LOW INDUCTIVITY ELECTROLYTE CAPACITOR
The solid electrolytic capacitor design addresses high-frequency and high-speed switching challenges by minimizing ESL and ESR, ensuring stable performance under harsh conditions and enhancing circuit efficiency.
Patent Information
- Application Number
- DE112024001364
- Authority / Receiving Office
- DE · DE
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-03-20
- Publication Date
- 2026-01-15
AI Technical Summary
Existing solid electrolytic capacitors struggle to meet the requirements of high-frequency applications and high-speed switching due to high inductance and equivalent series resistance, limiting their performance in modern electronic circuits.
A solid electrolytic capacitor design featuring a sintered anode body, dielectric material, and conductive polymer electrolyte, enclosed in a hermetically sealed housing, which minimizes equivalent series inductance (ESL) and resistance (ESR) to provide low impedance over a wide frequency range.
The capacitor achieves low ESL values of 1 nanohenry or less and ESR values of 800 mΩ or less, maintaining stability under high temperatures and humidity, enabling robust broadband decoupling and high-speed circuitry with improved miniaturization and effective DC power filtering.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Related Applications
[0001] The present application is based on the preliminary US patent application Serial No. 63 / 491,551, filed on March 22, 2023, which is incorporated herein by reference, and claims its priority. Background of the invention
[0002] Decoupling capacitors are frequently used to address noise problems in circuits. They provide stable, localized charge sources necessary for switching and refreshing the logic gates used in various digital circuits. However, decoupling capacitors today must operate at lower voltages and higher currents, requiring performance characteristics such as lower equivalent series resistance (ESR), higher capacitance, and lower inductance (or ESL equivalent series inductance) to function at the required level in today's diverse applications. In particular, with increasing switching speeds in electronic circuits, the need to reduce inductance becomes a serious constraint on improved system performance. Solid electrolytic capacitors (e.g.,Tantalum capacitors are typically manufactured by pressing a metal powder (e.g., tantalum) around a metal conductor wire, sintering the pressed portion, anodizing the sintered anode, and then applying a solid electrolyte. Conductive polymers are frequently used as the solid electrolyte because they have a low equivalent series resistance and do not burn or ignite. While solid electrolytic capacitors offer significant advantages in terms of ESR, they are unable to withstand high-frequency applications or exhibit the low inductance required for decoupling and high-speed switching. Therefore, there is currently a need for a solid electrolytic capacitor with improved performance. Summary of the invention
[0003] According to one embodiment of the present invention, a solid electrolytic capacitor is disclosed, comprising a capacitor element that includes a sintered anode body, a dielectric material covering the anode body, and a solid electrolyte covering the dielectric material, the solid electrolyte being a conductive polymer. The capacitor element has a first and a second end opposite each other, as well as a top and a opposite bottom. A first exposed anode conduction section extends laterally from the first end of the capacitor element, and a second exposed anode conduction section extends laterally from the second end of the capacitor element.The capacitor further comprises a housing that defines an inner cavity in which the capacitor element is arranged and hermetically sealed, with the first exposed anode conductor section and the second exposed anode conductor section being arranged within the inner cavity. A first anode terminal is in electrical contact with the first exposed anode conductor section, a second anode terminal is in electrical contact with the second exposed anode conductor section, and a cathode terminal is in electrical contact with the solid electrolyte.
[0004] Further features and aspects of the present invention are described in more detail below. Brief description of the drawing
[0005] A complete and enabling disclosure of the present invention, including the best embodiment, which is addressed to a person skilled in the art, is set out in particular in the remainder of the description, which refers to the accompanying figures, in which: Fig. Figure 1A is a side view of an embodiment of an anode body which can be used to form the capacitor of the present invention; Fig. Figure 1B is a side view of another embodiment of an anode body that can be used to form the capacitor of the present invention; Fig. Figure 1C is a side view of another embodiment of an anode body which can be used to form the capacitor of the present invention; Fig. Figure 2 is a cross-sectional view of an embodiment of a capacitor of the present invention; Fig.3 is a view from below of the capacitor of Fig. 2; Fig. Figure 4 is a graphical representation of the parameters S 11 and S 21 , which were modeled and measured over a wide frequency range for Example 1. Fig. 5 is an example equivalent circuit that was used in Example 1. Detailed description of representative embodiments
[0006] It is understood that the present discussion is only a description of exemplary embodiments and is not intended as a limitation of the broader aspects of the present invention embodied by the exemplary construction.
[0007] In general, the present invention relates to a capacitor capable of exhibiting good electrical properties under a wide variety of conditions. The capacitor comprises a capacitor element consisting of a sintered porous anode body, a dielectric material superimposed on the anode body, and a solid electrolyte superimposed on the dielectric material and containing a conductive polymer. The capacitor element has opposing first and second ends and opposing top and bottom surfaces. The capacitor also includes several anode conduction sections extending from the ends of the capacitor element. The capacitor further comprises a housing defining an internal cavity in which the capacitor element is arranged and hermetically sealed.
[0008] By selectively controlling its special configuration, the resulting capacitor can exhibit low ESL values, such as 1 nanohenry or less, in some embodiments about 750 picohenries or less, in some embodiments about 350 picohenries or less, in some embodiments from about 1 femtohenry to about 100 picohenries, and in some embodiments from about 50 femtohenries to about 10 picohenries. The low ESL values can also be characterized by a low impedance value, which is the inverse of the parasitic inductance. The impedance can be, for example, about 1 ohm or less, in some embodiments about 0.8 ohms or less, in some embodiments about 0.6 ohms or less, and in some embodiments from about 1 mOhm to about 0.3 ohms. Such a low ESL (e.g., impedance) can also occur over a wide frequency range, e.g.,from 1 kHz to approximately 100 MHz, in some embodiments from approximately 100 kHz to approximately 100 MHz, and in some embodiments from approximately 1 MHz to approximately 100 MHz. Minimizing parasitic inductance over a wide frequency range can contribute to good performance, particularly good decoupling performance, especially under high-speed transient conditions. In addition to low ESL values, the capacitor can also exhibit low ESR values, such as approximately 800 mΩ or less, in some embodiments approximately 600 mΩ or less, in some embodiments approximately 500 mΩ or less, in some embodiments approximately 350 mΩ or less, in some embodiments from approximately 0.01 to approximately 250 mΩ, and in some embodiments from approximately 0.1 to approximately 150 mΩ, measured at an operating frequency of 100 kHz and a temperature of 23 °C.
[0009] In particular, the low ESR and ESL values can remain stable even at high temperatures and / or high humidity. The ability to function under such conditions is achieved in part by enclosing the capacitor element in a housing and hermetically sealing it to limit the amount of oxygen and moisture introduced to the solid electrolyte of the capacitor element. In this respect, the resulting capacitor can exhibit ESR and / or ESL values within the aforementioned ranges, even after being exposed to temperatures of approximately 80°C or higher, in some embodiments from approximately 85°C to approximately 180°C, and in some embodiments from approximately 850°C to approximately 150°C (e.g.,approximately 85 °C, 105 °C, 125 °C, or 150 °C) and / or a relative humidity of approximately 40% or more, in some embodiments approximately 45% or more, in some embodiments approximately 50% or more, and in some embodiments approximately 70% or more (e.g., approximately 85% to 100%) for a substantial period of time, as mentioned above. The relative humidity may be determined, for example, according to ASTM E337-02, Method A (2007). The period during which the material is exposed to the high temperature and / or humidity may be approximately 100 hours or more, in some embodiments from approximately 150 hours to approximately 3,000 hours, and in some embodiments from approximately 200 hours to approximately 2,500 hours (e.g., 250, 500, 750, or 1,000 hours). For example, the ESR of the capacitor, after being exposed to high temperature (e.g., about 85 °C) and / or humidity (e.g., about 85%) for 500 hours, may be about 1,500 mOhm or less, in some embodiments about 1.The ESR of the capacitor, after being exposed to a high temperature (e.g., about 85°C) and / or high humidity (e.g., about 85% humidity) for 500 hours, may be about 10 or less, about 5 or less, about 3 or less, about 2 or less, and about 0.9 to about 1.5 in some embodiments, measured at an operating frequency of 100 kHz and a temperature of 23°C. Likewise, the ratio of the ESR of the capacitor, after it has been exposed to a high temperature (e.g., about 85°C) and / or high humidity (e.g., about 85%) for 500 hours, to the initial DCL of the capacitor (e.g., at about 23°C) may be about 10 or less, about 5 or less in some embodiments, about 3 or less in some embodiments, about 2 or less in some embodiments, and about 0.9 to about 1.5 in some embodiments.
[0010] Due to its ability to offer a combination of low ESL and ESR values, the resulting capacitor can be uniquely positioned to provide robust broadband decoupling and high-speed circuitry. For example, a single capacitor according to the present invention can be used to replace multiple decoupling capacitors with lower capacitance or limited frequency, thereby requiring less space, e.g., with a lower height, which further improves miniaturization.
[0011] The capacitor can exhibit excellent DC power filtering, for example, through excellent attenuation over a wide frequency range. As is well known in engineering, insertion loss measures the power transfer between the terminals. When the power increases, gain is observed; when the power decreases between the terminals, attenuation is observed. Thus, the capacitor can exhibit high attenuation over a wide frequency range, enabling effective filtering across a broad frequency spectrum. For example, the capacitor can have an attenuation (S) of 21-parameter) of about 15 dB or more, in some embodiments about 25 dB or more, in some embodiments about 30 dB or more, in some embodiments from about 35 dB to about 70 dB, and in some embodiments from about 50 dB to about 70 dB. Such attenuation can occur over a wide frequency range. For example, the capacitor can exhibit attenuation (S) at low frequencies from about 0.1 MHz to about 500 MHz and in some cases from about 1 MHz to about 100 MHz. 21 -parameter) of about 40 dB or more, in some embodiments about 50 dB or more, in some embodiments about 55 dB or more, and in some embodiments about 60 dB to about 70 dB. Likewise, the capacitor may exhibit attenuation (S) at high frequencies from about 500 MHz to about 10 GHz and in some cases from about 1 GHz to about 5 GHz. 21-parameter) of approximately 20 dB or more, in some embodiments approximately 25 dB or more, in some embodiments approximately 30 dB or more, and in some embodiments from approximately 30 dB to approximately 60 dB. Among other things, such attenuation can allow the capacitor to be readily used in DC filter applications. Furthermore, the capacitor can provide consistent performance over a wide temperature range. For example, in one embodiment, the capacitor can fluctuate by approximately 5 dB or less over a large temperature range, such as with a temperature change of approximately 25 °C or more, in some embodiments of approximately 50 °C or more, and in some embodiments of approximately 70 °C or more.
[0012] The capacitor may also exhibit other advantageous electrical properties. For example, the capacitor may exhibit a low leakage current (“DCL”) under a variety of conditions. Furthermore, after being subjected to an applied voltage (e.g., 16 volts) at a temperature of approximately 23°C for a certain period of time (e.g., from approximately 30 minutes to approximately 20 hours, in some embodiments from approximately 1 hour to approximately 18 hours, and in some embodiments from approximately 4 hours to approximately 16 hours), the capacitor may exhibit a DCL of approximately 10 microamperes (“µA”) or less, in some embodiments approximately 5 µA or less, in some embodiments approximately 1 µA or less, and in some embodiments from approximately 0.01 to approximately 5 µA. In one embodiment, the DCL of the capacitor may be further reduced after being subjected to a high temperature (e.g., approximately 85°C) and / or high humidity (e.g.,after exposure to approximately 85% humidity, the current may be approximately 10 µA or less, in some embodiments approximately 8 µA or less, in some embodiments approximately 6 µA or less, and in some embodiments approximately 0.1 to approximately 5 µA. Likewise, the ratio of the DCL of the capacitor after exposure to high temperature (e.g., approximately 85 °C) and / or humidity (e.g., approximately 85%) for 500 hours to the initial DCL of the capacitor (e.g., at approximately 23 °C) may be approximately 20 or less, in some embodiments approximately 15 or less, in some embodiments approximately 10 or less, in some embodiments approximately 5 or less, and in some embodiments from approximately 0.9 to approximately 4. The capacitor may also have a dry capacitance of approximately 30 nanofarads per square centimeter (nF / cm). 2 “) or more, in some embodiments approximately 100 nF / cm 2 or more, in some embodiments from about 200 to about 3,000 nF / cm 2and in some embodiments from about 400 to about 2,000 nF / cm 2, measured at a frequency of 120 Hz at a temperature of 23 °C. The actual capacitance can vary, e.g., from about 10 µF to about 1,000 µF, in some embodiments from about 50 µF to about 500 µF, and in some embodiments from about 60 µF to about 250 µF. Similar to the DCL and ESR values, the capacitance can remain stable even under the aforementioned high temperature and / or humidity conditions. In one embodiment, for example, the ratio between the capacitance value of the capacitor after it has been exposed to a high temperature (e.g., about 85 °C) and / or humidity (e.g., about 85%) for 500 hours and the initial capacitance value of the capacitor (e.g., at about 23 °C) may be about 3.0 or less, in some embodiments about 2.0 or less, in some embodiments about 1.8 or less, in some embodiments about 1.6 or less, and in some embodiments from about 0.9 to about 1.3.
[0013] It is also assumed that the capacitor's loss factor can be kept at a relatively low level. The loss factor generally refers to the losses occurring in the capacitor and is usually expressed as a percentage of the ideal capacitor rating. For example, the capacitor's loss factor is typically about 250% or less, in some embodiments about 200% or less, and in some embodiments from about 1% to about 180%, as determined at a frequency of 120 Hz.
[0014] Various embodiments of the present invention will now be explained in more detail. I. Capacitor elementA. anode body
[0015] The anode body consists of a powder containing a valve metal (i.e., an oxidizable metal) or a valve metal-based compound, such as tantalum, niobium, aluminum, hafnium, titanium, their alloys, oxides, nitrides, etc. The specific charge of the powder typically varies from about 5,000 to about 800,000 microfarads per gram (µF*V / g), depending on the desired application. For example, in certain embodiments, a highly charged powder with a specific charge of about 100,000 to about 600,000 µF*V / g can be used, in some embodiments from about 120,000 to about 500,000 µF*V / g, and in some embodiments from about 150,000 to about 400,000 µF*V / g. In other embodiments, a low-charge powder can be used, having a specific charge of about 5,000 to about 100,000 µF*V / g, in some embodiments of about 8,000 to about 90,000 µF*V / g, and in some embodiments of about 10.The specific charge ranges from 000 to approximately 80,000 µF*V / g. As is known in engineering, the specific charge can be determined by multiplying the capacitance by the anodizing voltage used and then dividing this product by the weight of the anodized electrode body.
[0016] In one embodiment, the powder is produced, for example, from tantalum. If desired, a reduction process can be used in which a tantalum salt (e.g., potassium fluorotanalate (K₂TaF₇), sodium fluorotanalate (Na₂TaF₇), tantalum pentachloride (TaCl₅), etc.) is reacted with a reducing agent. The reducing agent can be provided in the form of a liquid, a gas (e.g., hydrogen), or a solid, such as a metal (e.g., sodium), a metal alloy, or a metal salt. In one embodiment, for example, a tantalum salt (e.g., TaCl₅) can be heated to a temperature of approximately 900 °C to approximately 2,000 °C, in some embodiments from approximately 1,000 °C to approximately 1,800 °C, and in some embodiments from approximately 1,100 °C to approximately 1,600 °C to form a vapor that can be reduced in the presence of a gaseous reducing agent (e.g., hydrogen).Further details of such a reduction reaction are described in WO 2014 / 199480 by Maeshima et al. After reduction, the product can be cooled, crushed, and washed to form a powder.
[0017] The powder can be a free-flowing, finely dispersed powder containing primary particles. The primary particles of the powder generally have a medium size (D 50) of about 5 to about 250 nanometers, in some embodiments of about 10 to about 200 nanometers, and in some embodiments of about 20 to about 150 nanometers, as determined by a Beckman Coulter Corporation laser particle size distribution analyzer (e.g., LS-230), optionally after the particles have been subjected to ultrasonic wave vibration for 70 seconds. The primary particles typically have a three-dimensional granular shape (e.g., nodular or angular). Such particles typically have a relatively low aspect ratio, i.e., the average diameter or width of the particles divided by the average thickness (“D / T”). For example, the aspect ratio of the particles may be about 4 or less, in some embodiments about 3 or less, and in some embodiments about 1 to about 2.In addition to primary particles, the powder may also contain other types of particles, such as secondary particles, which are formed by aggregation (or agglomeration) of the primary particles. Such secondary particles can have an average size (D. 50 ) from about 1 to about 500 micrometers and in some embodiments from about 10 to about 250 micrometers.
[0018] The particles can be agglomerated by heating them and / or by using a binder. For example, agglomeration can occur at a temperature of approximately 0 °C to approximately 40 °C, in some embodiments from approximately 5 °C to approximately 35 °C, and in some embodiments from approximately 15 °C to approximately 30 °C. Suitable binders include, for example, polyvinyl butyral, polyvinyl acetate, polyvinyl alcohol, polyvinylpyrrolidone, cellulose polymers such as carboxymethylcellulose, methylcellulose, ethylcellulose, hydroxyethylcellulose, and methylhydroxyethylcellulose, atactic polypropylene, polyethylene, and polyethylene glycol (e.g., Carbowax from Dow Chemical Co.).Polystyrene, poly(butadiene / styrene); polyamides, polyimides and polyacrylamides, high molecular weight polyethers; copolymers of ethylene oxide and propylene oxide; fluoropolymers, such as polytetrafluoroethylene, polyvinylidene fluoride and fluoroolefin copolymers; acrylic polymers, such as sodium polyacrylate, poly(low alkyl acrylates), poly(low alkyl methacrylates) and copolymers of low alkyl acrylates and methacrylates; and fatty acids and waxes, such as stearic acid and other soapy fatty acids, vegetable wax, microwaxes (purified paraffins), etc. If desired, the powder can also be combined with sintering protectants in the presence of a dopant, such as aqueous acids (e.g., phosphoric acid). The amount of dopant added depends partly on the surface area of the powder, but is generally no more than about 200 parts per million (ppm). The doping agent can be added before, during and / or after agglomeration.The powder can also be subjected to one or more deoxidation treatments. For example, the powder can be exposed to a getter material (e.g., magnesium), as described in US Patent No. 4,960,471. The temperature at which the deoxidation of the powder takes place can vary, but is typically in the range of about 700 °C to about 1,600 °C, in some embodiments from about 750 °C to about 1,200 °C, and in some embodiments from about 800 °C to about 1,000 °C. The total duration of the deoxidation treatment(s) can range from about 20 minutes to about 3 hours.
[0019] The resulting powder has certain properties that improve its ability to be formed into a capacitor anode. For example, the powder typically has a specific surface area of approximately 0.5 to 10.0 m². 2 / g, in some embodiments from about 0.7 to about 5.0 m 2 / g and in some embodiments from about 2.0 to about 4.0 m 2 / g. Similarly, the bulk density of the powder can range from approximately 0.1 to approximately 0.8 grams per cubic centimeter (g / cm³). 3 ), in some embodiments from about 0.2 to about 0.6 g / cm³ 3 and in some embodiments from about 0.4 to about 0.6 g / cm³ 3 be.
[0020] Once the powder is formed, it is generally compacted or pressed to create a pellet using a conventional powder press. For example, a single-stage press with a die and one or more rams can be used. Alternatively, anvil presses containing only a die and a single lower ram can be used. Single-stage compaction presses come in various basic types, such as cam, toggle, and eccentric / crank presses, with different functions, such as single-acting, double-acting, or floating dies, movable plates, counter-rams, augers, impact, hot pressing, embossing, or coating. The powder is typically compressed to a density of approximately 0.5 to 20 g / cm³. 3 pressed, in some embodiments from about 1 to about 15 g / cm³ 3 and in some embodiments from about 2 to about 10 g / cm³ 3 .
[0021] Any binder present after pressing can be removed by heating the pellet under vacuum for several minutes at a specific temperature (e.g., from about 150 °C to about 500 °C). Alternatively, the binder can also be removed by contacting the pellet with an aqueous solution, as described in US Patent No. 6,197,252 by Bishop et al. After removal of the binder, the anode body can be subjected to an optional deoxidation process. In one embodiment, the deoxidation process includes, for example, exposing the anode body to a getter material (e.g., magnesium, titanium, etc.) capable of removing oxygen from the anode body by chemical reaction, adsorption, etc. Specifically, the anode body is first placed in a casing (e.g., a tantalum box) that also contains the getter material. The atmosphere inside the casing is typically an inert atmosphere (e.g., argon gas).To initiate deoxidation, the atmosphere inside the casing is heated to a temperature sufficient to melt and / or vaporize the getter material and deoxidize the anode body. The temperature can vary depending on the specific charge of the anode powder, but is typically in the range of about 700 °C to about 1,200 °C, in some embodiments from about 750 °C to about 1,100 °C, and in some embodiments from about 800 °C to about 1,000 °C. The total duration of deoxidation can range from about 20 minutes to about 3 hours. This can be carried out in one or more stages. Upon completion of deoxidation, the getter material typically vaporizes and forms a deposit on one wall of the casing.To ensure the removal of the getter material, the anode body can also be subjected to one or more acid leaching steps, for example with a solution of nitric acid, hydrofluoric acid, hydrogen peroxide, sulfuric acid, water, etc., or a combination thereof.
[0022] The resulting anode body can therefore have a relatively low oxygen content. For example, the anode body may contain no more than approximately 5,500 ppm oxygen, in some embodiments no more than approximately 5,000 ppm oxygen, and in some embodiments from approximately 500 to approximately 4,500 ppm oxygen. The oxygen content can be measured with the LECO Oxygen Analyzer and includes the oxygen in the natural oxide on the tantalum surface and the oxygen in the tantalum particles. The total oxygen content is controlled by the period of the tantalum crystalline lattice, which increases linearly with increasing oxygen content in the tantalum until the solubility limit is reached.This method was described in “Critical Oxygen Content In Porous Anodes Of Solid Tantalum Capacitors”, Pozdeev-Freeman et al: Materials In Electronics 9, (1998) 309-311, where X-ray diffraction analysis (XRDA) was used to measure the period of the crystalline lattice of tantalum. Oxygen in sintered tantalum anodes may be confined to thin natural surface oxides, while the bulk of the tantalum is practically free of oxygen.
[0023] After optional deoxidation, the anode body can be sintered to form a porous, integral mass. The anode body is typically sintered at a temperature of approximately 700 °C to 1600 °C, in some embodiments from approximately 800 °C to 1500 °C, and in some embodiments from approximately 900 °C to 1200 °C, for a time of approximately 5 minutes to 100 minutes, and in some embodiments from approximately 8 minutes to 15 minutes. This can be done in one or more steps. If desired, sintering can be carried out in an atmosphere that limits the transfer of oxygen atoms to the anode. For example, sintering can be performed in a reducing atmosphere, e.g., under vacuum, inert gas, hydrogen, etc.The reducing atmosphere can have a pressure of approximately 10 Torr to approximately 2000 Torr, in some embodiments from approximately 100 Torr to approximately 1000 Torr, and in some embodiments from approximately 100 Torr to approximately 930 Torr. Mixtures of hydrogen and other gases (e.g., argon or nitrogen) can also be used. As mentioned above, the sintering of the anode body generally takes place after any necessary deoxidation. However, it is understood that the anode body can also be subjected to one or more pre-sintering steps before oxidation to achieve the desired degree of green strength for the deoxidation process. Such pre-sintering steps can be carried out under the same or different conditions as the sintering process after deoxidation. For example, pre-sintering can be carried out in one or more steps at a temperature of approximately 700°C to approximately 1.Pre-sintering can be carried out at 600°C, in some embodiments from about 800°C to about 1,500°C, and in some embodiments from about 900°C to about 1,200°C, for a time of about 5 minutes to about 100 minutes, and in some embodiments from about 8 minutes to about 15 minutes. Pre-sintering can also be carried out in a reducing atmosphere, e.g., in a vacuum, under inert gas, hydrogen, etc., as described above.
[0024] As mentioned above, the capacitor also contains several anode lead sections that are electrically connected to the respective anode terminals. The anode lead sections can be configured as part of a single anode lead (e.g., with opposite ends) or as part of separate anode leads. The anode lead(s) can be of any desired shape and size and may be in the form of a wire, foil, etc. Typically, the anode lead(s) extend longitudinally along the anode body and consist of any electrically conductive material, such as tantalum, niobium, aluminum, hafnium, titanium, etc., as well as electrically conductive oxides and / or nitrides thereof. The connection of the lead(s) to the anode body can be made by any known technique, e.g., by welding the one or more leads to the body or by embedding the one or more anode leads in the anode body during its formation (e.g., by embedding).before compaction and / or sintering).
[0025] In Fig. Figure 1A shows an embodiment of an anode body 10, which has a first anode conductor 12 with an embedded section 24 within the anode body and an exposed first anode conductor section 26 extending from a first end 16 of the anode body 10. A second exposed anode conductor section 14 is also connected (e.g., by a weld 20) to a second end 18 of the anode body 10. As shown in Fig. As shown in Figure 1A, the second exposed anode conduction section 14 is designed as part of a separate, second anode conduction extending from a second end 18 of the anode body. Of course, as shown in Fig.As shown in Figure 1C, the first exposed anode conduction section 26 and the second exposed anode conduction section 14 can also be defined by opposing sections of a single, continuous anode conduction 22 extending through both ends 16 and 18 of the anode body 10. Regardless, it is typically desirable that the exposed anode conduction sections extend from the opposite ends of the anode body generally in the same plane. Referring again to Fig. 1A Optionally, a gap can exist between the embedded end of the first anode conductor and the end of the anode body, so that the electrical connection between the first and second anode conductors is established through the sintered anode body. Fig.1A This gap can, for example, be defined as the distance “t” between the end 18 of the anode body and the embedded end 28 of the anode lead, which is typically in the range of about 0.2 to about 5 millimeters, in some embodiments from about 0.4 to about 4 millimeters, and in some embodiments from about 0.5 to about 2 millimeters. The length of the anode “I” can also be in the range of about 1.5 to about 6 millimeters, and in some embodiments from about 2 to about 5 millimeters. In such embodiments, the ratio between the distance “t” and the length “I” can also be in the range of about 0.1 to about 0.8, in some embodiments from about 0.2 to about 0.7, and in some embodiments from about 0.3 to about 0.6.
[0026] Another embodiment is in Fig.Figure 1B shows an anode body 10 comprising a first anode conductor 12 with an embedded section 24 within the anode body and an exposed first anode conductor section 26 extending from a first end 16 of the anode 10. A second anode conductor 14 has an embedded section 32 arranged within the anode body and an exposed second anode conductor section 34 extending from a second end 18 of the anode body 10. Therefore, in this embodiment, a welded section for the second anode conductor is not required. Similar to the embodiment described above, a gap “t” may optionally exist between the embedded end of the first anode conductor and the embedded end of the second anode conductor, which may be located within the aforementioned areas. B. Dielectric
[0027] The anode body is coated with a dielectric. The dielectric can be formed by anodic oxidation (“anodizing”) of the sintered anode body, so that a dielectric layer forms on and / or within the anode body. For example, a tantalum (Ta) anode can be anodized to tantalum pentoxide (Ta₂O₅). Anodizing is usually carried out by first applying a solution to the anode, for example, by immersing the anode in the electrolyte. A solvent is typically used, such as water (e.g., deionized water). To improve the ionic conductivity, a compound that can dissociate in the solvent to form ions can be used. Examples of such compounds are acids, as described below in relation to the electrolyte. An acid (e.g., phosphoric acid) can, for example, be added at approximately 0.01 wt% to approximately 5 wt%, and in some embodiments at approximately 0.05 wt%.The anodizing solution comprises approximately 0.8 wt.% to 0.8 wt.%, and in some embodiments approximately 0.1 wt.% to 0.5 wt.%. If desired, mixtures of acids can also be used.
[0028] To form the dielectric layer, a current can be passed through the anodizing solution. The formation voltage controls the thickness of the dielectric layer. For example, the power supply can initially be set to a galvanostatic mode until the required voltage is reached. Afterward, the power supply can be switched to a potentiostatic mode to ensure that the desired dielectric layer thickness is formed across the entire surface of the anode. Of course, other established methods can also be used, such as pulsed or step potentiostatic methods.The forming voltage used during anodizing is generally about 20 volts or more, in some embodiments about 30 volts or more, in some embodiments about 35 volts or more, and in some embodiments from about 35 to about 70 volts, at temperatures of about 10 °C or more, in some embodiments from about 20 °C to about 200 °C, and in some embodiments from about 30 °C to about 100 °C. The resulting dielectric layer can form on the surface of the anode and in its pores.
[0029] By precisely controlling the specific way in which the anode body is shaped, the resulting capacitor can exhibit a high degree of dielectric strength, which can improve capacitance stability. "Dependency strength" generally refers to the ratio between the capacitor's "breakdown voltage" (the voltage at which the capacitor fails, in volts, "V") and the thickness of the dielectric (in nanometers, "nm"). The capacitor typically has a dielectric strength of about 0.4 V / nm or more, in some embodiments about 0.45 V / nm or more, in some embodiments about 0.5 V / nm or more, in some embodiments from about 0.55 to about 1 V / nm, and in some embodiments from about 0.6 to about 0.9 V / nm.The capacitor may, for example, have a relatively high breakdown voltage, such as 30 volts or more, in some embodiments about 35 volts or more, in some embodiments about 50 volts or more, in some embodiments about 65 volts or more, in some embodiments about 85 volts or more, in some embodiments about 90 volts or more, in some embodiments about 95 volts or more, and in some embodiments from about 100 volts to about 300 volts, as determined by increasing the applied voltage in steps of 3 volts until the leakage current reaches 1 mA.While the thickness of the dielectric can generally vary depending on the position of the anode body, the "dielectric thickness" for determining the breakdown strength is generally considered to be the greatest thickness of the dielectric, which is typically between about 50 and about 500 nm, in some embodiments between about 80 and about 350 nm, and in some embodiments between about 100 and about 300 nm. The dielectric thickness can be measured with the Zeiss Sigma FESEM at 20,000x to 50,000x magnification, with the sample being prepared by cutting a finished part in a plane perpendicular to the longest dimension of the finished part and the thickness being measured at points where the cut passes perpendicularly through the dielectric layer. C. Pre-coating
[0030] Although not required, a pre-coating can optionally be applied over the dielectric, which contains a metal-organic compound. The metal-organic compound can have the following general formula: where, M is a metal-organic atom, e.g. silicon, titanium, and so on; R1, R2 and R3 are independently an alkyl (e.g. methyl, ethyl, propyl, etc.) or a hydroxyalkyl (e.g. hydroxymethyl, hydroxyethyl, hydroxypropyl, etc.), wherein at least one of the residues R1, R2 and R3 is a hydroxyalkyl; n is an integer from 0 to 8, in some embodiments from 1 to 6 and in some embodiments from 2 to 4 (e.g. 3); and X is an organic or inorganic functional group, such as glycidyl, glycidyloxy, mercapto, amino, vinyl, etc.
[0031] In certain embodiments, R1, R2, and R3 can be a hydroxyalkyl (e.g., OCH3). In other embodiments, however, R1 can be an alkyl (e.g., CH3), and R2 and R3 can be a hydroxyalkyl (e.g., OCH3).
[0032] In certain embodiments, M can also be silicon, so that the metal-organic compound is an organosilane compound, such as an alkoxysilane. Suitable alkoxysilanes are, for example, 3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, 3-aminopropylmethyldimethoxysilane, 3-aminopropylmethyldiethoxysilane, 3-(2-aminoethyl)aminopropyltrimethoxysilane, 3-mercaptopropyltrimethoxysilane, 3-mercaptopropyltriethoxysilane, 3-Mercaptopropylmethyldimethoxysilane, 3-Mercaptopropylmethyldiethoxysilane, glycidoxymethyltrimethoxysilane, glycidoxymethyltriethoxysilane, glycidoxymethyltripropoxysilane, glycidoxymethyltributoxysilane,β-glycidoxyethyltrimethoxysilane,β-glycidoxyethyltriethoxysilane,β-glycidoxyethyltripropoxysilane, β-glycidoxyethyl-tributoxysilane,β-glycidoxyethyl-trimethoxysilane,α -Glycidoxyethyl-triethoxysilane, α -Glycidoxyethyl-tripropoxysilane, α -Glycidoxyethyl-tributoxysilane, γ-Glycidoxypropyl-trimethoxysilane, γ -Glycidoxypropyltriethoxysilane,γ - Glycidoxypropyl-tripropoxysilan,γ -Glycidoxypropyltributoxysilan, β-Glycidoxypropyltrimethoxysilan,β -Glycidoxypropyltriethoxysilan,β - Glycidoxypropyltripropoxysilan,α -Glycidoxypropyltributoxysilan, α-Glycidoxypropyltrimethoxysilan,α -Glycidoxypropyltriethoxysilan,α - Glycidoxypropyltripropoxysilan,α -Glycidoxypropyltributoxysilan,γ - Glycidoxybutyltrimethoxysilan, δ-Glycidoxybutyltriethoxysilan,δ - Glycidoxybutyltripropoxysilan,δ -Glycidoxybutyltributoxysilan,δ - Glycidoxybutyltrimethoxysilan, γ-Glycidoxybutyltriethoxysilan,γ - Glycidoxybutyltripropoxysilan,γ -propoxybutyltributoxysilan,δ - Glycidoxybutyltrimethoxysilan,δ -Glycidoxybutyltriethoxysilan, δ-Glycidoxybutyltripropoxysilan,α -Glycidoxybutyltrimethoxysilan,α - Glycidoxybutyltriethoxysilan,α -Glycidoxybutyltripropoxysilan,α - Glycidoxybutyltributoxysilan, (3,4-Epoxycyclohexyl)-methyl-trimethoxysilan, (3,4-Epoxycyclohexyl)methyl-triethoxysilan, (3,4-Epoxycyclohexyl)methyltripropoxysilan, (3,4-Epoxycyclohexyl)-methyl-tributoxysilan, (3,4-Epoxycyclohexyl)ethyl-trimethoxysilan, (3,4-Epoxycyclohexyl)ethyl-triethoxysilan, (3,4-Epoxycyclohexyl)ethyltripropoxysilan, (3,4-Epoxycyclohexyl)ethyltributoxysilan, (3,4-Epoxycyclohexyl)propyltrimethoxysilan, (3,4-Epoxycyclohexyl)propyltriethoxysilan, (3,4-Epoxycyclohexyl)propyl-tripropoxysilan, (3,4-Epoxycyclohexyl)propyltributoxysilan, (3,4-Epoxycyclohexyl)butyltrimethoxysilan, (3,4-Epoxycyclohexy)butyltriethoxysilan, (3,4-Epoxycyclohexyl)butyltripropoxysilan, (3,4-Epoxycyclohexyl)butyltributoxysilan und so weiter.,
[0033] The method used to apply the pre-coating to the capacitor housing can vary. In one particular embodiment, the compound is dissolved in an organic solvent and applied to the part as a solution, for example, by screen printing, dipping, electrophoretic coating, spraying, etc. The organic solvent can vary but is generally an alcohol, such as methanol, ethanol, etc. Organometallic compounds can constitute approximately 0.1 wt% to approximately 10 wt% of the solution, in some embodiments approximately 0.2 wt% to approximately 8 wt%, and in some embodiments approximately 0.5 wt% to approximately 5 wt%. The solvents can also constitute between approximately 90 wt% and approximately 99.9 wt% of the solution, in some embodiments between approximately 92 wt% and approximately 99.8 wt%, and in some embodiments between approximately 95 wt% and approximately 99.5 wt%.After application, the part can then be dried to remove the solvent and form a pre-coating containing the metal-organic compound. D. Solid electrolyte
[0034] A solid electrolyte lies above the dielectric and the optional pre-coating. The total thickness of the solid electrolyte is typically about 1 to about 50 µm, and in some embodiments about 5 to about 20 µm.
[0035] The solid electrolyte typically contains one or more layers of a conductive polymer (e.g., polyheterocycles such as polypyrroles, polythiophenes, polyanilines, etc., polyacetylenes, poly-p-phenylenes, polyphenolates, etc.). Thiophene polymers are particularly well suited for use in the solid electrolyte. In certain embodiments, for example, a thiophene polymer may be used having repeating units of the following formula (I): where, R7 is a linear or branched C1 to C18 Alkyl radical (e.g. methyl, ethyl, n- or iso-propyl, n-, iso-, sec- or tert-butyl, n-pentyl, 1-methylbutyl, 2-methylbutyl, 3-methylbutyl, 1-ethylpropyl, 1,1-dimethylpropyl, 1,2-dimethylpropyl, 2,2-dimethylpropyl, n-hexyl, n-heptyl, n-octyl, 2-ethylhexyl, n-nonyl, n-decyl, n-undecyl, n-dodecyl, n-tridecyl, n-tetradecyl, n-hexadecyl, n-octadecyl, etc.); C5 to C 12 Cycloalkyl radical (e.g. cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, cyclononyl, cyclodecyl, etc.); C6 to C 14 Aryl group (e.g., phenyl, naphthyl, etc.); C7- to C 18 -Aralkyl group (e.g. benzyl, o-, m-, p-tolyl, 2,3-, 2,4-, 2,5-, 2-6, 3-4-, 3,5-xylyl, mesityl, etc.); and q is an integer from 0 to 8, in some embodiments from 0 to 2, and in one embodiment 0.
[0036] Thiophene polymers are particularly suitable, in which “D” is an optionally substituted C2 to C3 alkylene residue. The polymer may, for example, optionally comprise substituted poly(3,4-ethylenedioxythiophene) or derivatives thereof, having repeating units of the following general formula (II):
[0037] In a particular embodiment, “q” is equal to 0. A commercially suitable example of 3,4-ethylenedioxythiophene is available from Heraeus under the name Clevios™ M. Other suitable monomers are also described in US patents Nos. 5,111,327 by Blohm et al. and 6,635,729 by Groenendaal et al. Higher molecular weight derivatives, i.e., tetramers, pentamers, etc., of the monomers are suitable for use in the present invention. The derivatives may consist of identical or different monomer units and may be used in pure form or in mixtures with each other and / or with the monomers. Oxidized or reduced forms of these precursors may also be used.
[0038] To form the polymer, the precursor monomer can be polymerized in the presence of an oxidative catalyst (e.g., chemically polymerized). The oxidative catalyst typically contains a transition metal cation, such as iron(III), copper(II), chromium(VI), cerium(IV), manganese(IV), manganese(VII), or ruthenium(III), etc. A dopant can also be used to impart excess charge to the conductive polymer and stabilize its conductivity. The dopant typically comprises an inorganic or organic anion, such as a sulfonic acid ion (e.g., p-toluenesulfonate). In certain embodiments, the oxidative catalyst has both a catalytic and a doping function, as it contains a cation (e.g., a transition metal) and an anion (e.g., a sulfonic acid). The oxidative catalyst can, for example, be a transition metal salt containing iron(III) cations such as iron(III) halides (e.g.,FeCl3) or iron(III) salts of other inorganic acids such as Fe(ClO4)3 or Fe. (2) (SO4)3 as well as the iron(III) salts of organic acids and inorganic acids with organic residues. Examples of iron(III) salts of inorganic acids with organic residues are, for example, iron(III) salts of sulfuric acid monoesters from C1 to C 20 -Alkanols (e.g., iron(III) salt of lauryl sulfate). Other examples of iron(III) salts of organic acids are iron(III) salts from C1 to C6. 20 -Alkanesulfonic acids (e.g., methanesulfonic, ethanesulfonic, propanesulfonic, butanesulfonic, or dodecanesulfonic acid), iron(III) salts of aliphatic perfluorosulfonic acids (e.g., trifluoromethanesulfonic acid, perfluorobutanesulfonic acid, or perfluorooctanesulfonic acid); iron(III) salts of aliphatic C1 to C 20-Carboxylic acids (e.g., 2-ethylhexylcarboxylic acid); iron(III) salts of aliphatic perfluorocarboxylic acids (e.g., trifluoroacetic acid or perfluorooctanoic acid); iron(III) salts of aromatic sulfonic acids, optionally modified by C1 to C 20 -Alkyl groups substituted (e.g., benzenesulfonic acid, o-toluenesulfonic acid, p-toluenesulfonic acid, or dodecylbenzenesulfonic acid); iron(III) salts of cycloalkanesulfonic acids (e.g., camphorsulfonic acid); and so on. Mixtures of the above-mentioned iron(III) salts can also be used. Iron(III) p-toluenesulfonate, iron(III) o-toluenesulfonate, and mixtures thereof are particularly suitable. A commercially suitable example of iron(III) p-toluenesulfonate is available from Heraeus under the name Clevios™ C.
[0039] The oxidation catalyst and the precursor monomer can be used either sequentially or together to initiate the polymerization reaction. For example, the monomer can first be mixed with the oxidative catalyst to form a precursor solution. In certain embodiments, less than the normally required stoichiometric amount of the oxidative catalyst can be used to slow down the polymerization of the monomer and form oligomers that are shorter than those obtained upon complete polymerization to a polymer, thus allowing for better penetration into the powder with a high specific charge. For example, if the monomer contains a thiophene monomer (e.g., 3,4-ethylenedioxythiophene), the molar ratio normally required for polymerization of the monomer is approximately 1 mole of monomer to 18 moles of oxidative catalyst.However, there may also be less than 18 mol of the oxidative polymerization catalyst in the polymerization solution per mol of monomer (e.g. 3,4-ethylenedioxythiophene), such as about 15 mol or less, in some embodiments about 4 to about 12 mol and in some embodiments about 5 to about 10 mol.
[0040] In addition to a monomer, an oxidation catalyst, and an optional dopant, the polymerization solution can also contain other components, such as one or more solvents. Particularly suitable solvents include water, alcohols (e.g., methanol, ethanol, n-propanol, isopropanol, and butanol), glycols (e.g., propylene glycol, butylene glycol, triethylene glycol, hexylene glycol, polyethylene glycols, ethoxydiglycol, and dipropylene glycol), glycol ethers (e.g., methyl glycol ethers, ethyl glycol ethers, and isopropyl glycol ethers), ethers (e.g., diethyl ether and tetrahydrofuran), triglycerides, ketones, esters (e.g., ethyl acetate, butyl acetate, diethylene glycol ether acetate, and methoxypropyl acetate), and amides (e.g., dimethylformamide, dimethylacetamide, dimethylcaprylic / capric acidamide, and N-alkylpyrrolidones). Nitriles (e.g., acetonitrile, propionitrile, butyronitrile, and benzonitrile); sulfoxides or sulfones (e.g., dimethyl sulfoxide (DMSO) and sulfolane); and so on, as well as mixtures of the aforementioned substances (e.g., nitriles, propionitrile, butyronitrile, and benzonitrile); sulfoxides or sulfones (e.g., dimethyl sulfoxide (DMSO) and sulfolan); and so forth, as well as mixtures of the aforementioned substances (e.g., sulfoxide ...B. water and alcohol).
[0041] The polymerization solution is typically maintained at a relatively low temperature during the reaction, such as -20 °C to about 50 °C, in some embodiments from about -15 °C to about 30 °C, and in some embodiments from about -10 °C to about 10 °C. The solution can be applied to the anode body using any suitable deposition technique known in the art, e.g., by screen printing, dipping, electrophoretic coating, and spraying. Regardless of the deposition technique, the monomer generally begins to react as soon as it is present on the anode body to form a polymer layer. The time that the monomer can react on the anode body is usually long enough to allow good impregnation of the polymer in the small pores of the powder with its high specific charge.In most embodiments, this time period (“impregnation time”) is, for example, about 1 minute or more, in some embodiments about 1.5 minutes or more, and in some embodiments about 2 to about 5 minutes. After the reaction, the resulting conductive polymer layer(s) can be brought into contact with a washing solution to remove various byproducts, excess catalysts, etc. The time during which the washing solution is in contact with the conductive polymer layer(s) (“washing time”) is generally long enough to ensure that the byproducts, excess catalyst, etc., can be adequately removed from the small pores of the high-specific-charge powder. The washing time can be, for example, about 25 minutes or more, in some embodiments about 30 minutes or more, and in some embodiments from about 45 minutes to about 90 minutes.During this period, washing can be performed in a single step or in several steps, with the total time of each step falling within the range mentioned above. The washing solution can vary as desired, but generally consists of one or more solvents (e.g., water, alcohol, etc.) and, if necessary, a dopant, as described above.
[0042] After washing, the conductive polymer layer(s) can be dried, typically at a temperature of about 15 °C or higher, in some embodiments at about 20 °C or higher, and in some embodiments from about 20 °C to about 80 °C. The polymer layer(s) can also be cured after formation. Curing can be performed after each application of a conductive polymer layer or after the application of the entire conductive polymer coating. In some embodiments, the conductive polymer can be cured by immersing the anode body in an electrolyte solution and subsequently applying a constant voltage to the solution until the current is reduced to a preselected level. If desired, such curing can be carried out in several steps. An electrolyte solution can, for example, be a dilute solution of the monomer, the catalyst, and the dopant in an alcoholic solvent (e.g., alcohol).Ethanol).
[0043] In the process described above, the conductive polymers are generally formed "in situ" on the anode body. This is, of course, not essential. In other embodiments, the conductive polymer can, for example, be prepolymerized. In one embodiment, the prepolymerized polymer is, for instance, an intrinsically conductive polymer that has a positive charge on the main chain, which is at least partially compensated by anions covalently bonded to the polymer. Such polymers can, for example, exhibit a relatively high specific conductivity in the dry state of about 1 Siemens per centimeter ("S / cm") or more, in some embodiments about 10 S / cm or more, in some embodiments about 25 S / cm or more, in some embodiments about 40 S / cm or more, and in some embodiments from about 50 to about 500 S / cm.An example of a suitable intrinsically conductive thiophene polymer may have recurring units of the following formula (III): where,. R is (CH2) a -O-(CH2) b -L, where L is a bond or HC([CH2] c H) is; a lies between 0 and 10, in some embodiments between 0 and 6 and in some embodiments between 1 and 4 (e.g. 1); b 1 to 18, in some embodiments 1 to 10 and in some embodiments 2 to 6 (e.g. 2, 3, 4 or 5); c lies between 0 and 10, in some embodiments between 0 and 6 and in some embodiments between 1 and 4 (e.g. 1); Z is an anion, like SO(3) - , C(O)O - , BF(4) - , CF3SO (3) - , SbF6 - , N(SO2CF3)2 - , C4H3O4 - , ClO4 - , etc; X is a cation, such as hydrogen, an alkali metal (e.g., lithium, sodium, rubidium, cesium or potassium), ammonium, etc.
[0044] In a particular embodiment, Z in formula (III) is a sulfonate ion, such that the intrinsically conductive polymer contains recurring units of the following formula (IV): wherein R and X are defined as above. In formulas (III) or (IV), a is preferably 1 and b is preferably 3 or 4. Likewise, X is preferably sodium or potassium.
[0045] If desired, the polymer can be a copolymer containing other types of repeating units. In such embodiments, the repeating units of formula (III) typically constitute about 50 mol% or more, in some embodiments about 75 mol% to about 99 mol%, and in some embodiments about 85 mol% to about 95 mol% of the total amount of repeating units in the copolymer. Of course, the polymer can also be a homopolymer, provided it contains 100 mol% of the repeating units of formula (III). Specific examples of such homopolymers are poly(4-(2,3-dihydrothieno-[3,4-b][1,4]dioxin-2-ylmethoxy)-1-butanesulfonic acid, salt) and poly(4-(2,3-dihydrothieno-[3,4-b][1,4]dioxin-2-ylmethoxy)-1-propanesulfonic acid, salt).
[0046] In another embodiment, the intrinsically conductive polymer has repeating thiophene units of the following general formula (V): where, a and b are defined as above; R5 is an optionally substituted linear or branched C1-C6 alkyl group (e.g. methyl) or a halogen atom (e.g. fluorine); X a hydrogen atom, an alkali metal (e.g. Li, Na or K), NH(R 1) 3 or HNC5H5, where R 1 each is independently a hydrogen atom or a possibly substituted C1-C6 alkyl group.
[0047] Specific examples of thiophene compounds used to form such repeats are described in US Patent No. 9,718,905 and include, for example, sodium 3-[(2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-ethyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-propyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-butyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-pentyl-1-propanesulfonate, sodium Sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-isopropyl-1-propanesulfonate, sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-isobutyl-1-propanesulfonate, Sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)-methoxy]-1-isopentyl-1-propanesulfonate,sodium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-fluoro-1-propanesulfonate, potassium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, 3-[(2,3-Dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonic acid, ammonium 3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, Triethylammonium-3-[(2,3-dihydrothieno[3,4-b]-[1,4]dioxin-2-yl)methoxy]-1-methyl-1-propanesulfonate, etc., as well as combinations thereof and derivatives thereof. Each of the thiophene monomers described above can be prepared from thieno[3,4-b]-1,4-dioxin-2-methanol and a branched sultone compound by a known procedure (e.g., Journal of Electroanalytical Chemistry, 443, 217 to 226 (1998)).
[0048] “Extrinsically” conductive polymers can also be used, which generally require the presence of a separate counterion that is not covalently bonded to the polymer. An example of such an extrinsically conductive polymer is poly(3,4-ethylenedioxythiophene). The counterion can be a monomeric or polymeric anion that counteracts the charge of the conductive polymer. For example, polymeric anions can be derived from polymeric carboxylic acids (e.g., poly(meth)acrylic acids such as poly-2-sulfoethyl(meth)acrylate or poly-3-propylsulfo(meth)acrylate, polymaleic acids, etc.), polymeric sulfonic acids (e.g., polystyrenesulfonic acids (“PSS”), polyvinylsulfonic acids, etc.), and so on, as well as their salts, such as alkali, alkaline earth, transition metal, or ammonium salts. Likewise, suitable monomeric anions from C1 to C2 can be used. 20-Alkanesulfonic acids (e.g., dodecanesulfonic acid), aliphatic fluorosulfonic acids (e.g., trifluoromethanesulfonic acid, perfluorobutanesulfonic acid, perfluorooctanesulfonic acid, trifluoromethanesulfonimide, etc.); aliphatic C1 to C 20 -Carboxylic acids (e.g., 2-ethylhexylcarboxylic acid); aliphatic fluorocarboxylic acids (e.g., trifluoroacetic acid or perfluorooctanoic acid); aromatic sulfonic acids, optionally substituted by C1 to C 20-Alkyl groups (e.g., benzenesulfonic acid, o-toluenesulfonic acid, p-toluenesulfonic acid, or dodecylbenzenesulfonic acid); cycloalkanesulfonic acids (e.g., camphorsulfonic acid), boron compounds (e.g., tetrafluoroboric acid), phosphorus compounds (e.g., hexafluorophosphoric acid), etc., as well as their salts, such as alkali, alkaline earth, transition metal, or ammonium salts. Particularly suitable counterions are polymeric anions, such as those derived from a polymeric carboxylic or sulfonic acid (e.g., polystyrenesulfonic acid ("PSS")). The molecular weight of such compounds is typically in the range of about 1,000 to about 2,000,000, and in some embodiments in the range of about 2,000 to about 500,000.
[0049] Regardless of whether they are intrinsically or extrinsically conductive, a prepolymerized polymer layer can be applied to the anode body in various forms, e.g., as a solution, a dispersion, etc. Intrinsically conductive polymers, for example, are preferably applied as a solution, while extrinsically conductive polymers are preferably applied as a dispersion.
[0050] When a solution is used, the polymer concentration can vary depending on the desired viscosity and the method of application to the anode. Typically, however, the polymer constitutes approximately 0.1 to 10 wt% of the solution, in some embodiments approximately 0.4 to 5 wt%, and in some embodiments approximately 0.5 to 4 wt%. The solvent(s) can also constitute approximately 90 wt% to 99.9 wt% of the solution, in some embodiments approximately 95 wt% to 99.6 wt%, and in some embodiments approximately 96 wt% to 99.5 wt%. While other solvents can be used, it is generally desirable for water to be the main solvent, so the solution is considered an "aqueous" solution. In most embodiments, for example, water constitutes at least approximately 50 wt%, and in some embodiments at least approximately 75 wt%.-% and in some embodiments between approximately 90 and 100 wt% of the solvent(s) used. If a solution is used, it can be applied to the anode by any known technique, e.g., by dipping, casting (e.g., curtain coating, spin coating, etc.), printing (e.g., gravure printing, offset printing, screen printing, etc.), etc. The resulting conductive polymer layer can be dried and / or washed after application to the anode.
[0051] When a dispersion is used, the conductive polymer is generally present in the form of prepolymerized conductive particles. Such particles typically have an average size (e.g., diameter) of about 1 to about 100 nanometers, in some embodiments from about 2 to about 80 nanometers, and in some embodiments from about 4 to about 50 nanometers. The diameter of the particles can be determined using known techniques, e.g., with an ultracentrifuge, laser diffraction, etc. The shape of the particles can also vary. In one particular embodiment, for example, the particles have a spherical shape. However, it is understood that other shapes are also possible within the scope of the present invention, such as plates, rods, discs, bars, tubes, irregular shapes, etc.The concentration of particles in the dispersion can vary depending on the desired viscosity of the dispersion and the specific way in which the dispersion is to be applied to the capacitor element. Typically, however, the particles constitute approximately 0.1 to approximately 10 wt.%, in some embodiments approximately 0.4 to approximately 5 wt.%, and in some embodiments approximately 0.5 to approximately 4 wt.% of the dispersion.
[0052] The dispersion may also contain one or more binders to increase the adhesion of the polymer layer and the stability of the particles in the dispersion. The binders can be organic in nature, such as polyvinyl alcohols, polyvinylpyrrolidones, polyvinyl chlorides, polyvinyl acetates, polyvinyl butyrates, polyacrylic esters, polyacrylamides, polymethacrylic esters, polymethacrylamides, polyacrylonitriles, styrene / acrylic esters, vinyl acetate / acrylic esters and ethylene / vinyl acetate copolymers, polybutadiene, polyisoprene, polystyrene, polyethers, polyesters, polycarbonates, polyurethanes, polyamides, polyimides, polysulfones, melamine-formaldehyde resins, epoxy resins, silicone resins, or celluloses. Crosslinking agents can also be used to improve the adhesion of the binders. Such crosslinking agents can be, for example,These could be melamine compounds, masked isocyanates or functional silanes, such as 3-glycidoxypropyltrialkoxysilane, tetraethoxysilane and tetraethoxysilane hydrolysate, or crosslinkable polymers, such as polyurethanes, polyacrylates or polyolefins, and subsequent crosslinking.
[0053] Dispersants can also be used to facilitate the application of the coating to the anode. Suitable dispersants include solvents such as aliphatic alcohols (e.g., methanol, ethanol, isopropanol, and butanol), aliphatic ketones (e.g., acetone and methyl ethyl ketones), aliphatic carboxylic acid esters (e.g., ethyl acetate and butyl acetate), aromatic hydrocarbons (e.g., toluene and xylene), aliphatic hydrocarbons (e.g., hexane, heptane, and cyclohexane), chlorinated hydrocarbons (e.g., dichloromethane and dichloroethane), aliphatic nitriles (e.g., acetonitrile), aliphatic sulfoxides and sulfones (e.g., dimethyl sulfoxide and sulfolane), aliphatic carboxylic acid amides (e.g., methylacetamide, dimethylacetamide, and dimethylformamide), aliphatic and araliphatic ethers (e.g., diethyl ether and anisole), water, and mixtures of the aforementioned solvents. Water is a particularly suitable dispersing agent.
[0054] In addition to those mentioned above, other components can also be used in the dispersion. For example, conventional fillers with a particle size of approximately 10 nanometers to approximately 100 micrometers, in some embodiments approximately 50 nanometers to approximately 50 micrometers, and in some embodiments approximately 100 nanometers to approximately 30 micrometers can be used. Examples of such fillers include calcium carbonate, silicates, silicic acid, calcium or barium sulfate, aluminum hydroxide, glass fibers or incandescent bulbs, wood flour, cellulose powder, carbon black, electrically conductive polymers, etc. The fillers can be incorporated into the dispersion in powder form, but can also be present in other forms, e.g., as fibers.
[0055] Surface-active substances, such as ionic or non-ionic surfactants, can also be used in the dispersion. Furthermore, adhesion promoters can be used, such as organofunctional silanes or their hydrolysates, e.g., 3-glycidoxypropyltrialkoxysilane, 3-aminopropyltriethoxysilane, 3-mercaptopropyltrimethoxysilane, 3-metacryloxypropyltrimethoxysilane, vinyltrimethoxysilane, or octyltriethoxysilane. The dispersion may also contain additives that increase conductivity, such as ether-containing compounds (e.g., tetrahydrofuran), lactone-containing compounds (e.g., γ-butyrolactone or γ-valerolactone), amide- or lactam-containing compounds (e.g., caprolactam, N-methylcaprolactam, N,N-dimethylacetamide, N-methylacetamide, N,N-dimethylformamide (DMF), N-methylformamide, N-methylformanilide, N-methylpyrrolidone (NMP), N-octylpyrrolidone, or pyrrolidone), sulfones and sulfoxides (e.g., sulfolane (tetramethylenesulfone) or dimethyl sulfoxide (DMSO)), sugars or sugar derivatives (e.g.,sucrose, glucose, fructose or lactose), sugar alcohols (e.g. sorbitol or mannitol), furan derivatives (e.g. 2-furan carboxylic acid or 3-furan carboxylic acid) and alcohols (e.g. ethylene glycol, glycerin, di- or triethylene glycol).
[0056] The dispersion can be applied using a variety of known methods, such as centrifugal coating, impregnation, casting, dropwise application, injection, spraying, doctor blade application, brushing, printing (e.g., inkjet, screen, or pad printing), or dipping. The viscosity of the dispersion typically ranges from approximately 0.1 to approximately 100,000 mPas (measured at a shear rate of 100 s⁻¹). -1 , in some embodiments at about 1 to about 10,000 mPas, in some embodiments at about 10 to about 1,500 mPas and in some embodiments at about 100 to about 1,000 mPas.
[0057] The solid electrolyte can consist of multiple layers, e.g., inner and / or outer layers. In this context, "inner" refers to one or more layers superimposed on the dielectric, either directly or over another layer (e.g., a pre-coating layer). The inner layer(s) typically contain, for example, an in-situ polymerized polymer and / or an intrinsically conductive polymer, as described above. One or more inner layers may be used. For example, the solid electrolyte typically contains 2 to 30, in some embodiments 4 to 20, and in some embodiments approximately 5 to 15 (e.g., 10 layers) inner layers. The solid electrolyte may contain only "inner layers," so that it consists essentially of the same material, i.e., intrinsically conductive polymers and / or in-situ polymerized layers.In other embodiments, however, the solid electrolyte may also contain one or more optional "outer" conductive polymer layers formed from a different material than and extending beyond the inner layer(s). The outer layer(s) may, for example, be formed from a dispersion of an extrinsically conductive polymer. In a particular embodiment, the outer layer(s) are formed mainly from such extrinsically conductive polymers, comprising approximately 50 wt.% or more, in some embodiments approximately 70 wt.% or more, and in some embodiments approximately 90 wt.% or more (e.g., 100 wt.%) of a respective outer layer. One or more outer layers may be used. Thus, the solid electrolyte may, for example, contain 2 to 30, in some embodiments 4 to 20, and in some embodiments approximately 5 to 15 outer layers. E. External polymer coating
[0058] Optionally, an external polymer coating can be used, positioned over the solid electrolyte. If used, the external polymer coating typically comprises one or more layers formed from prepolymerized conductive polymer particles, as described above (e.g., a dispersion of extrinsically conductive polymer particles). The external coating can extend further into the edge region of the capacitor body to increase adhesion to the dielectric and create a mechanically more robust component, which can reduce the equivalent series resistance and leakage current. Since the goal is usually to improve the degree of edge coverage rather than impregnating the interior of the anode body, the particles used in the external coating can be larger than those used in the outer layers of the solid electrolyte.Thus, the ratio of the average size of the particles used in the outer polymer coating to the average size of the particles used in a dispersion of the solid electrolyte is typically about 1.5 to about 30, in some embodiments about 2 to about 20, and in some embodiments about 5 to about 15. For example, the particles used in the dispersion of the outer coating may have an average size of about 80 to about 500 nanometers, in some embodiments about 90 to about 250 nanometers, and in some embodiments about 100 to about 200 nanometers.
[0059] If desired, a crosslinking agent can also be used in the external polymer coating to increase the degree of adhesion to the solid electrolyte. The crosslinking agent is typically applied before the dispersion for the outer coating. Suitable crosslinking agents are described, for example, in US Patent Publication No. 2007 / 0064376 by Merker et al. Described and include, for example, amines (e.g., diamines, triamines, oligomeric amines, polyamines, etc.), multivalent metal cations such as salts or compounds of Mg, Al, Ca, Fe, Cr, Mn, Ba, Ti, Co, Ni, Cu, Ru, Ce, or Zn, phosphonium compounds, sulfonium compounds, etc. Particularly suitable examples are, for example, 1,4-diaminocyclohexane, 1,4-bis(aminomethyl)cyclohexane, ethylenediamine, 1,6-hexanediamine, 1,7-heptanediamine, 1,8-octanediamine, 1,9-nonanediamine, 1,10-decanediamine, 1,12-dodecanediamine, N,N-dimethylethylenediamine, N,N,N',N'-tetramethylethylenediamine, N,N,N',N'-tetramethyl-1,4-butanediamine, etc., as well as mixtures. of that..
[0060] The crosslinking agent is typically applied from a solution or dispersion with a pH of 1 to 10, in some embodiments from 2 to 7, and in some embodiments from 3 to 6, determined at 25 °C. Acidic compounds can be used to achieve the desired pH. Examples of solvents or dispersants for the crosslinking agent include water or organic solvents such as alcohols, ketones, carboxylic acid esters, etc. The crosslinking agent can be applied to the condenser by any known method, e.g., centrifugal casting, impregnation, casting, dropwise application, spraying, vapor deposition, sputtering, sublimation, knife coating, painting, or printing, e.g., by inkjet, screen, or pad printing. After application, the crosslinking agent can be dried before the polymer dispersion is applied. This process can then be repeated until the desired thickness is achieved.The total thickness of the entire outer polymer coating, including the crosslinking agent and dispersion layer, can, for example, range from about 1 to about 50 µm, in some cases from about 2 to about 40 µm, and in some cases from about 5 to about 20 µm. F. Moisture barrier layer
[0061] If desired, a moisture barrier layer can be applied over the solid electrolyte and / or the optional external polymer coating. The moisture barrier layer can be formed from a variety of different materials, such as a hydrophobic elastomer, e.g., silicones, fluoropolymers, etc. Silicone polymers are particularly suitable for use in the moisture barrier layer of the present invention. Such elastomers are generally derived from polyorganosiloxanes, such as those with the following general formula: where, x is an integer greater than 1; and R1, R2, R3, R4, R5, R6, R7, and R8 are independent monovalent groups, typically containing 1 to about 20 carbon atoms, such as alkyl groups (e.g., methyl, ethyl, propyl, pentyl, octyl, undecyl, octadecyl, etc.); alkoxy groups (e.g., methoxy, ethoxy, propoxy, etc.); carboxyalkyl groups (e.g., acetyl); cycloalkyl groups (e.g., cyclohexyl); alkenyl groups (e.g., vinyl, allyl, butenyl, hexenyl, etc.); aryl groups (e.g., phenyl, tolyl, xylyl, benzyl, 2-phenylethyl, etc.); and halogenated hydrocarbon groups (e.g., 3,3,3-trifluoropropyl, 3-chloropropyl, dichlorophenyl, etc.). Examples of such polyorganosiloxanes are, for example,Polydimethylsiloxane (“PDMS”), polymethylhydrogensiloxane, dimethylidiphenylpolysiloxane, dimethyl / methylphenylpolysiloxane, polymethylphenylsiloxane, methylphenyl / dimethylsiloxane, polydimethylsiloxane with vinyldimethyl end groups, vinylmethyl / dimethylpolysiloxane, vinylmethyl / dimethylpolysiloxane with vinyldimethyl end groups, polydimethylsiloxane with divinylmethyl end groups, polydimethylsiloxane with vinylphenylmethyl end groups, polydimethylsiloxane with dimethylhydro end groups, methylhydro / dimethylpolysiloxane, methyloctylpolysiloxane with methylhydro end groups, methylhydro / phenylmethyl-polysiloxane, fluoromodified polysiloxane, etc. To form an elastomer, the polyorganosiloxane can be crosslinked using a variety of known techniques, e.g., catalyst curing (e.g., platinum catalysts), vulcanization at room temperature, moisture curing, etc. Crosslinking agents such as Alkoxysilanes with the formula Si-OR are used, where RH is alkyl (e.g.Methyl), alkenyl, carboxyalkyl (e.g., acetyl), etc.
[0062] In addition to hydrophobicity, it is generally desirable for the material used to form the moisture barrier to have a relatively low modulus and a degree of flexibility. This can help absorb some of the thermal stresses caused by the expansion of the enclosure and also allows it to withstand compressive forces. The flexibility of the material can be characterized by a correspondingly low modulus of elasticity (“Young’s modulus”), such as 5,000 kilopascals (“kPa”) or less, in some embodiments from about 1 to about 2,000 kPa, and in some embodiments from about 2 to about 500 kPa, measured at a temperature of about 25 °C. The material also typically possesses a degree of strength that allows it to retain its shape even when subjected to compressive forces. For example, the material may have a tensile strength of about 1 to about 5.The capacitor exhibits a pressure of approximately 000 kPa, in some embodiments from about 10 to about 2,000 kPa, and in some embodiments from about 50 to about 1,000 kPa, measured at a temperature of about 25 °C. Under the conditions mentioned above, the hydrophobic elastomer can further improve the capacitor's ability to function under extreme conditions.
[0063] To achieve the desired flexibility and strength properties, a non-conductive filler can be used in the moisture barrier layer. When such additives are used, they typically constitute about 0.5 to 30 wt.%, in some embodiments about 1 to 25 wt.%, and in some embodiments about 2 to 20 wt.% of the moisture barrier layer. The silicone elastomer can constitute about 70 wt.% to about 99.5 wt.%, in some embodiments about 75 wt.% to about 99 wt.%, and in some embodiments about 80 wt.% to about 98 wt.% of the moisture barrier layer. A particular example of such a filler is, for instance, silica. While most forms of silicon dioxide have a relatively hydrophilic surface due to the presence of silanol groups (Si-OH), the silicon dioxide can optionally be surface-treated so that its surface (CH3) nThe surface treatment agent contains -Si groups, where n is an integer from 1 to 3, further increasing the hydrophobicity of the moisture barrier layer. The surface treatment agent can be, for example, an organosilicon compound monomer with a hydrolyzable group or a partially hydrolyzed version thereof. Examples of such compounds are organosilasans, silane coupling agents as described above, etc.
[0064] The moisture barrier can be applied to any surface of the capacitor to achieve the desired properties. For example, the moisture barrier can be applied to the top, bottom, and / or side surfaces of the capacitor. The moisture barrier can also be applied to the front and / or back surfaces of the capacitor. The moisture barrier can cover the entire surface or only a portion of it. In one embodiment, for example, the moisture barrier covers about 30% or more, in some embodiments about 40% or more, and in some embodiments about 50% or more of the surface of the capacitor on which it is applied. G. Other optional components
[0065] If desired, the capacitor element can also contain other layers known in the art. For example, an adhesive layer can optionally be formed between the dielectric and the solid electrolyte. The adhesive layer can be located, for instance, between the dielectric and the pre-coating and / or between the pre-coating and the solid electrolyte. Regardless of the specific layer, the adhesive layer typically consists of a relatively insulating resinous material (natural or synthetic). Such materials can have a resistivity of more than 10 Ω·cm, in some embodiments more than 100 Ω·cm, in some embodiments more than 1,000 Ω·cm, and in some embodiments more than 1 × 10⁻⁶ Ω·cm. 5 Ω·cm and in some embodiments of more than 1 x 10 10exhibiting Ω·cm. Some resinous materials that can be used in the present invention include, among others, polyurethane, polystyrene, esters of unsaturated or saturated fatty acids (e.g., glycerides), and so on. Suitable fatty acid esters are, for example, lauric, myristic, palmitic, stearic, eleostearic, oleic, linoleic, linolenic, aleuritic, and shellolic acid esters, etc., but are not limited to these. These fatty acid esters have proven particularly useful when used in relatively complex combinations to form a “drying oil” that enables the resulting film to polymerize rapidly into a stable layer. Such drying oils may contain mono-, di-, and / or triglycerides having a glycerol backbone with one, two, or three esterified fatty acyl residues, respectively. Suitable drying oils are, for example,Olive oil, linseed oil, castor oil, tung oil, soybean oil, and shellac, but not only these. These and other adhesive layers are described in more detail in US patent no. 6,674,635 by Fife et al.
[0066] If desired, the component can also be coated with a carbon layer (e.g., graphite) or a silver layer. The silver layer can serve, for example, as a solderable conductor, contact layer, and / or charge collector for the capacitor, while the carbon layer can limit the contact between the silver layer and the solid electrolyte. Such coatings can partially or completely cover the solid electrolyte. Various techniques can be used to apply these layers, such as dipping, brushing, spraying, printing, etc. II. Housing
[0067] As mentioned above, the capacitor element is hermetically sealed within a housing. This hermetic sealing can optionally be achieved in the presence of a gas atmosphere, such as one containing air and / or at least one inert gas, to prevent oxidation of the solid electrolyte during use. The inert gas used can include, for example, nitrogen, helium, argon, xenon, neon, krypton, radon, etc., as well as mixtures thereof. Various materials, such as metals, plastics, ceramics, etc., can be used to manufacture the housing. In one embodiment, for example, the housing contains one or more layers of a metal such as tantalum, niobium, aluminum, nickel, hafnium, titanium, copper, silver, steel (e.g., stainless steel), their alloys (e.g., electrically conductive oxides), their composites (e.g., metal coated with electrically conductive oxide), etc.In another embodiment, the housing can contain one or more layers of a ceramic material such as aluminum nitride, aluminum oxide, silicon oxide, magnesium oxide, calcium oxide, glass, etc., as well as combinations thereof.
[0068] The casing can have any shape, e.g., cylindrical, D-shaped, rectangular, triangular, prismatic, etc. In the Fig. For example, an embodiment of a capacitor 100 is shown, comprising a housing 122 and a capacitor element 120. In this particular embodiment, the housing 122 is generally rectangular. Typically, the housing and the capacitor element have the same or a similar shape, so that the capacitor element can be easily accommodated in the inner cavity. In the illustrated embodiment, for example, both the capacitor element 120 and the housing 122 have a generally rectangular shape.
[0069] If desired, the capacitor of the present invention can exhibit a relatively high volumetric efficiency. To enable such a high efficiency, the capacitor element typically occupies a substantial portion of the volume of an internal cavity of the housing. For example, the capacitor element can occupy approximately 30 percent or more by volume, in some embodiments approximately 50 percent or more by volume, in some embodiments approximately 60 percent or more by volume, in some embodiments approximately 70 percent or more by volume, in some embodiments from approximately 80 percent to approximately 98 percent by volume, and in some embodiments from approximately 85 percent to 97 percent by volume of the internal cavity of the housing. For this purpose, the difference between the dimensions of the capacitor element and those of the internal cavity defined by the housing is typically relatively small.
[0070] With further reference to the Fig.2-3 The capacitor element 120 can, for example, have a length (excluding the length of the anode lead 6) that is relatively similar to the length of an inner cavity 126 defined by the housing 122. For example, the ratio of the length of the anode to the length of the inner cavity is in the range of about 0.40 to 1.00, in some embodiments from about 0.50 to about 0.99, in some embodiments from about 0.60 to about 0.99, and in some embodiments from about 0.70 to about 0.98. The capacitor element 120 can have a length of about 5 to about 10 millimeters, and the inner cavity 126 can have a length of about 6 to about 15 millimeters.Similarly, the ratio of the height of the capacitor element 120 (in the -z direction) to the height of the inner cavity 126 can be in the range of approximately 0.40 to 1.00, in some embodiments from approximately 0.50 to approximately 0.99, in some embodiments from approximately 0.60 to approximately 0.99, and in some embodiments from approximately 0.70 to approximately 0.98. The ratio of the width of the capacitor element 120 (in the -x direction) to the width of the inner cavity 126 can also be in the range of approximately 0.50 to 1.00, in some embodiments from approximately 0.60 to approximately 0.99, in some embodiments from approximately 0.70 to approximately 0.99, in some embodiments from approximately 0.80 to approximately 0.98, and in some embodiments from approximately 0.85 to approximately 0.95.For example, the width of the capacitor element 120 can be approximately 2 to approximately 7 millimeters and the width of the inner cavity 126 approximately 3 to approximately 10 millimeters, and the height of the capacitor element 120 can be approximately 0.5 to approximately 2 millimeters and the width of the inner cavity 126 approximately 0.7 to approximately 6 millimeters.
[0071] Although not strictly necessary, the capacitor element can be mounted to the housing in such a way as to form an anode and cathode connection outside the housing for later integration into a circuit. The specific configuration of the connections may depend on the intended application. In one embodiment, for example, the capacitor may be shaped to be surface-mountable yet mechanically robust. Thus, the anode lead may be electrically connected to external, surface-mountable anode and cathode connections (e.g., pads, plates, frames, etc.). These connections may extend through the housing to be connected to the capacitor. The thickness or height of the connections is generally chosen to minimize the thickness of the capacitor.For example, the thickness of the terminals can range from approximately 0.05 to approximately 1 millimeter, and in some embodiments from approximately 0.05 to approximately 0.5 millimeters and from approximately 0.1 to approximately 0.2 millimeters. If desired, the surface of the terminals can be electroplated with nickel, silver, gold, tin, etc., as is known in the art, to ensure that the finished part can be mounted on the printed circuit board. In one embodiment, the terminals are coated with nickel or silver flash, and the mounting surface is additionally covered with a tin solder layer. In another embodiment, the terminals are applied with thin outer metal layers (e.g., gold) on a base metal layer (e.g., a copper alloy) to further increase conductivity.
[0072] In certain embodiments, anode lead connectors can be used within the inner cavity of the housing to facilitate the connection to the terminals in a mechanically stable manner. For example, the capacitor 100, as in the Fig.Figures 2-3 show a first anode conductor connecting element 162a, consisting of a first section 167a and a second section 165a. The first anode conductor connecting element 162a can be formed from conductive materials similar to the external terminals. The first part 167a and the second part 165a can be integral or separate parts, connected either directly or via an additional conductive element (e.g., metal). In the illustrated embodiment, the second section 165a is provided in a plane that generally extends parallel to a lateral direction in which a first anode conductor section 26 extends (e.g., the -y direction). The first section 167a is "upright" in the sense that it is provided in a plane that is generally perpendicular to the lateral direction in which the first anode conductor section 26 extends.In this way, the first section 167a can limit the horizontal movement of the first anode conductor section 26 to improve surface contact and mechanical stability during use. If desired, an insulating material 7a (e.g., a Teflon™ disc) can be used around the first anode conductor section 26. The first section 167a can have a mounting area (not shown) that is connected to the first anode conductor section 26. The area can be U-shaped to further improve surface contact and the mechanical stability of the first anode conductor section 26. The connection of the area to the first anode conductor section 26 can be achieved using a variety of known techniques such as welding, laser welding, conductive adhesives, etc. In one particular embodiment, for example, the area is laser-welded to the first anode conductor section 26.Regardless of the chosen technique, the first part 167a can, however, keep the anode conductor in an essentially horizontal orientation to further improve the shape stability of the capacitor element.
[0073] The capacitor 100 can also include a second anode lead connection element 162b. The second anode lead connection element can be the same as or different from the first anode lead connection element. In the embodiment shown, the second anode lead connection element 162b is formed, for example, from a first section 167b and a second section 165b, similar to the first anode lead connection element 162a. In the embodiment shown, the second section 165b is provided in a plane that generally extends parallel to a lateral direction in which a second anode lead section 14 extends (e.g., the -y direction). The first section 167b is "upright" in the sense that it is provided in a plane that is generally perpendicular to the lateral direction in which the second anode lead section 14 extends.In this way, the first section 167b can limit the horizontal movement of the second anode conductor section 14 to improve surface contact and mechanical stability during use. If desired, an insulating material 7b (e.g., a Teflon™ disc) can be used around the second anode conductor section 14. The first section 167b can have a mounting area (not shown) that connects to the second anode conductor section 14. This area can be U-shaped to further improve surface contact and the mechanical stability of the second anode conductor section 14. The connection of the area to the second anode conductor section 14 can be achieved using a variety of known techniques, such as welding, laser welding, conductive adhesives, etc.Regardless of the technique chosen, the first part 167b can, however, keep the anode conductor in an essentially horizontal orientation to further improve the shape stability of the capacitor element.
[0074] The first and second connecting elements 162a and 162b, respectively, can be connected to the first and second anode terminals 127 and 129 in different ways. In the illustrated embodiment, the housing 122 comprises, for example, an outer wall 123 and two opposing side walls 124, between which a cavity 126 is formed containing the capacitor element 120. The outer wall 123 and the side walls 124 can consist of one or more layers of a metal, plastic, or ceramic material, as described above. In this particular embodiment, the first anode terminal 127 comprises a first region 127a, which is located inside the housing 122 and is electrically connected to the first anode terminal element 162a, and a second region 127b, which is located outside the housing 122 and forms a mounting surface 201.Likewise, the second anode terminal 129 comprises a first area 129a, which is located inside the housing 122 and is electrically connected to the second anode terminal element 162b, and a second area 129b, which is located outside the housing 122 and forms a mounting surface 203. It is understood that not the entirety of such areas need be located inside or outside the housing.
[0075] In the illustrated embodiment, a first conductive trace 127c extends in the outer wall 123 of the housing to connect the first region 127a and the second region 127b. Similarly, a second conductive trace 129c extends in the outer wall 123 of the housing to connect the first region 127a and the second region 127b. The conductive traces and / or termination regions can be separate or integrated. In addition to extending through the outer wall of the housing, the conductive traces can also be arranged at other locations, for example, outside the outer wall. Of course, the present invention is by no means limited to the use of conductive traces to form the desired terminations. Regardless of the specific configuration, the connection of the first and second terminals 127 and 129 to the capacitor element 120 can be made using any known technique, e.g., by welding, laser welding, conductive adhesives, etc.In a particular embodiment, for example, a first conductive adhesive 131a can be used to connect the second section 165a of the first anode connection element 162 to the first anode connection 127. Similarly, a second conductive adhesive 131b can be used to connect the second section 165b of the second anode connection element 162b to the second anode connection 129. The conductive adhesives can be formed from conductive metal particles contained in a resin composition. The metal particles can be silver, copper, gold, platinum, nickel, zinc, bismuth, etc. The resin composition can contain a thermosetting resin (e.g., epoxy resin), a curing agent (e.g., acid anhydride), and an adhesion promoter (e.g., silane adhesion promoter). Suitable conductive adhesives are described in US patent application no. 2006 / 0038304 by Osako, et al.
[0076] The cathode of the capacitor element 120 is also connected to a cathode terminal 305, which forms a mounting surface 309. In one embodiment, for example, one or more conductive traces (e.g., conductive traces 307) can extend in the outer wall 123 of the housing to connect a base surface of the capacitor element 120 to the cathode terminal 305. Besides extending through the outer wall of the housing, the conductive traces can also be arranged at other locations, for example, outside the outer wall. Of course, the present invention is by no means limited to the use of conductive traces to form the desired connections. Regardless of the specific configuration, the connection of the cathode terminal 305 to the capacitor element 120 can be made using any known technique, e.g., by welding, laser welding, conductive adhesives, etc.In a particular embodiment, for example, a conductive adhesive 131c, as described above, can be used to connect the underside of the capacitor element 120 to the cathode terminal 305. It is understood that, instead of a direct connection as described above, a cathode connecting element, similar to the anode connecting elements mentioned above, can also be used to facilitate the connection of the capacitor element 120 to the cathode terminal 305.
[0077] Optionally, a polymer retainer can also be arranged in contact with one or more surfaces of the capacitor element, such as the rear surface, the front surface, the top surface, the bottom surface, the side surface(s), or any combination thereof. The polymer retainer can reduce the likelihood of the capacitor element detaching from the housing. In this respect, the polymer retainer can possess a degree of rigidity that allows it to hold the capacitor element in a relatively secure position, even when subjected to vibration, but without being so strong as to cause it to crack.For example, the bracket may have a tensile strength of approximately 1 to approximately 150 megapascals (“MPa”), in some embodiments of approximately 2 to approximately 100 MPa, in some embodiments of approximately 10 to approximately 80 MPa, and in some embodiments of approximately 20 to approximately 70 MPa, measured at a temperature of approximately 25 °C. It is usually desirable that the bracket be non-electrically conductive.
[0078] Although a variety of materials exhibiting the desired strength properties mentioned above can be used, thermosetting resins have proven particularly suitable for use in the present invention. Examples of such resins include, for example, epoxy resins, polyimides, melamine resins, urea-formaldehyde resins, polyurethanes, silicone polymers, phenolic resins, etc. In certain embodiments, the retaining device may, for example, contain one or more polyorganosiloxanes. The silicon-bonded organic groups used in these polymers may include monovalent hydrocarbons and / or monovalent halogenated hydrocarbon groups. Such monovalent groups typically have 1 to about 20 carbon atoms, preferably 1 to 10 carbon atoms, and are, for example, but not exclusively, alkyl (e.g., methyl, ethyl, propyl, pentyl, octyl, undecyl, and octadecyl); cycloalkyl (e.g., cyclohexyl); alkenyl (e.g.,Vinyl, allyl, butenyl, and hexenyl; aryl (e.g., phenyl, tolyl, xylyl, benzyl, and 2-phenylethyl); and halogenated hydrocarbon groups (e.g., 3,3,3-trifluoropropyl, 3-chloropropyl, and dichlorophenyl). Typically, at least 50%, preferably at least 80%, of the organic groups are methyl groups. Examples of such methyl polysiloxanes are, for example, polydimethylsiloxane (“PDMS”), polymethylhydrogensiloxane, etc. Other suitable methyl polysiloxanes are dimethylidiphenylpolysiloxane, dimethyl / methylphenylpolysiloxane, polymethylphenylsiloxane, methylphenyl / dimethylsiloxane, polydimethylsiloxane with vinyldimethyl end groups, vinylmethyl / dimethylpolysiloxane, vinylmethyl / dimethylpolysiloxane with vinyldimethyl end groups, polydimethylsiloxane with divinylmethyl end groups, polydimethylsiloxane with vinylphenylmethyl end groups, polydimethylsiloxane with dimethylhydro end groups, methylhydro / dimethylpolysiloxane, methyloctylpolysiloxane with methylhydro end groups, methylhydro / phenylmethyl polysiloxane, etc.
[0079] The organopolysiloxane may also contain an additional polar functional side and / or end group, such as hydroxyl, epoxy, carboxyl, amino, alkoxy, methacrylic, or mercapto groups, which impart a degree of hydrophilicity to the polymer. For example, the organopolysiloxane may contain at least one hydroxyl group and, optionally, an average of at least two silicon-bonded hydroxyl groups (silanol groups) per molecule. Examples of such organopolysiloxanes include dihydroxypolydimethylsiloxane, hydroxytrimethylsiloxypolydimethylsiloxane, etc. Further examples of hydroxyl-modified organopolysiloxanes are described in US Patent Application No. 2003 / 0105207 by Kleyer et al., which is incorporated herein by reference in full for use in all contexts. Alkoxy-modified organopolysiloxanes may also be used, e.g.,Dimethoxypolydimethylsiloxane, methoxytrimethylsiloxypolydimethylsiloxane, diethoxypolydimethylsiloxane, ethoxytrimethylsiloxypolydimethylsiloxane, etc. Other suitable organopolysiloxanes are those modified with at least one amino-functional group. Examples of such amino-functional polysiloxanes are, for example, diamino-functional polydimethylsiloxanes. Various other suitable polar functional groups for organopolysiloxanes are also described in US patent application No. 2010 / 00234517 to Plantenberg et al., which is incorporated herein in its entirety by reference for all purposes.
[0080] Epoxy resins are also particularly well suited for use as a polymeric retention system. Suitable epoxy resins include, for example, glycidyl ether-type epoxy resins, such as bisphenol-A-type epoxy resins, bisphenol-F-type epoxy resins, phenol-novolac-type epoxy resins, orthocresol-novolac-type epoxy resins, brominated epoxy resins and biphenyl-type epoxy resins, cyclic aliphatic epoxy resins, glycidyl ester-type epoxy resins, glycidylamine-type epoxy resins, cresol-novolac-type epoxy resins, naphthalene-type epoxy resins, phenol-aralkyl-type epoxy resins, cyclopentadiene-type epoxy resins, heterocyclic epoxy resins, etc. Further suitable conductive adhesive resins are described in US Patent Application No. 2006 / 0038304 by Osako et al. and described in US patent application No. 7,554,793 by Chacko, which are incorporated in full into this document for all purposes.
[0081] If desired, curing agents can also be used in the polymeric binder to promote curing. These curing agents typically make up approximately 0.1 to 20% by weight of the substrate material. Examples of curing agents include amines, peroxides, anhydrides, phenolic compounds, silanes, acid anhydride compounds, and combinations thereof. Specific examples of suitable curing agents include dicyandiamide, 1-(2-cyanoethyl)-2-ethyl-4-methylimidazole, 1-benzyl-2-methylimidazole, ethylcyano-propylimidazole, 2-methylimidazole, 2-phenylimidazole, 2-ethyl-4-methylimidazole, 2-undecylimidazole, 1-cyanoethyl-2-methylimidazole, 2,4-dicyano-6,2-methylimidazolyl-(1)-ethyl-s-triazine and 2,4-dicyano-6,2-undecylimidazolyl-(1)-ethyl-s-triazine, imidazolium salts (such as 1-cyanoethyl-2-undecylimidazolium trimellitate, 2-methylimidazolium isocyanurate, 2-ethyl-4-methylimidazolium tetraphenylborate, and 2-Ethyl-1,4-Dimethylimidazolium Tetraphenylborate, etc.Other useful hardening agents include phosphine compounds such as tributylphosphine, triphenylphosphine, tris(dimethoxyphenyl)phosphine, tris(hydroxypropyl)phosphine, and tris(cyanoethyl)phosphine; phosphonium salts such as tetraphenylphosphonium tetraphenylborate, methyltributylphosphonium tetraphenylborate, and methyltricyanoethylphosphonium tetraphenylborate; amines such as 2,4,6-tris(dimethylaminomethyl)phenol, benzylmethylamine, tetramethylbutylguanidine, N-methylpiperazine, and 2-dimethylamino-1-pyrroline; ammonium salts such as triethylammonium tetraphenylborate; and diazabicyclo compounds such as 1,5-diazabicyclo[5,4,0]-7-undecene, 1,5-diazabicyclo[4,3,0]-5-nonene, and 1,4-diazabicyclo[2,2,2]-octane. Salts of diazabicyclo compounds, such as tetraphenylborate, phenol salt, phenol novolac salt and 2-ethylhexanoic acid salt; and so on.
[0082] Other additives can also be used, such as photoinitiators, viscosity modifiers, suspension aids, pigments, stress-reducing agents, coupling agents (e.g., silane coupling agents), non-conductive fillers (e.g., clay, silica, aluminum oxide, etc.), stabilizers, etc. Suitable photoinitiators include, for example, benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin n-propyl ether, benzoin isobutyl ether, 2,2-dihydroxy-2-phenylacetophenone, 2,2-dimethoxy-2-phenylacetophenone, 2,2-diethoxy-2-phenylacetophenone, 2,2-diethoxyacetophenone, benzophenone, 4,4-bisdialylaminobenzophenone, 4-dimethylaminobenzoic acid, alkyl-4-dimethylaminobenzoate, 2-ethylanthraquinone, xanthone, thioxanthone, 2-colorothioxanthone, etc. When additives are used, they usually make up about 0.1 to 20% by weight of the total composition.
[0083] In one embodiment, for example, a single polymer holder can be arranged in contact with a top and a rear surface of the capacitor element. It is understood that separate holders can also be used to perform the same function. Generally, any number of polymer holders can be used to contact any desired surface of the capacitor element. When multiple holders are used, they can be in contact with each other or remain spatially separated. In one embodiment, for example, a second polymer holder can be used that contacts the top and the front surfaces of the capacitor element. The first polymer holder and the second polymer holder can be in contact with each other or not.In another embodiment, a polymeric support can also contact a lower surface and / or side surface(s) of the capacitor element, either in conjunction with or instead of other surfaces. When used, it is typically desirable for the polymeric support to also be in contact with at least one surface of the housing to mechanically stabilize the capacitor element against potential delamination. For example, the support can be in contact with an inner surface of one or more side walls, an outer wall, a cover, etc.
[0084] Once the connection is established as desired, the resulting enclosure can be hermetically sealed as described above. Referring again to the Fig.2-3 The housing 122 can, for example, also include a cover 125, which is placed on an upper surface of the side walls 124 after the capacitor element 120 has been positioned in the housing 122. The cover 125 can be made of ceramic, metal (e.g., iron, copper, nickel, cobalt, etc., and their alloys), plastic, etc. If desired, a sealing element 187 can be arranged between the cover 125 and the side walls 124 to ensure a good seal. In one embodiment, the sealing element can, for example, comprise a glass-to-metal gasket, a Kovar® ring (Goodfellow Cambridge, Ltd.), etc. The height of the side walls 124 is generally dimensioned such that the cover 125 does not touch any surface of the capacitor element 120, thus preventing it from becoming contaminated. In the desired position, the lid 125 is joined to the side walls 124 by known techniques such as welding (e.g. resistance welding, laser welding, etc.), soldering, etc.Hermetically sealed. The hermetic sealing can optionally take place in the presence of a gaseous atmosphere, as mentioned above, so that the resulting condenser is essentially free of reactive gases, such as water vapor.
[0085] Of course, the embodiments described above are only examples of how the capacitor element can be installed in a housing. Other possible housing configurations can be used in the present invention. For example, a capacitor can be formed that is similar to the embodiment described above, except that terminal pins are used as the external connections for the anode and cathode, respectively. In other words, a first terminal pin can extend through a conductive track formed in the outer wall and is connected to the first anode terminal using known techniques (e.g., welding). Likewise, a second terminal pin can extend through a conductive track formed in the outer wall and is connected to the cathode via a conductive adhesive 133, as described above. The Fig.The embodiments shown here are discussed only in relation to a single capacitor element. It goes without saying, however, that multiple capacitor elements can also be hermetically sealed in a housing. The multiple capacitor elements can be attached to the housing using a variety of different techniques.
[0086] For a better understanding of the present invention, reference is made to the following example. Test procedure S parameters
[0087] The parameters S 11 and S 21 can be measured over a wide range of frequencies using a vector network analyzer. The parameter can also be measured using the one in Fig. The equivalent circuit diagram shown can be modeled. Equivalent Series Resistance (ESR)
[0088] The equivalent series resistance (ESR) can be measured using an HP4284A LCR meter with Kelvin leads, 0 V DC bias, and 10 mVAC signals. The operating frequency was 100 kHz and the temperature was 23 °C ± 2 °C. The ESR value can be measured across the cathode terminal and one or more anode terminals. If multiple anode terminals are used, an average ESR value can be determined. Dissipation factor
[0089] The loss factor can be measured with an LCZHP4284A LCR meter using Kelvin leads with 0-volt DC bias and 10 mVAC signals. The operating frequency can be 120 Hz and the temperature can be 23 °C to 2 °C. capacity
[0090] The capacitance can be measured using a Keithley 3330 precision LCZ meter with Kelvin leads, a 2.2 V DC bias, and a 0.5 V peak-to-peak sine wave. The operating frequency can be 120 Hz and the temperature can be 23 °C ± 2 °C. Leakage current
[0091] The leakage current can be measured with a leakage current meter (YHP4140B) at a temperature of 23 °C, with a 1 kOhm resistor to limit the charging current and at the nominal voltage (e.g. 2.5 V) after at least 5 minutes. EXAMPLE
[0092] 40,000 µFV / g tantalum powder was used to prepare anode samples. Each anode sample was heated to a density of 6.0 g / cm³. 3The pellets were pressed. The resulting pellets measured 2.90 x 2.56 x 1.27 mm. The pellets were sintered at 1275 °C, and then a first and second tantalum wire were welded to opposite ends of the pellet. After lead welding, the pellets were deoxidized at 860 °C and re-sintered at 1300 °C. To form the dielectric layer, the pellets were anodized in a water / phosphoric acid electrolyte at 40 °C with 76 volts. After anodizing, four pre-coatings of an organometallic compound containing a solution of (3-aminopropyl)trimethoxysilane in 1.0% ethanol were applied. Subsequently, a conductive polymer coating was formed by immersing the anode in a solution of poly(4-(2,3-dihydrothieno-[3,4-b][1,4]dioxin-2-ylmethoxy)-1-butanesulfonic acid with a solids content of 2.0% (Clevios™ K, Heraeus).After coating, the parts were dried at 125°C for 15 minutes. This process was repeated twice. Then, the parts were immersed in a dispersed poly(3,4-ethylenedioxythiophene) with a solids content of 1.1% and a viscosity of 20 mPa·s (Clevios™ K, Heraeus). After coating, the parts were dried at 125°C for 15 minutes. This process was repeated eight times. Then, the parts were immersed in a dispersed poly(3,4-ethylenedioxythiophene) with a solids content of 2.0% and a viscosity of 20 mPa·s (Clevios™ K, Heraeus). After coating, the parts were dried at 125°C for 20 minutes. This process was repeated three times. The parts were then immersed in a dispersed poly(3,4-ethylenedioxythiophene) with a solids content of 2.0% and a viscosity of 160 mPa·s (Clevios™ K, Heraeus). After coating, the parts were dried for 20 minutes at 125 °C.This process was repeated 14 times. The parts were then coated with a graphite dispersion and dried. Next, the parts were coated with a silver dispersion and dried. Finally, the parts were treated with the substances described here and in [reference missing]. Fig. The connections shown are mounted onto the substrate.
[0093] Several (10) 22mF / 35V capacitors were fabricated in this manner and hermetically encapsulated in a ceramic housing, as described here. The resulting capacitors were then tested for various electrical properties. The results are listed in the table below. Example Capacitance (µF) 24,0 Dissipation factor (%) 4,1 ESR 1* (mOhm) 128,6 ESR 2 † (mOhm) 129,4 Average ESR (mOhm) 129,0 Leakage current (µA) 32,9
[0094] These and other modifications and variations of the present invention can be carried out by those skilled in the art without departing from the spirit and scope of the present invention. Furthermore, it should be understood that aspects of the various embodiments can be exchanged, either in whole or in part. Moreover, those skilled in the art will understand that the foregoing description is only exemplary and is not intended to limit the invention as further described in the appended claims. * A measured portion that is in contact with the first anode terminal and the cathode terminal. † A measured portion that is in contact with the second anode terminal and the cathode terminal. QUOTES INCLUDED IN THE DESCRIPTION
[0000] This list of documents cited by the applicant was automatically generated and is included solely for the reader's convenience. The list is not part of the German patent or utility model application. The DPMA accepts no liability for any errors or omissions. Cited patent literature
[0000] US 63 / 491,551
[0001] WO 2014 / 199480
[0016] US 5,111,327
[0037] US 2007 / 0064376
[0059] US 6,674,635
[0065] US 2006 / 0038304 [0075, 0080] US 2003 / 0105207
[0079] US 2010 / 00234517
[0079] US 7,554,793
[0080] Cited non-patent literature
[0000] ASTM E337-02, Method A (2007
[0009] US Patent No. 6,197,252 by Bishop
[0021] Critical Oxygen Content In Porous Anodes Of Solid Tantalum Capacitors“, Pozdeev-Freeman et al: Materials In Electronics 9, (1998) 309-311
[0022] Journal of Electroanalytical Chemistry, 443, 217 bis 226 (1998
[0047]
Claims
[1] A capacitor comprising: a capacitor element comprising a sintered anode body, a dielectric lying over the anode body, and a solid electrolyte lying over the dielectric, wherein the solid electrolyte contains a conductive polymer, wherein the capacitor element defines a first and a second end opposite each other, and a top and a bottom opposite each other, wherein a first exposed anode conduction section extends from the first end of the capacitor element in a lateral direction, and a second exposed anode conduction section extends from the second end of the capacitor element in a lateral direction; a housing defining an inner cavity in which the capacitor element is arranged and hermetically sealed, wherein the first exposed anode conduction section and the second exposed anode conduction section are arranged within the inner cavity; a first anode terminal which is in electrical contact with the first exposed anode conductor section; a second anode terminal which is in electrical connection with the second exposed anode conductor section; and a cathode connection that is in electrical contact with the solid electrolyte. [2] Capacitor according to claim 1, wherein the anode body contains tantalum and the dielectric contains tantalum pentoxide. [3] Capacitor according to claim 1, wherein the solid electrolyte contains at least one layer formed from a dispersion of conductive polymer particles. [4] Capacitor according to claim 1, wherein the conductive polymer contains poly(3,4-ethylenedioxythiophene) or a derivative thereof. [5] Capacitor according to claim 1, wherein the anode body is formed from a valve metal powder having a specific charge of about 5,000 to about 100,000 µF*V / g. [6] Capacitor according to claim 1, wherein the anode body is formed from a valve metal powder having a specific charge of about 100,000 to about 600,000 µF*V / g. [7] Capacitor according to claim 1, wherein a first anode conductor is embedded in the anode body, which comprises the first exposed anode conductor section and an embedded section. [8] Solid electrolytic capacitor according to claim 7, further comprising a second anode conductor containing the second exposed anode conductor section. [9] Solid electrolytic capacitor according to claim 8, wherein the second anode conductor is connected to one end of the anode body. [10] Capacitor according to claim 9, wherein there is a gap between one end of the embedded part and the end of the anode body. [11] Capacitor according to claim 10, wherein the second anode conductor is embedded in the anode body and has an embedded section. [12] Capacitor according to claim 11, wherein there is a gap between one end of the embedded section of the first anode line and one end of the embedded section of the second anode line. [13] Capacitor according to claim 1, wherein a continuous anode conductor extends through the first end and the second end of the capacitor element and thereby defines the first exposed anode conductor section and the second exposed anode conductor section. [14] The capacitor according to claim 1, wherein the housing is made of a metal, plastic, ceramic or a combination thereof. [15] The capacitor according to claim 1 further comprises a first anode conductor connecting element, which includes a first section which is generally arranged perpendicular to the lateral direction of the first exposed anode conductor section and connected to it. [16] Capacitor according to claim 15, wherein the first anode conductor connecting element further comprises a second section which generally extends parallel to the lateral direction in which the first exposed anode conductor section extends. [17] Capacitor according to claim 16, wherein the second section of the first anode conductor connecting element is arranged inside the housing. [18] Capacitor according to claim 15, wherein the first anode terminal comprises a first area which is arranged inside the housing and is electrically connected to the first anode terminal element, and a second area which is arranged outside the housing and forms a mounting surface. [19] Capacitor according to claim 18, wherein a first conductor extends in an outer wall of the housing to connect the first area and the second area of the first anode terminal. [20] Capacitor according to claim 15, further comprising a second anode conductor connecting element comprising a first section which is generally arranged perpendicular to the lateral direction of the second exposed anode conductor section and connected to it. [21] Capacitor according to claim 20, wherein the second anode conductor connecting element further comprises a second section which generally extends parallel to the lateral direction in which the second exposed anode conductor section extends. [22] Capacitor according to claim 21, wherein the second section of the second anode conductor connecting element is arranged inside the housing. [23] Capacitor according to claim 20, wherein the second anode terminal comprises a first area which is arranged inside the housing and electrically connected to the second anode terminal element, and a second area which is arranged outside the housing and forms a mounting surface. [24] Capacitor according to claim 23, wherein a second conductor extends in an outer wall of the housing to connect the first area and the second area of the second anode terminal. [25] Capacitor according to claim 1, wherein a conductor track extends in an outer wall of the housing to connect the lower surface of the capacitor element to the cathode terminal.
Citation Information
Patent Citations
2007/0064376
US-PATENTANMELDUNGNR.2003/0105207
US-PATENTANMELDUNGNR.2006/0038304
US-PATENTANMELDUNGNR.2010/00234517
US-PATENTANMELDUNGNR.7.554.793