Infrared transmittance silicon membrane and its manufacturing process.

A porous n-doped silicon membrane with specific pore characteristics and manufacturing process addresses the opacity issue of aluminum oxide membranes, enabling efficient infrared transmission for microorganism characterization and analysis.

FR3137758B1Active Publication Date: 2024-09-20COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022007005
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-07-08
Publication Date
2024-09-20
Estimated Expiration
2042-07-08

AI Technical Summary

Technical Problem

Existing porous membranes, such as those made of aluminum oxide, are opaque to infrared wavelengths above 10 um, limiting the acquisition of information for characterizing microorganisms and other infrared-based analyses.

Method used

A porous n-doped silicon membrane with pores extending through its thickness, each with a diameter less than or equal to 400 nm and a slenderness ratio greater than or equal to 20, allowing for infrared transmittance between 5 um and 25 um, is manufactured using an electrochemical etching process with specific conditions including high hydrofluoric acid concentration and illumination.

Benefits of technology

The membrane achieves transmittance greater than 5% for wavelengths between 5 um and 25 um, enabling effective infrared radiation transmission for microorganism characterization and analysis.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000016_0000
    Figure 00000016_0000
  • Figure 00000016_0001
    Figure 00000016_0001
  • Figure 00000017_0000
    Figure 00000017_0000
Patent Text Reader

Abstract

Infrared transmittance silicon membrane and its manufacturing process. Fluidic transfer membrane (84) comprising a porous wall (82) of n-doped silicon having pores (54) extending through its thickness, each pore having a diameter less than or equal to 400 nm and a slenderness ratio greater than or equal to 20. Figure for the abstract: Fig. 9
Need to check novelty before this filing date? Find Prior Art

Description

Description Title of the invention: Silicon membrane with high transmittance in infrared and its manufacturing process.

[0001] — The present invention relates to the creation of a porous structure with high slenderness ratio for the manufacture of a porous membrane for the transfer of a fluid and capable of transmitting infrared radiation, particularly for the purpose of measuring a physical quantity in the infrared characteristic of an object or organism alive.

[0002] — In the field of life sciences and environmental sciences, it is known to characterize vibration modes or to measure absorption spectra in the infrared to, for example, discriminate healthy tissues from pathological tissues logical, locate tumors on histopathological samples, identify pathogenic elements in a tissue, or to quantify inde- undesirable substances such as pesticides or endocrine disruptors.

[0003] It is known, for example, from FR 3 108 983 A1, to characterize colonies of mid- organisms grown on an aluminum oxide membrane, using a Infrared radiation and transmission through the membrane. Such a membrane is porous and transfers the nutrient medium to microorganisms in the pores that penetrate its thickness. However, aluminum oxide is completely opaque to infrared wavelengths above 10 µm, which limits the the amount of information that can be acquired to characterize the colony.

[0004] — The invention therefore aims to provide a new membrane for transferring a fluid, for example water, alcohol, or a nutrient medium for culturing microorganisms, and which exhibits infrared transmittance over a range of wavelengths more extensive than an alumina membrane, as well as a manufacturing process for a such a membrane.

[0005] — The invention relates to a fluidic transfer membrane comprising a wall porous n-doped silicon having pores extending throughout its thickness, each pore having a diameter less than or equal to 400 nm and a ratio with a slenderness ratio greater than or equal to 20.

[0006] — The membrane thus transmits radiation over a wider range of wavelengths extended than an alumina membrane. Preferably, the membrane exhibits a trans- mittance greater than 5% to any radiation whose wavelength is between between 5 µm and 25 µm.

[0007] — Preferably, the membrane has a transmittance greater than or equal to 10%. or even greater than or equal to 20%, better yet greater than or equal to 30% at any radiation with a wavelength between 5 µm and 25 µm. The membrane can exhibit a transmittance greater than or equal to 20% to any radiation with a wavelength between 10 µm and 25 µm. Preferably, each pore has a diameter less than or equal to 350 nm and / or greater than or equal to 50 nm. Preferably, the pores have a slenderness ratio greater than or equal to 50, better greater than or equal to 100. Preferably, the pores extend transversely between the faces of the wall on which they open, i.e. substantially perpendicular to said faces. The shape of the pores is not limiting. Pores can have a variety of shapes, including tubular, for example cylindrical of revolution. The pores may have a diameter that varies along their axis of extension between the openings through which they open, preferably by no more than 100% in absolute value. In particular, the pores may have lateral faces that undulate along their axis of extension between the openings through which they open. Preferably, the length of each pore is greater than or equal to 10 µm, preferably greater than or equal to 30 µm, better greater than or equal to 50 µm. The openings of the pores can be of various shapes. In particular, they can be convex, especially polygonal, for example square, elliptical, circular or cross-shaped. Preferably, the surface pore density is between 0.1 µm” and 5.0 µm”. The porous wall may have a thickness greater than or equal to 10 µm, preferably greater than or equal to 30 µm, better greater than or equal to 50 µm. The porous wall is doped n, for example with phosphorus. Preferably, the membrane has a general shape of a plate, preferably flat, extending between two large faces. The membrane can have a length ranging from 20 µm to 90 mm. For example, it is adapted to the characteristics of an infrared analysis device, for example the beam size, on which it is mounted. The membrane may consist of the porous portion. In a preferred variant, the membrane further comprises a support superimposed on the porous wall, which includes at least one recess extending through the support and at least one pore opening into the recess. The support thus provides rigidity and mechanical strength to the membrane, facilitating its gripping and handling. Preferably, the substrate and the porous wall extend in parallel planes. The thickness of the substrate can be between 100 µm and 3 mm, in particular less than or equal to 11 mm. The support may contain, or even be made of, silicon. It may be made of same material as the porous wall. The support can be in contact with the porous wall. The substrate can be bonded to the porous wall. It can be bonded using a direct hydrophobic bonding technique, such as silicon-on-silicon bonding. Alternatively, it can be bonded using a hydrophilic surface bonding technique, for example, with silicon oxide. The surfaces can be deposited, prepared by nitrogen or oxygen plasma activation, or by a chemical-mechanical polishing process. Bonding can also involve other types of materials, such as organic polymers or metallic materials. Preferably, the support is dense, i.e. it has a total porosity of less than 0.1%, the total porosity of the support being equal to the ratio of the total volume of pores of the support divided by the volume of the support. The support and the wall can form a monolithic unit. The invention also relates to a method for manufacturing the membrane according to the invention, the method comprising: - The supply of an n-doped silicon substrate having an electrical resistivity between 1 Q.cm and 10 Q.cm, and an electrochemical cell comprising an electrical generator, a cathode and an anode electrically powered by the electrical generator, the electrochemical cell containing an aqueous electrolyte comprising hydrofluoric acid in a mass concentration greater than or equal to 10%, the substrate being positioned between the anode and the cathode, at least one face of the silicon substrate being in contact with the electrolyte, the cathode and the face of the silicon substrate opposite the cathode, called the "front face", being in contact with the electrolyte, the front face of the silicon substrate being distant from the cathode, - electrochemical etching of the substrate by applying a constant electrical voltage of 10 V or greater between the anode and cathode with an electrical generator, in order to form blind pores in the substrate, each with a diameter of 400 nm or less, extending from one face of the substrate to a depth of 10 jm or greater, the back face of the substrate being illuminated during the electrochemical etching with light radiation in order to generate charge carriers in the substrate, and - the removal of part of the substrate so that said pores are open and pass through at least a portion of the substrate from one side to the other in its thickness. The process according to the invention thus makes it possible to manufacture a membrane in which the pores have a diameter less than or equal to 400 nm, preferably between 50 nm and 350 nm. Such pores, having a size more than ten times smaller than Infrared radiation wavelengths between 5 µm and 25 µm do not substantially scatter or diffract this radiation, which can thus be easily transmitted through the membrane. Furthermore, the implementation of the process according to the invention allows for the rapid production of the membrane with a pore etching rate preferably greater than 4 µm / min. Preferably, the substrate has an electrical resistivity between 3 Ω2.cm and 6 Ω.cm. The aqueous electrolyte is a liquid. Preferably, it has a hydrofluoric acid mass concentration greater than or equal to 15%, preferably greater than or equal to 25%, preferably greater than or equal to 30%, and preferably greater than or equal to 35%. The hydrofluoric acid mass concentration of the aqueous electrolyte may be less than or equal to 50%. The aqueous electrolyte can be obtained by diluting in an aqueous solvent, in particular water, at least one compound chosen from hydrogen fluoride, ammonium fluoride and mixtures thereof, The aqueous electrolyte may also contain an additive, such as isopropanol and / or acetic acid. The anode and / or cathode can be metallic, for example platinum. Alternatively, the anode and / or cathode can be silicon. The process may involve, prior to electrochemical etching, illumination of the substrate with light radiation in order to generate charge carriers in the substrate. Prior to electrochemical etching, the substrate can have a thickness of between 100 µm and 3 mm, for example between 500 µm and 1.5 mm. The substrate may have an (100) or (111) orientation parallel to a normal to one of its faces. It preferably has the shape of a flat plate. Preferably, the cathode has a substantially flat face that is entirely superimposed on the front face of the substrate. Preferably, the face of the cathode opposite the front face of the substrate and said front face are parallel. According to one variant, the anode is at a distance from the "back face" of the substrate, which is opposite the front face of the substrate. Preferably, the anode is not superimposed on the "back face" of the substrate. The electrolytic cell can be divided into first and second sealed chambers, which are sealed by the substrate. The first chamber contains the electrolyte, while the second chamber contains either the electrolyte or another aqueous electrolyte. The front and rear faces of the substrate define a wall of the first chamber and a wall of the second chamber, respectively. Because the first and second chambers are sealed, the liquids within them do not mix. Furthermore, in order to illuminate the rear face of the substrate, the electrochemical cell may include a window transparent to the illumination radiation, which delimits the second chamber. The substrate can be fully immersed in the electrolyte. The back face of the substrate, opposite the front face, is then in contact with the electrolyte. Each of the first and second chambers contains the electrolyte. Alternatively, the second chamber can contain a different aqueous electrolyte than the one in the first chamber. This other electrolyte could be, for example, an aqueous solution of potassium sulfate (K₂SO₄). According to a second variant, the anode is in contact with the back face of the substrate and partially covers the back face of the substrate. The substrate is preferably illuminated with light radiation having an energy greater than 1.1 eV. For example, it is produced by one or more halogen lamps with a luminous power greater than or equal to 500 lumens. Electrochemical etching is performed at a constant electrical voltage, i.e., in potentiostatic mode. Preferably, it is carried out at a constant electrical voltage between 25 V and 100 V. Preferably, the electrochemical etching is carried out until the pores extend each, from one face of the substrate to a depth greater than or equal to 30 µm, preferably greater than or equal to 50 µm, or even greater than or equal to 75 µm. Preferably, the portion of the substrate that is ablated extends from the face of the substrate opposite the face on which the blind pores open to the bottom of the blind pores. Prior to the ablation step, the process may include a mechano-chemical polishing of the substrate face on which the blind pores open, in order to abrade a surface layer of nanoporous silicon with a thickness between 50 nm and 1 µm, formed on said face during electrochemical etching. Furthermore, removal can be carried out by mechanical polishing, wet chemical etching and / or dry deep etching. Preferably, the ablation is selective in order to extract only a part of the portion of the substrate overlying the blind pores, preferably to form at least one recess through which at least one, preferably several of the pores open. Preferably, selective ablation involves deep etching of the substrate. Deep etching involves applying a protective mask, preferably by photolithography of a photosensitive resin, to the surface of the substrate opposite the surface through which the blind pores open. The protective mask includes at less a window passing completely through its thickness. Deep etching can be chemical and involve contacting the surface of the substrate covered by the protective mask with a chemical ablation agent, for example, an aqueous composition based on hydrofluoric acid, so as to remove material from an area of ​​the substrate superimposed on the window(s). Alternatively, deep etching can be physical and involve ablation of material in an area of ​​the substrate superimposed on the window(s) by bombarding the surface of the substrate covered by the protective mask with a plasma. The plasma can consist of an ionized reactive gas, in particular a fluorinated gas, for example, selected from SF4, CF4, and mixtures thereof. Preferably, prior to the ablation step, the process may include the deposition of a protective layer, preferably composed of at least one oxide, in particular silicon dioxide, for example deposited by chemical vapor deposition (CVD) from tetraethyl orthosilicate (TEOS) or SiH₂ (silane), on the surface of the substrate where the support is exposed. The process may further include the removal of the protective layer after the ablation step. The process may include further treatment of the membrane, for example a functionalization treatment, to make the membrane hydrophilic or hydrophobic, in order to facilitate the diffusion of specific chemical species. The invention also relates to a membrane obtained by the process according to the invention. The invention also relates to a method for characterizing a colony of microorganisms, comprising: - the culture of microorganisms in a nutrient medium, the microorganisms being arranged on one face of a membrane according to the invention and / or obtained by the process according to the invention, the membrane being in contact with the nutrient medium such that the nutrient medium is transferred through the pores to the microorganisms, - the illumination of microorganisms in transmission through the membrane by light radiation having at least a wavelength between 5 µm and 25 µm and the acquisition of the light radiation having interacted with the microorganisms. The "transmittance" T of a body of incident radiation of wavelength λ is equal to the ratio of the intensity I of the transmitted radiation of wavelength λ to the intensity I of the incident radiation, i.e.: [Math.1] T=#£ Ah Transmittance T can be measured by infrared spectrometry. The "slenderness ratio" of a pore is equal to the ratio of the pore length to the diameter of the pore. The "diameter" of a pore is equal to the average of the diameters of the pore openings on the two opposite faces of the wall onto which the pore opens, or, if the pore is blind, the diameter of the pore is equal to the diameter of the opening through which it opens. The diameter of the opening of a pore is equal to the diameter of the smallest circle circumscribed about the opening of said pore. The "length" of a pore is the distance between the openings through which the pore opens onto the opposite faces of the wall, or if the pore is blind, the distance between the opening through which the pore opens and the bottom of the pore. The pore surface density is determined on one face of the wall or substrate, as applicable. It is equal to the ratio of the total area occupied by the pore openings on a given area of ​​the wall or substrate face, respectively, to the area of ​​that area. Preferably, the area of ​​that area on which the pore surface density is determined is between 2 µm and 500 µm. The "resistivity" of the substrate is measured using the four-point method. The "mass concentration" of hydrofluoric acid in the aqueous electrolyte corresponds to the ratio of the mass of hydrofluoric acid in the aqueous electrolyte to the mass of the aqueous electrolyte. The "etching speed" of the pores is equal to the ratio of the length of a pore to the duration of the etching step. The "anode" is an electrode where an oxidation reaction occurs in the electrochemical sense, i.e. an electronic transfer from the electrolyte to the electrode, or a transfer of holes from the electrode to the electrolyte. The "cathode" is an electrode where a reduction reaction occurs in the electrochemical sense, i.e. an electronic transfer from the electrode to the electrolyte. The invention will be better understood by reading the detailed description and the drawing that follows, in which: [Fig.1] represents an example of an electrochemical cell for the setting in work of the process according to the invention, [Fig.2]. [Fig.3a], [Fig.3b], [Fig.4], [Fig.5], [Fig.6], [Fig.7], [Fig.8] and [Fig.9] are photographs acquired by scanning electron microscopy of engraved substrates of examples 1 to 4 and 6 to 9 respectively, [Fig.10] represents the evolution of the transmittance of different substrates in function of wavelength, [Fig.11] and [Fig.12] are photographs acquired by electron microscopy. Scanning electronics of the etched substrates of examples 10 and 11 respec- actively, [Fig. 13] represents the evolution of substrate transmittance in the examples 10 and 11 depending on the wavelength, [Fig.14] schematically represents the steps involved in creating a membrane according to an example of implementation of the process, and [Fig. 15] illustrates another example of an electrochemical cell for the setting in implementation of the process according to the invention. The scientific literature is abundant regarding the fabrication of silicon membranes for multiple applications, as summarized, for example, in the journal article "Porous silicon membranes and their applications: Recent advances," R. Vercauteren et al., Sensors and Acuators, A318 (2021), 112486. For example, the articles - “Thick macroporous membranes made of p-type silicon”, J. Zheng et al, Phys. Status, Solidi. A, vol. 202, no. 8, pages 1402-1406 (2005), - “Integration of low-loss inductors on thin porous silicon membranes”, B. Bardet et al, Microelectron. Eng., vol. 194, pages 96-99 (2018), - “Highly insulating, fully porous silicon substrates for high temperature micro-hotplates”, F. Lucklum et al, Sensor. News. In Phys., vol. 213, pages 35-42 (2014), - «All-in-One Nanowire-Decorated Multifunctional Membrane for RapidCell Lysis and Direct DNA Isolation », H. So et al, ACS Appl. Mater Interfaces, vol 6, pages 20693-20699 (2014), - « Electrochemically etched nanoporous silicon membrane for separation of biological molecules in mixture », N. Burham et al, J. Micromech. MicroEng., vol. 27, page 075021 (2017), et - « Effects of nano / microstructures on performance of Si-based microfuel cells », Appl. Therm. Eng, Vol. 72, num. 2, Pages 298-303 (2014) décrivent différents procédés de fabrication de membranes de silicium. The process according to the invention involves the electrochemical etching of a substrate in an aqueous electrolyte based on hydrofluoric acid. In general, the electrochemical etching of silicon is a well-known and documented technique, as for example in the book "Electrochemistry of Silicon: Instrumentation, Science, Materials and Applications", Dr. Volker Lehmann, doi: 10.1002 / 3527600272, 2002 Wiley-VCH Verlag GmbH. The conditions for implementing the process according to the invention are, however, unconventional. To the inventors' knowledge, prior to this invention, work on the electrochemical etching of silicon had been primarily focused on finding pores with a regular profile and walls. Within this framework, studies for these substrate characteristics were mainly concentrated on pores with a diameter greater than 1 µm and up to approximately 10 µm, exhibiting the most regular tubular shapes possible and free from defects, without any particular attention being paid to infrared transmission properties. To this end, silicon substrate etchings had been carried out under conditions different from the invention, for example in galvanostatic mode or in potentiostatic mode but at a low electrical voltage less than 10 V, and in an aqueous electrolyte where the mass concentration of hydrofluoric acid was low, i.e. less than 10%. Examples Examples | and 2 comparative and 3 to 9 according to the invention were carried out using the electrochemical cell illustrated in [Fig.1]. The electrochemical cell 100 comprises a housing 102, a silicon anode 104 and cathode 106 arranged within the housing and electrically connected to an electrical generator 108. A silicon substrate 110 is placed between the anode and the cathode. The front face 112 of the substrate is opposite a face 114 of the cathode. The enclosure also includes a solid-walled casing 116, sealed by the silicon substrate. Sealing gaskets 118 are positioned on either side of the substrate's ends. Thus, the first 120 and second 122 chambers are defined, each sealed from the other. An aqueous electrolyte 124 containing hydrofluoric acid, the mass concentration of which was modified for the different tests, was introduced into each of the two chambers. The front 110 and rear 126 faces of the substrate were therefore in contact with the electrolyte, acting as electrodes to ensure electrical continuity during the redox reactions. Furthermore, the part 128 of the wall of the case superimposed on the rear face 126 is transparent to light, and an illumination I was generated by halogen lamps 134 and distributed over the entire rear face of the substrate by means of a hemispherical reflective mirror 136, in order to generate charge carriers in the substrate. The substrate was a silicon plate which had a thickness of 750 jm, was phosphorus-doped silicon, and therefore of type n, and had an electrical resistivity between 3 @.cm and 6 Q.cm. During the implementation of the electrochemical etching, the plate was illuminated by a light radiation of greater than 20000 lumens using halogen lamps. The electrochemical etching of the front face of the substrate was carried out under a potentiostatic regime, with a voltage maintained constant between the anode and the cathode of the cell throughout the etching. The electrochemical etching time was kept constant at 6 minutes for all tests, except for tests 2 and 6 for which the time was 15 minutes. Table 1 below summarizes the experimental conditions and results Tests marked with an asterisk are comparative. "N.A." means "not applicable". [Table 1] Pore ​​surface density (µm?) |= 32 um |= 50 µm |= 35 µm |= 15 pm |= 40 jm |= 60 µm [Test of surface mass concentration _ (V) of fluorine- |pores (hydric acid (%) be fs fs MA 20 |15 5 0.05 ee 5 + |i5 |s 0.38 5 25 = 0.45 660) 135 5 0.35 7 |ss # 0.65 8 35 35 0.50 = 45 = 0.85 F5 Speed ​​of = | > |pores |etching of |pores (nm) pores (um) (um / min) NANANA 1600 0.8 [= 15 um 230 5.3 [- 32 um 320 10.1 [- 50 um 230 5.8 [- 35 um 420 |L1 [= 15 um Jo los [= 40 jm 150 9.7 [- 60 um = 12 |= 65 um PO 15 15 188. 20 7 (SM) In the case of Example 1, outside the scope of this invention, the application of a low voltage of 5 V, as conventionally applied prior to the invention, with a hydrofluoric acid mass concentration of 15%, does not allow for etching of the substrate. This is observed in [Fig. 2]; the observed face of the substrate has been chemically attacked. The result is a rough surface covered with homogeneously distributed silicon aggregates, but no pores have been formed. In the case of Example 2, outside the scope of the invention, the application of a voltage of 15 V, unconventional until the invention, with a hydrofluoric acid mass concentration of 5%, results in the slow formation of pores with a diameter of approximately 1600 nm, observable in [Fig. 3a] and in the enlarged version of [Fig. 3b]. Increasing the voltage to 35 V, as in Example 6, outside the scope of the invention, does not allow for a pore size of 400 nm at most, as described in the invention, observable in [Fig. 6]. Furthermore, in these comparative examples, the etching speed is too slow, less than 2 µm / min. As can be seen in figures 4, 5 and 7 to 9, corresponding to examples 3, 4 and 7 to 9, the implementation of the process according to the invention makes it possible to manufacture a substrate in which the pores have a diameter between 50 nm and 400 nm. In the examples illustrated above, at the end of electrochemical etching, the pores The resulting openings were blind and opened through a single opening onto one face of the substrate. Transmittance measurements were performed on the substrates thus etched. The transmittance of the etched substrates, objects of examples 3 to 5 and 7 to 9, was measured on the spectrum of wavelengths in the infrared between 5 µm and 25 µm and is shown in [Fig. 10]. Curve 2 represents the evolution of the transmittance of a porous alumina layer having through cylindrical pores with a diameter between 20 nm and 200 nm, a thickness of 60 µm and distributed according to a surface density varying between 10 and 2000 µm? As shown in [Fig.10], this alumina layer exhibits high transmittance up to a wavelength of 10 µm but is totally opaque to radiation of longer wavelengths. The evolution of transmittance for a dense n-type substrate with a resistivity of 3-6 Q / cm is illustrated by curve 4. This substrate exhibits a transmittance greater than 20% over the entire wavelength range between Sum and 25 µm. However, being poreless, it cannot form a membrane for fluidic transfer. Curves 6 to 16 illustrate the evolution of transmittance for examples 3, 4, 5, 7, 8, and 9 according to the invention, respectively. As observed in [Fig. 10], the etched substrates of these examples thus exhibit a transmittance close to that of the dense substrate. This confirms that pores of a diameter and aspect ratio according to the invention interact only weakly with infrared radiation, and allow the preservation of the good infrared transmission properties in the wavelength range of 5 µm to 25 µm of the n-doped silicon substrate. For comparison, substrates of type n identical to those in Examples 1 to 9 were subjected to an electrochemical etching step in the same electrochemical cell, but under galvanostatic conditions, i.e., by imposing a constant current density. Thus, Example 10 was produced, with the same experimental setup, by immersing the anode in a hydrofluoric acid solution at a concentration of 35% and then performing the electrochemical etching under a constant current density of 14 mA·cm⁻¹. Example 11 was carried out under conditions identical to those of Example 10, except that the hydrofluoric acid concentration was 15% and the imposed constant current density was 20 mA·cm⁻¹. As observed in Figures 11 and 12, blind pores were formed, but all of them had a diameter greater than 2 µm. These large pores interact with infrared radiation and reduce transmittance. of the n-type substrate. This is observed in [Fig. 13]. Curves 20 and 22 represent the evolution of the transmittance of examples 10 and 11, respectively. The transmittance of these etched substrates, outside the scope of this invention, is less than 5% for radiation with wavelengths between 5 µm and 8 µm. It is less than 10% for radiation with wavelengths less than 17 µm for example 10 and less than 14 µm for example 11. Furthermore, a membrane was formed for a porous wall obtained under the conditions of example 3, as illustrated in [Fig.14]. The face 52 of the substrate 50, onto which the blind pores 54 opened, was polished to remove a layer 56 of nanoporous silicon formed on the surface by electrochemical etching. Next, a protective layer 58 made of silicon oxide (of the TEOS or SiH type, deposited by CVD) was deposited on the polished face 52 to prevent the pore openings from being damaged by subsequent ablation. The substrate was inverted (step 60) and then mechanically abraded (step 62) to reduce its thickness. A layer of photosensitive resin 64 was then deposited on the face 66 of the substrate opposite face 52 and was locally ablated under ultraviolet light radiation using conventional photolithography methods.Areas 68 of the portion 70 of the substrate superimposed on the blind pores were ablated by deep plasma etching, so as to form recesses 72 in the substrate, delimited by a mask, until the pores 54 opened into the recess. The photosensitive resin and the oxide layer were then removed (steps 74 and 76). Thus, the unablated areas 78 of the substrate form a support 80 with recesses, onto which a wall 82 is superimposed, having blind pores opening onto the unablated areas and pores passing through the wall from one side to the other through its thickness and opening through one of their openings into one of the recesses. A membrane 84 is thus obtained. The invention is not limited to the optional examples and embodiments and implementations presented by way of illustration and not limitation. In particular, the process can be implemented using the electrochemical cell illustrated in [Fig.15]. The cell 100 illustrated in [Fig.15] differs from that illustrated in [Fig.1] in that the second chamber 122 contains a different electrolyte, for example based on potassium sulfate, different from that contained in the first chamber.

Claims

Claims

1. Fluid transfer membrane (84) comprising a porcusc wall (82) in n-doped silicon having pores (54) extending from one side to the other in its thickness, each pore having a diameter less than or equal to 400 nm and an aspect ratio greater than or equal to 20, the membrane having a transmittance greater than or equal to 5% at any radiation whose wavelength is between 5 um and 25 um.

2. Membrane according to claim 1, having a transmittance su- greater than or equal to 10%, or even greater than or equal to 20%, better still greater than or equal to 30% to any radiation whose wavelength is between 5 um and 25 um.

3. A membrane according to any one of claims 1 and 2, each pore with a diameter less than or equal to 350 nm and / or greater or equal to 50 nm.

4. Membrane according to any one of the preceding claims, the pores have a slenderness ratio greater than or equal to 50, better greater than or equal to 100.

5. Membrane according to any one of the preceding claims, the pore surface density being between 0.1 um* and 5.0 um”.

6. Membrane according to any one of the preceding claims, further comprising a support (80) superimposed on the porous wall and which comprises at least one recess (72) passing through the support on either side part in its thickness, at least one pore (54) opening into the recess (72).

7. A method of manufacturing a membrane according to any one of the re- preceding claims, the method comprising - the provision of an n-doped silicon substrate which has a re- electrical sistivity between 1 @.cm and 10 ©@.cm, and a cell electrochemical comprising an electric generator, a cathode and an anode electrically powered by the electric generator, the electrochemical cell containing an aqueous electrolyte comprising hydrofluoric acid in a mass concentration greater than or equal to 10%, the substrate being arranged between the anode and the cathode, at least one of the faces of the silicon substrate being in contact with the electrolyte, the cathode and the face of the silicon substrate opposite the cathode, called “front face”, being in contact with the electrolyte, the front face of the substrate silicon being distant from the cathode, - electrochemical etching of the substrate by applying with the generator electric a constant electrical voltage greater than or equal to 10 V between the anode and the cathode, in order to form blind pores in the substrates which each have a diameter less than or equal to 400 nm and which extend from one face of the substrate to a greater depth or equal to 10 um, the rear face of the substrate being illuminated during the electrochemical etching with light radiation in order to generate charge carriers in the substrate, and - the removal of a part of the substrate so that said pores are de- blocking and passing through at least a portion of the substrate from one side to the other in its thickness.

8. A method according to claim 7, the aqueous electrolyte having a mass concentration of hydrofluoric acid greater than or equal to 15 %, preferably greater than or equal to 30%, better still greater than or equal at 35%.

9. A method according to any one of claims 7 and 8, comprising prior to electrochemical etching, illumination of the substrate with light radiation to generate charge carriers in the substrate.

10. A method according to any one of claims 7 to 9, the etching electrochemical being conducted until the pores expand each from one face of the support to a depth greater than or equal to 30 um, preferably greater than or equal to 50 um, or even su- greater than or equal to 75 um.

11. | A method according to any one of claims 7 to 10, the etching electrochemical being carried out at a constant electrical voltage between 25 V and 100 V.

12. A method according to any one of claims 7 to 11, the substrate having a thickness, prior to electrochemical etching, between 100 um and 3 mm, preferably between 500 um and 1.55 mm.

13. A method according to any one of claims 7 to 12, the ablation being operated by mechanical polishing, chemical etching by wet and / or deep etching by dry method, preferably ablation being selective.

14. A method according to any one of claims 7 to 13, comprising further treatment of the membrane to make the membrane hy- drophilic or hydrophobic.

15. Method for characterizing a colony of microorganisms, comprising: - the cultivation of microorganisms in a nutrient medium, the microor- organisms being arranged on one face of a membrane according to one any of claims | to 6 and / or obtained by the process according to any one of claims 7 to 14, the membrane being at contact of the nutrient medium such that the nutrient medium is transferred through the pores to microorganisms, - the illumination of microorganisms in transmission through the membrane by light radiation having at least one length wavelength between 5 um and 25 um and the acquisition of the radiation light having interacted with microorganisms.