COATING PROCESS
Patent Information
- Application Number
- DE502015016968
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2015-09-03
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2035-09-03
AI Technical Summary
Existing coating systems for producing thin layers, such as diamond films, face challenges with plasma stabilization, leading to inferior material deposition at the beginning of the process, which cannot be easily removed without damaging the layer, especially in layer systems with multiple compositions where interfaces become inaccessible.
A coating system with a displaceable substrate holder that allows the substrate to be moved from a rest position to a working position only when plasma conditions are stable, ensuring high-quality deposition by avoiding initial inferior material growth, and featuring a shielding element to maintain plasma stability and focus microwave radiation for uniform plasma formation.
Enables the production of high-quality thin layers and layer systems by stabilizing plasma conditions before deposition, preventing initial inferior material growth and allowing precise control over layer thickness and composition, even for homoepitaxial diamond layers.
Description
[0001] The invention relates to a method for coating a substrate, in which the substrate is introduced into an evacuable recipient by means of a substrate holder, at least one gaseous precursor is introduced into the recipient by means of at least one gas supply device, and the precursor is at least partially ionized by means of at least one plasma generation device. Devices and methods of the type mentioned above can be used, for example, for the epitaxial deposition of thin layers from the gas phase.
[0002] EP 0 822 572 A1 discloses a high-frequency wave device and method that provides a relatively high concentration of reactive species from a plasma. The plasma is used to treat a surface, in particular a substrate (31) with a complex geometry in a holder (62) that masks part of the substrate. The high-frequency waves are preferably microwaves or UHF waves.
[0003] US Pat. No. 5,479,875 discloses a method for producing a highly oriented diamond film with reduced thickness. The surface of a single-crystal substrate is cleaned and then left in a high vacuum of 10 -6 Torr or less at a temperature between room temperature and 800°C for 15 minutes to release gas molecules absorbed on the substrate surface. The substrate surface is then processed using a carbon-containing plasma.
[0004] US 2003 / 084839 A1 discloses an apparatus for producing diamond in a deposition chamber having a heat sink holder for holding a diamond and for establishing thermal contact with a side surface of the diamond. The method for producing diamond comprises positioning diamond in a holder such that thermal contact is established with a side surface of the diamond adjacent to an edge of a growth surface of the diamond. Single-crystal diamond can then be produced by microwave plasma chemical vapor deposition on the growth surface, with a diamond growth rate greater than 1 micrometer per hour.
[0005] A plasma processing apparatus is known from US 2011 / 092073 A1. It includes an evacuable processing vessel; a gas introduction unit that introduces a process gas into the interior of the processing vessel; a microwave introduction unit that introduces a microwave into the interior of the processing vessel; and a lifting pin that is inserted up and down by a placement platform provided inside the processing vessel, wherein one end surface of the lifting pin supports an object to be processed.
[0006] US 5,704,976 A discloses a process for the low-pressure synthesis of diamond in which the distance between the plasma cloud and the substrate surface can be changed.
[0007] DE 195 07 077 C1 discloses a device and method of the type mentioned above. This known coating system comprises a cavity resonator configured to focus microwave radiation onto a spatial region adjacent to the substrate surface. Gaseous precursors are introduced into this spatial region and are ionized by the microwave radiation. Single-crystal diamond layers can be deposited on the substrate from the resulting plasma.
[0008] However, this known coating system has the disadvantage that the plasma only stabilizes after an extended period of operation. This leads to lower-quality material being deposited at the beginning of the layer deposition. For example, at the beginning of the deposition of crystalline diamond, graphitic carbon phases may also be present in the growing layer. During the deposition of comparatively thick layers, the initially growing low-quality material can be easily removed, for example, by grinding or etching. In some embodiments, a small proportion of inferior material at the interface can also be tolerated if it does not adversely affect the intended use of the produced coating.
[0009] However, the production of very thin layers is problematic. These contain a very high percentage of low-quality material. This material cannot be removed without severely weakening or damaging the entire grown layer. In a layer system consisting of several thin layers of different compositions, the interfaces may become inaccessible after the individual layers have been produced, making subsequent removal of the material initially deposited with a different composition or crystal structure impossible.
[0010] Based on the prior art, the invention is therefore based on the object of specifying a coating method which can also be used for the production of high-quality thin layers or layer systems.
[0011] The object is achieved according to the invention by a method according to claim 1. Advantageous developments of the invention can be found in the subclaims.
[0012] According to the invention, a coating system is used which has at least one evacuable recipient. In some embodiments, the recipient can be made of stainless steel or an aluminum alloy. In some embodiments of the invention, the wall of the recipient consists at least partially of glass or ceramic and is thus at least partially permeable to electromagnetic radiation. The recipient can be evacuated using a known vacuum pump, for example a turbomolecular pump, a cryopump, or a rotary vane pump. Before the start of layer deposition, the residual gas pressure in the recipient can be less than 1 10 -6 < mbar, less than 1 10 -7 < mbar, or less than 1 10 -8 < mbar.
[0013] Furthermore, the coating system includes at least one substrate holder designed to hold a substrate. The substrate can be positioned on a flat support surface of the substrate holder solely by gravity. In other embodiments of the invention, the substrate can be fixed to the substrate holder by means of a clamp or a screw connection. This prevents accidental displacement of the substrate during movement of the substrate holder or during evacuation of the container.
[0014] The coating system further includes at least one gas supply device, by means of which at least one gaseous precursor can be introduced into the recipient. The precursor contains at least one gas or a gas mixture with layer-forming substances, which are deposited on the substrate during the coating process. For example, the precursor can contain silane to produce a silicon layer. To produce a diamond layer or a layer of diamond-like carbon, the precursor can contain a hydrocarbon, for example, acetylene or methane.
[0015] In addition, the gaseous precursor can contain a carrier gas, such as hydrogen or noble gases. Finally, the precursor can contain dopants, which can be used to adapt the growing coating to specific thermal or electrical properties. The composition of the precursor can change during the coating system's operation to create a layer system consisting of several individual layers. These can merge abruptly or gradually.
[0016] The coating system further comprises at least one plasma generation device. The plasma generation device can generate electromagnetic radiation that is absorbable by the gaseous precursor. Depending on the frequency range of the electromagnetic radiation emitted by the plasma generation device, the plasma can be an RF plasma, a microwave plasma, or an ECR plasma. In some embodiments of the invention, the plasma generation device can have a power of approximately 1 kW to approximately 10 kW or approximately 2 kW to approximately 6 kW.
[0017] According to the invention, it is now proposed that the substrate holder be displaceable within the evacuable recipient, so that it can be moved from a working position to a rest position. In the working position, the substrate arranged on the substrate holder is exposed to the influence of the partially ionized precursor, so that a layer deposition occurs on the substrate. In the rest position, the influence of the ionized precursor is less, so that no layer deposition and, in some embodiments of the invention, no etching of the substrate by the plasma occurs. Thus, the substrate can be stored in the rest position until the plasma in the recipient has stabilized. Only when the desired deposition conditions have been established can the substrate be moved from the rest position to the working position.Once a sufficient layer thickness has been achieved, layer growth can be interrupted by returning the substrate holder to its rest position. This prevents the deposited layers from exhibiting inferior crystal quality or an undesirable composition until the plasma conditions have stabilized. This allows even thin layers to be deposited with high quality.
[0018] In some embodiments of the invention, the layer deposited with the coating method of the invention may have a thickness of about 10 nm to about 1 µm. In other embodiments of the invention, the layer thickness may be between about 20 nm and about 250 nm.
[0019] In some embodiments of the invention, the substrate holder can be axially displaceable. This makes the invention easy to implement using a simple linear drive. The substrate can be positioned with great precision yet with minimal technical effort.
[0020] In some embodiments of the invention, the substrate holder can include a heating device. This allows the substrate to be heated to the desired temperature while in the rest position, which is expected to result in optimal properties of the deposited layer. This prevents unwanted material phases from being deposited initially after transport to the working position until the substrate has been heated by the action of the plasma.
[0021] If the substrate is additionally heated by the plasma in the working position, the heating power of the heating device can be reduced accordingly. A control device, such as a PI controller, a PD controller, or a PID controller, can be used for this purpose. The use of the heating device prevents unwanted phases from being deposited on the substrate at the beginning of the layer deposition at too low a substrate temperature, or prevents the layer quality from deteriorating. The proposed control system prevents the substrate from overheating due to the plasma.
[0022] In some embodiments of the invention, the coating system includes a shielding element having a bore through which the substrate holder can be moved into the working position. The shielding element shapes the electric field at the location of the plasma, so that a substrate holder made of an electrically conductive material, such as a metal or alloy, can be moved from the working position to the rest position and vice versa without disturbing the plasma.
[0023] In some embodiments of the invention, the substrate holder or the substrate can be flush with a side of the shielding element facing the plasma in the working position. This ensures that there are no sharp edges at the transition between the bore of the shielding element and the substrate or substrate holder, which would lead to a field increase that could disrupt plasma formation. Such disturbances can lead to inhomogeneous deposition behavior, so that the desired high layer quality cannot be achieved, or at least not over the entire surface.
[0024] In some embodiments of the invention, the recipient can have the shape of an ellipsoid. This allows the microwave radiation from the plasma generation device to be focused, resulting in a greater plasma density and / or a more uniform plasma in front of the substrate.
[0025] In some embodiments of the invention, the plasma generation device can generate a power of more than 1 kW, or more than 3 kW, or more than 4 kW at the working position. In some embodiments of the invention, the plasma generation device can generate a power of less than about 1 W, or less than 100 mW, or less than about 10 mW at the rest position. This ensures that the plasma neither etches the substrate nor deposits unwanted layers in the rest position over a period of more than about 0.75 h, or more than about 2 h, or more than about 3 h. In the working position, however, a layer can be generated with a deposition rate of more than 100 nm / h, more than 1 µm / h, or more than 3 µm / h.
[0026] In some embodiments of the invention, the heating device can heat the substrate in the rest position to a temperature between about 800°C and about 950°C. At this temperature, for example, high-quality diamond layers can be deposited, so that the growth of the layers begins immediately after the substrate is moved from the rest to the working position.
[0027] In some embodiments of the invention, at least one field mode at the working position can have at least one main maximum whose field strength is higher than the field strengths of neighboring secondary maxima. This makes it possible, on the one hand, to generate a high plasma density at the working position, so that high-quality layers with a correspondingly high deposition rate can be produced. Furthermore, by appropriately focusing the electromagnetic wave, the plasma can be confined to a region that is not or only slightly influenced by the retraction or extension of an electrically conductive substrate holder.
[0028] The device can be used, in particular, to produce homoepitaxial diamond layers. This means that a diamond layer with a predeterminable composition and doping is deposited on an existing diamond layer. The substrate can be placed in a rest position between the deposition of layers of different compositions until the plasma conditions, in particular the temperature, expansion, gas pressure, and gas composition, have stabilized. Only once the desired deposition conditions have been established is the substrate moved from the rest to the working position to deposit another diamond layer homoepitaxially. In this way, for example, semiconductor components based on diamond can be manufactured from differently doped layers.
[0029] The invention will be explained in more detail below with reference to figures without limiting the general inventive concept. The figures show: Figure 1 shows an embodiment of a coating system in which the substrate holder is in the rest position. Figure 2 shows an embodiment of the coating system in which the substrate holder is in the working position. Figure 3 shows an enlarged view of a part of the coating system in the working position. Figure 4 shows an enlarged view of a part of the coating system in the rest position. Figure 5 shows a flowchart of the method according to the invention.
[0030] Based on the Figures 1 and 2An embodiment of the coating system used is explained in more detail. The coating system has a recipient 3, into which a gaseous precursor can be introduced by means of a gas supply device (not shown). The recipient 3 can be evacuated to a background pressure of less than 1-10 -6 mbar. During operation of the coating system 1, the precursor in the recipient 3 can have a pressure of approximately 30 mbar to approximately 250 mbar.
[0031] The gaseous precursor contains at least one layer-forming substance, which is at least partially ionized and thereby decomposed in the plasma during operation of the coating system 1, so that the layer-forming substance is deposited as a coating on the substrate 4. The layer-forming substance can, for example, contain a hydrocarbon, in particular methane or acetylene. The precursor can also contain dopants, for example, nitrogen or boron. The gaseous precursor can be diluted in a carrier gas. Hydrogen, for example, is a suitable carrier gas.
[0032] The wall of the recipient 3 contains a dielectric material that is at least partially permeable to electromagnetic radiation. For example, the wall of the recipient 3 can be made at least partially of glass, quartz, or ceramic.
[0033] The receiver 3 is surrounded by a cavity resonator 10, which has the shape of a rotational ellipsoid. The cavity resonator has two focal points. At the upper focal point is an antenna 2 of a microwave source. At the lower focal point, the plasma 25 forms in the precursor. Figure 1 As shown, the microwave radiation 20 emitted approximately isotropically by the antenna 2 is reflected by the walls of the cavity resonator 10 and focused at the lower focal point. As a result, the microwave radiation arrives at the lower focal point approximately isotropically from all spatial directions, allowing a uniformly dense plasma 25 to form, which is only slightly or not at all influenced by the movement of the substrate holder.
[0034] At the bottom of the chamber 3 is a shielding element 45, which has a bore 46. A substrate holder 40 is arranged below the bore 46. The substrate 4 is located at the front of the substrate holder 40. The substrate holder 40 is movable by means of a linear drive. The substrate can be held by an optional clamp or inserted or removed in the rest position of the substrate holder 40 using an optional load lock.
[0035] In Figure 1The substrate holder 40 is shown in the rest position. This is characterized by the fact that the plasma 25 remains largely confined to the upper part of the recipient 3 by the shielding element 45, so that the plasma 25 does not act on the surface of the substrate 4 or only acts with negligible intensity. Therefore, no coherent layer is deposited from the gas phase on the substrate 4, at least for a period of more than 45 minutes or more than 2 hours.
[0036] In Figure 2 The substrate holder 40 is shown in the working position. This is characterized by the fact that the tip of the substrate holder 40 protrudes through the bore 46 and the substrate 4 lies approximately flush with the shielding element 45. In this position, the surface of the substrate 4 can be approximately flush with the front side 450 of the shielding element 45 facing the plasma.
[0037] In the working position, a layer is deposited from the plasma 25 on the substrate 4. The layer growth can occur at a rate of more than 100 nm / h, more than 1000 nm / h, or more than 2 µm / h. In some embodiments of the invention, the deposition rate of the precursor on the substrate 4 in the working position is increased by more than a factor of 10 4 , more than a factor of 10 6 , or more than a factor of 10 8 compared to the rest position.
[0038] According to the invention, it is now proposed to bring the substrate 4 into the rest position described above, then to introduce the gaseous precursor in the desired composition into the recipient 3, and to form the plasma 25 using the microwave radiation from the plasma generation device. Due to the shielding element 45 and the focusing of the microwave radiation in the cavity resonator 10, the plasma 25 is not influenced, or only slightly influenced, by the bore 46 and the resulting field distortion. The coating system can thus be operated until a stable plasma has formed. In some embodiments of the invention, this can last more than 30 minutes, more than 40 minutes, or more than 60 minutes. During this time, the substrate 4 is not coated by the plasma 25, so that no layer with an undesirable composition or other undesirable layer properties is formed.
[0039] When the plasma 25 burns stably in the recipient 3, the substrate can be brought into the working position so that the layer deposition takes place on the substrate 4.
[0040] Once the layer has been produced with the desired thickness and composition, the substrate 4 can be returned to its rest position to interrupt growth. If a second layer is to be deposited on top of the first layer, the pressure or composition of the precursor, the temperature of the substrate, and / or the microwave power can be adjusted to the new target values. Once the conditions in the recipient 3 have stabilized again, the substrate 4 can be returned to its working position to deposit the second layer.
[0041] Based on the Figures 3 and 4 is shown again an excerpt from the Figures 1 and 2The coating system shown is shown in greater detail. Like reference numerals denote like components of the invention so that the following description can be kept brief.
[0042] Figure 3 shows the substrate 4 in the working position in which a layer deposition takes place. In contrast, Figure 4 the substrate 4 in the rest position, in which the substrate 4 is protected from the action of the plasma 25 by the shielding element 45.
[0043] The plasma 25 forms in a recipient 3, which is made of a material permeable to microwave radiation. For example, the recipient 3 can be made of quartz or glass. The shielding element 4 can be made of a metal or an alloy and can be maintained at a predeterminable potential by means of a voltage source. This potential can be identical to the bias potential selected for the deposition of the layer, so that the plasma 25 continues to burn stably when the substrate holder 40 is moved from the rest position to the working position and back.
[0044] For this purpose, the shielding element 45 can have a bore 46 whose area is small compared to the total area of the shielding element 45. Thus, the shielding element 45 determines the potential in the recipient 3, which is only slightly or not at all influenced by the changing potential conditions on the surface of the bore 46 during the movement of the substrate holder.
[0045] In some embodiments of the invention, the recipient 3 may be omitted. In this case, the cavity resonator 10 can be used as the recipient and completely filled with the precursor.
[0046] Based on the Figure 5The sequence of the coating method according to the invention is explained again. In the first method step 51, the substrate holder 40 is moved to its rest position. In the rest position, a substrate 4 arranged on the substrate holder 40 is, on the one hand, protected from the effects of the plasma 25. On the other hand, a substrate can be removed from the substrate holder or applied to the substrate holder using a manipulator and a lock without ventilating the recipient.
[0047] In the second method step 52, a substrate 4 intended for coating is therefore applied to the substrate holder 40. In some embodiments of the invention, the substrate may contain or consist of a single-crystal diamond. For example, the diamond may have been produced heteroepitaxially on a molybdenum or silicon substrate and subsequently separated from the substrate. In other embodiments of the invention, the diamond may have been produced using an HPHT process. The invention does not teach the use of a specific substrate as a solution principle.
[0048] Once the substrate 4 has been arranged on the substrate holder 40, in the third method step 53, the substrate can be heated to a predeterminable temperature by means of a heating device arranged in the substrate holder 40. In the case of diamond deposition, the temperature can be, for example, between 800°C and approximately 850°C. At the same time, the fourth method step 54 can be carried out. In the fourth method step 54, a gaseous precursor is introduced into the recipient 3. The precursor can contain, for example, hydrogen and methane in order to deposit a nominally undoped diamond layer homoepitaxially on the substrate 4. The individual components of the precursor are introduced into the recipient 3 at predeterminable mass flows, and the microwave radiation of the plasma generation device 2 is activated. This leads to the formation of a plasma 25, which initially burns unstably.This means that the plasma density, temperature and composition are constantly changing, so that no homogeneous layer with the desired properties could be produced.
[0049] Process steps 53 and 54 continue until the plasma 25 burns stably, i.e., the plasma density, plasma composition, and plasma temperature are constant within the range of usual measurement accuracies. Process step 53 is continued until a stable substrate temperature has been established. This can be monitored and controlled by a control device and / or a measuring device (not shown).
[0050] After completion of process steps 53 and 54, which can also be performed sequentially in other embodiments of the invention, the substrate is moved into the working position in the fifth process step 55. The layer is then deposited on the substrate 4. Since the plasma 25 already burns stably and does not have a composition that fluctuates over time, the desired layer grows with high quality right from the start. Even at the transition to the substrate surface, no undesirable phases with a different crystal structure or chemical composition form.
[0051] After the desired layer has been deposited in the desired thickness, the substrate holder 40 is returned to its rest position. This stops the layer deposition instantly. Thus, the device according to the invention allows for very precise control of the layer thickness. Even thin layers can be deposited with high quality, since unstable plasma conditions cannot affect the substrate.
[0052] If a further layer with a different composition or crystal structure is to be created on the layer just created, the fourth process step 54 can be performed again. For example, an additional dopant can now be introduced into the recipient 3. When the plasma burns stably again, the substrate holder 40 is returned to the working position in process step 55. After the layer deposition is complete, the substrate holder is returned to the rest position in the sixth process step 56.
[0053] Process steps 54, 55, and 56 are repeated until the desired layer sequence is deposited. The substrate is then cooled and removed from the coating system.
[0054] Of course, the invention is not limited to the illustrated embodiments. The above description is therefore not to be considered restrictive, but rather explanatory. The following claims are to be understood as meaning that a stated feature is present in at least one embodiment of the invention. This does not exclude the presence of further features. Where the claims and the above description define "first" and "second" embodiments, this designation serves to distinguish between two similar embodiments without establishing a priority. Where the claims and the above description define "first" and "second" features, this designation serves to distinguish between two similar features without establishing a priority.
Claims
1. Method for coating a substrate, in which the substrate (4) is brought into an evacuable recipient (10) by means of a substrate holder (40), at least one gaseous precursor is introduced into the recipient (10) by means of at least one gas supply device and the precursor is at least partially ionized by means of at least one plasma generating device (2), characterized in that the recipient (10) contains a shielding element (45), which has a hole (46), through which the substrate holder is brought into a working position, the plasma (25) being ignited as long as the substrate holder (40) with the substrate (4) is in a rest position and the substrate holder (40) is moved into the working position after a predeterminable period of time.
2. Method according to claim 1, characterized in that, at the working position, the plasma generating device (2) has a power of more than 1 kW or more than 3 kW or more than 4 kW and / or in that, at the rest position, the plasma generating device (2) generates a power of less than 1 W or less than 100 mW or less than 10 mW.
3. Method according to any one of claims 1 to 2, characterized in that the predeterminable time period is between about 10 min and about 60 min or in that the predeterminable time period is between about 30 min and about 45 min.
4. Method according to any one of claims 1 to 3, characterized in that the substrate (4) is brought to a temperature between about 800°C and about 950°C in the rest position.
5. Method according to any one of claims 1 to 4, characterized in that the temperature of the substrate (4) is kept constant at the rest position and at the working position.
6. Method according to any one of claims 1 to 4, characterized in that the plasma generating device (2) contains a microwave transmitter and, at the working position, at least one field mode has at least one main maximum, the field strength of which is higher than the field strengths of adjacent secondary maxima.
7. Method according to any one of claims 1 to 6, characterized in that diamond is deposited on the substrate (4) in the working position.
8. Method according to claim 7, characterized in that the diamond has a thickness from about 10 nm to about 50 nm or from about 20 nm to about 40 nm.
9. Method according to any one of claims 7 or 8, characterized in that the diamond is deposited homoepitaxially.
10. Method according to any one of claims 1 to 9, characterized in that the recipient has the shape of an ellipsoid.
11. Method according to any one of claims 1 to 9, characterized in that the recipient (3) is surrounded by a cavity resonator (10), which has the shape of an ellipsoid.
12. Method according to claim 10 or 11, characterized in that the plasma generating device (2) contains a microwave transmitter and is arranged in a first focal point of the ellipsoid and the substrate (4) is arranged in the working position of the substrate holder (40) in a second focal point of the ellipsoid.
13. Method according to any one of claims 1 to 12, characterized in that the substrate holder (40) with the substrate (4) is axially moved from the rest position to the working position14. Method according to any one of claims 1 to 13, characterized in that, in the working position, the substrate holder (40) or the substrate (4) is flush with one side (450) of the shielding element (45) that faces the plasma.