Method for manufacturing a fusible / flowable explosive composition.
A temperature-dependent viscosity modifier addresses viscosity challenges in meltable/castable explosive compositions, enabling homogeneous loading and solidification in ammunition casings with standard equipment, improving stability and compliance with regulatory standards.
Patent Information
- Application Number
- FR2022010862
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-10-20
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2042-10-20
AI Technical Summary
Existing methods for manufacturing homogeneous meltable/castable explosive compositions face challenges in achieving uniformity and stability, particularly with multi-component formulations, requiring complex and costly equipment due to high viscosity and sedimentation issues, which are not compatible with standard production tools.
A process involving a viscosity modifier with temperature-dependent solubility and affinity for nitrated aromatic explosives like TNT, allowing for controlled viscosity adjustment and homogeneous mixing without specialized equipment, using 20-60% meltable explosive, 0-10% viscosity modifier, and inert/explosive granular species.
Enables homogeneous loading and solidification of explosive compositions in ammunition casings without complex tools, reducing energy consumption and production costs, while ensuring stability and compliance with regulatory standards.
Smart Images

Figure 00000010_0000 
Figure 00000011_0000
Abstract
Description
Title of the invention: Method for manufacturing a fusible / castable explosive composition.
[0001] The invention relates to a method of manufacturing a fusible / castable explosive composition, and its loading into a munition.
[0002] These charges are mostly based on 2,4,6-trinitrotoluene, acronym TNT; an explosive which has the particularity of melting at temperatures close to 80°C, thus allowing the loading in the liquid state of a metal casing, such as a munition body, by the sole action of gravity.
[0003] It is usual to add to this explosive other explosives such as hexogen (RDX), octogen (HMX) or oxynitrotriazole (ONTA) or even additives (phlegmatizers, stabilizers, sensitizers, etc.) in order to obtain a formulation meeting the requirements of the ammunition (detonation performance, insensitivity, etc.).
[0004] High added value formulations often incorporate five to seven constituents. They are by nature heterogeneous because different granular species are found randomly dispersed in a fusible media. Nevertheless, it is essential to ensure the best possible homogeneity of the explosive charge after solidification in the munition casing in order to ensure the reliability of the safety and performance of the munitions throughout their life profile (production, storage, transport, use and demilitarization). The parameters commonly used to ensure this homogeneity include increasing the viscosity and the particle size distribution of the additives.
[0005] Indeed, the granular species present in a very viscous mixture have almost no possibility of migrating (sedimentation or creaming), thus very significantly limiting the risks of inhomogeneity of the load. However, the implementation of viscous loads requires the use of complex technologies, limiting, among other things, production rates.
[0006] These formulations must also meet increasingly stringent requirements (low dispersion of properties and conservation of these properties after aging), described for France in general instruction S-CAT 17500 edition 6 dated December 2019, and for NATO members in STANAG.4170 edition 3 dated 2008. Complying with these regulatory requirements requires increased control of the homogeneity of loading of ammunition.
[0007] The criticality of the problem linked to the homogeneity of the explosive charge in the ammunition is quite recent and follows the evolution of the criteria associated with the safety of use and storage of ammunition. Maintaining this homogeneity on the formulations with more than three granular ingredients is even more critical.
[0008] Historically, munitions were loaded with picric acid and then trinitrotoluene after the Second World War. These loads were single-component, so they effectively addressed this problem. For reasons related to increasing the terminal performance of munitions, many formulations have been developed by adding additives to this TNT base.
[0009] It has been integrated into the historical formulations of granular explosives, such as RDX and HMX, in order to very significantly increase the detonation performance, in order to obtain the desired performance, as well as to maintain homogeneity throughout the product life cycle. In particular, a rate of around 60% by mass of solid species has been introduced (Composition B 60 / 40). This rate makes it possible to significantly increase the viscosity of the liquid mixture to limit phase shifts and sedimentation, but also makes it possible to play on the compactness of the species. The principle consists of determining as precisely as possible the particle size distribution allowing the introduction of the maximum number of granular species in a given space. This has the main effect of blocking the arrangement of the species relative to each other.
[0010] This very strong increase in the percentage of solid constituents (beyond 60% by mass) and this modulation of the particle size distribution of each of the solid additives makes it possible to achieve maximum compactness. Once this compactness is achieved, the different granular species are mechanically constrained not to sediment or dephase once loaded into the ammunition. However, upon reaching this compactness, the mixture becomes extremely viscous in the tank and results in a limitation of the flowability of the formulation. It is then often necessary to increase the temperature of the mixture, or even to generate a depression in the ammunition casings (vacuum of the order of 50 mbar). The increase in temperature results in a significant increase in the energy expenditure to produce ammunition, and the vacuuming of the loading operation is not compatible with the standard tools of the skilled person.
[0011] Surfactant-type additives were used to ensure the homogeneity and stability of the composition over time. These molecules have the capacity to possess a hydrophilic head and a hydrophobic tail, thus increasing the affinity between TNT and phlegmatizers. We can cite the patented compositions XF13333 and XF11585 from NEXTER mentioned in patents FR2750131 and FR2954308 using surfactants from the polyvinylpyrrolidone family. These compositions were the subject of a thesis entitled "Rheology of concentrated suspensions of recyclable energy materials - Modeling of the casting time". A technical report WL-TR-94-7058 studies the impact and chemical affinity between dif different families of phlegmatizers and TNT with the aim of replacing composition D-2 (MIL-C-18164A) present in formulation H-6 (compB / AI / D-2) and Destex (TNT / AI / D-3). In these cases, the use of soy lecithin as well as carbon black led to stabilizing the mixture.
[0012] Adding an additive to the formulation aims to significantly increase the viscosity of the mixture while maintaining a proportion of liquid phase greater than 50%. Such viscosities in the mixing tank require specific tools to ensure homogenization of the constituents such as stirring blades similar to hooks, Z-shaped blades or leaflet planets. These stirring methods are then no longer suitable for historical formulations and require manufacturers to set up tools dedicated to each formulation.
[0013] According to one aspect of the invention, there is provided a method of manufacturing a fusible / castable explosive composition comprising the following steps: - melting of a fusible explosive comprising a nitrated aromatic cycle, and preferably 2,4,6-trinitrotoluene; - addition of viscosity modifier to the molten fusible explosive, the viscosity modifier having a solubility in the fusible explosive, greater than a solubility threshold above a threshold temperature, and less than the solubility threshold below the threshold temperature, the threshold temperature being less than a mixing and loading temperature of the explosive composition, the viscosity of the composition being less than a viscosity threshold above the threshold temperature and greater than the viscosity threshold below the threshold temperature; the viscosity modifier being such that for a temperature variation of at most 5°C in absolute value around the threshold temperature, the corresponding variation in viscosity in absolute value is greater than 10 Pa.s times the temperature variation in absolute value, and the corresponding variation in solubility in absolute value is greater than 15% by mass. - addition of at least one inert granular species and / or at least one energetic granular species; the proportions of the components used being such that the composition obtained comprises 20 to 60% by mass of fusible explosive, and at most 10% by mass of viscosity modifier, and preferably 3 to 5% of viscosity modifier.
[0014] In one embodiment, the threshold temperature is between 85°C and 95°C, and the mixing and loading temperature is greater than 95°C.
[0015] According to one embodiment, the viscosity modifier is a derivative of benzene, or naphthalene, or anthracene.
[0016] In one embodiment, the viscosity modifier is benzene, or naphthalene, or anthracene, functionalized by one or more groups among the hydroxyl, carboxyl, or sulfonyl groups.
[0017] According to one embodiment, the viscosity modifier is naphthol, and preferably 1-naphthol or 2-naphthol.
[0018] In one embodiment, an inert granular species is aluminum or perchlorate salts.
[0019] According to one embodiment, an energetic granular species is RDX, HMX, or TKX-50.
[0020] In one embodiment, the method further comprises a step (4) of loading the composition into a munition delimited by a hollow body, comprising pouring the explosive composition into the hollow body of a munition.
[0021] According to one embodiment, the method further comprises a solidification step during cooling of the composition to a temperature of the composition below the threshold temperature, resulting in mass precipitation in a homogeneous manner and an increase in the viscosity of the mixture, above the viscosity threshold, instantly trapping the granular species.
[0022] The invention will be better understood by studying some embodiments described as non-limiting examples and illustrated by the appended drawings in which: - [Fig.l] schematically illustrates the solubility of the viscosity modifier soluble in TNT and the viscosity of the mixture, as a function of the temperature of the composition, according to one aspect of the invention; and - [Fig.2] schematically illustrates an example of a method for manufacturing a fusible / castable explosive composition, according to one aspect of the invention.
[0023] Throughout the figures, elements having identical references are similar.
[0024] [Fig.l] represents the solubility of the TNT-soluble viscosity modifier and the viscosity of the mixture, as a function of the temperature of the composition, according to one aspect of the invention.
[0025] The invention consists in particular of the use of a viscosity modifier whose chemical structure has very strong chemical affinities with a fusible explosive comprising a nitro aromatic cycle, such as 2,4,6-trinitrotoluene or TNT.
[0026] A fusible explosive comprising a nitro aromatic ring, such as TNT, exhibits strong Van der Waals interactions due to the benzene ring and the Nitro groups in positions 2, 4 and 6. The presence of non-bonding doublets on the oxygens of the Nitro groups means that TNT is also a strong Lewis base. To ensure miscibility and therefore maximum homogeneity of the solution, the structure of the viscosity modifier must therefore exhibit strong Van der Waals interactions and Lewis acid functions.
[0027] Also, the present invention uses a viscosity modifier having a solubility profile, strongly dependent on the temperature, in the fusible explosive comprising a nitro aromatic ring, with a threshold temperature Ts such that below this the viscosity modifier is considered not or slightly soluble in the liquid fusible explosive comprising a nitro aromatic ring, i.e. the solubility of the viscosity modifier is lower than a solubility threshold Ss, and that above this the viscosity modifier is considered very soluble in the liquid fusible explosive comprising a nitro aromatic ring, i.e. the solubility of the viscosity modifier is higher than the solubility threshold Ss.
[0028] Furthermore, above the threshold temperature Ts, the viscosity of the composition is considered to be of low viscosity, i.e. lower than a viscosity threshold Vs, and below the threshold temperature Ts, the viscosity of the composition is considered to be of high viscosity, i.e. higher than the viscosity threshold Vs.
[0029] The threshold temperature Ts is lower than a mixing and loading temperature of the explosive composition which is generally of the order of 95°C.
[0030] The viscosity modifier soluble in the fusible explosive comprising a nitro aromatic cycle makes it possible to control the viscosity of the mixture as required.
[0031] [Fig.2] schematically illustrates an exemplary method of manufacturing a fusible / castable explosive composition, according to one aspect of the invention.
[0032] The method for manufacturing a fusible / castable explosive composition comprises a first step 1 of melting (1) a fusible explosive comprising a nitro aromatic cycle, preferably 2,4,6-trinitrotoluene or TNT.
[0033] The melting of the fusible explosive comprising a nitro aromatic cycle is carried out at a temperature above 95°C.
[0034] The method comprises a second step 2 of adding viscosity modifier to the molten fusible explosive. The viscosity modifier has a solubility in the fusible explosive, greater than a solubility threshold Ss above the threshold temperature Ts, and less than the solubility threshold Ss below the threshold temperature Ts, the threshold temperature being less than a mixing and charging temperature of the explosive composition, generally greater than 95°C. The viscosity of the composition is less than a viscosity threshold Vs above the threshold temperature Ts and greater than the viscosity threshold Vs below the threshold temperature Ts.
[0035] The viscosity modifier being such that for a temperature variation AT = Ts ± 5°C of at most 5°C in absolute value around the threshold temperature Ts, the corresponding variation in viscosity in absolute value is greater than 10 Pa.s, and the corresponding variation in solubility in absolute value is greater than 15% by mass.
[0036] This step 2 being carried out at a mixing and loading temperature above 95°C, the composition has a low viscosity and the solubility of the viscosity modifier is high.
[0037] The proportions of the components used are such that the composition obtained comprises 20 to 60% by mass of fusible explosive, and at most 10% by mass of viscosity modifier, and preferably 3 to 5% of viscosity modifier.
[0038] Thus, during step 2, the viscosity modifier is very soluble in the fusible explosive comprising a nitro aromatic cycle, such as TNT, and the viscosity of the composition is considered to be very low or slightly viscous, i.e. lower than the viscosity threshold Vs.
[0039] The use of a viscosity modifier with very high chemical affinity with the fusible explosive comprising a nitro aromatic cycle, such as TNT, to make the latter very soluble above the threshold temperature Ts and very little or not at all soluble below, makes it possible to activate the function of the viscosity modifier depending on the step of the process and the need by controlling the temperature of the mixture.
[0040] It is incorporated, for all formulations based on a fusible explosive comprising a nitro aromatic cycle, such as TNT, several inert and explosive granular species. These compositions may or may not include inert species such as aluminum or perchlorate salts at different mass percentages, as well as energetic species such as RDX, HMX or TKX-50 at different rates.
[0041] This can be achieved by a person skilled in the art on known standard equipment, without having to modify existing production lines.
[0042] Furthermore, the present invention makes it possible to envisage reducing the mass fraction of fusible species in the formulations. This therefore gives access to formulations previously inaccessible by the cast-melt process and opens up the possibility of avoiding more complex and more expensive implementation processes (mixing, extrusion).
[0043] The viscosity modifier may be benzene, or naphthalene, or anthracene, functionalized by one or more groups among the hydroxyl, carboxyl, or sulfonyl groups.
[0044] Advantageously, the viscosity modifier may be naphthol, and preferably 1-naphthol or 2-naphthol.
[0045] Furthermore, the method may comprise a step 4 of loading explosive into a munition delimited by a hollow body, comprising pouring the explosive composition into the hollow body of a munition.
[0046] Thus, the fusible / castable explosive composition can then solidify during a solidification step 5 in the body of the munition, during its cooling. After loading, the modifier is activated by a uniform mass precipitation, thus drastically increasing the viscosity and blocking the mechanisms of sedimentation and creaming. Indeed, at the end of loading, the mixture present in the munitions has cooled and the temperature is below the threshold temperature Ts. The modifier precipitates in mass in a homogeneous manner and causes a very strong increase in the viscosity of the mixture, above the viscosity threshold Vs. The different granular species are then trapped almost instantly and the solidification conditions are greatly relaxed.
Claims
Claims
1. A method of manufacturing a fusible / castable explosive composition comprising the following steps: - melting (1) a fusible explosive comprising a nitro aromatic ring, and preferably 2,4,6-trinitrotoluene; - adding (2) a viscosity modifier to the melted fusible explosive, the viscosity modifier having a solubility in the fusible explosive, greater than a solubility threshold (Ss) above a threshold temperature (Ts), and less than the solubility threshold (Ss) below the threshold temperature (Ts), the threshold temperature (Ts) being less than a temperature (Tmc) for mixing and loading the explosive composition, the viscosity of the composition being less than a viscosity threshold (Vs) above the threshold temperature (Ts) and greater than the viscosity threshold (Vs) below the threshold temperature (Ts);the viscosity modifier being such that for a temperature variation of at most 5°C in absolute value around the threshold temperature, the corresponding variation in viscosity in absolute value is greater than 10 Pa.s times the temperature variation in absolute value, and the corresponding variation in solubility in absolute value is greater than 15% by mass. - addition (3) of at least one inert granular species and / or at least one energetic granular species; the proportions of the components used being such that the composition obtained comprises 20 to 60% by mass of fusible explosive, and at most 10% by mass of viscosity modifier, and preferably 3 to 5% of viscosity modifier.;
2. The method of claim 1, wherein the threshold temperature (Ts) is between 85°C and 95°C, and the mixing and loading temperature (Tmc) is greater than 95°C.
3. A method according to claim 1 or 2, wherein the viscosity modifier is a derivative of benzene, or naphthalene, or anthracene.
4. The method of claim 3, wherein the viscosity modifier is benzene, or naphthalene, or anthracene, functionalized by one or more groups among hydroxyl, carboxyl, or sulfonyl groups.
5. Method according to one of claims 3 or 4, in which the viscosity modifier is naphthol, and preferably 1-naphthol or 2-naphthol.
6. A method according to any preceding claim, wherein an inert granular species is aluminum or perchlorate salts.
7. A method according to any preceding claim, wherein an energetic granular species is RDX, HMX, or TKX-50.
8. Method according to one of the preceding claims, further comprising a step of loading (4) the composition into a munition delimited by a hollow body, comprising pouring the explosive composition into the hollow body of a munition.
9. Method according to one of the preceding claims, further comprising a solidification step (5) during cooling of the composition to a temperature of the composition below the threshold temperature (Ts) resulting in mass precipitation in a homogeneous manner and an increase in the viscosity of the mixture, above the viscosity threshold (Vs), instantly trapping the granular species.