METHOD FOR MANUFACTURING A SANDWICH COMPONENT, CORE FOR A SANDWICH COMPONENT AND SANDWICH COMPONENT

DE502018015179D1Active Publication Date: 2024-10-17AIRBUS OPERATIONS GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502018015179
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2017-08-17
Filing Date
2018-08-16
Publication Date
2024-10-17
Estimated Expiration
2038-08-16

AI Technical Summary

Technical Problem

Current methods for producing sandwich components are inefficient, requiring separate production steps for cover layers and core layers, which increases processing time and complexity, and lack design flexibility for improved mechanical properties.

Method used

A method involving the direct formation of a closed cover layer on a mold using prepreg tapes or semi-finished fiber products, followed by additive manufacturing to create a core structure integrated with the cover layer, allowing for automated production of sandwich components in a single tool device with enhanced mechanical properties and reduced processing time.

Benefits of technology

This method streamlines the production process, reduces the risk of delamination, and offers improved mechanical strength and design flexibility by integrating the core and cover layers during production, resulting in faster and more precise manufacturing of sandwich components.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a method for producing a sandwich component, a core for a sandwich component and a sandwich component.

[0002] Structural components with a so-called sandwich construction typically have at least one outer, flat cover layer and an adjoining core layer. The core layer is usually a honeycomb structure made of a low-density material. The cover layer is usually a thin, mechanically resistant, flat layer. This achieves a relatively high mechanical strength or rigidity with a low component weight, which is why structural components with sandwich construction are used in a variety of ways, particularly in aircraft and aerospace engineering.

[0003] WO 2015 / 105859 A1 describes a core layer for a sandwich component, which is manufactured from a plurality of open or closed cells using a 3D printing process. Typically, the cover layers of the sandwich component and the core are each manufactured separately and then bonded together, for example, by adhesive bonding.

[0004] DE102012020671A1 describes a method for producing a component using a generative layered construction process. The component is either solid, honeycomb-shaped, or at least has a hollow interior. A cover layer is applied over it.

[0005] EP3034208A1 discloses a method for producing stiffened structures such as anisotropic panels integrating mechanical and thermal functions, as well as the core and the resulting cover layers.

[0006] EP3045300A1 shows a component with a plurality of elementary units arranged in a regular pattern to form a mesoscopic geometric structure using an AM or 3D printing technique. US2008 / 0145597A1 discloses a honeycomb panel with cells comprising at least partially thermoplastic material.

[0007] DE102015105603A1 describes a sandwich panel for an aircraft, comprising two cover layers and a core layer arranged between them. The core layer has pins extending from one cover layer through the core layer to the other.

[0008] One of the objects of the present invention is to provide an improved method, in particular a method for producing a sandwich component that is improved in terms of process speed. A further object of the present invention is to provide an improved core for a sandwich component, in particular a core that simplifies the production of the sandwich component and / or that has improved mechanical properties.

[0009] These problems are solved by the subject matter of the independent claims.

[0010] Advantageous embodiments and further developments arise from the subclaims which refer back to the independent claims in conjunction with the description.

[0011] According to a first aspect of the invention, a method for producing a sandwich component is provided. According to the invention, a first cover layer is formed on a mold surface of a molding tool. In this step, a closed, flat layer is formed. This can be realized, for example, by depositing fiber tapes on the mold surface. So-called prepreg tapes, i.e. tapes made of a fiber material impregnated with a resin or matrix material, are deposited on a tool surface along a deposition direction, for example with the aid of a deposition head. This can comprise the formation of several superimposed layers of fiber tapes, wherein the fiber tapes within a layer preferably have the same fiber orientation and the fiber tapes of an adjacent layer preferably have a fiber orientation that differs from the fiber orientation of the underlying layer.The fiber slivers are optionally deposited in a state in which the matrix material is in a viscous aggregate state, at least on the surface, or the matrix material is converted into a viscous state immediately after deposition by applying heat, for example, using a heating device provided on the deposition head. This melts the individual fiber slivers and, if applicable, the individual layers of fiber slivers. Thus, a monolithic, closed, flatly extending first cover layer is formed. An outer surface of the first cover layer rests against the mold surface of the molding tool. An inner surface of the first cover layer is oriented opposite to the outer surface.

[0012] Alternatively, the first cover layer can also be formed by applying and, if necessary, reshaping a flat, extending fiber semi-finished product to the mold surface of the molding tool. The fiber semi-finished product can, in particular, be designed as a plate- or mat-shaped, flat semi-finished product comprising multiple layers of fiber layers embedded in matrix material. This semi-finished product is pressed against the mold surface of the molding tool in a state in which the matrix material is at least partially in a viscous aggregate state, and thus shaped accordingly. Optionally, the matrix material can be hardened or solidified before the next step of the process is carried out.

[0013] In a further step, a core of the sandwich component is created by building up a cellular structure with a large number of cells in a thickness direction on the first cover layer using an additive manufacturing process. The core is produced using a 3D printing process directly on the inner surface of the first cover layer. In this way, the core is bonded to the first cover layer during its manufacture. This accelerates and simplifies the production of the sandwich component by combining two process steps. Furthermore, 3D printing offers exceptional design freedom and allows, among other things, the production of individually adapted cellular structures with manageable effort, which would be impossible or only possible with considerable effort using conventional methods. An FDM 3D printing process is used to produce the core as an additive manufacturing process.FDM stands for "Fused Deposition Modeling." In this process, the walls forming the cells are created by heating a wire- or ribbon-shaped plastic material to liquefy it and extruding it onto the inner surface of the first cover layer using a nozzle. The plastic material then hardens at the desired position by cooling. The cells are typically constructed by repeatedly moving one work plane at a time and then stacking the work plane upwards, creating the cell structure layer by layer.

[0014] The cell structure is built up from the inner surface of the lower cover layer in a thickness direction. A multitude of individual cells are formed, which can in particular be designed as closed cells with multiple cell walls. The cells can, for example, be designed as convex polyhedra. A polyhedron is called convex if, for any two points of the polyhedron, the connecting line between these points lies entirely within the interior of the polyhedron. For example, cells can be provided in the shape of a cuboid, a hexahedron, an octahedron, a truncated octahedron, a tetrahedron, a double tetrahedron, a polygonal prism, a dodecahedron, an icosahedron, an icosidodecahedron, or the like. The thickness direction runs transversely to the inner surface of the lower cover layer. In particular, a cell structure is formed with a constant or varying thickness across the extent of the inner surface.The cells of the cell structure that are opposite to the thickness direction and located to the outermost form a deposition surface at a distance of the thickness of the cell structure.

[0015] In a further step, a second cover layer of the sandwich component is formed on the deposition surface of the core opposite the first cover layer. The deposition of the second cover layer onto the deposition surface of the core can be carried out in particular using the same device and in the same manner as described for the first cover layer, in particular by depositing fiber ribbons or by applying and optionally reshaping a flat fiber semi-finished product to the deposition surface. By forming the second cover layer directly on the core, it is already bonded to the core during deposition. This eliminates an additional process step and further accelerates the process. Furthermore, when deposited onto the deposition surface of the core, the second cover layer adapts to the surface contour of the deposition surface.In this way, a close, surface contact is achieved between the core and the second cover layer, which reduces the risk of delamination between the cover layer and the core.

[0016] The method according to the invention thus enables a sandwich component to be produced particularly quickly in a single tool device, in particular at a single workstation. The first cover layer can be produced in an automated manner by depositing fiber ribbons or by forming, in particular thermoforming, on a tool surface. For this purpose, an automated deposition device, such as a deposition head or an end effector, can be used. By producing the core directly on the first cover layer using an additive manufacturing process, a great deal of design freedom is enabled with regard to the core, while complex tools can be dispensed with. Since 3D printing devices operate based on data models, manual work steps such as manual alignment of the core or similar, which are often necessary with conventional processes, can be dispensed with.Furthermore, by producing the core directly on the first cover layer, alignment errors are avoided, thus improving the quality of the sandwich component. The second cover layer can also be produced in an automated manner, similar to the first cover layer. By doing this directly on the core, a high degree of precision is achieved in the positioning of the cover layer. With the method according to the invention, the sandwich component can thus be produced in a type of integral process or integrated process, in which all work steps are automated and can be carried out at a single workstation. This shortens or eliminates transport routes for the individual components and waiting times between process steps, thus reducing the overall production time.

[0017] According to one embodiment of the method, the fiber ribbons for forming the first cover layer and / or the second cover layer or the semi-finished fiber product for forming the first cover layer and / or the second cover layer each comprise a thermoplastic matrix material, for example polyphenylene sulfide, PPS for short, polyetheretherketone, PEEK for short, or a similar thermoplastic material. In particular, fiber ribbons or semi-finished fiber products based on thermoplastics are used to produce the cover layers. This offers the particular advantage that the matrix material can be easily melted by applying heat and no additional heat treatment is necessary to cure the matrix material. In particular, this eliminates the need for treating the cover layers in an autoclave, which further accelerates the process.

[0018] According to one embodiment, the cell structure of the core is constructed from a thermoplastic material. Thermoplastic materials such as polycarbonate (PC for short), polyetherimide (PEI for short), or similar thermoplastics are particularly suitable. Particularly advantageously, the matrix material of the first and second cover layers, as well as the material of the core, can each be constructed from a thermoplastic material. This achieves a particularly reliable and mechanically resistant connection between the core and cover layers.

[0019] According to one embodiment of the method, the cell structure of the core is formed with a deposition edge region located opposite the first cover layer in relation to the thickness direction, which edge region has a higher volume-related cell density than an adjacent inner region of the cell structure in the thickness direction. A cross-sectional region is therefore created at the edge of the cell structure, which forms the deposition surface. In this cross-sectional region, there are therefore more cells within a given volume than within the same volume in an adjacent inner region of the cross section in relation to the thickness direction. In this way, any openings in the deposition surface that may be present and are delimited by cell walls are reduced in size. This provides better support for the fiber ribbons when they are deposited on the deposition surface of the core, reliably preventing dents.Furthermore, the contact surface between the core and the second cover layer is increased, improving adhesion between these layers. A further advantage of this design is that the mechanical stiffness, particularly the bending resistance of the core, is increased.

[0020] According to a further embodiment, the cells located opposite the first cover layer with respect to the thickness direction and forming the deposition surface can be formed such that a longitudinal extent of the cells runs along a deposition direction in which the fiber ribbons are laid down with their fiber longitudinal direction. According to this embodiment, the outermost cells with respect to the thickness direction are formed such that the fibers of the fiber ribbon, when laid down on the deposition surface of the core in a specific direction, extend along the longitudinal extent of openings in the deposition surface defined by cell walls. If, for example, rectangular openings are formed in the deposition surface by cell walls of the cells, the cell walls are aligned such that when the fiber ribbons are laid down, the fibers run along the long side of the rectangular opening.This alignment offers the advantage that hardly any matrix material located between the fibers sags into the opening, which reliably prevents dents in the cover layer.

[0021] According to a further embodiment, the cells located opposite the first cover layer in relation to the thickness direction and forming the deposition surface are filled with a filler material. In this way, openings in the deposition surface defined by cell walls are completely closed. This provides a particularly large contact surface for the second cover layer, resulting in extremely reliable adhesion between the cover layer and the core. Furthermore, dents in the cover layer are avoided. Furthermore, this also reduces the risk of water or liquids in general penetrating the core layer.

[0022] Filling the cells to form the storage surface can be achieved, in particular, using the additive manufacturing process during the construction of the cell structure. In this case, the outermost cells in terms of thickness are formed directly as filled, solid cells during their construction. Alternatively, the cells can also be subsequently filled with a filler material, for example, the material from which the cells themselves are formed or a foam material.

[0023] According to a further embodiment, it can be provided that the cell structure of the core is formed with a contact edge region that directly adjoins the first cover layer in relation to the thickness direction and has a higher volume-related cell density than an inner region of the cell structure that adjoins it in the thickness direction. It can also be provided that in this contact edge region, the cells of the cell structure that are in direct contact with the first cover layer are filled with a filler material. These optional designs improve the adhesion between the first cover layer and the core as well as the mechanical resistance of the core. Furthermore, if the cells are filled, the penetration of liquid into the interior of the cell structure is reliably prevented.

[0024] According to a further embodiment of the method, the cell structure of the core can be constructed in such a way that regions are formed which have a higher volume-related cell density than adjacent regions in order to increase the mechanical strength of the core. Accordingly, cross-sectional regions in which high mechanical loading of the core is to be expected can be formed with smaller cells than other cross-sectional regions in which low mechanical loading of the core is to be expected. In this way, a one-piece core can be advantageously produced with little effort, low weight and high mechanical strength. Cross-sectional regions in which high mechanical loading of the core is to be expected can, in particular, be regions which are intended for the attachment of connecting or fastening devices such as screws, rivets, bolts or the like.Areas in which local inserts are to be embedded can also be areas subject to high mechanical stress.

[0025] Alternatively, to increase the mechanical strength of the core, the cell structure of the core can be constructed in such a way that regions are formed in which the cells are formed with cell walls made of a material that has greater mechanical strength than the cell walls of the cells in neighboring regions. In this case, in cross-sectional regions where high mechanical stress on the core is expected, the cell walls are formed of a more resistant or stable material than other cross-sectional regions where low mechanical stress on the core is expected. This offers the advantage that the individual cells can each be constructed with identical geometry, which simplifies the effort required for modeling the core and controlling the 3D printing device used to build the core.

[0026] According to a further alternative, in order to increase the mechanical strength of the core, the cell structure of the core can be constructed in such a way that regions are formed in which the cell walls of the cells have a greater wall thickness than the cell walls of the cells in adjacent regions.

[0027] According to a further alternative, in order to increase the mechanical strength of the core, the cell structure of the core can be constructed in such a way that regions are formed in which the cells are filled with a filling material.

[0028] According to a further embodiment of the method, a surface inspection to detect surface defects is carried out during the formation of the first cover layer and / or during the production of the core and / or during the formation of the second cover layer. Thus, an examination of the quality of the respective layer of fiber slivers produced can already take place during the deposition of the cover layers. This can be achieved, for example, using an optical or acoustic method. In particular, a camera or an ultrasonic sensor can be attached to a deposition head that deposits the fiber slivers in order to detect surface defects or foreign bodies. The surface of the respective applied material layer of the core can also be optically or acoustically examined for defects during the production of the core.Carrying out the respective inspection simultaneously with the production of the respective component of the sandwich component further shortens the manufacturing process.

[0029] Alternatively or additionally, after the formation of the second cover layer, the sandwich component can be examined non-destructively for component defects, such as delamination of the cover layers, defects, or inclusions of foreign bodies in the cover layers and in the core. For this purpose, the sandwich component can be examined using X-rays, for example.

[0030] According to a further aspect of the invention, a sandwich component is provided which is manufactured in the manner described above and accordingly has the features of the core described above.

[0031] The cells can be formed as closed cells, in particular with several cell walls.

[0032] In particular, it can be provided that the cell structure of the core has, with respect to the thickness direction, a deposition edge region which has a greater volume-related cell density than an inner region of the cell structure adjoining it in the thickness direction.

[0033] Furthermore, it can be provided that the cells forming a deposition surface of the core with respect to the thickness direction are filled with a filling material.

[0034] According to a further embodiment, the cell structure may have regions to increase the mechanical strength of the core, which have a greater volume-related cell density than adjacent regions, in which the cells have cell walls made of a material which has a greater mechanical strength than the cell walls of the cells in adjacent regions, or in which the cell walls of the cells have a greater wall thickness than the cell walls of the cells in adjacent regions.

[0035] According to a further embodiment of the core, the cell structure has a peripheral edge region which extends from a peripheral edge of the cell structure transversely to the thickness direction in a transverse direction, wherein the peripheral edge region has a greater volume-related cell density than an inner region of the cell structure adjoining it in the transverse direction. Generally, the core has a planar extension delimited by a peripheral edge. According to the present embodiment, a cross-sectional region of the core is provided which extends from the peripheral edge and extends over a discrete distance into the interior of the core and is referred to as the peripheral edge region. In this peripheral edge region, the cells of the cell structure forming the cross section of the core have a smaller volume than in a cross-sectional region adjoining the peripheral edge region.In this way, a larger amount of material is present per cell in the peripheral edge region, which, on the one hand, improves the mechanical strength of the core and, on the other hand, advantageously facilitates the attachment of fastening devices such as screws, rivets, bolts, or the like in the peripheral edge region. Alternatively, the cells of the peripheral edge region can also be filled with a filler material.

[0036] According to a further embodiment of the core, a connecting section for positively securing the core can also be formed in the peripheral edge region. For example, the connecting section can be formed by a pin protruding from or protruding from the peripheral edge or a recess extending from the peripheral edge into the cross-section of the core. In this way, the core can be particularly easily coupled to other cores in a positively locking manner, which facilitates the assembly of sandwich components comprising the core.

[0037] The features and advantages of the core described in connection with the method according to the invention apply analogously to the core described according to this aspect of the invention.

[0038] Herein, a "fiber material" or a "fiber material" is generally understood to mean a material which is formed from a plurality of reinforcing fibers, in particular thread-like or piece-like reinforcing fibers, such as carbon, glass, ceramic, aramid, boron, mineral, natural or plastic fibers or mixtures thereof.

[0039] "Fiber tapes" or "prepreg tapes" or a "semi-finished fiber product" is understood herein to mean a fiber material impregnated with a resin or matrix material, such as a thermosetting, thermoplastic, elastomeric resin, or generally a plastic resin or the like, or the fibers of the fiber material are embedded in the resin or matrix material. The fiber or prepreg tapes are manufactured into tapes extending in a longitudinal direction. The semi-finished fiber product can, in particular, be formed into a flat, closed mat or plate comprising several layers of fiber material stacked one above the other, with the fibers in adjacent layers preferably extending in different directions.

[0040] 3D printing processes within the meaning of this application encompass all generative or additive manufacturing processes in which, based on geometric models, objects of predefined shapes are produced from formless materials such as liquids and powders or form-neutral semi-finished products such as strip or wire material using chemical and / or physical processes in a special generative manufacturing system. 3D printing processes within the meaning of this application use additive processes in which the starting material is sequentially built up layer by layer in predetermined shapes.

[0041] Herein, the expression "one-piece", "one-piece", "integral" or "in one piece" refers generally to components being present as a single part forming a single material unit and, in particular, being manufactured as such, one component not being separable from the other without disrupting the material cohesion of the other.

[0042] With regard to directions and axes, in particular directions and axes relating to the course of physical structures, the course of an axis, a direction or a structure "along" another axis, direction or structure is understood to mean that these, in particular the tangents resulting at a respective point of the structures, each run at an angle of less than or equal to 45 degrees, preferably less than 30 degrees and particularly preferably parallel to one another.

[0043] The features and advantages of the core described in connection with the method according to the invention apply analogously to the core described according to this aspect of the invention.

[0044] According to a further aspect of the invention, a sandwich component is provided. The sandwich component comprises a first cover layer made of a fiber composite material, a second cover layer made of a fiber composite material, and a core arranged between the first and second cover layers, wherein the core is formed according to one of the embodiments described above. The sandwich component can be manufactured in a particularly simple and efficient manner, for example, using the method described above.

[0045] Herein, a "fiber material" or a "fiber material" is generally understood to mean a material which is formed from a plurality of reinforcing fibers, in particular thread-like or piece-like reinforcing fibers, such as carbon, glass, ceramic, aramid, boron, mineral, natural or plastic fibers or mixtures thereof.

[0046] "Fiber tapes" or "prepreg tapes" or a "semi-finished fiber product" is understood herein to mean a fiber material impregnated with a resin or matrix material, such as a thermosetting, thermoplastic, elastomeric resin, or generally a plastic resin or the like, or the fibers of the fiber material are embedded in the resin or matrix material. The fiber or prepreg tapes are manufactured into tapes extending in a longitudinal direction. The semi-finished fiber product can, in particular, be formed into a flat, closed mat or plate comprising several layers of fiber material stacked one above the other, with the fibers in adjacent layers preferably extending in different directions.

[0047] 3D printing processes within the meaning of this application encompass all generative or additive manufacturing processes in which, based on geometric models, objects of predefined shapes are produced from formless materials such as liquids and powders or form-neutral semi-finished products such as strip or wire material using chemical and / or physical processes in a special generative manufacturing system. 3D printing processes within the meaning of this application use additive processes in which the starting material is sequentially built up layer by layer in predetermined shapes.

[0048] Herein, the expression "one-piece", "one-piece", "integral" or "in one piece" refers generally to components being present as a single part forming a single material unit and, in particular, being manufactured as such, one component not being separable from the other without disrupting the material cohesion of the other.

[0049] With regard to directions and axes, in particular directions and axes relating to the course of physical structures, the course of an axis, a direction or a structure "along" another axis, direction or structure is understood to mean that these, in particular the tangents resulting at a respective point of the structures, each run at an angle of less than or equal to 45 degrees, preferably less than 30 degrees and particularly preferably parallel to one another.

[0050] With regard to directions and axes, in particular directions and axes relating to the course of physical structures, the term "transverse" to another axis, direction or structure is understood to mean that these, in particular the tangents resulting at a respective point of the structures, each run at an angle of greater than or equal to 45 degrees, preferably greater than or equal to 60 degrees and particularly preferably perpendicular to one another.

[0051] The invention is explained below with reference to the figures of the drawings. The figures show: Fig. 1 is a schematic view of a first step of a method for producing a sandwich component according to an embodiment of the present invention; Fig. 2 is a schematic view of a further step of the method according to an embodiment of the present invention; Fig. 3 is a schematic view of a further step of the method according to an embodiment of the present invention; Fig. 4 is a schematic sectional view of a sandwich component according to an embodiment of the present invention; Fig. 5 is a schematic sectional view of a core according to an embodiment of the present invention; Fig. 6 is a schematic sectional view of a core according to a further embodiment of the present invention; Fig. 7 is a schematic plan view of a deposition surface of a core according to a further embodiment of the present invention; Fig. 8 is a detailed view of the Fig. 7 area marked by the letter X; Fig. 9 is a schematic sectional view of a sandwich component according to a further embodiment of the present invention; Fig. 10 is a schematic sectional view of a sandwich component according to a further embodiment of the present invention with a core according to a further embodiment of the present invention; Fig. 11 is a schematic sectional view of a sandwich component according to a further embodiment of the present invention with a core according to a further embodiment of the present invention; Fig. 12 is a schematic sectional view of an arrangement of two sandwich components each according to a further embodiment of the present invention; and Fig. 13 is a schematic sectional view of a core according to a further embodiment of the present invention.

[0052] In the figures, the same reference symbols denote identical or functionally identical components, unless otherwise stated.

[0053] The Fig. 1 bis 3 show schematically the sequence of a method for producing a sandwich component 1.

[0054] In Fig. 1 A first step of the method is shown, in which a first cover layer 2 of the sandwich component 1 is formed. The first cover layer 2 is optionally formed by depositing fiber ribbons 20 on a mold surface 100a of a molding tool 100. The fiber ribbons 20 each have fibers F that are embedded in a matrix material M, in particular in a thermoplastic matrix material, e.g. PPS or PEEK. The first cover layer 2 is formed by depositing at least one flat, closed layer 21 of fiber ribbons 20. Optionally, several layers 21 can be deposited one on top of the other, as shown by way of example in Fig. 1 is shown. Here, the fiber ribbons 20 in adjacent layers 21 preferably have different fiber orientations. The fiber ribbons 20 are optionally laid down in a state in which the matrix material M is in a viscous aggregate state at least on the surface of the respective fiber ribbon 20. Alternatively, the matrix material M is converted into a viscous state immediately after deposition by means of heat. As a result, the individual fiber ribbons 20 and optionally the individual layers 21 melt together and a monolithic, flat, extending first cover layer 2 is formed. The first cover layer 2 can also be produced by applying a semi-finished fiber product (not shown) to the mold surface 100a. Here, a flat mat comprising several layers of a fiber material impregnated with matrix material is pressed against the mold surface 100a and thereby deformed according to the surface contour of the mold surface 100a.The matrix material is in a state suitable for deformation. Application to the mold surface 100a can be achieved, for example, by applying a vacuum to the mold surface 100a, by means of a second pressure stamp (not shown), by means of a roller (not shown), or in a similar manner.

[0055] The mold surface 100a of the mold 100 can in particular be a three-dimensional surface, as shown by way of example in the Fig. 1 bis 3 shown, or a flat surface. The design of the mold surface 100a defines the shape or profile of the first cover layer 2.

[0056] The laying down of the fiber bands 20 can be carried out, for example, by means of a laying head 101, as shown in Fig. 1 is shown schematically. For this purpose, the laying head 101 has one or more guide or laying rollers 102, by means of which the fiber ribbons 20 are guided to the surface on which they are to be laid and optionally pressed against it.

[0057] As in Fig. 1 As shown schematically, the deposition head 101 can further comprise an optional heating device 103 and a likewise optional inspection device 104. The optional heating device 103 serves to melt the matrix material M of the fiber ribbons 20. The inspection device 104 can be designed, for example, as a camera or as an ultrasonic detector and serves for the optional surface inspection of the surfaces of the fiber ribbons 20 during deposition to detect surface defects.

[0058] To form the first cover layer 2, the deposition head 101 is moved in a deposition direction L4 along the forming surface 100a of the forming tool 100, and the fiber slivers 20 are applied to the forming surface 100a or, if applicable, to the already deposited layer 20 by means of the roller 102. Optionally, the fiber slivers 20 can be heated during deposition by means of the heating device 103. Alternatively or additionally, the surface of the deposited fiber slivers 20 is optionally examined for surface defects or deposition errors during the deposition process by means of the inspection device 104. After the formation of the first cover layer 2, an outer surface 2b of the cover layer 2 rests against the forming surface 100a. An inner surface 2a of the cover layer 2 is oriented opposite to the outer surface 2b.

[0059] In a further step of the process, which is shown schematically in Fig. 2 As shown, a core 3 of the sandwich component 1 is produced. For this purpose, a cell structure 30 with a plurality of cells 35 in a thickness direction D is built up on the first cover layer 3 by means of an additive or generative manufacturing process. This can be realized, for example, by means of an FDM 3D printing process, as shown in Fig. 2 FDM is an abbreviation for "Fused Deposition Modeling". As shown in Fig. 3 As shown, the cells 35 are produced by means of a 3D printing device 50. This is guided along the inner surface 2a of the first cover layer 2 according to the desired course of the cell walls 36 forming the cells 35, as shown in Fig. 2 symbolically indicated by the arrow P1. The guidance of the 3D printing device 50 preferably takes place in a working plane above the inner surface 2a. The cell walls 36 are produced by liquefying a wire- or strip-shaped plastic material K by heating it using a heating device 51 provided in the 3D printing device 50 and applying it by extrusion onto the inner surface 2a of the first cover layer 2 using a nozzle 52 of the 3D printing device 50. There, the plastic material hardens by cooling. The cells 35 are constructed by repeatedly traversing one working plane at a time and then shifting the working plane upwards in a stacking manner, i.e., in the thickness direction D, thus increasing the distance to the inner surface 2a. As a result, the cell structure 30 is formed layer by layer in the thickness direction D.

[0060] As in Fig. 2 As shown schematically and by way of example, the 3D printing device 50 can comprise a supply roll 53 for storing and providing the plastic material K in strip form and a guide device 54, for example in the form of a pair of rollers as in Fig. 3 shown, for guiding the band-shaped plastic material K.

[0061] The core 3 produced in the manner described above has a planar extension along the inner surface 2a of the first cover layer 2. As in Fig. 3 As shown, the cell structure 30 of the core 3, in particular the cell walls 36 of the outermost cells 35 of the cell structure 30 with respect to the thickness direction D, forms a deposition surface 3a of the core 3. The thickness d3 of the core 3 with respect to the thickness direction D can vary along the planar extent of the core 3, as shown by way of example in Fig. 3 shown, or be constant.

[0062] As plastic material K, a thermoplastic material can be used, for example polycarbonate, PC for short, polyetherimide, PEI for short, or similar thermoplastics.

[0063] In a further step of the process, which is shown schematically in Fig. 3 As shown, a second cover layer 4 of the sandwich component 1 is formed. For this purpose, fiber ribbons 40 are preferably laid on the deposition surface 3a of the core 3. The fiber ribbons 40 can in particular be identical to the fiber ribbons 20 described above, which are used to form the first cover layer 2. The second cover layer 4 is formed by laying down at least one flat, closed layer 41 of fiber ribbons 40. Optionally, several layers 41 can be laid one on top of the other. The fiber ribbons 40 are optionally laid down in a state in which the matrix material M is in a viscous state of aggregation, at least on the surface of the respective fiber ribbon 40. Alternatively, the matrix material M is converted into a viscous state immediately after deposition by means of heat.As a result, the individual fiber bands 40 and, if applicable, the individual layers 41 merge and a monolithic, flatly extending second cover layer 4 is formed and simultaneously connected to the core 3.

[0064] The second cover layer 4 can also be formed by applying a semi-finished fiber product (not shown) to the deposition surface 3a of the core 3. In this case, a flat mat comprising multiple layers of a fiber material impregnated with matrix material is pressed against the deposition surface 3a and thereby deformed according to the surface contour of the deposition surface 3a. The matrix material is in a state suitable for deformation. The mat can be applied to the deposition surface 3a, for example, by applying a vacuum to the deposition surface 3a, by means of a second pressure stamp (not shown), by means of a roller (not shown), or in a similar manner.

[0065] During the production of core 3, a surface inspection can optionally be performed to detect defects in the cell structure. This can be achieved, for example, using an optional inspection device (not shown) provided on the 3D printing device 50, in particular in the form of a camera or an ultrasound detector.

[0066] To deposit the fiber slivers 40, the above-described deposition head 101 can be used in the same way as for forming the first cover layer 2. In particular, the fiber slivers 40 can optionally be heated during deposition using the heating device 103. Also optionally, the surface of the deposited fiber slivers 40 can be inspected for surface defects or deposition errors during the deposition process using the inspection device 104. After the formation of the second cover layer 4, an inner surface 4a of the second cover layer 4 rests against the deposition surface 3a of the core 3 or is integrally bonded thereto.

[0067] Fig. 4 shows a sandwich component 1 produced according to the described method with the first cover layer 3, the second cover layer 4 and the core 3 arranged between the first cover layer 2 and the second cover layer 4.

[0068] In the following, a core 3 for a sandwich component 1 is described. This can be used in particular in the Fig. 1 bis 3 explained method directly on the first cover layer 2 by means of an additive or generative manufacturing process, as described above. Alternatively, the core 3 can be produced by means of an additive or generative manufacturing process on a contour surface specifically provided for this purpose, for example the mold surface 100a of the mold 100. To produce the core 3 by means of an additive or generative manufacturing process, for example, the method described in Fig. 2 explained FDM process can be carried out, wherein the cell walls 36 forming the individual cells 35 of the cell structure 30 are formed by layer-by-layer application of the plastic material K according to the desired course of the cell walls described in detail below.

[0069] The Fig. 5 und 6 each show a core 3 with a cell structure 30 constructed by means of an additive manufacturing process in a thickness direction D, which cell structure has a plurality of cells 35. The cells 35 are each formed by a plurality of cell walls 36 and can in particular be present as closed cells 35. The core 3 has a planar extension, in particular along a transverse direction C extending transversely to the thickness direction, as shown for example in Fig. 6 can be seen. Furthermore, the core 3 has a first thickness edge region 3A and a second thickness edge region 3B located opposite thereto with respect to the thickness direction D. The outermost cells 35 with respect to the thickness direction D or the cell walls 36 of the second thickness edge region 3B forming them form a construction or contact surface 3b of the core 3. In the method for producing a sandwich component 1 described above, the contact surface 3b rests on the inner surface 2a of the first cover layer 2 or, when the cell structure 30 is built up, the second thickness edge region 3B is produced first. The outermost cells 35 with respect to the thickness direction D or the cell walls 36 of the first thickness edge region 3A forming them form the deposition surface 3a of the core 3, onto which the fiber ribbons 40 are laid to form the second cover layer 4. The first thickness edge region 3A thus forms a deposition edge region 31 of the cell structure 30.

[0070] As in Fig. 5 As shown by way of example, the deposition edge region 31 can have a greater volume-related cell density than an inner region 32 of the cell structure 30 adjoining it in the thickness direction D. The inner region 32 of the cell structure 30 is located between the first and second thickness edge regions 3A, 3B of the core 3 with respect to the thickness direction D. Optionally, the cell structure 30 can additionally have a greater volume-related cell density in the second thickness edge region 3B of the core 3 than in the inner region 32, as shown in Fig. 5 is shown as an example. In the Fig. 5 In the core 3 shown by way of example, the cells 35 forming the inner region 32 of the cell structure 30 each have essentially the same size or the same volume. In the method described above for producing a sandwich part 1, when constructing the cell structure 30 by means of a 3D printing process, the second thickness edge region 3B of the core 3 is first formed, optionally as a contact edge region with a high volume-related cell density, as in Fig. 5 shown. Subsequently, the inner region 32 and then the first thickness edge region 3A are formed, wherein in or through the first thickness edge region 3A, a deposition edge region 31 with a greater volume-related cell density than the inner region 32 is optionally formed. Due to the optionally increased cell density in the first and second thickness edge regions 3A, 3B, the contact surface for contact with the cover layers 2, 4 is increased. This results in improved adhesion of the cover layers to the core 3 and greater mechanical rigidity of the core 3.

[0071] Fig. 6 shows an example of a core 3 in which the cells 35 forming the support surface 3a of the core 3 are filled with a filling material. As in Fig. 6 The outermost cells 35 of the first thickness edge region 3A or of the storage edge region 31, respectively, with respect to the thickness direction D, are filled with filling material. In this way, openings or recesses defined by the cell walls 36 are filled, so that a closed storage surface 3a is formed, as shown in Fig. 6 is shown by way of example. Optionally, the outermost cells 35 of the second thickness edge region 3B with respect to the thickness direction D can also be filled with a filler material. The filling of the cells 35 can, for example, take place during the production of the cells 35 by means of the additive manufacturing process during the construction of the cell structure 30.

[0072] As the Fig. 6 and 13 further show, in order to increase the mechanical strength of the core 3, regions 37 can be provided within the cell structure 30, which have a greater volume-related cell density than adjacent regions 38. In the case of the Fig. 6 In the core 3 shown by way of example, a first partial region 37 with a high cell density is provided in the inner region 32, which extends transversely to the thickness direction D. This first partial region 37 is located between two second partial regions 38 with respect to the thickness direction D, each of which has a smaller volume-related cell density than the first partial region 37. Alternatively or additionally, it can also be provided that the cell walls 36 of the cells 35 of the first partial region 37 are formed from a material which has a greater mechanical strength than the material of the cell walls 36 of the cells 35 in the second partial regions 38. Furthermore, the cell walls 36 of the cells 35 of the first partial region 37 can also have a greater wall thickness than the cell walls 36 of the cells 35 in adjacent partial regions 38.

[0073] In the Fig. 13 In the core 3 shown as an example, a first partial region 37 is provided, which extends along the thickness direction D between the deposition surface 3a and the contact surface 3b of the core 3, which is opposite to the thickness direction D. The first partial region 37 can in particular be formed columnar, as in Fig. 13 shown by way of example, and has a greater volume-related cell density than the second sub-regions 38 surrounding it. Of course, instead of the increased cell density, it can also be provided that the cells 35 of the first sub-region 37 are filled with a filling material, are formed with a greater wall thickness or are made of a more resistant material than the cells 35 of the second sub-regions 38. In Fig. 13 It is further shown by way of example that a recess 60 extending between the support surface 3a and the contact surface 3b can be formed in the first partial region 37. This recess can be provided, for example, for receiving a fastening device, such as a bolt or the like.

[0074] In the Fig. 7 und 8 In each case a top view of the deposition surface 3a of a core 3 is shown. In the Fig. 8 In the top view, a fiber band 40 is additionally shown, which, for example, was deposited on the deposition surface 3a of the core 3 during the formation of the second cover layer 4 during the process explained above. During the production of the core 3, the cells 35 forming the deposition surface 3a, i.e. the cells 35 located opposite to the first cover layer 2 with respect to the thickness direction D, were formed as open cells 35 at least in partial areas of the planar extent of the deposition surface 3a. This means that the cell walls 36 forming the cells 35 define, as shown in Fig. 6 shown by way of example, openings or depressions 35A. When depositing fiber ribbons 40 onto the depositing surface 3a of the core 3, it should be avoided as far as possible that the fiber ribbons 40 extending over the openings 35A sag, which can occur in particular due to the viscous state of the matrix material M, in order to avoid the formation of dents in the second cover layer 4 of the sandwich component 1. In the case of the Fig. 5 In the core 3 shown as an example, the risk of sagging is reduced by making the openings 35A as small as possible due to the increased cell density in the deposition edge area 31. In the core 3 shown in Fig. 6 The openings 35A are filled with the core 3 shown in Fig. 8 In the optional design of the core 3 shown, the cells 35 in the deposition edge region 31 are aligned with their cell walls 36 according to the deposition direction L4 of the fiber bands 40 or are formed accordingly. Fig. 8 The cell walls 36 define a rectangular opening 35A with a longitudinal extension in the direction L35. This longitudinal extension L35 runs along the deposition direction L4, in which the fiber ribbons 40 are deposited with their fiber longitudinal direction LF. In this way, the inherently stiff fibers F span the openings 35A lengthwise, thereby preventing sagging.

[0075] The Fig. 9 bis 12 show optional designs of a sandwich component 1. The sandwich component 1 can be produced in particular using the method described above and in particular has a core 3 which can be designed as described above.

[0076] The Fig. 9 Sandwich part 1 shown as an example has the Fig. 5 shown core 3. It is arranged between a first cover layer 2 and a second cover layer 4 with respect to the thickness direction D. The first cover layer is connected to the outermost cells 35 of the second thickness edge region 3B of the core 3 with respect to the thickness direction D. The second cover layer 4 is connected to the outermost cells 35 of the first thickness edge region 3A with respect to the thickness direction D or to the deposition surface 3a of the core. As in Fig. 9 As is further shown, the first cover layer 2 and the second cover layer 4 each extend beyond a peripheral edge 33 of the core 3 or the cellular structure 30 of the core 3. The peripheral edge 33 delimits, limits, or defines the planar extent of the core 3. The regions of the first cover layer 2 that project beyond the peripheral edge 33 and the regions of the second cover layer 4 that project beyond the peripheral edge 33 are connected to one another, in particular by a material fit, and form a monolithic peripheral edge region 5 of the sandwich component 1. The material fit can be formed in particular when the fiber bands 40 are laid down during the formation of the second cover layer 4, when the fiber bands 40 are laid down with the matrix material M in the viscous state beyond the peripheral edge 33 of the cellular structure 30 onto the inner surface 2a of the lower cover layer 2.The peripheral edge region 5 can be used in particular for the structural connection of the sandwich component 1 and is suitable, for example, for the attachment of fastening devices such as screws, rivets, bolts and the like.

[0077] Fig. 10 shows a cross-sectional view of a further optional design of the peripheral edge region 5 of the sandwich component 1. As in Fig. 10 As shown by way of example, the cell structure 30 of the core 3 has a peripheral edge region 39 which extends from a peripheral edge 33 of the cell structure 30, in particular transversely to the thickness direction D into the interior of the cell structure 30. The cells 35 of the peripheral edge region 39 of the cell structure 30 are filled with a filler material, which can be done in particular during construction of the cell structure 30. The cell structure 30 can therefore be constructed with a solid peripheral edge region 39. Alternatively, the cells 35 of the peripheral edge region 39 of the cell structure 30 can be subsequently filled with a filler material. The first and second cover layers 2, 4 overlap the peripheral edge region 39 of the cell structure 30 and end flush with the peripheral edge 33 of the cell structure 30. Filling the cells 35 offers the advantage that the penetration of liquid into the interior of the core 3 is reliably prevented.Furthermore, fastening devices such as screws, rivets, bolts, or the like can be inserted into the filled cells 35 and anchored there with great reliability and load-bearing capacity. Reliable adhesion between core 3 and cover layers 2, 4 is also achieved in the outermost cells 35 with respect to the thickness direction D if these are also filled, as shown in FIG. Fig. 10 is shown as an example.

[0078] Fig. 11 shows a cross-sectional view of a further optional design of the peripheral edge region 5 of the sandwich component 1. In contrast to Fig. 10 are the cells 35 of the peripheral edge region 39 of the cell structure 30 of the core 3 of the Fig. 11 The sandwich component 1 shown as an example is not filled with a filler material, but rather has a higher volume-related cell density than an inner region 32 of the cell structure 30 adjacent to the peripheral edge region 39. This offers the advantage of increasing the mechanical rigidity of the core 3 while keeping the weight low. This design also facilitates the attachment of fastening devices in the peripheral edge region 39 and improves the adhesion between the core 3 and the cover layers 2, 4.

[0079] In Fig. 12 an arrangement of sandwich components 1 is shown. Here, the peripheral edge regions 5 of the sandwich components 1 are mechanically coupled to each other. Fig. 12 also shows a further optional design of the peripheral edge regions 5 of the sandwich components 1. The peripheral edge regions 39 of the cell structures 30 of the cores 3 of the sandwich components 1 are, as can be seen from Fig. 10 explained, with filled cells 35 or solid. As in Fig. 12 Further shown, a connecting section 39A, 39B is formed in the respective peripheral edge region 39. The connecting section can be realized in particular in the form of a pin 39A or a recess 39B. In Fig. 12 the peripheral edge region 39 of the cell structure 30 of the core 3 of the sandwich component 1, which in the illustration of the Fig. 12 located at the bottom, has a pin 39A projecting in the thickness direction D from the peripheral edge region 39. Of course, the pin 39 can also extend transversely to the thickness direction D from the peripheral edge 33 or generally from the peripheral edge region 39. The peripheral edge region 39 of the cell structure 30 of the core 3 of the sandwich component 1, which in the illustration of the Fig. 12 located at the top, has a recess 39B extending transversely to the thickness direction D from the peripheral edge 33. Of course, the recess 39B can also extend along the thickness direction D or generally into the peripheral edge region 39. As in Fig. 12 As shown, the pin 39A is inserted into the recess 39B, whereby a positive fastening of the cores 3 to each other is realized

[0080] Although the present invention has been explained above using exemplary embodiments, it is not limited thereto but can be modified in a variety of ways. In particular, combinations of the above embodiments are also conceivable. LIST OF REFERENCE SYMBOLS

[0081] 1Sandwich component 2First cover layer 2aInner surface of the first cover layer 2bOuter surface of the first cover layer 3Core 3AFirst thickness edge region of the core 3aDeposition surface of the core 3BSecond thickness edge region of the core 4Second cover layer 4aInner surface of the second cover layer 5Circumferential edge region of the sandwich component 20, 40Fiber bands 21,41Layer 30Cell structure of the core 31Deposition edge area of ​​the cell structure 32Inner area of ​​the cell structure 33Circumferential edge of the cell structure 35Cells 35ARecesses 36Cell walls 37Area of ​​the cell structure 38Area of ​​the cell structure 39Circumferential edge area of ​​the cell structure 39APin 39BRecess 503D printing device 51Heating device of the 3D printing device 52Nozzle of the 3D printing device 53Supply roll 54Guide device 60Recess 100Molding tool 100aMold surface 101Deposition head 102Deposition roll 103Heating device 104Inspection device CTransverse direction DThickness direction d3Thickness of the core FFiber KRecycling material L4Deposition direction L35Longitudinal extension of the cells LFFiber longitudinal direction MMatrix material P1Arrow,

Claims

1. Process for producing a sandwich component (1), comprising the following steps: forming a first cover layer (2) on a mould surface (100a) of a moulding tool (100) by depositing fibre strips (20) on the mould surface (100a) of the moulding tool (100) or by placing an areally extending fibre semi-finished product onto the mould surface (100a) of the moulding tool (100); creating a core (3) by constructing a cell structure (30) having a multiplicity of cells (35) in a thickness direction (D) on the first cover layer (2) by means of an additive manufacturing process; forming a second cover layer (4) on a deposition surface (3a), situated opposite the first cover layer (2), of the core (3) by depositing fibre strips (40) onto the deposition surface (3a) of the core (3) or by placing an areally extending fibre semi-finished product onto the deposition surface (3a) of the core (3); wherein the additive manufacturing process used to create the core (3) is a FDM 3D printing process.

2. Process according to Claim 1, wherein the fibre strips (20, 40) for forming the first cover layer (2) and / or the second cover layer (4) or the fibre semi-finished product for forming the first cover layer (2) and / or the second cover layer (4) each comprise a thermoplastic matrix material.

3. Process according to one of the preceding claims, wherein the cell structure (30) of the core (3) is constructed from a thermoplastic material.

4. Process according to one of the preceding claims, wherein the cell structure (30) of the core (3) is formed with a deposition boundary region (31) which is situated opposite the first cover layer (2) with respect to the thickness direction (D) and has a greater relative cell density than an inner region (32) of the cell structure (30) adjoining it in the thickness direction (D) does.

5. Process according to one of the preceding claims, wherein the cells (35) situated opposite the first cover layer (2) with respect to the thickness direction (D) and forming the deposition surface (3a) are formed such that a longitudinal extent (L35) of the cells (35) extends along a deposition direction (L4) matching the fibre longitudinal extent (LF) of the fibre strips (40) when the latter are deposited.

6. Process according to one of the preceding claims, wherein the cells (35) situated opposite the first cover layer (2) with respect to the thickness direction (D) and forming the deposition surface (3a) are filled with a filler material.

7. Process according to Claim 6, wherein the cells (35) for forming the deposition surface (3a) by means of the additive manufacturing process are filled when the cell structure (30) is being constructed.

8. Process according to one of the preceding claims, wherein, to increase the mechanical strength of the core (3), the cell structure (30) of the core (3) is constructed so as to form regions (37) - which have a greater relative cell density than adjacent regions (38) do, or - in which the cells (35) are formed with cell walls (36) made of a material which has a greater mechanical strength than the cell walls (36) of the cells (35) in adjacent regions (38) do, or - in which the cell walls (36) of the cells (35) have a greater wall thickness than the cell walls (36) of the cells (35) in adjacent regions (38) do, or - in which the cells (35) are filled with a filler material.

9. Process according to one of the preceding claims, wherein the surfaces are inspected to identify surface defects while the first cover layer (2) is being formed and / or while the core (3) is being created and / or while the second cover layer (4) is being formed.

10. Sandwich component (1) produced by a process according to one of the preceding claims.

11. Sandwich component (1) according to Claim 10, wherein the cell structure (30) of the core (3), with respect to the thickness direction (D), has a deposition boundary region (31) which has a greater relative cell density than an inner region (32) of the cell structure (30) adjoining it in the thickness direction (D) does.

12. Sandwich component (1) according to Claim 10 or 11, wherein the cells (35) forming a deposition surface (3a) of the core (3) with respect to the thickness direction (D) are filled with a filler material.

13. Sandwich component (1) according to one of Claims 10 to 12, wherein, to increase the mechanical strength of the core (3), the cell structure (30) has regions (37) - which have a greater relative cell density than adjacent regions (38) do, - in which the cells (35) have cell walls (36) made of a material which has a greater mechanical strength than the cell walls (36) of the cells (35) in adjacent regions (38) do, or - in which the cell walls (36) of the cells (35) have a greater wall thickness than the cell walls (36) of the cells (35) in adjacent regions (38) do.

14. Sandwich component (1) according to one of Claims 10 to 13, wherein the cell structure (30) has a peripheral boundary region (39) which extends from a peripheral boundary (33) of the cell structure (30), wherein the peripheral boundary region (39) has a greater relative cell density than an inner region (32) of the cell structure (30) adjoining the peripheral boundary region (39), or wherein the cells (35) of the peripheral boundary region (39) are filled with a filler material.

15. Sandwich component (1) according to Claim 14, wherein a connecting portion (39A; 39B), in particular in the form of a pin (39A) or a recess (39B), for form-fitting attachment of the core (3) is formed in the peripheral boundary region (39).