Article for the repair of painted surfaces, and method for manufacturing such an article

The article with controlled adhesion forces and protective layers facilitates quick and safe repair of painted surfaces, addressing the inefficiencies and health risks of conventional methods by eliminating the need for liquid paint application.

FR3147732A1Pending Publication Date: 2024-10-18CORSO MAGENTA
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
FR2023003776
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Conventional methods for repairing painted surfaces are tedious, time-consuming, and expose operators to harmful volatile organic compounds, while certain regulations prohibit simultaneous operations, lengthening maintenance times.

Method used

An article comprising a dry paint layer, an activatable adhesive layer, and a protective layer with controlled adhesion forces, along with a protective film, is used to facilitate the repair process, allowing for a method that avoids applying paint in liquid form and ensures quick, safe, and durable repairs.

Benefits of technology

The solution enables efficient and safe repair of painted surfaces, meeting regulatory health and safety criteria while minimizing exposure to hazardous substances and reducing maintenance time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention proposes an article comprising: - a layer (20) of dry paint, - a layer (30) of an activatable adhesive adjacent to the dry paint layer, - a protective layer (40) adhering to the dry paint layer on its side opposite the adhesive layer, and - a protective film (31; 31') attached to the adhesive layer (30) on its side opposite the dry paint layer, wherein the adhesion forces between the protective layer (40) and the dry paint layer (20) are controlled and are between the adhesion forces between the protective film (31; 31') and the adhesive layer before activation of the latter and the adhesion forces between the paint layer (20) and a final substrate, via the adhesive layer (30) after activation. Particularly applicable to the repair of painted surfaces in various industries. (Fig. 3)
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Article for repairing painted surfaces, and method of manufacturing such an article

[0001] The present invention relates generally to the repair of painted surfaces, in particular surfaces having a quality requirement from the point of view of technical regulations.

[0002] Conventionally, the repair of painted surfaces is carried out by stripping a minimal area to be repainted, smoothing and then applying one or more layers of paint in liquid form.

[0003] It is understood that these operations are tedious and time-consuming, and expose operators to volatile organic compounds that are dangerous to health. Furthermore, in certain fields such as aeronautical maintenance, certain rules prohibit such operations from being carried out simultaneously with other operations, which adversely lengthens maintenance times.

[0004] The present invention aims to provide an article making it possible to greatly facilitate the repair of damaged paint areas with regard to these problems, as well as a particular method of manufacturing such an article.

[0005] For this purpose, an article is proposed, in particular for the repair of painted surfaces, comprising: - a layer of dry paint, - a layer of activatable adhesive attached to the dry paint layer, - a protective layer adhering to the dry paint layer on the side of the latter opposite the adhesive layer, and - a protective film attached to the adhesive layer on the side opposite the dry paint layer, where the adhesion forces between the protective layer and the dry paint layer are controlled and range between the adhesion forces between the protective film and the adhesive layer before activation of the latter and the adhesion forces between the paint layer and a final support, via the adhesive layer after activation.

[0006] Certain preferred but non-limiting aspects of this article include the following features, taken individually or in any combinations that the person skilled in the art will understand to be technically compatible with each other:

[0007] * the protective layer is coated with an adhesive chosen to provide the forces controlled membership.

[0008] * the outline of the protective layer is distinguished from the outline of the formed assembly by the paint layer and the adhesive layer activatable by the presence of at least a gripping tab extending outwards.

[0009] * the outline of the protective film extends on all sides compared to the outline of the assembly formed by the layer of paint and the layer of activatable adhesive.

[0010] * the or each gripping tab is inscribed in the outline of the film of protection.

[0011] According to a second aspect, a method of manufacturing an article for the repair of painted surfaces is provided, comprising the following steps: - apply at least one layer of paint material on a temporary molding support, - dry the layer or layers of material to be painted, - apply a protective layer of paint to the intermediate article, - separate from the temporary support an intermediate article formed from the paint layer and the protective layer, - apply a layer of an activatable adhesive with a protective film against the exposed face of the paint layer, the protective film being on the side of the adhesive layer opposite the paint layer, where the adhesion forces between the protective layer and the dry paint layer are controlled and range between the adhesion forces between the protective film and the adhesive layer before activation of the latter and the adhesion forces between the paint layer and a final support, via the adhesive layer after activation.

[0012] According to a third aspect, there is provided a method of manufacturing an article for the repair of painted surfaces, comprising the following steps: - apply at least one layer of paint material on a temporary molding support, - dry the layer or layers of material to be painted, - apply a layer of an activatable adhesive with a protective film against the exposed face of the paint layer, the protective film being on the side of the adhesive layer opposite the paint layer, - separate from the temporary support an intermediate article formed from the paint layer, the adhesive layer and the protective film, and - apply a protective layer of paint to the intermediate article, where the adhesion forces between the protective layer and the dry paint layer are controlled and range between the adhesion forces between the protective film and the adhesive layer before activation of the latter and the adhesion forces between the paint layer and a final support, via the adhesive layer after activation.

[0013] Certain preferred but non-limiting aspects of this method include the features following characteristics, taken individually or in any combination that the person skilled in the art will understand to be technically compatible with each other:

[0014] * the temporary molding support is provided with aero performance hollows / reliefs dynamics transferred to the paint layer during its application.

[0015] * the protective layer is provided on its outer face with a marking indicating the orientation of the hollows / reliefs.

[0016] * the first protective layer is coated with an adhesive chosen to provide the controlled adhesion forces.

[0017] * the outline of the first protective layer is distinguished from the outline of the assembly formed by the layer of paint and the layer of adhesive activatable by the presence of at least one gripping tab projecting externally.

[0018] * the outline of the protective film extends on all sides compared to the outline of the assembly formed by the layer of paint and the layer of activatable adhesive.

[0019] * the or each gripping tab is inscribed in the outline of the film of protection. Brief description of the drawings

[0020] Other aspects, aims and advantages of the present invention will appear better on reading the following detailed description of preferred embodiments thereof, given by way of non-limiting example and made with reference to the appended drawings, in which:

[0021] [Fig.lA] to [Fig.lE] are enlarged sectional views illustrating different stages of manufacturing an article according to a first exemplary embodiment of the invention,

[0022] [Fig.2] is a sectional view, enlarged in the direction of the thickness, of an article according to an example of an embodiment of the invention,

[0023] [Fig.3] is a bottom plan view of the article of [Fig.2], and

[0024] [Fig.4] is a sectional view of the article after application, and

[0025] [Fig.5A] to [Fig.5E] are enlarged sectional views illustrating various steps of manufacturing an article according to a second exemplary embodiment of the invention,

[0026] Detailed description of preferred embodiments

[0027] We will now describe an article which makes it possible in particular to repair a damage to paint applied to a structure, in particular an aircraft, while avoiding having to resort again to all the phases necessary for applying the paint in liquid form, thus saving time and easily satisfying the regulatory criteria of health, safety and environment (HSE) while obtaining a repair of very good durability.

[0028] With reference to the drawings, and firstly to Figs. 1A to 1E, there is firstly provided ([Fig.1A]) a temporary molding support 10, the state of the molding surface 11 of which is suitable for determining, by molding effect, the surface condition of a layer of paint. In this embodiment, this surface is generally smooth, or has a surface condition adapted to the adhesiveness of a layer of adhesive as will be described below.

[0029] This molding support is made for example from one of the following materials: polypropylene, polyethylene, polyethylene terephthalate, silicone paper.

[0030] At the step of [Fig.lB], one or more layers of paint 20 are applied to the face 11 of the molding support.

[0031] If necessary, an agent for modifying the surface activity of the face 11 of the molding support 10, such as a surfactant, is applied thereto before the application of the paint 20 to limit coalescence and make it possible to obtain a film of uniform thickness.

[0032] The paint may be of the single-component or two-component type, for example of the polyurethane, epoxy, acrylic or polyester type. Depending on the desired application, one or more layers of appropriate thickness are applied.

[0033] Generally speaking, the total thickness of the paint layer(s) 20 is chosen according to the type of paint and the application. For an application in aeronautical repair, the thickness is chosen to be as thin as possible, in line with any regulatory requirements, for reasons of minimizing weight. It may depend on the repair area concerned. For other applications, criteria of mechanical resistance to shocks, erosion, UV barrier, chemical resistance to certain aggressive agents, etc. may in particular be retained.

[0034] By “paint” we also mean gel-coats, colorless varnishes, a layer of varnish then being applied first on the temporary support 10, to become the outer layer as will be understood below.

[0035] In the case of an article qualified for repair for a certain application, a paint is used which is itself qualified for this application, available from various manufacturers. For example, for an aeronautical application, a paint conforming to the AMS 3095A standard is used, while for naval or industrial applications, a paint certified by the ACQPA is advantageously used.

[0036] One property that may be important for applications is resistance to aggressive agents such as Skydrol®.

[0037] As stated, the thickness of the layer 20 depends in particular on the type of paint and the application considered. It may result from a compromise between a degree of protection to be provided (for example UV barrier) and weight constraints, in particular in aeronautics.

[0038] As a general rule, the total thickness of the layer 20 is of the order of 25 to 100 μm, preferably around 40 to 70 pm for application in aeronautical repair on unexposed parts.

[0039] For certain applications, in particular for the repair of anti-erosion coatings on certain parts of aircraft (leading edges of wings, radome in particular), the thickness of the paint layer can reach 600 μm. In industrial or naval applications, intermediate thicknesses can be used.

[0040] Referring now to [Fig. 1C], a protective film 40 intended to protect the paint layer during application of the article as will be described later is applied to the intermediate article consisting of the intermediate support 10 and the paint layer 20, once dried, on the side of the latter.

[0041] This protective film 40 is preferably made up of:

[0042] - either the combination of a transfer film (“application tape” in English) by example of polypropylene and a layer of adhesive, such as an acrylic adhesive or an elastomer / resin mixture, typically having a total thickness of between 25 and 100 pm,

[0043] - either a peelable varnish which is applied for example by coating on the layer of paint and which, after drying, forms a flexible, non-brittle and cohesive protective film; this varnish can be based on polyvinyl acetate or polyester for example, and have a thickness after drying of between 100 and 300 pm.

[0044] The adhesive properties of the protective film 40 on the paint layer 20 after application are determined so that the adhesive forces between the film 40 and the paint layer 20 are greater than the adhesive forces between said paint layer 20 and the temporary support 10. In this way, it becomes possible to separate the assembly formed by the paint layer 20 and the protective film 40, from the temporary support 10 by exerting traction at the protective film, as illustrated in [Fig. 1D]. An intermediate article consisting of the paint layer 20 and the protective film 40 is thus obtained.

[0045] With reference to [Fig. 1E], the following step consists of applying, on the face of the paint layer 20 opposite the protective film 40, a layer of adhesive 30. The adhesive is advantageously chosen from a group comprising pressure-sensitive adhesives (PSA), structural liquid adhesives, in particular of the acrylic, polyurethane, cyanoacrylate, vinyl acetate, epoxy, phenolic, cyanoacrylate, anaerobic type (for example with UV polymerization), or even of the hotmelt type.

[0046] The application of the adhesive depends on its nature. In the case of film adhesive, this is simply laminated with the assembly formed by the protective film of the paint layer 20, on the side of the paint layer. It should be noted that the adhesive layer 30 at this stage may be secured to a protective film 31 (“liner” in ter Anglo-Saxon minology) which aims to support and / or protect it.

[0047] If necessary, the protective film 31 which accompanied the adhesive 30 during its application can be removed and replaced by another protective film 31' of dimensions larger than the final size of the assembly formed by the layer of paint 20 and the layer of adhesive 30, as will be seen in detail below. The film 31 or 31' is advantageously a paper coated with polyethylene, polypropylene or polyester, coated with a silicone-type release agent, with a thickness of the order of 50 to 150 μm.

[0048] The adhesive is preferably a pressure-sensitive adhesive (PSA), chosen according to the constraints of the application concerned (in particular resistance to various aggressive phenomena: thermal differences, UV radiation, chemical attack by products such as Skydrol® in the aeronautical industry or other aggressive agents in other industries), and to provide adhesion properties adapted to the application (resistance to detachment by traction or by shear.

[0049] The thickness of the adhesive layer is typically between 25 and 250 μm.

[0050] A successfully tested product is an acrylic type adhesive transfer tape with a thickness of around 50 μm.

[0051] The final article is illustrated in Figs. 2 and 3.

[0052] The assembly formed by the layers of paint 20 and adhesive 30 is here generally circular in shape, with a diameter typically between 1 and 100 cm, the outline of this assembly being designated by CL. All other shapes can of course be envisaged.

[0053] The protective film 31' of the adhesive 30 here has larger dimensions than those of the assembly 20, 30, so as to have a contour C2, here of square shape, which extends beyond the contour C1 on all sides, for purposes explained later, forming a marginal zone 310'.

[0054] Finally, the protective film 40 for the application has a contour generally identical to the contour C1, with the notable presence of a gripping tab 42 (or two or more tabs) projecting outwards relative to this contour, for purposes explained later.

[0055] The application of the article will now be described.

[0056] Firstly, the protective film 31' is gripped at any of the regions of its marginal zone 310', to progressively expose the adhesive layer on the side of the final support, consisting of an area to be repaired, previously cleaned and prepared, here an area to be repaired of an aircraft. This removal of the film 31' is carried out progressively as the article is applied against the area to be repaired, avoiding the trapping of air bubbles. For this purpose, the mechanical properties of the film 31 are chosen to allow its bending over 180° with a limited radius of curvature without inducing a risk of breakage.

[0057] This type of procedure is suitable for certain PSA or hotmelt-PSA type adhesives, allowing significant flexing without loss of cohesion. With other types of adhesive such as a structural adhesive, it may be preferable to first remove the entire protective film 31' and then apply the article to the surface to be repaired, using any appropriate debubbling method.

[0058] The fact that the film 31' extends on all sides relative to the contour C1 makes it easier to remove regardless of the orientation of the article at the time of application.

[0059] Once the article has been applied and the protective film 31' has been completely removed, a roller-type tool is applied with appropriate pressure to the exposed surface of the protective film 40 to smooth the article and activate the adhesive 30 of material to achieve final bonding between the article and the area to be repaired. It will be noted here that the presence of the thin layer of adhesive between the film 40 and the layer of paint 20 makes it possible to avoid relative slippage between these two elements during this operation. This risk of slippage, or damage to the film 40 or, even more disadvantageously, to the layer of paint, can further be minimized by having minimal friction forces between the external surface of the film 40 and the tool, thanks to the materials chosen for these elements.

[0060] After this activation, the adhesion forces between the treated area (or final support) and the article are greater than the adhesion forces between the paint layer 20 and the protective film 40, given by the adhesive 41. Thus, by exerting progressive traction at the level of the tab 42, the protective film 40 can be removed without risking detaching the article from its final support. The assembly obtained is illustrated in [Fig.4], with an exaggerated thickness.

[0061] In practice, the thicknesses of the layers 30 and 20 are such that the transition between the edges of the article and the rest of the substrate S (aircraft part) is barely visible, and the physical and chemical resistance of the article is comparable to that of the neighboring parts of the substrate S.

[0062] It should be noted that from an industrial point of view, it may be advantageous to provide the articles as described above in the form of a larger element in which a plurality of articles are obtained by cutting.

[0063] In this case, the manufacturing method described above comprises the production of a set of individual intermediate articles on a strip constituting the molding support 10, and the transfer, by calendering, of the intermediate articles onto the protective film 40 then constituting, for the handling part, a common support for the articles.

[0064] Another embodiment will now be described with reference to Figs. 5A-5E. of a method for producing an article according to the invention.

[0065] First of all, a temporary molding support 10 is provided ([Fig.5A]), the state of the molding surface 11 of which is here appropriate for determining, by molding effect, the surface state of a layer of paint which will be exposed on the exterior after the article has been installed, as will be understood below.

[0066] This molding support 10 may be structurally similar to that of the first embodiment. It may be smooth or have any desired hollow or relief pattern, such as a material effect or micro-grooves or micro-ribs, obtained for example by calendering, to form by molding effect corresponding hollow-reliefs on the exposed face of the paint as will be understood below.

[0067] At the step of [Fig.5B], one or more layers of paint 20 are applied to the face 11 of the molding support.

[0068] Here again, if necessary, an agent for modifying the surface activity of the face 11 of the molding support 10, such as a surfactant, is applied thereto before the application of the paint 20 to limit coalescence and make it possible to obtain a film of uniform thickness.

[0069] The type of paint (or varnish), the number of layers and the thicknesses of the layers may be similar to what has been described for the first embodiment, with the necessary adaptations to the type of application. It should be noted, however, that the first layer (the one applied to the support 10) will be the layer exposed on the outside, and its characteristics are adapted if necessary (whereas in the first embodiment, it is the final layer which is exposed on the outside).

[0070] With reference to [Fig.5C], the next step consists of applying to the layer of paint 20, after drying, a layer of adhesive 30. The nature of the adhesive and its application method may be of the same type as those described in the first embodiment of the method.

[0071] Here again, the choice of the adhesive 30, its thickness and the conditions of its application to the paint layer 20 are such that the adhesive forces between the adhesive 30 and the paint are greater than the adhesive forces between the paint film 20 and the temporary support 10. In this way, it becomes possible to separate the assembly formed by the paint layer 20 and the adhesive layer 30 possibly provided with its film 31, from the temporary support 10 by exerting traction at the adhesive layer 30, as illustrated in [Fig.5D]. An intermediate article is thus obtained consisting of the paint layer 20 and the adhesive layer 30 possibly protected by its film 31.

[0072] As previously, if necessary, the protective film 31 which accompanied the adhesive 30 during its application can be removed and replaced by another protective film 31' of dimensions larger than the final size of the assembly formed. by the paint layer 20 and the adhesive layer 30, as will be seen in detail below. The film 31 or 31' is advantageously identical or similar to that described previously.

[0073] Referring now to [Fig.5E], a protective film 40 is applied to the intermediate article, on the side of the paint layer 20, intended to protect the paint layer during the application of the article as will be described later.

[0074] This protective film 40 is for example identical or similar to that described with reference to the first embodiment.

[0075] The final article in its general configuration is as illustrated in Figs. 2 and 3. The contours and dimensions of the various constituents of the article may also be as previously described, and its method of installation will also be similar.

[0076] As stated, the present invention has numerous applications, including repair and decoration in the fields of aeronautics, aerospace, naval / maritime / offshore, land transport, industry, construction, and renewable energy. Decoration is understood here to mean the application of articles of any shape, such as decoration, marking, or identification, on bare (metallic, synthetic, composite, etc.) or painted surfaces.

[0077] The person skilled in the art will be able to make numerous variations and modifications to it using his normal skills.

[0078] In particular, in an aeronautical application, with the implementation of the second embodiment, the layer of paint can be, as has been said, provided with aerodynamic performance hollows / reliefs (in particular of the “riblets” type in English), obtained by molding effect by appropriately structuring the molding support 10.

[0079] These aerodynamic elements must have a certain orientation relative to the air flow to which the aircraft is exposed in flight, and in this case, it is possible to provide on the visible surface of the layer 40 a marking indicating the orientation of these hollows / reliefs, so that when the article is laid, it is applied with the appropriate orientation relative to the air flow which will circulate over this area during flight.

Claims

Claims

1. Article in particular for the repair of painted surfaces, comprising: - a layer (20) of dry paint, - a layer (30) of an activatable adhesive adjoining the layer of dry paint, - a protective layer (40) adhering to the layer of dry paint on the side thereof opposite the adhesive layer, and - a protective film (31; 31') attached to the adhesive layer (30) on the side thereof opposite the layer of dry paint, wherein the adhesion forces between the protective layer (40) and the layer of dry paint (20) are controlled and comprised between the adhesion forces between the protective film (31; 31') and the layer of adhesive before activation of the latter and the adhesion forces between the layer of paint (20) and a final support, via the layer of adhesive (30) after activation.

2. The article of claim 1, wherein the protective layer (40) is coated with an adhesive (41) selected to provide controlled adhesion forces.

3. Article according to claim 1 or 2, in which the contour of the protective layer (40) is distinguished from the contour (Cl) of the assembly formed by the layer of paint (20) and the layer of activatable adhesive (30) by the presence of at least one gripping tab (42) projecting externally.

4. Article according to one of claims 1 to 3, in which the contour (C2) of the protective film (31; 31') extends on all sides relative to the contour (Cl) of the assembly formed by the layer of paint (20) and the layer of activatable adhesive (30).

5. Article according to claims 3 and 4 taken in combination, in which the or each gripping tab (42) is inscribed in the contour (C2) of the protective film (31; 31').

6. Method of manufacturing an article for the repair of painted surfaces, comprising the following steps: - applying at least one layer of paint material (20) to a temporary molding support (10), - drying the or each layer (20) of material to be painted, - applying to the intermediate article a layer (40) for protecting the layer of paint (20), - separating from the temporary support (10) an intermediate article formed of the paint layer (20) and the protective layer (40), - applying a layer (30) of an activatable adhesive provided with a protective film (31) against the exposed face of the paint layer (20), the protective film (31) being located on the side of the adhesive layer (30) opposite the paint layer (20), where the adhesion forces between the protective layer (40) and the dry paint layer (20) are controlled and comprised between the adhesion forces between the protective film (31; 31') and the adhesive layer before activation of the latter and the adhesion forces between the paint layer (20) and a final support, via the adhesive layer (30) after activation.

7. A method of manufacturing an article for repairing painted surfaces, comprising the following steps: - applying at least one layer of paintable material (20) to a temporary molding support (10), - drying the or each layer (20) of material to be painted, - applying a layer (30) of an activatable adhesive provided with a protective film (31) against the exposed face of the paint layer (20), the protective film being located on the side of the adhesive layer (30) opposite the paint layer (20), - separating from the temporary support (10) an intermediate article formed from the paint layer (20), the adhesive layer (30) and the protective film (31), and - applying to the intermediate article a layer (40) for protecting the paint layer (20), where the adhesion forces between the protective layer (40) and the dry paint layer (20) are controlled and between the adhesion forces between the protective film (31 ;31') and the adhesive layer before activation of the latter and the adhesion forces between the paint layer (20) and a final support, via the adhesive layer (30) after activation.;

8. A method according to claim 7, wherein the temporary moldable support is provided with aerodynamic performance depressions / reliefs transferred to the paint layer during its application.

9. Method according to claim 8, in which the protective layer (40) is provided on its outer face with a marking indicating the orientation of the hollows / reliefs.

10. A method according to one of claims 7 to 9, wherein the first protective layer (40) is coated with an adhesive (41) selected to provide controlled adhesion forces.

11. Method according to one of claims 7 to 10, in which the contour of the first protective layer (40) is distinguished from the contour (Cl) of the assembly formed by the layer of paint (20) and the layer of activatable adhesive (30) by the presence of at least one gripping tab (42) projecting externally.

12. Method according to one of claims 7 to 11, in which the contour (C2) of the protective film (31; 31') extends on all sides relative to the contour (Cl) of the assembly formed by the layer of paint (20) and the layer of activatable adhesive (30).

13. Method according to claims 11 and 12 taken in combination, in which the or each gripping tab (42) is inscribed in the contour (C2) of the protective film (31; 31').

Citation Information

Patent Citations

  • Process for repairing locally defined defects in a lacquer using a repairing device comprises applying a lacquer layer onto a film-like support and applying the lacquer layer before hardening onto the region to be repaired

    DE10139729A1

  • Dry primer film composite and use thereof

    EP2969253B1

  • Extrusion method of making a dry paint transfer laminate

    US20040159969A1

  • Multi-layer dry paint decorative laminate having discoloration prevention barrier

    US20050196607A1