Method for producing molten iron and liquid slag in an electric melter
The method addresses the disposal challenge of CFRP residues by utilizing an electric melter to convert CFRP into molten iron and slag, ensuring complete carbon fiber decomposition and recycling, with optional pre-processing to remove impurities, and operates using renewable energy.
Patent Information
- Application Number
- DE102023107828
- Authority / Receiving Office
- DE · DE
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-02
AI Technical Summary
There is no economical solution for disposing of short-fiber carbon fiber reinforced plastic (CFRP) residues, as combustion methods fail to completely burn the carbon fibers, leading to residue accumulation and environmental issues.
A method for producing molten iron and liquid slag in an electric melter using carbon-containing and iron-containing feedstocks, where CFRP and/or GRP are used as slag formers, ensuring complete carbon fiber decomposition at high temperatures and long residence times, with optional pre-processing to remove disruptive components.
This method effectively recycles CFRP residues by converting them into molten iron and slag, eliminating fiber residues and enabling environmentally friendly operation using renewable energy.
Abstract
Description
[0001] The invention relates to a method for producing an iron melt in an electric melter.
[0002] Methods and devices for producing iron melts and liquid slags in electrical Melting devices are described in the prior art, see for example EP 3 954 786 A1.
[0003] Completely different industries are concerned with the use of fiber-plastic composites as Glass fibre reinforced plastic (hereinafter referred to as GRP) is used, for example, in the construction of In contrast, carbon fiber reinforced plastic (CFRP) is a popular material in automotive or aircraft construction. Until now, components made of these fiber-reinforced plastics have been difficult to dispose of. In particular, there is still no economical solution for disposing of short-fiber CFRP residues. Combustion in a waste incineration plant or rotary kiln cannot completely burn the carbon fibers. The inner fiber layers are thermally insulated, the residence times are too short and released fiber residues are conductive and create short circuits in the electrical exhaust air purification system. Unburned CFRP is found in the grate of the Waste incineration plants and must be disposed of in a special landfill. Due to the high C content, landfilling is not provided for and is also costly. DE 10 2021 114 676 A1 describes a process for the recovery and / or Disposal of carbon-containing carbon fibres and carbon fibre-containing and / or carbon fibre-reinforced plastics in metallurgical slag systems. The carbon in the carbon fibers is said to be Slag system with oxygen to carbon monoxide and / or carbon dioxide and released as reaction gas from the system.
[0004] The object of the present invention is to provide a possibility for the further use of used Fiber-reinforced plastic composites or production residues from the manufacture of fiber-reinforced plastic composites.
[0005] This object is achieved by a method having the features of claim 1. Further Embodiments are described in the subclaims.
[0006] The invention relates to a process for producing an iron melt and a liquid slag in a electric melter, where iron-containing and carbon-containing feedstocks as well as slag formers are introduced and melted, the electric melter comprising several electrodes which melt the provide the energy required to convert the feedstocks and slag formers into a liquid phase comprising a Iron melt and a liquid slag arranged on the iron melt, with carbon-containing Carbon-reinforced plastic and / or glass-fiber-reinforced plastic used as slag former become.
[0007] The invention takes advantage of the fact that the high temperatures and the long residence time in the electric melter ensures that the carbon reinforced plastic (CFRP) and / or glass fibre reinforced Plastic (GFRP) is converted without residue, so that no fiber residues remain or are released. The fibers, which are used, for example, as short or long fibers, are embedded in a plastic matrix, whereby the The plastic of the matrix can be a thermoplastic or thermoset.
[0008] The CFRP and / or GFRP is preferably free of components which are detrimental to the recycling in It is therefore particularly preferred that prior to recycling in the electrical Melters have undergone CFRP and / or GFRP deposition processes to remove interfering components essentially such as, for example, and if present, residual amounts of copper, brass, nickel, zinc, phosphorus and Halogens. Impurities in CFRP and / or GFRP can be up to 5 wt.%, especially up to 4 wt.%, preferably up to 3 wt%.
[0009] Depending on the type of previous application of the CFRP / GFRP, impurities may include balsa wood, paint residues, Foams, compact plastic layers may be included.
[0010] The preferred iron-containing feedstock is reduced iron ore in the form of sponge iron pieces or Sponge iron pellets with a carbon content between 0 and 4.5 wt.%, in particular > 0 wt.%, and a A metallization degree of at least 85% is used. The metallization degree reflects the ratio of the metallic Iron content in relation to the total iron content in the sponge iron. If a defined carbon content in the Iron melt, which contains between 2.0 and 5.0 wt.%, in particular between 3.0 and 4.8 wt.%, preferably between 3.5 and 4.5 wt.%, cannot be adjusted via the iron-containing feedstocks, carbon-containing feedstocks are taken into account in the amount that the desired carbon content (carbon target content) in the iron melt can be achieved and, for example, a residual reduction of the non-metallized portion of the sponge iron can take place.
[0011] Depending on the carbon content, which is associated with the iron-containing feedstock in the electrical When the melter is introduced, additional carbon is added, based on the carbon content (in wt%) in the carbonaceous feedstock to be introduced, with > 0 to a maximum of 50 kg per tonne of molten iron produced admitted.
[0012] In order to carburize the molten iron in the electric melter, the carbon in the Carbon fiber of CFRP is particularly well suited. The amount of CFRP to be used depends on the Carbon target content in the iron melt. If the carbon target content cannot be achieved exclusively by using CFRP can be achieved or only a certain amount of CFRP can be used due to the plant, further carbon-containing feedstocks are added, including carbon carriers, which in principle have a contain reducible free carbon, such as coke dust, coke slaked coal, coke breeze, petroleum coke, soot pellets or anthracite coal.
[0013] The plastic matrix of the fiber-reinforced plastic composite has the particular advantage that, due to the high carbon content of the plastic can also perform the function of the carbon carrier. For example, components which pass into the gas phase during pyrolysis, which are extracted as process gas can be used calorically.
[0014] In total, the carbon content in the CFRP can be considered, so the proportion of CFRP in the material to be used carbon-containing feedstock between 20 and 100 %, with the CFRP content in particular being at least 30 %, preferably at least 40 %, preferably at least 50 %.
[0015] The preferred use of sponge iron as iron-containing feedstock also brings slag-forming Components that are naturally contained in iron ore and not in a previous reduction process can be expelled and is called gangue. Is the gangue provided by the sponge iron not sufficient to produce a liquid slag suitable for further processing, further Slag formers are added as additives. Slag formers are preferably added so that a Basicity B3 in the liquid slag is set between 0.9 and 1.8. B3 can in particular be at least 1.0, preferably at least 1.1 and in particular a maximum of 1.7, preferably a maximum of 1.6. The basicity B3 corresponds to the Ratio (CaO+MgO) to (SiO +Al O ), whereby the determination of the characteristic sizes in the slag in the solid 2 2 3 state are familiar to the person skilled in the art. The slag former comprises at least one or more of the elements from the Group (CaO, MgO, SiO, AlO). 2 2 3
[0016] In order to condition the liquid slag in the electric melter, the SiO in the glass fiber 2 of the GRP is particularly suitable. The amount of GRP to be used depends on the basicity B3 to be set in the Liquid slag. If the desired basicity B3 cannot be achieved solely by using GRP or if only a certain amount of GRP can be used due to the plant, other slag formers can also be used be added, including one or more of the elements already mentioned above.
[0017] In order to improve or increase the recycling rate, scrap can be recycled in addition to the ferrous feedstocks, preferably added to the sponge iron pieces or sponge iron pellets. This can be done, for example, in the Type that > 0 kg, in particular at least 20 kg, preferably at least 50 kg, preferably at least 80 kg to up to 200 kg of scrap can be added per ton of molten iron produced.
[0018] CFRP and / or GFRP can be fed to the electric melter as shredder material and / or as grinding material To improve handling, CFRP and / or GFRP can be ground into agglomerated bricks, especially with a defined size, can be processed, see for example DE 10 2005 062 036 A1, which in wt.% 5-20 % of a cement binder, 50-75 % of a fiber-reinforced plastic composite, optionally up to 10 % of a setting and Solidification accelerators, and as a residue ferrous residues and recycle materials and unavoidable impurities The iron-containing residues and recyclables can make up to 45%. Furthermore, The iron-containing residues and recycling materials are in particular fine particles of the pig iron ladle slag, Mill scale or mill scale sludge, top sludge, dust from the oxygen steelworks, but also iron ore in the form of of fine and / or very fine particles. As setting and solidification accelerators, water glass, Alumina cement, calcium chloride, an alkali salt, in particular a sodium salt, a cellulose adhesive or a paste In particular, the setting and solidification accelerator can be completely omitted. As cement Portland cement or granulated cement can be used as a binding agent, are available at low cost. Also suitable are blast furnace cement, Portland composite cement, composite cement, Pozzolanic cement or another type of normal cement or special cement or a special cement.
[0019] The agglomerate stone can comprise at least 50%, in particular at least 55% of the fibre-reinforced plastics composite millbase. Specifically, the agglomerated stone may preferably contain at least 60%, preferably at least 65% fiber-reinforced plastics composite A higher proportion of fiber-reinforced plastics regrind can produce a larger amount of used fiber-plastic composites or the production residues from the production of fiber-plastic composites In addition, the proportion of optional additional carbon carriers and / or additional slag formers can be reduced because the fiber-reinforced plastics composite mill material is either CFRP carbon and / or GFRP silicon dioxide is provided.
[0020] Agglomerate stones can be produced on commercially available stone machines, so that different Sizes between 45 and 200 mm can be produced. The geometry of the agglomerated stone, whether rectangular, hexagonal or diamond-shaped in plan view, can be designed in any way.
[0021] The use of the invention is also conceivable in electrical melters which work with scrap and / or crude steel as iron-containing feedstocks when virtually no sponge iron is used.
[0022] To melt the iron-containing solids, the electric melter has several electrodes, which can be supplied with electrical current and thus provide the necessary energy to process the input materials into a liquid phase comprising molten iron and liquid slag. Depending on the size / dimension of the Three, four, five, six or more than six electrodes can be used in the electric melter. The energy required for melting is preferably provided from renewable energy sources (sun, wind, water, biomass). This allows the electric melter to be operated in a more environmentally friendly manner.
[0023] The electric melter may preferably be an OSBF (Open Slag Bath Furnace) furnace. include electric arc furnaces, especially SAF (Submerged Electric Arc Furnace), which are melting furnaces with arc Resistance heating is the formation of arcs between the electrode and the feedstock and / or the liquid phase or which heat the feedstock and / or the liquid phase using the Joule effect. In SAF, the electrodes are located in the Feed material and / or the liquid phase, especially immersed in the liquid slag. Depending on the operating principle / Operation, the electric arc furnaces can be operated as alternating current submerged arc furnaces (SAFac) or direct current Submerged arc furnaces (SAFdc) can be used. Alternatively, melting furnaces with direct Arc exposure, which deviates from the functional principle / mode of operation described above, so-called EAF (Electric Arc Furnace) are used, which form arcs between the electrode and the liquid phase. This includes the alternating current arc melting furnace (EAFac), the direct current arc melting furnace (EAFdc) and the Ladle Furnace LF (Ladle Furnace).
[0024] The advantage of using electric arc resistance heating (SAF) furnaces is that These are operated with a reducing atmosphere, whereas melting furnaces with direct arc action (EAF) with an oxidizing atmosphere.
[0025] The invention is explained in more detail using an embodiment.
[0026] The invention provides a process for producing an iron melt and a liquid slag in a non- Electric melter shown. Ferrous and carbonaceous feedstocks as well as slag formers are introduced and melted. The required input materials and Slag formers are added. The iron-containing feedstocks include or consist of sponge iron pieces or pellets. In addition, other iron-containing feedstocks, such as iron-containing scrap, can be used to The electric melter includes several electrodes (not shown), which provide the energy required for melting the feedstock and the slag formers into a Liquid phase comprising an iron melt and a liquid slag arranged on the iron melt. The electrical energy required for melting can preferably be obtained from renewable energy (sun, wind, water) be generated.
[0027] CFRP is used as carbon-containing feedstock. GFRP is used as slag former. Depending on the desired objective, whether an adjustment of the target carbon content in the iron melt and / or the required basicity B3 in the liquid slag is required, either only CFRP, only GRP or both fiber-reinforced plastics can be used in The combination must be used in the quantity required to meet the requirements.
[0028] If required, additional carbon-containing feedstocks and / or slag formers can be added, especially if the so-called gangue of the preferably used sponge iron is not sufficient to Depending on the ability to adjust the desired basicity of the liquid slag to be tapped. The desired basicity can be achieved by appropriate mixing / addition. The amount of iron-containing feedstocks is determined by the desired yield of the iron melt.
[0029] In one embodiment, 100 kg of sponge iron were extracted from a 100% Direct reduction was used with hydrogen as the reducing gas. Thus, the total amount of Carbon content of the sponge iron was less than 0.20 wt.%. Slag formers in the form of GRP were measured at approx. 10 kg as ground material, especially with a particle size between 0.7 and 4.5 mm, and carbonaceous feedstocks in Form of CFRP with approx. 4 kg as shredder material, especially with a material size between 10 and 50 mm, After the melting operation, a carbon content of 4.15 wt.% was determined in the iron melt. Liquid slag with a basicity of 1.1 could be removed. The determination of the carbon content is The determination of the components in the slag to determine basicity B3 is also Known to experts.
[0030] The operation of electrical melters is also familiar to the person skilled in the art.
[0031] Also not shown is how the molten iron is removed and fed to a further processing step Preferably, the iron melt is subjected to a treatment to reduce the carbon in the iron melt to a to the desired extent. This is done, for example, using oxygen in a so-called oxygen blowing process, particularly preferably in a converter. The tapped liquid slag is also preferably subjected to granulation to produce slag, particularly for the construction industry. QUOTES CONTAINED IN THE DESCRIPTION
[0000] This list of documents submitted by the applicant was generated automatically and is intended solely for This list is not part of the German patent or trademark law. Utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature
[0000] EP 3954786 A1
[0002] DE 102021114676 A1
[0003] DE 102005062036 A1
[0018]
Claims
1. A process for producing an iron melt and a liquid slag in an electric melter, wherein iron-containing and carbon-containing feedstocks as well as slag formers are introduced and melted, whereby the electric melter comprises several electrodes which provide the energy required for melting the Feed materials and the slag formers into a liquid phase comprising an iron melt and a arranged liquid slag, characterized in that as carbon-containing feedstocks carbon-reinforced plastic and / or glass-fiber-reinforced plastic can be used as a slag former.
2. Process according to claim 1, wherein the iron-containing feedstocks used are reduced iron ore in the form of sponge iron Pieces or sponge iron pellets with a carbon content between 0 and 4.5 wt.% and a A metallization degree of at least 85% must be used.
3. Process according to claim 1, wherein the iron-containing feedstocks are scrap and / or crude steel and no sponge iron is supplied.
4. A process according to any one of the preceding claims, wherein a carbon content in the iron melt is between 2.0 and 5.0 wt.%.
5. A process according to any one of the preceding claims, wherein the carbonaceous feedstock is mixed with > 0 to a maximum of 50 kg per ton of molten iron produced.
6. Method according to one of the preceding claims, wherein in total the carbon content in the carbon-reinforced plastic, the proportion of carbon-reinforced plastic of the material to be used carbon-containing feedstock is between 20 and 100%.
7. Method according to one of the preceding claims, wherein glass fibre reinforced plastic and optional further Slag formers are added so that a basicity B3 in the liquid slag between 0.9 and 1.8 is established.
8. Method according to one of the preceding claims, wherein carbon-reinforced plastic and / or glass fibre reinforced plastic is fed to the electric melter as shredder material and / or as regrind become.
9. Method according to one of the preceding claims, wherein carbon-reinforced plastic and / or glass fibre reinforced plastic with 50 to 75 wt.%, 5 to 20 wt.% of a cement binder, optionally up to 10 wt.- % of a setting and solidification accelerator, and the remainder iron-containing residual and recycled materials and unavoidable impurities are processed into an agglomerate stone and as an agglomerate stone is subjected to the electrical is fed to the melter.
10. Method according to one of the preceding claims, wherein the energy required for melting is from regenerative Energy is provided.
Citation Information
Patent Citations
Agglomerate stone used in blast furnaces for recovering pig iron comprises cement binder, organic fibers, carbon support, residue materials, solidifying accelerator and a balance of iron ore in the form of fine and / or very fine particles
DE102005062036A1
Processes for the recycling of carbon fibers (CF) or carbon fiber reinforced plastics (CFRP)
DE102021114676A1
Method for producing raw steel and unit for producing the same
EP3954786A1
process for briquetting powdered alloy surcharges from steel, foundry and non-ferrous metallurgy using fibrous structure-forming agents and a briquette
DE102015011067B4
Methods for recycling components that contain or consist of carbon fiber reinforced plastic (CFRP).
DE102022101835A1