Component made of a material consisting predominantly of renewable raw materials, with at least one compressed area, as well as method and tool for producing the compressed area
Patent Information
- Application Number
- DE502020009573
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-07-31
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2040-07-31
AI Technical Summary
Conventional screw connections in wood materials suffer from settling and relaxation phenomena due to low material density, which limits the connection strength and requires additional elements like washers or inserts to increase surface pressure, but these methods do not fully utilize the material's compressive strength.
A component made predominantly of renewable raw materials with locally compressed areas around holes, created using a rotating mandrel to increase material density, allowing for radial and axial compression, thereby enhancing the mechanical properties without additional connecting means.
The local compression increases the material's density and mechanical properties, resulting in a permanent non-slip prestressed connection that withstands higher loads and reduces settling and relaxation phenomena, achieving a stronger screw connection without the need for additional reinforcing elements.
Description
[0001] The invention relates to a component made of a material consisting predominantly of renewable raw materials, with at least one compacted area, as well as a method and a tool for producing the compacted area and is used in particular for fatigue-resistant screw connections.
[0002] The use of nails and screws as fasteners, as well as bolted connections requiring prior pre-drilling with tools with a geometrically defined cutting edge, is known from the state of the art. With nails and screws, the withdrawal resistance depends largely on the density of the material. All types of connections usually experience settlement phenomena, which are detrimental to the strength of the connection, primarily in the wood-based material. A fatigue-resistant connection for a metal fastener requires a high tightening torque, which results in high surface pressure, among other things, under the screw head / nut / washer. This increases the stress in the wood-based material, and relaxation and retardation phenomena occur, which are detrimental to the strength of the connection. In the state of the art, this effect is counteracted by enlarging the contact surface, e.g.weakened by additional elements such as washers or by the use of inserts or sleeves in the borehole.
[0003] The documents DE 26 32 695 C2 and DE 76 23 015 U1 describe a compensating bushing for attaching handles or similar items. Conical bushings are arranged between the object to be attached (e.g. handle) and the base (e.g. wooden panel). The base has a through-hole in the area of the attachment point. When the handle is screwed to the base, the bushings are pressed into the base. According to the description, this displacement and thus compaction and strengthening of the wood occurs. Furthermore, the components center themselves relative to one another, which leads to more precise positioning. These effects result in a connection that is capable of absorbing high radial, axial, and tilting forces.
[0004] DE 197 24 284 C2 describes a coupling purlin made up of several overlapping wooden beams, as well as a screw for a coupling purlin. This invention uses screws characterized by a stepped shaft. Both areas are provided with threads of the same pitch but different diameters. The threads do not primarily have a cutting function, but rather a displacing function. The stepped design of the screw shaft results in a two-stage hardening of the material, thus further increasing the load-bearing capacity of the connection. A further positive effect is achieved by the screw head being designed as a relatively slender cone. This design means that it can be easily countersunk without the need for an additional work step to form a countersink. The screw head cone further hardens the material.The patent states that the screws can be installed without pre-drilling and without the risk of the wood cracking at its ends.
[0005] DE 10 2016 120 728 A1 describes a conical screw for foamed plastics. This is a connection in a plastic with a defined elasticity. The screw thread is conical. When the thread is screwed in, the material is not destroyed, but rather displaced and compressed. The deeper the thread is screwed in, the larger the diameter of the cone becomes and the more material is displaced. This leads to an increase in the restoring torque required for screwing in and thus also in the contact force that develops between the parts to be joined. This creates a high surface pressure between them, resulting in a resilient connection.
[0006] WO 2016 162 111 A1 describes a reversible connection between machine parts. A flowable medium is introduced into a cavity of a component, which is then sealed. In the exemplary embodiment, this is a shaft. A conical body is screwed into the flowable medium, displacing it. This creates pressure in the cavity, causing it to expand, allowing, for example, a shaft-hub connection to be realized. Further prior art is known from US Pat. No. 4,248,820 A and DE 20 2009 007835 U.
[0007] Some of the above-mentioned patents regarding compaction generally refer to the compaction of the local area being caused by the fastener during tightening of the fastener. The quality of compaction is therefore only as great as the maximum preload of the fastener, dependent on the screw head area in combination with the compressive strength of the material to be compacted. The maximum possible compaction to 1.4 g / cm 3 <, at which density the material exhibits its maximum possible mechanical properties, is generally not achievable with pin-shaped fasteners and their resulting screw head area. The tensile strength of the screw is already exhausted well before the material reaches its maximum possible compressive strength. However, retardation or relaxation phenomena are only significantly reduced at this limit.
[0008] During the conventional production of bores in plate-shaped semi-finished products made of wood-based materials, the material undergoes a machining-related geometric deformation. A disadvantage is that the mechanical material properties in the borehole edge area of the material, particularly with regard to density properties and compressive strength, are not changed or are changed so slightly that they are not significantly relevant. The object of the invention is to develop a component made of a material that consists predominantly of renewable raw materials and has at least one compacted area, as well as a method and tool for producing the compacted area, which enables a local increase in the material density and thus the mechanical properties without the need to introduce an additional connecting element such as inserts or sleeves with a higher density or strength than the original wood-based material.
[0009] This problem is solved by the features of the first, third, and ninth patent claims. Advantageous embodiments emerge from the subclaims.
[0010] The component consists of a material predominantly made from renewable raw materials, wherein the component has at least one hole with a longitudinal axis. According to the invention, the material of the component exhibits local compaction in the area circumferentially adjacent to the hole. This local compaction reduces the settling phenomena that occur when establishing a screw connection with another component.
[0011] The area of the component adjacent to the hole on the circumference shows radial and / or axial local compaction.
[0012] During axial compaction, the component can be radially compacted beforehand. This would result in a combined compression of 1. radial and 2. axial. Thus, the hole recess would be introduced prior to axial compaction.
[0013] The second option would be axial compaction and subsequent drilling (by machining).
[0014] This would mean that the compaction would not be a combination, but only a single-stage compaction with the subsequent screw recess in the machining process.
[0015] If the hole has a diameter, the circumference of the compacted area adjacent to the hole is up to five times the diameter of the hole.
[0016] The height of the compacted area is up to twenty times the hole diameter and is preferably reduced compared to the height of the component.
[0017] The hole present in the component is a cylindrical or nearly cylindrical hole and is designed as a through hole in the component or has a bottom.
[0018] The material of the component consists of wood or contains at least 50% renewable raw materials.
[0019] Particularly preferred is the material a wood-based material, to which less than 50% of other renewable raw materials such as grass materials (bamboo) are added, if necessary,
[0020] The component can also be a hybrid material such as wood plastic composite (WPC) with renewable raw materials.
[0021] Furthermore, the component can have one or more material layers made of metal, plastic, fiber composite material, paper or cardboard or a combination of these material layers.
[0022] The component is preferably designed in the form of a plate and has at least two layers of renewable raw materials, preferably three layers of wood, which can be combined with further material layers if required.
[0023] The hole is preferably made at an angle of 90° to 45° to the top of the component.
[0024] The method for producing at least one compacted area in a component made of a material which consists of at least 50% renewable raw materials is carried out in that at least one rotating mandrel penetrates into the material of the component and thereby creates a hole in the component and displaces the material radially and / or axially and in the process creates a local compaction (V) in the area of the material surrounding the hole.
[0025] Alternatively, the method for producing at least one compacted region in a component from a material which consists of at least 50% renewable raw materials is carried out in that at least one rotating mandrel penetrates into the material of the component and thereby creates a depression in the component and displaces the material radially and / or axially and thereby creates a local compaction (V) in the material.
[0026] According to one embodiment of the invention, two opposing mandrels can be used, which penetrate into the component alternately from opposite directions and create the hole with the diameter, thereby displacing the material and compacting it in the area surrounding the hole.
[0027] Alternatively, two opposing mandrels can be used, creating a depression in the component from opposite directions and compacting the area of the component located between the mandrels. At least one mandrel or the opposing mandrels rotate at least during penetration into the component.
[0028] After a mandrel has partially penetrated the component, a return stroke movement of the engaged mandrel can take place and then a further forward stroke movement of the mandrel, during which the mandrel penetrates further into the component until the mandrel has completely penetrated the component.
[0029] If two opposing mandrels are used, the return stroke of one mandrel can be accompanied by a forward stroke of the opposite mandrel into the component. This is repeated alternately until the through hole is created in the component.
[0030] A maximum penetration depth of the mandrel per forward stroke is preferably determined depending on the component (material and density of the component) as well as on a rotational speed of the mandrel and / or a feed speed of the mandrel.
[0031] After reaching this specified maximum penetration depth per feed movement, the mandrel performs a return stroke. This prevents the component from becoming excessively heated due to the resulting friction.
[0032] The corresponding values can be easily determined through reference tests. Therefore, the rotational speed and / or feed rate and / or maximum penetration depth are preferably determined empirically.
[0033] The maximum penetration depth of each punch per stroke is set so that the temperature acting on the component due to the friction of the punch does not exceed 200°C (possibly more or less, depending on the construction material).
[0034] The tool for carrying out the process serves to produce a predominantly radial compaction and is designed in the form of at least one mandrel with a cylindrical or polygonal shaft and a tip whose diameter reduces in the direction of the component.
[0035] To produce a predominantly axial compaction in the direction of the component, the tool has a flat / plane / conical surface with an obtuse angle and / or widens in diameter away from the component.
[0036] The angle of the blunt-shaped (temperature-treated or cold) forming tool must be at least equal to the angle of the maximum possible elongation of the adjacent side prior to compaction, which becomes the hypotenuse spanned by the triangle after compaction. This elongation must be at least 1%, and thus the corresponding angle of the forming tool depends on the elongation.
[0037] The tip of the mandrel can also be in the form of a conical tip, a truncated cone or another shape that reduces in diameter towards the component.
[0038] A counterholder can be arranged on the side of the component opposite the mandrel, and / or the mandrel can also be surrounded by a hold-down device. The mandrel can be set in rotation by a first drive and moved in the direction of the mandrel's longitudinal axis by a second drive when radial compression is to be achieved and a hole is to be created.
[0039] Alternatively, the mandrel can only be moved in the direction of the longitudinal axis of the mandrel by means of a second drive if only axial compaction is to be achieved.
[0040] According to a variant of the invention, the mandrel can be heated.
[0041] With an unheated rotating punch, high temperatures can also be reached through friction.
[0042] The tool can have a temperature sensor.
[0043] The axially or radially acting punch can also be unheated (cold), whereby high temperatures can also be reached passively with the rotating punch due to friction with the component.
[0044] During axial compaction, after reaching the desired final shape, the forming tool (the mandrel) can be cooled (if heated) or removed while hot. Cooling can be achieved actively or passively.
[0045] The invention relates to the formation of a permanently slip-resistant prestressed connection point in a material which consists of at least 50% renewable raw materials, with metallic connecting means, by minimizing the differences in the mechanical properties between the material and the metallic connecting means.
[0046] The sharp drop in preload force of slip-resistant preloaded metal fasteners, such as screws, due to relaxation and retardation phenomena occurring in the material of a component is achieved according to the invention by a locally defined increase in the material's bulk density. This local density increase can be achieved by the inventive solution in the form of axial and / or radial compaction during semi-finished product production or subsequently using appropriate tools according to the invention.
[0047] Fasteners for direct screwing, such as self-tapping, thread-forming screws, are excluded from this because they do not allow for a permanent, slip-resistant, pre-tensioned connection.
[0048] According to the method according to the invention, the joint is compacted to such a high degree across the entire connection cross-section that a permanent, slip-resistant, preloaded screw connection is created without the need for additional fasteners or re-tensioning. This type of material compaction is not possible with conventional fasteners in a one- or two-stage process because the permissible preload of the fastener is too low. The deformation of the material, in particular the wood-based material or another renewable raw material (e.g., bamboo or a mixture of various renewable raw materials) in the joint is plastic; it is fixed during the manufacturing process using plant-derived components such as cellulose, hemicellulose, and lignin through physico-chemical processes.
[0049] Lignins form a group of phenolic macromolecules composed of various monomer building blocks. They are solid biopolymers that are incorporated into the plant cell wall, thereby causing the cell to become woody (lignified). These inclusions are found in the cell walls of woody plants such as bamboo, grasses, perennials, shrubs, and trees. As a support material and hardened polymer, lignin has several important functions for the plant. Lignins are essential for the strength of plant tissues, especially their compressive strength, while the incorporated cellulose fibers ensure tensile strength. Tear-resistant, flexible fibers (cellulose) are thus interpenetrated by a dense and rigid polymer as a filler (lignin).
[0050] For the first time, the lignin contained in the component is used to create local densification points within the component, which are created by the forming of the component in the area of the holes. The lignin stabilizes the densification points because it reacts similarly to a thermoplastic.
[0051] The friction that occurs when the holes are made with the tool heats the material, causing the lignin to plasticize and harden again when it cools, thereby stabilizing the formed area again.
[0052] During or after the forming of the joint, neither the forming tool nor the fastener for forming the joint remain in use after the forming process is completed. The heavy-duty joint, including standard fasteners (engineering screws, washers, nuts), is then used to create the permanent, slip-resistant, preloaded connection.
[0053] The component according to the invention has at least one local axially and / or radially generated compaction point with a defined hole diameter, whereby the screw connection created on the component can withstand higher loads and settlement phenomena and internal stress relief in the area of the screw connection due to the local compaction points are reduced compared to conventional connections in which the components do not have compaction points. According to the method, the local hardening in the component is carried out by means of a corresponding tool that acts on the component from one direction or from two opposite directions. This is carried out with at least one rotating mandrel, which exerts a defined material-dependent force on the workpiece. This is achieved by the feed of the mandrel as a function of the rotation speed and the temperature occurring at the point of action.
[0054] Renewable raw materials are primarily used as materials, with the proportion of renewable raw materials being at least 50%. Wood-based materials are preferred, or wood-based materials in combination with a proportion of renewable raw materials <50%.
[0055] In particular, the material of the components consists predominantly of renewable raw materials such as wood-based materials, grass-based materials (bamboo) or hybrid materials such as wood-plastic composite (WPC) or wood-based materials with metallic layers, plastic layers, paper or cardboard layers as cover and / or intermediate layers or any combination of the aforementioned materials.
[0056] If wood materials are used, these are primarily components with a layered structure consisting of at least three interconnected layers. Such components are referred to as laminated wood.
[0057] The component is preferably made of laminated wood, especially plywood. Plywood is the more specific type of veneer, where the directional properties are enhanced by a grain orientation, particularly at 0°-90°, resulting in a blocking effect. However, other plywoods with orientations deviating from 0°-90° can also be used.
[0058] However, components made of bamboo or containing bamboo, or generally renewable raw materials containing lignin, can also be used.
[0059] The components are primarily plate-shaped, but can also be in other geometric shapes.
[0060] With regard to the surface of the component, an attack angle of the workpiece of 90° can preferably be used, but a different angle of the machining direction, such as up to 45°, can also be used.
[0061] The tool creates a nearly cylindrical hole, which can be a through hole or have a bottom. The area of local hardening, depending on the diameter D of the hole produced, is preferably up to five times the diameter for radial compaction and up to twenty times the diameter for axial compaction.
[0062] D is the forming tool diameter. The compression area is larger and depends on D (a multiple = 20x), the local area of influence of a created cylindrical hole. All processes take place within the defined local area of up to twenty times the diameter around the hole created with the punch.
[0063] It is possible to create the hole with the surrounding compaction point without pre-drilling or with pre-drilling.
[0064] For a diameter-to-plate thickness ratio (for a plate-shaped component) that does not require pre-drilling, the ratio is up to 1:2 (e.g., 10mm tool diameter, 20mm plate thickness). For a ratio of 1:4 to 10:1 between the diameter D of the hole to be created and the plate thickness, diameter-dependent pre-drilling should be performed.
[0065] The pre-drilled diameter should be 0.1 to 0.9 x D.
[0066] The temperature range at the point where the workpiece acts, i.e., at the point of action, should be between 0°C - 210°C, preferably 100°C - 150°C, particularly preferably 140°C. Particularly at temperatures above 100°C, the lignin contained in the material is plasticized in conjunction with the forming pressure acting on the material and solidifies again upon cooling.
[0067] The holes can be created with or without a counterholder. A counterholder is possible, for example, for single-sided and double-sided radial compaction processes, for single-sided or double-sided hole pressing, and / or combined compaction—axial and / or radial.
[0068] Preferably, the process is carried out without a hold-down device.
[0069] However, a hold-down device can also be provided on the side of the tool, which surrounds the tool and acts on the surface of the component with a hold-down force.
[0070] This can be the case with a one-sided compaction process, ie when only one tool is used to produce the hole, or with a two-sided radial compaction process, ie when two opposing tools act on the component, one mandrel on each side of the plate-shaped component.
[0071] Thus, the hold-down device can be used for one-sided / two-sided pressing and / or combined compaction.
[0072] With the solution according to the invention, when the holes required for a screw connection are made, local hardening is created in the component, which ensures a higher load-bearing capacity of the screw connection.
[0073] The invention is explained in more detail below using an embodiment and associated drawings.
[0074] They show: Figure 1 shows the principle of the process sequence for penetrating the component on one side with a mandrel, Figure 2 shows the principle of the process sequence for penetrating the component on both sides with two mandrels arranged opposite one another, Figure 3 shows the principle of a component with radial compression according to the invention, Figure 4 shows the principle of axial compression according to the invention over the entire connection cross-section of the component, Figure 5 shows the principle of generating radial and axial compression using a counterholder, Figure 6 shows the screw connection of two components 1 with axial and radial compression.
[0075] In Figure 1is the basic representation of the process sequence for the one-sided penetration of the component 1 with a tool which has a mandrel 2 or is designed as a mandrel 2 which has a longitudinal axis A2, shown in steps A to D. The component 1 is a multi-glued wooden panel (laminated wood) with a first side 1.1 and a second side 1.2 and a height h. The mandrel 2 has a cylindrical shaft 3 with a diameter D2, to which a tip 4 is connected in the direction of the component 1. The tip 4 is essentially conical in this case and has a cone angle a which is preferably between 15° and 20° (but the angle can also be larger or smaller).
[0076] In step A, the rotating mandrel 2 is moved with the tip 4 towards the top side 1.1 of the component 1, where it rests on the side 1.1 and is then pressed into the component 1 with a force F in the forward stroke, whereby the material of the component 1 is largely radially displaced and partially compacted according to step B. In step C, the mandrel 2 has penetrated the component 1 and a hole L has formed in the component 1 due to the displacement of the material. Local radial compactions V over the entire height h of the component 1 were generated around the hole L by the displacement of the material of the component 1. The mandrel 2 is then removed from the component 1 in a return stroke, preferably in a rotating manner according to step D in the direction of the arrow. The hole L created in the component 1 has a longitudinal axis A1 and a diameter d, whereby the diameter d corresponds to the diameter D2 of the mandrel 2.The local compaction V surrounding the hole L remains in the component 1 after the mandrel 2 has been removed, since it is stabilized by the thermoplastically reacting lignin in the forming area of the material.
[0077] It is also possible for the mandrel 2 to first partially penetrate into the component 1, to be retracted again and then to penetrate deeper into the component 1 again, thus performing an alternating forward and backward stroke movement until the mandrel 2 has completely penetrated the component 1.
[0078] Figure 2shows the basic representation of the process sequence with steps A to D for the two-sided penetration of the component 1 with two mandrels 2 arranged opposite one another, whose longitudinal axes A2 are aligned and which penetrate the component 2 alternately from both sides 1.1, 1.2, always with a feed rate, until the hole L has been completely formed in the component 1 (step C). According to step A, no rotating mandrel 2 has yet penetrated the component 1. In step B, the upper mandrel 2 has penetrated into the component 1 from the direction of the top side 1.1 of the component 1, but has not yet penetrated it. The upper mandrel 2 has retracted from the component 1 according to step C and the lower mandrel 2 has penetrated into the component 1 from the direction of the bottom side 1.2 of the component 1 and has completely penetrated it and created the hole L. The lower mandrel 2 was then also disengaged according to step D and the process is finished.
[0079] In the aforementioned examples, the mandrel 2 is inserted essentially at a right angle = 90° to the top side 1.1 or the bottom side 1.2 of the component 1. It is also possible to form the mandrel 2 into the component 1 at a different angle of inclination, thereby creating a hole L whose longitudinal axis A1 runs obliquely in the component.
[0080] It is also possible for the punch to be surrounded by a hold-down device which acts on the top or bottom side 1.1, 1.2 of the component 1 during the forming of the hole, depending on the direction from which the mandrel 2 acts.
[0081] The principle representation of a component 1 with a radial compression V according to the invention is shown in Figure 3 shown.
[0082] Here, a hole L with a diameter d was created in component 1 without pre-drilling. The radial compaction V of the material, which adjoins the hole L on the circumference, has a circumferential diameter dv of up to 5 x d. In the example shown, dv is approximately 2 x d.
[0083] According to Figure 4 it is also possible to generate only an axial compression V that extends over the entire connection cross-section of component 1.
[0084] The hole L was created by pre-drilling, and then the area of the hole L adjacent to the hole on the circumference was provided with the axial compaction V by an axially acting punch (not shown). The height hv of the compacted area V in the area of the hole L is approximately 0.5 x h.
[0085] Figure 5shows a schematic diagram of the generation of a radial and axial compression V using a mandrel 2 which has a shoulder 5 with a diameter D5 which is connected to the shaft 3 and a counterholder 6. First, in step A, the radial compression V was generated with the mandrel 2 and its tip 4 by the mandrel 2 penetrating into the component 1 from the direction of the top side 1.1 and completely penetrating it, so that the hole L with the diameter d was generated.
[0086] With a further feed, the shoulder 5 is pressed axially into the component 1 (see step B), so that in addition to the radial compression, an axial compression V of the material in the component 1 is generated from the direction of the upper side 1.1, whereby the height h of the component 1 in the area of the acting shoulder 5 is reduced to a height hv.
[0087] On the underside 1.2 of the component 1, there is a counterholder 6 at both stages, which has a bore 6.1 through which the mandrel 2 can engage.
[0088] A screw connection with axial and radial compression V is in Figure 6 Two components 1 rest against each other with their flat undersides 1.2 and are connected to each other by a screw 7 and a nut 8, with the screw 7 protruding through the aligned holes L of the components 1. A washer 9 is provided under the screw head 7.1 and under the nut 8.
[0089] The compacted area V in the two components 1 enables a higher prestress and reduces the settlement phenomena or relaxation and retadation phenomena. List of reference symbols
[0090] 1 Component 1.1 Top 1.2 Bottom 2 Mandrel 3 Shaft 4 Tip 5 Shoulder 6 Counterholder 7 Screw 7.1 Screw head 8 Nut 9 Washer aCone angle of the tip bPenetration angle of the mandrel dDiameter of the hole L dvCircumference of the compacted area hHeight of the component 1 hvHeight of the compacted area ALongitudinal axis D2Diameter of the mandrel that adjoins the tip 4 D5Diameter of the shoulder 5 FForce LHole VCompaction
Claims
1. Component made of a material which consists predominantly of renewable raw materials, - wherein the component (1) • consists of plywood or • is in the form of a panel and has at least three layers of renewable raw materials which are combined with further layers of material, wherein the component has one or more layers of material made of metal, plastic, fiber composite material, paper or cardboard or a combination of these layers of material, and - wherein the component has at least one hole (L) with a longitudinal axis (A1) serving to produce a connection by means of a screw connection with a further component in order to produce a connection by means of a screw connection and - wherein the material of the component (1) in the region adjoining the hole (L) on the circumferential side has a local compaction (V) which is produced by the penetration of a rotating mandrel and realizes a permanently slip-resistant pretensioned connection point for the screw connection, wherein the hole (L) is a cylindrical or almost cylindrical hole (L) and is formed as a through-hole in the component (1) or has a bottom, and wherein the region of the component (1) adjoining the hole (L) on the circumferential side has radial and / or axial local compactions (V) and wherein the hole (L) has a diameter (d) and - the circumference (dv) of the compacted region adjoining the hole (L) on the circumferential side is up to five times the diameter (d) and / or that the height (hv) of the compacted region is up to twenty times the diameter (d) and / or is reduced in comparison to the height (h) of the component (1).
2. Component according to claim 1, characterized in that the hole (L) is introduced into the component (1) at an angle (b) of 90° to 45° to the upper side (1.1) of the component (1).
3. Method for producing a component according to claim 1, characterized in that at least one mandrel (2) with a cylindrical shank (3) and a tip (4) which reduces in diameter in the direction of the component (1) penetrates into the material of the component (1) and thereby produces a hole (L) in the component (1) and displaces the material radially and / or axially, thereby producing a local compaction (V) in the region of the material surrounding the hole (L), wherein the mandrel (2) rotates at least during penetration into the component (1).
4. Method according to claim 3, characterized in that two mutually opposing mandrels (2) are used, which penetrate alternately into the component (1) from opposite directions and produce the hole (L) with the diameter (d), thereby displacing the material and compacting it in the region surrounding the hole (L), wherein both mandrels (2) rotate at least during penetration into the component (1).
5. Method according to claim 3 or 4, characterized in that a return stroke movement of the engaged mandrel (2) takes place and then a renewed forward stroke movement of the mandrel (2), during which the mandrel (2) penetrates further into the component (1) and / or in that, during a return stroke movement of a mandrel (2), a forward stroke movement of an opposite mandrel (2) into the component (1) takes place.
6. Method according to one of claims 3 to 5, characterized in that a maximum penetration depth of the mandrel (2) is determined as a function of - the component (1) and - a rotational speed of the mandrel (2) and / or - a feed speed of the mandrel (2), and in that the mandrel (2) performs a return stroke after reaching the penetration depth.
7. Method according to claim 6, characterized in that the rotational speed and / or the feed speed and / or the maximum penetration depth are determined empirically.
8. Method according to claim 6 or 7, characterized in that the maximum penetration depth is determined in such a way that a temperature acting on the component (1) due to the friction of the punch is at most 210°C.
9. Use of a tool in the form of a mandrel (2) having a cylindrical shank (3) and a tip (4) in a method according to claim 3.
10. Use of a tool according to claim 9, characterized in that the tip (4) is designed in the form of a conical tip, a truncated cone or in another form which reduces in diameter in the direction of the component (1) and the tool can be set in rotation by means of a first drive and can be moved in the direction of the longitudinal axis of the mandrel (2) by means of a second drive.
11. Use of a tool according to claim 9 or 10, characterized in that the mandrel (2) is heated and in that the tool has a temperature sensor if required.