Laminated luminous glazing including a functional coating
The laminated glazing system with optimized dielectric layer combinations addresses chromatic changes and intensity attenuation by minimizing absorption in guided mode, ensuring consistent luminosity and neutral aesthetics in automotive applications.
Patent Information
- Application Number
- FR2022005564
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-06-09
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-06-09
AI Technical Summary
Luminous glazing used in automotive applications faces issues with chromatic changes and light intensity attenuation due to high absorption of guided mode light by functional coatings, particularly at long wavelengths, leading to unsuitable optical properties and aesthetics.
A laminated glazing system with a functional coating comprising specific combinations of dielectric layers, optimized for low absorption in guided mode, particularly in the red, achieved by controlling the nature, thickness, and position of dielectric layers to minimize energy density and absorption.
The solution maintains consistent light intensity and color across the pattern, ensuring low emissivity and neutral aesthetics by minimizing absorption in guided mode, particularly in the red, thus preserving the luminous effect over the length of the pattern.
Smart Images

Figure 00000023_0000 
Figure 00000023_0001 
Figure 00000024_0000
Abstract
Description
Title of the invention: Laminated luminous glazing comprising a functional coating
[0001] The invention relates to the field of luminous glazing. Luminous glazing is glazing that emits light. It comprises a light source and a substrate having, on one of its principal faces, a light-extracting layer such as a diffusing layer forming a pattern. The light source is optically coupled to the substrate, for example, edge-on. The light injected at the edge of the substrate propagates within the substrate by total internal reflection. The substrate acts as a light guide.
[0002] According to the present invention, the mode of light propagation within the substrate by total internal reflection is called the "guided mode." The guided mode thus corresponds to the use of light at grazing incidence within a substrate. The critical parameter for the guided mode is the critical angle of total internal reflection. This corresponds to the angle with respect to the normal to the substrate above which any light ray arriving at a separating surface or interface, from a medium with a higher refractive index to a medium with a lower refractive index, is totally reflected by said surface or interface. The critical angle (0c) is determined by applying Snell's law. It corresponds to the angle (within the substrate) for which the light ray is refracted at 90° (into the medium with a lower refractive index than the substrate).
[0003] For luminous glazing, the surrounding medium can be air, another substrate, or a polymer interlayer. For example, the critical angle of total internal reflection at the interface between a glass substrate with a refractive index of 1.51 and air is approximately 40°. In the case of a glass / polyvinyl butyral (PVB) polymer interlayer interface, the critical angle is approximately 80°.
[0004] All light rays injected into the substrate having an angle of incidence: - above this critical angle are reflected and continue to propagate in the substrate, - below this critical angle, they are partially refracted and gradually exit the substrate.
[0005] In the case of luminous glazing, the light sources used are preferably light-emitting diodes (LEDs). The light is extracted at the level of the extraction layer, which allows the pattern to be illuminated.
[0006] There is a growing demand for luminous glazing for automotive applications, particularly for car roofs. However, this option is not compatible with most of the glazing traditionally used for these applications. In fact, automotive glazing must also have a low-emissivity function to reduce the amount of energy dissipated to the outside. The "low-emissivity" function or property corresponds to the ability of glazing to prevent heat from escaping by reflecting infrared radiation.
[0007] To this end, functional coatings exhibiting infrared (IR) reflective properties are used. In the following description, the term "functional" qualifying a coating or layer means "capable of acting on solar radiation and / or infrared radiation." For example, functional coatings may include a conductive oxide layer disposed between two dielectric coatings. Patent application WO2018 / 206236 is known in particular. This application discloses, starting from the substrate, functional coatings comprising: - a dielectric coating comprising dielectric layers such as silicon nitride and / or silicon oxide layers, - a functional layer based on a transparent conductive oxide (TCO) such as an indium tin oxide (ITO) layer, - a dielectric coating comprising dielectric layers such as silicon nitride and silicon oxide layers.
[0008] The absorption of visible light by the conductive oxide-based functional layers of these functional coatings is not negligible, particularly in the red region. However, the absorption of visible light at normal incidence remains low because the light passes perpendicularly through the conductive oxide-based functional layer. The interaction between the radiation and the functional layer occurs only over the thickness of the functional layer (ef).
[0009] The situation is different for guided-mode light. When functional coatings are placed close to the substrate in which guided-mode light propagates, the light propagating in the substrate is likely to interact with the functional layer. The interaction angles between the guided-mode light and the substrate are defined directly within the substrate into which the light is injected. The guided-mode rays are therefore largely grazing (0° greater than 80°) with respect to the normal to the substrate in which they propagate.
[0010] A ray from the guided mode therefore traverses the functional layer over a distance corresponding to: Thickness of the functional layer (ef) / cos (0). The more grazing the angle, the smaller cos (0), the greater the distance the rays from the guided mode interact with the functional layer, and therefore the greater the proportion of absorbed rays.
[0011] In conclusion, when the substrate in which the light propagates comprises or is in contact with a functional coating, a significant portion of the light enters contact with this functional coating at a grazing angle and is therefore likely to be absorbed when the functional coating includes absorbent layers.
[0012] This is why, depending on the injected light, we observe an alteration, a chromatic change, a decrease or even an erasure of the pattern as we move away from the point of light injection due to the high absorption in guided mode at grazing angles of the functional layer.
[0013] This problem is particularly pronounced at long wavelengths in the visible spectrum because the absorption of conductive oxide layers, and in particular of ITO, increases with wavelength. Therefore, in the case of luminous glazing, the guided-mode optical properties of the functional coating are crucial.
[0014] When using light sources emitting red light (red LEDs), guided-mode absorption of wavelengths corresponding to red results in a color (or brightness) that diminishes along the pattern (as one moves away from the light source). When using light sources emitting white light, guided-mode absorption of wavelengths corresponding to red results in a color that changes and a light intensity that diminishes along the pattern.
[0015] The applicant, aware of this phenomenon, became interested in controlling the distribution of electromagnetic energy in the stack using the interference effect. The objective is to minimize the energy density at the functional layer level and thus minimize absorption, particularly in the red region.
[0016] Indeed, the absorption of light energy in a coating, attributable to the presence of an absorbing layer, depends on both its thickness and the material it is made of, as well as its position within the coating. In particular, the local amplitude of the electric field at a layer of the coating depends on its position within the coating, which acts as an interference filter. The absorption of light energy varies proportionally to the square of the amplitude of this electric field. If the absorbing layer is located in a region of the coating where the amplitude of the electric field for a given wavelength is low, the absorption of that wavelength will be lower compared to a coating with the same absorbing layer located where the amplitude of the electric field is higher.
[0017] It is possible to selectively increase or decrease the absorption properties of a coating for certain wavelengths. To do this, it is possible to advantageously select the "position" of the absorbing layer by placing it at a location on the coating where the amplitude of the electric field for that wavelength is high or low. To select the most advantageous "position" from the point of view of absorption, it is possible to adjust the thickness and nature of the layers. electrical properties of the dielectric coatings surrounding the functional layer.
[0018] The applicant has therefore demonstrated that by selecting the nature and thicknesses of the dielectric layers constituting the dielectric coatings of the functional coatings, it is possible to selectively reduce absorption in the red in guided mode without harming other properties and functions, in particular low emissivity and aesthetics.
[0019] To achieve this goal, it was necessary to characterize the absorption of guided light by the functional coating. It is not possible to experimentally determine colorimetric parameters since guided mode exists only within the substrate. The inventors developed a specific optical model that allows for the simulation evaluation of a* and b* reflection values in guided mode at the substrate / functional coating interface. This reflection corresponds to an 80° angle of incidence in the glass substrate. These colorimetric parameters in guided mode are called Rgm, a*gm, and b*gm. Rgm corresponds to the total amount of light reflected at each reflection on the layer interface. Lower absorption in the red region in guided mode results in higher Rgm values and less negative, or even neutral, a*gm and b*gm values.A high Rgm parameter denotes low absorption and therefore better preservation of the guided mode in terms of its total intensity.
[0020] Thanks to this model, the applicant has thus succeeded in developing families of solutions meeting these criteria in the form of particular combinations of dielectric layers in dielectric coatings having specific thicknesses and optical indices.
[0021] The present invention therefore relates to a material comprising a substrate coated with a functional coating, intended to be implemented in luminous glazing, exhibiting low absorption in guided mode in the visible, particularly in the red when the glazing is illuminated, and thus making it possible to avoid any colorimetric drift over the length of the pattern.
[0022] The improvement stems from the precise control of optical interference effects between the different layers composing the coating. This control is achieved by choosing the nature, thickness, and sequence of dielectric layers constituting the dielectric coatings. This makes the functional coatings compatible with use in luminous glazing.
[0023] The invention relates to a material comprising a substrate coated with a functional coating comprising, starting from the substrate: - possibly a first dielectric coating located below the functional layer comprising: - a layer with a higher refractive index and an optical thickness between 0 and 110 nm and - a layer with a lower refractive index and an optical thickness between 0 nm and 170 nm, the higher refractive index layer, if present, has a higher refractive index than the lower refractive index layer, if present, and the variation in refractive index at 550 nm between these two layers is greater than 0.25, greater than 0.30, or greater than 0.40, - a functional layer based on a transparent conductive oxide (TCO), - a second dielectric coating located above the functional layer comprising: - a layer with a higher refractive index and an optical thickness between 80 and 170 nm and - a layer with a lower refractive index and an optical thickness between 80 and 190 nm, the higher refractive index layer has a higher refractive index than the lower refractive index layer and the variation in refractive index at 550 nm between these two layers is greater than 0.25, greater than 0.30, or greater than 0.40, the sum of the optical thicknesses of the first and second dielectric coating is greater than 200 nm.
[0024] Surprisingly, the best results in terms of low absorption in the red in guided mode, low emissivity and / or neutral aesthetics in transmission are obtained with a functional coating having the following characteristic(s): - the functional layer is chosen from fluorine-doped tin oxide, antimony-doped tin oxide and / or indium tin oxide, - the functional layer has a geometric thickness between 70 and 200 nm, between 75 and 150 nm, between 80 and 130 or between 90 and 110 nm, - lower refractive index dielectric layers of dielectric coatings have a refractive index of less than 1.7, less than 1.6, or less than 1.5, - Layers with a lower refractive index are silicon oxide-based layers, - the dielectric layers with a higher refractive index of the dielectric coatings have a refractive index greater than 1.9, or greater than 2.0, - The dielectric layers with the highest refractive index of each dielectric coating are chosen from: - Nitride-based layers of one or more elements selected from silicon, aluminum or zirconium, preferably silicon nitride-based, - zinc and tin oxide-based coatings, - zinc oxide-based or - titanium oxide-based coatings, - The dielectric layers with a lower refractive index in the dielectric coatings are either identical or different and are chosen from silicon oxide-based layers, - the dielectric layers with higher refractive index of the dielectric coatings are identical or different and are chosen from layers based on silicon nitride or zinc tin oxide.
[0025] The applicant has notably highlighted two particularly advantageous combinations exhibiting specific optical thickness ranges for each dielectric layer of the dielectric coatings. This means that by choosing a functional coating satisfying one of these combinations of ranges, it is possible to obtain a number of the advantageous properties sought by the invention. However, not every selection within these combinations makes it possible to obtain all the preferred properties of the invention.
[0026] According to a first preferred combination, the invention relates to a material of which: The dielectric coating located beneath the functional layer comprises: - a layer with a higher refractive index and an optical thickness between 0 nm and 20 nm, - a layer with a lower refractive index and an optical thickness between 0 nm and 25 nm, preferably between 10 and 20 nm, The dielectric coating located above the functional layer comprises: - a layer with a higher refractive index and an optical thickness between 100 nm and 140 nm, - a layer with a lower refractive index and an optical thickness between 80 and 140 nm.
[0027] According to the invention, the lower bound in the ranges "between 0 nm" means that the layer may be absent. The bound is therefore included.
[0028] According to another preferred combination, the invention relates to a material in which: the dielectric coating located below the functional layer comprises: - a layer with a higher refractive index of optical thickness between 40 nm and 110 nm or between 60 nm and 80 nm, - a layer with a lower refractive index and an optical thickness between 20 nm and 145 nm or between 75 nm and 105 nm, The dielectric coating located above the functional layer comprises: - a layer with a higher refractive index and an optical thickness between 80 nm and 170 nm or between 90 nm and 130 nm, - a layer with a lower refractive index and an optical thickness between 125 and 190 nm or between 150 and 165 nm.
[0029] According to this advantageous combination, the sum of the optical thicknesses of the first and second dielectric coating is greater than 300 nm, 350 nm, 380 nm or 400 nm.
[0030] The invention advantageously presents colors in reflection at 60° of low intensity.
[0031] The invention also relates to laminated glazing comprising a material according to the invention and at least one second substrate, the material and the second substrate are linked together via a lamination interlayer.
[0032] Conventionally, the faces of a glazing are designated from the outside by numbering the surfaces of the substrates from the outside towards the inside of the passenger compartment or room it equips. This means that the incident sunlight passes through the surfaces in ascending order of their number.
[0033] In the case of laminated glazing, all the faces of the substrates are numbered but the faces of the lamination interlayers are not numbered.
[0034] The laminated glazing according to the invention comprises a face 1 located on the exterior of the building or vehicle it equips, faces 2 and 3 in contact with the lamination interlayer, and a face 4 on the interior of the building or vehicle. The functional coating is preferably positioned on face 4.
[0035] The invention also relates to: - laminated glazing according to the invention mounted on a vehicle or building, and - the use of laminated glazing according to the invention as low-emissivity glazing for buildings or vehicles, - a building, a vehicle comprising glazing according to the invention.
[0036] The laminated glazing according to the invention is preferably automotive glazing such as automotive roof glazing.
[0037] The laminated glazing according to the invention may include curved substrates.
[0038] Laminated glazing may have a light transmission of less than 50%, less than 30%, less than 20% or less than 10%.
[0039] Laminated glazing may also have a light transmission greater than 60%, greater than 70%, or greater than 80%.
[0040] The invention also relates to a luminous glazing comprising a laminated glazing according to the invention, a light source optically coupled to form a light guide and a light extractor element to extract the guided light.
[0041] The light source is preferably peripheral.
[0042] The light source is preferably optically coupled to the substrate of the material according to the invention. Optical coupling can be achieved: - by the slice of the substrate of the material of the invention, - by a wall delimiting a hole, preferably a through hole, in the substrate of the material, Or - by redirecting light for example, the source can be on the F4 side (offset or opposite the F4 face) and a light redirecting element such as a prismatic reflector film is positioned on the F3 face.
[0043] The light-extracting element preferably a diffusing element, in particular a layered diffusing element forming a pattern.
[0044] The luminous glazing of the invention can be chosen from a side window, a rear window, a roof window or a windshield.
[0045] The preferred characteristics which appear in the following description are applicable both to the material according to the invention and, where applicable, to the glazing, the process, the use, the building or the vehicle according to the invention.
[0046] All the luminous characteristics described are obtained according to the principles and methods of ISO 9050 relating to the determination of the luminous and solar characteristics of glazing used in glass for construction.
[0047] Conventionally, refractive indices are measured at a wavelength of 550 nm.
[0048] According to the invention, two elements such as layers or substrates have substantially equal refractive indices, when the absolute value of the difference between the refractive indices of the two materials constituting said layers or substrates at 550 nm is less than or equal to 0.15.
[0049] Layers with a higher refractive index and layers with a lower refractive index have different refractive indices. According to the invention, two elements such as layers or substrates have different refractive indices, when the absolute value of the difference between the refractive indices of the two materials constituting said layers or substrates at 550 nm is greater than or equal to 0.25, greater than 0.30, greater than 0.40, greater than 0.50, greater than 0.60, greater than 0.70 or greater than 0.80.
[0050] The refractive indices are defined at the wavelength of 550 nm.
[0051] Unless otherwise stated, the thicknesses referred to in this document without further specification are physical, real, or geometric thicknesses denoted Ep and are expressed in nanometers (and not optical thicknesses). The optical thickness Eo is defined as the physical thickness of the layer in question multiplied by its refractive index at a wavelength of 550 nm: Eo = n*Ep. Since the refractive index is a dimensionless value, the unit of the optical thickness can be considered to be the same as that chosen for the physical thickness.
[0052] According to the invention, a dielectric coating corresponds to a sequence of dielectric layers, located between the substrate and the functional layer, or above the functional layer.
[0053] If a dielectric coating is composed of several dielectric layers, the optical thickness of the dielectric coating corresponds to the sum of the optical thicknesses of the different dielectric layers constituting the dielectric coating.
[0054] The functional coating is deposited by magnetic field-assisted sputtering (magnetron process). According to this advantageous embodiment, all coating layers are deposited by magnetic field-assisted sputtering. Unless otherwise specified, the terms "above" and "below" do not necessarily mean that two layers and / or coatings are in contact with each other. When it is specified that a layer is deposited "in contact" with another layer or coating, this means that there cannot be one (or more) layer(s) interposed between these two layers (or layer and coating).
[0055] In this description, unless otherwise indicated, the expression "based on", used to describe a material or layer as to what it contains, means that the mass fraction of the constituent it comprises is at least 50%, in particular at least 70%, preferably at least 90%.
[0056] According to the invention: - Light reflection corresponds to the reflection of solar radiation in the visible part of the spectrum. - Light transmission corresponds to the transmission of solar radiation in the visible part of the spectrum. - Light absorption corresponds to the absorption of solar radiation in the visible part of the spectrum.
[0057] The luminous characteristics are measured with respect to illuminant D65 at 2° perpendicular to the material mounted in single glazing (unless otherwise specified): - TL corresponds to the light transmission in the visible spectrum in % - Rc corresponds to the external light reflection in the visible spectrum as a percentage, observer on the functional coating side. - Rs corresponds to the internal light reflection in the visible spectrum as a percentage, observed on the side opposite to that containing the functional coating. - a*T and b*T correspond to the colors in transmission a* and b* in the L*a*b* system, - a*Rc and b*c correspond to the colors reflected a* and b* in the L*a*b* system, observer on the functional coating side. - a*Rs and b*Rs correspond to the colors in reflection a* and b* in the L*a*b* system, observer on the side opposite to that including the functional coating.
[0058] The parameters a*60° and b*60° correspond to the colors a* and b* in the L*a*b* system at an angle of 60° with respect to the normal to the plane of the glazing measured according illuminant D65 at 2° perpendicular to the material mounted in single glazing with the functional coating positioned on face 1, observer on the functional coating side.
[0059] The materials according to the invention make it possible to obtain on a clear glass substrate (single glazing): , - an emissivity of less than 30%, or even less than 20%, and / or, - a low Rs reflection, particularly less than 7%, and, - neutral colors in reflection and, - weak colors in angular reflection resulting in a 60° reflection of less than 17% and neutral colors.
[0060] Preferably, the material gives the glazing incorporating it colors in transmission and in external reflection or in internal reflection (single glazing) as defined below: , - values of a*Rc between -8 and 4, between -2 and 2, between -2 and 1.5, and / or, - values of b*Rc between -5 and +5, between -2 and 2, and / or, - values of a*Rc 60° between -8 and 6, between -2 and 1.5, and / or - values of b*Rc 60° between -8 and 8, between -2 and 2.
[0061] These properties are measured on ordinary clear glass. Ordinary clear glass 4 to 6 mm thick has the following luminous characteristics: - a light transmission between 87 and 91.5% - a light reflection of between 7 and 9.5%, - a light absorption of between 0.3 and 5%.
[0062] The parameters Rgm, a*gm and b*gm correspond to the reflection and the a* and b* colors in reflection in guided mode at the substrate / functional coating interface at an angle of 80° in the glass substrate.
[0063] In configurations using laminated glazing, the colorimetric properties are calculated with:
[0064] - materials comprising a substrate coated with a functional coating mounted in laminated glass, - laminated glazing comprises a material including a 2mm ordinary soda-lime glass substrate and another 2mm soda-lime glass substrate, the two substrates being separated by a 0.76mm Polyvinyl Butyral (PVB) lamination interlayer, - the functional coating is preferably positioned on face 4.
[0065] The functional coating preferably comprises a single functional layer.
[0066] Preferably, the functional coating is deposited on a flat glass and the assembly It is domed and tempered. This improves the emissivity of a TCO such as ITO. The functional coating can also be heated during deposition.
[0067] The dielectric layers are conventionally chosen from the base layers Oxide-based, nitride-based, or oxynitride-based layers. Oxide-based layers of one or more elements consist primarily of oxygen and very little nitrogen. Oxide-based layers include, in particular, at least 90% oxygen by atomic percentage relative to the oxygen and nitrogen in said layer. Nitride-based layers consist primarily of nitrogen and very little oxygen. Nitride-based layers include at least 90% nitrogen by atomic percentage relative to the oxygen and nitrogen in said layer. Oxynitride-based layers comprise a mixture of oxygen and nitrogen. Oxynitride-based layers include 10 to 90% (exclusive limits) nitrogen by atomic percentage relative to the oxygen and nitrogen in said layer.
[0068] The quantities of oxygen and nitrogen in a layer are determined as atomic percentages relative to the total quantities of oxygen and nitrogen in the layer considered.
[0069] The dielectric layers are conventionally chosen from: - layers comprising silicon, aluminum and / or zirconium, possibly doped with at least one other element, - zinc and tin oxide-based coatings, - titanium oxide-based coatings, - zinc oxide-based coatings.
[0070] The layers comprising silicon comprise at least 50% by mass of silicon relative to the mass of all the elements constituting the layer comprising silicon other than nitrogen and oxygen.
[0071] Layers comprising silicon can be selected from oxide-based, nitride-based or oxynitride-based layers such as silicon oxide-based layers, silicon nitride-based layers and silicon oxynitride-based layers.
[0072] Silicon oxide-based layers comprise at least 90% oxygen relative to the oxygen and nitrogen in the silicon oxide-based layer. Silicon nitride-based layers comprise at least 90% nitrogen relative to the oxygen and nitrogen in the silicon nitride-based layer. Silicon oxynitride-based layers comprise 10 to 90% (exclusive) nitrogen relative to the oxygen and nitrogen in the silicon oxide-based layer. Preferably, silicon oxide-based layers are characterized by a refractive index at 550 nm of 1.55 or less. Preferably, silicon nitride-based layers are characterized by a refractive index at 550 nm of 1.95 or greater.
[0073] The layers comprising silicon may comprise or be made up of elements other than silicon, oxygen, and nitrogen. These elements may be chosen from aluminium, boron, titanium, and zirconium. Layers comprising silicon may comprise at least 2%, at least 5% or at least 8% by mass of aluminium relative to the mass of all elements constituting the layer comprising silicon other than oxygen and nitrogen.
[0074] The layers comprising aluminium can be selected from oxide-based, nitride-based or oxynitride-based layers such as aluminium oxide-based layers such as A12O3, aluminium nitride-based layers such as AIN and aluminium oxynitride-based layers such as AlOxNy.
[0075] Among dielectric layers, a distinction is made, based on their refractive index at 550 nm, between low-refractive-index layers, intermediate-refractive-index layers, and high-refractive-index layers. Low-refractive-index layers have a refractive index below 1.70. Intermediate-refractive-index layers have a refractive index between 1.70 and 2.2. High-refractive-index layers have a refractive index above 2.2.
[0076] Low index coatings may have a refractive index of less than 1.70, less than 1.6 or less than 1.5. Low index coatings with a low refractive index are preferably silicon oxide-based coatings.
[0077] The intermediate refractive index layers can be selected from: - zinc oxide-based coatings (n550 = 2.0), - tin oxide-based layers (n550 = 2.0), - zinc and tin oxide-based layers (n550 = 2.0), - layers based on silicon nitride and / or aluminium (n550 = 2.1), - layers based on silicon oxynitride and / or aluminium.
[0078] High refractive index coatings may have a refractive index: - greater than 2.30, greater than 2.35 or greater than 2.40. - less than 2.60, less than 2.50, less than 2.40. High refractive index coatings can be chosen from: - titanium oxide-based coatings (n550=2.4), - layers based on a mixed oxide of titanium and another component chosen from the group consisting of Zn, Zr and Sn, - the layers based on a layer of zirconium nitride, - Silicon nitride and zirconium-based layers (n550 nm = 2.20 - 2.40), - Zirconium oxide-based layers, - layers based on manganese oxide MnO (n550 = 2.16), - layers based on a layer of tungsten oxide (n550 = 2.15), - layers based on a layer of niobium oxide (n550 = 2.30), - layers based on a layer of bismuth oxide (n 550 = 2.60).
[0079] The layer with a lower refractive index can be chosen from among the layers with a low refractive index. In this case, the layers with a higher refractive index are chosen from among the layers having a refractive index greater than 1.7. They are therefore chosen from among the intermediate refractive index layers and the high refractive index layers.
[0080] The layer with a lower refractive index can be chosen from among the layers with an intermediate refractive index. In this case, the layers with a higher refractive index are chosen from among the layers with a high refractive index.
[0081] The sum of the physical thicknesses of all the silicon-containing layers of each dielectric coating is greater than 50%, 60% or 70% of the total thickness of the dielectric coating under consideration.
[0082] The substrates may be mineral glass or transparent polymer material. The substrates are preferably mineral glass.
[0083] The mineral glass substrates that constitute the glazing can be made of soda-lime glass, aluminosilicate or borosilicate.
[0084] The substrates may be made of transparent polymer material which include poly(methyl methacrylate) (PMMA), polycarbonate (PC), polyurethane or polyurea (PU) substrates
[0085] Preferably, the lamination interlayers comprise one or more sheets of organic polymers.Organic polymers are selected from polyvinyl butyral (PVB), polyurethanes (PU), polyureas, ethylene vinyl acetate (EVA), polyolefins (including polyethylene (PE), polypropylene (PP), or polyisobutylene (P-IB)), polyvinyl chloride and its derivatives (e.g., poly(vinyl dichloride) (PVDC)), styrenic polymers (e.g., polystyrene (PS), acrylostyrene butadiene (ABS), styrene acrylonitrile (SAN)), polyacrylics (including polyacrylonitrile (PAN) and poly(methyl methacrylate) (PMMA)), polyesters (including poly(ethylene terephthalate) (PET) and poly(butylene terephthalate) (PBT)), polyoxymethylene (POM), polyamides (PA), and fluorinated polymers such as Polychlorotrifluoroethylene (PCTFE), polycarbonates (PC), aromatic polysulfones including polysulfone (PSU), polyphenylene ether (PPE), epoxies (EP) alone or in mixtures and / or copolymers of several of them. The lamination interlayer may be tinted.
[0086] Preferably the substrate material is clear and better extra clear to limit absorption.
[0087] The substrate can be an ultrathin glass, for example, with a thickness of less than 0.7 mm.
[0088] The substrate can be tempered (thermally).
[0089] The invention also relates to a luminous glazing comprising a laminated glazing according to the invention, a light extracting element, preferably a layer diffusing element and light sources.
[0090] The diffusing layer element can be in contact with or formed on the face of a substrate of the laminated glazing by a surface treatment such as sandblasting, by acid attack, by deposition of diffusing layer.
[0091] Examples of diffusing layer elements for acid-etched glass include SAINT-GOBAIN GLASS's Satinovo® glass and SAINT-GOBAIN GLASS's Smoothlite® diffusing glass.
[0092] The layered diffusing element can be formed within the mass of a substrate or interlayer, for example by a laser etching process. The layered diffusing element, in the form of a substrate or interlayer, is then attached to the surface of the substrate of the material according to the invention, for example by lamination.
[0093] The diffusing layer element can be placed on the substrate of the material according to the invention, in particular on the face opposite to that of the functional coating.
[0094] The layered diffusing element can be a self-supporting diffusing film, preferably bonded to a glazing substrate.
[0095] The diffusing layer may be a layer deposited on a substrate. The layer may be based on a diffusing enamel. It may be deposited discontinuously on one face of a substrate so as to form a pattern. The layer may be a diffusing ink printed on a substrate or an interlayer.
[0096] The diffusing layer may comprise an organic or mineral matrix and diffusing particles, for example, of a metal oxide such as titanium dioxide. An example of a transparent mineral diffusing layer is the transparent enamel as described in application FR3084355. An example of a transparent organic diffusing layer is the transparent layer as described in application WO2022023638.
[0097] The diffusing elements are placed at the desired locations for light extraction. It is thus possible to trace the path of light on the surface of the glazing by diffusing it through diffusing surfaces with well-defined areas and contours, according, for example, to geometric patterns or even text.
[0098] The layer diffusing element can be opaque or transparent.
[0099] The diffusing layer may comprise a matrix (organic or mineral) and diffusing particles, for example of metal oxide (TiO2 etc).
[0100] As an example of a transparent mineral diffusing coating, transparent enamel as described in application FR3084355 may be cited.
[0101] As an example of an organic transparent diffusing layer, one can cite the transparent layer as described in application WO2022023638
[0102] The laminated glazing may include a masking layer of opaque material (in particular black) preferably on the main inner face (interlayer side) of the second substrate (face 2). This peripheral layer forms a frame and defines a clear From a visual standpoint, the light source is preferably masked from the outside, notably by the masking layer. This layer can be an enamel located on the second glass substrate or an ink located on the interlayer.
[0103] The light source capable of emitting light is preferably an electroluminescent element such as light-emitting diodes (LEDs). The light source may be polychromatic (white light) or monochromatic, in particular red.
[0104] The light source can be linear such as a strip of diodes.
[0105] The light source can be coupled directly to the substrate material or via a guide, a collimation optic
[0106] The light source is preferably optically coupled to the substrate of the material according to the invention. The optical coupling can be achieved: - by the slice of the substrate of the material of the invention, - by a wall delimiting a hole, preferably through, in the substrate of the material, or - by redirecting light for example, the source can be on the F4 side (offset or opposite the F4 face) and a light redirecting element such as a prismatic reflector film is positioned on the F3 face.
[0107] The light source may be located opposite or near the edges of the substrate to be coupled by the edge of the substrate. Reference may be made to patent application WO2010049638.
[0108] The light source can also be placed in a hole made in the glazing (circular or oblong). Reference may be made to patent applications WO2013110885 and WO2018178591.
[0109] The light source may be located nearby, for example on face 4 (offset or opposite face 4), and a light redirection element such as a prismatic reflector film is positioned to redirect the light (for example on face 3). Reference may be made to patent application WO2022096365.
[0110] Several light sources can be used, for example near opposite edges of the substrate.
[0111] The diodes can be front-emitting or side-emitting. The diodes are preferably surface-mounted components on a substrate with electroconductive tracks such as a printed circuit board (PCB), for example, a rectangular substrate.
[0112] When the glazing is used as a rear window, the light source preferably emits in the red range. When the glazing is used as a rear window or as a windscreen, the design may be a pictogram such as a warning triangle. Example I. Materials and coatings
[0113] In these examples, the glass substrates are aluminosilicate type glass substrates. The interlayers for the laminates are made of polyvinyl butyral. (PVB) of 0.76 mm. The functional layers (F) are layers of tin and indium oxide. Dielectric coatings include: - layers based on silicon nitride (Si3N4, n550 = 2.0), - layers based on silicon oxide (SiO2, n550 = 1.5). The conditions for the deposition of the layers, which were deposited by sputtering (so-called "magnetron cathode sputtering"), are summarized in Table 1.
[0114] [Tables 1] Target Coating Used Deposition Pressure Gas ITO In2O3 90%, SnO2 10% wt 2.103 mbar Ar / (Ar + O2) at 99% SiO2 Si:Al at 92:8% wt 2.103 mbar Ar / (Ar + O2) at 62.5% Si3N4 Si:Al at 92:8% wt 3.2103 mbar Ar / (Ar + N2) at 55%
[0115] Table 2 lists the materials and physical thicknesses in nanometers (unless otherwise indicated) of each layer or coating that constitutes the coatings according to their position with respect to the substrate carrying the stack (last line at the bottom of the table).
[0116] [Tables2] [ tx î Ex 2 EX4 8x5 Cpl “ A g fe :.'.4 i Ep ia? ...............:........... ----------------- to i F. Sa 62 "T % 93 1 ? E. Eh 63 im 100 i - go jm §3 i lîO 74 î ' i isè 57 iœ i - 04 E- ® i 75 ai 18 F, §5 97.5 r 3-' 103 i - w Si©; î o 0 5 7.5 26 32 54 i 81 17 i 35.5 10 i 15 RD W $ S 0 0 43 î 86 33 i 36 i 72 30 î 88 15 j 30 Ep. TerRD | g Ep. 2^ RO | 14 j J Eiû RO pt RD ' rAyeteine \ asc J 232 e®1; 11? - 20 3 •V n î: F- gag ■© '2' >8 OS» -T ,57 ISS i 265.5 i 1 / 3 l 29ES i 151 I 270 i SS i 93 2?f 25 IR '3 uche *ûf"t enne * H Eoa wi» qc"1-' et "lp SS :! 1275 - Prt ■ Optical thickness; Thickness. II. Illustration of the attenuation phenomenon
[0117] Figures 1 and 2 each represent photographs of luminous glazing illuminated respectively from above by blue light-emitting diodes ([Fig.1]) and red ([Fig.2]). In each photograph, the glazing on the left includes a functional coating of the earlier art Cp-2 and the glazing on the right does not include a functional coating. When blue LEDs are used, the pattern is visible on both panes of glass. However, the pattern remains less bright when the glass also has a functional coating. When red diodes are used, the pattern quickly becomes invisible on the left pane of glass. Figure 3 shows a photograph of a luminous glazing unit comprising a Cp-2 prior art functional coating illuminated from above and in the center by white LEDs (element S). It includes a diffusing layer in the form of dots. Light is injected from above and extracted along the propagation path by the diffusion points. In this photograph, only the twelve framed points (element A) appear white. All the others appear cyan, a color that oscillates between blue and green, with the blue-green intensity increasing with distance from the injection point.
[0118] III. Characterization of the effect of guided mode absorption
[0119] The Rgm, a*gm and b*gm values in guided mode reflection at the substrate / interface Functional coatings have been determined. This reflection corresponds to an angle of incidence of 80° in the glass substrate. By definition of guided mode, where the propagation angle is greater than the critical angle of the system, light cannot be transmitted through the coating. What is not reflected is therefore absorbed. According to the invention, it is very useful to have the highest possible Rgm value because this parameter denotes low absorption. Indeed, the conservation of energy in a guided mode requires Rgm + Agm = 1, where Agm is the absorption of the guided mode. Low absorption results in high Rgm values. A high Rgm value indicates both lower absorption, particularly in the red region of the guided mode, and better preservation of the guided mode in terms of its total intensity. The parameters a*gm and b*gm indicate the change in colorimetric parameters of light at reflection, for a white incident light, of the type of illuminant D65. A positive a*gm means that the reflection becomes redder than the incident ray. A negative a*gm means that the reflection becomes greener than the incident ray. A positive b*gm means that the reflection becomes yellower than the incident ray. A negative b*gm means that the reflection becomes bluer than the incident ray. A reflection of a certain color indicates light absorption of the complementary color. Thus, for example, a negative a*gm is synonymous with green reflection. and absorption in the red. The higher the absolute values of the parameters a* and b*, the more pronounced the color of the reflections / absorptions will be. According to the invention, we are looking for less negative, or even neutral, values of a*gm and b*gm. A functional coating is particularly suitable for use in luminous glazing if: - the values of a*gm are between -4 and 2, and - the values of b*gm are greater than -2. However, this must be considered in relation to the Rgm values. As explained above, a high Rgm value indicates low absorption. Therefore, it can be advantageous to have structures with high Rgm values even if the associated a*gm and b*gm values are higher in absolute terms, as these colors will be less intense.
[0120] Table 4 summarizes the optical properties.
[0121] [Tables4] Tab.4 Ex.l Ex.2 Ex.3 Ex.4 Ex.5 Cp.l Cp.2 TL 89.8 86.3 88.6 90.3 87.2 89.3 88.5 a*T -0.9 0.1 -0.6 -0.8 0.5 -0.4 -0.2 b*T 0.0 -0.2 0.1 1.1 0.7 2.7 0.6 RLc 5.4 9.1 6.1 4.7 7.4 7.1 6.9 a*c 0.0 -5.1 -1.8 -0.1 -8.4 -1.5 -4.0 b*c 2.6 2.8 2.0 -5.4 -2.2 -11.0 -0.8 Rgm 96.0 95.5 91.9 94.7 91.7 90.9 90.9 a*gm -2.8 -3.2 1.0 -1.9 -0.1 -4.0 -5.3 b*gm 0.4 -0.2 1.8 6.2 0.7 -3.4 -3.5
[0122] Prior art coatings of type Cp.1 and Cp.2 cannot be used in luminous glazing because they do not exhibit sufficiently stable color in the substrate under guided light conditions. Their Rgm values are lower than the Rgm values of the examples according to the invention. Furthermore, their a*gm and b*gm values are too negative. This explains why, when the light source is a red light, we quickly observe an extinction of this red light as we move away from the point of light injection ([Fig.2], left photograph). The functional coatings of the invention exhibit: - Ex.1, Ex.2 and Ex.4: very high Rgm values and values a*gm and b*gm less negative than that of Cp. 1 and Cp. 2, - Ex.3 and Ex.5: high Rgm values and neutral a*gm and b*gm values. II. Configurations
[0123] Figure 4 illustrates a luminous laminated glazing according to the invention. It comprises: - a material according to the invention (1) comprising a functional coating (2) located on face 4 of the laminated glazing, - a lamination interlayer preferably made of PVB (3), - a second glass substrate (4), - a diffusing element in a layer forming a pattern (5), - a light source capable of injecting light into the substrate.
Claims
Claims
1. Material comprising a substrate coated with a functional coating comprising, starting from the substrate: - optionally a first dielectric coating located below the functional layer comprising: - a layer of higher refractive index with an optical thickness of between 0 and 110 nm and - a layer of lower refractive index with an optical thickness of between 0 nm and 170 nm, the layer of higher refractive index, if present, has a refractive index higher than that of the lower refractive layer, if present, and the variation in refractive index at 550 nm between these two layers is greater than 0.25, - a functional layer based on a transparent conductive oxide,- a second dielectric coating located above the functional layer comprising: - a layer of higher refractive index with an optical thickness of between 80 and 170 nm and - a layer of lower refractive index with an optical thickness of between 80 and 190 nm, the layer of higher refractive index has a refractive index higher than that of the lower refractive layer and the variation in refractive index at 550 nm between these two layers is greater than 0.25, the sum of the optical thicknesses of the first and second dielectric coatings is greater than 200 nm.,
2. Material according to claim 1 characterized in that the functional layer is chosen from fluorine-doped tin oxide, antimony-doped tin oxide and / or indium tin oxide.
3. 3. Material according to any one of the preceding claims characterized in that the dielectric layers of lower refractive index of the dielectric coatings have a refractive index of less than 1.
7.
4. Material according to the preceding claim, characterized in that the layers of lower refractive index are layers based on silicon oxide.
5. 5. Material according to any one of the preceding claims, characterized in that the dielectric layers of refractive index Higher dielectric coatings have a refractive index greater than 1.
9.
6. Material according to any one of the preceding claims, characterized in that the dielectric layers of higher refractive index of each dielectric coating are chosen from: - layers based on nitride of one or more elements chosen from silicon, aluminum or zirconium, preferably based on silicon nitride, - layers based on zinc and tin oxide, - layers based on zinc oxide or - layers based on titanium oxide.
7. 7. Material according to any one of the preceding claims, characterized in that: the dielectric coating located below the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 0 nm and 20 nm, - a layer of lower refractive index with an optical thickness of between 0 nm and 25 nm, the dielectric coating located above the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 100 nm and 140 nm, - a layer of lower refractive index with an optical thickness of between 80 and 140 nm.
8. 8. Material according to any one of claims 1 to 6 characterized in that the dielectric coating located below the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 40 nm and 110 nm, - a layer of lower refractive index with an optical thickness of between 20 nm and 145 nm, the dielectric coating located above the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 80 nm and 170 nm, - a layer of lower refractive index with an optical thickness between 125 and 190 nm.
9. Material according to the preceding claim, characterized in that the sum of the optical thicknesses of the first and second dielectric coatings is greater than 300 nm.
10. 10. Material according to claim 8 or 9 characterized in that: the dielectric coating located below the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 60 nm and 80 nm, - a layer of lower refractive index with an optical thickness of between 75 nm and 105 nm, the dielectric coating located above the functional layer comprises: - a layer of higher refractive index with an optical thickness of between 90 nm and 130 nm, - a layer of lower refractive index with an optical thickness of between 150 and 165 nm.
11. Laminated glazing comprising a material according to any one of claims 1 to 10 and at least one second substrate, the material and the second substrate are bonded together by means of a lamination interlayer.
12. Laminated glazing according to the preceding claim, characterized in that it comprises a face 1 located outside the building or vehicle which it equips, faces 2 and 3 in contact with the lamination interlayer and a face 4 inside the building or vehicle, the functional coating is positioned on face 4.
13. A luminous glazing comprising a laminated glazing according to any one of claims 11 to 12, a light source optically coupled to form a light guide and a light extracting element for extracting the guided light.
14. Luminous glazing according to the preceding claim characterized in that the extractor element is a diffusing element in a layer forming a pattern.
15. Luminous glazing according to the preceding claim chosen from a side window, a rear window, a roof window or a windshield.