METHOD FOR THE PRODUCTION OF MINERAL HIGH-TEMPERATURE FIBERS WITH A HIGH SILICON DIOXIDE CONTENT

DE502019012118D1Active Publication Date: 2024-10-02SCHIERZ CLAUS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502019012118
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-06-03
Filing Date
2019-05-31
Publication Date
2024-10-02
Estimated Expiration
2039-05-31

AI Technical Summary

Technical Problem

Existing processes for producing high-temperature mineral fibers with a high proportion of silicon dioxide are costly and inefficient, particularly when aiming for high-quality mineral fiber nonwovens for applications like catalytic converters, where the fibers' strength and processing are compromised.

Method used

A cost-effective process involving gentle leaching of glass or basalt filaments to achieve 80% to 98% SiO2 content, using air texturing to increase filament volume and surface area, followed by acid treatment to remove alkaline components, resulting in stronger, more processable fibers with enhanced temperature resistance.

Benefits of technology

This process significantly reduces filament destruction during processing, enhances final strength, and allows for the production of high-quality mineral fiber fleece with improved temperature resistance, making it more effective and gentler than traditional methods while being more cost-effective.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Method for the production of mineral high-temperature fibers with a high proportion of silicon dioxide for the production of mineral fiber fleece, preferably for use in catalysts or silencers for internal combustion engines.

[0002] By treating mineral fibers in a specific acid concentration, alkaline components can be removed, or leached, from the fibers. As a result, only silicon dioxide (SiO2) and aluminum oxide (Al2O3) remain in the glass fiber filament. These two components give the fiber material a maximum temperature resistance of 1100°C. The processes for this have been known since the mid-1950s. For example, the textbook "Industrial Inorganic Chemistry" published by Wiley-VCH describes the treatment of low-melting-point textile glass fibers, such as A- or E-glass fibers, with acids as an efficient method for obtaining high-temperature-resistant textile fibers with high silicon dioxide content. These textile glass fibers are produced either via the direct melting process or via the two-stage ball or pellet melting process.Fibers with a SiO₂ content greater than 99% can be obtained using an acid-induced, diffusion-controlled ion exchange process on Si-OM glass network groups. In this process, the monovalent alkali metal ions, such as Li, Na, and K ions, which act as glass network interfacials, are almost completely exchanged for the acid protons. The doubly charged alkaline earth metal ions and the triply charged network-forming metal ions, with the exception of boron and Al ions, are only exchanged in trace amounts from the glass structure. The ion exchange reaction of alkali or boron ions for hydrogen ions on Si-OM network groups (M = Na, K, B) transforms the glass network into a three-dimensionally cross-linked polysilicic acid. As a result of this transformation, the melting point of the fibers rises, depending on the chemical composition, into the temperature range above 1400°C.

[0003] To create bulk in textile yarns, so-called effect yarns are known as decorative or novelty yarns, in which a dynamic, textured, or expressive surface structure is produced through various manufacturing processes. This is achieved, for example, in effect yarns by twisting two or more threads of different thicknesses on an effect yarn twisting machine. Effect yarns can also be created through uneven spinning, the addition of foreign fibers or particles, color and luster effects, and modified manufacturing steps. Synthetic fibers are frequently used in the production of effect yarns.

[0004] In publication WO 2006 / 079542 A1, a method and a device for generating periodic thread deflection on an effect thread during the production of an effect yarn are described. In this method, a core thread is combined with an effect thread to form the effect yarn, wherein the effect points on the effect yarn are created by the periodic formation and dissolution of a thread loop through deflection of the effect thread between two thread guides. To generate the highest possible density of effect points in the effect yarn, the thread loop of the effect thread is, according to the invention, created by a rotating forming disc with an asymmetrical outer contour, wherein the thread is guided transversely to the forming disc and deflected by the outer contour of the rotating forming disc.

[0005] US3578426 primarily concerns the moistening of glass fibers. Surface etching is only mentioned in passing and is not the subject of the application. Etching (leaching) serves to improve the subsequent adhesion of (synthetic) resin. US3356561 concerns fiber mats that can be used in catalysts. GB-824972 concerns the etching of glass fibers.

[0006] The object of the present invention is to create a more cost-effective method compared to previous, known methods while simultaneously ensuring high quality in the production of mineral fibers, e.g. for the subsequent use of these fibers in mineral fiber nonwovens for use, e.g., in catalysts for motor vehicles.

[0007] Surprisingly, it was discovered that commercially available continuous glass fiber filaments, preferably made of E-glass, can be chemically modified by selectively altering their physical properties, for example, by increasing their surface area and thus their volume and structure, followed by a short, gentle leaching process. This modification results in a filament structure with a specific SiO2 content of 80% to 98%. The result is a soft, fluffy fiber with good strength, which is significantly better suited for processing into insulation products than commercially available silica fibers. Furthermore, it was possible for the first time to leach basalt continuous fiber filaments, again with surprising results for their potential use in the production of mineral fiber fleeces.

[0008] This comprehensive process enables the refinement of a wide variety of commercially available fiberglass products and the targeted creation of new properties for diverse products. The new process is significantly more cost-effective than the traditional silica process. A second key difference from previously known methods is that the filaments are expanded before the chemical refining process. This is considerably more efficient and gentler. Filament damage during further processing is reduced by approximately 80% with the new process, ultimately resulting in higher final strength, for example, in the production of mineral fiber fleeces.

[0009] Extensive practical trials have so far successfully processed the following types of glass fibers: E-glass, C-glass, D-glass, ECR-glass, R-glass, AR-glass, S-glass, S-2-glass, A-glass, and also basalt filaments.

[0010] Advantageous embodiments of the invention are explained in more detail with reference to the drawing. The drawing schematically illustrates the process flow.

[0011] Two galettes, 3 and 4, where galette 3 carries the core filament 1 and galette 4 carries the effect filament 2, feed the core filament 1 and the effect filament 2 to the air texturing nozzle(s) 5. The effect filament 2 is fed at a higher velocity than the core filament 1. This causes the effect filament 2 to swell around the core filament 1 in the area of ​​the air texturing nozzle 5, creating the so-called effect yarn 6, which has a significantly larger volume than two adjacent filaments. It has been found that, when the effect yarn 6 is used for the production of mineral fiber nonwovens, the core filament 1 has a larger diameter than the effect filament 2.

[0012] The two filaments, core filament 1 and effect filament 2, and thus ultimately the effect yarn 6, are gently textured (opened) using special texturing nozzles 5. This texturing enables faster yet gentler leaching in the subsequent acid bath 7. This results in fewer filament breaks and therefore higher strength during further processing in the final product, e.g., in a mineral fiber fleece.

[0013] In one variant of the process, several effect filaments 2, which are supplied by additional galettes, are used.

[0014] Basalt filaments can also be used instead of glass filaments. Due to the high Al2O3 content in the basalt filament, up to 20%, even higher temperature resistance is achieved with the leached fiber product (up to over 1100 degrees Celsius).

[0015] The effect yarn 6 produced in the air texturing nozzle 5 is subsequently fed into the acid bath 7 for the leaching process 7. Here, the alkaline components in the effect yarn 6 are dissolved. The residence time in the acid bath 7 is determined by experience. Compilation of reference symbols

[0016] 1 - Core filament 2 - Effect filament 3 - Galette 4 - Galette 5 - Air texturing nozzle 6 - Effect yarn 7 - Acid bath, leaching

Claims

1. Procedure for the production of mineral high-temperature fibres with a high proportion of silicon dioxide using continuous glass fibre filaments and / or continuous basalt filaments, characterised in that at least two filaments, as core filament (1) and as effect filament (2), are each fed at different speeds from a godet (3, 4) to one or more air texturing nozzles (5), where they are textured to form a fancy yarn (6) and this fancy yarn (6) is then subjected to an acid bath (leaching) (7).

2. Procedure for the production of insulating glass elements according to claim 1, characterised in that the core filament (1) has a larger diameter than the effect filament (2).

3. Procedure for the production of mineral high-temperature fibres according to one of the preceding claims, characterised in that several effect filaments (2) are used to produce the fancy yarn (6).

4. Procedure for the production of mineral high-temperature fibres according to one of the preceding claims, characterised in that basalt filaments are used for the core filament (1) and / or for the effect filament (2).

5. Procedure for the production of mineral high-temperature fibres according to one of the preceding claims, characterised in that E-glass is used as the base material for the core filament (1) and for the effect filament (2).

6. Procedure for the production of mineral high-temperature fibres according to one of the preceding claims, characterised in that the fancy yarn (6) is leached until, depending on the content of aluminium oxide (Al2O3), a proportion of 96% silicon dioxide (SiO2) is reached.

7. Procedure for the production of mineral high-temperature fibres according to one of the preceding claims, characterised in that a thermally activatable foaming agent is applied to the fancy yarn (6) after leaching.