pre-assembled components with add-on parts, while minimizing defects and maintaining component integrity.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[0001] The invention relates to a method for joining at least two components by means of a laser welding method according to the preamble of claim 1. The invention further relates to a component arrangement having at least two components joined by means of such a method.
[0002] DE 103 50 953 A1 discloses a method for joining two elements made of metallic material, wherein at least a first element represents a cover layer as part of a composite material, which has a particularly heat-sensitive core and an outer cover layer. The connection is made by means of molten pool-protected fusion welding in a laser welding process such that a non-melted layer remains between the molten area and the core for a certain period of time. The joining process is controlled such that the cover layers are only partially melted. A high welding speed is set with a relatively low heat input.
[0003] DE 10 2022 000 181 A1 discloses an electrical contacting of components by means of a welded joint whose primary path has two ends. The electrical contacting is characterized in that a terminal contour of the welded joint, which has a curved profile, is arranged at each end of the primary path.
[0004] DE 10 2021 005 518 A1 discloses a method for producing a welded joint of at least two components by means of an energy beam, wherein a first component is arranged relative to at least one second component such that the first component and the at least one second component form at least one connecting region, wherein the at least one connecting region is subjected to an energy beam, wherein the energy beam is displaced relative to the first component and the at least one second component along a displacement direction, wherein the energy beam is deflected in an oscillating manner transversely to the displacement direction to form repeating oscillating paths, wherein the oscillating paths are spaced apart from one another at a distance such that the first component is welded to the at least one second component in the at least one connecting region,by a melt pool following each of the pendulum tracks mixing with the melt pool of the adjacent pendulum tracks and solidifying to form a weld seam.
[0005] US 2012 / 0 160 815 A1 discloses a method for laser lap welding by irradiating a laser beam from one side of a plurality of overlapped workpieces, the method comprising the steps of: scanning the laser beam in a forward direction along a predetermined portion of the workpieces; reversing the scanning direction of the laser beam at a terminal end of the predetermined portion; scanning the laser beam in a reverse direction and terminating the irradiation of the laser beam on the predetermined portion, wherein the scanning of the laser beam in the reverse direction is offset from the scanning of the laser beam in the forward direction such that a part of the weld formed by the laser scanning in the reverse direction overlaps the weld formed by the laser scanning in the forward direction.
[0006] JP 6 560 003 B2 discloses a welded structure comprising a first element and a second element. The second element is joined to the first element by laser welding and has a welded end portion with at least one weld line formed thereon. Each end of the weld line is separated by an outer circumferential line enclosing the welded end portion with the shortest length.
[0007] The invention is based on the object of providing a novel method for joining at least two components by means of a laser welding method, and a novel component arrangement with at least two components joined by means of such a method.
[0008] The object is achieved according to the invention by a method which has the features specified in claim 1 and by a component arrangement which has the features specified in claim 9.
[0009] Advantageous embodiments of the invention are the subject of the subclaims.
[0010] In a method for joining at least two components using a laser welding process, the components are arranged relative to one another such that they lie against one another in an overlapping region. According to the invention, to produce at least one weld seam in the overlapping region, a laser beam is guided in a path-like movement over a surface of one of the components. During the path-like movement, a closed path is traced across the surface, in the region of which the components are melted and, after solidification, are joined to one another in a material-to-material manner. The path has a first circular arc of a first circular segment having a radius and a second circular arc of a second circular segment running concentrically to the first circular arc and having a larger second radius, wherein the circular segments have a matching central angle and the first circular segment is completely contained in the second circular segment.The path further comprises a curved first partial path tangentially adjoining an end of the first circular arc located on a first radius of the first circular segment, which is tangentially connected to a start of the second circular arc located on the first radius of the second circular segment. Furthermore, the path comprises a curved second partial path tangentially adjoining an end of the second circular arc located on a second radius of the second circular segment, which is tangentially connected to a start of the first circular arc located on the second radius of the first circular segment.The laser beam is guided at a path speed of at least 10 meters per minute (m / min), for example 15 m / min or 20 m / min, and emitted in such a way that at an impact point on the surface it has a beam diameter in a range between 50 micrometers (µm) and 250 µm, for example in a range of 100 µm to 200 µm.
[0011] When joining temperature-sensitive components or components with adjacent temperature-sensitive components and / or attachments in a fusion welding process, impairments and damage caused by the introduced process heat and the resulting heating of the components to be joined as well as the components and / or attachments must be avoided.
[0012] By means of the present method, a weld seam geometry is advantageously created due to the movement of the laser beam along the path at the path movement speed and the beam diameter. Compared to wobble welds with superimposed beam oscillation, for example, this results in a very low temperature input while simultaneously providing a broad connection between the weld seam and the components. Due to the high welding speed and the small incident beam cross-sectional area, the overlapping components are only melted very locally, and the surrounding areas are only minimally thermally affected. To widen the weld seam and connect a component, the path is traversed. This means that even temperature-sensitive components and components with temperature-sensitive components and / or attachments arranged adjacent to the weld seam can be fusion-welded without damaging the components, components, and attachments.This makes it possible, for example, to prevent melting of surrounding plastics when welding metallic materials, thus preventing the ingress of plastics into the weld seam and thus preventing defects that impair the weld quality. The weld seam created in this way is characterized by high strength and current-carrying capacity with low electrical resistance. Furthermore, the process can be carried out quickly with a short cycle time. Because the weld seam geometry is adjusted by selecting the center angle, additional welds with the same criteria can also be added. Furthermore, the process enables the joining of components made of different or similar materials, for example, components made of aluminum, copper, steel, nickel-plated steel, etc.The process can also be carried out using conventional laser welding system technology, particularly with laser scanner welding optics, so no additional hardware is required to carry out the process. Due to the weld seam geometry, the process is particularly suitable for joining components in an overlapping manner, where at least one of the components has a round cross-section. This allows, for example, connections between the cell poles of cylindrical battery cells and cell connectors and connections to power electronics to be created.
[0013] According to one possible embodiment of the method, the laser beam is guided such that the beginning and end of the path lie on the first circular arc or the second circular arc. This ensures that the required distance from temperature-sensitive sections of the parts, components, and / or attachments is reliably maintained. Since the beginning and end of the weld seam represent potential weak points in a weld seam, the design in which the beginning and end of the path lie on the first, inner circular arc prevents these points from pointing outward along the overall contour.
[0014] According to another possible embodiment of the process, the laser beam is guided such that the beginning and end of the path are at half the center angle. This enables reliable and reproducible creation of the weld seam with a homogeneous appearance.
[0015] According to another possible embodiment of the method, the center angle is selected in a range between 5° and 270°. Such center angle values have proven particularly advantageous for reliable weld seam production.
[0016] According to another possible embodiment of the method, the radius of the first circular arc is selected to be greater than 5 mm, for example, 7 mm or 10 mm. Such values for the radius of the first circular arc have proven particularly advantageous for reliably producing the weld seam.
[0017] According to another possible embodiment of the method, the radius of the second circular arc is selected to be less than 75 mm, for example, 70 mm or 60 mm. Such values for the radius of the second circular arc have proven particularly advantageous for reliably producing the weld seam.
[0018] According to another possible embodiment of the method, a difference between the radius of the second circular arc and the radius of the first circular arc is selected to be less than 10 mm, for example, 8 mm, 6 mm, or 5 mm. This enables the creation of a weld seam geometry with very low heat input, despite the high path speed and small beam diameter of the laser beam, while simultaneously ensuring a wide connection between the weld seam and the components.
[0019] According to a further possible embodiment of the method, at least one of the components has, on its side facing away from the other component, a connected attachment with a material recess that completely penetrates the attachment, wherein the laser beam is guided through the material recess such that the path runs at a distance from sections of the attachment that delimit the material recess. In this way, heat input into the attachment is minimized, so that damage to the latter can be avoided. Furthermore, this makes it possible for components with attachments to be fed to the welding process in a pre-assembled state, thus reducing assembly effort or even enabling the assembly of components with attachments to other components.
[0020] The component assembly according to the invention comprises at least two components joined by means of a method described above. Due to the low temperature input during welding of the components, they exhibit no welding-induced damage, thus maximizing their reliability and service life. At the same time, the weld seam is broadly connected to the components.
[0021] According to one possible configuration of the component arrangement, one of the components is an electrical cell terminal of a battery cell, and the other component is a cell connector. The weld seam connecting the components is characterized by high strength and current-carrying capacity with low electrical resistance, which allows an electric battery containing the battery cells to be highly efficient and operate reliably.
[0022] According to one possible configuration of the component arrangement, one of the components is a power electronics unit and the other is an electrical connector. The weld seam connecting the components is characterized by high strength and current-carrying capacity with low electrical resistance, thus optimizing the function of the power electronics.
[0023] Embodiments of the invention are explained in more detail below with reference to drawings.
[0024] Showing: Fig. 1 schematically shows a perspective view of a first embodiment of a component arrangement, Fig. 2 schematically shows a plan view of a path movement carried out to produce a weld seam by means of a laser beam and Fig. 3 schematically shows a perspective view of a second embodiment of a component arrangement.
[0025] Corresponding parts are provided with the same reference numerals in all figures.
[0026] In Fig. 1 shows a perspective view of a first possible embodiment of a component arrangement 1.
[0027] The component arrangement 1 comprises two components 2, 3, for example, formed of metal, which have a round contour at least in sections and lie adjacent to one another in an overlapping area UB. For example, a lower component 2 is an electrical cell terminal of a cylindrical battery cell, and an upper component 3 is a cell connector for electrically connecting the cell terminal to other cell terminals of other battery cells or electrical connections.
[0028] A connected attachment 4 with a material recess completely penetrating the attachment 4 is attached to the upper component 3 on a side facing away from a lower component 2. The attachment 4 is formed, for example, from a plastic and is intended for electrical insulation, as is known, for example, from Fig. 1 becomes apparent.
[0029] The components 2, 3 are connected to each other in sections by means of a weld seam S1.
[0030] A possible embodiment of a method for producing such a weld seam S1 is described below with reference to Fig. 2 is explained in more detail. Fig. 2 schematically shows a plan view of a path movement carried out by means of a laser beam to produce the weld seam S1.
[0031] Before welding, the components 2, 3 are first arranged in such a way that they lie against each other in the overlap area UB.
[0032] Subsequently, to create the weld seam S1 in the overlap area UB, a laser beam is guided over a surface of the upper component 3 in the illustrated path. In a further embodiment, the path movement can also be performed in the opposite direction. During the path movement, the laser beam follows a closed path B on the surface, in the area of which the components 2, 3 are melted and, after solidification, are / are bonded to one another.
[0033] The path B has a first radius r i having a circular arc B1 of a first circular segment, wherein the radius r ifor example, is greater than 5 mm. Furthermore, the path B and a concentric to the first circular arc B1 have a larger radius r a having a second circular arc B2 of a second circular segment, wherein the radius r a for example, is less than 75 mm. For example, a difference between the radius r a of the second circular arc B2 and the radius r i of the first circular arc B1 is less than 10 mm. The circular segments have a matching central angle β, with the first circular segment being completely contained within the second circular segment. The central angle β lies, for example, in a range between 5° and 270°.
[0034] Path B further comprises a curved first partial path B3 which adjoins tangentially an end (B1E) of the first circular arc B1 located on a first radius s1 of the first circular segment and which is tangentially connected to a start (B2A) of the second circular arc B2 located on the first radius s1 of the second circular segment. Path B further comprises a curved second partial path B4 which adjoins tangentially an end (B2E) of the second circular arc B2 located on a second radius s2 of the second circular segment and which is tangentially connected to a start (B1A) of the first circular arc B1 located on the second radius s2 of the first circular segment. A respective start and a respective end of the circular arcs B1, B2 result from a direction of movement of the laser beam during welding, which is represented here by arrows.A beginning A and an end E of path B result from a starting point at which the laser beam first hits the surface of component 3, and an end point at which the laser beam is deactivated. In the illustrated embodiment, the beginning A and the end E of path B lie on the first circular arc B1 at half (β / 2) of the central angle β and thus within the generated weld seam S1.
[0035] In order to minimize heat input into the components 2, 3 and especially into the attachment 4, the laser beam is moved at a path speed v Lof at least 10 m / min and emitted in such a way that at an impact point on the surface it has a beam diameter in a range between 50 µm and 250 µm. Furthermore, to minimize the heat input into the attachment 4, the laser beam is guided in particular in such a way that it runs through the material recess of the attachment 4 and the path B runs at a distance from the sections of the attachment 4 that delimit the material recess. Due to the high path movement speed v L Due to the small cross-sectional area of the incident beam, the overlapping components 2 and 3 are only melted very locally, and the surrounding areas are only slightly thermally affected. To widen the weld seam S1 and connect the component, path B is traversed, creating a weld seam geometry corresponding to path B.
[0036] In Fig. 3 shows a perspective view of a second possible embodiment of a component arrangement 1. The component arrangement 1 according to the second embodiment shown corresponds to the Fig. 1, with the difference that in the area of the material recess of the attachment part 4, further weld seams S2, S3 are formed to connect the components 2, 3.
[0037] The weld seams S2, S3 are, for example, supplementary or repair weld seams and are created analogously to the weld seam S1. To create the weld seams S2, S3 shown in the illustrated embodiment, circle segments are selected with a matching center angle β, which is smaller than when creating the weld seam S1. It is conceivable that the supplementary weld seams S2, S3, as in the Fig.3, on the circular arcs B1, B2 are arranged next to the first weld S1 or with changed radii r i , r a each run parallel to path B of the weld seam S1.
[0038] The features and advantages described herein with respect to the method for connecting at least two components may also relate to the component arrangement described herein and vice versa. List of reference symbols 1 Component arrangement 2 component 3 Component 4 Attachment A beginning B track B1 circular arc B2 circular arc B3 partial line B4 partial line B1A Beginning B1E End B2A beginning B2E End E End r a radius r i radius s1 radius distance s2 radius distance S1 weld seam S2 weld seam S3 weld seam UB overlap area v L Path movement speed β central angle
Claims
[1] Method for joining at least two components (2, 3) by means of a laser welding process, wherein the components (2, 3) are arranged relative to one another in such a way that they lie against one another in an overlapping area (UB), characterized by , that - to produce at least one weld seam (S1 to S3) in the overlapping area (UB), a laser beam is guided in a path movement over a surface of one of the components (2, 3), - in the path movement, a closed path (B) is travelled on the surface, in the area of which the components (2, 3) are melted and, after solidification, are bonded to one another, - the path (B) has a first radius (r i ) having a circular arc (B1) of a first circular segment and a concentric to the first circular arc (B1) having a larger second radius (r a) having a second circular arc (B2) of a second circular segment, wherein the circular segments have a matching central angle (β) and the first circular segment is completely contained in the second circular segment, - the path (B) has a curved first partial path (B3) which is tangentially connected to an end (B1E) of the first circular arc (B1) located on a first radius section (s1) of the first circular segment and which is tangentially connected to a beginning (B2A) of the second circular arc (B2) located on the first radius section (s1) of the second circular segment, - the path (B) has a curved second partial path (B4) which is tangentially connected to an end (B2E) of the second circular arc (B2) located on a second radius section (s2) of the second circular segment and which is tangentially connected to a beginning (B1A) of the first circular arc (B1) located on the second radius section (s2) of the first circular segment, - the laser beam with a path movement speed (v L ) of at least 10 m / min and - the laser beam is emitted in such a way that at an impact point on the surface it has a beam diameter in a range between 50 µm and 250 µm. [2] Method according to claim 1, characterized by that the laser beam is guided in such a way that a beginning (A) and an end (E) of the path (B) lie on the first circular arc (B1) or the second circular arc (B2). [3] Method according to claim 2, characterized by that the laser beam is guided in such a way that the beginning (A) and the end (E) of the path (B) are at half the central angle (β). [4] Method according to one of the preceding claims, characterized by that the central angle (β) is chosen in a range between 5 ° and 270 °. [5] Method according to one of the preceding claims, characterized bythat the radius (r i ) of the first circular arc (B1) is chosen to be greater than 5 mm. [6] Method according to one of the preceding claims, characterized by that the radius (r a ) of the second circular arc (B2) is chosen to be less than 75 mm. [7] Method according to one of the preceding claims, characterized by that a difference between the radius (r a ) of the second circular arc (B2) and the radius (r i ) of the first circular arc (B1) is chosen to be less than 10 mm. [8] Method according to one of the preceding claims, characterized bythat at least one of the components (2, 3) has, on its side facing away from the other component (2, 3), a connected attachment (4) with a material recess completely penetrating the attachment (4), wherein the laser beam is guided through the material recess in such a way that the path (B) runs at a distance from sections of the attachment (4) delimiting the material recess. [9] Component arrangement (1) comprising at least two components (2, 3) connected by means of the method according to one of the preceding claims. [10] Component arrangement (1) according to claim 9, wherein - one of the components (2, 3) is an electrical cell pole of a battery cell and the other component (2, 3) is a cell connector or - one of the components (2, 3) is a power electronics unit and the other component (2, 3) is an electrical connector.
Citation Information
Patent Citations
Method for producing a welded joint between at least two components using an energy beam
DE102021005518A1
Electrical contacting of components and battery module
DE102022000181A1
connection of composite materials
DE10350953A1
Welded Structures
JP6560003B2
Laser lap welding method
US20120160815A1