System and method for adjusting and prestressing to adjust the surface of a part

The combined adjustment and prestressing system addresses reproducibility and efficiency issues by integrating abrasive and compression functions in a single tool, reducing defects and processing time.

FR3142110B1Active Publication Date: 2024-10-25SAFRAN AIRCRAFT ENGINES SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022012164
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-11-22
Publication Date
2024-10-25
Estimated Expiration
2042-11-22

AI Technical Summary

Technical Problem

Existing adjustment and local retouching methods face issues with reproducibility, incomplete local compression, increased risk of new defects, and prolonged processing time due to separate operations and manual handling, especially when using flexible abrasive tools and shot peening.

Method used

A combined adjustment and prestressing system with a split rod and woven strip impregnated with resin, featuring controllable rotation and alternating abrasive zones and tungsten carbide balls, allowing simultaneous adjustment and compression using a single tool.

Benefits of technology

Enables efficient, reproducible, and time-saving surface adjustment and compression with reduced risk of new defects by integrating abrasive and compression functions in a single operation, eliminating the need for intermediate steps and masking.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000010_0000
    Figure 00000010_0000
  • Figure 00000010_0001
    Figure 00000010_0001
  • Figure 00000011_0000
    Figure 00000011_0000
Patent Text Reader

Abstract

A fitting and preloading system for adjusting and compressing a surface of a part, comprising a rod (2), at least one first fin and a second fin fixed to the rod and arranged on either side of the rod, balls (4) and abrasive zones (5a, 5b) arranged on each fin, the system further comprising controllable rotation means configured to rotate the rod (2) in at least one direction of rotation so that the balls (4) and abrasive zones (5a, 5b) come into contact with the surface to be adjusted. Figure for the abstract: Fig 1
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: System and method for adjusting and pre-stressing a surface of a part technical field

[0001] The invention relates technically to tools for adjusting and local retouching. Previous techniques

[0002] Adjustment by flexible abrasive tool is generally used at the end of the retouching range of a surface in order to eliminate a defect (impact, scratch, ...) and to obtain at least the surface condition prescribed in the plan of the part.

[0003] There are different types of soft abrasive tools: flap brushes, compact impregnated brushes (such as "Scotch-Brite™"), or combination brushes (flaps and compact impregnated brushes) are the main types of tools used. These tools can have different shapes, chosen according to the nature of the operation and the area to be treated.

[0004] Beyond its shape, the characteristics of the abrasive are also important. Two main characteristics are distinguished: the nature of the abrasive, in other words, the material constituting the abrasive; and the grade of the abrasive, in other words, the size of the abrasive particles. Silicon Carbide (SiC) and Aluminum Oxide (Al₂O₃) are the two most commonly used types of abrasives, and their selection depends on the material of the workpiece being finished. Regarding the abrasive grade, it is chosen according to the desired objective: to achieve significant material removal during the initial fitting stages, coarse grains will be used, and to smooth the surface and reduce its roughness, fine grains will be preferred.

[0005] To perform a touch-up, it is necessary to use a succession of abrasive tools, starting with a coarse grade, in order to carry out the essential removal of material, then to carry out a finishing using finer grade abrasives in order to obtain the desired surface condition.

[0006] Rotary shot peening is a local compression process, generally used on a pre-prepared surface, with the aid of a flexible or rigid abrasive tool. The rotary shot peening tool consists of a slotted rod to which is attached a resin-impregnated woven belt with one or more rows of tungsten carbide balls (from 1 to 4 rows of 4 to 16 balls). The belt is rotated using a handheld device so that the carbide balls impact the surface to be treated and introduce residual compressive stresses.

[0007] Implementing this method for applying local compression to a reworked area requires prior surface preparation by adjustment with a soft abrasive. If this preparation is not sufficiently well carried out, the verification of The effectiveness of the operation via visual inspection is not possible. It is therefore necessary to repeat the adjustment operation.

[0008] As an alternative to rotary shot peening, conventional shot peening (or prestressing shot peening) can be used to re-compress the reworked area. This operation is commonly used in the normal manufacturing process of a part to introduce compressive stresses into large areas. When used to treat reworked areas, lengthy masking operations are required on the unreworked surfaces, and handling of the part increases the risk of creating new defects.

[0009] The following problems arise from the use of this prior art:

[0010] - local adjustment and retouching are not necessarily carried out by the same This can lead to a lack of reproducibility, or incomplete local compression if the fitted area is not fully covered during the roto-shot blasting operation.

[0011] - the two operations being carried out separately in locations that may be When working remotely, handling operations are necessary for the part, increasing the risk of creating new impacts and scratches and lengthening processing time.

[0012] - the multiplication of the number of tools used in the adjustment and roto- Shot blasting leads to an increased risk of creating new impacts on the workpiece due to tool strikes, as the operation is manual, and

[0013] - the use of conventional shot blasting requires lengthy operations masking of untreated areas. Description of the invention

[0014] The invention relates to an adjustment and preloading system for adjusting and compressing a surface of a part, comprising a rod, at least a first fin and a second fin fixed on the rod and arranged on either side of the rod, balls and abrasive zones are arranged on each fin, the system further comprising controllable rotation means configured to rotate the rod in at least one direction of rotation so that the balls and abrasive zones come into contact with the surface to be adjusted.

[0015] The balls can be arranged so as to be further away from the rod than the abrasive areas.

[0016] The abrasive zones can be arranged so that the abrasive zones covered with larger grain size abrasive grains are arranged closer to the stem than the abrasive zones covered with smaller grain size abrasive grains.

[0017] Each fin comprises a first face and a second face opposite the first face, the first faces being arranged on the same side of the assembly formed by the first fin and the second fin, the second faces also being arranged on the same side of this assembly, the balls and the abrasive areas can be arranged on the first face of the first fin and on the second face of the second fin.

[0018] Each fin comprises a first face and a second face opposite the first face, the first faces being arranged on the same side of the assembly formed by the first fin and the second fin, the second faces also being arranged on the same side of this assembly, the balls can be arranged on the first face of the first fin and on the second face of the second fin, the abrasive areas being arranged on the second face of the first fin and on the first face of the second fin.

[0019] The first fin and the second fin can be formed respectively by a first part and a second part of the same strip fixed on the rod.

[0020] Another object of the invention is a fitting and preloading method in which the surface of a part undergoes a fitting step and a local compression step via the fitting and preloading system described above, in which the tool is rotated in at least one direction of rotation so that the balls and abrasive areas are successively brought into contact with the surface of the part.

[0021] Yet another object of the invention is a fitting and preloading method in which the surface of a part undergoes a fitting step and a local compression step via the fitting and preloading system described above, in which the tool is rotated in one direction only so that the abrasive areas covered with larger grains come into contact with the surface of the part to be fitted before the abrasive areas covered with smaller grains and the balls.

[0022] Yet another object of the invention is a fitting and pre-stressing method in which the surface of a part undergoes a fitting step and a local compression step by means of the fitting and pre-stressing system described above, in which the tool is rotated in a first direction with a first rotational speed so that the abrasive areas come into contact with the surface of the part to be fitted and in a second direction with a second rotational speed so that the balls come into contact with the surface of the part to be fitted and put into compression.

[0023] The change in the direction of rotation can then be carried out by request from the operator.

[0024] The change in direction of rotation can also be carried out automatically, particularly depending on the time elapsed. Brief description of the drawings

[0025] Other objects, features and advantages of the invention will become apparent from the following description, given solely by way of non-limiting example and made with reference to the accompanying drawings in which:

[0026] - Figure [Fig.1] illustrates the adjustment and preload system according to the invention,

[0027] - Figure [Fig.2] illustrates a side view of the adjustment and preload system during an adjustment phase,

[0028] - Figure [Fig.3] illustrates a side view of the adjustment and preload system during a prestressing phase,

[0029] - Figure [Fig.4] illustrates another embodiment of the adjustment and adjustment system prestressing. Detailed description

[0030] The adjustment and preloading system according to the invention is illustrated in Figure [Fig. 1]. The adjustment and preloading system 1 comprises a slotted rod 2, in the slot of which a woven strip 3 is disposed, such that a portion of the woven strip 3 is positioned on each side of the slotted rod 2, thus forming a first fin and a second fin on either side of the rod. It will be understood that this embodiment is not limited to two fins formed from the same strip, and that these two fins could be distinct from one another, without continuity of material between them. It will also be understood that this embodiment is not limited to a single slotted rod, and that the woven strip 3 can be held in place by screwing or clipping, possibly via a flat surface.Similarly, it will be understood that alternatives to the woven strip 3 can be used without departing from the scope of the present invention, such as a plastic material or fiberglass, provided that a fin thus produced is flexible (to deform upon contact with a workpiece, in particular to adapt to the surface of that workpiece). Alternatively, such a material can be reinforced by a mesh or a weave. The adjustment and preloading system includes controllable rotation means, not shown, capable of rotating the slotted rod 2.

[0031] The woven strip 3 is impregnated with resin to give it a certain rigidity. The woven strip 3 is defined as comprising a first face and a second face opposite the first face. By analogy, it is stated that the first face of the first fin and the first face of the second fin face the same area of ​​space relative to the tool 1. Similarly, the second face of the first fin and the second face of the second fin face the same area of ​​space relative to the tool 1.

[0032] A first part of the woven strip 3 extending from a first side of the split rod 2 comprises, on its first face, at least two balls 4, in particular made of tungsten carbide and two abrasive zones 5a,5b covered with abrasive grains of different sizes.

[0033] A second part of the woven strip 3 extending from a second side of the split rod 2 comprises, on its second face, at least two balls 4, in particular made of tungsten carbide and two abrasive zones 5a,5b covered with abrasive grains of different sizes.

[0034] On both sides of the split rod 2, the balls 4 are arranged so as to be further away from the split rod 2 than the abrasive areas 5a,5b.

[0035] Similarly, on both sides of the split rod 2, the abrasive areas 5b covered with abrasive grains of a first size are arranged so as to be further away from the split rod 2 than the abrasive areas 5a covered with abrasive grains of a second size larger than the first size.

[0036] The arrangement of the balls 4 and the abrasive zones 5a, 5b is advantageously chosen so that, during use, the coarsest abrasive grains come into contact with the material first, followed by the finer grains, which in turn precede the balls 4. This arrangement allows for the simultaneous removal of the defect present on the surface to be machined, while simultaneously generating a suitable surface finish, before the impact of the tungsten balls 4, which compresses the surface. In such a rotation mode, the tool rotates in only one direction, so that the faces of the woven belt 3 covered with grains and balls 4 come into contact with the surface.

[0037] In such an embodiment, the tool is rotated at a speed intermediate between the tool rotation speed when an abrasive belt is used for abrasive fitting and the tool rotation speed when a roto-grooving tool is used. In particular, the tool rotation speed is chosen to obtain a level of preload required for the workpiece.

[0038] Usually, for rotary tools of comparable size, the rotational speed is about 10 times higher for fitting than for shot peening.

[0039] More specifically, the rotational speed for the adjustment is usually between 3000 and 30000 rpm, typically 10000 or 20000 rpm, while the speed for the roto-shot blasting is about 1000 rpm.

[0040] By contrast, in the embodiment described above, a rotation speed between 500 and 15000 rpm, or even between 700 and 5000 rpm or even between 1000 and 3000 rpm would be suitable.

[0041] Figure [Fig. 2] illustrates an adjustment phase during which abrasive grains come into contact with the surface. Figure [Fig. 3] illustrates a modification phase of the prestressing during which balls 4 come into contact with the surface.

[0042] In a second embodiment illustrated by figure [Fig.4], the arrangement of the balls 4 and the abrasive zones 5a,5b on each side of the split rod 2 differs.

[0043] The woven strip 3 extending from a first side of the split rod 2 comprises at least two balls 4, on the first face of the woven strip 3 and two abrasive zones 5a,5b covered with abrasive grains of different sizes on the second face of the woven strip 3.

[0044] The woven strip 3 extending from a second side of the split rod 2 comprises at least two balls 4, on the second face of the woven strip 3 and two abrasive areas 5a,5b covered with abrasive grains of different sizes on the first face of the woven strip 3.

[0045] On both sides of the split rod 2, the balls 4 are arranged so as to be further away from the split rod 2 than the abrasive areas 5a,5b arranged opposite each other on the opposite face.

[0046] Similarly, on both sides of the split rod 2, the abrasive areas 5a,5b covered with abrasive grains of a first size are arranged so as to be further away from the split rod 2 than the abrasive areas covered with abrasive grains of a second size larger than the first size.

[0047] In such an embodiment, the slotted rod 2 is rotated first in a first direction at a first speed so that only the abrasive areas 5a, 5b come into contact with the surface. The slotted rod 2 is then rotated in a second direction at a second speed so that only the balls 4 come into contact with the surface.

[0048] It is thus possible to use the same fitting and preloading system to perform only fitting or only preloading by the same operator. Another advantage of this embodiment is that it does not require an intermediate rotational speed resulting from a compromise between the rotational speed during fitting and the rotational speed during shot peening.

[0049] The change in direction of rotation can be carried out automatically, for example after a predetermined time, or on the operator's instructions.

[0050] Regardless of the embodiment described above considered, and in a specific embodiment, the part of the woven strip 3 extending from a first side of the split rod 2 has the same size as the part of the woven strip 3 extending from the second side of the split rod 2.

[0051] Similarly, the adjustment and prestressing system has been described with a single woven strip 3. However, a larger number of woven strips can be considered, in particular two woven strips.

[0052] The adjustment and preload system thus combines the action of an abrasive tool The flexible design, similar to that of a rotary shot blasting belt, combines tungsten carbide shot (4) and abrasive grains of various types and grades (5a, 5b) on the same support, enabling adjustment and local compression using a single tool. This combination of actions offers significant synergy, particularly when performed simultaneously, by minimizing the repetition of masking operations and workpiece handling. It also results in time savings and increased reliability due to the difficulty of omitting any of the actions.

[0053] The adjustment and preloading system may be in the form of a handheld tool that can be held in at least one hand by an operator, well suited for local touch-ups.

[0054] Finally, and surprisingly, it is possible to visually check that the shot blasting has been carried out correctly, even though the two operations are carried out at the same time.

Claims

Claims

1. Adjustment and prestressing system for adjusting and compressing a surface of a part, comprising a rod (2), at least a first fin and a second fin fixed on the rod (2) and arranged on either side of the rod (2), balls (4) and abrasive zones (5a, 5b) are arranged on each fin, the system further comprising controllable rotation means configured to rotate the rod (2) in at least one direction of rotation so that the balls (4) and the abrasive zones (5a, 5b) come into contact with the surface to be adjusted and compressed, characterized in that the abrasive zones (5a, 5b) are arranged so that the abrasive zones covered with abrasive grains of larger grain size (5a) are arranged closer to the rod (2) than the abrasive zones covered with abrasive grains of smaller grain size (5b).

2. Adjustment and prestressing system according to claim 1, in which the balls (4) are arranged so as to be further from the rod (2) than the abrasive zones (5a, 5b).

3. Adjustment and prestressing system according to one of claims 1 or 2, in which each fin comprises a first face and a second face opposite the first face, the first faces being arranged on the same side of the assembly formed by the first fin and the second fin, the second faces also being arranged on the same side of this assembly, the balls (4) and the abrasive zones (5a, 5b) being arranged on the first face of the first fin and on the second face of the second fin.

4. Adjustment and prestressing system according to one of claims 1 or 2, in which each fin comprises a first face and a second face opposite the first face, the first faces being arranged on the same side of the assembly formed by the first fin and the second fin, the second faces also being arranged on the same side of this assembly, the balls (4) being arranged on the first face of the first fin and on the second face of the second fin, the abrasive zones (5a, 5b) being arranged on the second face of the first fin and on the first face of the second fin.

5. An adjustment and prestressing system according to any one of claims 1 to 4, wherein the first fin and the second fin are formed respectively by a first part and a second part of the same strip (3) fixed on the rod (2).

6. A method of adjusting and prestressing in which the surface of a part undergoes an adjusting step and a local compression step by means of the adjusting and prestressing system according to one of claims 1 or 2, in which the tool is rotated in at least one direction of rotation so that the balls and the abrasive zones are successively brought into contact with the surface of the part.

7. A method of adjusting and prestressing in which the surface of a part undergoes an adjusting step and a local compression step by means of the adjusting and prestressing system according to claim 3, in which the tool is rotated in a single direction so that the abrasive zones covered with larger grains come into contact with the surface of the part to be adjusted before the abrasive zones covered with smaller grains and the balls.

8. A method of adjusting and prestressing in which the surface of a part undergoes an adjusting step and a local compression step by means of the adjusting and prestressing system according to claim 4, in which the tool is rotated in a first direction with a first rotational speed so that the abrasive zones come into contact with the surface of the part to be adjusted and in a second direction with a second rotational speed so that the balls come into contact with the surface of the part to be adjusted and compressed.

9. A method of adjusting and prestressing according to claim 8, wherein the change of direction of rotation is carried out at the request of the operator.

10. Adjustment and prestressing method according to claim 8, in which the change of direction of rotation is carried out automatically, in particular as a function of the elapsed time.